Excimer lamp
The foil electrode design with a flat portion and wedge-shaped ends enhances adhesion and suppresses peeling in small excimer lamps, ensuring stable and efficient operation with low discharge voltage.
Patent Information
- Application Number
- JP2023047045
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-23
- Publication Date
- 2024-10-04
- Estimated Expiration
- 2043-03-23
AI Technical Summary
Small excimer lamps face challenges in ensuring sufficient surface area for electrodes, adhesion between the inner electrode and inner tube, and preventing peeling due to size constraints and electric field concentration.
A foil electrode with a flat portion and wedge-shaped ends is used, where the flat portion has a substantially constant thickness and the ends are sharply angled, enhancing adhesion to the dielectric and suppressing peeling, while maintaining a low discharge starting voltage.
The solution improves adhesion between the foil electrode and dielectric, reduces peeling, and maintains stable discharge with low voltage, ensuring efficient and durable operation of small excimer lamps.
Smart Images

Figure 2024136076000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to an excimer lamp, and more particularly to an electrode configuration. [Background technology]
[0002] In an excimer lamp, an excimer discharge is generated in a discharge space by applying a high-frequency voltage of several kV between a pair of electrodes. For example, in a double-tube excimer lamp, the light-emitting part is composed of two coaxial cylindrical tubes extending in the axial direction, and a discharge gas is sealed in the discharge space formed between the inner tube and the outer tube.
[0003] Then, a high-frequency voltage is applied between an electrode provided in the inner tube or on the tube wall and an electrode (outer electrode) on the surface side of the outer tube, to cause discharge light emission. Also known is an electrode structure in which a foil-shaped electrode is covered with an inner tube and embedded in a dielectric (see Patent Documents 1 and 2). [Prior art documents] [Patent documents]
[0004] [Patent Document 1] Patent No. 6557011 [Patent Document 2] Patent No. 5504095 Summary of the Invention [Problem to be solved by the invention]
[0005] For example, in the case of small excimer lamps with an arc tube outer diameter of 30 mm or less, unlike large excimer lamps, there are restrictions on the shape and structure of the arc tube and electrodes, input voltage, etc. Therefore, an electrode shape that takes into account the lighting startability of the lamp is required.
[0006] Specifically, by making the edge portions of a foil-like electrode (foil electrode) thinner than the center portion, electric field concentration is generated at the electrode edge portions, allowing discharge to occur between the electrodes even with a relatively low input voltage.
[0007] However, in the case of small excimer lamps, the size (diameter) and thickness of the inner tube are limited in order to secure the discharge space. Therefore, the surface area of the inner electrode is not sufficiently secured, and there is a risk of problems with the adhesion between the inner electrode and the inner tube. In particular, if the adhesion with the inner tube that covers the inner electrode is not sufficient, there is a risk of peeling between the inner tube and the inner electrode.
[0008] Therefore, in an excimer lamp, it is necessary to improve the adhesion between the foil electrode and the inner tube to prevent peeling. [Means for solving the problem]
[0009] The present invention is directed to the technical trend of providing a cross-sectional shape that enhances adhesion to foil electrodes, which have traditionally been recognized as having little effect on adhesion in small excimer lamps and the like.
[0010] The excimer lamp of the present invention comprises a foil electrode extending in a strip shape along the lamp axis, a dielectric covering the foil electrode, and a discharge vessel that is fused to the dielectric to form a discharge space. The "foil" electrode can be configured so that the electrode thickness is 1 / 30 or less of the electrode width.
[0011] In the present invention, the foil electrode has a flat portion having a substantially constant thickness along the width direction between both ends of the foil electrode in the width direction. Here, the degree of "flatness" of the flat portion does not require strict smoothness (flatness) without irregularities in a microscopic cross-sectional observation enlarged to a degree that allows the thickness of the foil electrode to be visually recognized. For example, "substantially constant" can be defined as a difference in thickness being allowed as long as the thickness of any point of the flat portion is 0.7 or more (or 0.8 or more) relative to the maximum thickness of the foil electrode.
