Method for manufacturing laminated molded article and adhesive sheet used therefor
The adhesive sheet with a stretchable film and smaller base material addresses the issue of excessive decorative film use in textured molded products, reducing waste and costs by enabling efficient separation and lamination.
Patent Information
- Application Number
- JP2023053235
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-29
- Publication Date
- 2024-10-10
AI Technical Summary
Existing methods for decorating textured molded products, such as mobile phone covers, require excessive use of decorative films due to trimming processes, leading to waste and increased costs.
A method involving an adhesive sheet with a stretchable film and a base material of smaller surface area than the film, which is laminated onto the textured molded product and then separated, minimizing the use of base material.
The method reduces unnecessary use of base material by allowing the film to be separated from the base material, thereby minimizing waste and lowering production costs.
Smart Images

Figure 2024141526000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for producing a laminated molded product and an adhesive sheet used in said method. [Background technology]
[0002] For example, surface decoration methods for uneven molded products such as cell phone covers have been attracting attention in recent years for the purpose of increasing the added value of molded products and giving them a luxurious feel. Since the surfaces of molded products often have complex three-dimensional shapes, one such surface decoration method is to apply a pattern to the molded product and then apply a protective coating to this pattern layer. However, this method requires labor and time in the work process, which increases costs.
[0003] For this reason, a method of directly adhering a decorative film to a concave-convex molded product is desired as a method of decorating the surface with fewer work steps and at low cost. For example, Patent Document 1 discloses such a method for manufacturing a laminated molded product, which includes a lamination step of laminating a decorative film onto the surface of a concave-convex molded product by vacuum forming (TOM forming). [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2015-196288 A Summary of the Invention [Problem to be solved by the invention]
[0005] In the above manufacturing method, after the decorative film is laminated on the surface of the uneven molded product, a trimming process is performed in which excess decorative film protruding from the uneven molded product is cut off using a cutting means. As a result, a relatively expensive decorative film (corresponding to the substrate) is used more than necessary, resulting in waste.
[0006] The present invention has been made to solve the above problems, and has an object to provide a method for producing a laminated molded product that can suppress the use of more substrate than necessary. Another object of the present invention is to provide an adhesive sheet that can be suitably used in the method for producing the laminated molded product. [Means for solving the problem]
[0007] The manufacturing method of the laminated molded product of the present invention, which achieves the above-mentioned object, includes a lamination step of laminating an adhesive sheet formed by adhering a substrate having a smaller surface area than a stretchable film to the surface of an uneven molded product, and a separation step of separating the film from the substrate.
[0008] Further, an adhesive sheet according to the present invention that achieves the above-mentioned other object has the following configuration.
[0009] (2) A stretchable film; a substrate that is adhered to the film and has a smaller surface area than the film.
[0010] (3) an adhesive layer is formed on the entire surface of the substrate on which the film is provided; The adhesive sheet according to (2), wherein the film has an opening through which a portion of the adhesive layer is exposed.
[0011] (4) The adhesive sheet according to (2), in which an adhesive layer is formed over the entire surface of the film on which the substrate is provided.
[0012] (5) an adhesive layer is formed on the entire surface of the substrate opposite to the surface on which the film is provided; the film has an opening through which a portion of the substrate is exposed, The adhesive sheet according to (2), wherein the substrate and the film are adhered with a double-sided tape.
[0013] (6) The adhesive sheet according to any one of (2) to (5), wherein the film is formed from at least one material selected from the group consisting of polyethylene, unstretched polypropylene, acrylic resin, polyvinyl chloride resin, polyvinylidene fluoride, and polyurethane resin. Effect of the Invention
[0014] According to the above-mentioned method for manufacturing a laminated molded product, an adhesive sheet having a stretchable film and a substrate with a smaller surface area than the film is laminated onto the surface of a concave-convex molded product, and then the film is separated from the substrate, thereby preventing the substrate from being used more than necessary. [Brief description of the drawings]
