Screw extruder and method for producing resin composition

The screw extruder's segmented reaction zone and strategic element placement enhance resin modification efficiency, addressing insufficient reaction time and reactant excess issues, achieving high-quality resin production with increased output.

JP2024144384APending Publication Date: 2024-10-11KANEKA CORP
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2024054827
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-30
Filing Date
2024-03-28
Publication Date
2024-10-11

AI Technical Summary

Technical Problem

Existing screw extruders face challenges in efficiently modifying raw resin compositions due to insufficient reaction time when increasing resin flow rates, often requiring excess reactant use and subsequent separation methods.

Method used

A screw extruder design with a preheating, mixing, reaction, homogenization, and delivery zones, featuring a divided reaction zone with seal rings and strategically placed flight and kneading elements, along with color elements in the reaction blocks to extend reaction time and prevent excessive temperature rise.

Benefits of technology

The design promotes efficient resin modification with increased production capacity while minimizing reactant usage, ensuring high-quality resin composition production without excess reactant treatment.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024144384000001_ABST
    Figure 2024144384000001_ABST
Patent Text Reader

Abstract

To provide a screw extruder capable of efficiently modifying a raw resin.SOLUTION: A screw extruder 1 for modifying a raw resin according to one embodiment of the present invention includes: a preheating zone Z1 for melting the raw resin; a mixing zone Z2 in which a reactant is mixed with the raw resin; and a reaction zone Z3 in which the raw resin and the reactant are reacted. The reaction zone Z3 is divided into a plurality of reaction blocks B by seal rings 25.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a screw extruder and a method for producing a resin composition. [Background technology]

[0002] There is a known method for producing a resin composition containing a resin whose properties are different from those of the raw resin by continuously modifying the raw resin using a screw extruder. The screw of the screw extruder is configured by attaching, for example, a flight element for moving the material, a kneading element for kneading, a seal ring for blocking the material, etc. to a shaft. In the screw extruder, a reactant is mixed with the molten raw resin, and kneading is performed in a zone having a kneading element, thereby reacting the raw resin with the reactant (for example, see Patent Document 1). [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Patent Publication No. 2021-62552 Summary of the Invention [Problem to be solved by the invention]

[0004] In order to increase the production amount, it is necessary to increase the flow rate of the resin inside the screw extruder, and the time to pass through the kneading zone is shortened, which may result in insufficient reaction. When a resin composition is produced by mixing a reactant with a raw resin, the reaction time can be shortened by increasing the amount of the reactant injected. However, since it may be necessary to separate the excessively injected reactant and dispose of the separated reactant by a method such as combustion, it is desirable to modify the raw resin without using an excessive amount of the reactant. Therefore, the object of the present invention is to provide a screw extruder and a method for producing a resin composition that can efficiently modify the raw resin. [Means for solving the problem]

[0005] A screw extruder according to one embodiment of the present invention is a screw extruder that modifies a raw resin, and is provided with a preheating zone that melts the raw resin, a mixing zone that mixes a reactant with the raw resin, and a reaction zone that reacts the raw resin with the reactant, and the reaction zone is divided into a plurality of reaction blocks by sealing rings.

[0006] In the above-mentioned screw extruder, the reaction blocks may each have a flight element, a color element, and a kneading element.

[0007] In the above-mentioned screw extruder, the reaction block may have, from the mixing zone side, the flight element, the color element, and the kneading element in this order.

[0008] In the above-mentioned screw extruder, the color elements may be disposed only in the reaction block.

[0009] In the above-mentioned screw extruder, the color elements may be disposed only in the reaction block.

[0010] The above-mentioned screw extruder may further include at least one of a homogenization zone for stirring and homogenizing the resin, and a delivery zone for delivering the resin, downstream of the reaction zone.

[0011] The above-mentioned screw extruder may further include, downstream of the reaction zone, a homogenization zone for stirring and homogenizing the resin, and a delivery zone for delivering the resin, in this order.

[0012] In the method for producing a resin composition according to another embodiment of the present invention, the reactants may be mixed with the raw resin by using the above-mentioned screw extruder to cause the reaction.

