Paper laminate tube
The paper laminate tube addresses cohesion and peeling issues by using a single-layer paper base with optimized fiber lengths and resin layers to enhance bonding strength and moisture resistance, ensuring structural stability.
Patent Information
- Application Number
- JP2023051188
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-28
- Publication Date
- 2024-10-10
AI Technical Summary
Existing tube containers made of a paper base layer are prone to cohesion and peeling due to moisture intrusion from the contents or external sources, which affects their structural integrity.
A paper laminate tube design featuring a single-layer paper base material with specific fiber length ratios and resin layers to enhance bonding strength, combined with a resin-impregnated structure to prevent moisture ingress and layer separation.
The design effectively suppresses aggregation and peeling of the paper base material, maintaining structural integrity even under repeated use and moisture exposure.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
[Technical field]
[0001] The present disclosure relates to a paper laminate tube. [Background technology]
[0002] For example, JP 2021-104851 A (Patent Document 1) describes a tube container. The tube container described in Patent Document 1 has a body. The body is made of a sheet member bent into a cylindrical shape. The sheet member has a paper base layer. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2021-104851 A Summary of the Invention [Problem to be solved by the invention]
[0004] In the tube container described in Patent Document 1, the inside of the body is filled with contents. In addition, the tube container described in Patent Document 1 may be exposed to external moisture. In the tube container described in Patent Document 1, moisture in the contents or external moisture may penetrate into the paper base layer, causing coagulation and peeling in the paper base layer.
[0005] The present disclosure has been made in consideration of the problems of the conventional techniques as described above. More specifically, the present disclosure provides a paper laminate tube capable of suppressing cohesive peeling of the paper base material constituting the body portion. [Means for solving the problem]
[0006] The paper laminate tube of the present disclosure includes a body portion. The body portion is made of a sheet member having a first surface and a second surface opposite to the first surface, and is bent into a cylindrical shape so that the first surface faces inward. The sheet member has a paper substrate. The paper substrate includes a first single-ply paper.
[0007] In the above paper laminate tube, the first monolayer paper may include a plurality of first fibers and a plurality of second fibers. The length of each of the plurality of first fibers may be longer than the length of each of the plurality of second fibers and may be 4 mm or less. The length of each of the plurality of second fibers may be 0.2 mm or more and 1.5 mm or less. The content of the first fibers in the first monolayer paper may be 50 percent or more.
[0008] In the above paper laminate tube, the basis weight of the first single layer paper is 165g / m 2 It may be less than.
[0009] In the above-mentioned paper laminate tube, the paper substrate may further include a second monolayer paper layered on the first monolayer paper.
[0010] In the above-mentioned paper laminate tube, the paper base material may further have a resin layer sandwiched between the first monolayer paper and the second monolayer paper. The resin layer may be impregnated into the surface of the first monolayer paper and the surface of the second monolayer paper.
[0011] In the above-mentioned paper laminate tube, the resin layer may be made of a resin material having a melting point of 300° C. or lower.
[0012] In the above-mentioned paper laminate tube, the distance between the center of the sheet member in the thickness direction and the resin layer may be 10 percent or less of the thickness of the sheet member.
[0013] In the above-mentioned paper laminate tube, the sheet member may have a first end and a second end, which are both ends in a second direction perpendicular to the first direction corresponding to the longitudinal direction of the body, when not bent. The sheet member may have a first surface at the first end and a second surface at the second end bonded together when bent into a cylindrical shape. The sheet member may have a first surface resin layer on the first surface and a second surface resin layer on the second surface. The thickness of the first surface resin layer may be equal to or greater than the thickness of the second surface resin layer.
[0014] The paper laminated tube may further include a spout having an opening communicating with the inside of the body. The spout may be made of a resin material having an MFR of 0.5 g / 10 min or more, have a maximum thickness of 2.0 mm or less, and be welded to one end of the body in the longitudinal direction. Effect of the Invention
[0015] The paper laminated tube of the present disclosure can suppress cohesive peeling of the paper base material that constitutes the body portion. [Brief description of the drawings]
[0016] [Figure 1] FIG. 2 is a front view of the paper laminate tube 100. [Diagram 2] FIG. 1 is a plan view of a paper laminate tube 100. [Diagram 3] FIG. 2 is a schematic cross-sectional view taken along line III-III in FIG. [Figure 4] FIG. 4 is a schematic cross-sectional view taken along line IV-IV in FIG. [Diagram 5] FIG. [Figure 6] FIG. 6 is a cross-sectional view taken along line VI-VI in FIG. [Figure 7] 4 is a partially enlarged view of FIG. 3 in the vicinity of the first end 20c and the second end 20d. [Figure 8] 5 is a partially enlarged view of FIG. 4 in the vicinity of the opening 10a. [Figure 9] 11 is a cross-sectional view of a sheet member 20 according to a modified example. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0017] The details of the embodiment of the present disclosure will be described with reference to the drawings. In the following drawings, the same or corresponding parts are given the same reference numerals, and the overlapping description will not be repeated. The paper laminate tube according to the embodiment is referred to as a paper laminate tube 100.
