Method for producing hydroxymethylfurfural

The use of activated carbon washed with lower alcohols and acetic acid esters enhances HMF purity by removing impurities, addressing the low conversion and purification challenges in existing HMF production methods.

JP2024146567APending Publication Date: 2024-10-15CUYUSYOJI
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
JP2023059550
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-31
Publication Date
2024-10-15

AI Technical Summary

Technical Problem

Existing methods for producing hydroxymethylfurfural (HMF) result in low conversion rates and require complex purification steps due to the adsorption of HMF on activated carbon, leading to the need for additional separation and purification processes to achieve high purity.

Method used

A method involving the use of activated carbon washed with an aqueous solution containing 5 to 50% lower alcohol followed by extraction with lower alcohol or acetic acid ester to enhance the purity of HMF, utilizing a solid Lewis acid catalyst like phosphorylated titanium oxide for glucose conversion.

Benefits of technology

The method achieves high-purity HMF separation and purification by effectively removing impurities such as glucose and by-product saccharides, improving the overall yield and simplifying the purification process.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

To provide a method for producing HMF of higher purity by separating and purifying HMF (hydroxymethylfurfural) or the like containing a large amount of glucose and saccharides.SOLUTION: A method for producing hydroxymethylfurfural has: (1) a step of bringing hydroxymethylfurfural and solution containing saccharides in contact with active carbon to allow hydroxymethylfurfural and saccharides to be adsorbed to active carbon, and (2) a step of cleaning the active carbon to which hydroxymethylfurfural and saccharides have been adsorbed by active carbon containing lower alcohol by 5 to 50 vol.%, and then bringing the active carbon in contact with lower alcohol or acetic acid ester to extract hydroxymethylfurfural; or( 3) a step of bringing active carbon to which hydroxymethylfurfural and saccharides have been adsorbed in contact with acetic acid ester to extract hydroxymethylfurfural.SELECTED DRAWING: None
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to hydroxymethylfurfural (hereinafter sometimes referred to as "HMF" in this specification) and to a method for producing highly pure HMF by separating and purifying it from a mixture containing sugars. [Background technology]

[0002] Hydroxymethylfurfural is an important intermediate chemical that can be synthesized using glucose as a raw material, but its synthetic pathway is very complicated. The raw material glucose undergoes skeletal isomerization in the presence of an acid catalyst to convert it into fructose. The resulting fructose is converted into hydroxymethylfurfural by a dehydration reaction with the acid catalyst, but hydroxymethylfurfural is further hydrolyzed by the acid catalyst in the reaction system to organic acids (formic acid, levulinic acid). Therefore, a new catalyst for highly selectively producing hydroxymethylfurfural is desired.

[0003] By treating amorphous hydrous titanium oxide with phosphoric acid, a phosphoric acid residue is covalently bonded to the surface of the hydrous titanium oxide to produce a phosphate titanium oxide, which can convert glucose to HMF with high efficiency and is inactive against the hydrolysis of the resulting HMF. As such, this solid Lewis acid can produce HMF from glucose in high yield (see patent documents).

[0004] In order to carry out a continuous reaction in a flow reactor using the solid Lewis acid, it was necessary to support the solid Lewis acid catalyst on some kind of carrier. A method is known in which a molded body of the solid Lewis acid is obtained using at least one selected from the group consisting of polytetrafluoroethylene, aluminum oxide, silicone, silica, permethylpolysilane, and carbon black as a binder, and the molded body is filled in a flow reactor to produce HMF from glucose in a continuous reaction (Patent Document 2). [Prior art documents] [Patent documents]

[0005] [Patent Document 1] International Publication No. 2012-108472 [Patent Document 2] JP 2021-041344 A Summary of the Invention [Problem to be solved by the invention]

[0006] However, by supporting the solid Lewis acid, the conversion rate of glucose to HMF decreased, and the resulting reaction solution contained HMF, glucose, and by-product sugars (hereinafter, in this specification, sometimes referred to as "HMF, etc."), and a further separation and purification step was required to obtain high-purity HMF. Thus, Patent Document 2 describes that the reaction solution is passed through an activated carbon column to adsorb HMF, etc. onto the activated carbon, then water is passed through to bleed out glucose and by-product sugars, and finally methanol is passed through to bleed out HMF, thereby obtaining HMF with a purity of 93%, but a step of separating and purifying HMF with a higher purity is desired.