[0012] In the present invention, the foil electrode is sharpened from both ends of the flat portion toward both ends in the width direction of the foil electrode. Here, "sharpened" means that both ends of the foil electrode are so sharply pointed that they have no thickness and are represented as dots in a microscopic cross-sectional observation enlarged to a degree that allows the thickness of the foil electrode to be visually recognized. The flat portion with a large cross-sectional area is formed in a large proportion of the foil electrode, including the center of the electrode, and the cross-sectional shape near both ends of the foil electrode is sharpened, resulting in a relatively angular edge shape near both ends of the foil electrode. This provides a cross-sectional shape that corresponds to the Joule heat (current capacity) of the foil electrode and compactness in the electrode width direction.
[0013] The foil electrode may be wedge-shaped from near both ends of the flat portion toward both ends in the width direction of the foil electrode. The foil electrode may be configured so that the inclination angle (wedge angle) is constant from both ends in the width direction of the foil electrode toward both ends of the flat portion. The inclination angle may be set in the range of 2° to 15°.
[0014] Considering that the proportion (of the cross-sectional area) occupied by the flat portion in the foil electrode is relatively large, it is possible to configure it so that, for example, the widthwise length of the flat portion relative to the widthwise length between both ends of the foil electrode in the widthwise direction is 0.6 or more.
[0015] The cross-sectional shape of the dielectric may vary. For example, the widthwise cross section of the dielectric may be semicircular or semielliptical at least in the portions surrounding both ends of the foil electrode from both ends of the flat portion in the widthwise direction. Effect of the Invention
[0016] According to the present invention, in an excimer lamp, the adhesion between a foil electrode and an inner tube can be increased, thereby suppressing peeling. [Brief description of the drawings]
[0017] [Figure 1] 1 is a schematic cross-sectional view of an excimer lamp according to an embodiment of the present invention. [Diagram 2]FIG. 2 is a cross-sectional view of the excimer lamp taken along line II-II in FIG. [Diagram 3] FIG. 3 is an enlarged cross-sectional view of the foil electrode of FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0018] Hereinafter, an excimer lamp according to this embodiment will be described with reference to the drawings.
[0019] Fig. 1 is a schematic cross-sectional view of an excimer lamp according to the present embodiment, and Fig. 2 is a cross-sectional view of the excimer lamp taken along line II-II in Fig. 1.
[0020] The excimer lamp 10 includes a tubular discharge tube (discharge vessel) 20 made of a dielectric material such as quartz glass, and is configured here as a discharge tube with a circular cross section. A rare gas such as xenon gas or a mixture of rare gases is sealed inside the discharge tube 20 as a discharge gas.
[0021] A foil electrode 30 extending in a strip shape along the tube axis (lamp axis) C is disposed inside the discharge tube 20. The foil electrode 30 is covered by a columnar dielectric 50 and is not exposed to the discharge space S, but is embedded within the dielectric 50. Here, the cross section of the dielectric 50 is approximately circular.
[0022] The foil electrode 30 is arranged coaxially with its center position in the width direction and thickness direction aligned with the center position of the dielectric 50. Furthermore, the dielectric 50 is arranged coaxially with the discharge tube 20. Therefore, the foil electrode 30 is arranged coaxially with the discharge tube 20, and arranged symmetrically with respect to the tube axis C. In Fig. 2, the width direction of the foil electrode 30 is defined as the Y direction, and the direction perpendicular thereto (thickness direction) is defined as the X direction.
[0023] The outer electrode (hereinafter referred to as the external electrode) 40 disposed on the outer surface of the discharge tube 20 is configured by winding a linear electrode portion made of a conductive metal along the outer surface of the discharge tube 20, spirally wound along the tube axis C, and disposed at predetermined intervals. The power supply line 70 is connected to the end of the foil electrode 30 along the tube axis C, and is also connected to an externally installed power supply unit (not shown).
