Anisotropic electroconductive film

An elastomer-based anisotropic conductive film with through-holes and conductive layers addresses the challenges of uniform stretching and particle-related issues, ensuring stable electronic component connections.

JP2024136143APending Publication Date: 2024-10-04DEXERIALS CORP
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023047135
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-23
Publication Date
2024-10-04

AI Technical Summary

Technical Problem

Conventional anisotropic conductive films with conductive particles face challenges in uniform biaxial stretching, leading to potential short circuits and conduction failures during electronic component connections.

Method used

An anisotropic conductive film is developed without conductive particles, utilizing an elastomer layer with through-holes and conductive layers on the inner walls to ensure electrical connectivity between electrodes, providing resilience and stability.

Benefits of technology

The film achieves reliable and stable anisotropic conductive connections with reduced resin flow influence, minimizing short circuits and conduction defects.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024136143000001_ABST
    Figure 2024136143000001_ABST
Patent Text Reader

Abstract

To provide an anisotropic electroconductive film in which short circuits and conduction failures do not occur when a connection structure is manufactured by making anisotropic electroconductive connection of a first electronic component such as an IC chip that is an anisotropic electroconductive connection object to a second electronic component such as a wiring board using an anisotropic electroconductive film.SOLUTION: An anisotropic electroconductive film includes an elastomer layer provided with through-holes, a first electrode formed on the obverse surface of the elastomer layer, and a second electrode formed on the reverse surface thereof. The first electrode and the second electrode are made conductive via an electroconductive layer formed on the inner walls of through-holes in an insulating resin layer of the elastomer layer. The compression hardness of the elastomer layer at 20% compression deformation is 1,500 MPa or more and 8,000 MPa or less.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to an anisotropic conductive film. [Background technology]

[0002] Conventionally, when electronic components such as IC chips are mounted on a wiring board, anisotropic conductive connection is often made using an anisotropic conductive film in which conductive particles, each having a metal layer formed on the surface of a compression-resistant resin core, are dispersed in a large number in an insulating resin layer. During such anisotropic conductive connection, there is a concern that a short circuit may occur due to a large number of conductive particles coming into contact with each other, etc., so in recent years, in order to prevent such short circuits and achieve good capture stability of conductive particles at the terminals to be connected, a conductive particle-aligned anisotropic conductive film in which conductive particles are regularly aligned in a single layer in an insulating resin layer has been attracting attention (Patent Document 1).

[0003] Such particle-aligned anisotropic conductive films are manufactured by the so-called biaxially stretched film method, which uses a stretched film in which conductive particles are densely arranged. Specifically, conductive particles are spread in a single layer on an adhesive layer formed on the surface of a stretched film, and the stretched film on which the conductive particles are spread is biaxially stretched to obtain a stretched film in which the conductive particles are aligned in a single layer, and an insulating adhesive film that becomes an insulating resin layer is placed on the conductive particle-arranged surface of the obtained stretched film and pressed to transfer and further embed the conductive particles in the insulating adhesive film, and then the stretched film is peeled off together with the adhesive layer. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] Patent No. 5147048 Summary of the Invention [Problem to be solved by the invention]

[0005] However, in the case of the particle-aligned anisotropic conductive film disclosed in Patent Document 1, it is difficult to stretch a stretched film having conductive particles regularly arranged on one side uniformly in biaxial directions at a constant rate, making it difficult to precisely arrange the conductive particles in an orderly manner. There is also concern that it is impossible to eliminate the possibility of conductive particles falling out or agglomerating not only when the stretched film is biaxially stretched, but also when the conductive particles aligned in the biaxially stretched film are transferred from the biaxially stretched film to an insulating adhesive film.

[0006] For this reason, when a connection structure is manufactured by anisotropically conductively connecting a first electronic component such as an IC chip to a second electronic component such as a wiring board using the conductive particle-aligned anisotropic conductive film disclosed in Patent Document 1, there is a problem in that the possibility of short circuits or poor conductivity occurring increases.

[0007] The object of the present invention is to solve the problems of the prior art and to provide an anisotropic conductive film that does not cause short circuits or poor conductivity when a connection structure is manufactured by anisotropically conductively connecting a first electrode of a first electronic component, such as an IC chip, which is an anisotropic conductive connection object, to a second electrode of a second electronic component, such as a wiring board, using the anisotropic conductive film. [Means for solving the problem]

[0008] The inventors hypothesized that the problems with the conventional technology were caused by the fact that the first electrode of the first electronic component and the second electrode of the second electronic component, which face each other, are electrically connected by conductive particles in an anisotropic conductive film, and discovered that if an anisotropic conductive film could be constructed without using conductive particles, it would be possible to solve the problems with the conventional technology. To this end, they discovered that if through holes with a conductive layer formed on their inner surface are used instead of conductive particles, it is possible to construct an anisotropic conductive film without using conductive particles, and furthermore the effects of resin flow can be reduced, and that if an elastomer layer is used as the insulating resin layer that constitutes the anisotropic conductive film, it is possible to ensure the same resilience to compression as the resin core of the conductive particles, and thus completed the present invention.

