Resin pipe member, manufacturing method therefor, and prefabricated pipe

The resin piping member with a strong flange portion, formed by molding a thermoplastic resin tube in a mold, addresses the instability of fusion joints and simplifies construction by enhancing flange strength and workability.

JP2024146086APending Publication Date: 2024-10-15SEKISUI CHEMICAL CO LTD +1
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
JP2023058799
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-31
Publication Date
2024-10-15

AI Technical Summary

Technical Problem

Existing resin piping members face challenges with unstable quality in fusion joints, complexity in connection processing, and limitations in applying to vertical pipes due to insufficient strength of flange portions, necessitating a simplification of on-site construction work.

Method used

A resin piping member with a cylindrical body and an integral flange portion is manufactured by inserting the end of a thermoplastic resin tube into a mold, heating it above its melting point, and forming the flange by pressing it into the mold, ensuring a strong interface between the flange and the pipe body.

Benefits of technology

The method enhances the strength of the flange portion, allowing for easier and more reliable connections without the need for on-site fabrication, thereby improving workability and earthquake resistance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024146086000001_ABST
    Figure 2024146086000001_ABST
Patent Text Reader

Abstract

To increase strength of a flange part, in a resin pipe member having the flange part.SOLUTION: A resin pipe member has: a cylindrical pipe body 10 made of a thermoplastic resin; and a flange part 20 that is integral with the pipe body 10, is located at one edge of the pipe body 10, and protrudes outward from a peripheral edge of an opening part of the pipe body 10, where a specific test method proves that a portion corresponding to the flange part 20 does not crack. The method comprises a step of inserting an end part of a cylindrical element pipe made of a thermoplastic resin into a mold having a cavity corresponding to the shape of the flange part 20, and forming the flange part 20 from the end part of the element pipe at a specific temperature and pressure.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a resin piping member, a manufacturing method thereof, and a prefabricated piping member. [Background technology]

[0002] Resin piping members (resin piping members) are used as pipes and joints for water supply pipes, etc. Resin piping members have the advantage of being highly earthquake-resistant. For example, polyethylene resin piping members need to be connected to each other using so-called electric fusion joints. However, the connection process using electric fusion joints at the construction site can be cumbersome. The resin piping members are connected by so-called butt fusion. In butt fusion, the ends of a pair of resin pipes are heated and butted together to fuse them. In butt fusion, the quality of the fusion part is unstable, and burrs must be removed from the fusion part. In addition, the resin pipes must be brought to the butt fusion machine at the construction site, and this method cannot be applied to piping such as vertical pipes. Furthermore, at construction sites, there is a demand for simplification and speed-up of on-site construction work (improvement of workability). In response to these problems, a plastic piping component has been proposed that has a melt-formed connection part (flange part) on the end side of the plastic pipe, and that can be used to connect the pipes (Patent Document 1). The invention of Patent Document 1 aims to improve workability on site. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2019-203549 A Summary of the Invention [Problem to be solved by the invention]

[0004] However, the invention of Patent Document 1 has a problem in that the strength of the flange portion is insufficient. SUMMARY OF THE PRESENT EMBODIMENT An object of the present invention is to provide a resin piping member having a flange portion with high strength. [Means for solving the problem]

[0005] As a result of the inventor's investigation, it was found that in the conventional technology, when the end of the plastic pipe is melted in a mold while the flange portion is formed, the end of the plastic pipe is folded back to form the flange portion. With such a manufacturing method, an interface is formed near the boundary between the flange portion formed by folding back and the piping body, and the present invention was completed by making this interface difficult to break. The present invention has the following aspects. <1> The pipe has a cylindrical pipe body made of a thermoplastic resin, and a flange portion that is integral with the pipe body, is located at one end edge of the pipe body, and protrudes outward from a peripheral edge of an opening of the pipe body, A resin piping component, the portion corresponding to the flange portion of which does not crack when tested according to the following test method: <Test Method> A test piece including a flange is obtained by cutting a resin pipe member along a cross section along the axis. The part of the test piece corresponding to the flange is pulled at 50 mm / min in a direction away from the part corresponding to the pipe body, and the presence or absence of cracking of the part corresponding to the flange is judged. <2> The thermoplastic resin is a polyolefin resin. <1> The resin piping member according to claim 1.

[0006] <3> <1> or <2> A prefabricated piping having the resin piping component described above.