[0015] [Figure 1] 1 is a plan view showing an adhesive sheet according to a first embodiment of the present invention. [Diagram 2] 1 is a cross-sectional view showing an adhesive sheet according to a first embodiment of the present invention. [Figure 3A] FIG. 2 is a schematic diagram illustrating a lamination step in a method for producing a laminated molded product using the adhesive sheet according to the first embodiment of the present invention. [Figure 3B] FIG. 2 is a schematic diagram illustrating a lamination step in a method for producing a laminated molded product using the adhesive sheet according to the first embodiment of the present invention. [Figure 3C] FIG. 2 is a schematic diagram illustrating a lamination step in a method for producing a laminated molded product using the adhesive sheet according to the first embodiment of the present invention. [Figure 3D] FIG. 2 is a schematic diagram illustrating a lamination step in a method for producing a laminated molded product using the adhesive sheet according to the first embodiment of the present invention. [Figure 3E] FIG. 2 is a schematic diagram illustrating a lamination step in a method for producing a laminated molded product using the adhesive sheet according to the first embodiment of the present invention. [Figure 3F] FIG. 2 is a schematic diagram illustrating a separation step in the method for producing a laminated molded product using the adhesive sheet according to the first embodiment of the present invention. [Figure 4]FIG. 4 is a plan view showing an adhesive sheet according to a second embodiment of the present invention. [Diagram 5] FIG. 4 is a cross-sectional view showing an adhesive sheet according to a second embodiment of the present invention. [Figure 6A] FIG. 6 is a schematic diagram illustrating a lamination step in a method for producing a laminated molded product using an adhesive sheet according to a second embodiment of the present invention. [Figure 6B] FIG. 6 is a schematic diagram illustrating a lamination step in a method for producing a laminated molded product using an adhesive sheet according to a second embodiment of the present invention. [Figure 6C] FIG. 6 is a schematic diagram illustrating a lamination step in a method for producing a laminated molded product using an adhesive sheet according to a second embodiment of the present invention. [Figure 6D] FIG. 6 is a schematic diagram illustrating a lamination step in a method for producing a laminated molded product using an adhesive sheet according to a second embodiment of the present invention. [Figure 6E] FIG. 6 is a schematic diagram illustrating a lamination step in a method for producing a laminated molded product using an adhesive sheet according to a second embodiment of the present invention. [Figure 6F] FIG. 6 is a schematic diagram illustrating a separation step in a method for producing a laminate molded product using an adhesive sheet according to a second embodiment of the present invention. [Figure 7] FIG. 4 is a plan view showing an adhesive sheet according to a third embodiment of the present invention. [Figure 8] FIG. 4 is a cross-sectional view showing an adhesive sheet according to a third embodiment of the present invention. [Figure 9A] FIG. 11 is a schematic diagram illustrating a lamination step in a method for producing a laminated molded product using an adhesive sheet according to a third embodiment of the present invention. [Figure 9B] FIG. 11 is a schematic diagram illustrating a lamination step in a method for producing a laminated molded product using an adhesive sheet according to a third embodiment of the present invention. [Figure 9C] FIG. 11 is a schematic diagram illustrating a lamination step in a method for producing a laminated molded product using an adhesive sheet according to a third embodiment of the present invention. [Figure 9D] FIG. 11 is a schematic diagram illustrating a lamination step in a method for producing a laminated molded product using an adhesive sheet according to a third embodiment of the present invention. [Figure 9E]FIG. 11 is a schematic diagram illustrating a lamination step in a method for producing a laminated molded product using an adhesive sheet according to a third embodiment of the present invention. [Figure 9F] FIG. 11 is a schematic diagram illustrating a separation step in a method for producing a laminated molded product using an adhesive sheet according to a third embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0016] First Embodiment Hereinafter, a first embodiment of the present invention will be described with reference to the attached drawings. In the description of the drawings, the same elements are given the same reference numerals, and duplicated descriptions will be omitted. In addition, the dimensional ratios in the drawings are exaggerated for the convenience of explanation, and may differ from the actual ratios.
[0017] An adhesive sheet 1 according to a first embodiment will be described below with reference to Figures 1 and 2. Figure 1 is a plan view showing an adhesive sheet 1 according to a first embodiment of the present invention. Figure 2 is a cross-sectional view showing an adhesive sheet 1 according to a first embodiment of the present invention.
[0018] The adhesive sheet 1 according to the first embodiment, as shown in Figures 1 and 2, comprises, from the bottom, a stretchable film 10, an adhesive layer 20, and a substrate 30. The adhesive layer 20 is formed on the entire surface of the substrate 30 on which the film 10 is provided. Furthermore, as shown in Figure 2, the film 10 has an opening 11 through which a part of the adhesive layer 20 is exposed. Each component will be described in detail below.
[0019] <Film 10> As described below, the film 10 stretches together with the substrate 30 when the adhesive sheet 1 is laminated onto the concave-convex molded article 50.
[0020] The material constituting the film 10 is not particularly limited as long as it can be stretched together with the substrate 30 when the adhesive sheet 1 is laminated on the concave-convex molded product 50, but it is preferable that it can be stretched by 50 to 300%. Specifically, the film 10 may be made of polyolefins such as polyethylene, unstretched polypropylene, polybutene, and polybutadiene, acrylic resins, vinyl chloride resins, polyurethane resins, unstretched polyesters such as unstretched polyethylene terephthalate (PET), unstretched polybutylene terephthalate, and unstretched polyethylene naphthalate. Among these, polyethylene, unstretched polypropylene, acrylic resins, vinyl chloride resins, and polyurethane resins are preferable in consideration of stretchability (three-dimensional shape conformability), peelability, cost, productivity, and the like. In addition, from the viewpoint of ease of TOM molding, it is preferable that the film 10 is an unstretched film. Here, the above-mentioned materials may be used alone or in the form of a mixture of two or more kinds. In addition, the film 10 may be used alone or by laminating different kinds of materials.