[0013] In the above-mentioned method for producing a resin composition, the raw material resin may be an acrylic resin, and the reactant may be an imidizing agent. Effect of the Invention

[0014] According to the screw extruder and the method for producing a resin composition of the present invention, the raw material resin can be efficiently modified. [Brief description of the drawings]

[0015] [Figure 1] FIG. 1 is a schematic diagram showing a configuration of a screw extruder according to one embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0016] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. Note that the dimensions of various members in the drawings are adjusted for ease of viewing. Fig. 1 is a schematic diagram showing the configuration of a screw extruder 1 according to one embodiment of the present invention.

[0017] The screw extruder 1 is used to modify a raw material resin. The screw extruder 1 may be a multi-screw extruder, and is typically a twin-screw extruder. The screw extruder 1 includes a barrel 10 and a screw 20 inserted into the barrel.

[0018] The barrel 10 has a main feed port 11 through which pellets of raw resin are supplied, a side feed port 12 through which a reactant for modifying the raw resin is supplied, and a discharge port 13 through which a resin composition obtained by modifying the raw resin is discharged. A metering feeder 31 for supplying pellets of the raw resin is connected to the main feed port 11. A supply line 32 for supplying a liquid or gaseous reactant is connected to the side feed port 12. A pipe or the like for sending the modified resin composition to the next process may be connected to the discharge port 13. A well-known component such as a breaker plate may be disposed in the discharge port 13.

[0019] The screw 20 has a shaft 21, and flight elements 22, kneading elements 23, color elements 24, and a seal ring 25 attached to the shaft 21. The flight elements 22 move the resin downstream. The kneading elements 23 knead the resin. The color elements 24 allow the resin to pass through with as little force as possible. The seal ring 25 blocks the resin and provides resistance to its passage.

[0020] The screw extruder 1 defines a resin flow path by the barrel 10 and the screw 20. The flow path of the screw extruder 1 includes a preheating zone Z1 for melting the raw resin, a mixing zone Z2 for mixing (dispersing and dissolving) a reactant into the raw resin, a reaction zone Z3 for reacting the raw resin with the reactant, a homogenization zone Z4, and a delivery zone Z5 as a plurality of flow path sections through which the resin passes in sequence.

[0021] The preheating zone Z1 has a main feed port 11 and may be configured to include a plurality of flight elements 22. In the preheating zone Z1, pellets of the raw material resin are heated and melted by the conveying pressure of the flight elements 22 and the radiant heat of the cylinder of the extruder.

[0022] The mixing zone Z2 has a side feed port 12 and may be configured to include a plurality of kneading elements 23. The mixing zone Z2 is preferably configured to include a flight element 22 in the center. By providing the flight element 22 between the kneading elements 23, it is possible to prevent the temperature of the resin composition from rising excessively.

[0023] The reaction zone Z3 is divided into a plurality of reaction blocks B, preferably three or more, by seal rings 25. That is, each reaction block B is a section sandwiched between two seal rings 25. The reaction block B includes at least one kneading element 23, and preferably includes flight elements 22 and color elements 24. More specifically, the reaction block B preferably includes one or more flight elements 22, one or more color elements 24, and one or more kneading elements 23 in this order. Also, in the reaction block B, when a large number of kneading elements 23 are provided, as in the mixing zone Z2, it is preferable to provide color elements 24 between the kneading elements 23. That is, the reaction block B may include flight elements 22, and repetitions of color elements 24 and kneading elements 23.

[0024] Since the color elements 24 do not have protrusions acting on the resin composition, they form a flow path with a relatively large volume. Therefore, by disposing the color elements 24 in the reaction zone Z3, the residence time of the resin can be increased, and the reaction of the resin composition can be promoted. In addition, by disposing the color elements 24 between the kneading elements 23, the temperature of the resin composition can be prevented from rising excessively. In other words, by disposing the color elements 24 in the reaction zone Z3, the number of kneading elements 23 can be increased to more effectively promote the modification reaction, and discoloration of the resin composition can be suppressed.

[0025] The homogenization zone Z4 includes a kneading element 23 and homogenizes the reacted resin composition by stirring it. The homogenization zone Z4 is also preferably sandwiched between seal rings 25 in order to maintain pressure and improve stirring efficiency.

