Molecular sieve membrane element, and molecular sieve membrane element manufacturing method

The use of a heat-shrinkable silicone covering member simplifies the assembly of molecular sieve membrane elements, enhancing sealing and adhesion, thereby improving manufacturing efficiency and productivity.

JP2024146912APending Publication Date: 2024-10-15MITSUBISHI CHEM CORP

Patent Information

Application Number
JP2024057229
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-31
Filing Date
2024-03-29
Publication Date
2024-10-15

AI Technical Summary

Technical Problem

The manufacturing process of molecular sieve membrane elements, particularly those using addition reaction type silicone rubber, is inefficient due to the need for solidification and application of materials, which complicates the production process.

Method used

The use of a heat-shrinkable silicone covering member to connect the first and second members of the molecular sieve membrane element, optionally with an additional fluororesin covering member, allows for efficient assembly by heating and shrinking the covering member to cover the ends of the members, eliminating the need for additional fillers and simplifying the manufacturing process.

Benefits of technology

This method enables efficient production of molecular sieve membrane elements with improved sealing and adhesion, reducing manufacturing time and increasing productivity while maintaining high separation performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024146912000001_ABST
    Figure 2024146912000001_ABST
Patent Text Reader

Abstract

To provide a technique capable of manufacturing a molecular sieve membrane element with good efficiency.SOLUTION: A molecular sieve membrane element (1) has: a first member (11) having a molecular sieve membrane on an inner wall and / or an outer wall; a second member (12) connected to at least one end of the first component (11) by a connection member (13). The connection member (13) is a coating member made of heat shrinkable silicone that coats surfaces at an end of the first member (11) and an end of the second member (12), or a heat shrinkable coating member of which an inclination of stress-strain curve is 0.69 or more and a tensile strength is 28 MPa or less when strain in tensile test is 0.75 or more and 1.0 or less.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a molecular sieve membrane element and a method for producing a molecular sieve membrane element. [Background technology]

[0002] Conventionally, as a method for separating and concentrating a mixture of gas or liquid containing an organic compound, a membrane separation and concentration method using a membrane such as a polymer membrane or a zeolite membrane has been proposed. As a membrane separation and concentration method using a zeolite membrane, a molecular sieve membrane element is known that has a first member having a molecular sieve membrane, a second member connected to an end of the first member, a covering member covering the surfaces of the ends of the first member and the second member, and a member made of an addition reaction type silicone rubber interposed between the covering member and the surfaces of the first member and the second member (for example, see Patent Document 1). [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2022-037674 A Summary of the Invention [Problem to be solved by the invention]

[0004] The member made of addition reaction type silicone rubber in Patent Document 1 is formed by applying the material to the relevant portion and solidifying it. Therefore, the molecular sieve membrane element in Patent Document 1 leaves room for improvement in terms of workability in production.

[0005] The present invention has been made in consideration of the above circumstances, and an object of the present invention is to provide a technique capable of efficiently producing a molecular sieve membrane element. [Means for solving the problem]

[0006] A first aspect of the present invention is a molecular sieve membrane element comprising: a first member having a molecular sieve membrane on an inner wall and / or an outer wall of a tubular porous substrate; and a second member having an end, disposed coaxially with the first member at an end of the first member, and connected to at least one end of the first member by a connecting member, wherein the connecting member is a covering member made of heat-shrinkable silicone that covers an outer surface of the end of the first member that is parallel to the axial direction of the first member and an outer surface of the end of the second member.

[0007] A second aspect of the present invention relates to the molecular sieve membrane element of the first aspect, which further includes an additional covering member that covers at least a part of the connecting member.

[0008] A third aspect of the present invention relates to the molecular sieve membrane element of the second aspect, wherein the further covering member is made of a fluororesin.

[0009] A fourth aspect of the present invention is the molecular sieve membrane element according to any one of the first to third aspects, wherein the molecular sieve membrane is a zeolite membrane.