[0007] <4> <1> or <2> A method for producing the resin piping member according to the present invention, a die having a cavity corresponding to a shape of the flange portion; heating the end of the blank tube to 150°C or higher; and pressing the blank tube in the direction of insertion into the die at 0.07 MPa or higher to form the flange portion. Effect of the Invention

[0008] According to the resin piping member of the present invention, the strength of the flange portion can be increased. [Brief description of the drawings]

[0009] [Figure 1] 1 is a partial cross-sectional side view of a resin piping member according to an embodiment of the present invention; [Diagram 2] FIG. 2 is a front view of a resin piping member according to one embodiment of the present invention. [Diagram 3] 1A is a front view of the test piece, and FIG. 1B is a left side view of the test piece. [Figure 4] FIG. 1 is a process diagram illustrating a tensile test. [Diagram 5] FIG. 2 is a schematic diagram showing an example of a mold. [Figure 6] 5A to 5C are process diagrams illustrating a manufacturing method of a resin piping member. [Figure 7] FIG. 2 is a side view showing an example of the prefabricated piping of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0010] In this specification and claims, the use of "to" indicating a range of numerical values ​​means that the numerical values ​​before and after it are included as the lower limit and upper limit.

[0011] (Plastic piping components) DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS A resin piping member according to the present invention has a cylindrical piping body and a flange portion located at an end edge of the piping body. The resin piping members are preferably used for piping or joints for air conditioning, water / hot water supply, gas, fuel, and industrial wastewater.

[0012] 1 has a cylindrical piping body 10 with an axis O1 as a pipe axis, and a flange portion 20 located at an end of the piping body 10 in the direction of the axis O1. The piping body 10 and the flange portion 20 are integral with each other. An end surface 22 of the flange portion 20 forms an end surface of the resin piping member 1. The piping body 10 may be either cylindrical or polygonal tubular, but when the resin piping member 1 is used as a water supply pipe, a drainage pipe, or a joint thereof, the piping body 10 is usually cylindrical.

[0013] The flange portion 20 is an end edge of the piping body 10, and protrudes outward from the periphery of the opening 2. The flange portion 20 goes around the periphery of the opening 2 (FIG. 2). That is, the flange portion 20 is annular about the axis O1 when viewed from the front.

[0014] Examples of the thermoplastic resin constituting the resin piping member 1 include polyolefin-based resins, polyvinyl chloride, thermoplastic polyesters (thermoplastic polyethylene terephthalate, etc.), etc. Among them, from the viewpoints of further improving earthquake resistance and durability, the thermoplastic resin constituting the resin piping member 1 is preferably a polyolefin-based resin. Olefin resin pipes have a higher tensile breaking elongation measured according to JIS K 6815-1 and JIS K 6815-3 than rigid polyvinyl chloride pipes. The tensile breaking elongation of rigid polyvinyl chloride pipes is 50-150%, while the tensile breaking elongation of olefin resin pipes is 350% or more. In particular, by the extrapolation method specified in ISO / TR9080, high density polyethylene pipes (PE100) have a tensile breaking elongation of 500% or more, which can better prevent damage caused by earthquakes. The polyolefin resin is not particularly limited, but examples thereof include polypropylene, polybutene, low-density polyethylene, high-density polyethylene, linear low-density polyethylene, atactic polypropylene, isotactic polypropylene, syndiotactic polypropylene, poly-α-olefin, and the like.

[0015] The melt mass flow rate (MFR) of the thermoplastic resin is, for example, preferably 0.1 to 25 g / 10 min, more preferably 0.1 to 10 g / 10 min, and even more preferably 0.29 to 0.45 g / 10 min. When the MFR is equal to or higher than the lower limit, the flange portion 20 can be formed more easily. When the MFR is equal to or lower than the upper limit, the thermal stability can be further improved. MFR can be measured in accordance with JIS K 7210:1999 at a test temperature of 220°C and a test load of 10 kg.

[0016] The specific gravity of the thermoplastic resin is not particularly limited, but is, for example, 942 to 953 kg / m 3 It is. The specific heat of the thermoplastic resin is not particularly limited, but is, for example, 1.9 to 2.3 kJ / kg·[K]. The thermal conductivity of the thermoplastic resin is not particularly limited, but is, for example, 0.46 to 0.5 W / m·K.

[0017] The thermoplastic resin may be a composition containing additives such as pigments, ultraviolet absorbers, antioxidants, and lubricants.