[0021] The thickness of the film 10 is not particularly limited, but is preferably 5 to 500 μm, and more preferably 50 to 300 μm, taking into consideration stretchability (ability to conform to a three-dimensional shape), peelability, cost, workability, etc. With such a thickness, TOM molding can be easily performed in the lamination step (1), and the film 10 can also fully exhibit the ability to conform to the three-dimensional shape of the uneven molded article 50 by this molding.
[0022] <Adhesive layer 20> The adhesive layer 20 is a layer that contains an adhesive (not shown). There are no particular limitations on the specific composition of the adhesive contained in the adhesive layer 20. In addition, when selecting an adhesive, it is advisable to take into consideration the material of the uneven molded product 50 that is the adherend in the TOM molding, and either an adhesive or a pressure-sensitive adhesive may be used. In the present invention, the adhesive includes a pressure-sensitive adhesive (pressure-sensitive adhesive).
[0023] Specific examples of adhesives include acrylic adhesives, silicone adhesives, rubber adhesives, vinyl ether adhesives, and hot melt adhesives. These adhesives may be either solvent-based or emulsion-based. Among these, examples of acrylic adhesives include copolymers of one or more (meth)acrylic acid esters such as n-butyl (meth)acrylate, hexyl (meth)acrylate, 2-diethylbutyl (meth)acrylate, isooctyl (meth)acrylate, 2-methoxyethyl (meth)acrylate, 2-ethylhexyl (meth)acrylate, decyl (meth)acrylate, dodecyl (meth)acrylate, and tridecyl (meth)acrylate, and a functional monomer copolymerizable with the (meth)acrylic acid esters, such as (meth)acrylic acid, itaconic acid, maleic acid, maleic anhydride, hydroxyethyl acrylate, hydroxypropyl acrylate, acrylamide, dimethylacrylamide, methylaminoethyl methacrylate, and methoxyethyl (meth)acrylate. Specific examples of silicone adhesives include those composed of a mixture and / or polymer of dimethylsiloxane gum and dimethylsiloxane resin. Specific examples of rubber adhesives include those mainly composed of synthetic rubber or natural rubber such as styrene-isoprene-styrene block copolymer rubber, styrene-butadiene rubber, polybutene rubber, and butyl rubber. Specific examples of vinyl ether adhesives include ethyl vinyl ether, propyl vinyl ether, butyl vinyl ether, and 2-ethylhexyl vinyl ether. Hot melt adhesives / pressure-sensitive adhesives are adhesives that melt once due to heat and return to their original solid state upon cooling. Specific examples of hot melt adhesives / pressure-sensitive adhesives include various types such as acrylic, rubber, urethane, ester, and polyamide adhesives, and more specifically, styrene block copolymers such as polyolefin, ethylene-vinyl acetate copolymer, styrene-butadiene-styrene block copolymer, and styrene-isoprene-styrene block copolymer.
[0024] Alternatively, a chemically reactive adhesive may be used. Here, the chemically reactive adhesive refers to an adhesive of a type in which the constituent components are polymerized and solidified by a chemical reaction, and specific examples thereof include a heat-curing adhesive that initiates a chemical reaction when heat is applied from the outside, and a light / electron beam curing adhesive that initiates a chemical reaction when irradiated with visible light, ultraviolet light, electron beams, etc. A specific example of a heat-curing adhesive is an epoxy adhesive, and a specific example of a light / electron beam curing adhesive is polyester acrylate.
[0025] The thickness of the adhesive layer 20 is not particularly limited, but is preferably 5 to 100 μm, and more preferably 15 to 50 μm. The thickness of the adhesive layer 20 is appropriately selected and set depending on the size of the irregularities on the surface (adhering surface) of the irregular molded article 50.
[0026] The adhesive layer 20 may further contain other additives that are conventionally known. Examples of such additives include tackifiers, fillers, and antioxidants. Examples of tackifiers include natural resins such as rosin resins and polyterpene resins, petroleum resins such as C5, C9, and dicyclopentadiene resins, and synthetic resins such as coumarone-indene resins and xylene resins. Examples of fillers include zinc oxide, silica, and calcium carbonate. Titanium dioxide can also function as a filler.
[0027] <Base material 30> 1 and 2, the substrate 30 is provided with a smaller surface area than the film 10. The size of the substrate 30 is such that, when the substrate 30 is laminated on the uneven molded product 50, the substrate 30 can cover the entire front surface side of the uneven molded product 50. The substrate 30 can be stretched together with the film 10.