[0010] A fifth aspect of the present invention is a method for producing a molecular sieve membrane element according to any one of the first to fourth aspects, comprising the steps of: arranging the first member and the second member coaxially; providing the covering member around an end of the first member and an end of the second member; and heating and shrinking the covering member to cover surfaces of the end of the first member and the end of the second member with the covering member. Effect of the Invention

[0011] According to one aspect of the present invention, a technique capable of efficiently producing a molecular sieve membrane element can be provided. [Brief description of the drawings]

[0012] [Figure 1] FIG. 1 is a cross-sectional view of a molecular sieve membrane element and an apparatus used in a gas separation test according to an embodiment and an example of the present invention. [Diagram 2]FIG. 2 is a diagram of a stress-strain curve of Example 1. [Diagram 3] FIG. 1 is a diagram of a stress-strain curve of Example 2. [Figure 4] FIG. 13 is a diagram showing a stress-strain curve of Comparative Example 2. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0013] The embodiments of the present invention are described below, but the present invention is not limited to the above-mentioned embodiments, and various modifications are possible within the scope of the claims. The technical scope of the present invention also includes embodiments obtained by appropriately combining the technical means disclosed in different embodiments. Unless otherwise specified in this specification, "A to B" representing a numerical range means "A or more (including A and greater than A) and B or less (including B and smaller than B)". In this specification, "and / or" means one or both of two related items.

[0014] [Embodiment 1] Hereinafter, the first embodiment of the present invention will be described in detail.

[0015] <Molecular sieve membrane element> In the molecular sieve membrane element of the present invention, a second member is connected to an end of a first member having a molecular sieve membrane on the inner wall and / or outer wall of a tubular porous substrate by a connecting member. The connecting member is a covering member made of heat-shrinkable silicone that covers the outer surface of the end of the first member that is parallel to the axial direction of the first member and the surface of the end of the second member. The molecular sieve membrane element of the present invention may further have an additional covering member that covers at least a part of the connecting member.

[0016] In addition, in the molecular sieve membrane element of the present invention, a filler may be interposed between the connecting member and the first and second members. Alternatively, the connecting member may be in direct contact with the first and second members. That is, there may be no filler between the connecting member and the outer side surface parallel to the axial direction of the first member and the surface of the end of the second member. An example of the filler is grease. Not having a filler is preferable from the viewpoint of preventing the influence of the filler in separation using the separation sieve membrane element. Furthermore, not using a filler may significantly improve the work efficiency.

[0017] <First component> The first member has a molecular sieve membrane on the inner circumferential surface and / or the outer circumferential surface of a tubular porous substrate.

[0018] <Porous substrate> The porous substrate functions as a support for supporting the molecular sieve membrane. The material constituting the porous substrate can be various materials such as glass, ceramics, metal, carbon molded body, or resin. In the case of a ceramic support, any porous inorganic material having chemical stability that allows zeolite to be crystallized in a membrane on its surface or the like may be used. Specifically, for example, ceramic sintered bodies such as silica, α-alumina, γ-alumina, mullite, zirconia, titania, yttria, silicon nitride, or silicon carbide are listed. Among them, alumina such as α-alumina and γ-alumina and mullite are preferred, and alumina is particularly preferred. If these supports are used, partial zeoliteization is easy, so that the bond between the support and zeolite is strong and a dense membrane with high separation performance is easily formed.

[0019] In the present invention, the porous substrate itself does not need to have molecular sieving ability. The porous substrate has fine pores (holes, gaps) that communicate from the outer wall side (outer peripheral surface) to the inner wall side (inner peripheral surface). Any known porous substrate having pores can be used.

[0020] The porosity of the porous substrate is usually 20% or more, preferably 25% or more, more preferably 30% or more, and usually 80% or less, preferably 60% or less, more preferably 50% or less, and the average pore size is usually 0.01 μm or more, preferably 0.05 μm or more, more preferably 0.1 μm or more, and the upper limit is usually 20 μm or less, preferably 10 μm or less, more preferably 5 μm or less. A porous substrate having such pores has sufficient strength to properly support the molecular sieve membrane, and can allow molecules that have passed through the molecular sieve membrane to pass through at a sufficient speed, or can allow molecules to reach the molecular sieve membrane at a sufficient speed. The porosity and pore size of the porous substrate can be easily specified by mercury intrusion porosimetry, observing the cross section with a scanning electron microscope (SEM), etc. The same applies to the average pore size, but it can also be calculated from the volume and mass using the true specific gravity.

