Butt joint structure and compactor

The butt joint structure with a relief part on the opposite side to the heat source in keyhole welding addresses hot cracking issues by improving molten metal flow, thereby enhancing weld integrity and reducing processing loads.

JP2024146026AInactive Publication Date: 2024-10-15DAIKIN INDUSTRIES LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023058689
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-31
Publication Date
2024-10-15
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Keyhole welding of aluminum or aluminum alloy materials is prone to hot cracking, particularly as penetration depth increases, due to poor flow of molten metal and residual stress.

Method used

A butt joint structure with a relief part on the opposite side to the heat source, filled by welding, to improve molten metal flow and reduce the risk of hot cracking, with a cross-sectional area of the relief part not exceeding 1 mm².

Benefits of technology

The structure effectively reduces the occurrence of hot cracking and blowholes by enhancing molten metal flow, maintaining weld integrity and reducing processing loads.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024146026000001_ABST
    Figure 2024146026000001_ABST
Patent Text Reader

Abstract

To reduce a risk of a hot crack in keyhole welding.SOLUTION: A butt joint structure has, in two or more members which are subjected to keyhole welding, an escape part 173 for a metal flow in a side opposite to a side to which is irradiated with a high energy beam 100 as a heat source, and the escape part 173 is buried with keyhole welding.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a butt joint structure and a compressor. [Background technology]

[0002] Patent Document 1 describes that in laser welding of aluminum or aluminum alloy materials, grooves are provided to allow metal vapor, hydrogen, and the like generated during welding to be discharged to the outside. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Japanese Patent Application Publication No. 10-156564 Summary of the Invention [Problem to be solved by the invention]

[0004] Keyhole welding entails the risk of hot cracking, which is caused by defects that can occur during the solidification process of the molten metal. It is also known that the risk of hot cracking increases the deeper the penetration of the molten metal. The present disclosure aims to reduce the risk of hot cracking in keyhole welding. [Means for solving the problem]

[0005] The butt joint structure of the present disclosure that achieves the above object is characterized in that two or more members to be keyhole welded have a relief portion for molten metal flow on the opposite side to the side where the heat source is irradiated, and the relief portion is filled by welding. In this case, the risk of hot cracking in keyhole welding can be reduced. Here, the two or more members may be provided with at least one of a fitting portion that fits with the other member and a contact portion that contacts the other member, and the escape portion for avoiding interference between the fitting portion and the contact portion may be formed in one of the two or more members. In this case, since there is a width at the position where the escape portion for the flow of molten metal is provided, the processing burden is reduced. In addition, the cross-sectional area of ​​the space forming the recess is 1 mm 2 If the cross-sectional area of ​​the space that forms the escape for the molten metal flow is too large, poor penetration is likely to occur. 2 If it does not exceed this value, poor penetration is unlikely to occur, and the risk of hot cracking can be reduced. The two or more members may be members having a circumference, and the recess may be formed in the direction of the circumference. In this case, the present invention is applicable not only to rectangular plate materials and square materials, but also to tubular members. The butt joint structure of the present disclosure, which achieves the above object, is a compressor characterized in that two or more members to be keyhole welded have a relief portion for molten metal flow on the opposite side to the side to which the heat source is irradiated, and the relief portion is filled by the welding. In this case, the risk of hot cracking in keyhole welding can be reduced. [Brief description of the drawings]

[0006] [Figure 1] 1A to 1D are diagrams showing specific examples of a butt joint structure according to the present embodiment. [Diagram 2] 1A to 1C are diagrams showing a specific example of a butt joint structure according to the present embodiment. [Diagram 3] 1A and 1B are diagrams showing a specific example of a location where keyhole welding according to the present embodiment has been performed. [Figure 4] 1(A) and 1(B) are diagrams showing a specific example of a hot crack, which is an example of a welding defect. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0007] Hereinafter, embodiments will be described in detail with reference to the accompanying drawings. <Keyhole welding> First, we will explain keyhole welding. Keyhole welding is a type of butt welding that joins two or more components on the same plane by irradiating a high-energy beam such as a laser beam or an electron beam (hereinafter referred to as "high-energy beam welding"). Specifically, high-energy beam welding is a welding technique in which a high-energy beam is irradiated toward the metal to be welded, melting the metal locally and then solidifying it to join the metal.