[0024] The foil electrode 30 and the external electrode 40 have polarities set to anode and cathode here. High frequency (for example, in the range of several kHz to several tens of MHz) and high voltage (for example, in the range of several kV to several tens of kV) are supplied to the discharge lamp 10 via the power supply line 70. As a result, a dielectric barrier discharge occurs between the dielectric 50 covering the foil electrode 30 and the external electrode 40, and excimer light of a predetermined spectrum (for example, a wavelength of 172 nm) is emitted from the discharge space S.
[0025] The excimer lamp 10 of this embodiment is configured as a small excimer lamp. For example, the axial length (light emission length) in which discharge occurs in the discharge tube 20 can be set in the range of 20 mm to 400 mm. The outer diameter of the discharge tube 20 can be set in the range of 5 mm to 30 mm, preferably in the range of 8 mm to 25 mm.
[0026] The wall thickness of the discharge tube 20 can be set in the range of, for example, 0.8 mm to 1.5 mm, taking into consideration prevention of discharge tube deterioration due to excimer light and suppression of an increase in discharge start voltage. Also, the inner diameter of the discharge tube 20 is set in the range of, for example, 4 mm to 28 mm, preferably in the range of 6 mm to 23 mm, taking into consideration prevention of discharge instability due to a long discharge distance and insufficient illuminance due to a short discharge distance.
[0027] The discharge distance, i.e., the distance between the dielectric 50 and the inner diameter of the discharge tube 20, can be set in the range of 2 mm to 12 mm, preferably in the range of 3 mm to 10 mm, taking into consideration prevention of insufficient illuminance due to narrowing of the discharge space and prevention of instability of the discharge due to increase in the discharge distance.
[0028] The foil electrode 30 is configured as an extremely thin strip-shaped electrode with a thickness that is suppressed relative to the electrode width. Here, the thickness of the foil electrode 30 relative to the electrode width is set to 1 / 30 or less, preferably 1 / 50 or less, and more preferably 1 / 100 or less. Note that the thickness of the foil electrode 30 is exaggerated in FIG. 2.
[0029] For example, the thickness of the foil electrode 30 can be set in the range of 20 μm to 50 μm, taking into consideration the current capacity, ease of manufacture, and prevention of peeling from the dielectric 50. On the other hand, the width of the foil electrode 30 can be set in the range of 1.2 mm to 10 mm, taking into consideration the current capacity, ease of manufacture, prevention of blocking of discharge light due to an increase in the electrode area, and the like.
[0030] The electrode material of the foil electrode 30 can be formed from a highly conductive metal or alloy. It can also be made from a material that is easy to electropolish. In this example, molybdenum or an alloy containing molybdenum is used.
[0031] Here, the dielectric 50 is made of a dielectric material (such as SiO2). The thickness of the dielectric 50 can be set in the range of, for example, 0.1 mm to 2 mm, taking into consideration the limit for maintaining the insulation property and the prevention of an increase in the discharge start voltage.
[0032] FIG. 3 is an enlarged cross-sectional view of the foil electrode 30 of FIG.
[0033] As described above, the foil electrode 30 is an electrode formed with a very thin thickness (electrode thickness) compared to the electrode width (electrode width) w, and the thickness t compared to the electrode width w is suppressed to 1 / 30 or less. The foil electrode 30 has a flat portion 32 with a substantially constant thickness t, and has wedge-shaped portions 34A, 34B that taper in a wedge shape from both widthwise ends 32A, 32B of the flat portion 32 to both widthwise ends E1, E2 of the foil electrode 30.
[0034] Here, the wedge-shaped portions 34A and 34B of the foil electrode 30 are sharply wedge-shaped up to the edge E. That is, the foil electrode 30 is not sharpened between the center and the edge in the width direction, but is sharpened from both ends 32A and 32B along the width direction of the flat portion 32 to both ends E1 and E2 in the width direction of the entire foil electrode 30. In addition, both ends E1 and E2 in the width direction of the foil electrode 30 are not rounded and thick, but are sharp and have an edge shape such that both ends E1 and E2 in the width direction are represented as dots in the cross section. In addition, the thickness of the foil electrode 30 becomes thinner at constant inclination angles θ1 and θ2 from both ends 32A and 32B in the width direction of the flat portion 32 to both ends E1 and E2 in the width direction.
