Method for producing heating device
The method for manufacturing heating tools with protrusions using a laminated sheet and controlled heating/pressure forms stable protrusions with controlled air permeability and strength, addressing the challenges of conventional methods.
Patent Information
- Application Number
- JP2023050563
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-27
- Publication Date
- 2024-10-09
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Conventional methods struggle to simultaneously control air permeability and maintain the strength of protrusions in heating tools with micropores, especially when forming protrusions in a short time, leading to potential collapse and inconsistent heat generation characteristics.
A method involving the use of a laminated sheet with nonwoven fabric layers and a breathable porous resin sheet, subjected to controlled heating and pressure using molds with specific conditions to form protrusions, followed by filling with a heat-generating material, ensuring controlled air permeability and strength.
The method effectively controls air permeability fluctuations and maintains protrusion strength, enabling efficient heat generation and improved production efficiency while preventing protrusion collapse.
Smart Images

Figure 2024139563000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for manufacturing a heating implement having protrusions. [Background technology]
[0002] Conventionally, heating devices having protrusions have been known as heating devices, and a method for manufacturing such a heating device is known in which a raw material sheet containing a thermoplastic resin is heated and pressurized to form protrusions, and then a heat-generating material is placed within or near the protrusions formed in the sheet to obtain a sheet-like heating device.
[0003] For example, Patent Document 1 describes a method of forming a sheet with protrusions by heating and pressurizing a raw material sheet between a first mold having convex portions for forming the protrusions and a second mold having concave portions corresponding to the convex portions, and of obtaining a heating device with protrusions by overlapping the sheet with the protrusions with a main sheet containing a heat-generating material. Furthermore, Patent Document 2 describes arranging a heat-generating material within the protrusions of a sheet having protrusions formed by heating and pressurizing a raw material sheet. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2019-171007 A [Patent Document 2] JP 2018-175857 A Summary of the Invention [Problem to be solved by the invention]
[0005] In order to control the heat generation characteristics of a heating device, it is necessary to adjust the amount of air supplied to the heat generation material. From this perspective, even in a heating device with protrusions, it is preferable to place an air permeable sheet with a controlled air permeability within a predetermined range inside the heating device to control the heat generation characteristics, such as the heating rate, maximum temperature, and heat generation duration. Heating devices that generate steam are also known, and it is preferable to be able to control the amount of steam released to the outside by providing a breathable sheet whose air permeability is controlled within a predetermined range. However, with the method of forming projections and then opening holes, it is difficult to form fine holes, and the sheet tends to have excessive air permeability. On the other hand, even when protrusions are formed on a sheet having fine holes by post-processing, there have been cases where the air permeability changes significantly due to the micropores being blocked, and the strength of the formed protrusions, particularly the strength of the tips, is significantly reduced. As such, in heating devices with protrusions, it is desirable to achieve both an appropriate range of breathability for the sheet with the protrusions and to obtain the strength of the molded protrusions without causing the protrusions to collapse. However, with conventional methods for molding protrusions, it is often difficult to achieve both, and this issue is particularly pronounced when forming protrusions in a short period of time.
[0006] The present invention relates to a method for producing a sheet-type heating implement, which can achieve both control of the variation in air permeability of an air-permeable sheet when forming protrusions in a short time and strength of the protrusions of the sheet-type heating implement. [Means for solving the problem]
[0007] The present invention relates to the manufacture of a heating device having protrusions. This manufacturing method preferably includes a heating and deformation step in which a band-shaped laminate sheet is heated and pressurized using a first mold having a convex portion for forming the protrusion and a second mold having a concave portion corresponding to the protrusion to form a protrusion in the laminate sheet, and a material filling step in which a heat-generating material is placed within the protrusion of the laminate sheet in which the protrusion has been formed. The laminate sheet preferably has a structure in which nonwoven fabrics are laminated on both sides of a resin sheet. The resin sheet is preferably a breathable porous sheet containing polyethylene and / or polypropylene. When the melting point of the resin having the lowest melting point among the constituent resins of the nonwoven fabric is defined as the first melting point, and the melting point of the resin having the highest constituent ratio among the constituent resins of the resin sheet is defined as the second melting point, it is preferable that the first melting point is lower than the second melting point. In the heat deformation step, the heating temperature is preferably set to ±15° C. of the second melting point. In the heat deformation step, the applied pressure is preferably 0.1 MPa or more and 1 MPa or less. The heat deformation process is preferably carried out with a stop time of movement, that is, the time during which the first and second dies are stopped from the start of deformation of the laminate sheet to the end of pressing in which the portion of the laminate sheet that will become the protrusion is clamped between the convex portion of the first die and the concave portion of the second die, of 0.5 seconds or more and 200 seconds or less. Effect of the Invention
[0008] According to the present invention, in the production of a sheet-type heating implement, it is possible to control the variation in air permeability of the breathable sheet when forming protrusions in a short period of time, and to control the strength of the protrusions of the sheet-type heating implement. [Brief description of the drawings]
[0009] [Figure 1] FIG. 1(a) is a diagram showing a schematic diagram of one embodiment of a manufacturing method for a sheet-like heating implement of the present invention, and FIG. 1(b) is a plan view of a workpiece conveyed in the manufacturing apparatus shown in FIG. 1(a). [Diagram 2] Figures 2(a) to (d) are diagrams showing the heat deformation process, and are cross-sectional views showing the state in which the laminated sheet, which is the material for the sheet-shaped heating implement that has been transported, is pressed between a first mold and a second mold while being heated. [Diagram 3] FIG. 3 is an enlarged cross-sectional view showing a part of the laminate sheet. [Figure 4]FIG. 4(a) is a perspective view of a laminated sheet having a protrusion formed by the heat-deformed portion shown in FIG. 1, and FIG. 4(b) is a perspective view of the laminated sheet of FIG. 4(a) viewed from the recess side of the protrusion. [Diagram 5] FIG. 5(a) is a perspective view of the heating device obtained by the manufacturing method shown in FIG. 1, and FIG. 5(b) is a cross-sectional view taken along line II in FIG. 5(a). [Figure 6] FIG. 6 is an explanatory diagram for explaining the heat deformation step. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] Hereinafter, the present invention will be described based on preferred embodiments with reference to the drawings. Fig. 1 shows an example of a manufacturing device suitable for use in the manufacturing method of the present invention. Fig. 1(a) shows the main parts of a manufacturing device 10 used to implement the manufacturing method of the heating device 1. Fig. 1(b) shows a plan view of the workpiece in each part of the manufacturing device 10. The manufacturing device 10 transports the workpiece in a predetermined direction, and performs a heating deformation process (see Fig. 2), a material filling process, and a laminated sheet joining process, which will be described later, on the workpiece during the transport in this order, to manufacture the heating device.
