Photosensitive resin, and method for producing the same and use thereof

The integration of a specific epoxy group-containing compound into an acid anhydride-modified fluorene-containing acrylic resin addresses the curability and solvent solubility issues of existing resins, resulting in a photosensitive resin with improved stability and consistency during manufacturing.

JP2024144196APending Publication Date: 2024-10-11OSAKA GAS CHEM KK
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2024035121
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-28
Filing Date
2024-03-07
Publication Date
2024-10-11

AI Technical Summary

Technical Problem

The existing photosensitive resin, as described in Patent Document 1, faces issues with both high curability and high solvent solubility, particularly precipitating or becoming cloudy when diluted with solvents like cellosolve acetates, leading to concentration inconsistencies during manufacturing.

Method used

A photosensitive resin is developed by incorporating a specific epoxy group-containing compound into an acid anhydride-modified fluorene-containing acrylic resin, featuring a unique molecular structure represented by specific formulas, which enhances curability and solvent solubility.

Benefits of technology

The new resin achieves excellent curability and solvent solubility, preventing precipitation and clouding during equipment cleaning, ensuring consistent concentration and performance in manufacturing processes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024144196000001
    Figure 2024144196000001
  • Figure 2024144196000002
    Figure 2024144196000002
  • Figure 2024144196000003
    Figure 2024144196000003
Patent Text Reader

Abstract

To provide a photosensitive resin which is excellent in curability and solvent solubility.SOLUTION: A photosensitive resin is prepared by adding a monoepoxy compound having a specific structure to an acid anhydride-modified fluorene-containing acrylic resin having a repeating unit represented by the following formula (1).SELECTED DRAWING: None
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a photosensitive resin that can be used for photoresist applications and the like, and a method for producing the same and applications thereof. [Background technology]

[0002] Photolithography is a method of forming a desired pattern on a substrate or the like by applying a photosensitive composition containing a photopolymerizable resin such as a photoresist onto the substrate or the like, exposing the photosensitive composition through a photomask, and then developing the photosensitive composition with a developer. The photosensitive composition used in this photolithography method has properties such as high photosensitivity and good developability in order to realize a precise pattern, and the cured product is required to have properties such as heat resistance, excellent mechanical properties, high adhesion, and chemical resistance, and is also required to be transparent for optical applications. In addition, in the development process of the photolithography method, photosensitive compositions that are developed with an alkaline aqueous solution without using an organic solvent are mainstream due to environmental pollution and other reasons. As a photopolymerizable composition that can be developed with such an alkaline aqueous solution, an alkali-soluble photopolymerizable resin having a fluorene skeleton is known.

[0003] Japanese Patent No. 6175259 (Patent Document 1) discloses an acid anhydride-modified fluorene-containing acrylic resin obtained by reacting an epoxy (meth)acrylate having a bisarylfluorene skeleton with a tetracarboxylic dianhydride. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] Patent No. 6175259 Summary of the Invention [Problem to be solved by the invention]

[0005] However, the photosensitive resin of Patent Document 1 cannot achieve both high curability and high solvent solubility (low precipitation). In particular, (meth)acrylate resins tend to precipitate or become cloudy when diluted with a solvent such as cellosolve acetates. Therefore, even with the photosensitive resin of Patent Document 1, precipitation or cloudiness occurs during equipment cleaning, which is a low concentration state in the manufacturing process, and this is a problem.

[0006] Therefore, an object of the present disclosure is to provide a photosensitive resin having excellent curability and solvent solubility, as well as a production method and uses thereof. [Means for solving the problem]

[0007] As a result of intensive research to achieve the above object, the present inventors have discovered that a photosensitive resin obtained by adding a specific epoxy group-containing compound to a specific acid anhydride-modified fluorene-containing acrylic resin has excellent curability and solvent solubility, and have completed the present invention (or the present disclosure).

[0008] That is, the photosensitive resin according to embodiment [1] of the present disclosure comprises an acid anhydride-modified fluorene-containing acrylic resin having a repeating unit represented by the following formula (1) to which an epoxy group-containing compound represented by the following formula (2) is added.

[0009] [ka]

[0010] (In the formula, Ring Ar 1 and ring Ar 2 each independently represents a fused polycyclic hydrocarbon ring; A 1 and A 2 each independently represents an alkylene group; n1 and n2 each independently represent an integer of 0 or more; R 1 and R 2 each independently represents a substituent; m1 and m2 each independently represent an integer of 0 or more; R 3represents a substituent, k represents an integer of 0 to 8, Ring Ar 3 represents a hydrocarbon ring, R 4 represents a substituent, p represents an integer of 0 or more, R 5 and R 6 each independently represents a hydrogen atom or an alkyl group, (s indicates an integer of 1 or more)

[0011] [ka]

[0012] (In the formula, A 3 represents an alkylene group, t represents an integer of 0 or more, and X represents a substituent.

[0013] The embodiment [2] of the present disclosure relates to a compound represented by the formula (1) of the embodiment [1], in which the ring Ar 1 and ring Ar 2 is a naphthalene ring.

[0014] The embodiment [3] of the present disclosure relates to a compound represented by the formula (1) of the embodiment [1] or [2], wherein the ring Ar 3 is a biphenyl ring.

[0015] The embodiment [4] of the present disclosure relates to any one of the embodiments [1] to [3], wherein in the formula (2), A 3 C 2-4 In this embodiment, it is an alkylene group, t is an integer of 0 to 10, and X is an alkyl group or a polymerizable substituent.

[0016] The embodiment [5] of the present disclosure relates to any one of the embodiments [1] to [4], wherein in the formula (2), A 3 C 2-4 In this embodiment, X is an alkylene group, t is an integer of 1 to 10, and X is an alkenylcarbonyl group represented by the following formula (3).

[0017] [ka]

[0018] (In the formula, R 7 represents a hydrogen atom or an alkyl group.

[0019] The embodiment [6] of the present disclosure is any one of the embodiments [1] to [5], wherein the terminal of the acid anhydride-modified fluorene-containing acrylic resin is C 4-10 Cycloalkene ring or C 6-12 In this embodiment, the compound is terminated with a dicarboxylic acid anhydride having a bicycloalkene ring.

[0020] An embodiment [7] of the present disclosure is any one of the above embodiments [1] to [6], in which the acid value is 20 to 200 mgKOH / g.

[0021] An embodiment [8] of the present disclosure is any one of the above embodiments [1] to [7], in which the weight average molecular weight is 5,000 or more.

[0022] The present disclosure also includes, as aspect [9], a method for producing a photosensitive resin of any one of aspects [1] to [8] by reacting an acid anhydride-modified fluorene-containing acrylic resin having a repeating unit represented by formula (1) with an epoxy group-containing compound represented by formula (2).