[0008] Keyhole welding is a so-called deep penetration type of high energy beam welding, in which a high energy beam such as a laser beam or an electron beam with high energy density is irradiated onto a metal to melt and evaporate the metal, forming a deep depression (keyhole) in the metal. When a keyhole is formed in the metal, the irradiated high energy beam reaches the inside of the metal. Therefore, keyhole welding enables deep penetration welding, in other words, welding with a long distance between the deepest position of the part where the members are melted by irradiation with the high energy beam and the surface of the welded surface. Keyhole welding is used, for example, to join flat plates together or to join pipes.

[0009] Keyhole welding can be performed either by placing a so-called backing metal such as a metal or ceramic (hereinafter referred to as a "backing material") on the members to be welded, or by not placing a backing material on the members to be welded. When keyhole welding is performed with a backing material on the members to be welded, it is common to perform welding after subjecting the weld to simple processing in order to avoid interference between the members at the weld or to ensure the strength and quality of the weld. Examples of simple processing performed on the weld include chamfering to remove convex parts such as burrs, and groove processing to cut or trim the end of the member to be welded into a shape suitable for welding.

[0010] When high-energy beam welding is performed as keyhole welding by placing a backing material on the components to be welded, the beam does not penetrate the components to be welded, which creates a risk of weld defects. In contrast, full penetration welding, which penetrates the components to be welded, creates a risk of defects such as spatter (molten metal particles contained in sparks generated during welding) scattering and adhering to the components, because the high-energy beam penetrates the components. Thus, there are two types of keyhole welding: full penetration and non-perforation, and both types involve risks, but full penetration welding is often chosen.

[0011] Hot cracks and blowholes are examples of welding defects that may occur when non-penetration welding is selected as keyhole welding. "Hot cracks" refer to cracks that occur during the process of solidifying the metal of the weld. Figures 4(A) and (B) show specific examples of hot cracks, which are an example of welding defects. The frames 200 shown in Figures 4(A) and (B) each show the location of hot cracks that occurred during conventional keyhole welding. Hot cracks lead to a decrease in the performance of the welded joint. In addition, costs increase when welding is performed for rework. "Blowholes" refer to gases that are generated in the weld metal or that have entered the weld metal and are trapped in the weld metal when the molten metal solidifies, rather than being released into the atmosphere. If a load is applied to a component with blowholes, it may cause breakage or rupture.

[0012] One of the causes of welding defects is poor flow of molten metal. "Flow of molten metal" refers to the flow of metal molten by the heat of a high-energy beam filling the inside of a keyhole. The manner in which the flow of molten metal changes is affected by residual stress, material components, groove shape, welding heat input, etc. Residual stress refers to the internal force that resists an external force remaining in a component after the external force applied to it is removed. Groove shape refers to the shape of the part where groove preparation has been performed. Welding heat input refers to the amount of heat applied to the weld from the outside during welding.

[0013] For example, if the temperature of the molten metal becomes lower than intended due to the influence of residual stress, material components, groove shape, welding heat input, etc., the molten metal may solidify during the flow, causing hot cracks, or gas may be entrained in the molten metal, causing blowholes. In keyhole welding, the deeper the penetration, the higher the risk of hot cracks.