[0018] The melting point of the thermoplastic resin (i.e., the melting temperature of the resin piping member 1) is preferably 125 to 260° C., and more preferably 150 to 260° C. When the melting point of the thermoplastic resin is equal to or higher than the above lower limit, the occurrence of burns on the end surface 22 can be more effectively suppressed in the manufacturing method described below. When the melting point of the thermoplastic resin is equal to or lower than the above upper limit, the fluidity is increased in the manufacturing method described below, and the flange portion 20 can be more easily formed.

[0019] The resin piping member 1 may have a multi-layer structure having a surface layer on at least one of the outer peripheral surface and the inner peripheral surface. For example, by having a surface layer containing an ethylene-vinyl alcohol copolymer resin, the resin piping member 1 is more suitable for air conditioning, hot water supply, gas, or fuel. This is because the surface layer containing an ethylene-vinyl alcohol copolymer resin makes it difficult for gases such as hydrogen, oxygen, propane, and butane, and hydrocarbons such as gasoline and benzene to permeate. The surface layer may contain, for example, at least one of inorganic fibers and organic fibers. Examples of inorganic fibers include glass fibers, carbon fibers, silicon-titanium-carbon composite fibers, boron fibers, and metal fibers. Examples of organic fibers include aramid fibers, vinylon fibers, polyester fibers, and polyamide fibers. When the surface layer contains these fibers, the tensile strength of the resin piping member 1 can be increased and thermal expansion can be further suppressed. The surface layer may also contain a fluororesin. When the surface layer contains fluorine, the resistance (chemical resistance) to acids, alkalis, and the like can be increased. Moreover, a layer similar to the above-mentioned surface layer may be provided inside the wall of the resin piping member 1 .

[0020] The length of the resin piping member 1 (the distance from one end face 22 to the other end face) is appropriately determined depending on the application.

[0021] The diameter of the pipe body 10 of the resin pipe member 1 (excluding the enlarged diameter portion 12) is appropriately determined depending on the application, etc. For example, if the pipe body 10 is a water supply pipe or a drainage pipe, the outer diameter (nominal diameter) R1 of the pipe body 10 may be determined in accordance with the provisions of the JIS standard. The outer diameter R1 is preferably 27 to 216 mm, and more preferably 45 to 114 mm. The inner diameter r1 of the pipe body 10 is determined appropriately according to the nominal diameter R1.

[0022] The thickness t1 of the cylindrical wall 11 of the pipe body 10 can be determined taking into consideration the nominal diameter R1, the strength required for the pipe body 10, and the like. The thickness t1 is, for example, preferably 2 to 30 mm, more preferably 3.5 to 20 mm, and even more preferably 3.5 to 10 mm. When the thickness t1 is equal to or greater than the above lower limit, the strength of the pipe body 10 can be further increased. When the thickness t1 is equal to or less than the above upper limit, both light weight and high strength can be achieved, and therefore workability can be further improved.

[0023] The height h1 of the flange portion 20 is determined taking into consideration the nominal diameter R1, the strength required of the flange portion 20, and the like. The height h1 is, for example, preferably 10 to 50 mm, and more preferably 15 to 30 mm. When the height h1 is equal to or greater than the above-mentioned lower limit, the strength of the flange portion 20 can be further increased. When the height h1 is equal to or less than the above-mentioned upper limit, a general-purpose clamp corresponding to the nominal diameter R1 can be used when the flange portion 20 is butted against a flange portion of another member and fixed with a clamp or the like.

[0024] The width w1 of the flange portion 20 is determined in consideration of the nominal diameter R1, the strength required for the flange portion 20, and the like. For example, the width w1 is preferably 15 to 90 mm, and more preferably 20 to 75 mm. When the width w1 is equal to or greater than the lower limit, the rigidity against the pull-out stress can be increased. The pull-out stress is a stress generated when the plastic piping member 1 is pulled in a direction away from the object to be connected while connected to the object to be connected. When the width w1 is equal to or less than the upper limit, the rigidity of the flange portion 20 can be increased. This is because, when the flange portion 20 is fixed to the object to be connected with bolts or the like, the interval between the bolts becomes large. When the interval between the bolts becomes large, it becomes necessary to increase the tightening force of the bolts, and the load on the flange portion 20 becomes large. In addition, when the width w1 is equal to or less than the upper limit, the maximum diameter of the plastic piping member 1 does not become excessively large, and the plastic piping member 1 can be made more compact. The width w1 is the distance from the inner edge 23 to the outer edge 24 of the flange portion 20 in a front view. The width w1 may increase toward the end edge s22. In this case, the width w1 means the shortest length in the direction of the axis O1.