[0018] (Configuration of Paper Laminated Tube 100) The structure of the paper laminate tube 100 will be described below.
[0019] Fig. 1 is a front view of the paper laminated tube 100. Fig. 2 is a plan view of the paper laminated tube 100. Fig. 3 is a schematic cross-sectional view taken along line III-III in Fig. 1. Fig. 4 is a schematic cross-sectional view taken along line IV-IV in Fig. 2. As shown in Figs. 1 to 4, the paper laminated tube 100 has a body 10 and a spout 30.
[0020] The body portion 10 is formed by bending a sheet member 20 into a cylindrical shape. FIG. 5 is a plan view of the sheet member 20. FIG. 6 is a cross-sectional view taken along line VI-VI of FIG. 5. As shown in FIGS. 5 and 6, the sheet member 20 is sheet-like. The sheet member 20 has a first surface 20a and a second surface 20b. The first surface 20a and the second surface 20b are end surfaces of the sheet member 20 in the thickness direction. The first surface 20a faces the inside of the body portion 10 when bent into a cylindrical shape. The second surface 20b is the surface opposite to the first surface 20a. That is, the second surface 20b faces the outside of the body portion 10 when bent into a cylindrical shape.
[0021] The sheet member 20 has a paper base material 21. The paper base material 21 is made of a single layer paper 21a. The single layer paper 21a preferably includes a plurality of first fibers and a plurality of second fibers. The length of each of the plurality of first fibers is longer than the length of each of the plurality of second fibers. The length of each of the plurality of first fibers is preferably 4 mm or less. The length of each of the plurality of second fibers is preferably 0.2 mm or more and 1.5 mm or less.
[0022] The content of the first fibers in the single layer paper 21a is preferably 50 percent or more. The content of the first fibers in the single layer paper 21a is the number of the first fibers contained in the single layer paper 21a divided by the number of fibers contained in the single layer paper 21a. The lengths of the first fibers and the second fibers are calculated based on an automatic optical measurement method defined in JAPAN TAPPI Paper and Pulp Testing Method No. 52 (Testing Method for Fiber Length of Paper and Pulp).
[0023] The basis weight of the single-ply paper 21a is 165 g / m 2 The basis weight of the single-ply paper 21a is measured according to the method for measuring the basis weight of paper defined in the JIS standard (JIS P 8124:2011).
[0024] The sheet member 20 may further have a first surface resin layer 22 and a second surface resin layer 23. The first surface resin layer 22 constitutes the first surface 20a. The thickness of the first surface resin layer 22 is defined as thickness T1. The second surface resin layer 23 constitutes the second surface 20b. The thickness of the second surface resin layer 23 is defined as thickness T2. It is preferable that the thickness T1 is greater than the thickness T2. The resin material constituting the first surface resin layer 22 and the second surface resin layer 23 is, for example, polyethylene (PE). However, the resin material constituting the first surface resin layer 22 and the second surface resin layer 23 is not limited to this.
[0025] The sheet member 20 may further have a barrier layer 24, a first adhesive layer 25, and a second adhesive layer 26. The barrier layer 24 is disposed between the paper base material 21 and the first surface resin layer 22. The first adhesive layer 25 is disposed between the paper base material 21 and the barrier layer 24, and the second adhesive layer 26 is disposed between the barrier layer 24 and the first surface resin layer 22.
[0026] The material of the barrier layer 24 is, for example, aluminum. The material of the first adhesive layer 25 is, for example, ethylene-methacrylic acid copolymer (EMAA). The material of the second adhesive layer 26 is, for example, polyethylene terephthalate (PET). However, the material of the barrier layer 24 is not limited thereto. For example, the material of the barrier layer 24 is ethylene-vinyl alcohol copolymer (EVOH). In this case, the material of the first adhesive layer 25 may be polyethylene, and the second adhesive layer 26 may be omitted.
