Semiconductor device, and method for manufacturing semiconductor device
The semiconductor device design addresses warpage issues in CSP structures by employing a structured layout of metal and resin layers with controlled thermal expansion, achieving reduced warpage and stability.
Patent Information
- Application Number
- JP2023045929
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-22
- Publication Date
- 2024-10-04
AI Technical Summary
Warping of semiconductor wafers during the manufacturing process of CSP structures is a challenge, particularly influenced by the size of the semiconductor chip and its electrodes, which existing methods have not adequately addressed.
A semiconductor device design featuring a support base with thin-film and thick-film metal electrodes and resin layers, along with specific films and resin bodies, arranged to manage thermal expansion coefficients, reducing stress and warpage through a structured layout.
The design effectively reduces warpage in semiconductor devices by managing thermal stress, ensuring a flat and stable structure for chip size packages.
Smart Images

Figure 2024135306000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a semiconductor device and a method for manufacturing the same. [Background technology]
[0002] Patent Document 1 discloses minimizing bending of a semiconductor device obtained by dividing a wafer. This manufacturing method includes a first bonding step, a thinning step, a division step, a second bonding step, and a peeling step. In the first bonding step, a support plate is bonded to a first main surface of a wafer having an integrated circuit formed on the first main surface. In the thinning step, the second main surface of the wafer is polished or ground after the first bonding step to thin the wafer. In the dividing step, the wafer is divided into a plurality of chip body parts simultaneously with or after the thinning step. In the second bonding step, after the dividing step, a plurality of reinforcing layers are bonded to the second main surfaces of the plurality of chip body parts 10, respectively. In the peeling step, the support plate is peeled off after the second bonding step. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2016-146395 A Summary of the Invention [Problem to be solved by the invention]
[0004] In a manufacturing method of a semiconductor device for a CSP structure (chip size package, or chip scale package), warpage of a wafer during the manufacturing process can become an obstacle in various processes.
[0005] In the past, attention has been focused on reducing warpage in large semiconductor chips in the CSP structure, but warpage is related not only to the size of the semiconductor chip but also to the size of the electrodes related to the CSP structure in the semiconductor chip.
[0006] An object of the present invention is to provide a semiconductor device having a CSP structure capable of reducing warpage, and a method for manufacturing the semiconductor device. [Means for solving the problem]
[0007] A semiconductor device according to a first aspect of the present invention includes a support base having a first main surface and a second main surface opposite to the first main surface and comprising a semiconductor, at least one thin-film metal electrode provided on the first main surface of the support base, a thin-film resin layer having a first opening on the thin-film metal electrode and covering an edge of the thin-film metal electrode, at least one thick-film metal body located on the thin-film metal electrode and the thin-film resin layer and including a metal film comprising copper, a thick-film resin body covering a side surface of the thick-film metal body and provided on the first main surface of the support base, a first film provided on at least a portion of the first main surface of the support base, and a second film provided on at least a portion of the second main surface of the support base. a structure including at least one of two films, the first film being provided between the thin film resin layer and the thick film resin body, and the support base being provided between the second film and the thick film resin body, wherein the thick film metal body, the thin film metal electrode, and the support base are arranged in the direction of a first axis, an upper surface of the thick film metal body and an upper surface of the thick film resin body extend along a reference plane intersecting the first axis, a thickness of the thick film metal body is greater than a thickness of the thin film metal electrode, a thickness of the thick film resin body is greater than a thickness of the thin film resin layer, a thermal expansion coefficient of the first film is between a thermal expansion coefficient of the thick film resin body and a thermal expansion coefficient of the semiconductor, and a thermal expansion coefficient of the second film is smaller than a thermal expansion coefficient of the thick film resin body.