[0011] In a preferred embodiment, a laminated sheet 20 is used as the workpiece. As shown in FIG. 3, the laminated sheet 20 has an inner layer 22 and outer layers 21, 23 arranged on both sides of the inner layer 22. More specifically, the laminated sheet 20 has a structure in which nonwoven fabrics as the outer layers 21, 23 are laminated on both sides of a resin sheet as the inner layer 22. The resin sheet constituting the inner layer 22 is a porous sheet having polypropylene (hereinafter referred to as PP) and / or polyethylene (hereinafter referred to as PE) as a constituent resin and having air permeability. This air permeable porous sheet (hereinafter also referred to as "air permeable porous sheet") is a sheet that has the property of allowing air to pass through but not allowing water to pass through, and is preferably one that has water vapor permeability. Whether or not a sheet has air permeability can be determined by whether or not the air permeability measured in accordance with JIS P8117 is 50000 sec / 100 cc or less. In other words, a sheet with an air permeability of 50000 sec / 100 cc or less is considered to have air permeability. As the breathable porous sheet, various known sheets can be used, for example, a sheet in which a thermoplastic molten resin containing an inorganic filler such as calcium carbonate is extruded into a sheet shape and then uniaxially or biaxially stretched to form micropores, etc. Such micropores are openings of 100 μm or less provided in the breathable porous sheet. The breathable porous sheet has an air permeability measured in accordance with JIS P8117: of preferably 1 sec / 100 cc or more, more preferably 3 sec / 100 cc or more, and preferably 20,000 sec / 100 cc or less, more preferably 10,000 sec / 100 cc or less.
[0012] The resin sheet constituting the inner layer 22 contains PP and / or PE. The resin sheet preferably contains PP and / or PE as the main resin, and the mass ratio of PP or PE to the mass of the entire resin sheet is preferably 85% or more and 100% or less, more preferably 90% or more and 100% or less, and even more preferably 95% or more and 100% or less. When the resin sheet contains both PP and PE, the total mass ratio is preferably in the above range. Examples of PP include homopolymers of propylene and copolymers of propylene with other components such as α-olefins. Examples of PP copolymers include random copolymers containing propylene and ethylene, etc. Examples of the random copolymers include those containing ethylene at a ratio of 4.5 mass percent or less. The melting peak temperature of the PP measured using a differential scanning calorimeter (DSC6200 manufactured by Seiko Instruments Inc.) is preferably 140° C. or higher and 180° C. or lower, and more preferably 150° C. or higher and 170° C. or lower. This melting peak temperature is the value of the resin alone, not including inorganic fillers, etc. Examples of PE include low-density PE, high-density PE, and linear low-density PE.
[0013] The laminate sheet 20 used has a resin sheet used as the inner layer 22 and a nonwoven fabric used as the outer layers 21, 23 that satisfy the specific condition A shown below. [Condition A] When the melting point of the resin having the lowest melting point among the constituent resins of the nonwoven fabric is defined as a first melting point, and the melting point of the resin having the highest constituent ratio among the constituent resins of the resin sheet is defined as a second melting point, the first melting point is lower than the second melting point. When the nonwoven fabrics constituting the outer layers 21 and 23 are the same, the melting point of the resin with the lowest melting point among the resins constituting the nonwoven fabric is taken as the first melting point. For example, when the nonwoven fabric is made of only a single type of fiber made of a single type of polyolefin resin, the first melting point is the melting point of the polyolefin resin. When the nonwoven fabric is made of only a single type of composite fiber made of multiple types of resins, the first melting point is the melting point of the resin with the lowest melting point among the resins constituting the composite fiber. On the other hand, when the nonwoven fabric contains multiple types of fibers with different types of constituent resins, the fiber containing the constituent resin with the lowest melting point is selected from the multiple types of fibers, and the melting point of the resin with the lowest melting point is set as the first melting point. However, among the resins constituting the nonwoven fabric, resins that are present in an extremely small amount relative to the mass of the nonwoven fabric, for example, resins that are present in an amount of 10% or less relative to the mass of the nonwoven fabric, are excluded from the resins to be compared in terms of melting point. The nonwoven fabrics constituting the two outer layers 21, 23 are preferably made of fibers containing the same resin. In this case, the nonwoven fabrics constituting the outer layers 21, 23 have a common first melting point, which makes it easier to satisfy the condition A. When the two outer layers 21, 23 have a common first melting point, this first melting point needs to be lower than the second melting point.
[0014] The resin sheet constituting the inner layer 22 is preferably composed of a single resin. In that case, the melting point of the resin constituting the resin sheet is the second melting point. The resin constituting the inner layer 22 may be a single type of resin or multiple types of resin. When the inner layer 22 is composed of multiple types of resin, the melting point of the resin having the highest composition ratio is the second melting point. Here, an example of a form in which the resin sheet constituting the inner layer 22 is composed of multiple types of resin is one in which the resin sheet contains two or more types selected from PP, polyethylene terephthalate (hereinafter referred to as PET), and PE.