[0023] The present disclosure also includes, as an embodiment

[10] , a resin composition including the photosensitive resin according to any one of the above embodiments [1] to [8] and a photopolymerization initiator.

[0024] The present disclosure also includes, as an embodiment

[11] , a cured product obtained by curing the resin composition of the embodiment

[10] .

[0025] In this specification and claims, the number of carbon atoms of a substituent, etc. is represented as C1, C6, C 10 For example, "C1 alkyl group" means an alkyl group with one carbon atom, and "C 6-10 The term "aryl group" refers to an aryl group having 6 to 10 carbon atoms.

[0026] In the present specification and claims, the term "independently" means that two components are independent components, for example, an alkylene group A 1 and A 2 In the case of A 1 and A 2 and do not have to be the same alkylene group, but may be different alkylene groups.

[0027] Furthermore, in this specification and claims, when a numerical range is indicated using "X to Y," the endpoints X and Y may be included. Effect of the Invention

[0028] The present disclosure provides a novel photosensitive resin obtained by adding a specific epoxy group-containing compound to an acid anhydride-modified fluorene-containing acrylic resin obtained by reacting an epoxy(meth)acrylate having a 9,9-bis(condensed polycyclic aryl)fluorene skeleton with a tetracarboxylic dianhydride, and the photosensitive resin has excellent curability and solvent solubility. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0029] [Photosensitive resin] The photosensitive resin of the present invention is a novel photosensitive resin obtained by adding an epoxy group-containing compound represented by the above formula (2) (the epoxy group of this compound) to an acid anhydride-modified fluorene-containing acrylic resin having a repeating unit represented by the above formula (1) (the carboxyl group of the resin).

[0030] (Acid anhydride modified fluorene-containing acrylic resin) In the formula (1) which represents the repeating unit of the acid anhydride-modified fluorene-containing acrylic resin, 1 and ring Ar 2 The fused polycyclic hydrocarbon ring represented by the formula (I) may be a fused bicyclic to tetracyclic aromatic hydrocarbon ring. The fused bicyclic aromatic hydrocarbon ring may be a fused bicyclic C ring such as an indene ring or a naphthalene ring. 8-20Examples of the fused tricyclic aromatic hydrocarbon ring include fused tricyclic C rings such as acenaphthylene ring, fluorene ring, phenalene ring, anthracene ring, and phenanthrene ring. 14-20 Examples of the fused tetracyclic aromatic hydrocarbon ring include fused tetracyclic C rings such as pyrene rings and naphthacene rings. 16-22 These condensed polycyclic hydrocarbon rings can be used alone or in combination of two or more. 10-16 Fused bicyclic hydrocarbon rings are preferred, and fused bicyclic C rings such as naphthalene rings are preferred. 10-14 An arene ring is preferred, and a naphthalene ring is particularly preferred. Ring Ar 1 and ring Ar 2 may be different, but are usually the same.

[0031] Ring Ar to the 9-position of the fluorene ring 1 and ring Ar 2 The bonding position of is not particularly limited, and for example, 1 and ring Ar 2 When is a naphthalene ring, it is at the 1- or 2-position, preferably the 2-position.

[0032] A 1 and A 2 Examples of the alkylene group represented by the formula (I) include an ethylene group, a propylene group (1,2-propanediyl group), a trimethylene group, a 1,2-butanediyl group, a tetramethylene group, and the like. 2-6 These alkylene groups can be used alone or in combination of two or more. 2-4 Alkylene groups are preferred, and C groups such as ethylene and propylene groups are preferred. 2-3 An alkylene group is more preferred, and an ethylene group is most preferred. 1 and an alkylene group A 2 may be different, but are usually the same.

[0033] The repeat numbers n1 and n2 are each 0 or more and can be selected, for example, from the range of integers from 0 to 15, preferably 0 to 10, 0 to 8, 0 to 6, 0 to 4, 0 to 3, 0 to 1, and most preferably 0. The repeat numbers n1 and n2 may be the same or different from each other; when n1 and n2 are integers of 2 or more, two or more alkylene groups A 1 and A 2 The types may be the same or different.

[0034] In this specification and claims, the "repetition number (number of moles added)" may be an average value (arithmetic mean value, additive mean value) or an average number of moles added, and preferred embodiments are the same as the preferred ranges (range of integers) described above.

[0035] R 1 and R 2 The substituent represented by the formula (I) may be a non-reactive substituent that is inactive in the reaction, and examples thereof include a halogen atom, an alkyl group, an aryl group, an alkoxy group, an acyl group, a nitro group, a cyano group, and a mono- or di-substituted amino group.

[0036] Examples of the halogen atom include a fluorine atom, a chlorine atom, a bromine atom, and an iodine atom.

[0037] The alkyl group includes linear or branched alkyl groups, and C groups such as methyl, ethyl, propyl, isopropyl, n-butyl, and t-butyl groups. 1-10 Alkyl groups, preferably C 1-6 Alkyl groups, more preferably C 1-4 Examples of the aryl group include C alkyl groups such as phenyl groups, alkylphenyl groups, biphenylyl groups, and naphthyl groups. 6-12 Aryl groups; mono- or tri-C such as methylphenyl (or tolyl), dimethylphenyl (or xylyl) groups 1-4 Examples include alkyl-phenyl groups.

[0038] The alkoxy group is a C group such as a methoxy group, an ethoxy group, a propoxy group, an n-butoxy group, or a t-butoxy group. 1-10 Examples of acyl groups include C alkoxy groups such as acetyl groups. 1-6 Examples include alkyl-carbonyl groups.

[0039] The mono- or di-substituted amino group is a mono- or di-C group such as a dimethylamino group. 1-4 Alkylamino groups; bis(C 1-4 alkyl-carbonyl)amino groups.

[0040] Representative Substituent R 1 and R 2 Examples of the C alkyl group include an alkyl group, an aryl group, an alkoxy group, an acyl group, a nitro group, and a cyano group. Among these, the alkyl group and the alkoxy group are preferable, and C 1-6 Alkyl group, C 1-4 Alkyl groups are more preferred, and C groups such as methyl groups are preferred. 1-4 Alkyl groups are most preferred. 1 and the substituent R 2 may be the same or different.

[0041] The numbers of substitutions m1 and m2 are integers of 0 to 4, preferably integers of 0 to 2, more preferably 0 or 1, and even more preferably 0. When m1 and m2 are integers of 2 or more, two or more substituents R 1 and the substituent R 2 The types may be the same or may be different combinations.