[0008] A method for fabricating a semiconductor device according to a second aspect of the present invention includes the steps of: preparing a base substrate having a first main surface and a second main surface opposite to the first main surface, and an array of a plurality of sections each including a semiconductor element on the first main surface; forming a thin-film metal electrode on the first main surface in each of the sections of the base substrate; forming a thin-film resin layer on the first main surface in each of the sections of the base substrate, the thin-film resin layer having a first opening above the thin-film metal electrode and covering an edge of the thin-film metal electrode; forming a structure including at least one of a first film and a second film, the first film being formed on the thin-film resin layer on the first main surface of the base substrate and the second film being formed on the second main surface of the base substrate; forming a thick metal film including a metal film comprising copper on the first main surface in each of the sections of the base substrate, the thick metal film comprising the thin-film metal electrode and the thin-film resin layer having a first opening above the thin-film metal electrode and covering an edge of the thin-film metal electrode. forming a thick metal film located on an electrode and connected to the thin-film metal electrode via the first opening of the thin-film resin layer; forming a thick resin film on the first main surface of each of the sections of the base substrate, the thick resin film covering an upper surface and a side surface of the thick metal film; and, after forming a structure, grinding the thick resin film and the thick metal film to form a thick-film resin body and a thick-film metal body from the thick resin film and the thick metal film, respectively; The thin film metal body, the thin film metal electrode, and the base substrate are arranged in the direction of a first axis, the upper surface of the thick film metal body and the upper surface of the thick film resin body extend along a reference plane intersecting the first axis, the thickness of the thick film metal body is greater than the thickness of the thin film metal electrode, the thickness of the thick film resin body is greater than the thickness of the thin film resin layer, the thermal expansion coefficient of the first film is between the thermal expansion coefficient of the thick film resin body and the thermal expansion coefficient of the semiconductor, and the thermal expansion coefficient of the second film is smaller than the thermal expansion coefficient of the thick film resin body. Effect of the Invention
[0009] According to the above aspect, a semiconductor device having a CSP structure capable of reducing warpage and a method for manufacturing the semiconductor device are provided. [Brief description of the drawings]
[0010] [Figure 1] FIG. 1 is a plan view that illustrates a schematic configuration of a semiconductor device according to the present embodiment. [Diagram 2] FIG. 2 is a diagram showing the semiconductor device according to the present embodiment in a cross section taken along the line II-II shown in FIG. [Diagram 3] FIG. 3 is a diagram showing the semiconductor device according to the present embodiment in a cross section taken along the line III-III shown in FIG. [Figure 4] FIG. 4 is a cross-sectional view showing a step in a method for manufacturing a semiconductor device according to this embodiment. [Diagram 5] FIG. 5 is a cross-sectional view showing a step in a method for manufacturing a semiconductor device according to this embodiment. [Figure 6] FIG. 6 is a cross-sectional view showing a step in a method for manufacturing a semiconductor device according to this embodiment. [Figure 7] FIG. 7 is a cross-sectional view showing a step in a method for manufacturing a semiconductor device according to this embodiment. [Figure 8] FIG. 8 is a cross-sectional view showing a step in a method for manufacturing a semiconductor device according to this embodiment. [Figure 9] FIG. 9 is a cross-sectional view showing a step in a method for manufacturing a semiconductor device according to this embodiment. [Figure 10] FIG. 10 is a cross-sectional view showing a step in a method for manufacturing a semiconductor device according to this embodiment. [Figure 11] FIG. 11 is a cross-sectional view showing a step in a method for manufacturing a semiconductor device according to this embodiment. [Figure 12] FIG. 12 is a diagram showing main steps in the method for manufacturing a semiconductor device according to this embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] Hereinafter, embodiments of the present invention will be described with reference to the drawings.
[0012] Fig. 1 is a plan view showing a schematic diagram of a semiconductor device according to the present embodiment. Fig. 2 is a drawing showing a semiconductor device according to the present embodiment in a cross section taken along line II-II shown in Fig. 1. Fig. 3 is a drawing showing a semiconductor device according to the present embodiment in a cross section taken along line III-III shown in Fig. 1. Hatching in the cross sections of Figs. 2 and 3 is omitted.
[0013] 1, 2 and 3, the semiconductor device 11 has a CSP structure. Specifically, the semiconductor device 11 includes a support base 13 having a semiconductor (e.g., a VI group semiconductor such as silicon), at least one thin-film metal electrode 15, at least one thick-film metal body 17, a thick-film resin body 19, a thin-film resin layer 21, and a structure 24 including at least one of a first film 23 and a second film 25.
[0014] The semiconductor device 11 may have one or more semiconductor elements 31 (e.g., active elements such as transistors) provided in the support base 13. The semiconductor device 11 may also include an insulating structure 33 provided between the thin-film metal electrodes 15 and the semiconductor elements 31. At least one of the semiconductor elements 31 may be electrically connected to at least one thick-film metal body 17 through an opening in the insulating structure 33. The insulating structure 33 may include, for example, one or more insulating films, which may include a silicon-based inorganic insulating film or a resin film.
[0015] The support base 13 has a first main surface 13b and a second main surface 13c opposite to the first main surface 13b. The first main surface 13b has an element area 13d and a peripheral area 13e. The element area 13d includes a semiconductor element 31, and also carries a thick-film resin body 19, a thin-film metal electrode 15, and a thick-film metal body 17. The peripheral area 13e carries a thick-film resin body 19. The thin-film metal electrode 15 and the thick-film metal body 17 are spaced apart from the peripheral area 13e. The peripheral area 13e surrounds the element area 13d. In this embodiment, an exemplary boundary between the peripheral area 13e and the element area 13d is located at the outer edge of the thin-film resin layer 21. However, the position of the boundary is not limited to this example.