[0009] That is, the present invention provides an anisotropic conductive film having an elastomer layer having a through hole, a first electrode formed on the front surface of the elastomer layer, and a second electrode formed on the back surface, wherein the first electrode and the second electrode are electrically connected via a conductive layer formed on the inner wall of the through hole in the elastomer layer.

[0010] The present invention also provides a connection structure in which a first electronic component and a second electronic component are anisotropically conductively connected via the above-mentioned anisotropic conductive film of the present invention.

[0011] The present invention further provides a method for producing a connection structure in which a first electronic component and a second electronic component are anisotropically conductively connected via the above-mentioned anisotropic conductive film of the present invention. Effect of the Invention

[0012] The anisotropic conductive film of the present invention has an elastomer layer with through holes, a first electrode formed on the front surface of the elastomer layer, and a second electrode formed on the back surface. These first and second electrodes are electrically connected via a conductive layer formed on the inner wall of the through hole of the elastomer layer. Therefore, when manufacturing the anisotropic conductive film of the present invention, conductive particles are not used, so there is no need to apply the biaxially stretched film method, which is a manufacturing method of a conventional particle-aligned anisotropic conductive film. Moreover, since the through holes are fixed in the elastomer layer, the influence of the resin flow can be reduced compared to the conductive particles, and the elastomer layer itself can ensure the same resilience against compression as the resin core of the conductive particles, so that anisotropic conductive connection can be performed reliably and stably. [Brief description of the drawings]

[0013] [Figure 1] 1 is a schematic cross-sectional view of an anisotropic conductive film of the present invention. [Diagram 2] 1 is a schematic cross-sectional view of an anisotropic conductive film of the present invention. [Diagram 3] 1 is a schematic cross-sectional view of an anisotropic conductive film of the present invention. [Figure 4]1 is a schematic cross-sectional view of an anisotropic conductive film of the present invention. [Diagram 5] 1 is a schematic cross-sectional view of an anisotropic conductive film of the present invention. [Figure 6] 1 is a schematic cross-sectional view of an anisotropic conductive film of the present invention. [Figure 7] 1 is a schematic cross-sectional view of an anisotropic conductive film of the present invention. [Figure 8A] 1 is a process diagram for producing an anisotropic conductive film of the present invention. [Figure 8B] 1 is a process diagram for producing an anisotropic conductive film of the present invention. [Figure 8C] 1 is a process diagram for producing an anisotropic conductive film of the present invention. [Figure 8D] 1 is a manufacturing process diagram of an anisotropic conductive film of the present invention. [Figure 9] 1 is a schematic cross-sectional view of a connection structure of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0014] The present invention will now be described in detail with reference to the drawings, in which the same reference numerals denote the same or equivalent components.

[0015] <<Basic structure of anisotropic conductive film>> 1 shows a schematic cross-sectional view of an anisotropic conductive film 10 of the present invention. This anisotropic conductive film 10 has an elastomer layer 1 in which a through hole 2 is formed, a first electrode 3 formed on the front surface of the elastomer layer 1, and a second electrode 4 formed on the back surface. The first electrode 3 and the second electrode 4 are electrically connected via a conductive layer 5 formed on the inner wall of the through hole 2 in the elastomer layer 1.

[0016] <Elastomer layer 1> The elastomer layer 1 constituting the anisotropic conductive film 10 of the present invention has a film-like shape and is insulating itself, ensuring the same resilience to compression as the resin core of conventional conductive particles while also ensuring the mechanical strength of the anisotropic conductive film 10.

[0017] (Compression hardness of elastomer layer at 20% compression deformation) The resilience against compression of the elastomer layer 1 can be evaluated by compressing the elastomer layer 1 in the thickness direction and measuring the hardness when the thickness is reduced by 20% (compressive hardness at 20% compression deformation (K value [MPa])). This K value is specifically calculated from the following formula, and the smaller the K value, the softer the film.

[0018]

number

[0019] In the above formula, "F" is the load [N] at the time of 20% compressive deformation of the elastomer layer 1, "S" is the displacement [mm] at the time of 20% compressive deformation, and "R" is the thickness [mm] of the elastomer layer 1 before compression.