[0028] The substrate 30 is not particularly limited, but may be, for example, a decorative film capable of decorating the uneven molded product 50. The decorative film is provided for the purpose of improving aesthetics, and is, for example, a film having a lustrous appearance (metallic appearance). There is no particular limit to the specific configuration of the decorative film, and conventionally known knowledge may be appropriately referred to. As an example, the decorative film preferably contains a colorant and a binder.
[0029] Examples of colorants include organic pigments such as quinacridones, anthraquinones, perylenes, perinones, diketopyrrolopyrroles, isoindolinones, condensed azos, benzimidazolones, monoazos, insoluble azos, naphthols, flavanthrones, anthrapyrimidines, quinophthalones, pyranthrones, pyrazolones, thioindigos, anthanthrones, dioxazines, phthalocyanines, and indanthrones; metal complexes such as nickel dioxin yellow and copper azomethine yellow; metal oxides such as titanium oxide, iron oxide, and zinc oxide; metal salts such as barium sulfate and calcium carbonate; color pigments such as carbon black; and luster pigments.
[0030] The glittering pigment is not particularly limited, and conventionally known knowledge may be appropriately referred to. The glittering pigment may be, for example, one or more selected from the group consisting of aluminum materials, pearl pigments, and glass materials. Specific examples of the aluminum material include aluminum powder, aluminum paste, and aluminum flakes. Aluminum powder is a metallic pigment that does not contain a solvent component, and includes materials in which aluminum particles are coated with a resin such as an acrylic resin. Aluminum paste is a material in which scaly fine particles of aluminum are surface-treated and made into a paste with an organic solvent or the like. Furthermore, an example of the aluminum flake is a material in which an aluminum vapor deposition film is made into a pigment. An example of the pearl pigment is white pearl, which is made by pulverizing mica and applying a surface treatment. An example of the glass material is scaly glass flakes, or glittering pigment-type materials in which the flakes are further coated with metal or metal oxide.
[0031] The average particle diameter of the luster pigment is not particularly limited, but is preferably 5 to 30 μm, and more preferably 10 to 25 μm. The average particle diameter of the luster pigment having a scaly shape like the aluminum particles in the aluminum paste means the average particle diameter of the larger surface of the particle, and the D50 value (50% cumulative weight particle diameter) of the particle diameter measured by a light scattering method using a particle size distribution measuring device is adopted as the "average particle diameter".
[0032] The photoluminescent film containing the photoluminescent pigment preferably contains a binder. Examples of binders that can be used include acrylic resins, vinyl chloride resins, polyolefin resins, polyester resins, alkyd resins, epoxy resins, and polyurethane resins, and transparent resins are more preferable. These binders can also be used in combination with crosslinking agents such as amino resins, methylolated melamine resins, alkyl etherified melamine resins, urea resins, and polyisocyanate compounds.
[0033] In addition, the substrate 30 is not limited to a decorative film containing a colorant and a binder, but may be in any form, such as a supporting substrate alone, a supporting substrate having a decorative layer on its surface, or a supporting substrate having a decorative film formed on it.
[0034] In the latter case, the supporting substrate is preferably a resin film. Here, as the resin film, for example, a film made of a resin such as polyolefins such as polyethylene and polypropylene, polyesters such as polyethylene terephthalate and polybutylene terephthalate, polyvinyl chloride, polystyrene, polyurethane, polycarbonate, polyamide, polyimide, polymethyl methacrylate, polybutene, polybutadiene, polymethylpentene, ethylene vinyl acetate copolymer, ethylene (meth)acrylic acid copolymer, ethylene (meth)acrylic acid ester copolymer, ABS resin, ionomer resin, foamed film, or a laminated film thereof can be used. The resin film may be a commercially available one, or may be formed by a cast film forming method using a process material. Among these, a film made of polyvinyl chloride is preferred from the viewpoint of excellent curved surface conformability. In addition, when the decorative layer described later is formed by printing, a film made of polyvinyl chloride is also preferred from the viewpoint of excellent ink fixation. In addition, when the supporting substrate is made of a resin film, the supporting substrate may be opaque or transparent. In addition, the supporting substrate may have a through hole as necessary. In addition, in the case where the decorative film is formed on the supporting substrate, it is preferable that the supporting substrate is transparent since the design of the decorative film is easily visible from the outside. In addition, in the case where the decorative film is formed on the supporting substrate, it is preferable that the supporting substrate is the surface side (attached to the adherend) of the decorative film since the supporting substrate plays a role of surface protection.
[0035] The thickness of the supporting substrate is also not particularly limited, but is preferably about 1 to 500 μm, more preferably about 25 to 200 μm, but can be appropriately changed depending on the desired application.
[0036] The decorative layer formed on the surface of the supporting substrate is provided on the front side of the supporting substrate when the supporting substrate is opaque, but when the supporting substrate is transparent, the decorative layer may be provided on either side (front side, back side) or on both sides of the supporting substrate.