[0026] The delivery zone Z5 has flight elements 22 and delivers the resin composition to the next process. The number of flight elements 22 in the delivery zone Z5 is selected depending on the pressure required for supplying the resin composition to the next process. The next process may include further modification such as esterification, mixing with additives such as lubricants, ultraviolet absorbers, and antioxidants, mixing with other resins, and the like.

[0027] In the screw 20, the color element 24 is provided in the reaction block B to ensure reaction time. On the other hand, even if the color element 24 is provided in the preheating zone Z1, the mixing zone Z2, the homogenization zone Z4 and the delivery zone Z5, no advantageous effect can be obtained and the length of the shaft 21 is meaninglessly occupied. For this reason, it is preferable that the color element 24 is provided only in the reaction block B.

[0028] The screw extruder 1 having the above-described configuration is provided with a reaction zone Z3 having a plurality of reaction blocks B whose residence time is increased by the color elements 24, thereby effectively promoting the modification reaction and efficiently modifying the raw resin, thereby making it possible to increase the production amount without supplying an excess of reactants.

[0029] As is clear from the above description, one embodiment of the method for producing a resin composition according to the present invention involves mixing and reacting a raw material resin with a reactant by the above-mentioned screw extruder 1. More specifically, the method for producing a resin composition according to one embodiment of the present invention includes a step of melting the raw material resin (melting step), a step of mixing the raw material resin with a reactant (mixing step), and a step of promoting a modification reaction of the raw material resin (reaction promotion step).

[0030] (Melting process) In the melting step, the pellet-shaped raw resin is melted in the preheating zone Z1 of the screw extruder 1. The raw resin is supplied to the main feed port 11 of the screw extruder 1 by a metering feeder 31. The raw resin is not particularly limited, but examples of the raw resin that can be used include maleimide resin and acrylic resin. As the raw acrylic resin, for example, a homopolymer of methyl (meth)acrylate, a (meth)acrylic acid ester-aromatic vinyl copolymer, and the like are suitably used.

[0031] (Mixing process) In the mixing step, the reactant is supplied to the side feed port 12 of the screw extruder 1 through the supply line 32, and is mixed into the molten raw material resin by stirring with the kneading element 23 in the mixing zone Z2 of the screw extruder 1. As the reactant, for example, an imidizing agent, alcohol, etc. can be used.

[0032] As the reactant, typically, an imidizing agent that imparts positive birefringence to the acrylic resin is used. Examples of the imidizing agent include aliphatic hydrocarbon group-containing amines such as ammonia, monomethylamine, ethylamine, n-propylamine, i-propylamine, n-butylamine, i-butylamine, tert-butylamine, and n-hexylamine, aromatic hydrocarbon group-containing amines such as aniline, benzylamine, toluidine, and trichloroaniline, and alicyclic hydrocarbon group-containing amines such as cyclohexylamine. In addition, urea-based compounds that generate the amines exemplified above by heating, such as urea, 1,3-dimethylurea, 1,3-diethylurea, and 1,3-dipropylurea, can also be used. Among these imidizing agents, it is preferable to use monomethylamine, ammonia, and cyclohexylamine in terms of cost and physical properties, and it is particularly preferable to use monomethylamine. In addition, monomethylamine and the like that are gaseous at room temperature may be used in a state dissolved in alcohols such as methanol. In the mixing step, in addition to the reactants, a catalyst such as a ring closure promoter may be added, if necessary.

[0033] (Reaction promotion step) In the reaction promotion step, in the reaction zone Z3 of the screw extruder 1, retention by the color elements 24 to ensure reaction time and kneading by the kneading elements 23 to promote the modification reaction are repeated.

[0034] The resin temperature in the reaction zone Z3 of the screw extruder 1 can be appropriately set according to the type and molecular weight of the resin used, but when the resin is set to the glass transition temperature (Tg), it is preferably Tg+50°C or higher, more preferably Tg+60°C or higher. On the other hand, the upper limit of the resin temperature in the reaction zone Z3 is preferably Tg+160°C or lower, more preferably Tg+150°C or lower. By setting it in this range, the reaction of the resin can be effectively promoted. For example, the lower limit of the resin temperature is preferably 180°C, more preferably 200°C. On the other hand, the upper limit of the resin temperature in the reaction zone Z3 is preferably 280°C, more preferably 260°C. By setting the resin temperature in the reaction zone Z3 to the lower limit or higher, when an acrylic resin is used as the resin, the imidization reaction can be effectively promoted. In addition, by setting the resin temperature in the reaction zone Z3 to the upper limit or lower, decomposition of the resin can be suppressed, and the strength of the finally obtained resin composition can be prevented from being impaired.