[0025] The protruding width w11 of the flange portion 20 is determined taking into consideration the nominal diameter R1, the strength required for the flange portion 20, and the like. The protruding width w11 is preferably 15 to 90 mm, and more preferably 20 to 75 mm, for example. When the protruding width w11 is equal to or greater than the lower limit, the rigidity against the pull-out stress can be increased. The pull-out stress is a stress generated when the plastic piping member 1 is pulled in a direction away from the connection object in a state where it is connected to the connection object. When the protruding width w11 is equal to or less than the upper limit, the rigidity of the flange portion 20 can be increased. This is because, when the flange portion 20 is fixed to the connection object with bolts or the like, the interval between the bolts becomes large. When the interval between the bolts becomes large, it becomes necessary to increase the tightening force of the bolts, and the load on the flange portion 20 becomes large. In addition, when the width w1 is equal to or less than the upper limit, the maximum diameter of the plastic piping member 1 does not become excessively large, and it can be made more compact. The protruding width w11 is the distance from the boundary between the outer surface of the piping main body 10 and the flange portion 20 to the outer surface 25 of the flange portion 20 in a side view.

[0026] In the resin piping member 1 of this embodiment, the apex angle (i.e., the intersection between the inner side surface 27 and the end face 22) of the peripheral edge 23 of the opening 2 (i.e., the inner edge of the flange portion 20) is approximately 90°. However, the present invention is not limited to this, and the inner edge 23 may be chamfered to have a tapered shape, or the end face 22 and the inner edge 23 may be a fillet that is an R surface (curved surface). In the resin piping member 1, the apex angle of the outer edge 24 of the flange portion 20 (i.e., the intersection between the outer side surface 25 and the end face 22) is approximately 90°. However, the present invention is not limited to this, and the outer edge 24 may be chamfered to have a tapered shape, or the end face 22 and the outer edge 24 may be a fillet that is an R surface (curved surface).

[0027] In the resin piping member 1, it is preferable that the portion corresponding to the flange portion 20 (the portion corresponding to the flange) does not crack in a tensile test according to the test method described below. When the flange portion 20 is molded in the resin piping member 1, an interface 21 is formed at the boundary between the trace of the piping main body 10 and the flange portion 20. Although this interface 21 cannot be seen with the naked eye, it is more likely to crack than other portions. In the present invention, the strength of the resin piping member 1 is further increased because the test piece does not split in a specific tensile test.

[0028] <Test method> Tensile test A test piece including a flange is obtained by cutting a resin pipe member along a cross section along the axis. The part of the test piece corresponding to the flange is pulled at 50 mm / min in a direction away from the part corresponding to the pipe body, and the presence or absence of cracking of the part corresponding to the flange is judged.

[0029] 2, a test piece s1 is cut out from the resin piping member 1. The test piece s1 is obtained by cutting the resin piping member 1 along a cross section along the axis O1. 3(a) and (b) show the test piece s1. Fig. 3(a) is a diagram showing a cut surface of the test piece s1. Fig. 3(b) is a diagram showing the resin piping member 1 as viewed from the radial outside. The test piece s1 in Fig. 3 has a long rectangular pipe body equivalent part s10 and a rectangular flange equivalent part s20 located at the end in the longitudinal direction of the pipe body equivalent part s10. The width sw1 of the flange equivalent part s20 is larger than the width sw10 of the pipe body equivalent part s10.

[0030] In the test piece s1, the pipe main body corresponding portion s10 is a portion corresponding to the pipe main body 10. In the test piece s1, the flange corresponding portion s20 is a portion corresponding to the flange portion 20. In the test piece s1, an end edge s22 (the end edge opposite to the piping main body equivalent portion s10) corresponds to an end face 22 of the resin piping member 1. In the test piece s1, the end edge s25 corresponds to the outer surface 25 of the resin piping member 1. In the test piece s1, the edge s27 is an edge in the direction of the inner surface 27 of the resin piping member 1. In the test piece s1, the apex angle s24 corresponds to the outer edge 24 of the resin piping member 1.