[0014] <Butt joint structure> 1(A) to (D) and 2(A) to (C) are diagrams showing a specific example of a butt joint structure according to this embodiment. In the following description, the side irradiated with a high-energy beam 100, which is a heat source, is called the "irradiation side", and the opposite side to the side irradiated with the high-energy beam 100 is called the "opposite irradiation side". In addition, metals other than aluminum alloy materials can be used for the two or more members that are the targets of the butt joint structure according to this embodiment. In this case, for example, SB410, an alloy of iron and carbon, etc., is used.

[0015] In the butt joint structure according to the present embodiment, a melt flow escape is provided on the opposite side of at least one of the two or more components to be keyhole welded. The "melt flow escape" refers to a space for escaping molten metal. By providing a melt flow escape on the opposite side, melt flow in the vicinity of a position where a welding defect may occur is improved. As a result, the risk of occurrence of welding defects such as hot cracks and blowholes is reduced.

[0016] In the butt joint structure according to the present embodiment, the escape portion for the molten metal flow provided on the opposite side is filled by the melting of the metal during keyhole welding. That is, the space as the escape portion is filled with the molten metal and disappears. Therefore, even if the escape portion for the molten metal flow is formed before welding, it does not become a factor that reduces the strength of the welded portion after welding.

[0017] The left diagram of FIG. 1(A) is a diagram showing the external configuration of a first member 11 among two or more members to be keyhole welded. The right diagram of FIG. 1(A) is a diagram showing a state in which the first member 11 and a second member 12 to be keyhole welded to the first member 11 are butted together. As shown in the left diagram of FIG. 1(A), the first member 11 is a metal plate having a first surface 111, a second surface 112, a third surface 113, a fourth surface 114, a fifth surface 115, and a sixth surface 116. As shown in the right diagram of FIG. 1(A), the second member 12 is a metal plate having a first surface 121, a second surface 122, a third surface 123, a fourth surface 124, a fifth surface 125, and a sixth surface 126.

[0018] A fitting portion 117 is formed between the first surface 111 and the fifth surface 115 of the first member 11. The fitting portion 117 has a welding surface 171, a backing portion 172, and a relief portion 173. The welding surface 171 is a portion that is welded to the fifth surface 125 of the second member 12, and constitutes a welded portion together with the fifth surface 125 of the second member 12. The backing portion 172 functions as a backing material in keyhole welding, and is a portion that is welded to the second surface 122 of the second member 12.

[0019] The clearance 173 is a groove formed to form a space when the first member 11 and the second member 12 are butted together. The cross section of the clearance 173 shown in FIG. 1(A) is a substantially circular shape with a portion missing. The cross-sectional area of ​​the clearance 173 is 1 mm 2 The relief portion 173 functions as a space for allowing the molten metal to escape during keyhole welding and improving the flow of the molten metal.

[0020] When a high-energy beam 100 is irradiated toward the end of the weld on the irradiation side, the weld is keyhole welded. At this time, the molten metal is allowed to escape to a relief portion 173 formed on the opposite side to the irradiation, improving the flow of the molten metal. The molten metal allowed to escape to the relief portion 173 fills the space in the relief portion 173.

[0021] The left diagram of FIG. 1(B) is a diagram showing the external configuration of a first member 21 among two or more members to be keyhole welded. The right diagram of FIG. 1(B) is a diagram showing a state in which the first member 21, the second member 22 to be keyhole welded to the first member 21, and the third member 23 as a backing member are butted together. As shown in the left diagram of FIG. 1(B), the first member 21 is a metal plate having a first surface 211, a second surface 212, a third surface 213, a fourth surface 214, a fifth surface 215, and a sixth surface 216. As shown in the right diagram of FIG. 1(B), the second member 22 is a metal plate having a first surface 221, a second surface 222, a third surface 223, a fourth surface 224, a fifth surface 225, and a sixth surface 226. The third member 23 is a metal plate having a first surface 231, a second surface 232, a third surface 233, a fourth surface 234, a fifth surface 235, and a sixth surface 236.