[0027] In a plan view, the first direction DR1 corresponds to the longitudinal direction of the body 10 when the sheet member 20 is bent. The second direction DR2 is a direction perpendicular to the first direction DR1 in a plan view. The sheet member 20 has a first end 20c and a second end 20d in the second direction DR2. The second end 20d is an end opposite to the first end 20c. The sheet member 20 is bent into a cylindrical shape so that the first surface 20a faces the inside of the body 10, and the first end 20c and the second end 20d are bonded to each other to form the body 10. The first end 20c and the second end 20d are bonded, for example, by heating while applying pressure to the first end 20c and the second end 20d in a state where they are overlapped.
[0028] Fig. 7 is a partial enlarged view of Fig. 3 in the vicinity of the first end 20c and the second end 20d. As shown in Fig. 7, the side surface of the paper base material 21 at the first end 20c and the side surface of the paper base material 21 at the second end 20d are covered with a resin layer 27. The resin layer 27 is formed by melt-mixing the resin material constituting the first surface resin layer 22 and the resin material constituting the second surface resin layer 23.
[0029] The body portion 10 has an opening 10a at one end in the longitudinal direction of the body portion 10. The other end in the longitudinal direction of the body portion 10 is closed.
[0030] The spout 30 is attached to one end of the body 10 in the longitudinal direction so as to close the opening 10a. The spout 30 is attached by welding. The material constituting the spout 30 is a resin material. The spout 30 is preferably formed by injection molding. That is, it is preferable that the MFR (Melt Flow Rate) of the resin material constituting the spout 30 is 0.5 g / 10 min or more and the maximum thickness of the spout 30 is 2.0 mm or less. If this condition is not satisfied, it is difficult to form the spout 30 by injection molding. The MFR of the resin material constituting the spout 30 is measured according to the test method defined in the JIS standard (JIS K 7210:2014).
[0031] The MFR of the resin material constituting the spout 30 may be, for example, 40 g / 10 min or less. The maximum thickness of the spout 30 may be 1.5 mm or less. The minimum thickness of the spout 30 is, for example, 0.2 mm or more.
[0032] The spout 30 has a protruding portion 31. A thread groove (not shown) is formed on the outer peripheral surface of the protruding portion 31. The thread groove of the protruding portion 31 is screwed into a thread groove (not shown) formed in the cap 40, whereby the cap 40 is detachably attached to the spout 30. An opening 31a is formed in the protruding portion 31. The opening 31a communicates with the inside of the body 10. Therefore, by compressing the body 10, the contents filled inside the body 10 are discharged from the opening 31a.
[0033] Fig. 8 is a partial enlarged view of Fig. 4 in the vicinity of the opening 10a. As shown in Fig. 8, the spout 30 is welded to the body 10 by the resin layer 28. The resin layer 28 is formed from the same resin material as that of the spout 30. The resin material of the resin layer 28 may be melt-mixed with the resin material of the first outer resin layer 22 and / or the resin material of the second outer resin layer 23. The resin layer 28 covers the side surface of the paper base material 21 at the opening 10a.
[0034] <Modification> Fig. 9 is a cross-sectional view of a sheet member 20 according to a modified example. As shown in Fig. 9, the paper base material 21 may have a single-layer paper 21b in addition to the single-layer paper 21a. The single-layer paper 21b may be a single-layer paper similar to the single-layer paper 21a, or may be a single-layer paper different from the single-layer paper 21a. The single-layer paper 21a and the single-layer paper 21b are overlapped in the thickness direction of the paper base material 21.
[0035] The paper base material 21 may further include a resin layer 21c. The resin layer 21c is sandwiched between the single layer paper 21a and the single layer paper 21b to bond the single layer paper 21a and the single layer paper 21b. The resin layer 21c is impregnated into the surface of the single layer paper 21a (the surface of the single layer paper 21a facing the single layer paper 21b) and into the surface of the single layer paper 21b (the surface of the single layer paper 21b facing the single layer paper 21a). The resin layer 21c is preferably impregnated to a depth of 3 μm or more from the surface of the single layer paper 21a (single layer paper 21b), and more preferably to a depth of 5 μm or more from the surface of the single layer paper 21a (single layer paper 21b).