[0016] The thin-film metal electrode 15 is provided on the first main surface 13b of the support base 13, and specifically, can be electrically connected to at least one semiconductor element 31. The thin-film metal electrode 15 can include, for example, aluminum.
[0017] The thick film metal body 17 is located on the thin film metal electrode 15 and the thin film resin layer 21. The thick film metal body 17 may include a metal film comprising copper. The thick film metal body 17 may include, for example, a copper plating film and a seed layer for plating.
[0018] The thick film resin body 19 is provided on the first main surface 13b of the support base 13, and covers the side surface 17b of the thick film metal body 17. The thick film resin body 19 may contain an epoxy resin.
[0019] The thin-film resin layer 21 has one or more first openings 22b, 22c, and each of the first openings (22b, 22c) is located above the thin-film metal electrode 15. In one embodiment, the edge 16b of the thin-film metal electrode 15 can be covered, and the thin-film resin layer 21 prevents the thick-film metal body 17 from reaching the underlying structure of the thin-film metal electrode 15 in the element area 13d. The thin-film resin layer 21 can include a polyimide resin.
[0020] The support base 13, the thin-film metal electrode 15, and the thick-film metal body 17 are arranged in the direction of a first axis Ax1. The upper surface 17c of the thick-film metal body 17 and the upper surface 17c of the thick-film resin body 19 can extend along a reference plane REF intersecting the first axis Ax1, and there is substantially no level difference between the upper surface 17c of the thick-film metal body 17 and the upper surface 19c of the thick-film resin body 19.
[0021] The first film 23 of the structure 24 can be provided on at least a portion of the first main surface 13b of the support base 13, and the second film 25 of the structure 24 can be provided on at least a portion of the second main surface 13c of the support base 13. The first film 23 is a single connected region in which the total area of the second openings 23b of the first film 23 is greater than the total area of the upper surface of the first film 23. In this embodiment, the first film 23 can extend outward beyond the boundary between the peripheral area 13e and the element area 13d and reach the edge of the first main surface 13b of the support base 13. In addition, the second film 25 can extend outward on the second main surface 13c beyond the boundary between the element area 13d and the peripheral area 13e and reach the edge of the second main surface 13c of the support base 13.
[0022] The structure 24 can include one or both of a first film 23 and a second film 25. In the exemplary structure 24, the first film 23 can be provided between the thick film resin body 19 and the thin film resin layer 21, and the support base 13 can be provided between the thick film resin body 19 and the second film 25.
[0023] The first film 23 separates the thick film resin body 19 from the support base 13 and the thin film resin layer 21 in the element area 13d. The second film 25 extends along the second main surface 13c of the support base 13. In this example, the second film 25 is provided over the entire second main surface 13c, however, this embodiment is not limited to this arrangement and can be provided over a major portion of the second main surface 13c.
[0024] The thickness D17 of the thick-film metal body 17 is greater than the thickness D15 of the thin-film metal electrode 15, and the thickness D19 of the thick-film resin body 19 is greater than the thickness D21 of the thin-film resin layer .
[0025] In this embodiment, the first film 23 can have a thermal expansion coefficient between the thermal expansion coefficient of the thick-film resin body 19 and the thermal expansion coefficient of the semiconductor of the support base 13. The second film 25 can have a thermal expansion coefficient smaller than the thermal expansion coefficient of the thick-film resin body 19.
[0026] According to the semiconductor device 11, the thickness D17 of the thick-film metal body 17 is greater than the thickness D15 of the thin-film metal electrode 15, and the thickness D19 of the thick-film resin body 19 is greater than the thickness D21 of the thin-film resin layer 21. In this semiconductor device 11, the upper surface 17c of the thick-film metal body 17 and the upper surface 19c of the thick-film resin body 19 extend along the reference plane REF, and a structure for chip size packaging (e.g., a CSP structure) can be provided. In this structure, the structure 24 including at least one of the first film 23 and the second film 25 can reduce warping of the support base 13 due to stress from the thick-film metal body 17 and the thick-film resin body 19.
[0027] In addition, the thermal expansion coefficient of the first film 23 is between the thermal expansion coefficient of the thick film resin body 19 and the thermal expansion coefficient of the semiconductor of the support base 13, thereby reducing the tensile stress from the thick film metal body 17 and the thick film resin body 19 to the support base 13.