[0022] The fifth surface 215 of the first member 21 constitutes a welding surface, and a relief portion 273 is formed between the second surface 212 and the fifth surface 215. The fifth surface 215 is a portion that is welded to the fifth surface 225 of the second member 22, and constitutes a welded portion together with the fifth surface 225 of the second member 22. The relief portion 273 is a portion that is notched so as to form a space when the first member 21, the second member 22, and the third member 23 are butted together. The cross section of the relief portion 273 shown in FIG. 1(B) is triangular. The cross-sectional area of ​​the relief portion 273 is 1 mm 2 The relief portion 273 functions as a space for allowing the molten metal to escape during keyhole welding and improving the flow of the molten metal.

[0023] When a high-energy beam 100 is irradiated toward the end of the irradiated side of the weld, the weld is keyhole welded. At this time, the molten metal is allowed to escape to the escape portion 273 formed on the opposite side of the irradiated side, improving the flow of the molten metal. The molten metal allowed to escape to the escape portion 273 fills the space in the escape portion 273.

[0024] The left diagram of FIG. 1(C) is a diagram showing the external configuration of a first member 31 among two or more members to be keyhole welded. The right diagram of FIG. 1(C) is a diagram showing a state in which the first member 31, a second member 32 to be keyhole welded to the first member 31, and a third member 33 as a backing member are butted together. As shown in the left diagram of FIG. 1(C), the first member 31 is a metal plate having a first surface 311, a second surface 312, a third surface 313, a fourth surface 314, a fifth surface 315, and a sixth surface 316. As shown in the right diagram of FIG. 1(C), the second member 32 is a metal plate having a first surface 321, a second surface 322, a third surface 323, a fourth surface 324, a fifth surface 325, and a sixth surface 326. The third member 33 is a metal plate having a first surface 331, a second surface 332, a third surface 333, a fourth surface 334, a fifth surface 335, and a sixth surface 336.

[0025] The fifth surface 315 of the first member 31 constitutes a welding surface, and a relief portion 373 is formed between the second surface 312 and the fifth surface 315. The fifth surface 315 is a portion that is welded to the fifth surface 325 of the second member 32, and constitutes a welded portion together with the fifth surface 325 of the second member 32. The relief portion 373 is a portion that is curved so as to form a space when the first member 31, the second member 32, and the third member 33 are butted together. The cross section of the relief portion 373 shown in FIG. 1(C) is a curved, approximately triangular shape. The cross-sectional area of ​​the relief portion 373 is 1 mm 2 The relief portion 373 functions as a space for allowing the molten metal to escape during keyhole welding and improving the flow of the molten metal.

[0026] When the high energy beam 100 is irradiated toward the end of the weld on the irradiation side, the weld is keyhole welded. At this time, the molten metal is allowed to escape to the escape portion 373 formed on the opposite side to the irradiation, improving the flow of the molten metal. The molten metal allowed to escape to the escape portion 373 fills the space in the escape portion 373.

[0027] The left diagram of FIG. 1(D) is a diagram showing the external configuration of a first member 41 among two or more members to be keyhole welded. The right diagram of FIG. 1(D) is a diagram showing a state in which the first member 41, a second member 42 to be keyhole welded to the first member 41, and a third member 43 as a backing member are butted together. As shown in the left diagram of FIG. 1(D), the first member 41 is a metal plate having a first surface 411, a second surface 412, a third surface 413, a fourth surface 414, a fifth surface 415, and a sixth surface 416. As shown in the right diagram of FIG. 1(D), the second member 42 is a metal plate having a first surface 421, a second surface 422, a third surface 423, a fourth surface 424, a fifth surface 425, and a sixth surface 426. The third member 43 is a metal plate having a first surface 431, a second surface 432, a third surface 433, a fourth surface 434, a fifth surface 435, and a sixth surface 436.