[0020] The compression hardness (K value) of the elastomer layer 1 at 20% compressive deformation calculated by the above formula is preferably 1500 MPa or more, more preferably 3000 MPa or more, and is preferably 8000 MPa or less, more preferably 4000 MPa or less, since if it is too soft, it will be difficult to break through the oxide film on the terminal surface of the electronic component to be connected with the anisotropic conductive film, and if it is too hard, it will be likely to cause defects such as bending of the electronic component (substrate) on the stage side. In either case, the resilience against compression that can achieve good conductive performance cannot be expected. Therefore, the compression hardness is preferably 1500 MPa or more, more preferably 3000 MPa or more, and is preferably 8000 MPa or less, more preferably 4000 MPa or less.

[0021] (Melt Viscosity of Elastomer Layer) The melt viscosity of the elastomer layer 1 is preferably 1.1 times or more, more preferably 1.2 times or more, of the minimum melt viscosity of the elastomer layer 1 in the temperature range during compression bonding, for example, thermocompression bonding, in order to suppress unnecessary deformation when the anisotropic conductive film 10 is anisotropically conductively connected. As an example, the melt viscosity can be determined using a rotational rheometer (manufactured by TA Instruments) with a measurement pressure of 5 g kept constant and a measurement plate with a diameter of 8 mm. More specifically, the melt viscosity can be determined at a temperature range of 30 to 250°C, a heating rate of 10°C / min, a measurement frequency of 10 Hz, and a load fluctuation of 5 g on the measurement plate. The melt viscosity can be adjusted by changing the type and amount of fine solid matter used as a melt viscosity adjuster, the adjustment conditions of the resin composition, etc.

[0022] (thickness of elastomer layer) The thickness of the elastomer layer 1 is determined mainly according to the surface irregularities of the anisotropic conductive connection object and the handleability of the anisotropic conductive film. For example, when applied to a semiconductor device, taking into consideration the bump height and its variation, the thickness is preferably 1 μm or more, more preferably 2 μm or more, and particularly preferably 5 μm or more. The upper limit of the thickness is not particularly limited, but is usually 100 μm or less, preferably 50 μm or less, and more preferably 30 μm or less, taking into consideration the handleability of the anisotropic conductive film and fine pitch compatibility. The thickness of the elastomer layer can be measured using a known thickness meter (for example, Fujiwork Co., Ltd., Film Tester Continuous Thickness Measuring Instrument, HKT Handy Series).

[0023] (Elastomer material) Examples of the elastomer material constituting the elastomer layer 1 include thermoplastic elastomers, such as polybutadiene, natural rubber, polyisoprene, conjugated diene rubbers such as SBR and NBR and their hydrogenated products, block copolymers such as styrene-butadiene block copolymers and styrene-isoprene block copolymers and their hydrogenated products, chloroprene, urethane rubber, polyester rubber, epichlorohydrin rubber, silicone rubber, ethylene-propylene copolymer, ethylene-propylene-diene copolymer, etc., and when weather resistance is required, thermoplastic elastomers other than conjugated diene rubbers are preferred, and silicone rubber in film form is particularly preferred from the viewpoint of moldability and electrical properties. Note that the elastomer layer 1 may contain, as necessary, known thermosetting elastomers, thermoplastic resin compositions such as phenoxy, polyimide, polyamide, polyacetal, polycarbonate, polyethylene, polypropylene, polystyrene, polyvinyl chloride, and polyvinyl acetate, high-viscosity adhesive resin compositions, and curable resin compositions such as epoxy and acrylic, or mixtures thereof.

[0024] <Through hole> In the elastomer layer 1 of the anisotropic conductive film 10 of the present invention, a through hole 2 having a conductive layer 5 on the inner surface is provided in order to ensure the anisotropic conductivity of the anisotropic conductive film instead of conductive particles. That is, the anisotropic conductive film of the present invention does not require conductive particles for the purpose of conducting between opposing terminals. The through hole 2 can be made by preparing a flat elastomer material in advance in the form of a film, for example, by a known method such as punching, photolithography, or laser processing. It may also be made by stamping or pressing a master plate with a convex shape against it. It may also be formed when the elastomer material is in a state where it is easy to shape, such as before it is dried or cured.

[0025] The through holes 2 may be arranged randomly in the elastomer layer 1 as long as adjacent through holes 2 do not short-circuit during anisotropic conductive connection. However, it is preferable to arrange them in a regular arrangement pattern in order to reliably prevent short-circuiting. The arrangement pattern may be designed according to the pitch of the terminal arrangement (so-called L / S (line / space)). As the regular arrangement pattern, a general lattice pattern such as a square lattice pattern or a hexagonal lattice pattern may be adopted. Note that a pattern corresponding to the terminals of the anisotropic conductive connection object may also be used. The arrangement may be substantially the same as that of the conductive particles in a general conductive particle-aligned anisotropic conductive film.