[0007] An object of the present invention is to provide a method for separating and purifying HMF and the like that contains a large amount of glucose and sugars, thereby producing HMF with a higher purity. [Means for solving the problem]

[0008] As a result of intensive research aimed at solving the above-mentioned problems, the inventors discovered that highly pure hydroxymethylfurfural can be obtained by washing activated carbon that has adsorbed HMF and sugars with an aqueous solution containing water and a lower alcohol, or by extracting it with acetic ester, and thus completed the present invention.

[0009] That is, the present invention relates to a method for producing hydroxymethylfurfural, comprising the steps of: (1) contacting a solution containing hydroxymethylfurfural and sugars with activated carbon to adsorb the hydroxymethylfurfural and the sugars onto the activated carbon; and (2) washing the activated carbon on which the hydroxymethylfurfural and the sugars are adsorbed with an aqueous solution containing 5 to 50 volume % of a lower alcohol and then contacting the activated carbon with a lower alcohol or an acetate ester to extract the hydroxymethylfurfural; or (3) contacting the activated carbon on which the hydroxymethylfurfural and the sugars are adsorbed with an acetate ester to extract the hydroxymethylfurfural.

[0010] In the step (2), the step of washing the activated carbon having the adsorbed hydroxymethylfurfural and saccharides with an aqueous solution containing 5 to 50% by volume of a lower alcohol is preferably a step of washing with an aqueous solution containing 5 to 20% by volume of a lower alcohol. The lower alcohol is preferably at least one selected from the group consisting of methanol, ethanol, and isopropanol. The solution containing hydroxymethylfurfural and saccharides is preferably a reaction solution obtained by reacting glucose or fructose in a solvent in the presence of a solid Lewis acid. The solid Lewis acid is preferably a titanium oxide phosphate having phosphoric acid residues covalently bonded to the surface of an amorphous hydrous titanium oxide functioning as a Lewis acid. In addition, the amorphous hydrous titanium oxide functioning as a Lewis acid is preferably an amorphous hydrous titanium oxide that can be obtained by reacting an organic titanium compound that is hydrolyzed in an aqueous solution to form an oxide with water, together with an acid catalyst or a base catalyst. Furthermore, the organic titanium compound that is hydrolyzed in the aqueous solution to form an oxide is preferably at least one selected from the group consisting of titanium chloride, titanium sulfate, and titanium alkoxide. Effect of the Invention

[0011] By using the method of the present invention, it is possible to separate and purify HMF with high purity from a mixture containing a large amount of impurities such as sugars. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0012] The method for producing HMF of the present invention comprises the steps of: (1) contacting a solution containing HMF and sugars with activated carbon to adsorb hydroxymethylfurfural and sugars onto the activated carbon; (2) washing the activated carbon on which hydroxymethylfurfural and sugars are adsorbed with an aqueous solution containing 5 to 50 volume % of a lower alcohol, and then contacting the activated carbon with a lower alcohol or an acetate to extract hydroxymethylfurfural; or (3) contacting the activated carbon on which hydroxymethylfurfural and sugars are adsorbed with an acetate to extract hydroxymethylfurfural.

[0013] The solution containing HMF and saccharides in the step (1) is preferably a reaction solution obtained by reacting glucose or xylose in a solvent in the presence of a solid Lewis acid. Specific examples of the sugars include glucose, which is a raw material, xylose, fructose, cellobiose, maltose, sucrose, and the like.

[0014] The solvent used in the reaction is preferably water. The temperature during the reaction is preferably 60°C to 180°C, more preferably 100°C to 150°C. The time required for the reaction is appropriately selected depending on the reaction temperature, and is preferably 10 minutes to 24 hours, more preferably 2 hours to 6 hours. The amount of glucose or fructose used in the reaction is preferably 0.0002 to 200 parts by mass, more preferably 0.025 to 2 parts by mass, relative to 1 part by mass of the solid Lewis acid.