[0042] R 3 The substituent represented by the formula (I) may be a non-reactive substituent that is inactive in the reaction, and examples thereof include a cyano group; a halogen atom such as a fluorine atom, a chlorine atom, or a bromine atom; and a hydrocarbon group such as an alkyl group or an aryl group. Examples of the alkyl group include a C group such as a methyl group, an ethyl group, an n-propyl group, an isopropyl group, an n-butyl group, or a t-butyl group. 1-12The aryl group includes a C alkyl group such as a phenyl group. 6-10 Aryl groups and the like are preferred. 3 Examples of the alkyl groups include cyano groups, halogen atoms, and alkyl groups, particularly alkyl groups. 1-8 Alkyl groups are preferred, C 1-6 Alkyl groups are preferred, and C groups such as methyl groups are preferred. 1-4 Alkyl groups are particularly preferred.

[0043] In addition, the substituent R 3 When the number of substitutions k is 2 or more, two or more substituents R 3 The types of R may be the same or different, and two or more groups R substituted on different benzene rings may be 3 The types of the groups R may be the same or different. 3 The bonding positions (substitution positions) of are not particularly limited as long as they are positions 1 to 8 of the fluorene ring, and examples thereof include positions 2, 7, and 2,7 of the fluorene ring.

[0044] The number of substitutions k may be, for example, an integer of 0 to 6, and is preferably 0 to 4, 0 to 3, 0 to 2, 0 or 1 in the following stepwise order, and is most preferably 0. In addition, in the two benzene rings constituting the fluorene ring, the group R 3 The number of substitutions in each of the above may be different from each other, but is preferably the same.

[0045] Ring Ar 3 Examples of the hydrocarbon ring represented by the formula (I) include an aromatic hydrocarbon ring and an aliphatic hydrocarbon ring.

[0046] Examples of the aromatic hydrocarbon ring include a monocyclic aromatic hydrocarbon ring, a condensed polycyclic aromatic hydrocarbon ring, and a non-condensed polycyclic aromatic hydrocarbon ring.

[0047] Monocyclic aromatic hydrocarbon rings include C rings such as benzene ring, toluene ring, and xylene ring. 1-4Examples of the alkylbenzene ring include an alkyl group.

[0048] The fused polycyclic hydrocarbon ring includes the ring Ar 1 and ring Ar 2 Examples of the aromatic ring include the fused bicyclic to tetracyclic aromatic hydrocarbon rings exemplified as above.

[0049] Non-condensed polycyclic hydrocarbon rings include diphenyl C rings such as biphenyl ring, diphenyl ether ring, diphenyl thioether ring, diphenyl sulfone ring, benzophenone ring, diphenyl methane ring, and diphenyl propane ring. 1-10 Examples include an alkane ring.

[0050] The aliphatic hydrocarbon ring includes a ring obtained by hydrogenating the aromatic hydrocarbon ring, for example, a saturated aliphatic hydrocarbon ring (e.g., C cyclopentane, cyclohexane, cycloheptane, etc.). 3-10 Cycloalkane ring, tetralin ring, etc.), unsaturated aliphatic hydrocarbon ring (e.g., C 4-10 Cycloalkene rings, etc.

[0051] These hydrocarbon rings can be used alone or in combination of two or more. Among these hydrocarbon rings, non-condensed polycyclic hydrocarbon rings are preferred from the viewpoint of excellent moisture absorption resistance, and ring assembly arene rings are more preferred.

[0052] As the ring assembly arene ring, there are C 12-20 Biarene ring, terphenyl ring, etc. 16-20 Terarene ring; 9,9-diC such as 9,9-diphenylfluorene ring, 9,9-dinaphthylfluorene ring, and 9,9-bis(phenylphenyl)fluorene ring 6-18 Arylfluorene ring; 9,9-bis(C 1-3 9,9-bis(C 1-3 Alkyl C 6-18 Ring assembly C such as aryl)fluorene ring 6-30 arene rings. Among these, C12-16 A biarene ring is preferred.

[0053] R 4 The substituent represented by the formula: 3 Preferred substituents R 4 Examples of the alkyl groups include cyano groups, halogen atoms, and alkyl groups, particularly alkyl groups. 1-8 Alkyl groups are preferred, C 1-6 Alkyl groups are preferred, and C groups such as methyl groups are preferred. 1-4 Alkyl groups are particularly preferred.

[0054] The number of substitutions p is, for example, an integer of 0 to 4, preferably an integer of 0 to 2, more preferably 0 or 1, and even more preferably 0. When p is an integer of 2 or more, two or more substituents R 4 The types may be the same or may be in different combinations.

[0055] R 5 and R 6 Examples of the alkyl group represented by the formula (I) include a methyl group, an ethyl group, a propyl group, an isopropyl group, a butyl group, a s-butyl group, and a t-butyl group. 1-10 Alkyl groups and the like are examples of R 5 and R 6 may be different, but are usually the same. 5 and R 6 Examples of C groups include hydrogen atoms and methyl groups. 1-4 It is an alkyl group, more preferably a hydrogen atom or a methyl group, and most preferably a hydrogen atom.

[0056] The repeating number s of the repeating unit is an integer of 1 or more, and is usually about 1 to 100, preferably 2 to 50, more preferably 3 to 30, and most preferably 5 to 20.

[0057] The weight average molecular weight of the acid anhydride modified fluorene-containing acrylic resin, as measured by gel permeation chromatography (standard resin: polystyrene), can be selected from the range of about 1000 to 20000, preferably in the following stepwise order: 1000 to 18000, 1500 to 15000, 2000 to 10000, 2500 to 8000, 3000 to 7000, 4000 to 6000. If the molecular weight is too large, there is a risk that the viscosity increases and the handling properties decrease, whereas if the molecular weight is too small, there is a risk that the modification effect by the acid anhydride is not exhibited.

[0058] The acid anhydride-modified fluorene-containing acrylic resin can be produced by a conventional method of reacting a fluorene-containing epoxy (meth)acrylate (fluorene-containing acrylic resin) with a tetracarboxylic dianhydride, for example, by the method described in Patent Document 1.

[0059] (End-capping acid anhydride modified fluorene-containing acrylic resin) The acid anhydride-modified fluorene-containing acrylic resin may be a terminal-capped acid anhydride-modified fluorene-containing acrylic resin in which its own hydroxyl group (terminal hydroxyl group) is capped with dicarboxylic anhydride. In the present invention, by capping the terminal hydroxyl group of the acid anhydride-modified fluorene-containing acrylic resin with dicarboxylic anhydride, the molecular weight can be adjusted, the generation of gel can be suppressed, and the handling property can be further improved.

[0060] The end-capping acid anhydride-modified fluorene-containing acrylic resin is obtained by reacting an acid anhydride-modified fluorene-containing acrylic resin with a dicarboxylic acid anhydride. By using a dicarboxylic acid anhydride as an end-capping agent in addition to a raw material (tetracarboxylic acid dianhydride) for forming a repeating unit as the acid anhydride, the proportion of terminal hydroxyl groups can be adjusted and handling properties can be improved.