[0026] (Inner diameter of through hole 2) The inner diameter of the through hole 2 is determined according to the terminal width and terminal pitch of the anisotropic conductive connection object, the number density and arrangement pitch of the through holes 2, the method of forming the conductive layer 5 formed on the inner wall, etc., but if the inner diameter is too small, it will hinder the flow of the resin, which is likely to cause air bubbles and cause deterioration of adhesion, and if it is too large, it will be difficult to adapt to fine pitches, it will be difficult to reuse the same product, and it will lead to increased manufacturing costs, so it is preferably 1.0 μm or more, more preferably 2.5 μm or more, preferably 200 μm or less, and more preferably 50 μm or less. The inner diameter of the through hole 2 can be measured by microscope observation. When the through hole diameter is large, it can be used for an anisotropic conductive connection object with a rough pitch, and the number density of the through holes can be reduced, which increases the cost advantage. In addition, the elastomer film may be present in the center of the film thickness direction, so it is easy to expect reuse by repair.

[0027] (Number density of through holes 2) If the number density of the through holes 2 is too low, the resin flow is easily hindered, whereas if it is too high, the area covered with the conductive material becomes too large, resulting in an increase in costs. Therefore, the number density of the through holes 2 is preferably 10 holes / mm 2 More preferably, 30 pieces / mm 2 More than 500,000 pieces / mm 2 Less than or equal to 250,000 pieces / mm 2The number density can be determined by measuring the field of view of the film surface by microscopic observation. The observation area during microscopic observation is preferably 2 mm 2 More than 10mm, preferably 2 That is all. This number density may be obtained by measuring the observed image using image analysis software (for example, WinROOF (Mitani Corporation) or Azokun (registered trademark) (Asahi Kasei Engineering Corporation)). The observation method and measurement technique are not limited to those described above.

[0028] In the present invention, the size of the through holes is unified, so that the effect of the invention can be more pronounced. To achieve this, it is desirable that the size and depth of the opening of the through holes satisfy the following conditions. That is, in the anisotropic conductive film, when the total observation area is 1 mm 2 More than 2mm, preferably 2 In the above, it is desirable that 95% or more, preferably 98% or more, more preferably 99.5% or more of the total number of through holes contained in a region having 1000 or more through holes (preferably 2000 or more) have the same size and depth of the opening. Here, "matching" in "the size and depth of the openings are the same" means that the size and depth of the opening of a certain through hole are within ±15%, preferably ±10%, more preferably ±5% of the average size and average depth of the openings of the through holes contained in a predetermined region, taking into account measurement errors. Note that the size of the opening may be the diameter when the area of ​​the opening is converted into a circle, since there are openings with different shapes.

[0029] (arrangement pitch of through holes 2) In addition, the arrangement pitch of the through holes 2 is determined according to the terminal width and terminal pitch of the anisotropic conductive connection object, the regular arrangement pattern, and the number density, etc., but if it is too narrow, the terminals will be easily connected when coated with the conductive material, and if it is too wide, the freedom of the terminal layout that can be used will decrease, resulting in increased manufacturing costs, so the arrangement pitch is preferably 0.5 times or more and preferably 200 times or less the inner diameter of the through holes 2.

[0030] <Conductive layer 5 formed on the inner wall of the through hole> A conductive layer 5 is formed on the inner wall of the through hole 2 to ensure electrical continuity between the front and back surfaces of the through hole 2. The conductive layer 5 is preferably formed on the entire inner wall, but may be provided on a part of the inner wall so as to be continuous from the front opening to the back opening of the through hole 2, as long as electrical continuity between the front and back surfaces of the through hole 2 can be ensured. The conductive layer 5 can be formed by a known method such as sputtering, electroless plating, electrolytic plating, photolithography, laser processing, etc.

[0031] (Thickness of conductive layer) The thickness of the conductive layer 5 varies depending on the method of preparation, etc., but if it is too thin, it may peel off during compression, and if it is too thick, it may crack during compression, so there is no particular limit, but the lower limit is preferably 0.05 μm or more, more preferably 0.1 μm or more, and even more preferably 0.3 μm or more. There is also no particular limit on the upper limit, but it is preferably 3 μm or less, more preferably 1 μm or less, and even more preferably 0.5 μm or less.

[0032] (Material of conductive layer 5) Examples of materials for the conductive layer 5 include metal materials and alloy materials such as gold, silver, nickel, copper, indium titanium oxide, aluminum, and solder. Materials that can be plated or sputtered, or materials that can be applied by inkjet printing are preferable.