[0015] The melting point is measured by the following method. [Method of measuring melting point] The melting point of the resin is measured by taking resin samples from the outer layers 21, 23 and the inner layer 22, and using a differential scanning calorimeter (DSC6200 manufactured by Seiko Instruments Inc.) to perform thermal analysis of the finely cut resin samples at a heating rate of 10°C / min to measure the melting peak temperature of the resin components. The resin samples are 2 mg of fiber samples taken from each of the outer layers 21, 23 and the inner layer 22, and are taken from 20 different positions on each of the outer layers 21, 23 and the inner layer 22. That is, 20 samples are taken each. The melting peak temperatures are measured using the differential scanning calorimeter for the 20 resin samples taken from the outer layers 21 and 23. The first melting point is the lowest melting peak temperature among the lowest melting peak temperatures (hereinafter also referred to as "minimum melting peak temperatures") in the resin samples of the outer layers 21 and 23 that appears in three or more of the 20 samples. The melting peak temperatures of the 20 resin samples taken from the inner layer 22 are measured using the above-mentioned differential scanning calorimeter. The melting peak temperature that appears most frequently among the 20 samples of the resin samples of the inner layer 22 is determined as the second melting point.
[0016] In order to control the heat generating characteristics of the sheet-like heating device to be manufactured, such as one or more of the temperature rise rate, maximum temperature, and heat generation duration, it is necessary to control the air permeability of the inner layer 22 which is a resin sheet. When the resin sheet of the inner layer 22 is perforated to impart breathability when the protrusions are formed, the degree of perforation may depend on the thickness and stretching characteristics of the nonwoven fabric of the outer layers 21 and 23 and the resin sheet of the inner layer 22. The degree of perforation in the inner layer 22 affects the heat generation performance of the protrusions 5. On the other hand, when perforations are formed in the resin sheet of the inner layer 22 after the protrusions are formed in the laminate sheet 20, the nonwoven fabric of the outer layers 21 and 23 is also perforated, and in the subsequent material filling step described below, the material such as paint 4A filled in the protrusions 5 may leak out. Therefore, by using an air-permeable porous sheet having micropores from the beginning as the resin sheet of the inner layer 22, it becomes unnecessary to open holes in the resin sheet when forming the protrusions 5 in the heat deformation step and after the protrusions 5 are formed after the heat deformation step, and it becomes possible to control the air permeability of the sheet. The method for measuring the air permeability will be described later in the examples.
[0017] 1, the symbol MD indicates the machine direction of a laminated sheet 20, which is a workpiece, and the symbol CD indicates a cross machine direction perpendicular to the machine direction MD. The laminated sheet 20 is strip-shaped, and the machine direction MD coincides with the longitudinal direction of the laminated sheet 20. The manufacturing apparatus 10 of this embodiment includes a workpiece constructing section 15 that manufactures a laminated sheet 20, a heat deformation section 11 that performs a heat deformation process on the laminated sheet 20, which is the workpiece, a material filling section 12 that performs a material filling process, and a laminated sheet joining section 13 that performs a laminated sheet joining process. In the manufacturing apparatus 10, the workpiece constructing section 15, the heat deformation section 11, the material filling section 12, and the laminated sheet joining section 13 are arranged in this order from the upstream side to the downstream side in the conveying direction MD.
[0018] In the manufacturing apparatus 10 of the embodiment shown in FIG. 1(a), the workpiece constituting section 15 laminates the outer layers 21 and 23, which are nonwoven fabrics, above and below the inner layer 22, which is a resin sheet, to manufacture a strip-shaped laminated sheet 20. Specifically, the sheets 21, 22, and 23, which are the raw materials of the laminated sheet 20, are each a strip-shaped sheet, and are arranged in a predetermined position (the workpiece constituting section 15) of the manufacturing apparatus 10 in the form of original rolls 210, 220, and 230 wound in a roll shape. In the workpiece constituting section 15, the sheets 21, 22, and 23 are fed from the multiple original rolls 210, 220, and 230, merged, and laminated, and further introduced into the nip device 16, where they are compressed in the thickness direction to be integrated, thereby manufacturing the laminated sheet 20. The strip-shaped laminated sheet 20 with a three-layer structure manufactured in this manner is transported to the heat deformation section 11, which performs the heat deformation process. At this stage, it is preferable that no adhesive be provided between the inner layer 22 and each of the outer layers 21, 23 of the laminated sheet 20 in order to ensure the breathability of the breathable porous sheet.
[0019] In the heat deformation process, the laminated sheet 20 is deformed to form protrusions 5, which are deformed convexly on one side (the outer layer 21 side) of the laminated sheet 20 and have a concave portion 50 on the other side (the outer layer 23 side), as shown in Figures 4(a) and (b). The side from which the protrusions 5 protrude is the side that becomes the surface 1a of the sheet-like heating device 1 (see Figure 5).
[0020] In the present invention, the shape of the protrusion 5 is not particularly limited, and may be, for example, a bullet shape, a cone shape, an elliptical cone shape, an oblong cone shape, or a truncated cone shape, such as a truncated cone shape, an elliptical truncated cone shape, or an oblong truncated cone shape. In the illustrated embodiment, the shape of the protrusion 5 is a cone shape. The protrusion 5 typically has a tapered shape toward its tip (as it moves away from the back surface 1b) as in the illustrated embodiment. It is preferable that the tip of the protrusion 5 is not sharp, but has a rounded shape as in the illustrated embodiment. When the heating device 1 has a plurality of protrusions 5, the shapes and / or dimensions of the protrusions 5 may be the same or different from each other. Furthermore, in the present invention, the arrangement of the protrusions 5 is not particularly limited, and may be, for example, a square lattice pattern, in addition to a houndstooth pattern.