[0015] The reaction may be carried out in a batch system or a flow system, but is preferably carried out in a flow system. In the flow system, it is preferable to use a flow microreactor. A chemical reaction is carried out by pouring raw materials into a flow channel filled with a solid Lewis acid. In the flow microreactor, the flow effect and micromixing effect can be expected to improve the reaction yield, ease the reaction conditions, and simplify the operation.

[0016] The solid Lewis acid is preferably a titanium phosphate oxide having a phosphoric acid residue covalently bonded to the surface of an amorphous titanium oxide hydrous functioning as a Lewis acid. The titanium oxide hydrous can be obtained by reacting an organotitanium compound that is hydrolyzed in an aqueous solution to form an oxide with water, together with an acid catalyst or a base catalyst.

[0017] Examples of the organic titanium compound include inorganic titanium compounds such as titanium hydroxide, titanic acid, titanium trichloride, titanium tetrachloride, titanium tetrabromide, titanium sulfate, and titanium oxysulfate; titanium alkoxide compounds such as tetraisopropoxytitanium, tetra-n-butoxytitanium, tetrakis(2-ethylhexyloxy)titanium, and tetrastearyloxytitanium; titanium acylate compounds; titanium chelate compounds such as diisopropoxybis(acetylacetonato)titanium, isopropoxy(2-ethyl-1,3-hexanediolato)titanium, and hydroxybis(lactato)titanium; organic acid titanium compounds such as titanium oxalate and titanium tetraacetate; and water-soluble titanium complexes. Among these, at least one selected from the group consisting of titanium chloride, titanium oxalate, and titanium alkoxide is preferred.

[0018] The number of carbon atoms constituting the alkoxy group in the titanium alkoxide is preferably 1 to 6, more preferably 2 to 4. The alkoxy group may be linear, branched, or cyclic.

[0019] Examples of the acid used in the hydrolysis reaction include hydrochloric acid, sulfuric acid, and nitric acid. Examples of the base used in the hydrolysis reaction include ammonia, sodium hydroxide, and potassium hydroxide. The temperature during the hydrolysis reaction is preferably 10 to 100° C., and more preferably 20 to 30° C. The time required for the hydrolysis reaction can be appropriately set depending on the reaction temperature, reaction scale, and the like, and is preferably 0.5 to 48 hours, and more preferably 10 to 24 hours.

[0020] The titanium oxide phosphate can be obtained by treating the amorphous titanium oxide hydrous with phosphoric acid. The phosphoric acid treatment can be carried out by immersing the amorphous titanium oxide hydrous in an aqueous phosphoric acid solution and stirring it. The temperature during this treatment is preferably 10°C or higher and lower than 100°C, more preferably 20°C or higher and 30°C or lower. The reaction time can be appropriately set depending on the reaction temperature, reaction scale, etc., but is preferably 1 hour to 96 hours, more preferably 24 hours to 72 hours.

[0021] The solid Lewis acid may be doped with a metal element or may be coated with a compound containing a metal element, such as aluminum, gallium, indium, thallium, magnesium, manganese, calcium, niobium, tantalum, zirconium, silicon, zinc, cerium, iron, tungsten, molybdenum, or vanadium.

[0022] The solid Lewis acid may be mixed with a binder to form a molded product, if necessary. Specific examples of the binder include crystalline aluminosilicate molecular sieves such as mordenite, chabazite, erionite, ferrierite, faujasite, levin, ZSM-5, zeolite A, zeolite β, FU-1, Rho, ZK-5, RUB-3, RUB-13, NU-3, NU-4, NU-5, NU-10, NU-13, NU-23, and MCM-22; SAPO-5, SAPO-11, SAPO-17, SAPO-18, SAPO-26, SAPO-31, SAPO-33, SAPO-34, SAPO-35, and SAPO-26-17; Examples of the silicoaluminophosphate molecular sieve include crystalline silicoaluminophosphate molecular sieves such as SAPO-42, SAPO-43, SAPO-44, SAPO-47, and SAPO-56; clay compounds such as kaolinite, sericite, talc, mica (muscovite, phlogopite, biotite, lepidolite, vanadium mica, chromium mica, and fluorine mica), montmorillonite, sepiolite, attapulgite, and smectite; silica, alumina (aluminum oxide), titania, zirconia, yttria; polytetrafluoroethylene, silicone, permethylpolysilane, and carbon black. Among these, at least one selected from the group consisting of polytetrafluoroethylene, aluminum oxide, silicone, silica, permethylpolysilane, and carbon black is preferred.