[0021] The cross section of the tubular porous substrate perpendicular to the axial direction of the tube is preferably circular on both the outer and inner peripheral surfaces. The thickness of the tubular porous substrate (the difference between the radius of the outer peripheral surface and the radius of the inner peripheral surface) varies depending on the material, porosity, etc., but is preferably 0.5 mm or more, more preferably 0.8 mm or more, and even more preferably 1.3 mm or more.

[0022] The inner diameter of a tubular porous substrate varies depending on the material, porosity, and the like, but for example, the ratio of the inner diameter (diameter) to the thickness of the porous substrate described above (inner diameter (mm) / thickness (mm)) is preferably 20 or less, more preferably 17 or less, even more preferably 13 or less, and particularly preferably 9 or less, from the viewpoint of the weight when introduced into a separation membrane module. In the case of a porous substrate made of a sintered ceramic body, the inner diameter is preferably 5 mm or more, particularly 7 mm or more, and 15 mm or less, particularly preferably 11 mm or less, from the viewpoint of shape retention during substrate preparation.

[0023] The length (axial length) of the porous substrate can be adjusted depending on the application and is not particularly limited. From the viewpoint of handling the separation membrane element and securing the membrane area, however, it is preferably 50 mm or more, particularly 80 mm or more, and is preferably 1500 mm or less, particularly 1300 mm or less.

[0024] <Molecular sieve membrane> The molecular sieve membrane is formed on the outer peripheral surface and / or the inner peripheral surface of the porous substrate. The form of the molecular sieve membrane is not particularly limited as long as it can adequately exhibit molecular sieving function.

[0025] The molecular sieve membrane is preferably any one of a zeolite membrane, a silica membrane, and a carbon membrane, or a combination thereof, among which a zeolite membrane or a silica membrane is preferred, and a zeolite membrane is particularly preferred from the viewpoints of separation performance, water resistance, and durability.

[0026] Here, when a zeolite membrane is used as the molecular sieve membrane, the zeolite is preferably an aluminosilicate, but metal elements such as Ga, Fe, B, Ti, Zr, Sn, and Zn may be used in place of Al within the range in which the desired performance of the membrane is obtained, and elements such as Ga, Fe, B, Ti, Zr, Sn, Zn, and P may be contained together with Al.

[0027] Moreover, the skeleton of the crystalline zeolite that forms the pores of the zeolite membrane is preferably an 8- or less-membered oxygen ring, more preferably a 6- to 8-membered oxygen ring, from the viewpoint of separation performance for water and other gas molecules.

[0028] Examples of the structure of zeolite include AEI, AFG, AFX, ANA, CHA, DDR, EAB, ERI, ESV, FAR, FRA, GIS, ITE, KFI, LEV, LIO, LOS, LTA, LTN, MAR, MFI, MWF, PAU, RHO, RTH, SOD, STI, TOL, and UFI. Among these, it is preferable to use a membrane composed of AEI, AFX, CHA, DDR, ERI, KFI, LEV, MFI, MWF, PAU, RHO, RTH, SOD, LTA, or UFI type zeolite from the viewpoint of separation performance for specific components, and it is more preferable to use a membrane composed of CHA, DDR, MWF, RHO, or SOD type zeolite. The value of n of a zeolite having an oxygen n-membered ring refers to the pore composed of the zeolite framework and T element (an element other than oxygen constituting the framework) with the largest number of oxygen atoms.

[0029] When synthesizing a zeolite membrane as a molecular sieve membrane, an organic template (structure-directing agent) can be used if necessary. However, there are no particular limitations on the template as long as it can produce the desired zeolite structure. In addition, if a zeolite membrane can be synthesized without a template, it is not necessary to use an organic template.