[0033] <First electrode and second electrode> In the anisotropic conductive film 10 of the present invention, a first electrode 3 is formed on the front surface of the elastomer layer 1 and a second electrode 4 is formed on the back surface thereof, and electrical conductivity between these electrodes is ensured by a conductive layer 5 formed on the inner wall of the through hole 2.

[0034] Since it is usually advantageous in manufacturing to form the first electrode 3 and the second electrode 4 simultaneously with the conductive layer 5, it is preferable that the first electrode 3 is formed around the opening of the through hole 2 on the front side of the elastomer layer 1, and the second electrode 4 is formed around the opening of the through hole 2 on the back side. Here, the surroundings of the opening preferably means the entire circumference of the opening from the viewpoint of ensuring reliable conduction, but may be a part of the opening as long as anisotropic conductive connection is ensured. When the first electrode 3 and the second electrode 4 are provided on the front or back side of the elastomer layer 1 corresponding to the terminal of the anisotropic conductive connection object, they can be provided in various shapes on the front or back side of the elastomer layer 1 at a position away from the opening, rather than around the opening of the through hole 2. In that case, it is preferable to simultaneously form a connection line connecting the first electrode 3 and the second electrode 4 to the conductive layer 5 of the through hole 2 when forming the electrodes.

[0035] (Thickness and constituent materials of the first electrode 3 and the second electrode 4) The thickness and constituent materials of the first electrode 3 and the second electrode 4 can be the same as those of the conductive layer 5 .

[0036] In addition, it is preferable that protrusions are formed on the surface of either or both of the first electrode 3 and the second electrode 4 in order to easily break through the oxide film on the terminal surface of the anisotropic conductive connection object. The protrusions may be the same as or different from the electrode material. The number, shape, size, and formation method of the protrusions may be the same as the protrusions formed on the conductive particles of a conventional anisotropic conductive film.

[0037] <Another embodiment of anisotropic conductive film 1> As shown in FIG. 2, the anisotropic conductive film 20 of the present invention has a structure in which the front and back sides of the elastomer layer 1 are covered with the same adhesive layer. Here, the adhesive layer on the front side is adhesive layer 6a, and the adhesive layer on the back side is adhesive layer 6b. In FIG. 2, from the viewpoint of productivity, the inside of the through hole 2 is also filled with a resin composition constituting an adhesive layer. In this way, by providing the adhesive layer 6a and the adhesive layer 6b, the anisotropic conductive film 20 can be temporarily fixed during anisotropic conductive connection, so that not only the alignment accuracy but also the connection reliability can be improved. It can also function as an underfill agent.

[0038] (Thickness of adhesive layers 6a, 6b) In the anisotropic conductive film 20 of Fig. 2, the thicknesses of the adhesive layer 6a and the adhesive layer 6b may be the same or different, but are determined in consideration of the type of resin composition constituting the adhesive layer, the anisotropic conductive connection object, etc., and are each independently preferably 2 µm or more, more preferably 5 µm or more, and are preferably equal to or less than the height of the bump, so are 20 µm or less, more preferably 10 µm or less. The total thickness may be 50 µm or less, preferably 30 µm or less, and more preferably 22 µm or less.

[0039] (Materials for Adhesive Layers 6a and 6b) As the material constituting the adhesive layer 6a and the adhesive layer 6b, a material constituting an insulating adhesive layer of a conventional anisotropic conductive film, for example, a thermosetting resin composition or a photocurable resin composition, can be adopted. Examples of the thermosetting resin composition include a thermal radical polymerization type resin composition containing an acrylate compound and a thermal radical polymerization initiator, a thermal cationic polymerization type resin composition containing an epoxy compound and a thermal cationic polymerization initiator, and a thermal anionic polymerization type resin composition containing an epoxy compound and a thermal anionic polymerization initiator. Examples of the photocurable resin composition include a photoradical polymerization type resin composition containing an acrylate compound and a photoradical polymerization initiator, and a photocationic polymerization type resin composition containing an epoxy compound and a photocationic polymerization initiator.