[0031] The thickness st1 of the test piece s1 is, for example, 5 to 25 mm. The thickness st1 is the length of the resin piping member 1 in the circumferential direction. The length sh1 of the test piece s1 is, for example, 80 to 150 mm. The length sh1 is the length of the resin piping member 1 in the direction of the axis O1. The circumferential direction of the resin piping member corresponds to the thickness direction of the test piece, and the axial direction of the resin piping member corresponds to the length direction of the test piece. The width sw1 of the flange-equivalent portion s20 of the test piece s1 is, for example, preferably 15 to 90 mm, and more preferably 20 to 75 mm. The length sw1 is the radial length of the resin piping member 1. The width sw1 may be the same as or different from the width w1. For example, if the thickness t1 of the cylindrical wall 11 is excessively thick, the width sw1 may be adjusted by cutting off the side edge s27 of the test piece s1. The width sw10 of the pipe main body equivalent portion s10 of the test piece s1 is, for example, preferably 2 to 30 mm, more preferably 3.5 to 20 mm, and even more preferably 3.5 to 10 mm. The length sw1 is the radial length of the pipe main body 10. The width sw10 may be the same as or different from the thickness t1. For example, when the thickness t1 of the cylindrical wall 11 is excessively thick, the side edge s27 side of the test piece s1 may be cut off to adjust the width sw10.

[0032] A through hole 90 is formed in the obtained test piece s1. The opening diameter sr1 of the through hole 90 is, for example, 3 to 15 mm. The position of the through hole 90 is, for example, a distance d1 of 5 to 15 mm from the edge s22 toward the portion s10 corresponding to the piping main body, and a distance d2 of 5 to 15 mm from the edge s25 toward the edge s27. However, it is preferable to position the through hole 90 so as to avoid the interface between the flange portion and the piping main body.

[0033] A jig 92 is attached to the through hole 90 of the test piece s1. An example of the jig 92 is a combination of a metal rod that passes through the through hole 90 and a metal wire connected to the metal rod. A jig 92 attached to the test piece s1 is connected to a tensile testing machine, and the jig 92 is pulled in a direction F away from the piping main body portion s10 (i.e., away from the end edge s27) (FIG. 4). The test piece s1 taken from the resin piping member 1 of the present invention has excellent strength because the flange equivalent portion s20 does not crack (has high cracking strength) when the tensile stress reaches 25 MPa. If the degree of fusion between the flange portion 20 and the piping main body 10 is low, for example, a crack 99 will occur and the flange equivalent portion s20 will crack. If the flange equivalent portion s20 cracks in the tensile test, the strength of the resin piping member from which the test piece was taken is insufficient.

[0034] An example of the tensile tester is Tensilon Universal Material Tester RTF-2410 (A&D Co., Ltd.). The tensile stress in the tensile test is preferably 25 MPa or more, and more preferably 30 MPa or more. When the tensile stress is equal to or more than the above lower limit, the strength of the flange portion 20 can be further increased. The upper limit of the tensile stress in the tensile test is not particularly limited.

[0035] (Manufacturing method for resin piping components) The manufacturing method of the resin piping component of the present invention includes a step of inserting an end of a cylindrical body of thermoplastic resin into a mold, heating the end of the cylindrical body at a temperature above the melting point of the thermoplastic resin, and pressing the cylindrical body in the direction of insertion into the mold to form a connection portion (flange molding step). An example of a method for manufacturing a resin piping member will be described below.

[0036] The method for manufacturing a resin piping member according to the present embodiment includes, for example, a flange molding step and a demolding step. The flange forming step is a step of forming a flange portion at the end of a cylindrical body of thermoplastic resin (hereinafter, sometimes referred to as a "blank tube"). The base pipe is a member having substantially the same thickness from one edge to the other edge. The thermoplastic resin constituting the base pipe is the same as the thermoplastic resin constituting the resin piping member.