[0028] Furthermore, by providing the second film 25 with a thermal expansion coefficient smaller than that of the thick-film resin body 19, the thermal expansion coefficient of the second film 25 can be made closer to that of the support base 13 with reference to the thermal expansion coefficient of the thick-film resin body 19. Therefore, the second film 25 acts to reduce warping of the support base 13.
[0029] The first film 23 may include an inorganic insulator containing silicon and nitrogen, such as SiN, and the second film 25 may include an inorganic insulator containing silicon and nitrogen, such as SiN.
[0030] These films (23, 25) can be formed on a base structure including a resin body such that the film formation temperature does not exceed the heat-resistant temperature of the base structure. The structure 24 can include a silicon-based inorganic oxide film and / or a silicon-based inorganic oxynitride film that can be deposited at a film formation temperature that does not exceed the heat-resistant temperature of the base structure.
[0031] In the structure 24, specifically, the first film 23 has a second opening 23b, and the second opening 23b is located above the first openings 22b, 22c of the thin-film resin layer 21 and the thin-film metal electrode 15. The thick-film metal body 17 is connected to the thin-film metal electrode 15 via the second opening 23b of the first film 23, and in this embodiment, the thick-film metal body 17 is located above the thin-film metal electrode 15 and the thin-film resin layer 21. The first film 23 extends between the support base 13 and the thick-film resin body 19 from the edge of the second opening 23b of the first film 23 toward the edge 13h of the support base 13.
[0032] According to this semiconductor device 11, the first film 23 extends along the support base 13 from the edge of the second opening 23b of the first film 23 toward the edge 13h of the support base 13, and is provided so as to surround the bottom of the thick-film metal body 17. The first film 23 acts to maintain the coplanarity of the support base 13 between the support base 13 and the thick-film resin body 19.
[0033] In this embodiment, the second film 25 can extend from an edge or near the edge of the second major surface 13c, for example a position away from the edge, along the second major surface 13c toward the center of the second major surface 13c.
[0034] In the semiconductor device 11, the second film 25 extends along the second main surface 13c of the support base 13 and acts to maintain the coplanarity of the support base 13.
[0035] 1, four thick-film metal bodies 17 are provided with thick-film resin bodies 19 between them to provide a CSP structure. In the exemplary semiconductor device 11, each of the thick-film metal bodies 17 is connected to the underlying thin-film metal electrodes 15 via a single first opening 22b and a single second opening 23b. In the exemplary semiconductor device 11, the potential stress applied by the thick-film metal body 17 to the support base 13 is related to the volume of the thick-film metal body 17 as well as the area of the top surface 17c of the thick-film metal body 17. The proportion of the thick-film metal body 17 in the support base 13 (hereinafter referred to as the "fill factor") can be defined, for example, in a wafer product in a wafer process or in a semiconductor chip.
[0036] By some estimates, conventional semiconductor chips have a fill factor of 20 to 30 percent. Higher fill factors can be expected in wafer production during wafer processing and in semiconductor chips from the finished wafer production.
[0037] 1, 2 and 3, the thin-film metal electrode 15 may include one or more pad electrodes. The thick-film metal body 17 may include one or more metal posts connected to the pad electrodes of the thin-film metal electrode 15. The first main surface 13b of the support base 13 includes a first area 13f and a second area 13g, in which the first area 13f carries the metal posts of the thick-film metal body 17 and the second area 13g carries the thick-film resin body. In this embodiment, the area of the first area 13f is larger than the area of the second area 13g.
[0038] In this semiconductor device 11, since the area of the first area 13f is larger than the area of the second area 13g, the semiconductor device 11 has a structure in which the support base 13 receives stress from the thick-film metal body 17 in the first area 13f. The thick-film resin body 19 is provided so as to cover the side surface 17b of the thick-film metal body 17 in the second area 13g of the support base 13. In this structure, the support base 13 receives stress from the thick-film resin body 19 in the second area 13g.
[0039] 3, the second main surface 13c has a third area 13i and a fourth area 13j. The third area 13i and the fourth area 13j are defined to correspond to the first area 13f and the second area 13g of the first main surface 13b, respectively, and to be associated with the second main surface 13c.
[0040] The second film 25 can be provided on at least the third area 13i and supports the support base 13 against the thick-film metal body 17. The second film 25 can extend outward (onto the fourth area 13j) beyond the boundary between the third area 13i and the fourth area 13j and supports the support base 13 against the thick-film metal body 17 and the thick-film resin body 19. The second film 25 can be separated from the edge 13h of the support base 13.
[0041] 2 and 3, the thin-film metal electrode 15 is located directly below the thick-film metal body 17. The first openings 22b, 22c of the thin-film resin layer 21 are located above the thin-film metal electrode 15. The thick-film metal body 17 covers the entire upper surface of the thin-film metal electrode 15 at the first openings 22b, 22c of the thin-film resin layer 21, and extends beyond the edge of the thin-film resin layer 21 onto the upper surface of the thin-film resin layer 21.