[0035] The lower limit of the residence time of the resin in the reaction zone Z3 is preferably 10 seconds, more preferably 30 seconds. On the other hand, the upper limit of the residence time of the resin in the reaction zone Z3 is preferably 180 seconds, more preferably 60 seconds. By making the residence time of the resin in the reaction zone Z3 equal to or greater than the lower limit, the reactants can be sufficiently reacted with the raw material resin. In addition, by making the residence time of the resin in the reaction zone Z3 equal to or less than the upper limit, the flow rate of the resin and therefore the production amount of the resin composition can be increased.

[0036] The lower limit of the resin pressure (relative pressure) in the reaction zone Z3 is preferably 0.5 MPa, more preferably 1.0 MPa. On the other hand, the upper limit of the resin pressure in the reaction zone Z3 is preferably 50 MPa, more preferably 10 MPa. By setting the resin pressure in the reaction zone Z3 to the lower limit or more, the dissolution of the reactants can be promoted and the reaction rate can be improved. In addition, by setting the resin pressure in the reaction zone Z3 to the upper limit or less, it is possible to prevent unnecessary increases in equipment costs due to the pressure resistance of the screw extruder 1.

[0037] The resin production method of this embodiment, which uses the screw extruder 1 capable of efficiently modifying the raw resin, can increase the production amount without supplying an excess of reactants, and therefore can efficiently produce a high-quality resin composition.

[0038] Although the embodiment of the present invention has been described above, the present invention is not limited to the above-mentioned embodiment, and various modifications and variations are possible. For example, in the screw extruder according to the present invention, the homogenization zone and the delivery zone are not essential. [Explanation of symbols]

[0039] 1. Screw extruder 10 barrels 11 Main feed port 12 Side feed port 13 Outlet 20 Screw 21 Shaft 22 Flight Element 23 Kneading element 24 Color Elements 25 Seal ring 31 Weigh Feeder 32 Supply Line B Reaction block Z1 Preheat Zone Z2 Mixed Zone Z3 Reaction Zone Z4 Homogenization Zone Z5 Sending Zone

Claims

1. A screw extruder for modifying a raw material resin, a preheating zone for melting the raw resin; a mixing zone for mixing the raw resin with a reactant; a reaction zone in which the raw resin and a reactant are reacted; Equipped with A screw extruder, wherein the reaction zone is divided into a plurality of reaction blocks by seal rings.

2. 2. The screw extruder of claim 1, wherein the reaction blocks each include a flight element, a color element, and a kneading element.

3. 3. The screw extruder according to claim 2, wherein the reaction block has, from the mixing zone side, the flight element, the color element, and the kneading element in this order.

4. 3. The screw extruder of claim 2, wherein the color elements are disposed only in the reaction block.

5. The screw extruder according to any one of claims 1 to 4, further comprising at least one of a homogenization zone for stirring and homogenizing a resin and a delivery zone for delivering a resin downstream of the reaction zone.

6. The screw extruder according to any one of claims 1 to 4, further comprising, downstream of the reaction zone, a homogenization zone for stirring and homogenizing the resin, and a delivery zone for delivering the resin, in this order.

7. A method for producing a resin composition, comprising mixing a raw material resin with a reactant and reacting the raw material resin with the screw extruder according to any one of claims 1 to 4.

8. The method for producing a resin composition according to claim 7, wherein the raw material resin is an acrylic resin, and the reactant is an imidizing agent.

Citation Information

Patent Citations

  • Double-screw kneading extruder

    JP1992189106A

  • Imide resin with excellent molding stability and method for producing imide resin

    JP2008285615A

  • Imide resin, production method of the same, and usage of the same

    JP2013231188A

  • Twin screw extruder with thread-free mixing zones

    US4900156A

  • Method of producing resin composition and screw type kneading devolatilization extruder

    JP2021062552A