[0037] The decorative layer is not particularly limited, and may be one color or may display a color-coded pattern of two or more colors. The pattern may be a predetermined pattern, a photograph, or characters. The method of forming the decorative layer is not particularly limited, and the decorative layer can be formed by, for example, printing, printing, coating of paint, transfer from a transfer sheet, deposition, sputtering, or other methods. The supporting substrate may have an undercoat layer such as an easy-adhesion coat or a gloss adjustment coat for forming the decorative layer, or a topcoat layer such as a hard coat, an anti-stain coat, or a coat for adjusting surface roughness and specular gloss. The decorative layer, undercoat layer, or topcoat layer may be formed on the entire surface of the supporting substrate, or may be formed partially.
[0038] <Forming equipment 100> Next, the configuration of a molding apparatus 100 for TOM molding will be described with reference to Fig. 3A. Here, TOM molding refers to vacuum and pressure molding.
[0039] "Vacuum forming" refers to a method of softening the adhesive sheet 1 by heating or the like, placing it on the uneven molded product 50, and forming the adhesive sheet 1 by adhering it to the uneven molded product 50 by creating a vacuum in the space between the adhesive sheet 1 and the uneven molded product 50. Examples of vacuum forming include, but are not limited to, the straight method, the drape method, the plug assist method, the air slip method, the snap back method, the reverse draw method, the plug assist reverse draw method, and the air cushion method.
[0040] "Compressed air molding" refers to a method of softening the adhesive sheet 1 by heating or the like, placing it on the concave-convex molded product 50, and flowing gas from the adhesive sheet 1 side toward the concave-convex molded product to pressurize the space above the adhesive sheet 1 (between the adhesive sheet 1 and the side where the concave-convex molded product 50 is not present), thereby pressing and molding the adhesive sheet 1 onto the concave-convex molded product 50. Note that molding may be performed by combining vacuum molding and compressed air molding.
[0041] In this way, TOM molding involves heating and softening the adhesive sheet 1 onto the surface of the desired uneven molded product 50 while spreading it, and then reducing the pressure in the space on the side where the adhesive sheet 1 is to be attached (vacuum molding) and pressurizing the space on the opposite side (compressed air molding), making it possible to attach and laminate the adhesive sheet 1 while molding it to the three-dimensional shape of the surface of the uneven molded product 50.
[0042] As shown in FIG. 3A, the molding apparatus 100 has a lower mold 101, an upper mold 102 arranged so as to be able to move toward and away from the lower mold 101, a table 103 provided inside the lower mold 101, a heating means 104 provided inside the upper mold 102, a pressure means 105 provided inside the upper mold 102, and a vacuum means 106.
[0043] The concave-convex molded product 50 is placed on the table 103. The table 103 is placed within the lower mold 101 so as to be movable vertically.
[0044] The heating means 104 heats the adhesive sheet 1 to soften it, making it easier for the adhesive sheet 1 to conform to the shape of the concave-convex molded article 50 .
[0045] The pressure applying means 105 is disposed below the heating means 104. The pressure applying means 105 applies a pressure inside the upper die 102 greater than the pressure inside the lower die 101, thereby attaching the adhesive sheet 1 to the concave-convex molded product 50.
[0046] The vacuum means 106 creates a vacuum inside the molding apparatus 100. The vacuum means 106 has a vacuum means 106 for creating a vacuum inside the lower mold 101, and a vacuum means 106 for creating a vacuum inside the upper mold 102.
[0047] <Manufacturing method for laminated molded products> Next, a method for producing a laminated molded product using the adhesive sheet 1 according to the first embodiment will be described with reference to Fig. 3A to Fig. 3F. Fig. 3A to Fig. 3E are diagrams for explaining the lamination step of the method for producing a laminated molded product, and Fig. 3F is a diagram for explaining the separation step of the method for producing a laminated molded product. Note that the adhesive layer 20 is omitted in Fig. 3A to Fig. 3F.
[0048] The method for producing a laminate molded product using the adhesive sheet 1 according to the first embodiment of the present invention includes a lamination step of laminating the adhesive sheet 1 onto the concave-convex molded product 50 and a separation step of separating the film 10 from the substrate 30.
[0049] According to the method of this embodiment, the adhesive sheet 1 can be adhered to the entire surface of the concave-convex molded product 50 by conforming to the three-dimensional shape of the intended concave-convex molded product 50. Furthermore, since the method of the present invention is excellent in conformity to the three-dimensional shape of the intended concave-convex molded product 50, it is possible to laminate (attach) the adhesive sheet 1 to a fine structure in close correspondence with the shape of the concave-convex molded product 50 without causing localized ductility in the adhesive sheet 1. Furthermore, in the TOM molding according to the present invention, the lamination (attachment) step is performed under reduced or increased pressure and in a short time, so that the inclusion of air bubbles during lamination (attachment) can be suppressed and prevented.