[0061] Examples of dicarboxylic anhydrides include saturated aliphatic dicarboxylic anhydrides such as succinic anhydride; unsaturated aliphatic dicarboxylic anhydrides such as itaconic anhydride, maleic anhydride, and fumaric anhydride; saturated alicyclic dicarboxylic anhydrides such as tetrahydrophthalic anhydride; unsaturated alicyclic dicarboxylic anhydrides such as hexahydrophthalic anhydride and 5-norbornene-2,3-dicarboxylic anhydride; and aromatic dicarboxylic anhydrides such as phthalic anhydride. These dicarboxylic anhydrides can be used alone or in combination of two or more. Among these dicarboxylic anhydrides, dicarboxylic anhydrides having a monocyclic or condensed polycyclic aromatic hydrocarbon ring such as a benzene ring or a naphthalene ring, dicarboxylic anhydrides having a saturated aliphatic hydrocarbon ring such as cyclohexane or norbornane, and dicarboxylic anhydrides having an unsaturated aliphatic hydrocarbon ring such as cyclohexene or norbornene are preferred, and dicarboxylic anhydrides having an unsaturated aliphatic hydrocarbon ring such as cyclohexene or norbornene are preferred because they can improve the solvent solubility, improve the optical properties, and provide a polymerizable group. 4-10 Dicarboxylic anhydrides having a cycloalkene ring (e.g., tetrahydrophthalic anhydride, etc.), C such as norbornene 6-12 Dicarboxylic anhydrides having a bicycloalkene ring (e.g., 5-norbornene-2,3-dicarboxylic anhydride, etc.) are preferred, and C 6-12 Dicarboxylic anhydrides having a bicycloalkene ring, C 6-10 Dicarboxylic acid anhydrides having a bicycloalkene ring are particularly preferred.

[0062] The blending ratio of the dicarboxylic anhydride to the tetracarboxylic dianhydride for producing the acid anhydride-modified fluorene-containing acrylic resin may be adjusted according to the target molecular weight and the blocking ratio of the terminals. The ratio of the dicarboxylic anhydride is, for example, 0.01 to 1 mol, preferably 0.05 to 0.9 mol, more preferably 0.1 to 0.8 mol, more preferably 0.2 to 0.5 mol, and most preferably 0.3 to 0.4 mol, relative to 1 mol of the tetracarboxylic dianhydride.

[0063] The weight average molecular weight of the end-capping acid anhydride modified fluorene-containing acrylic resin, as measured by gel permeation chromatography (standard resin: polystyrene), can be selected from the range of about 1000 to 20000, preferably in the following stepwise order: 1000 to 18000, 2000 to 15000, 2000 to 10000, 2500 to 8000, 3000 to 7000, 4000 to 6000. If the molecular weight is too large, there is a risk that the viscosity increases and the handling properties decrease, whereas if the molecular weight is too small, there is a risk that the modification effect by the acid anhydride will not be exhibited.

[0064] In the end-blocked acid anhydride-modified fluorene-containing acrylic resin, the blocking rate of the terminal hydroxyl groups (blocking ratio of the terminal hydroxyl groups of the acid anhydride-modified fluorene-containing acrylic resin) is, for example, 10% or more, preferably 30% or more, more preferably 50% or more, and more preferably 70% or more.

[0065] The end-capping acid anhydride-modified fluorene-containing acrylic resin can be produced by a conventional method (end-capping method for acid anhydride-modified fluorene-containing acrylic resin), for example, by the method described in Patent Document 1.

[0066] (Epoxy group-containing compound) In the formula (2), A 3 The alkylene group represented by the formula (I) is a linear C alkylene group such as an ethylene group, a trimethylene group, a tetramethylene group, a 1,2-butanediyl group, or a tetramethylene group. 2-6 Alkylene group; branched chain C such as propylene group (1,2-propanediyl group), 1,2-butanediyl group, and 1,3-butanediyl group 3-6 These alkylene groups can be used alone or in combination of two or more. 2-4 Alkylene groups are preferred, and linear C 3-4 An alkylene group is more preferred, and a butylene group is most preferred.

[0067] The repeat number t is 0 or more, and can be selected, for example, from the range of integers from 0 to 10, and is preferably 0 to 5, more preferably 0 to 3, and more preferably 0 to 2. When X is a non-polymerizable substituent such as an alkyl group, the repeat number t is, for example, 0 to 3, preferably 0 to 2, more preferably 0 or 1, and more preferably 0. When X is a polymerizable substituent such as an alkenylcarbonyl group, the repeat number t is, for example, 1 to 10, preferably 1 to 5, more preferably 1 to 3, more preferably 1 or 2, and most preferably 1. When the repeat number t is an integer of 2 or more, the alkylene group A 3 The types may be the same or different.

[0068] The substituent represented by X may be a non-polymerizable substituent or a polymerizable substituent.

[0069] Examples of the non-polymerizable substituent include an alkyl group, a cycloalkyl group, and an aryl group. Examples of the alkyl group include a C group such as a methyl group, an ethyl group, a propyl group, an isopropyl group, a butyl group, a s-butyl group, a t-butyl group, a pentyl group, a hexyl group, an octyl group, a 2-ethylhexyl group, a nonyl group, a decyl group, and a lauryl group. 1-20 Examples of cycloalkyl groups include C alkyl groups such as cyclopentyl and cyclohexyl groups. 5-10 Examples of the aryl group include a C phenyl group, an alkylphenyl group, a biphenylyl group, and a naphthyl group. 6-12 Examples of such groups include aryl groups.

[0070] These non-polymerizable substituents can be used alone or in combination of two or more. Among these non-polymerizable substituents, alkyl groups (straight-chain or branched-chain alkyl groups, preferably branched-chain alkyl groups) are preferred. 3-18 Alkyl groups are particularly preferred, C 4-12 Alkyl groups are more preferred, C 6-10 Alkyl groups are more preferred, and branched C 6-10 Alkyl groups are most preferred.

[0071] Examples of the polymerizable substituent include an alkenyl group and an alkenylcarbonyl group.

[0072] Examples of the alkenyl group include vinyl, 1-propenyl, allyl, 1-butenyl, 2-butenyl, and 3-butenyl groups. 2-20 Alkenyl groups and the like.

[0073] The alkenylcarbonyl group includes the alkenylcarbonyl group represented by the above formula (3).

[0074] In the formula (3), R 7 Examples of the alkyl group represented by the formula (I) include methyl, ethyl, and propyl groups. 1-6 Alkyl groups and the like.

[0075] These polymerizable substituents may be used alone or in combination of two or more. Among these polymerizable substituents, C 3-12 Alkenyl group; R 7 is a hydrogen atom or C 1-4 The alkyl group, alkenylcarbonyl, is preferred.