[0037] An example of a mold used in the flange forming process will be described with reference to the drawings. 5 has a base mold 52 and an opening / closing mold 54. The base mold 52 and the opening / closing mold 54 form a cavity 51 therein. The cavity 51 has a shape corresponding to the flange portion 20. The opening / closing mold 54 opens and closes the cavity 51 by moving in the X direction relative to the base mold 52. The mold 50 has an insertion opening 59. The base mold 52 has a pillar portion 56 that rises from a bottom surface 57 toward the insertion opening 59. The pillar portion 56 is cylindrical. In a state where the base mold 52 and the open / close mold 54 are combined, the mold 50 has a flow path 60 at the boundary between the base mold 52 and the open / close mold 54. The flow path 60 communicates between the cavity 51 and the outside of the mold 50. In the mold 50, the boundary between the base mold 52 and the open / close mold 54 is located at the side wall 53. That is, the flow path 60 is separated from the bottom surface 57 inside the base mold 52. The flow path 60 may be a so-called through hole or a slit as long as it can communicate between the inside and the outside of the mold 50 . The shape of the flow channel 60 is not particularly limited, and the cross-sectional (transverse) shape perpendicular to the direction connecting both openings of the flow channel 60 may be a polygon such as a rectangle, or may be a circle. The size of the cross section of the flow path 60 is such that the molten thermoplastic resin is unlikely to enter the flow path 60 and the gas (e.g., air) in the cavity 51 is discharged from the flow path 60 to the outside of the mold 50. For example, the size of the opening of the flow path 60 is preferably 0.05 to 0.4 mm. When the size of the opening is equal to or greater than the lower limit, clogging due to gas tar can be prevented. When the size of the opening is equal to or less than the upper limit, the molten thermoplastic resin can be prevented from flowing into the flow path 60 in the flange molding process. If the cross section of the flow path 60 is circular, the size of the opening is the diameter of the cross section of the flow path 60. If the cross section of the flow path 60 is polygonal, the size of the opening is the diameter of a circumscribing circle for the cross-sectional shape of the flow path 60. If the flow path 60 is a slit, the size of the opening is the width of the flow path 60 (the short side direction of the opening surface).

[0038] First, a blank tube is obtained. The blank tube may be prepared in advance or may be produced according to a conventional method.

[0039] The end of the mother tube is inserted into the cavity 51 through the insertion opening 59. At this time, the mother tube is inserted into the cavity 51 while the column portion 56 is received inside the mother tube. Before inserting the mother tube into the cavity 51, the mother tube may be preheated. Next, the end of the blank tube is heated and melted in the die 50. While the end of the blank tube is in a melted state, the end of the blank tube is pressed against the bottom surface 57. That is, the blank tube is pressed in the direction of insertion into the die 50. When the end of the blank tube is pressed against the bottom surface 57, the end is folded back and the molten thermoplastic resin spreads into the cavity, forming the shape of the flange portion 20 (flange forming process). At this time, the air in the cavity 51 flows out of the flow path 60 and the die 50, and the air in the cavity 51 is removed. Removing the air from the cavity 51 prevents the air between the blank tube and the die from being overheated, thereby preventing burning.

[0040] The process of forming the flange portion 20 will be described with reference to FIG. When the blank tube 70 (FIG. 6(a)) is heated in the mold 50 and pressed against the bottom surface 57 of the mold, the end becomes a folded-back portion 72 (FIG. 6(b)). When the blank tube 70 is further heated in the mold 50 and pressed against the bottom surface 57 of the mold, the molten thermoplastic resin and the folded-back portion 72 become one with each other to form the flange portion 20 (FIG. 6(c)). In this manner, the flange portion 20 is formed in the die 50, and the blank pipe is made into the resin piping member 1. The surface in contact with the bottom surface 57 becomes the end surface 22 of the resin piping member 1 .

[0041] The temperature at which the end of the blank pipe is heated (heating temperature) can be determined taking into consideration the melting point of the thermoplastic resin constituting the resin piping member 1. When the thermoplastic resin constituting the resin piping member 1 is high density polyethylene (HDPE), the heating temperature is preferably 150°C or higher, more preferably 150 to 260°C, and even more preferably 180 to 240°C. When the heating temperature is equal to or higher than the lower limit, the end of the blank pipe is sufficiently melted, and the splitting strength can be further increased. When the heating temperature is equal to or lower than the upper limit, the occurrence of "burns" in the flange portion 20 can be suppressed, and the strength can be further improved. The heating temperature is the temperature reached by the thermoplastic resin melted in the mold.

[0042] The heating temperature is preferably 20 to 40°C higher than the melting point of the thermoplastic resin constituting the resin piping member 1. When the heating temperature is equal to or higher than the lower limit, the end of the blank pipe is sufficiently melted, the splitting strength is further increased, and the end of the blank pipe is melted quickly, thereby improving work efficiency. When the heating temperature is equal to or lower than the upper limit, the occurrence of "burns" in the flange portion 20 is suppressed, and the strength can be further improved.