[0021] The dimensions of each of the protrusions 5 are not particularly limited, and can be set appropriately depending on the application of the sheet-like heating implement 1, etc. The height H of the protrusion 5 (see FIG. 5(b)) is, for example, 2 mm or more and 15 mm or less, and preferably 3 mm or more and 10 mm or less. The diameter D of the protrusion 5 (see FIG. 4(b)) is, for example, 2 mm to 38 mm, and preferably 5 mm to 20 mm. The diameter D of the protrusion 5 is the diameter of the recess 50 of the protrusion 5 in a plan view. The thickness T (see FIG. 5(b)) of the laminated sheet 20 in the sheet-like heating implement 1 is, for example, 0.03 mm or more and 2.6 mm or less, and preferably 0.08 mm or more and 1.25 mm or less.
[0022] The heat deformation unit 11 performing the heat deformation process includes a first mold 11A and a second mold 11B, which are a pair of molds having interlocking concaves and convexes, as shown in FIG. 1(a) and FIG. 2(a) to (d). In this embodiment, the first mold 11A is disposed above the laminated sheet 20 and has a convex portion 110 protruding downward. The second mold 11B is disposed below the workpiece and has a concave portion 111 corresponding to the convex portion 110 of the first mold 11A. The first mold 11A and the second mold 11B are supported by a support (not shown) that periodically rises and falls. The first molds 11A and 11B are disposed so that when the first mold 11A descends and the second mold 11B ascends, the convex portion 110 of the first mold 11A fits into the concave portion 111 of the second mold 11B. The heat deformation unit 11 repeats the operation of fitting the convex portion 110 into the concave portion 111 by periodically raising and lowering the first mold 11A. The "lifting" means an up and down movement in the direction of gravity, and is performed by a lifting mechanism (not shown) such as a hydraulic cylinder or a pneumatic cylinder connected to the molds 11A and 11B. The first mold 11A and the second mold 11B may be arranged in other configurations that allow them to approach and move away from each other, other than being arranged above and below each other.
[0023] The heat deformation section 11 is equipped with a heating means (not shown) for heating the workpiece (laminate sheet 20). The heating means heats and softens the workpiece, which is made easier to deform (form the protrusions 5) by the outer layers 21, 23 and inner layer 22 of the workpiece containing a thermoplastic resin. As the heating means, any known means that can be used for this type of so-called heat press can be used without any particular restriction.
[0024] The heating means in the thermal deformation section 11 may be, for example, built into one or both of the pair of dies 11A, 11B, the first die 11A and the second die 11B, so that the workpiece is heated by the heating means while being compressed by the pair of dies 11A, 11B. Furthermore, the heating means may be disposed upstream of the pair of dies 11A, 11B in the conveying direction MD, so that the workpiece before being compressed by the pair of dies 11A, 11B is preheated by the heating means.
[0025] A laminate sheet 20 is introduced into the interlocking portion of a pair of molds 11A, 11B, i.e., the portion where the convex portion 110 of the first mold 11A and the concave portion 111 of the second mold 11B can fit together, and the laminate sheet 20 is compressed in the thickness direction by the first mold 11A and the second mold 11B, and the laminate sheet 20 is heated by the heating means, thereby imparting an uneven shape to one side of the laminate sheet 20, as shown in Figure 1(a), which includes protrusions 5 that protrude beyond the surrounding area and flat portions (non-protrusions) 6 that do not protrude. More specifically, the heat deformation process carried out by the heat deformation section 11 includes a deformation stage in which the convex portion 110 of the first mold 11A is pressed against the laminated sheet 20 to deform it while heating it, and a pressing stage in which the portion of the laminated sheet 20 that will become the protrusion portion 5 is clamped between the convex portion 110 of the first mold 11A and the concave portion 111 of the second mold 11B.
[0026] The heat deformation step is carried out so as to satisfy the following conditions 1 to 3. [Condition 1] The heating temperature is set to ±15°C of the second melting point. That is, regardless of the heating method, the heating temperature when heating the laminated sheet 20 is set to ±15°C of the second melting point. The second melting point is specified in the above-mentioned condition A. The heating temperature in the heat deformation step is the set temperature of the heating means described above. As a method for setting the heating temperature to a predetermined temperature within ±15°C of the second melting point, it is preferable to set both the first mold 11A and the second mold 11B to a common temperature within ±15°C of the second melting point. The heating temperature is preferably closer to the second melting point from the viewpoint of more reliably ensuring the breathability of the resin sheet constituting the inner layer 22 and from the viewpoint of further improving the formability of the protrusions 5. For example, the heating temperature is preferably within ±10°C, more preferably ±5°C, of the second melting point.
[0027] [Condition 2] The applied pressure is 0.1 MPa or more and 1 MPa or less. The applied pressure is a value (thrust force / pressure applied area) obtained by dividing the thrust force of the lifting mechanism (air cylinder, etc.) for lifting and lowering the pair of dies 11A and 11B when the laminated sheet 20 is sandwiched between the convex portion 110 of the first die 11A and the concave portion 111 of the second die 11B by the pressure applied area. The pressure applied area is the contact area of the die 11 with the laminated sheet 20 when the laminated sheet 20 is sandwiched. In other words, the pressure applied area is the same as the area of the concave portion 50 of the protrusion 5 in a plan view. The applied pressure can also be said to be the applied pressure to the laminated sheet 20 by the pair of dies 11A and 11B, the first die 11A and the second die 11B, and is the pressure applied to the laminated sheet 20 by the dies 11A and 11B when the laminated sheet 20 is sandwiched between the convex portion 110 of the first die 11A and the concave portion 111 of the second die 11B. From the viewpoint of further improving the strength of the protrusions 5, the applied pressure is preferably 0.1 MPa or more and 0.7 MPa or less, and more preferably 0.1 MPa or more and 0.4 MPa or less.