[0050] In summary, in the lamination step, the adhesive sheet 1 is laminated onto the surface of the concave-convex molded article 50 by TOM molding so that the adhesive layer 20 is disposed on the concave-convex molded article 50 side.
[0051] In the lamination step, first, as shown in Fig. 3A, the adhesive sheet 1 is placed between the lower die 101 and the upper die 102 of the molding device 100, and the concave-convex molded product 50 is placed on the table 103. At this time, as shown in Fig. 3A, the adhesive sheet 1 is placed so that, from the top, it is the substrate 30, the adhesive layer 20, and the film 10. In addition, the adhesive layer 20 is placed so that the bottom surface thereof is exposed through an opening 11 formed in the film 10 (see Fig. 2).
[0052] Next, as shown in FIG. 3B, lower mold 101 and upper mold 102 are brought close to each other, and adhesive sheet 1 is sandwiched between lower mold 101 and upper mold 102.
[0053] Next, as shown in FIG. 3C, the table 103 is moved upward, and the inside of the molding device 100 is evacuated by the vacuum means 106. Then, the adhesive sheet 1 is heated and softened by the heating means 104, and air or an inert gas (nitrogen gas, argon gas, helium gas, etc.) is introduced into the upper mold 102 by the pressurizing means 105 to pressurize the space in the upper mold 102, and a pressure difference is generated between the space in the upper mold 102 and the space in the lower mold 101. Here, the heating conditions are not particularly limited as long as they are conditions that can soften the adhesive sheet 1 to an extent that it can sufficiently follow the shape of the uneven molded product 50 during TOM molding, and are appropriately selected depending on the materials of the film 10, the adhesive layer 20, the substrate 30, etc. Specifically, the heating temperature is preferably 50 to 200° C., and more preferably 70 to 150° C. The heating time is preferably 0.1 to 10 minutes, and more preferably 1 to 5 minutes.
[0054] As a result, as shown in FIG. 3D, the pressure difference generated between the space in the upper die 102 and the space in the lower die 101 causes the adhesive sheet 1 to be laminated (attached) along the shape of the concave-convex molded product 50.
[0055] Next, as shown in FIG. 3E, the introduction of air or inert gas into upper mold 102 is stopped, and upper mold 102 is separated from lower mold 101.
[0056] 3F, the film 10 is separated from the substrate 30. Specifically, the concave-convex molded product 50 on which the adhesive sheet 1 is laminated is removed from the molding device 100, and then the excess substrate 30 protruding from the concave-convex molded product 50 is cut off using an appropriate cutting means such as a thermocutter or a cutter, to obtain a laminated molded product in which the substrate 30 is adhered onto the concave-convex molded product 50.
[0057] As described above, the manufacturing method of the laminated molded product according to the first embodiment includes a lamination step of laminating an adhesive sheet 1 formed by adhering a base material 30 having a smaller surface area than the film 10 to a stretchable film 10, onto the surface of a concave-convex molded product 50, and a separation step of separating the film 10 from the base material 30. According to this manufacturing method, the adhesive sheet 1 having the stretchable film 10 and the base material 30 having a smaller surface area than the film 10 is laminated onto the surface of the concave-convex molded product 50 by TOM molding, and then the film 10 is separated from the base material 30, so that it is possible to prevent the use of more base material 30 than necessary.
[0058] As described above, the adhesive sheet 1 according to the present embodiment has the stretchable film 10 and the substrate 30 that is adhered to the film 10 and has a smaller surface area than the film 10. With the adhesive sheet 1 configured in this manner, it is possible to prevent the substrate 30 from being used more than necessary.
[0059] Additionally, adhesive layer 20 is formed over the entire surface of substrate 30 on which film 10 is provided, and film 10 has openings 11 through which part of adhesive layer 20 is exposed. According to adhesive sheet 1 configured in this manner, adhesive layer 20 is provided over the entire surface of substrate 30, so the amount of adhesive used can be reduced compared to adhesive sheet 2 according to the second embodiment described below.
[0060] <Second embodiment> Next, the configuration of an adhesive sheet 2 according to a second embodiment will be described with reference to FIGS.
[0061] Fig. 4 is a plan view showing an adhesive sheet 2 according to the second embodiment. Fig. 5 is a cross-sectional view showing an adhesive sheet 2 according to the second embodiment. Explanation of parts common to the first embodiment will be omitted, and only features unique to the second embodiment will be explained. Note that the same members as those in the above-mentioned first embodiment will be denoted by the same reference numerals and repeated explanations will be omitted.
[0062] As shown in FIGS. 4 and 5, adhesive sheet 2 according to the second embodiment has, from the bottom, substrate 130, adhesive layer 120, and stretchable film 110.