[0043] The pressure (forcing pressure) with which the blank tube is pressed against the bottom surface 57 of the die 50 is, for example, preferably 0.07 MPa or more, more preferably 0.07 to 3.0 MPa, and even more preferably 1.0 to 2.0 MPa. When the forcing pressure is equal to or more than the above lower limit, the flange portion 20 can be molded while the thermoplastic resin is appropriately held at pressure in accordance with the molten state of the thermoplastic resin. When the forcing pressure is equal to or more than the above lower limit, the molten resin is sufficiently filled in the cavity of the die, and better molding can be achieved. If the forcing pressure is high, the parting surface of the die may open momentarily due to the pressure, causing burrs or the like around the resin piping member 1. For this reason, when the forcing pressure is equal to or less than the above upper limit, the generation of burrs or the like is suppressed, and poor appearance can be suppressed. The pushing pressure is the pressure measured by a pressure gauge attached to the machine that pushes the blank tube (pushing pressure (MPa) = the force pushed by the machine (N / m 2 ) / cross-sectional area of ​​raw tube (m 2 )).

[0044] Next, in the demolding step, after the resin piping member 1 is cooled, the mold 50 is opened and the resin piping member 1 is taken out.

[0045] The die for forming the flange portion is not limited to the above-mentioned configuration. For example, the base mold may have the flow path 60. When the base mold has the flow path 60, the flow path 60 may be in contact with the bottom surface 57. That is, a part of the inner surface of the flow path 60 is flush with the bottom surface 57. Within cavity 51, air tends to accumulate at the boundary between bottom surface 57 and the inner surface of side wall 53. By having flow passage 60 in contact with bottom surface 57, air can be more easily removed from cavity 51 during the molding process.

[0046] Alternatively, the base mold 52 may have a core. The core is a member having a column portion extending from the bottom surface 57 toward the insertion port 59, and is movable in the X direction relative to the base mold 52. The flow path 60 of the metal mold 50 is located at the boundary between the opening / closing mold 54 and the base mold 52. When a mold having a core is used, in the demolding step, the open / close mold 54 is moved in a direction away from the base mold 52, and the core is moved in a direction away from the open / close mold 54, to remove the resin piping member 1. When a groove (for example, a groove going around the axis O1) is formed on the end surface 22 of the flange portion 20, air tends to accumulate in the groove. For this reason, the core 58 may be further divided to form a flow path similar to the flow path 60 in the core 58.

[0047] (Prefabricated piping) The prefabricated piping of the present invention has the resin piping member of the present invention. An example of prefabricated piping will be described with reference to the drawings. 6 includes a resin piping member 101, a socket portion 121, a vent portion 122, and a pipe 123. The vent portion 122 connects the resin piping member 101 and the pipe 123. The socket portion 121 is located at an end of the pipe 123.

[0048] The socket 121 is a so-called electric fusion joint, and has an electric heating wire inside. The socket 121 has a terminal 124 connected to the electric heating wire. The socket 121 is fused to a pipe 123. The vent portion 122 is fused to the pipe 123 and the resin pipe member 101 . The resin piping member 101 has a flange portion 20 at an end edge.

[0049] The prefabricated piping 100 shown in the figure is an example, and various known configurations can be used as joints. In addition, the flange portion 20 may be connected to a known configuration for connecting to a piping.

[0050] According to the prefabricated piping of this embodiment, the flange portion of the resin piping component of the present invention is butted against the flange portion of other equipment (e.g., a pump, a water heater, other prefabricated piping, etc.) and secured with a clamp, thereby making it possible to easily perform piping work at the construction site. In addition, because there is no need to prepare the flanges at the construction site, butt welding at the construction site is unnecessary, and therefore beads associated with butt welding are not formed near the flanges of the prefabricated pipes.

[0051] In the prefabricated piping 100 of this embodiment, the receiving portion 121, the vent portion 122, the piping 123, and the resin piping member 101 are fused to one another. That is, the receiving portion 121, the vent portion 122, the piping 123, and the resin piping member 101 are all formed of a resin material, but the present invention is not limited to this. Any of the receiving portion 121, the vent portion 122, and the piping 123 may be a member formed of a metal material, and may be configured to be connected to a dissimilar material.

[0052] Examples of the metal material include iron, brass, copper, stainless steel, aluminum, titanium, silver alloy, etc. The inner surface of the metal pipe may be lined with a resin material such as a fluororesin. EXAMPLES

[0053] The present invention will be described in more detail below using examples, but the present invention is not limited to these examples.