[0028] [Condition 3] The movement stop time must be between 0.5 and 200 seconds. The stop time is the time during which the first mold 11A and the second mold 11B are stopped from the time when the first mold 11A starts to deform the laminate sheet 20 to the time when the pressing process in which the portion of the laminate sheet 20 that will become the protrusion 5 is clamped between the convex portion 110 of the first mold 11A and the concave portion 111 of the second mold 11B is completed. By setting the movement stop time to 0.5 seconds or more, it is possible to ensure sufficient strength for the produced protrusions, and by setting the movement stop time to 200 seconds or less, the time required to form the protrusions can be shortened, thereby improving the production efficiency of the formation of sheets with protrusions and the heating device. The movement stop time is preferably 0.5 seconds or more, more preferably 1 second or more, and is preferably 60 seconds or less, more preferably 10 seconds or less.
[0029] The heat deformation process has three stages: a first stage from when one or both of the first mold 11A and the second mold 11B start to move toward each other until the convex portions 110 of the first mold 11A come into contact with the laminate sheet 20; a second stage from when the laminate sheet starts to deform due to the pressure of the convex portions 110 (at the start of deformation) until the portions of the laminate sheet 20 that will become the protrusions 5 are pressed into the recesses 111 while being deformed; a third stage from when the pressing of the convex portions 110 ends until the start of release, in which the first mold 11A is moved to the side opposite the second mold 11B; and a fourth stage from when the laminate sheet 20 with the protrusions formed thereon starts to move from between the first mold 11A and the second mold 11B to the location for the next process (see Figure 6). The second stage is a stage from when the laminate sheet 20 and the convex portions 110 start to come into contact with each other until the convex portions 110 and the concave portions 111 fit together, sandwiching the laminate sheet 20, and the convex portions 110 push into the concave portions 111, thereby deforming the portions of the laminate sheet 20 that will become the protrusions 5. In the third stage, the portions of the laminate sheet 20 that will become the protrusions 5 are sandwiched (pressed) between the convex portions 110 and the concave portions 111. The movement stop time is the time during which the movement of the first mold 11A (convex portion 110) and the second mold 11B (concave portion 111) stops in the second and third stages. In other words, it is the time during which the movement of the convex portion 110 and the concave portion 111 toward or away from each other stops in the second and third stages. The movement stop time includes the time spent from the end of the second stage to the end of the third stage. Furthermore, if the heat deformation process includes a deformation stop process described below, the movement stop time includes a temporary pause time described below.
[0030] The protrusions 5 formed in the heat deformation process are formed so that the ratio (percentage) of the surface area to the bottom area is 120% or more, where the surface area is the area of the surface of the protrusions 5 on one side of the laminated sheet 20 (the area of the outer surface of the protrusions) and the bottom area is the area of the bottom of the protrusions 5 located at the starting point of the protrusions 5 on the upper side in the direction of gravity on the back surface 1b of the laminated sheet 20. By making this ratio [(surface area / bottom area) area x 100] 120% or more, there is an advantage that it is easier to feel a sensation of being pressed when pressing the skin. From the viewpoint of such an advantage, the ratio is preferably 130% or more. From the viewpoint of ensuring sufficient strength for the protrusions, the ratio of the surface area to the bottom area is preferably 320% or less, more preferably 200% or less.
[0031] In the heat deformation step, the protrusions 5 may be formed on the laminated sheet 20 during transportation, but from the viewpoint of facilitating the formation of the protrusions 5 and reliably forming the protrusions 5 as designed, it is preferable to form the protrusions 5 on the laminated sheet 20 in a state where transportation is stopped. When the protrusions 5 are formed during transportation of the laminated sheet 20, restrictions arise on the protrusion shape (convex shape) of the protrusions 5, but when the protrusions are formed in a state where transportation is stopped, it is possible to stably process any shape. In the latter case, the strip-shaped laminated sheet 20 is transported in the transport direction MD, and when the region of the laminated sheet 20 to be subjected to the heat deformation step (hereinafter also referred to as the "protrusion formation planned region") is introduced into the heat deformation section 11 (between the first mold 11A and the second mold 11B), the transport of the laminated sheet 20 is stopped, and the protrusion formation planned region is compressed by the pair of molds 11A and 11B to form the protrusions 5. Thereafter, the transport of the laminated sheet 20 is resumed. In the manufacturing method of the heating device 1, the laminated sheet 20 is continuous in the conveying direction MD, and the regions of the laminated sheet 20 where the protrusions are to be formed are introduced intermittently at a fixed cycle into the heat deformation section 11, so that when the above-mentioned preferred embodiment is implemented, a series of operations such as "conveying the workpiece (laminated sheet 20) → stopping → forming the protrusions (heat deformation process)" is repeated. The manufacturing device 10 is preferably equipped with an intermittent processing system that performs such repeated operations.
[0032] It is preferable that the heat deformation process includes a deformation stopping step for stopping the pressure deformation of the laminated sheet by the convex portion for a certain period of time during the second stage described above, i.e., between the start of deformation of the laminated sheet and the start of the pressing. It is preferable to continue heating the laminated sheet 20 even in the deformation stopping step. The start of deformation of the laminated sheet refers to the time when the laminated sheet starts to deform due to the pressing of the laminated sheet 20 by the convex parts 110. The start of pressing refers to the time when the convex parts 110 and the concave parts 111 engage with each other while sandwiching the laminated sheet 20 and the movement of the convex parts 110 and the concave parts 111 stops, and is the time when pressing begins to sandwich and press the parts of the laminated sheet 20 that will become the protrusions 5 between the convex parts 110 and the concave parts 111. When the heat deformation process includes a deformation stopping process, the movement stop time is the total time of the time spent from the end of the second stage to the end of the third stage and the temporary stop time during which the pressurized deformation of the laminated sheet 20 by the convex portion 110 in the second stage is stopped. In the deformation stopping process, the temporary stop time is preferably 50% or more and less than 100% of the movement stop time.