[0035] Here, the angles θ1 and θ2 (angle θ of edge E) of both ends E1 and E2 in the width direction of the foil electrode 30 are determined in consideration of the difficulty of peeling due to gaps generated at the boundary with the dielectric to be covered, the size of the cross-sectional area of the flat part according to the current capacity, and the suppression of temperature rise due to Joule heat generation. Here, the angles θ1 and θ2 are both set in the range of 2° to 15°, preferably in the range of 2° to 10°, and are set to the same angle (hereinafter also referred to as θ). However, the angles θ1 and θ2 are defined as angles at which the thickness increases from the edge E of the foil electrode toward both ends 32A and 32B in the width direction of the flat part 32 by enlarging and observing a cross section in the vicinity of a range of about 100 μm from the edge E of the foil electrode 30. In the foil electrode 30, the edge-like edge E having such angles θ1 and θ2 is formed over the entire electrode along the tube axis C direction.
[0036] The flat portion 32 is formed so that its widthwise center (central portion) coincides with the tube axis C, and the wedge-shaped portions 34A and 34B are symmetrical with respect to the flat portion 32. The widthwise lengths d1 and d2 (d1 / w and d2 / w) of the wedge-shaped portions 34A and 34B relative to the electrode width W of the foil electrode 30 are set to 0.2 or less. Accordingly, the length d (d / w) of both ends 32A and 32B in the widthwise direction of the flat portion 32 relative to the electrode width w of the foil electrode 30 is set to 0.6 or more. As described above, the inclination angles θ1 and θ2 of the cross section from both ends E1 and E2 in the widthwise direction toward both ends 32A and 32B in the widthwise direction of the flat portion 32 are equal and constant, but the angles θ1 and θ2 may be different.
[0037] The thickness t of the flat portion 32 is not strictly constant, and it is sufficient that the thickness t can be regarded as approximately flat while having slight curvatures, minute irregularities, etc. when observed under magnification. Here, the flat portion 32 is formed so that the thickness of any point along the electrode width direction of the flat portion 32 has a ratio of 0.7 or more to the maximum thickness of the foil electrode 30 (flat portion 32).
[0038] Such an electrode shape makes it possible to provide a compact excimer lamp 10 with excellent lighting startability while increasing the adhesion between the foil electrode 30 and the dielectric 50 and suppressing peeling.
[0039] First, electric field concentration occurs due to the sharply pointed edge E of the foil electrode 30 extending along the tube axis C. This allows discharge to occur while keeping the discharge initiation voltage low. In addition, because the wedge-shaped portions 34A and 34B have a sharply pointed wedge shape up to the edge E, the cross section of the foil electrode 30 near the edge E becomes linear in the axial direction, making it possible to keep the discharge initiation voltage lower and also making it difficult for gaps to occur at the boundary with the covered dielectric 50, making it difficult for peeling to occur.
[0040] Furthermore, the foil electrode 30 is arranged coaxially with the dielectric 50 and the discharge tube 20, and the discharge distance, which is the distance from both edges E of the foil electrode 30 to the inner surface of the discharge tube 20, is equal. Therefore, light is emitted from the discharge tube 20 in an overall well-balanced manner.
[0041] On the other hand, by forming the flat portion 32 on the foil electrode 30, the adhesion between the foil electrode 30 and the dielectric 50 can be increased, and peeling can be suppressed. That is, by providing the flat portion 32 with a substantially constant thickness t, a relatively large cross-sectional area is ensured for the foil electrode 30 with an extremely thin thickness t. In particular, since the flat portion 32 occupies 60% or more of the foil electrode 30, the generation of Joule heat in the foil electrode 30 is suppressed by the current flowing through the flat portion 32 with a relatively large cross-sectional area during lamp lighting.
[0042] As a result, thermal expansion of the foil electrode 30 in the thickness direction (X direction) and width direction (Y direction) can be suppressed. That is, there is no need to make the foil electrode 30 particularly long in the width direction to ensure a large cross-sectional area, and large thermal expansion along the width direction can be prevented. In addition, there is no need to particularly increase the thickness of the foil electrode 30, and therefore large thermal expansion along the thickness direction can be prevented.