[0042] The area of the upper surface of the thin-film metal electrode 15 (size W15) is larger than the area of the upper surface of the thin-film resin layer 21 (size W21).
[0043] According to this semiconductor device 11, the thick film metal body 17 is bonded to the thin film metal electrode 15 provided on the first main surface 13b of the support base 13 via the first openings 22b, 22c of the thin film resin layer 21. The thin film resin layer 21 is provided on the first main surface 13b of the support base 13 so as to avoid bonding between the thin film metal electrode 15 and the thick film metal body 17, and provides a planarized surface on the first main surface 13b of the support base 13. The planarized surface is provided to the base of the first film 23, and a potential increase in thermal stress due to bending or steps in the base of the thick film resin body 19 and / or the thick film metal body 17 is avoided.
[0044] 1, 2 and 3, the thick-film metal body 17 covers the entire upper surface of the thin-film metal electrode 15 at the first openings 22b, 22c of the thin-film resin layer 21. The thin-film resin layer 21 is a single connected region in which the total area of the first openings 22b, 22c of the thin-film resin layer 21 is greater than the total area of the upper surface of the thin-film resin layer 21.
[0045] According to this semiconductor device 11, the thin-film resin layer 21 is provided on the first main surface 13b of the support base 13 so as to avoid bonding between the thick-film metal body 17 and the thin-film metal electrode 15, and the total area of the first openings 22b, 22c of the thin-film resin layer 21 is larger than the total area of the upper surface of the thin-film resin layer 21. By forming the thin-film resin layer 21 as a single connected region, the thin-film resin layer 21 can be provided so as to cover a larger portion of the first main surface 13b of the support base 13. A planarized base can be provided for the first film 23.
[0046] Similarly, the thick-film resin body 19 is provided on the first main surface 13b of the support base 13 so as to avoid bonding between the thick-film metal body 17 and the thin-film metal electrode 15. The thick-film resin body 19 is a single connected region in which the total area of the openings of the thick-film resin body 19 is larger than the total area of the upper surface of the thick-film resin body 19.
[0047] 2, the thin-film resin layer 21 has an inner edge 22f that defines the first openings 22b, 22c of the thin-film resin layer 21, and an outer edge 22g that defines the size of the thin-film resin layer 21. The outer edge 22g of the thin-film resin layer 21 is spaced apart from the edge 13h of the support base 13, while the thick-film resin body 19 reaches the edge 13h of the support base 13.
[0048] According to this semiconductor device 11, the thin film resin layer 21 can be provided up to the vicinity of the edge 13h of the support base 13, for example up to the edge of the scribe region of the support base 13.
[0049] Figures 4 to 11 are cross-sectional views showing major steps in a method for manufacturing a semiconductor device according to the present embodiment. Each of Figures 4 to 11 shows the progress of a wafer product during manufacture in a cross section corresponding to the line III-III shown in Figure 1. Hatching has been omitted in each cross section of Figures 4 to 11. Figure 12 is a flow diagram showing major steps in a method for fabricating a semiconductor device according to the embodiment. In the following description, for the purpose of facilitating understanding, the same or similar parts will use, where possible, reference symbols already used in the above description.
[0050] In the first step shown in FIG. 4 (for example, S101 in FIG. 12), a base substrate 41 is prepared by processing, for example, a semiconductor wafer. The base substrate 41 may include a semiconductor, for example, silicon. The semiconductor region of the base substrate 41 has a first main surface 42b and a second main surface 42c opposite to the first main surface 42b. The base substrate 41 has an arrangement (for example, a one-dimensional or two-dimensional array) of a plurality of sections (40 in FIG. 4) on the first main surface 42b. Each of the sections 40 includes a semiconductor element 43. In FIG. 4 to FIG. 11, one section is depicted. The semiconductor element 43 is formed in the semiconductor region. The semiconductor element 43 includes elements, for example, transistors, electrodes, and interconnection wiring, and these elements can be created by applying a plurality of semiconductor processes to a semiconductor substrate, such as a wafer.
[0051] In a second step, the base substrate 41 is covered with an insulating structure 33 to obtain a wafer product 40a. The insulating structure 33 can include at least one of an inorganic insulator and an organic insulator, and specifically, the insulating structure 33 covers the region of the semiconductor element 43.