[0023] The amount of the binder is not particularly limited as long as it allows production of a molded body, but is preferably 10 to 100 parts by mass, more preferably 10 to 50 parts by mass, and further preferably 10 to 20 parts by mass, relative to 100 parts by mass of the solid Lewis acid.

[0024] The solid Lewis acid molded body can be obtained, for example, by kneading a binder and a solid Lewis acid, optionally with water, molding, drying, and optionally firing. The kneading is preferably performed under pressure. From the viewpoint of workability, the kneading is preferably performed continuously using a kneader or other kneading machine. The drying conditions are not limited as long as moisture can be removed, and can be performed, for example, at a temperature range of 80°C to 150°C for 1 to 168 hours. After the drying, the product is adjusted to a desired size and, if necessary, fired. The firing temperature and time vary depending on the type of solid Lewis acid molded body. The firing can be performed, for example, at 400°C to 800°C for 1 to 168 hours.

[0025] The molded product of the solid Lewis acid may be in the form of powder, granules, pellets, thin film, nanotubes, etc., as necessary. Molded products in various shapes can be obtained by, for example, extrusion molding, compression molding (e.g., tablet molding, etc.), rolling molding, spray drying, etc.

[0026] More specific examples of the molded article of the solid Lewis acid include a method in which a binder precursor such as tetraethoxysilane, the organotitanium compound, and phosphoric acid or a precursor thereof are mixed to form a liquid or slurry, which is then subjected to casting, slush molding, coating, or the like, followed by hydrolysis; and a method in which a binder precursor such as tetraethoxysilane and the organotitanium compound are mixed to form a liquid or slurry, which is then subjected to casting, slush molding, coating, or the like, followed by hydrolysis, followed by phosphoric acid treatment.

[0027] The activated carbons used in steps (1) to (3) are carbonaceous materials that have been treated to enhance their pore structure and are porous solids with very high surface areas. They can be obtained from a variety of sources, including coal, wood, coconut shells, nut shells, and peat. The activated carbons can be produced from the sources using physical activation involving heating in a controlled environment, or chemical activation using strong acids, bases, or oxidizing agents. The activated carbons can be used alone or in combination of two or more types.

[0028] Examples of the method for contacting the activated carbon in steps (1) to (3) include a continuous flow method in which the solution to be contacted with the activated carbon is passed through a column packed with activated carbon, and a batch method in which the activated carbon is placed in a tank containing the solution to be contacted with the activated carbon, and the like. The continuous flow method is preferred.

[0029] Specific methods for packing activated carbon into a column include a method in which activated carbon is brought into contact with a solvent (particularly water) to form a slurry and then packed, a method in which activated carbon is packed as a solid, a method in which activated carbon is packed as a solid and then immersed in a solvent to replace the gas in the activated carbon with the solvent, etc. In order to efficiently adsorb HMF and sugars, a method in which activated carbon is packed as a solid and then immersed in a solvent to replace the gas in the activated carbon with the solvent is preferred.

[0030] The step (1) can be carried out by passing a mixture containing HMF and saccharides through the column packed with activated carbon and a solvent. If the solution that has passed through the column contains HMF, the solution can be passed through the same column or a different column to adsorb the remaining HMF onto the activated carbon.

[0031] In the step (2), the activated carbon to which the HMF and saccharides are adsorbed is washed with an aqueous solution containing 5 to 50% by volume of a lower alcohol, and then contacted with a lower alcohol or an acetate ester to extract hydroxymethylfurfural. Like the step (1), the step (2) can be carried out by the continuous flow method, the batch method, or the like, but it is preferable to carry out the step (2) by the continuous flow method, since the column used in the step (1) can be used as it is.