[0040] (Minimum melt viscosity of adhesive layers 6a, 6b) The minimum melt viscosity of the adhesive layer 6a and the adhesive layer 6b may be equivalent to that of a general anisotropic conductive connection material so that conventional knowledge can be utilized to realize a necessary and sufficient resin flow for applying the anisotropic conductive film 10 to an anisotropic conductive connection, and may be 200 Pa·s or more, preferably 1500 Pa·s or more, more preferably 2000 Pa·s or more, even more preferably 3000 Pa·s or more, and preferably 15000 Pa·s or less, more preferably 10000 Pa·s or less, and particularly preferably 8000 Pa·s or less. The minimum melt viscosity can be determined, for example, using a rotational rheometer (manufactured by TA Instruments) with a measurement pressure of 5 g kept constant and a measurement plate with a diameter of 8 mm. More specifically, it can be determined at a temperature range of 30 to 200°C, a heating rate of 10°C / min, a measurement frequency of 10 Hz, and a load fluctuation of 5 g on the measurement plate. The minimum melt viscosity can be adjusted by changing the type and amount of fine solid matter used as a melt viscosity adjuster, or by changing the preparation conditions of the resin composition.

[0041] (Adhesive strength of adhesive layers 6a and 6b) The adhesive layers 6a and 6b preferably have an adhesive strength that allows temporary pressure bonding before pressure bonding to an article to which the anisotropic conductive film is to be pressure-bonded or thermocompression-bonded. The adhesive strength can be measured in accordance with JIS Z 0237, and can also be measured as tack strength by a probe method in accordance with JIS Z 3284-3 or ASTM D 2979-01. The tack strength of each of the adhesive layers 6a and 6b constituting the anisotropic conductive film 10 by the probe method is preferably 1.0 kPa (0.1 N / cm) or less when measured, for example, at a probe pressing speed of 30 mm / min, a pressure of 196.25 gf, a pressure time of 1.0 sec, a peel speed of 120 mm / min, and a measurement temperature of 23°C ± 5°C. 2 ) or more, more preferably 1.5 kPa (0.15 N / cm 2 ) or more, particularly preferably 3.0 kPa (0.3 N / cm 2 )That's all.

[0042] The adhesive strength of the anisotropic conductive film can also be determined according to the adhesive strength test described in JP 2017-48358 A. In this adhesive strength test, for example, an anisotropic conductive film is sandwiched between two glass plates, one of the glass plates is fixed, and the other glass plate is peeled off at a peeling speed of 10 mm / min and a test temperature of 50° C. By strengthening the adhesive state between the fixed glass plate and the anisotropic conductive film, it is possible to measure the adhesive strength between the glass plate being peeled off and the surface of the anisotropic conductive film attached to the glass plate. The adhesive strength (adhesive strength) measured in this way is preferably 1 N / cm 2 (10kPa) or more, more preferably 10N / cm 2 This is the adhesive strength between the surface of the anisotropic conductive film in the direction of peeling and the article to be peeled off.

[0043] In addition, the adhesive strength of anisotropic conductive film can also be determined by a test in which one end of a test piece is aligned and glued (pasted) together, and the other end is pulled up to peel the test piece off. The adhesive strength measured by this test method is equivalent to that of the above adhesive strength test (1 N / cm 2 (10 kPa) or more) may be acceptable if the adhesive strength measured by the above adhesive strength test is sufficiently large (e.g., 10 N / cm 2 (100 kPa or more), and the adhesive strength in this test method should be 10% or more of the adhesive strength in the above-mentioned adhesive strength test.

[0044] <Another embodiment of anisotropic conductive film 2> As shown in FIG. 3, the anisotropic conductive film 30 of the present invention can have a first adhesive layer 7 on the front side of the elastomer layer 1 and a second adhesive layer 8 different from the first adhesive layer 7 on the back side. This is to accommodate cases where the anisotropic conductive connection objects are different between the front side and the back side. In FIG. 3, from the viewpoint of productivity, the inside of the through hole 2 is also filled with a resin composition constituting the first adhesive layer 7 and the second adhesive layer 8. Here, the differences between the first adhesive layer 7 and the second adhesive layer 8 are, for example, differences in the composition of the constituent resin composition, optical properties (refractive index, light transmittance, etc.), mechanical properties (compressive hardness, tensile strength, etc.), and thermal properties (glass transition point, softening point, minimum melt viscosity, etc.). In particular, it is preferable that the minimum melt viscosity is different from the viewpoint of ensuring adhesiveness by controlling the flow of the resin. The minimum melt viscosity is a value measured with a viscoelasticity measuring device (Rheometer RS150, Haake).

[0045] (Constituent materials and characteristics of first adhesive layer 7 and second adhesive layer 8) The first adhesive layer 7 and the second adhesive layer 8 can be formed independently from the same material as the material constituting the adhesive layer 6a or the adhesive layer 6b. Furthermore, the minimum melt viscosity and adhesive strength of the first adhesive layer 7 and the second adhesive layer 8 each exhibit the same characteristics as those of the adhesive layer 6a or the adhesive layer 6b.