[0063] The substrate 130 is configured to have a smaller surface area than the film 110. The adhesive layer 120 is provided on the entire surface of the film 110 facing the substrate 130, as shown in FIG.
[0064] The materials constituting the film 110, the adhesive layer 120, and the base material 130, their thicknesses, etc. are the same as those of the adhesive sheet 1 according to the above-described first embodiment, and therefore a description thereof will be omitted.
[0065] <Manufacturing method for laminated molded products> Next, a method for producing a laminated molded product using an adhesive sheet 2 according to the second embodiment will be described with reference to Fig. 6A to Fig. 6F. Fig. 6A to Fig. 6E are diagrams for explaining the lamination step of the method for producing a laminated molded product, and Fig. 6F is a diagram for explaining the separation step of the method for producing a laminated molded product. Note that the adhesive layer 120 is omitted in Fig. 6A to Fig. 6F.
[0066] The method for producing a laminate molded product using the adhesive sheet 2 according to the second embodiment of the present invention includes a lamination step of laminating the adhesive sheet 2 onto the concave-convex molded product 50, and a separation step of separating the film 110 from the substrate 130.
[0067] In the lamination step, first, as shown in FIG. 6A, an adhesive sheet 2 is placed between a lower die 101 and an upper die 102 of a molding device 100, and a concave-convex molded product 50 is placed on a table 103. At this time, as shown in FIG. 6A, the adhesive sheet 2 is placed in the order of film 110, adhesive layer 120, and substrate 130 from the top. The substrate 130 is adhered to the film 110 by the adhesive layer 120. The lower surface of the adhesive layer 120 is exposed in a portion where the substrate 130 is not provided. An adhesive layer (not shown) for adhering to the concave-convex molded product 50 is formed on the lower side of the substrate 130. The substrate 130 is adhered to the concave-convex molded product 50 via this adhesive layer.
[0068] Next, as shown in FIG. 6B, lower mold 101 and upper mold 102 are brought close to each other, and adhesive sheet 2 is sandwiched between lower mold 101 and upper mold 102.
[0069] Next, as shown in FIG. 6C, table 103 is moved upward, adhesive sheet 2 is heated and softened by heating means 104, and air or an inert gas is introduced into upper mold 102 by pressure applying means 105 to pressurize the space within upper mold 102, thereby generating a pressure difference between the space within upper mold 102 and the space within lower mold 101.
[0070] As a result, as shown in FIG. 6D, the adhesive sheet 2 is laminated (attached) along the shape of the concave-convex molded product 50 due to the pressure difference generated between the space in the upper mold 102 and the space in the lower mold 101.
[0071] Next, as shown in FIG. 6E, the introduction of air or inert gas into upper mold 102 is stopped, and upper mold 102 is separated from lower mold 101.
[0072] 6F, the film 110 is separated from the substrate 130. Specifically, the film 110 is peeled off from the substrate 130 to obtain a laminated molded product in which the substrate 130 is bonded onto the concave-convex molded product 50.
[0073] As described above, in the adhesive sheet 2 according to the second embodiment, the adhesive layer 120 is formed on the entire surface of the film 110 on which the base material 130 is provided. With the adhesive sheet 2 configured in this manner, as described above, the film 110 can be peeled off from the base material 130 to obtain a laminated molded product, which eliminates the need for the cutting means described in the adhesive sheet 1 according to the first embodiment and allows a laminated molded product to be easily obtained.
[0074] <Third embodiment> Next, the configuration of an adhesive sheet 3 according to a third embodiment will be described with reference to FIGS.
[0075] Fig. 7 is a plan view showing an adhesive sheet 3 according to a third embodiment. Fig. 8 is a cross-sectional view showing an adhesive sheet 3 according to a third embodiment. Explanation of parts common to the first embodiment will be omitted, and only features unique to the third embodiment will be explained. Note that the same members as those in the above-mentioned first embodiment will be denoted by the same reference numerals and repeated explanations will be omitted.
[0076] As shown in FIGS. 7 and 8, adhesive sheet 3 according to the third embodiment has adhesive layer 220, substrate 230, double-sided tape 240, and film 210, in that order from the bottom.
[0077] 7, the film 210 has an opening 211 through which a portion of the substrate 230 is exposed. The substrate 230 is configured to have a smaller surface area than the film 210. As shown in FIG. 8, the adhesive layer 220 is provided on the entire surface of the substrate 230 opposite to the side on which the film 210 is provided.
[0078] The double-sided tape 240 is provided outside the opening 211. The double-sided tape 240 is provided in a rectangular shape between the film 210 and the base material 230, and bonds the film 210 and the base material 230 together.
[0079] The materials constituting the film 210, the adhesive layer 220, and the base material 230, their thicknesses, etc. are the same as those of the adhesive sheet 1 according to the above-described first embodiment, and therefore a description thereof will be omitted.