[0076] Preferred examples of the substituent represented by X include an alkyl group and a polymerizable substituent, and from the viewpoint of excellent curability and solvent solubility, a polymerizable substituent is more preferred, a (meth)acryloyl group is more preferred, and from the viewpoint of excellent optical properties, an acryloyl group is most preferred.

[0077] Specific examples of epoxy group-containing compounds in which X is an alkyl group include linear or branched C glycidyl ethers such as hexyl glycidyl ether, 2-ethylhexyl glycidyl ether, octyl glycidyl ether, nonyl glycidyl ether, 2-methyloctyl glycidyl ether, decyl glycidyl ether, and lauryl glycidyl ether. 4-18Examples of compounds in which X is an alkenyl group include vinyl glycidyl ether and allyl glycidyl ether. 2-6 Examples of compounds in which X is an alkenylcarbonyl group include glycidyl (meth)acrylate, 2-hydroxyethyl (meth)acrylate glycidyl ether, 3-hydroxypropyl (meth)acrylate glycidyl ether, 4-hydroxybutyl (meth)acrylate glycidyl ether, di- or polypropylene glycol (meth)acrylate glycidyl ether, and the like.

[0078] The ratio of the epoxy group-containing compound is, for example, 0.1 to 1 mol, preferably 0.3 to 0.8 mol, more preferably 0.4 to 0.7 mol, and even more preferably 0.5 to 0.6 mol, relative to 1 mol of the acid anhydride-modified fluorene-containing acrylic resin. If the ratio of the epoxy group-containing compound is too low, the photosensitivity may decrease, and if it is too high, the alkali solubility may decrease.

[0079] (Photosensitive resin properties) The photosensitive resin may be alkali-soluble, and the acid value can be adjusted by the ratio of the acid anhydride and the epoxy group-containing compound. The acid value (solid acid value) of the photosensitive resin can be selected from the range of about 20 to 200 mgKOH / g, for example, 30 to 180 mgKOH / g, preferably 40 to 150 mgKOH / g, more preferably 50 to 120 mgKOH / g, more preferably 60 to 100 mgKOH / g, and most preferably 70 to 90 mgKOH / g. If the acid value is too small, the photosensitivity may decrease. If the acid value is too high, the development may be excessive, and the pattern may peel off.

[0080] In the present specification and claims, the acid value can be measured in accordance with JIS K 0070.

[0081] The weight average molecular weight of the photosensitive resin, as measured by gel permeation chromatography (standard resin: polystyrene), is 1000 or more, preferably 5000 or more, but can be selected from the range of about 1000 to 30000, preferably in the following stepwise order: 2000 to 20000, 3000 to 18000, 5000 to 15000, 6000 to 13000, 7000 to 12000, and 8000 to 10000. If the molecular weight is too large, there is a risk of reduced developability, and conversely, if it is too low, there is a risk of reduced mechanical strength of the pattern.

[0082] (Method of manufacturing photosensitive resin) The addition reaction between the acid anhydride-modified fluorene-containing acrylic resin having a repeating unit represented by the formula (1) and the epoxy group-containing compound represented by the formula (2) may be carried out in the absence of a solvent or in the presence of a solvent inert to the reaction.

[0083] Examples of the solvent include aliphatic hydrocarbons such as hexane and heptane; aromatic hydrocarbons such as benzene, toluene, and xylene; halogenated hydrocarbons such as methylene chloride, chloroform, and carbon tetrachloride; dialkyl ethers such as diethyl ether; cyclic ethers such as tetrahydrofuran; ketones such as acetone, methyl ethyl ketone, methyl isobutyl ketone, diisobutyl ketone, and cyclohexanone; esters such as ethyl acetate and butyl acetate; sulfoxides such as dimethyl sulfoxide; amides such as formamide, N-methyl-pyrrolidone, dimethylformamide, and dimethylacetamide; nitriles such as acetonitrile; cellosolves; carbitols; cellosolve acetates; and carbitol acetates. These solvents can be used alone or in combination. These solvents may be the same solvents used in the production of the acid anhydride-modified fluorene-containing acrylic resin.

[0084] Among these solvents, cellosolves, carbitols, cellosolve acetates, and carbitol acetates are preferred from the viewpoint of effectively improving the solubility of the photosensitive resin in the solvent.

[0085] Cellosolves include C methyl cellosolve, ethyl cellosolve, butyl cellosolve, etc. 1-4 Alkyl cellosolve, propylene glycol mono C 1-4 Alkyl ethers such as propylene glycol monomethyl ether are included.

[0086] Carbitols include C carbitol, such as methyl carbitol, ethyl carbitol, propyl carbitol, and butyl carbitol. 1-4 Alkyl carbitols and the like.

[0087] Cellosolve acetates include C ethyl cellosolve acetate, butyl cellosolve acetate, etc. 1-4 Alkyl cellosolve acetate; propylene glycol monomethyl ether acetate, etc. 1-4 Alkyl ether acetates and the like.

[0088] Carbitol acetates include C carbitol acetate, ethyl carbitol acetate, butyl carbitol acetate, etc. 1-4 Alkyl carbitol acetate; dipropylene glycol monomethyl ether acetate, etc. 1-4 Alkyl ether acetates and the like.

[0089] Among these, cellosolve acetates are preferred, and propylene glycol monomethyl ether acetate and other propylene glycol mono-C 1-4 Alkyl ether acetates are most preferred.

[0090] The proportion of the solvent is not particularly limited, but is, for example, 10 to 300 parts by mass, preferably 20 to 200 parts by mass, more preferably 30 to 150 parts by mass, and even more preferably 50 to 100 parts by mass relative to 100 parts by mass of the acid anhydride-modified fluorene-containing acrylic resin.

[0091] A catalyst may be added to the addition reaction to accelerate the reaction. Examples of the catalyst include aliphatic amines, aromatic amines, heterocyclic amines, quaternary ammonium salts, phosphines, and phosphonium salts.

[0092] Examples of the aliphatic amine include aliphatic tertiary amines such as triethylamine, tri-n-propylamine, tri-n-butylamine, triisopropylamine, diisopropylethylamine, dicyclohexylethylamine, dimethylcyclohexylamine, diethylcyclohexylamine, dimethylbenzylamine, tribenzylamine, N,N,N',N'-tetramethylethylenediamine, N,N,N',N'-tetramethylpropanediamine, 1-methylpiperidine, 1-ethylpiperidine, 1,2,2',6,6'-pentamethylpiperidine, 1-methylpyrrolidine, 1-ethylpyrrolidine, 4-methylmorpholine, 4-ethylmorpholine, 2,6-dimethylpiperazine, and tris(N,N-dimethylaminomethyl)phenol.