[0028] The fifth surface 415 of the first member 41 constitutes a welding surface, and a relief portion 473 is formed between the second surface 412 and the fifth surface 415. The fifth surface 415 is a portion that is welded to the fifth surface 425 of the second member 42, and constitutes a welded portion together with the fifth surface 425 of the second member 42. The relief portion 473 is a portion that is notched so as to form a space when the first member 41, the second member 42, and the third member 43 are butted together. The cross section of the relief portion 473 shown in FIG. 1(D) is rectangular. The cross-sectional area of ​​the relief portion 473 is 1 mm 2 The relief portion 473 functions as a space for allowing the molten metal to escape during keyhole welding and improving the flow of the molten metal.

[0029] When a high-energy beam 100 is irradiated toward the end of the weld on the irradiation side, the weld is keyhole welded. At this time, the molten metal is allowed to escape to a relief portion 473 formed on the opposite side of the weld, improving the flow of the molten metal. The molten metal allowed to escape to the relief portion 473 fills the space in the relief portion 473.

[0030] The left diagram of FIG. 2(A) is a diagram showing the external configuration of a third member 53 as a backing member among two or more members to be keyhole welded. The right diagram of FIG. 2(A) is a diagram showing a state in which a first member 51, a second member 52 to be keyhole welded to the first member 51, and a third member 53 are butted together. As shown in the right diagram of FIG. 2(A), the first member 51 is a metal plate having a first surface 511, a second surface 512, a third surface 513, a fourth surface 514, a fifth surface 515, and a sixth surface 516. The second member 52 is a metal plate having a first surface 521, a second surface 522, a third surface 523, a fourth surface 524, a fifth surface 525, and a sixth surface 526. Also, as shown in the left diagram of Figure 2(A), the third member 53 is a metal plate having a first surface 531, a second surface 532, a third surface 533, a fourth surface 534, a fifth surface 535, and a sixth surface 536.

[0031] The fifth surface 515 of the first member 51 and the fifth surface 525 of the second member 52 form a welded portion to be keyhole welded. A relief portion 573 is formed on the first surface 531 of the third member 53. The relief portion 573 is a grooved portion that forms a space when the first member 51, the second member 52, and the third member 53 are butted together. The cross section of the relief portion 573 shown in FIG. 2(A) is rectangular. The cross-sectional area of ​​the relief portion 573 is 1 mm 2 The relief portion 573 functions as a space for allowing the molten metal to escape during keyhole welding and improving the flow of the molten metal.

[0032] When a high-energy beam 100 is irradiated toward the end of the weld on the irradiation side, the weld is keyhole welded. At this time, the flow of the molten metal is improved by allowing the molten metal to escape to the escape portion 573 formed on the opposite side to the irradiation. The molten metal that has escaped to the escape portion 573 fills the space in the escape portion 573.

[0033] The left diagram of FIG. 2(B) is a diagram showing the external configuration of a third member 63 as a backing member among two or more members to be keyhole welded. The right diagram of FIG. 2(A) is a diagram showing a state in which a first member 61, a second member 62 to be keyhole welded to the first member 61, and a third member 63 are butted together. As shown in the right diagram of FIG. 2(B), the first member 61 is a metal plate having a first surface 611, a second surface 612, a third surface 613, a fourth surface 614, a fifth surface 615, and a sixth surface 616. The second member 62 is a metal plate having a first surface 621, a second surface 622, a third surface 623, a fourth surface 624, a fifth surface 625, and a sixth surface 626. Also, as shown in the left diagram of Figure 2(B), the third member 63 is a metal plate having a first surface 631, a second surface 632, a third surface 633, a fourth surface 634, a fifth surface 635, and a sixth surface 636.

[0034] The fifth surface 615 of the first member 61 and the fifth surface 625 of the second member 62 form a welded portion to be keyhole welded. A relief portion 673 is formed on the first surface 631 of the third member 63. The relief portion 673 is a grooved portion that forms a space when the first member 61, the second member 62, and the third member 63 are butted together. The cross section of the relief portion 673 shown in FIG. 2(B) is half-moon shaped. The cross-sectional area of ​​the relief portion 673 is 1 mm 2 The relief portion 673 functions as a space for allowing the molten metal to escape during keyhole welding and improving the flow of the molten metal.