[0052] 5 (e.g., S102 in FIG. 12), a thin-film metal electrode 15 is formed in each of the sections 40 to obtain a wafer product 40b. The thin-film metal electrode 15 is formed on the first main surface 42b of the base substrate 41, specifically on the insulating structure 33, and can be connected to the semiconductor element 43 in the section 40 through an opening in the insulating structure 33. Semiconductor processes such as metal layer deposition, photolithography, and etching are used to form the thin-film metal electrode 15. The thin-film metal electrode 15 can comprise, for example, aluminum.
[0053] 6 (e.g., S103 in FIG. 12), a thin-film resin layer 21 is formed on the first main surface 42b in each of the sections 40 to obtain a wafer product 40c. The thin-film resin layer 21 has a first opening 22b on the thin-film metal electrode 15 and covers the edge 16b of the thin-film metal electrode 15. The thin-film resin layer 21 is formed using semiconductor processes such as coating of an organic substance, baking, photolithography, and etching. The thin-film resin layer 21 may contain, for example, a polyimide resin.
[0054] 7 (for example, S104 in FIG. 12), a structure 24 is formed. In this step, a first film 23 is formed as an example of the structure 24 to obtain a wafer product 40d. The first film 23 is formed on the thin-film resin layer 21 on the first main surface 42b of the base substrate 41. The first film 23 has a second opening 23b on the thin-film metal electrode 15, and the second opening 23b is aligned with the first opening 22b. In this embodiment, the size of the second opening 23b is larger than the size of the first opening 22b. The first film 23 may include a silicon-based inorganic nitride such as SiN.
[0055] Another example of the structure 24, specifically, the formation of the second film 25, will be described later.
[0056] In a sixth step (e.g., S105 in FIG. 12) shown in FIG. 8, a thick metal film 18 is formed on the first main surface 42b in each of the sections 40 to obtain a wafer product 40e. The thick metal film 18 may comprise copper. The thick metal film 18 is located on the thin-film metal electrode 15 and is connected to the thin-film metal electrode 15 via the first opening 22b of the thin-film resin layer 21. The thick metal film 18 has a thickness greater than that of the thick-film metal body 17. For example, a plating method is used to form the thick metal film 18, and specifically, a semiconductor process such as deposition of a seed layer (and pattern formation, if necessary), formation of an electrolytic plating film, and removal of a sheet layer, if necessary, is used.
[0057] 9 (e.g., S106 in FIG. 12), a thick resin film 20 is formed on the first main surface 42b in each of the sections 40 to obtain a wafer product 40f. The thick resin film 20 is formed so as to cover the upper and side surfaces of the thick metal film 18. The thick resin film 20 has a thickness greater than that of the thick-film resin body 19. The thick resin film 20 also has a thickness greater than that of the thick metal film 18. For example, coating is used to form the thick resin film 20, and more specifically, a semiconductor process such as coating of coating and baking is used. The thick resin film 20 may contain, for example, an epoxy resin.
[0058] 10 (for example, S107 in FIG. 12), the thick resin film 20 and the thick metal film 18 are ground to form a thick-film resin body 19 and a thick-film metal body 17 from the thick resin film 20 and the thick metal film 18, respectively, to obtain a wafer product 40g. Prior to grinding, the wafer product 40e is fixed to a support plate 45. Specifically, the support plate 45 is attached to the second main surface 42c, and is separated from the wafer product 40g after grinding.
[0059] In the wafer product 40 g , in each of the sections 40 , the side surface 17 b of the thick film metal body 17 is covered with the thick film resin body 19 , and the thick film metal body 17 is housed in the opening of the thick film resin body 19 .
[0060] The base substrate 41, the thin-film metal electrode 15, and the thick-film metal body 17 are disposed in the direction of the first axis Ax1. The upper surface 17c of the thick-film metal body 17 and the upper surface 17c of the thick-film resin body 19 can extend along a reference plane REF intersecting the first axis Ax1, and there is substantially no level difference between the upper surface 17c of the thick-film metal body 17 and the upper surface 17c of the thick-film resin body 19.
[0061] According to this manufacturing method, the thickness of the thick-film metal body 17 is greater than the thickness of the thin-film metal electrode 15, and the thickness of the thick-film resin body 19 is greater than the thickness of the thin-film resin layer 21. In this semiconductor device 11, the upper surface 17c of the thick-film metal body 17 and the upper surface 19c of the thick-film resin body 19 extend along the reference plane REF, and a structure for a chip size package can be provided. In this structure, the structure 24 (including the first film 23) can reduce warping of the base substrate 41 due to stress from the thick-film metal body 17 and the thick-film resin body 19 in each section 40.
[0062] In the above manufacturing method, the formation of the structure 24 is described in the fifth step. However, the structure 24 can be formed after the thin film resin layer 21 is formed and before the thick film resin body 19 is formed. Specifically, the first film 23 of the structure 24 can be formed after the thick film metal body 17 is formed, and the first film 23 covers the surface of the thin film resin layer 21 and the side and top surfaces of the thick metal film 18.