[0093] Examples of the aromatic amine include aromatic tertiary amines such as N,N-dimethylaniline and N,N-diethylaniline.

[0094] Examples of heterocyclic amines include pyridine, quinoline, lutidine, collidine, 4-(dimethylamino)pyridine, 4-pyrrolidinopyridine, imidazole, 2-methylimidazole, 2-ethyl-4-methylimidazole, triethylenediamine, 1,5-diazabicyclo[4.3.0]-5-nonene, and 1,8-diazabicyclo[5.4.0]-7-undecene.

[0095] Examples of the quaternary ammonium salt include tetramethylammonium chloride, tetramethylammonium bromide, benzyltrimethylammonium chloride, benzyltrimethylammonium bromide, and tetramethylammonium hydroxide.

[0096] Examples of the phosphines include tributylphosphine and triphenylphosphine.

[0097] The phosphonium salt includes n-butyltriphenylphosphonium bromide.

[0098] These catalysts can be used alone or in combination of two or more. The ratio of the catalyst is not particularly limited, but is, for example, 0.01 to 5 parts by mass, preferably 0.05 to 3 parts by mass, and more preferably 0.1 to 2 parts by mass, relative to 100 parts by mass of the acid anhydride-modified fluorene-containing acrylic resin.

[0099] A polymerization inhibitor may be added to the addition reaction. Examples of the polymerization inhibitor include hydroquinone, hydroquinone monomethyl ether, t-butyl hydroquinone, t-butyl catechol, N-methyl-N-nitrosoaniline or N-nitrosophenylhydroxylamine ammonium salt, N-nitrosophenylhydroxylamine aluminum salt, 2,2,6,6-tetramethylpiperidine-1-oxyl, and 4-hydroxy-2,2,6,6-tetramethylpiperidine-1-oxyl. These polymerization inhibitors may be used alone or in combination.

[0100] The proportion of the polymerization inhibitor is 1 to 5000 ppm, preferably 3 to 3000 ppm, and more preferably 5 to 2000 ppm, based on the total amount of the acid anhydride-modified fluorene-containing acrylic resin and the polymerization inhibitor.

[0101] The addition reaction is preferably heated to increase the reaction rate. The heating temperature is, for example, 60 to 150°C, preferably 80 to 130°C, and more preferably 100 to 120°C.

[0102] [Resin composition or photosensitive resin composition] The photosensitive resin of the present disclosure has a 9,9-bis(condensed polycyclic aryl)fluorene skeleton (particularly a bisnaphtholfluorene skeleton), and has characteristics specific to the fluorene skeleton, such as high heat resistance, high refractive index, and low linear expansion. Moreover, despite having such a fluorene skeleton, it has excellent curability and solvent solubility. Therefore, the photosensitive resin of the present invention can be suitably used as a heat- or light-curable (meth)acrylic resin. The photosensitive resin may be prepared as a photosensitive resin composition (or a curable resin composition) that usually contains a polymerization initiator and the like.

[0103] Examples of photopolymerization initiators include benzoins such as benzoin, methylbenzoin, and ethylbenzoin; benzoin alkyl ethers such as benzoin methyl ether, benzoin ethyl ether, and benzoin isopropyl ether; acetophenones such as acetophenone diethyl ketal, diethoxyacetophenone, benzyl methyl ketal, 2-hydroxy-2-methyl-1-phenylpropan-1-one, and 1-hydroxy-cyclohexyl-phenyl ketone; and 2-methyl-1-[4-(methylthio)phenyl]-2-methyl-1-phenylpropan-1-one and 1-hydroxy-cyclohexyl-phenyl ketone. Examples of the photopolymerization initiator include aminoacetophenones such as fluoroaminopropanone-1, anthraquinones such as anthraquinone and 2-methylanthraquinone, thioxanthones such as thioxanthone, 2,4-dimethylthioxanthone, 2,4-diethylthioxanthone, and 2-chlorothioxanthone, and benzophenones such as benzophenone, 4-hydroxybenzophenone, bis-N,N-dimethylaminobenzophenone, bis-N,N-diethylaminobenzophenone, and 4-methoxy-4'-dimethylaminobenzophenone. These photopolymerization initiators can be used alone or in combination of two or more.

[0104] The photopolymerization initiator may be combined with a photosensitizer. Tertiary amines are commonly used as photosensitizers. Examples of tertiary amines include trialkylamines; trialkanolamines such as triethanolamine; dialkylaminobenzoic acid alkyl esters such as ethyl N,N-dimethylaminobenzoate [ethyl p-(dimethylamino)benzoate, etc.] and amyl N,N-dimethylaminobenzoate [amyl p-(dimethylamino)benzoate, etc.]; bis(dialkylamino)benzophenones such as 4,4-bis(diethylamino)benzophenone (Michler's ketone); and dialkylaminobenzophenones such as 4-(dimethylamino)benzophenone. The photosensitizers can be used alone or in combination of two or more.

[0105] The total amount of the polymerization initiator and the photosensitizer is 0.1 to 30 parts by mass, preferably 1 to 20 parts by mass, and more preferably 2 to 10 parts by mass, based on 100 parts by mass of the photosensitive resin.

[0106] The photosensitive resin composition of the present disclosure may further contain other multifunctional (meth)acrylates, such as difunctional (meth)acrylates, trifunctional or higher multifunctional (meth)acrylates, urethane (meth)acrylates, epoxy (meth)acrylates, and polyester (meth)acrylates.

[0107] Bifunctional (meth)acrylates include C such as ethylene glycol di(meth)acrylate. 2-10 Alkylene glycol di(meth)acrylates such as alkylene glycol di(meth)acrylate; Poly(C) such as polyethylene glycol di(meth)acrylate 2-4 Examples of the alkylene glycol di(meth)acrylate include alkylene glycol di(meth)acrylate and bisphenol A di(meth)acrylate.

[0108] Examples of the trifunctional or higher polyfunctional (meth)acrylates include tri- or tetraol tri- or tetra(meth)acrylates such as glycerin tri(meth)acrylate, trimethylolpropane tri(meth)acrylate, and pentaerythritol tri- or tetra(meth)acrylate; ditrimethylolpropane tetra(meth)acrylate; and dipentaerythritol tetra- or hexa(meth)acrylate.

[0109] These other polyfunctional (meth)acrylates can be used alone or in combination.

[0110] The proportion of the other polyfunctional (meth)acrylate is, for example, 1 to 100 parts by mass, preferably 2 to 60 parts by mass, and more preferably 5 to 30 parts by mass, relative to 100 parts by mass of the photosensitive resin.

[0111] The photosensitive resin composition of the present disclosure may further contain a diluent. The diluent includes a reactive diluent and a non-reactive diluent (solvent).