[0030] When a silica membrane is used as the molecular sieve membrane, the silica content in the silica membrane is not particularly limited as long as the effects of the present invention can be obtained. For example, in a silicon oxide composition, the ratio of silicon to all electropositive elements including silicon is usually 50 mol% or more.

[0031] The silica film is formed on the inorganic porous substrate by the sol-gel method, the CVD method, the polymer precursor method, or the like. In the sol-gel method, a metal alkoxide is reacted with water on the inorganic porous substrate to form a gel through hydrolysis and dehydration condensation, and the silica film can be formed. In the counter diffusion CVD method, for example, when the inorganic porous substrate is a porous tubular substrate, oxygen is circulated on the inside and a silica source is circulated on the outside, and an amorphous silica layer is vapor-deposited in the substrate pores to form the silica film. In the polymer precursor method, a silica precursor such as an alkoxysilane or polysilazane is applied to the inorganic porous substrate, and then heat treatment is performed to form the silica film.

[0032] When a carbon membrane is used as the molecular sieve membrane, the carbon membrane precursor solution is dip-coated on a porous substrate, heat-treated at about 600 to 800°C, and dried to form a carbon membrane. From the viewpoint of ease of carbon membrane formation, examples of the carbon membrane precursor include aromatic polyimide, polypyrrolone, polyfurfuryl alcohol, polyvinylidene chloride, phenolic resin, lignin derivative, wood tar, bamboo tar, etc. As the solvent, an organic solvent such as tetrahydrofuran, acetone, methanol, ethanol, or N-methylpyrrolidone can be suitably used.

[0033] The thickness of the molecular sieve membrane is not particularly limited, but in the case of a zeolite membrane, the lower limit of the thickness is usually 0.01 μm or more. The upper limit of the thickness is preferably 30 μm or less, more preferably 10 μm or less, from the viewpoint of molecular permeation resistance. In the case of a silica membrane, the membrane may be a single layer membrane or a membrane consisting of two or more layers, and the thickness is preferably 1 nm or more. The thickness is preferably 10 μm or less, more preferably 1 μm or less. In the case of a carbon membrane, the thickness is preferably 0.05 μm or more, more preferably 0.1 μm or less, from the viewpoint of molecular permeation resistance. The upper limit of the thickness is preferably 5 mm or less, more preferably 500 μm or less, but it is preferable that the membrane thickness is thin within the range in which the effects of the present invention can be obtained.

[0034] In addition to the above-mentioned methods, other methods for forming a molecular sieve membrane on the surface of a porous substrate include, for example, (1) a method in which a substance capable of forming a molecular sieve membrane is fixed to the surface of a porous substrate with a binder or the like, (2) a method in which a porous substrate is impregnated with a slurry or solution in which a substance capable of forming a molecular sieve membrane is dispersed, and the substance is fixed to the surface of the porous substrate, and (3) a method in which a substance capable of forming a molecular sieve membrane (particularly, zeolite) is crystallized into a membrane on the surface of a porous substrate (see, for example, International Publication No. WO 2013 / 125660, etc.).

[0035] The first member may be in any one of the following forms: a molecular sieve membrane formed only on the outer peripheral surface of the porous substrate, a molecular sieve membrane formed only on the inner peripheral surface of the porous substrate, and a molecular sieve membrane formed on both the outer peripheral surface and the inner peripheral surface of the porous substrate. In general, the form in which the molecular sieve membrane is formed on the outer peripheral surface of the porous substrate is desirable, since the coating material has an inward contraction force.

[0036] <Second member> The second member is a member to be connected to an end of the first member, and has an end portion. In order to facilitate connection to the first member, the second member is preferably tubular or cylindrical in shape.

[0037] When the second member is tubular, there is no particular restriction on the outer diameter and inner diameter of the second member, but from the viewpoint of sealing property at the time of connection, it is desirable that the outer diameter of the first member and the outer diameter of the second member are equal. In addition, the ends of the first member and the second member may be structured such that one end is inserted into the other end. In this case, when a molecular sieve membrane is provided on the outer peripheral surface of the first member, from the viewpoint of protecting the molecular sieve membrane, it is preferable that the end of the second member is structured such that it is inserted into the end of the first member. In this case, it is more preferable that the inner diameter of the first member and the outer diameter of the second member are approximately equal, because gaps are unlikely to be formed between the covering member and the first and second members after connection, improving sealing property.