[0043] Furthermore, the wedge-shaped portions 34A, 34B formed from both widthwise ends 32A, 32B of the flat portion 32 toward both widthwise ends E1, E2 of the foil electrode 30 respectively have a sharply pointed wedge shape up to the edge E, so that the electric field strength can be concentrated at the edge E of the foil electrode 30 while suppressing the occurrence of peeling between the dielectric 50 and the foil electrode 30.
[0044] Furthermore, by forming the wedge-shaped portions 34A, 34B with constant cross-sectional inclination angles θ1, θ2, it becomes easy to polish the surfaces of the wedge-shaped portions 34A, 34B by electrolytic polishing, etc. This makes it possible to suppress peeling at the boundary with the dielectric 50.
[0045] The excimer lamp 10 having such a foil electrode 30 can be manufactured, for example, by the manufacturing method described below.
[0046] First, a power supply line is connected to the foil electrode by resistance welding or the like, and then inserted into a glass tube that will become the dielectric coating material. After inserting the foil electrode, the glass tube is evacuated, and then the dielectric coating material is heated from the outside to fuse it to the foil electrode. Note that a process of coating a dielectric may be performed instead.
[0047] A brim-shaped, so-called bead-shaped sealing portion is formed at a position on the glass tube that corresponds to the edge of the electrode along the tube axis direction.A discharge tube made of quartz glass or the like is then formed with an exhaust tube at one end and an insertion port at the other end, and a dielectric with foil electrodes welded thereto is inserted into the discharge tube, and the insertion port of the discharge tube is welded to the bead-shaped sealing portion.
[0048] While the entire discharge tube is heated, a vacuum is drawn through the exhaust tube of the discharge tube to remove impurities, and after the discharge gas is filled in, the exhaust tube is sealed and an external electrode is disposed on the outer surface of the discharge tube.
[0049] According to this embodiment, in the excimer lamp 10 in which the foil electrode 30 is covered with the dielectric 50 and a discharge space S is formed between the welded dielectric 50 and the discharge tube 20, the foil electrode 30 is formed with a flat portion 32 of a constant thickness and with wedge-shaped portions 34A, 34B formed toward both ends E1, E2 in the width direction. This makes it possible to increase the adhesion between the foil electrode 30 and the dielectric 50 and suppress peeling while ensuring good lighting startability even in the case of a small excimer lamp 10, even in the case of restrictions on the size (outer diameter) of the discharge tube 20 and restrictions on the size of the discharge space S.
[0050] Here, the dielectric 50 is configured to have a circular cross section, but may be formed to have an elliptical or oblong cross section. That is, since there is no need to particularly increase the thickness of the foil electrode 30, a portion (corresponding to a straight line portion of an elliptical or oblong cross section) having a substantially constant thickness of the dielectric may be formed along the flat portion 32, and the cross section surrounding the vicinity of both ends 32A, 32B of the flat portion 32 in the width direction and the wedge-shaped portions 34A, 34B of the foil electrode 30 may be formed to have a semicircular or semielliptical cross section. In other words, a cross section in which the length of the straight line portion of the elliptical or oblong cross section is smaller than the width of the foil electrode 30 may be formed. Also, a dielectric may be formed to have an elliptical cross section (a cross section without a straight line portion of an oblong cross section).
[0051] By forming such a dielectric, it becomes possible to consider the temperature of the flat portion 32 of the foil electrode 30 to be approximately equal to the outer surface temperature of the dielectric covering the foil electrode 30. Then, by measuring the temperature of the center portion of the flat portion 32, the measured temperature can be estimated as the temperature of the entire foil electrode.