[0112] Examples of reactive diluents include alkyl (meth)acrylates such as methyl (meth)acrylate; cycloalkyl methacrylates such as cyclohexyl (meth)acrylate; aryl (meth)acrylates such as phenyl (meth)acrylate; hydroxyalkyl (meth)acrylates such as hydroxyethyl (meth)acrylate; and (poly)oxy C such as diethylene glycol mono(meth)acrylate. 2-6 Examples of the reactive diluent include alkylene glycol mono(meth)acrylate, N,N-dialkyl(meth)acrylamides such as N,N-dimethyl(meth)acrylamide, and glycidyl(meth)acrylate. These reactive diluents can be used alone or in combination of two or more kinds.

[0113] The proportion of the reactive diluent is, for example, 1 to 1000 parts by mass, preferably 5 to 500 parts by mass, and more preferably 10 to 200 parts by mass, relative to 100 parts by mass of the photosensitive resin.

[0114] The solvent can be selected from solvents used in the production of photosensitive resins. The solvents can be used alone or in combination of two or more. Among the solvents, cellosolves, carbitols, cellosolve acetates, and carbitol acetates are preferred, cellosolve acetates are more preferred, and propylene glycol monomethyl ether acetate and other propylene glycol monomethyl ether acetates are more preferred. 1-4 Alkyl ether acetates are most preferred.

[0115] The ratio of the solvent can be selected from the range of about 1 to 500 parts by mass relative to 100 parts by mass of the photosensitive resin, and is, for example, 10 to 400 parts by mass, preferably 20 to 300 parts by mass, and more preferably 30 to 200 parts by mass.

[0116] The photosensitive resin composition of the present disclosure may contain conventional additives, such as colorants, stabilizers (thermal stabilizers, antioxidants, ultraviolet absorbers, etc.), fillers, antistatic agents, flame retardants, flame retardant assistants, leveling agents, silane coupling agents, polymerization inhibitors (or thermal polymerization inhibitors), surfactants, etc. These additives may be used alone or in combination of two or more. The proportion of these additives is, for example, 0.01 to 100 parts by mass, preferably 0.1 to 50 parts by mass, and more preferably 1 to 30 parts by mass, relative to 100 parts by mass of the photosensitive resin.

[0117] [Cured product of photosensitive resin composition] The cured product of the photosensitive resin composition of the present disclosure can be produced by subjecting the photosensitive resin composition to a curing treatment. For example, a film-like cured product may be produced by applying the photosensitive resin composition to a substrate to form a coating film (or thin film) and then subjecting the substrate to a curing treatment. In the present invention, a coating film having high adhesion to the substrate can be formed.

[0118] The thickness of the film-like coating (or thin film) can be selected depending on the application and is, for example, 0.1 to 1000 μm, preferably 1 to 500 μm, and more preferably 5 to 300 μm.

[0119] In this method, a cured product can be produced without the need for dilution with a large amount of diluent (solvent, polymerizable diluent, etc.) or heating to reduce viscosity, etc. Therefore, it is easy to introduce a 9,9-bis(condensed polycyclic aryl)fluorene skeleton into the cured product at a high concentration, and a cured product with excellent properties (high refractive index, high heat resistance, etc.) can be easily produced.

[0120] Examples of the curing treatment include ultraviolet treatment and light irradiation treatment such as electron beam treatment. In the light irradiation treatment (exposure treatment), the amount of light irradiation energy varies depending on the application, the thickness of the coating film, etc., but is usually 0.1 to 10,000 mJ / cm 2 , preferably 1 to 8000 mJ / cm 2 , and more preferably 10 to 5000 mJ / cm 2 , more preferably 100 to 1000 mJ / cm 2 , and most preferably 300 to 800 mJ / cm 2 It is.

[0121] The refractive index nD of the cured film at a temperature of 20° C. and a wavelength of 589 nm may be 1.55 or more, for example, 1.55 to 1.7, preferably 1.57 to 1.65, further preferably 1.58 to 1.64, more preferably 1.59 to 1.63, and most preferably 1.60 to 1.63.

[0122] In this specification and claims, the refractive index nD of the cured film can be measured by the method described in the examples below.

[0123] When the photosensitive resin composition of the present disclosure is used as a photoresist, it is applied as a solution or paste onto a substrate. The application method is not particularly limited, but screen printing, curtain coating, blade coating, spin coating, spray coating, dip coating, slit coating, etc. are applied. The applied solution or paste is irradiated with light through a predetermined mask. When applying using a solvent, a drying treatment may be performed. A pattern can be formed by wet developing the exposed coating film. The development method can be any of a spray type, a paddle type, an immersion type, etc., but a spray type that leaves less residue is preferred. If necessary, ultrasonic waves or the like can also be applied. As the developer, it is preferable to use weak alkaline water. EXAMPLES

[0124] The present disclosure will be described in more detail below based on examples, but the present disclosure is not limited to these examples. Details of evaluation items and raw materials are shown below.

[0125] [Evaluation method] (Weight average molecular weight) The weight average molecular weight of the obtained photosensitive resin was measured by gel permeation chromatography (reference resin: polystyrene) using a 10% by volume solution of acetic acid in tetrahydrofuran as an eluent with an HLC-8220GPC (manufactured by Tosoh Corporation).

[0126] (Refractive index of cured film nD) To 100 parts by mass of the total amount of the obtained photosensitive resin, 3 parts by mass of Omnirad 184 (manufactured by BASF Japan Ltd.) was added as a photopolymerization initiator. The obtained resin composition was applied to a TAC (cellulose acetate) film with an applicator to a film thickness of 100 to 250 μm, and then dried on a hot plate at 100° C. for 180 seconds. The obtained coating film was then irradiated with UV (500 mJ / cm 2) was performed once to form a cured film, and the refractive index of the obtained cured film was measured at 25°C and 589 nm using a multi-wavelength Abbe refractometer (ATAGO Corp.'s "DR-M4" <using circulating thermostatic water bath 60-C3>).

[0127] (Acid value of solid content) The solid content acid value of the obtained photosensitive resin was measured in accordance with the neutralization titration method described in JIS K0070.

[0128] (Whether or not there is cloudiness when diluting with PGMEA) The obtained photosensitive resin was diluted with propylene glycol monomethyl ether acetate (PGMEA) to a concentration of 5% by mass and allowed to stand (25° C.), and the presence or absence of cloudiness was visually evaluated.