[0038] The type of material constituting the second member may be appropriately selected according to the type of gas / liquid to be separated by the first member. The material constituting the second member may be any of metal, ceramics, synthetic resin, etc. Examples of the metal include nickel, chromium, molybdenum, cobalt, tungsten, copper, titanium, zirconium, tin, cadmium, niobium, tantalum, etc., and may be an alloy containing these. Other examples include Tribaloy T, cobalt nichrome tungsten, high chromium iron, chromium aluminum iron, Emclary, molybdenum iron, stainless steel, etc.

[0039] Examples of the nickel or nickel alloy include pure nickel, Monel, Inconel, Incoloy, Nimonic, Ilium, Hastelloy, MC alloy, nickel aluminide, Ni-Cr alloy, Invar alloy, Ni-Al alloy, Ni-Co alloy, Ni-Mn alloy, Ni-Cu-Al alloy, and Ni-Cu-Si alloy.

[0040] The chromium or chromium alloy may be a chromium-nickel alloy or Inconel.

[0041] Examples of the copper or copper alloy include pure copper, brass, red brass, bronze, beryllium copper, titanium copper, nickel silver, cupronickel (cupronickel), copper nickel, and aluminum bronze.

[0042] Examples of the titanium and titanium alloys include pure titanium, Ti-0.2Pd, Ti-0.8Ni-0.3Mo, Ti-0.5Ta, Ti-6Al-4V, and Ti-3Al-2.5V.

[0043] The zirconium and zirconium alloys include Zr, Zr-1.5Sn-0.05Ni, and Zr-1.5Sn.

[0044] The stainless steels may be austenitic, ferritic, two-phase (austenitic-ferritic), martensitic, or precipitation hardened.

[0045] Among these, it is preferable that the material is any one selected from stainless steel, titanium alloy, and nickel alloy.

[0046] The second member may be an end member that seals one end of the first member, or may be a tubular member such as a boss portion for supplying or discharging a fluid into the first member. The second member may be a tubular member having a molecular sieve membrane like the first member.

[0047] <Connection parts> The connecting member integrally covers the outer peripheral surface of the end of the first member and at least the surface of the end of the second member, thereby connecting the first member and the second member. The connecting member is preferably in the form of a tube, a ring, or a sheet. The connecting member is made of heat-shrinkable silicone.

[0048] Here, the term "heat shrinkable" refers to the property of shrinking when heated. For example, when a heat shrinkable member shaped into a tube is heated, its inner diameter shrinks and becomes smaller than before heating. When a heat shrinkable member is used, it is used for a member with a larger diameter than when it is shrunk to the maximum in order to ensure adhesion after shrinkage. Therefore, whether or not a material has heat shrinkability can be determined by peeling off the heat shrinkable member used and heating it with a heat gun or oven to see if it shrinks further. Whether or not a material has shrunk can be determined, for example, by measuring the dimensions of the longest part of the material with a micrometer or laser microscope.

[0049] "Heat-shrinkable silicone" refers to silicone that has heat-shrinkability. That is, a heat-shrinkable silicone connection member shaped into a tube has heat-shrinkability that shrinks to the inside of the connection member, and also has sealing properties with respect to the first and second members, for example, by adhering to the outer peripheral surface of the end of the first member and at least the surface of the end of the second member. Because of its good sealing properties, it can be suitably used for gas separation.

[0050] The thickness and length of the connecting member (the length along the axial direction of the first and second members) can be changed as appropriate. For example, the second member may be covered entirely on its outer circumferential surface by a connecting member that is longer than the first member. When the diameter D of the first and second members is 9 to 20 mm, the thickness of the connecting member is preferably 0.2 to 3.5 mm, and more preferably 0.3 to 0.8 mm. In this case, the overlap length (axial length) between the connecting member and the first member and the overlap length (axial length) between the connecting member and the second member are preferably 540 times D, and more preferably 10 to 30 times D.