[0033] By providing the deformation stop step, the amount of deformation of the laminated sheet when the protrusions 5 are formed by the first mold 11A can be divided, so that damage to the laminated sheet 20 can be reduced. More specifically, a series of movements in which the convex parts 110 and the concave parts 111 approach each other in the second stage is divided into two, the first and second pressings, with a temporary stop time in between. In this case, the amount of deformation can be reduced during pressing by the convex parts 110 until the temporary stop time (first pressing), so that the stress applied to the edge (boundary) between the part where deformation occurs and the part where deformation does not occur in the laminated sheet 20 can be suppressed. When pressing by the convex parts 110 after the temporary stop time (second pressing), the sheet has been somewhat deformed by the first pressing, so that the shear applied by pressing is weakened, the stress is reduced, and damage to the laminated sheet 20 due to stretching can be suppressed. In this way, damage caused by stretching to the inner layer resin sheet during deformation and damage such as melting due to heating and molding can be suppressed to maintain the required air permeability while ensuring the protrusion strength of the protrusions of the laminated sheet, making it easy to achieve both control of air permeability fluctuations and protrusion strength.
[0034] In the heat deformation process, there are cases where the deformation stop step does not need to be provided. For example, instead of stopping the formation of the protrusions on the laminated sheet 20 by the first mold 11A for a certain period of time, the laminated sheet 20 may be pressed between the concave portion of the second mold 11B while decelerating the first mold 11A to a very low speed, and the laminated sheet 20 may be gradually deformed along the concave portion 111 of the second mold 11B while moving the first and second molds 11A and 11B at a low speed. In order to further reduce damage to the laminated sheet 20, if the deformation stop step is not provided in the heat deformation process, the moving speed (rising and lowering speed) of the first mold 11A and the second mold 11B can be preferably 15 mm / sec or less, and may be, for example, more than 0 mm / sec and 1 mm / sec or less. In addition, when a deformation stop process is provided in the heating and deformation process, the movement speed (raising and lowering speed) of the first mold 11A and the second mold 11B is preferably more than 0 mm / sec and not more than 30 mm / sec, more preferably more than 15 mm / sec and not more than 30 mm / sec, and even more preferably 25 mm / sec or more and not more than 30 mm / sec.
[0035] After the deformation stopping process, the descent of the first mold 11A is resumed, the convex portion 110 of the first mold is engaged with the concave portion 111 to clamp the laminated sheet 20, and the formation of the protrusion portion 5 on the laminated sheet 20 is completed by applying pressure by the pair of molds 11A, 11B (third stage). In the heat deformation step, the deformation amount of the laminated sheet 20 until the deformation stopping step is preferably 50% to 90% of the deformation amount of the laminated sheet 20 after the deformation stopping step, i.e., the final deformation amount of the sheet 20, and more preferably 50% to 85%. The ratio of the deformation amount of the laminated sheet 20 until the deformation stopping step to the final deformation amount [(deformation amount of the laminated sheet 20 until the deformation stopping step / the final deformation amount)×100] is also called the "intermediate deformation rate" (%). When the final deformation amount is taken as 100%, it is easier to ensure the strength of the protrusions 5 by providing the deformation stopping step after the latter half of the final deformation amount (when the intermediate deformation rate is 50% or more).
[0036] The material filling step is a step of filling the recesses 50 of the protrusions 5 formed on one side of the laminate sheet 20 in the heat deformation step with the heat generating material 4 including the paint 4A, the electrolyte 4B, and the water retention material 4C (e.g., water-absorbent polymer) from the other side (the side facing the back surface layer 3) of the laminate sheet 20. That is, in the material filling step, the heat generating material 4 is filled in the protrusions 5.
[0037] The heat generating material 4 used in the present invention may contain an oxidizable metal or may contain water. In the material filling step, all the components contained in the heat generating material may be filled into the recess 50 in a single filling operation, or all the components contained in the heat generating material 4 may be filled into the recess 50 in multiple filling operations. Generally, the entire recess 50 is filled with the heat generating material 4, but the amount of heat generating material filled in the recess 50 is not particularly limited and can be adjusted as appropriate.
[0038] From the viewpoint of improving handleability, when the coating material 4A is filled into the recess 50, it may be filled into the recess 50 as a slurry containing an oxidizable metal and water. The slurry may contain other components in addition to the oxidizable metal and water, and a preferred example of the other components is a carbon component (such as activated carbon) that can be used as the inorganic water retention material 4C. By including an oxidizable metal and a carbon component in this slurry, the exothermic reaction of the exothermic material 4 is promoted.
[0039] An example of a filling operation of the heat generating material 4 that can be performed in the material filling step is filling the recesses 50 with a water retention material 4C separately from the paint 4A and the electrolyte 4B. The water retention material 4C absorbs and retains moisture, so the viscosity of a slurry containing the water retention material 4C becomes relatively high. By filling the recesses 50 with the water retention material 4C, the paint 4A, and the electrolyte 4B at different times, the handling of the heat generating material 4 to be filled is improved, and the heat generating material 4 can be filled with even greater precision.
[0040] Another example of the filling operation of the heat generating material 4 that can be performed in the material filling step is the operation of filling the recess 50 with the electrolyte 4B separately from the paint 4A and the water retaining material 4C. This makes it possible to more reliably prevent the occurrence of rust on the metal parts of the manufacturing apparatus 10, including the device for filling the heat generating material 4, even when an electrolyte 4B such as sodium chloride is used.
[0041] As shown in Figure 1(a), the material filling section 12 which carries out the material filling process includes, from the upstream side in the conveying direction MD, a first filling device 12A which handles paint 4A, a second filling device 12B which handles electrolyte 4B, and a third filling device 12C which handles water-retaining material 4C, and is configured to fill the recesses 50 of the protrusions 5 of the laminated sheet 20 which has undergone the heating deformation process with the paint 4A, the electrolyte 4B, and the water-retaining material 4C in that order.