[0046] (Thickness of the first adhesive layer 7 and the second adhesive layer 8) The thicknesses of the first adhesive layer 7 and the second adhesive layer 8 are determined in consideration of the type of resin composition constituting the adhesive layer, the anisotropic conductive connection object, etc., and are each independently preferably 2 μm or more, more preferably 5 μm or more, and are preferably equal to or less than the height of the bump, so are 20 μm or less, more preferably 10 μm or less. The total thickness may be 50 μm or less, preferably 30 μm or less, and more preferably 22 μm or less.

[0047] <Anisotropic Conductive Film Variation 3> In the case of the anisotropic conductive films 20 and 30 in FIG. 2 and FIG. 3, the through-hole 2 is filled with a resin composition constituting each adhesive layer, but the inside of the through-hole 2 may be a void (internal space) as in the anisotropic conductive film 40 in FIG. 4 and the anisotropic conductive film 50 in FIG. 5. Such an internal space is generated when a high-viscosity resin composition is used to form the adhesive layer or when adhesive layer films are laminated. Note that, when the anisotropic conductive film 40 or 50 is usually compressed, for example, thermocompression-bonded, during anisotropic conductive connection, the resin composition constituting each adhesive layer melts and fills the through-hole 2. Alternatively, when the anisotropic conductive film 40 or 50 is wound on a reel to form a reel body, the resin composition may enter the through-hole during storage.

[0048] <Anisotropic Conductive Film Variation 4> In the case of the anisotropic conductive films 20 and 30 in FIG. 2 and FIG. 3, the through-holes 2 are filled with the resin compositions constituting the respective adhesive layers. However, as in the anisotropic conductive film 60 in FIG. 6 and the anisotropic conductive film 70 in FIG. 7, the through-holes 2 may be filled with a resin composition 9 different from the resin composition constituting the adhesive layers on both sides. As the resin composition 9, a material similar to the material constituting the adhesive layer 6a (6b) can be used. By filling the through-holes 2 with a material different from the adhesive layers on both sides of the elastomer layer 1 in this way, it is possible to fine-tune the physical properties of the anisotropic conductive film. These anisotropic conductive films can be obtained by filling only the through-holes 2 of the anisotropic conductive film 10 in FIG. 1 with a resin composition by a known method, and then forming the adhesive layers 6a and 6b or the first adhesive layer 7 and the second adhesive layer 8 as necessary.

[0049] <Production of anisotropic conductive film> The anisotropic conductive film 10 of the present invention shown in FIG. 1 can be manufactured using a known method. For example, as shown in FIG. 8A, a laser beam is irradiated onto an elastomer film 81 to provide a through hole 82. Next, as shown in FIG. 8B, a resist layer 86 is formed on a front surface 81a and a back surface 81b of the elastomer film 81 in a region 85 excluding a region 83 to become a first electrode and a region 84 to become a second electrode, using a photolithography technique. Next, as shown in FIG. 8C, a conductive layer 87 is formed in the through hole 82 using a known dry process plating method (vacuum deposition method, chemical vapor deposition method, etc.) or a wet process plating method (electroless plating method, electrolytic plating method, etc.), and a conductive layer CL is formed on the front and back surfaces of the elastomer film 81 including the resist layer 86, and then the resist layer 86 is removed. As a result, a first electrode 88 is formed on the front surface of the elastomer film 81 and a second electrode 89 is formed on the back surface, and an anisotropic conductive film 80 shown in FIG. 8D having the same configuration as that shown in FIG. 1 is obtained. The through holes 82 of the anisotropic conductive film 80 can be filled with a resin by a conventional method. The adhesive layers 6a and 6b, the first adhesive layer 7, and the second adhesive layer 8 in Fig. 2 to Fig. 7 can each be formed by a conventional method. For example, they can be formed by applying a resin composition for forming an adhesive layer and drying it.

[0050] <Connection structure> A connection structure 90 as shown in FIG. 9 can be manufactured from the anisotropic conductive film of the present invention. This connection structure 90 is also a part of the present invention. This connection structure 90 is a connection structure in which a first electronic component 91 such as an IC chip, mini LED, or micro LED and a second electronic component 92 such as a wiring board are anisotropically conductively connected via, for example, the anisotropic conductive film 20 of the present invention shown in FIG. 2. In this connection structure 90, an electrode 91a of the first electronic component 91 and an electrode 92a of the second electronic component 92 are anisotropically conductively connected to the first electrode 3 and the second electrode 4 of the anisotropic conductive film 20, respectively, and the first electrode 3 and the second electrode 4 are electrically connected to each other via a conductive layer 5.