[0051] The shrinkage rate of the connecting member can be appropriately selected according to the other members, but the inner diameter of the connecting member before heating must be larger than the diameters of the first and second members, and the inner diameter of the connecting member after sufficient heating must be smaller than the diameters of the first and second members. For example, when the diameter D of the first and second members is 0.5 to 280 mm, it is preferable to use a heat-shrinkable silicone tube or the like having a shrinkage rate of 50% and an inner diameter d before heating of 0.9 to 285 mm as the connecting member. Here, the term "shrinkage rate" refers to the ratio of the inner diameter after sufficient heating to the inner diameter before heating for a heat-shrinkable member shaped into a tube or ring.

[0052] Examples of heat-shrinkable silicone connection members having the above-mentioned characteristics include ST-65DG manufactured by Shin-Etsu Chemical Co., Ltd., SRFR-15 / 9.6-8-SP manufactured by Tyco Electronics, and SST12-030S manufactured by Nissei Electric Co., Ltd.

[0053] To provide the connection member around the outer peripheral surfaces of the ends of the first member and the second member, for example, when the connection member is tubular, the end of the first member may be inserted from one end of the connection member and the second member may be inserted from the other end. When the connection member is sheet-shaped, the connection member may be wrapped around the outer peripheral surface of the end of the first member and the surface of the end of the second member so as to integrally cover them.

[0054] As described above, the first member has a porous substrate and a molecular sieve membrane, and therefore has minute irregularities on its outer peripheral surface. For this reason, in order to connect the first member and the second member while ensuring sealing performance with materials such as fluororesin that have been conventionally used, it was necessary to use additives such as grease and silicone rubber to deal with the irregularities on the outer peripheral surface. By using the heat-shrinkable silicone connecting member according to the present invention to connect the first member and the second member, the connecting member itself adheres closely to the irregularities on the outer peripheral surface of the first member, ensuring sealing performance, and eliminating the need for a process using additives.

[0055] <Further covering materials> The molecular sieve membrane element of the present invention may have an additional covering member that covers at least a part of the connecting member, and it is preferable to use a heat-shrinkable synthetic resin or rubber film. Examples of the material of the additional covering member include polyolefins such as polyethylene and polypropylene, nylon, polyether ether ketone (PEEK), fluororesin, silicone resin, polyvinyl chloride resin, acrylic resin, ABS resin, modified PPO resin, polycarbonate, polyester, polysulfone, polyurethane, TPX, cellulose-based, polyvinyl alcohol-based, polyimide-based, nitrile rubber (NBR), styrene-brassine rubber (SBR), silicone rubber, fluororubber, chloroprene rubber, ethylene propylene rubber, and butyl rubber. In particular, fluororesin is preferable from the viewpoints of impact resistance and chemical resistance.

[0056] Examples of fluororesins include polyvinylidene fluoride resin (PVDF), polytetrafluoroethylene (PTFE), tetrafluoroethylene copolymer (ETFE), tetrafluoroethylene hexafluoropropylene copolymer (FEP), and tetrafluoroethylene / perfluoroalkyl vinyl ether copolymer (PFA).

[0057] The shape of the additional covering member may be tubular, ring-shaped, or sheet-shaped. For example, when the covering member is tubular, the method of providing the additional covering member may be a method of inserting the molecular sieve membrane element from one end side of the covering member to cover the connecting member and preferably the outer peripheral surface of the first member and the outer peripheral surface of the second member, etc. When the connecting member is sheet-shaped, the method may be a method of winding the connecting member so as to integrally cover the connecting member and preferably the outer peripheral surface of the first member and the outer peripheral surface of the second member, etc.

[0058] Examples of the further covering member having the above-mentioned properties include Teflon (registered trademark) heat shrink tube 10F manufactured by Gunze Ltd. and Junflon NF-120 manufactured by Junkosha.

[0059] <Structure of molecular sieve membrane element> A molecular sieve membrane element having the components described above has a structure as shown in FIG. FIG. 1 shows a cross section of a molecular sieve membrane element 1 according to an embodiment of the present invention.