[0063] If necessary, the method for manufacturing the semiconductor device 11 can include a ninth step of forming another exemplary structure 24. In the ninth step, a second film 25 is formed on at least a portion of the second main surface 42b to provide a wafer product. The second film 25 can include a silicon-based inorganic nitride, such as SiN.
[0064] The ninth step can be, for example, after any of the first to fourth steps and before the sixth or seventh step.
[0065] 11 (for example, S108 in FIG. 12), the array of sections 40 in the wafer product 40g is separated to obtain a plurality of semiconductor devices 11. Each semiconductor device 11 has the form of a semiconductor chip.
[0066] According to the above manufacturing method, the semiconductor device 11 and the wafer product 40g are provided.
[0067] Next, a description will be given of another method for forming the structure 24. The manufacturing method can include at least the first to fourth steps and the sixth to ninth steps.
[0068] Next, another method for forming the structure 24 will be described. This manufacturing method can include at least steps 1 to 10. In the semiconductor device 11 obtained by this manufacturing method, the structure 24 including both the first film 23 and the second film 25 is provided.
[0069] 10 and 11, it can be seen that each of the sections 40 includes a device area 44b and half of an isolation area 44c. The wafer product 40g (and base substrate 41) comprises a two-dimensional array of sections 40.
[0070] The wafer product 40g (and the base substrate 41) includes a lattice-like arrangement (two-dimensional arrangement) of the element areas 44b, and lattice-like separation areas 44c that define the arrangement of the element areas 44b. The separation area 44c runs between any one of the element areas 44b in the lattice-like arrangement and an element area 44b adjacent to that element area 44b.
[0071] According to this manufacturing method, the warpage of base substrate 41 can be reduced without reducing the shot rate in photolithography.
[0072] The wafer product 40g includes a base substrate 41 and includes element areas 44b in the sections 40 arranged in a lattice pattern and lattice-patterned separation areas 44c running along the boundaries of the sections 40. The wafer product 40g further includes at least one thin-film metal electrode 15 provided on the first main surface 42b in each section or at least one section, and at least one thick-film metal body 17 provided on the first main surface 42b. The wafer product 40g also includes a thick-film resin body 19 provided on the first main surface 42b across the sections 40 and filling the spaces between the thick-film metal bodies 17. The wafer product 40g further includes a structure 24 provided on at least one of the first main surface 42b and the second main surface 42c of the base substrate 41. The structure 24 includes at least one of the first film 23 and the second film 25.
[0073] Wafer product 40g is provided with the above features and, as previously described, wafer product 40g has a large fill factor.
[0074] Referring again to FIG. 12, a method 100 for manufacturing a semiconductor device 11, including some exemplary methods for creating structures, includes a fifth step (step S105) and / or a ninth step. The method 100 may further include at least one of steps S101 to S104 and steps S106 to S108. The individual steps will be described below. In step S101, a base substrate 41 is prepared. In step S102, a thin-film metal electrode 15 is formed. In step S103, a thin-film resin layer 21 is formed. In step S104, a structure 24 including at least one of a first film 23 and a second film 25 is formed. In step S105, a thick metal film 18 is formed. In step S106, a thick resin film 20 is formed. In step S107, the thick metal film 18 and the thick resin film 20 are ground to form a thick-film metal body 17 and a thick-film resin body 19 from the thick metal film 18 and the thick resin film 20, respectively. In step S108, the array of sections 40 in the wafer product 40g is separated to obtain a plurality of semiconductor devices 11. According to the above method 100, the semiconductor device 11 and the wafer product 40g are provided.
[0075] According to the present embodiment, a semiconductor device 11 having a CSP structure capable of reducing warpage and a method 100 for manufacturing the semiconductor device are provided.
[0076] The present invention is not limited to the above-described embodiment, and various modifications can be made without departing from the spirit and scope of the present invention, all of which are included in the technical concept of the present invention. [Explanation of symbols]
[0077] REFERENCE SIGNS LIST 10 chip body, 11 semiconductor device, 13 support base, 13b first main surface, 13c second main surface, 13d element area, 13e peripheral area, 13f first area, 13g second area, 13h edge, 13i third area, 13j fourth area, 15 thin-film metal electrode, 16b edge, 17 thick-film metal body, 17b side, 17c top surface, 18 thick metal film, 19 thick-film resin body, 19c top surface, 20 thick resin film, 21 thin film resin layer, 22b···first opening, 22f···inner edge, 22g···outer edge, 23···first film, 23b···opening, 24···structural body, 25···second film, 31···semiconductor element, 33···insulating structure, 40···section, 40a, 40b, 40c, 40d, 40e, 40f, 40g···wafer product, 41···base substrate, 42b···first main surface, 42c···second main surface, 43···semiconductor element, 44b···element area, 44c···separation area, 45···support plate, Ax1···first axis, REF···reference surface.