[0035] When a high-energy beam 100 is irradiated toward the end of the irradiated side of the weld, the weld is keyhole welded. At this time, the flow of the molten metal is improved by allowing the molten metal to escape to the escape portion 673 formed on the opposite side of the irradiated side. The molten metal that has escaped to the escape portion 673 fills the space in the escape portion 673.

[0036] The left diagram of FIG. 2(C) is a diagram showing the external configuration of a first member 71 among two or more members to be keyhole welded. The right diagram of FIG. 2(C) is a diagram showing a state in which the first member 71 and a second member 72 to be keyhole welded to the first member 71 are butted together. As shown in the left diagram of FIG. 2(C), the first member 71 is a metal plate having a first surface 711, a second surface 712, a third surface 713, a fourth surface 714, a fifth surface 715, and a sixth surface 716. As shown in the right diagram of FIG. 2(C), the second member 72 is a metal plate having a first surface 721, a second surface 722, a third surface 723, a fourth surface 724, a fifth surface 725, and a sixth surface 726.

[0037] A fitting portion 717 is formed between the first surface 711 and the fifth surface 715 of the first member 71. The fitting portion 717 has a welding surface 741 and a backing portion 742. The welding surface 741 is a portion that is welded to the fifth surface 725 of the second member 72, and constitutes a welded portion together with the fifth surface 725 of the second member 72. The backing portion 742 functions as a backing material in keyhole welding, and is a portion that forms a space together with a relief portion 773 of the second member 72.

[0038] The fifth surface 725 of the second member 72 constitutes a welding surface, and a relief portion 773 is formed between the second surface 722 and the fifth surface 725. The relief portion 773 is a portion that is cut out so as to form a space when the first member 71 and the second member 72 are butted together. The cross section of the relief portion 773 shown in FIG. 2(C) is triangular. The cross-sectional area of ​​the relief portion 773 is 1 mm 2 The relief portion 773 functions as a space for allowing the molten metal to escape during keyhole welding and improving the flow of the molten metal.

[0039] When a high-energy beam 100 is irradiated toward the end of the irradiated side of the weld, the weld is keyhole welded. At this time, the flow of the molten metal is improved by allowing the molten metal to escape to the escape portion 773 formed on the opposite side of the irradiated side. The molten metal that has escaped to the escape portion 773 fills the space in the escape portion 773.

[0040] 3(A) and (B) are diagrams showing specific examples of locations where keyhole welding according to this embodiment has been performed. 3(A) and (B), by performing keyhole welding according to this embodiment, the occurrence of welding defects such as hot cracks and blowholes in the metal solidified in the keyhole is suppressed. Note that in the keyhole welding according to this embodiment, welding of about 8 mm (millimeters) to 16 mm (millimeters), for example, is assumed. <Other embodiments> In addition, the configurations described above are not limited to the above-described embodiments and their modifications, and can be modified without departing from the spirit of the invention. In other words, it is understood that various modifications of the form and details are possible without departing from the spirit and scope of the claims. The present invention is not limited to the above-described configurations, and some of the configurations described above may be omitted, or other functions may be added to the configurations described above. Further, although multiple embodiments have been described above, the configurations included in one embodiment may be interchanged with the configurations included in other embodiments, or the configurations included in one embodiment may be added to other embodiments.

[0041] For example, the specific examples shown in Figures 1(A) to (D) and Figures 2(A) to (C) show a specific example in which metal plate materials are welded as the two or more components to be keyhole welded, but the two or more components to be keyhole welded are not limited to plate materials. For example, the two or more components to be keyhole welded may be components having a circumference. In this case, an escape portion for the molten metal flow may be formed in the circumferential direction. An example of a "component having a circumference" is a metal pipe.