[0042] The electrolyte 4B handled by the second filling device 12B and the water-retaining material 4C handled by the third filling device 12C are both in a dry state, typically in powder form. Therefore, the order of filling the recess 50 with the heat generating material by the material filling unit 12 is "paint 4A (slurry containing oxidizable metal and water), electrolyte 4B (powder), and water-retaining material 4C (powder)". In the present invention, the order of filling the heat generating material 4 into the recess 50 is not limited to this and can be set arbitrarily, but if the slurry is filled into the recess 50 before the powder, the powder filled into the recess 50 thereafter absorbs the moisture of the slurry already filled in the recess 50, so that the powder is less likely to scatter and spill out of the recess 50. For this reason, in this embodiment, a method is adopted in which the components contained in the heat generating material 4 (paint 4A, electrolyte 4B, and water-retaining material 4C) are divided into three portions and filled into the recess 50 in the above order.
[0043] Each of the filling devices 12A to 12C includes a discharge means 120 such as a nozzle that discharges a slurry or powder toward the recess 50. As the filling devices 12A to 12C, a known filling device capable of filling the laminated sheet 20 with a slurry or powder without contacting the laminated sheet 20 can be used. The number of discharge means 120 provided in the filling device 12A is not particularly limited, and may be one, but is preferably equal to or greater than the number of rows of recesses 50 arranged in a row in the conveying direction MD in the laminated sheet 20. For example, as shown in FIG. 1(b) in this embodiment, the number of rows of recesses 50 arranged in a row in the conveying direction MD in the laminated sheet 20 is three rows in total, including one row located at the center of the laminated sheet 20 in the conveying cross direction CD, and two rows located on both sides of the central row in the conveying cross direction CD and having a shorter interval between adjacent recesses 50 in the conveying direction MD than the central row, so that the filling device 12A preferably has at least three discharge means 120 corresponding to the three rows of recesses 50, respectively. This makes it easier to efficiently and uniformly fill the multiple recesses 50 in the laminated sheet 20 with the heat generating material 4.
[0044] The laminated sheet joining process is a process in which a covering sheet 30 which forms the back layer 3 is placed on the other side of the laminated sheet 20 (the side filled with the heat generating material 4) and the laminated sheet 20 and the covering sheet 30 are joined by sealing, resulting in a heating device continuum 40 (see Figure 1 (b)) in which multiple heating devices 1 are lined up in a row in the conveying direction MD.
[0045] As shown in FIG. 1(a), the laminated sheet joining section 13 that performs the laminated sheet joining process includes a supply mechanism for the covering sheet 30 that forms the back layer 3, and a joining device 14. The covering sheet 30 in this embodiment is a strip-shaped sheet, and is arranged at a predetermined position in the manufacturing device 10 in the state of a roll of original fabric wound into a roll. A fusion device can be used as the joining device 14. The laminated sheet joining section 13 uses the supply mechanism for the covering sheet 30 to unwind the covering sheet 30 from the original fabric roll, and overlaps it on the surface of the heating material 4 filled side of the strip-shaped laminated sheet 20 that is being transported through the material filling process, introduces it into the joining device 14, and joins the laminated sheet 20 and the covering sheet 30 to form a joint 7, thereby manufacturing the heating device continuum 40.
[0046] The continuous body 40 of heating implements thus produced in the laminated sheet joining process is then conveyed in the conveying direction MD and cut into a predetermined product unit size. In this way, a plurality of individual heating implements 1 are continuously produced.
[0047] According to the manufacturing method of the heating device configured as described above, particularly in the material filling step, the recesses 50 of the protrusions 5 in the laminated sheet 20 are filled with a heat generating material 4 containing paint 4A, water retention material 4C and electrolyte 4B. This allows greater freedom in the design of the heating device 1 compared to a method in which a sheet already containing the heat generating material 4 is used as a constituent member of the heating device 1, and also allows for the consistent manufacture of high-quality heating devices 1 regardless of the shape of the protrusions 5 (recesses 50).
[0048] While the present invention has been described above based on its preferred embodiments, the present invention is not limited to the above-described embodiments and can be modified as appropriate without departing from the spirit of the present invention. EXAMPLES
[0049] Example 1 In Example 1, a sheet-shaped heating device 1 was produced using the device shown in Figs. The laminate sheet 20 used a nonwoven fabric consisting of 60% PET fiber and 40% low-melting-point PET fiber as the nonwoven fabric of the outer layers 21 and 23, and a microporous PP sheet as the resin sheet of the inner layer 22. The second melting point (melting point of PP) of the laminate sheet was 160°C, and the first melting point (low-melting-point PET) was 80°C. The laminated sheet 20 was conveyed at a conveying speed of 1.8 m / min, and the conveyance of the laminated sheet 20 was stopped when the laminated sheet 20 was introduced into the heat deformation section 11 (between the first mold 11A and the second mold 11B), and the heat deformation process was carried out on the laminated sheet 20 using the first molds 11A and 11B. In the heat deformation process of Example 1, a deformation stopping process was carried out. After the heat deformation process, a material filling process was carried out in which the inside of the protrusions 5 was filled with the heat generating material 4, and then a covering sheet was superimposed and joined to the other side of the laminated sheet 20. The heating device continuous body 40 thus obtained was cut into individual sheets so that there were five protrusions 5, and a sheet-like heating device 1 was obtained (see FIG. 5(a)).