Claims
1. a support base having a first major surface and a second major surface opposite the first major surface, the support base comprising a semiconductor; at least one thin film metal electrode disposed on the first major surface of the support base; a thin-film resin layer having a first opening on the thin-film metal electrode and covering an edge of the thin-film metal electrode; at least one thick-film metal body located on the thin-film metal electrode and the thin-film resin layer and including a metal film comprising copper; a thick-film resin body covering a side surface of the thick-film metal body and provided on the first main surface of the support base; a structure including at least one of a first film provided on at least a portion of the first main surface of the support base and a second film provided on at least a portion of the second main surface of the support base, wherein the first film is provided between the thin film resin layer and the thick film resin body, and the support base is provided between the second film and the thick film resin body; Equipped with the thick film metal body, the thin film metal electrode, and the support base are arranged in a direction of a first axis; an upper surface of the thick-film metal body and an upper surface of the thick-film resin body extend along a reference plane intersecting the first axis; the thickness of the thick film metal body is greater than the thickness of the thin film metal electrode; the thickness of the thick film resin body is greater than the thickness of the thin film resin layer; a thermal expansion coefficient of the first film is between a thermal expansion coefficient of the thick-film resin body and a thermal expansion coefficient of the semiconductor; the thermal expansion coefficient of the second film is smaller than the thermal expansion coefficient of the thick-film resin body; Semiconductor device.
2. the thin-film metal electrode includes one or more pad electrodes; the thick-film metal body includes one or more metal pillars connected to the pad electrode, the first main surface of the support base includes a first area on which the metal pillars are mounted and a second area on which the thick-film resin body is mounted; The area of the first area is larger than the area of the second area.
2. The semiconductor device according to claim 1.
3. the thick-film metal body covers the entire upper surface of the thin-film metal electrode in the first opening of the thin-film resin layer, the area of the top surface of the thin-film metal electrode is larger than the area of the top surface of the thin-film resin layer; 2. The semiconductor device according to claim 1.
4. the thin film resin layer is a single connected region, and the total area of the first openings in the thin film resin layer is greater than the total area of the top surface of the thin film resin layer; 2. The semiconductor device according to claim 1.
5. the first film includes an inorganic insulator including silicon and nitrogen; 2. The semiconductor device according to claim 1.
6. the second film includes an inorganic insulator containing silicon and nitrogen; 2. The semiconductor device according to claim 1.
7. providing a base substrate including a semiconductor, the base substrate having a first main surface and a second main surface opposite the first main surface, and an arrangement of a plurality of compartments including semiconductor elements on the first main surface; forming a thin film metal electrode on the first major surface in each of the sections of the base substrate; forming a thin-film resin layer on the first main surface in each of the sections of the base substrate, the thin-film resin layer having a first opening above the thin-film metal electrode and covering an edge of the thin-film metal electrode; forming a structure including at least one of a first film and a second film, the first film being formed on the thin film resin layer on the first main surface of the base substrate, and the second film being formed on the second main surface of the base substrate; forming a thick metal film on the first main surface in each of the sections of the base substrate, the thick metal film including a metal film comprising copper, the thick metal film being located on the thin-film metal electrode and connected to the thin-film metal electrode through the first opening in the thin-film resin layer; forming a thick resin film on the first main surface of each of the sections of the base substrate, the thick resin film covering an upper surface and a side surface of the thick metal film; After forming the structure, grinding the thick resin film and the thick metal film to form a thick film resin body and a thick film metal body from the thick resin film and the thick metal film, respectively; Equipped with the thick-film metal body, the thin-film metal electrode, and the base substrate are arranged in a direction of a first axis; an upper surface of the thick-film metal body and an upper surface of the thick-film resin body extend along a reference plane intersecting the first axis; the thickness of the thick film metal body is greater than the thickness of the thin film metal electrode; the thickness of the thick film resin body is greater than the thickness of the thin film resin layer; a thermal expansion coefficient of the first film is between a thermal expansion coefficient of the thick-film resin body and a thermal expansion coefficient of the semiconductor; the thermal expansion coefficient of the second film is smaller than the thermal expansion coefficient of the thick-film resin body; A method for fabricating a semiconductor device.
Citation Information
Patent Citations
Method for manufacturing semiconductor device and semiconductor device
JP2016146395A