[0052] Therefore, in order to measure the temperature at or near the center of flat portion 32 of foil electrode 30 of excimer lamp 10, a non-contact surface thermometer (such as a radiation thermometer) is placed around excimer lamp 10, particularly facing flat portion 32, and the temperature is measured. This makes it possible to measure the temperature of the foil electrode while the lamp is lit, without being affected by the nitrogen-containing outside air or by the wedge-shaped portions 34A and 34B that have been thinned by electrolytic polishing. Furthermore, it also becomes possible to estimate the temperature state of the discharge space.
[0053] It is possible to provide an excimer lamp that can be lit with an optimized temperature during rated operation by measuring the surface temperature of the center of flat portion 32 of foil electrode 30 of excimer lamp 10. The temperature of the flat portion of the foil electrode may be estimated by measuring the outer surface temperature of the dielectric covering the flat portion of the foil electrode.
[0054] By controlling the lighting of excimer lamp 10 so that the temperature of the flat parts of the foil electrodes falls within the range of 50° C. to 350° C., it is possible to maintain a good lighting state for a long period of time and provide the excimer lamp with durability. The lamp temperature (the temperature of the flat parts of the foil electrodes) during rated lighting can be adjusted by taking into consideration the current capacity and Joule heat according to the cross-sectional area of the foil electrodes, the temperature rise due to discharge in the discharge space, the shape and structure of the lamp taking into account the insulation by the inner tube, outer tube and external electrodes, control of the voltage, frequency, etc. supplied to the lamp, cooling and heat dissipation by a fan, etc.
[0055] For example, by keeping the temperature of the flat portion of the foil electrode at 350°C or less, it is possible to suppress the occurrence of cracks in the dielectric due to thermal expansion. Also, by keeping the temperature of the flat portion of the foil electrode at 200°C or less, it is possible to suppress the decrease in ultraviolet radiation efficiency. In particular, when ozone is generated by ultraviolet rays emitted from an excimer lamp, it is possible to suppress the thermal decomposition of ozone by keeping the temperature of the flat portion of the foil electrode at 150°C or less.
[0056] On the other hand, the progression of distortion of the dielectric can be suppressed by setting the temperature of the flat portion of the foil electrode to 50° C. or higher. Note that the lamp lighting with the above-mentioned temperature measurement and temperature control by measuring the temperature of the flat portion (center portion) of the foil electrode is also effective for excimer lamp 10 having a dielectric with a circular or elliptical cross section. [Explanation of symbols]
[0057] 10 Excimer Lamp 20 Discharge tube (discharge vessel) 30 foil electrode 40 External electrode 50 Dielectric
Claims
1. A foil electrode extending in a strip shape along the lamp axial direction; a dielectric covering the foil electrode; a discharge vessel that is fused to the dielectric to form a discharge space, An excimer lamp characterized in that the foil electrode has a flat portion having a substantially constant thickness along the width direction between both widthwise ends of the foil electrode, and is tapered from both ends of the flat portion toward both widthwise ends of the foil electrode.
2. 2. The excimer lamp according to claim 1, wherein the foil electrode is wedge-shaped from the vicinity of both ends of the flat portion toward both ends in the width direction of the foil electrode.
3. 3. The excimer lamp according to claim 2, wherein the foil electrode has a constant inclination angle from both ends of the foil electrode in the width direction to both ends of the flat portion.
4. 4. The excimer lamp according to claim 3, wherein the inclination angle is between 2 degrees and 15 degrees.
5. 2. The excimer lamp according to claim 1, wherein a ratio of a widthwise length of said flat portion to a widthwise length between both ends of said foil electrode in the widthwise direction is 0.6 or more.
6. 2. The excimer lamp according to claim 1, wherein the cross section in the width direction of the dielectric body is semicircular or semielliptical at least in the portions surrounding both ends of the flat portion in the width direction and both ends of the foil electrode.
7. 7. The excimer lamp according to claim 1, wherein the thickness of the flat portion is 0.7 or more times the maximum thickness of the foil electrode.
8. 7. The excimer lamp according to claim 1, wherein the foil electrode is configured as a foil electrode in which the ratio of the electrode thickness to the electrode width is 1 / 30 or less.
Citation Information
Patent Citations
Arc-shaped molybdenum sheet
CN211295039U
lamp
JP1986237363A