[0032] Specific examples of the lower alcohol used in the step (2) include methanol, ethanol, n-propanol, isoproponol, n-butyl alcohol, isobutyl alcohol, s-butyl alcohol, t-butyl alcohol, n-pentanol, s-pentanol, isopentanol, t-pentanol, and neopentanol, among which methanol, ethanol, and isopropanol are preferred. These may be used alone or in combination of two or more.

[0033] In the step (2), the activated carbon with adsorbed HMF and sugars is washed with an aqueous solution of the lower alcohol at 5 to 50% by volume, and it is preferable to use an aqueous solution of the lower alcohol at 5 to 20% by volume. If the aqueous solution is less than 5% by volume, the sugars cannot be sufficiently removed, and if the aqueous solution is more than 50% by volume, the HMF will flow out and the yield of HMF will be reduced.

[0034] The step (2) is a step of contacting the activated carbon that has been washed with an aqueous solution containing a lower alcohol with a lower alcohol or an acetic ester to extract hydroxymethylfurfural. The lower alcohol used in the HMF extraction in the step (2) above can be the same as those exemplified in the step (2) above. Specific examples of the acetate ester used in the step (2) include methyl acetate, ethyl acetate, isopropyl acetate, and n-propyl acetate. The lower alcohol or acetate ester may be used alone or in combination of two or more thereof, or a mixture of a lower alcohol and an acetate ester may be used.

[0035] The amount of the lower alcohol or acetate ester used in the step (2) is not particularly limited, but it is preferable to use an amount sufficient to sufficiently extract HMF.

[0036] The step (3) is a process of contacting the activated carbon to which HMF and sugars are adsorbed with an acetate ester to extract hydroxymethylfurfural. The step (3) can be carried out by the continuous flow method, the batch method, or the like, as in the step (1). However, when the step (1) is carried out by the continuous flow method, the column can be used as it is, so that the step (3) is preferably carried out by the continuous flow method.

[0037] Specific examples of the acetate ester used in the step (3) include those exemplified in the step (2). The acetate ester may be used alone or in combination of two or more.

[0038] The amount of acetate ester used in the step (3) is not particularly limited, but it is preferable to use an amount sufficient to sufficiently extract HMF.

[0039] In addition to the steps (2) and (3), a step (4) of washing the activated carbon to which the hydroxymethylfurfural and saccharides are adsorbed with water can be provided. The step (4) can be carried out by the continuous flow method, the batch method, or the like, as in the step (1). However, when the steps (1) and (2) are carried out by the continuous flow method, the column can be used as it is, so that the step (4) is preferably carried out by the continuous flow method.

[0040] The amount of water used in the step (4) is not particularly limited, but it is preferable to use an amount sufficient to sufficiently extract impurities such as sugars. Moreover, the step (4) can be performed before the step (2) or (3).

[0041] Next, the present invention will be described in more detail using examples, but the scope of the present invention is not limited to the examples.

[0042] <Production Example> 20 ml of titanium tetraisopropoxide was added to 100 ml of distilled water and stirred at room temperature for 3 hours. The white precipitate was removed by filtration, added to 200 ml of 1.0 M aqueous hydrochloric acid, and stirred for 1 hour to promote condensation of the oxide framework. This filtration, addition, and stirring (condensation) process was repeated two more times (for a total of three times). The resulting precipitate was washed with distilled water until neutral, and then dried in an oven at 80°C to obtain amorphous hydrous titanium oxide. The amorphous hydrous titanium oxide was added to an aqueous phosphoric acid solution (0.1 M) and stirred at room temperature for 48 hours. The white solid was filtered off and washed with distilled water until neutral to obtain the solid Lewis acid 1. Solid Lewis acid 1 was added to 100 ml of a 10% glucose solution and reacted at 100° C. for 17 hours. Analysis of the resulting reaction solution A showed that it contained 74.69 mM HMF, 341.68 mM glucose, 22.13 mM fructose, 4.96 mM cellobiose, and 2.62 mM furfural. EXAMPLES