[0051] <Method of Manufacturing Connection Structure> The connection structure of FIG. 9 can be manufactured by anisotropically conductively connecting the first electronic component and the second electronic component via the anisotropic conductive film of the present invention. In this case, the anisotropic conductive film is first bonded to the first electronic component or the second electronic component, and the bonding method can be pressure bonding, for example, thermocompression bonding, or light irradiation may be used during bonding. One example of using light irradiation is to separate the anisotropic conductive film according to the laser lift-off method described in JP 2022-151816 A and then transfer it. The resin material and adhesive material to be used to obtain an anisotropic conductive film suitable for the laser lift-off method can be selected from those described in JP 2022-151816 A and used. As a specific example of the manufacturing of the connection structure, for example, the through hole of the anisotropic conductive film 40 in FIG. 4 is aligned between the electrode 91a of the first electronic component 91 and the electrode 92a of the second electronic component 92, and when the adhesive layer 6a and the adhesive layer 6b are made of a thermosetting resin composition, the anisotropic conductive connection is made by heating while pressing from the first electronic component side. When the adhesive layer 6a and the adhesive layer 6b are made of a photocurable resin composition, the anisotropic conductive connection is made by pressing from the first electronic component side and then irradiating light (preferably ultraviolet light) from both the first electronic component side and the second electronic component side. During these anisotropic conductive connections, the internal space of the through hole 2 is filled with the resin composition. [Industrial Applicability]

[0052] The anisotropic conductive film of the present invention has an elastomer layer with through holes, a first electrode formed on the front surface of the elastomer layer, and a second electrode formed on the back surface. These first and second electrodes are electrically connected via a conductive layer formed on the inner wall of the through hole of the elastomer layer. Therefore, when manufacturing the anisotropic conductive film of the present invention, conductive particles are not used, so there is no need to apply the biaxially stretched film method, which is a manufacturing method of a conventional particle-aligned anisotropic conductive film. Moreover, since the through holes are fixed in the elastomer layer, the influence of resin flow can be reduced compared to conductive particles, and since the elastomer layer itself has repulsive properties against compression, anisotropic conductive connection can be performed reliably and stably. [Explanation of symbols]

[0053] 1 Elastomer layer 2 Through holes 3 1st electrode 4 Second electrode 5 Conductive layer 6a, 6b adhesive layer 7 First adhesive layer 8 Second adhesive layer 9 Resin composition 10, 20, 30, 40, 50, 60, 70, 80 Anisotropic Conductive Film 81 Elastomer Film 81a Surface of elastomer film 81b Back side of elastomer film 82 Through hole 83 Area to become the first electrode 84 Area to become the second electrode 85 Area that is neither the first nor the second electrode 86 Resist layer 87, CL conductive layer 88 1st electrode 89 2nd electrode 90 Connection structure 91 First Electronic Parts 91a Electrode of first electronic component 92 Second Electronic Parts 92a Electrode of second electronic component

Claims

1. An anisotropic conductive film having an elastomer layer having a through hole, a first electrode formed on the front surface of the elastomer layer, and a second electrode formed on the back surface, wherein the first electrode and the second electrode are electrically connected via a conductive layer formed on the inner wall of the through hole in the elastomer layer.

2. 2. The anisotropic conductive film according to claim 1, wherein the elastomer layer has a compression hardness of 1,500 MPa or more and 8,000 MPa or less at 20% compression deformation.

3. 3. The anisotropic conductive film according to claim 1, wherein the through holes are provided in the elastomer layer in a regularly arranged pattern.

4. 3. The anisotropic conductive film according to claim 1, wherein the first electrode is formed around the opening of the through-hole on the front side of the elastomer layer, and the second electrode is formed around the opening of the through-hole on the back side of the elastomer layer.

5. 3. The anisotropic conductive film according to claim 1, wherein protrusions are formed on the surfaces of the first electrode and the second electrode.

6. 3. The anisotropic conductive film according to claim 1, wherein the elastomer layer has an adhesive layer formed on the front and back surfaces thereof, the adhesive layer being the same or different from each other.

7. 7. The anisotropic conductive film according to claim 6, wherein adhesive layers having different minimum melt viscosities are formed on the front and back surfaces of the elastomer layer.

8. 7. The anisotropic conductive film according to claim 6, wherein the through holes are filled with a resin composition.

9. A connection structure in which a first electronic component and a second electronic component are anisotropically conductively connected via the anisotropic conductive film according to claim 1 .

10. A method for manufacturing a connection structure, comprising anisotropically conductively connecting a first electronic component and a second electronic component via the anisotropic conductive film according to claim 1 .

Citation Information

Patent Citations

  • Ehokishijushisoseibutsu

    JP1976047048A