[0080] <Manufacturing method for laminated molded products> Next, a method for producing a laminated molded product using an adhesive sheet 3 according to the third embodiment will be described with reference to Fig. 9A to Fig. 9F. Fig. 9A to Fig. 9E are diagrams for explaining the lamination step of the method for producing a laminated molded product, and Fig. 9F is a diagram for explaining the separation step of the method for producing a laminated molded product. Note that the adhesive layer 220 and the double-sided tape 240 are omitted in Fig. 9A to Fig. 9F.
[0081] The method for producing a laminate molded product using the adhesive sheet 3 according to the third embodiment of the present invention includes a lamination step of laminating the adhesive sheet 3 onto the concave-convex molded product 50, and a separation step of separating the film 210 from the substrate 230.
[0082] In the lamination step, first, as shown in Fig. 9A, an adhesive sheet 3 is placed between a lower die 101 and an upper die 102 of a molding device 100, and a concave-convex molded product 50 is placed on a table 103. At this time, the adhesive sheet 3 is placed in the order of film 210, double-sided tape 240, substrate 230, and adhesive layer 220 from the top, as shown in Fig. 9A. That is, the adhesive layer 220 located at the bottom is attached to the concave-convex molded product 50.
[0083] Next, as shown in FIG. 9B, lower mold 101 and upper mold 102 are brought close to each other, and adhesive sheet 3 is sandwiched between lower mold 101 and upper mold 102.
[0084] Next, as shown in FIG. 9C , table 103 is moved upward, adhesive sheet 3 is heated and softened by heating means 104, and air or an inert gas is introduced into upper mold 102 by pressure applying means 105 to pressurize the space within upper mold 102, thereby generating a pressure difference between the space within upper mold 102 and the space within lower mold 101.
[0085] As a result, as shown in FIG. 9D, the adhesive sheet 3 is laminated (attached) along the shape of the concave-convex molded product 50 due to the pressure difference generated between the space in the upper mold 102 and the space in the lower mold 101.
[0086] Next, as shown in FIG. 9E, the introduction of air or inert gas into upper mold 102 is stopped, and upper mold 102 is separated from lower mold 101.
[0087] 9F, the film 210 is separated from the substrate 230. Specifically, the film 210 is peeled off from the substrate 230 to obtain a laminated molded product in which the substrate 230 is bonded onto the concave-convex molded product 50.
[0088] As described above, in the adhesive sheet 3 according to the third embodiment, the adhesive layer 220 is formed on the entire surface of the substrate 230 opposite to the side on which the film 210 is provided, the film 210 has an opening 211 through which a part of the substrate 230 is exposed, and the substrate 230 and the film 210 are adhered with double-sided tape 240. According to the adhesive sheet 3 configured in this manner, as described above, the film 210 can be peeled off from the substrate 230 to obtain a laminated molded product, which eliminates the need for the cutting means described in the adhesive sheet 1 according to the first embodiment and allows a laminated molded product to be easily obtained.
[0089] Although the present invention has been described through the above embodiments, the method for producing a laminated molded product according to the present invention is not limited to the described method, and can be modified in various ways based on the scope of the claims. [Explanation of symbols]
[0090] 1, 2, 3 adhesive sheet, 10, 110, 210 film, 11, 211 opening, 20, 120, 220 adhesive layer, 30, 130, 230 base material, 240 double-sided tape.
Claims
1. a lamination step of laminating an adhesive sheet formed by adhering a substrate having a smaller surface area than a stretchable film to the surface of the uneven molded product; and a separating step of separating the film from the substrate.
2. A stretchable film; a substrate that is adhered to the film and has a smaller surface area than the film.
3. an adhesive layer is formed on the entire surface of the substrate on which the film is provided; The adhesive sheet according to claim 2 , wherein the film has an opening through which a portion of the adhesive layer is exposed.
4. The adhesive sheet according to claim 2 , wherein an adhesive layer is formed on the entire surface of the film on which the substrate is provided.
5. an adhesive layer is formed on the entire surface of the substrate opposite to the surface on which the film is provided; the film has an opening through which a portion of the substrate is exposed, The adhesive sheet according to claim 2 , wherein the substrate and the film are adhered to each other with a double-sided tape.
6. 4. The adhesive sheet according to claim 2, wherein the film is formed from at least one material selected from the group consisting of polyethylene, unoriented polypropylene, acrylic resin, polyvinyl chloride resin, polyvinylidene fluoride, and polyurethane resin.
Citation Information
Patent Citations
JP1991090998U
Decorative film pasting method
JP2005035130A
Method and apparatus for pasting up decorative film
JP2006001068A
Apparatus and method for producing laminated sheet
JP2013071346A
Decorative molded product and method of producing the same
JP2016083860A
Cited By
TOM process and device for automotive upholstery
CN120003017A