[0054] (Raw materials used) · Thermoplastic resin A: Polyethylene (melting point = 130°C).

[0055] (Examples 1 to 4, Comparative Example 1, Reference Example 1) Thermoplastic resin A was melted and extruded to obtain a blank tube of 100A (nominal diameter = 114 mm, thickness = 6 mm). Using a mold A similar to the mold 50 in Fig. 5, the blank pipe was inserted into the mold and the flange portion was formed (flange forming process) to obtain the resin piping member of this example. The heating temperature and pressing pressure in the flange forming process are shown in the table. The resin piping member of this example had a nominal diameter (outer diameter) R1 = 114 mm, thickness t1 = 10.4 mm, width w1 = 28.4 mm, protruding width w11 = 18 mm, and height h1 = 25 mm. A test piece similar to the test piece s1 in Figure 3 (length sh1 = 100 mm, thickness st1 = 10 mm, width sw1 = 10.4 mm, width sw10 = 28.4 mm) was cut out from the resin piping material. A through hole (opening diameter sr1 = 3 mm, distance d1 = 5 mm, distance d2 = 5 mm) was formed in the obtained test piece. A metal rod was passed through the through hole, both ends of the metal rod were supported by U-shaped metal fittings, and a metal wire was attached to the U-shaped metal fittings. The wire attached to the U-shaped metal fittings was pulled (50 mm / min) with a Tensilon universal material testing machine RTF-2410 (A & D Co., Ltd.), and the presence or absence of cracking of the flange equivalent part was visually confirmed at a tensile stress of 25 MPa. Those where no cracking was confirmed were marked with "◯", and those where cracking was confirmed were marked with "×". The resin piping members thus obtained were evaluated for strength and burntness, and the results are shown in the table. In Reference Example 1, the pressing pressure was low and the flange portion could not be formed.

[0056] (Evaluation method) <Strength> The resin piping member of each example was dropped from a height of 1 m onto a concrete surface with the flange portion facing downward. After the drop, the flange portion was visually observed and evaluated according to the following evaluation criteria. Evaluation Criteria ○: The flange is not damaged and has sufficient strength. ×: The flange portion is damaged and has insufficient strength.

[0057] <Burnt> The end face of the flange portion of each example of the resin piping member was visually observed to check for the presence or absence of burning.

[0058] [Table 1]

[0059] As shown in Table 1, in Examples 1 to 4 in which the present invention was applied, the strength was evaluated as "good." In addition, in Examples 1 to 3 in which the heating temperature was 180 to 220° C., no burning was observed. Comparative Example 1, which gave an "X" in the tensile test, was evaluated as "X" in strength. From these results, it was confirmed that the strength can be increased by applying the present invention. [Explanation of symbols]

[0060] 1 Plastic piping components 2 Opening 10 Piping body 20 Flange 22 End face 50 Mold 51 Cavity 59 Insertion port 100 Prefabricated Piping O1 axis s1 Test piece s10 Pipe body equivalent s20 Flange equivalent part

Claims

1. The pipe has a cylindrical pipe body made of a thermoplastic resin, and a flange portion that is integral with the pipe body, is located at one end edge of the pipe body, and protrudes outward from a peripheral edge of an opening of the pipe body, A resin piping component, the portion corresponding to the flange portion of which does not crack when tested according to the following test method: <Test Method> A test piece including a flange is obtained by cutting a resin pipe member along a cross section along the axis. The part of the test piece corresponding to the flange is pulled at 50 mm / min in a direction away from the part corresponding to the pipe body, and the presence or absence of cracking of the part corresponding to the flange is judged.

2. The resin piping member according to claim 1 , wherein the thermoplastic resin is a polyolefin resin.

3. A prefabricated piping comprising the resin piping member according to claim 1 or 2.

4. A method for manufacturing a resin piping member according to claim 1 or 2, A method for manufacturing a resin piping member, comprising the steps of: inserting an end of a cylindrical blank tube made of thermoplastic resin into a mold having a cavity corresponding to the shape of the flange portion, heating the end of the blank tube to 150°C or higher, and pressing the blank tube in the direction of insertion into the mold at 0.07 MPa or more to form the flange portion.

Citation Information

Patent Citations

  • Method for forming flange at end part of plastic pipe and die therefor

    JP2003322287A

  • Resin pipe for piping connection and connection structure including the same

    JP2019203549A