[0129] Comparative Example 1 According to Example 2 described in Patent Document 1, a solution containing an acid anhydride-modified fluorene-containing acrylic resin (acid anhydride-modified resin) A was obtained. That is, as shown in the following formula, a reaction product (BNFGA) of 9,9-bis(6-glycidyloxy-2-naphthyl)fluorene and acrylic acid was reacted with biphenyltetracarboxylic acid (s-BPDA), and then 1,2,3,6-tetrahydrophthalic anhydride (TPHA) was added to cap the ends, and a solution containing an end-capped acid anhydride-modified fluorene-containing acrylic resin (end-capped acid anhydride-modified resin) A was obtained [propylene glycol monomethyl ether acetate (PGMEA) solution in which the concentration of end-capped acid anhydride-modified resin A was 53.5% by mass]. The molecular weight of the obtained end-capped acid anhydride-modified resin A was measured, and the weight average molecular weight was 5200.

[0130] [ka]

[0131] Example 1 39.2 g (0.20 mol) of 4-hydroxybutyl acrylate glycidyl ether (4HBAGE) was added to 848.8 g of the solution containing the end-capped acid anhydride modified resin A obtained in Comparative Example 1, and reacted at 110°C for 4 hours as shown in the following formula (wherein the bonding position of 4HBAGE is an example), to synthesize photosensitive resin A, which was then allowed to cool to room temperature. The molecular weight of the obtained photosensitive resin A was measured, and it was found to be a weight average molecular weight of 8,800.

[0132] [ka]

[0133] Comparative Example 2 A solution containing an acid anhydride-modified fluorene-containing acrylic resin (acid anhydride-modified resin) B was obtained in accordance with Example 2 described in Patent Document 1, except that 5-norbornene-2,3-dicarboxylic anhydride (NDA) was used instead of TPHA. That is, as shown in the following formula, a reaction product (BNFGA) of 9,9-bis(6-glycidyloxy-2-naphthyl)fluorene and acrylic acid was reacted with biphenyltetracarboxylic acid (s-BPDA), and then 5-norbornene-2,3-dicarboxylic anhydride (NDA) was added to cap the ends, thereby obtaining a solution containing an end-capped acid anhydride-modified fluorene-containing acrylic resin (end-capped acid anhydride-modified resin) B [propylene glycol monomethyl ether acetate (PGMEA) solution in which the concentration of end-capped acid anhydride-modified resin B is 47.9% by mass]. The molecular weight of the obtained end-capped acid anhydride-modified resin B was measured, and the weight average molecular weight was 5100.

[0134] [ka]

[0135] Example 2 12.5 g (0.56 mol) of 2-ethylhexyl glycidyl ether (2EHGE) was added to 227.9 g of the solution containing the end-capped acid anhydride modified resin B obtained in Comparative Example 2, and reacted at 110° C. for 4 hours as shown in the following formula (wherein the bonding position of 2EHGE is an example), to synthesize photosensitive resin B, which was then allowed to cool to room temperature. The molecular weight of the obtained photosensitive resin B was measured, and the weight average molecular weight was 5,800.

[0136] [ka]

[0137] The evaluation results of Comparative Examples 1 and 2 and Examples 1 and 2 are shown in Table 1.

[0138] [Table 1]

[0139] As is clear from Table 1, in Examples 1 and 2, the photosensitive resin had excellent solvent solubility, and in addition, a cured film having a high refractive index was formed, and the curability was also excellent. [Industrial Applicability]

[0140] The photosensitive resin of the present disclosure can be used for coating materials, ink materials, light-emitting materials, organic semiconductors, graphitized precursors, gas separation membranes, coating agents, lenses, polarizing films, anti-reflection films, films for touch panels, films for flexible substrates, films for displays, overcoats, flexible film substrates, anisotropic conductive adhesive films (ACF), color filters, photoresists, interlayer insulating films, solder resists, photospacers for liquid crystal displays, membranes for fuel cells, optical fibers, optical waveguides, holograms, etc. In particular, the photosensitive resin composition containing the photosensitive resin has a high refractive index and excellent developability, and is therefore suitable for photoresist applications that form cured patterns in optical applications, and can be used for color filters such as lens filters and display filters; photoresists for TFT array etching, pigment-dispersed photoresists, dye-type photoresists, negative photoresists for liquid crystal display devices such as protective films; interlayer insulating films; solder resists; photospacers for liquid crystal displays, etc.

Claims

1. A photosensitive resin in which an epoxy group-containing compound represented by the following formula (2) is added to an acid anhydride-modified fluorene-containing acrylic resin having a repeating unit represented by the following formula (1). [Formula 1] (In the formula, Ring Ar 1 and ring Ar 2 each independently represents a fused polycyclic hydrocarbon ring; A 1 and A 2 each independently represents an alkylene group; n1 and n2 each independently represent an integer of 0 or more; R 1 and R 2 each independently represents a substituent; m1 and m2 each independently represent an integer of 0 or more; R 3 represents a substituent, k represents an integer of 0 to 8, Ring Ar 3 represents a hydrocarbon ring, R 4 represents a substituent, p represents an integer of 0 or more, R 5 and R 6 each independently represents a hydrogen atom or an alkyl group, s represents an integer of 1 or more) [chemical 2] (In the formula, A 3 represents an alkylene group, t represents an integer of 0 or more, and X represents a substituent.

2. In the formula (1), the ring Ar 1 and ring Ar 2 2. The photosensitive resin according to claim 1, wherein is a naphthalene ring.

3. In the formula (1), the ring Ar 3 3. The photosensitive resin according to claim 1, wherein is a biphenyl ring.

4. In the formula (2), A 3 C 2-43. The photosensitive resin according to claim 1, wherein X is an alkylene group, t is an integer of 0 to 10, and X is an alkyl group or a polymerizable substituent.

5. In the formula (2), A 3 C 2-4 3. The photosensitive resin according to claim 1, wherein X is an alkylene group, t is an integer of 1 to 10, and X is an alkenylcarbonyl group represented by the following formula (3): [C3] (In the formula, R 7 represents a hydrogen atom or an alkyl group)

6. The acid anhydride-modified fluorene-containing acrylic resin has a terminal of C 4-10 Cycloalkene ring or C 6-12 3. The photosensitive resin according to claim 1, which is terminated with a dicarboxylic acid anhydride having a bicycloalkene ring.

7. 3. The photosensitive resin according to claim 1, having an acid value of 20 to 200 mgKOH / g.

8. 3. The photosensitive resin according to claim 1, which has a weight average molecular weight of 5,000 or more.

9. 3. The method for producing a photosensitive resin according to claim 1, comprising reacting an acid anhydride-modified fluorene-containing acrylic resin having a repeating unit represented by formula (1) with an epoxy group-containing compound represented by formula (2).

10. A resin composition comprising the photosensitive resin according to claim 1 or 2 and a photopolymerization initiator.

11. A cured product obtained by curing the resin composition according to claim 10.

Citation Information

Patent Citations

  • Electromagnetic ultrasonic transducer

    JP1986075259A