[0036] The melting point of the resin material constituting the resin layer 21c is, for example, 300° C. or less. The melting point of the resin material constituting the resin layer 21c may be 200° C. or less. Specific examples of the resin material constituting the resin layer 21c include olefins and esters. The thickness of the sheet member 20 is defined as thickness T. The distance between the center in the thickness direction of the sheet member 20 (see the front line in FIG. 9) and the resin layer 21c is defined as distance DIS. It is preferable that the distance DIS is 10 percent or less of the thickness T.
[0037] (Effects of Paper Laminated Tube 100) The effects of the paper laminate tube 100 will be described below.
[0038] Since paper is hydrogen-bonded in the planar direction (the direction perpendicular to the thickness direction of the paper), the bonding strength in the planar direction is strong. On the other hand, since paper is bonded in the thickness direction by pulp entanglement and intermolecular forces due to additives (e.g., sizing agents, paper strength improvers, etc.), the bonding strength in the thickness direction is weaker than the bonding strength in the planar direction. Therefore, when the paper base material 21 is composed of multi-layer paper, the paper base material 21 is likely to coagulate and peel when moisture penetrates into the paper base material 21.
[0039] On the other hand, in the paper laminate tube 100, the paper base material 21 is made of single-layer paper 21a. In the single-layer paper 21a, the binding force in the thickness direction is increased due to the entanglement of fibers contained in the single-layer paper 21a. Therefore, in the paper laminate tube 100 in which the paper base material 21 is made of single-layer paper 21a, it is possible to suppress the occurrence of coagulation peeling when moisture penetrates into the paper base material 21, compared to when the paper base material 21 is made of multi-layer paper. The paper laminate tube is repeatedly squeezed to squeeze out the contents. During this, peeling occurs between the layers of the paper base material, and the function (rigidity, etc.) of the paper laminate tube is deteriorated. In the paper laminate tube 100, since the paper base material 21 is made of single-layer paper 21a, peeling between the layers of the paper base material 21 is unlikely to occur, and even if the above-mentioned operation is repeatedly performed, the function of the paper laminate tube 100 is unlikely to deteriorate.
[0040] The higher the content of long fibers in the single layer paper 21a, the more likely it is that fibers will become entangled. Therefore, when the content of the first fibers in the single layer paper 21a is 50 percent or more, the binding strength in the thickness direction of the single layer paper 21a is further increased, and the occurrence of cohesive peeling when moisture penetrates into the paper base material 21 is further suppressed. Also, since the greater the basis weight of the paper, the more likely it is that cohesive peeling will occur, the single layer paper 21a has a basis weight of 165 g / m 2 By setting the thickness to less than 100 μm, the occurrence of cohesion and peeling when moisture penetrates into the paper base material 21 can be further suppressed.
[0041] In order to improve the paper yield of the body 10 (the ratio of the mass of paper to the mass of the body 10), it is necessary to increase the thickness of the single-ply paper 21a. However, as the thickness increases, even the single-ply paper 21a is more likely to experience cohesive peeling. Therefore, by ensuring the thickness of the paper base material 21 by overlapping the single-ply paper 21a and the single-ply paper 21b, it is possible to increase the paper yield of the body 10 while suppressing the occurrence of cohesive peeling when moisture penetrates into the paper base material 21.
[0042] When resin layer 21c is sandwiched between single layer paper 21a and single layer paper 21b and resin layer 21c is impregnated into the surface of single layer paper 21a and the surface of single layer paper 21b, adhesion between single layer paper 21a and single layer paper 21b is improved by resin layer 21c. In particular, when the melting point of the resin material constituting resin layer 21c is 300°C or lower, resin layer 21c is more likely to impregnate the surface of single layer paper 21a and the surface of single layer paper 21b, so adhesion between single layer paper 21a and single layer paper 21b is further improved.
[0043] Because sheet member 20 is bent to form body 10, bending stress acts between each layer that forms sheet member 20. When distance DIS is 10 percent or less of thickness T, the distance from the neutral axis of bent sheet member 20 to the boundary between single layer paper 21a and single layer paper 21b becomes small, so that the bending stress is less likely to act on the boundary. Therefore, in this case, it is possible to suppress peeling between single layer paper 21a and single layer paper 21b.