[0042] In addition, the use of the butt joint structure according to the above-mentioned embodiment is not particularly limited. For example, it may be adopted in a compressor that is provided in the refrigerant circuit of an air conditioner and compresses a refrigerant as a fluid. Although not shown in the figure, an example of a compressor having the butt joint structure according to the above-mentioned embodiment is a compressor having an electric motor that converts electric energy into mechanical energy, a compression mechanism that compresses the refrigerant as a fluid, a body pipe as a casing that houses the electric motor and the compression mechanism, a suction pipe that takes in low-pressure refrigerant, and a discharge pipe that sends the refrigerant compressed by the compression mechanism to the outside.

[0043] Here, each of the embodiments described above can be understood as follows. That is, in the butt joint structure of the present disclosure, two or more members to be keyhole welded (for example, first member 11 and second member 12 in FIG. 1(A)) have a molten metal flow escape (for example, escape 173 in FIG. 1(A)) on the opposite side to where high-energy beam 100 as a heat source is irradiated, and the molten metal flow escape is filled by keyhole welding. In this case, the risk of hot cracking in keyhole welding can be reduced.

[0044] Here, at least one of a fitting portion that fits with the other (e.g., fitting portion 117 in FIG. 1(A)) and a contact portion that comes into contact with the other (e.g., fifth surface 115 in FIG. 1(A)) may be provided on the two or more components to be keyhole welded, and a molten metal flow escape portion for avoiding interference between the fitting portion and the contact portion may be formed on any of the two or more components to be keyhole welded. In this case, since there is a width at the position where the escape portion for the molten metal flow is provided, the processing burden is reduced.

[0045] In addition, the cross-sectional area of ​​the space that forms the escape area for the molten metal flow is 1 mm 2 If the cross-sectional area of ​​the space that forms the escape for the molten metal flow is too large, poor penetration is likely to occur. 2 If it does not exceed this value, poor penetration is unlikely to occur, and the risk of hot cracking can be reduced.

[0046] In addition, the two or more components to be keyhole welded may have a circumference, and the escape portion for the molten metal flow may be formed in the circumferential direction. In this case, the method can be applied not only to rectangular plate materials and square materials, but also to tubular members.

[0047] Furthermore, the compressor of the present disclosure, which achieves the above object, has a butt joint structure in which two or more members (e.g., first member 11 and second member 12 in FIG. 1(A)) to be keyhole welded have a molten metal flow escape (e.g., escape 173 in FIG. 1(A)) on the opposite side to where high-energy beam 100 as a heat source is irradiated, and the escape for molten metal flow is filled by keyhole welding. In this case, the risk of hot cracking in keyhole welding can be reduced. [Explanation of symbols]

[0048] 11, 21, 31, 41, 51, 61, 71 ... first member, 12, 22, 32, 42, 52, 62, 72 ... second member, 23, 33, 43, 53, 63 ... third member, 100 ... high energy beam, 173 ... escape portion

Claims

1. In the two or more components to be keyhole welded, a melt flow escape portion is provided on the opposite side to the side to which the heat source is irradiated, The recess is filled by welding. Butt joint construction.

2. The two or more members are provided with at least one of a fitting portion that fits with the other member and a contact portion that contacts the other member, The recess for avoiding interference between the fitting portion and the contact portion is formed in any one of the two or more members. The butt joint structure of claim 1.

3. The cross-sectional area of ​​the space forming the recess is 1 mm 2 characterized in that 3. A butt joint structure according to claim 1 or 2.

4. the two or more members are members having a circumference, The recess is formed in the circumferential direction. The butt joint structure of claim 1.

5. A butt joint structure according to any one of claims 1 to 4, Compressor.

Citation Information

Patent Citations

  • Laser welding method for aluminum or aluminum alloy

    JP1998156564A