[0050] [Examples 2 to 4] In Example 2, the heating device 1 was manufactured in the same manner as in Example 1, except that the intermediate deformation ratio in the deformation stopping step [(deformation amount of the laminated sheet 20 up to the deformation stopping step / final deformation amount)×100] was changed. In Example 3, the heating device 1 was manufactured in the same manner as in Example 1, except that the applied pressure in Condition 2 was changed and the deformation stopping step was not performed. In Example 4, the heating device 1 was manufactured in the same manner as in Example 1, except that the deformation stopping step was not carried out. In Example 5, the heating device 1 was manufactured in the same manner as in Example 1, except that the intermediate deformation rate in the deformation stopping step was changed.
[0051] Table 1 shows conditions 1 to 3 (applied pressure, heating temperature, and movement stop time) of the heat deformation process in each Example. In Table 1, the number of stops indicates the number of times the process was temporarily stopped during the second stage of the heat deformation process. The movement stop time is the time spent from the end of the second stage to the end of the third stage, and was set to 1.0 second regardless of whether there was a pause time. The movement stop time in Examples 1, 2, and 5 is the total time of the pause time in the deformation stopping process and the time spent from the end of the second stage to the end of the third stage. The movement stop time in Examples 3 and 4 is the time spent from the end of the second stage to the end of the third stage.
[0052] [Collapse rate] After measuring the height H of the five projections 5 in the obtained sheet-like heating implement 1, weights were placed on the projections 5, and a load of about 3.18N was applied to the five projections 5. The load of 3.18N is the assumed load applied to the heating implement 1 when it is worn on the body (lower back, etc.). After the load was applied, the height H of the projections 5 was measured. Then, the ratio of the height H1 of the projections 5 after the load was applied to the height H0 of the projections 5 before the load was applied [(H1 / H0)×100] was calculated, and this was calculated as the projection crush rate (%) of the projections 5 crushed by the load. Such measurements were performed on three heating implements, and the average crush rate (%) was calculated. The results are shown in Table 1 below. The lower the crushing rate, the greater the projection strength of the projection 5 against a load.
[0053] [Air permeability of laminated sheet] The air permeability of the laminated sheet 20 after the projections 5 were formed by the above-mentioned heat deformation process was measured using an automatic Gurley densometer (Yasuda Seiki Seisakusho). The measurement points for such air permeability were the entire heating device 1 shown in Fig. 5(a), including the points where the projections 5 were formed and the points other than the projections 5. The air permeability of the laminated sheet 20 before the heat deformation process was 2767 to 4558 (sec / 100cc). The measurement results are shown in Table 1 below. It was also confirmed separately that when the air permeability of the laminated sheet is in the range of 2000 to 5000 seconds / 100 cc, there is no effect on the product performance such as the heat generation characteristics of the heating device.
[0054] [Table 1]
[0055] The results shown in Table 1 indicate that Examples 1 to 5 have sufficient breathability for use as a heating device. In particular, the results showed that there was no significant difference in the breathability of the laminate sheet 20 before and after the heat deformation step. Furthermore, the projections of Examples 1 to 5 had a low crush rate of less than 30% when subjected to a load of 3.18 N. These results demonstrated that Examples 1 to 5 had sufficient projection strength for use as a heating device. The above results demonstrate that the heating devices of Examples 1 to 5 are excellent in both the strength of the protrusions and the breathability of the sheet after processing. [Explanation of symbols]
[0056] 1. Sheet-type heating device (heating device) 5 Protrusion 11 Heat-deformed part 11A, 11B A pair of dies 11A First Mold 11B Second mold 20 Laminated Sheet 21 Outer layer (non-woven fabric) 22 Inner layer (resin sheet) 23 Outer layer (non-woven fabric) 40 Heating Tool Continuum 50 Recess 110 Convex 111 Recess
Claims
1. A method for manufacturing a heating tool having a protrusion, a heat deformation step of heating and pressurizing a strip-shaped laminated sheet using a first mold having a convex portion for forming the protrusion portion and a second mold having a concave portion corresponding to the convex portion to form the protrusion portion on the laminated sheet; and a material filling step of disposing a heat generating material inside the protrusions of the laminated sheet on which the protrusions are formed, The laminate sheet has a structure in which nonwoven fabrics are laminated on both sides of a resin sheet, The resin sheet is a breathable porous sheet containing polypropylene and / or polyethylene, When the melting point of the resin having the lowest melting point among the resins constituting the nonwoven fabric is defined as a first melting point, and the melting point of the resin having the highest composition ratio among the resins constituting the resin sheet is defined as a second melting point, the first melting point is lower than the second melting point, The heat deformation step includes: The heating temperature is set to ±15° C. of the second melting point, The applied pressure is 0.1 MPa or more and 1 MPa or less, This method for manufacturing a heating device comprises the steps of: (1) setting a stop time for which the first and second dies are stopped from the start of deformation of the laminated sheet to the end of pressing in which the portion of the laminated sheet that will become the protrusion is clamped between the convex portion of the first die and the concave portion of the second die of 0.5 seconds or more and 200 seconds or less.
2. The method for manufacturing a heating implement according to claim 1, wherein the applied pressure is 0.3 MPa or more.
3. The method for manufacturing a heating implement according to claim 1 or 2, wherein the heat deformation process includes a deformation stopping process for stopping the pressure deformation of the laminated sheet by the convex portion for a certain period of time between the start of deformation of the laminated sheet and the end of the pressing.
4. The method for manufacturing a heating implement according to claim 3, wherein the temporary stop time in the deformation stopping step is 50% or more and less than 100% of the movement stop time.
5. A method for manufacturing a heating device according to any one of claims 3 to 4, wherein in the heat deformation process, the amount of deformation of the laminated sheet up to the deformation stopping process is 50% or more and 90% or less of the final deformation amount of the laminated sheet in the heat deformation process.
6. The method for manufacturing a heating implement according to any one of claims 1 to 5, wherein the protrusions formed in the heat deformation step have a surface area that is 120% or more relative to a base area.
Citation Information
Patent Citations
Heating instrument
JP2018175857A
Hyperthermia tool
JP2019171007A