[0044] When thickness T1 is greater than thickness T2, the side of the paper base material 21 at the first end 20c and the side of the paper base material 21 at the second end 20d are more likely to be covered by the resin layer 27. When the side of the paper base material 21 at the first end 20c and the side of the paper base material 21 at the second end 20d are covered by the resin layer 27, moisture is less likely to penetrate into the paper base material 21 from the side, and the occurrence of cohesion and peeling due to moisture penetrating into the paper base material 21 is further suppressed.
[0045] The larger the MFR of the resin material constituting the spout 30, the higher the fluidity of the resin material when melted, and the easier it is for the resin layer 28 to cover the side surface of the paper base material 21 at the opening 10a. When the side surface of the paper base material 21 at the opening 10a is covered by the resin layer 28, moisture is less likely to penetrate into the interior of the paper base material 21 from the side surface, and the occurrence of cohesion and peeling due to moisture penetrating into the interior of the paper base material 21 is further suppressed. When the maximum thickness of the resin material constituting the spout 30 is reduced, the mass of the resin material used in the spout 30 is reduced, and it is possible to increase the paper conversion rate of the paper laminate tube 100 (the proportion of the mass of the paper base material 21 in the mass of the paper laminate tube 100).
[0046] Although the embodiment of the present disclosure has been described above, the above-mentioned embodiment can be modified in various ways. The scope of the present invention is not limited to the above-mentioned embodiment. The scope of the present invention is defined by the claims, and is intended to include all modifications within the meaning and scope equivalent to the claims. [Explanation of symbols]
[0047] 10 body portion, 10a opening, 20 sheet member, 20a first surface, 20b second surface, 20c first end portion, 20d second end portion, 21 paper base material, 21a, 21b single layer paper, 21c resin layer, 22 first surface resin layer, 23 second surface resin layer, 24 barrier layer, 25 first adhesive layer, 26 second adhesive layer, 27, 28 resin layer, 30 spout, 31 protrusion portion, 31a opening portion, 40 cap, 100 paper laminate tube, DIS distance, DR1 first direction, DR2 second direction, T, T1, T2 thickness.
Claims
1. A torso is provided. the body portion is made of a sheet member having a first surface and a second surface opposite to the first surface, the sheet member being bent into a cylindrical shape so that the first surface faces inward, The sheet member has a paper base material, The paper substrate comprises a first monolayer paper.
2. The first monoply paper includes a plurality of first fibers and a plurality of second fibers, a length of each of the plurality of first fibers is longer than a length of each of the plurality of second fibers and is 4 mm or less; The length of each of the plurality of second fibers is equal to or greater than 0.2 mm and equal to or less than 1.5 mm, The paper laminate tube according to claim 1 , wherein the content of the first fiber in the first single layer paper is 50 percent or more.
3. The basis weight of the first single layer paper is 165 g / m 2 The paper laminate tube of claim 1 , wherein the thickness of the tube is less than 1 mm.
4. The paper laminate tube according to claim 1 , wherein the paper substrate further comprises a second monolayer paper layered on the first monolayer paper.
5. The paper base material further includes a resin layer sandwiched between the first monolayer paper and the second monolayer paper, The paper laminate tube according to claim 4 , wherein the resin layer is impregnated into the surface of the first monolayer paper and into the surface of the second monolayer paper.
6. The paper laminate tube according to claim 5 , wherein the resin layer is made of a resin material having a melting point of 300° C. or less.
7. 6. The paper laminate tube according to claim 5, wherein the distance between the center of the sheet member in the thickness direction and the resin layer is 10 percent or less of the thickness of the sheet member.
8. the sheet member has, in an unbent state, a first end and a second end which are both ends in a second direction perpendicular to a first direction corresponding to a longitudinal direction of the body portion, the sheet member is bent into a cylindrical shape, and the first surface at the first end and the second surface at the second end are bonded to each other; the sheet member has a first surface resin layer on the first surface and a second surface resin layer on the second surface; The paper laminate tube according to claim 1 , wherein the first surface resin layer has a thickness equal to or greater than a thickness of the second surface resin layer.
9. A spout having an opening communicating with the interior of the body is further provided, 9. The paper laminated tube according to claim 1, wherein the spout is made of a resin material having an MFR of 0.5 g / 10 min or more, has a maximum thickness of 2.0 mm or less, and is welded to one end of the body in the longitudinal direction.
Citation Information
Patent Citations
Tube container
JP2021104851A