[0043] 100 ml of the reaction solution A was passed through a 24 mmφ chromatography column packed with 12.5 g of activated carbon (manufactured by Fujifilm Wako Co., Ltd., bulk density 0.182), and the components contained in the reaction solution A were adsorbed by the activated carbon. When the reaction solution A discharged from the chromatography column was analyzed, the components originally contained in the reaction solution A were not detected. Next, a 5% by volume aqueous solution of methanol was passed through the chromatographic column, and then 100 ml of methanol was passed through the chromatographic column. The resulting methanol solution was analyzed and found to contain 102.08 mM HMF, 0.24 mM glucose, 0.27 mM cellobiose, and 2.7 mM furfural. As a result, HMF with a purity of 97% was obtained. EXAMPLES

[0044] The same procedure was carried out as in Example 1, except that a 20% by volume aqueous methanol solution was used instead of a 5% by volume aqueous methanol solution. Analysis of the resulting methanol solution revealed that it contained 115.93 mM HMF, 0.28 mM glucose, 0.03 mM fructose, 0.03 mM cellobiose, and 4.38 mM furfural. As a result, HMF with a purity of 96% was obtained.

[0045] [Comparative Example 1] The same procedure as in Example 1 was repeated, except that distilled water was used instead of the 5% by volume aqueous methanol solution. The resulting methanol solution was analyzed and found to contain 108.05 mM HMF, 0.71 mM glucose, 1.92 mM cellobiose, and 3.25 mM furfural. As a result, HMF with a purity of 95% was obtained. [Industrial Applicability]

[0046] The method of the present invention is useful as a method for purifying HMF when synthesizing HMF from natural resources such as cellulose.

Claims

1. The method for producing hydroxymethylfurfural includes the steps of: (1) contacting a solution containing hydroxymethylfurfural and sugars with activated carbon to adsorb the hydroxymethylfurfural and sugars onto the activated carbon; (2) washing the activated carbon on which the hydroxymethylfurfural and sugars are adsorbed with an aqueous solution containing 5 to 50 volume % of a lower alcohol, and then contacting the activated carbon with a lower alcohol or an acetate to extract the hydroxymethylfurfural; or (3) contacting the activated carbon on which the hydroxymethylfurfural and sugars are adsorbed with an acetate to extract the hydroxymethylfurfural.

2. The method for producing hydroxymethylfurfural according to claim 1, wherein in the step (2), the activated carbon having hydroxymethylfurfural and sugars adsorbed thereon is washed with an aqueous solution containing 5 to 50% by volume of a lower alcohol, and the washing is performed with an aqueous solution containing 5 to 20% by volume of a lower alcohol.

3. 3. The method for producing hydroxymethylfurfural according to claim 1 or 2, wherein the lower alcohol is at least one selected from the group consisting of methanol, ethanol, and isopropanol.

4. 2. The method for producing hydroxymethylfurfural according to claim 1, wherein the solution containing hydroxymethylfurfural and saccharides is a reaction solution obtained by reacting glucose or fructose in a solvent in the presence of a solid Lewis acid.

5. The method for producing hydroxymethylfurfural according to claim 1, wherein the solid Lewis acid is a phosphated titanium oxide having phosphoric acid residues covalently bonded to the surface of an amorphous hydrous titanium oxide functioning as a Lewis acid.

6. The method for producing hydroxymethylfurfural according to claim 5, wherein the amorphous hydrous titanium oxide functioning as a Lewis acid is an amorphous hydrous titanium oxide obtainable by reacting an organic titanium compound which is hydrolyzed in an aqueous solution to form an oxide with water, together with an acid catalyst or a base catalyst.

7. The method for producing hydroxymethylfurfural according to claim 6, wherein the organic titanium compound that is hydrolyzed in the aqueous solution to form an oxide is at least one selected from the group consisting of titanium chloride, titanium sulfate, and titanium alkoxide.

Citation Information

Patent Citations

  • Molded body of solid lewis acid catalyst

    JP2021041344A

  • Amorphous hydrous titanium oxide and solid lewis acid catalyst containing same

    WO2012108472A1