[0060] That is, in the molecular sieve membrane element 1 according to the present invention, one end of the first member 11 and one end of the second member 12 are connected so as to be covered with the connecting member 13, and the connecting portion is provided with a predetermined sealing property and pressure resistance only by the connecting member 13.

[0061] The molecular sieve membrane element 1 according to the present invention may further include an additional covering member 14 that covers at least a part of the connecting member 13. In this case, the additional covering member 14 imparts impact resistance, chemical resistance, and tensile strength to the connecting portion between one end of the first member 11 and one end of the second member 12.

[0062] The axial length of the further covering member 14 need only be long enough to cover at least the connecting portion between one end of the first member 11 and one end of the second member 12, and it is preferable for the axial length of the further covering member 14 to be longer than the axial length of the connecting member 13 in order to maintain the strength of the connecting portion between one end of the first member 11 and one end of the second member 12.

[0063] <Manufacturing method of molecular sieve membrane element> The method for producing a molecular sieve membrane element of the present invention will be described below by taking the molecular sieve membrane element shown in FIG. 1 as an example.

[0064] In the method for manufacturing the molecular sieve membrane element 1, for example, one end of the first member 11 is inserted from one end of the connecting member (heat-shrinkable silicone tube) 13, one end of the second member 12 is inserted from the other end of the connecting member 13, and the end face of the first member 11 and the end face of the second member 12 are coaxially butted together in the connecting member 13, thereby circumferentially attaching the connecting member 13 to the end of the first member 11 and the end of the second member 12. Next, the connecting member 13 is heated with a heat gun or the like to thermally shrink the connecting member 13 and to be brought into close contact with the end of the first member 11 and the end of the second member 12, thereby forming the molecular sieve membrane element 1.

[0065] In addition to the above, the method of providing a covering member around the end of the first member 11 and the end of the second member 12 may be, for example, a method in which the end face of the first member 11 and the end face of the second member 12 are coaxially butted together, and then a connecting member (heat-shrinkable silicone sheet) 13 is wrapped around the outer circumferential surface of the end of the first member 11 and at least the end surface of the second member 12 so as to integrally cover the outer circumferential surface of the end of the first member 11 and at least the end surface of the second member 12.

[0066] The end of the first member 11 and the end of the second member 12 may be fitted together. At this time, it is preferable from the viewpoint of strength to adopt a method of providing a step at the end of the second member 12 for fitting.

[0067] The second member 12 may be cylindrical or tubular.

[0068] Furthermore, after the connection member 13 is brought into close contact with the end of the first member 11 and the end of the second member 12, a further covering member 14 that covers at least a portion of the connection member 13 may be further provided around the connection member 13.

[0069] <Applications of molecular sieve membrane elements> The molecular sieve membrane element of the present invention can be suitably used for applications in which a liquid, gas or solid mixture consisting of multiple components is contacted with the membrane element, and a highly permeable substance in the mixture is allowed to permeate therethrough, thereby separating the highly permeable substance from the mixture, or a less permeable substance is allowed to permeate therethrough, thereby concentrating the less permeable substance. As described above, the connecting member of the present invention is particularly suitable for gas separation, and therefore the molecular sieve membrane element of the present invention can be suitably used for separating or concentrating a gas mixture consisting of multiple components.

[0070] There is no limitation on the liquid, gas or solid component, and examples thereof include water, organic matter, carbon dioxide, oxygen, hydrogen, nitrogen, helium or inorganic matter.

[0071] Examples of the organic substances include alcohols such as ethanol, methanol, and isopropyl alcohol; ethers such as diethyl ether and tetrahydrofuran; phenols such as phenol, cresol, and xylenol; aldehydes such as formaldehyde and acetaldehyde; organic acids such as formic acid and acetic acid; hydrocarbons such as saturated hydrocarbons such as methane, ethane, and propane, and unsaturated hydrocarbons such as acetylene and ethylene; polysaccharides such as sugars, oligosaccharides, cellulose, and carrageenan, and glycans such as sialylated glycans; polymer compounds such as polyols, polyamines, polycarboxylic acids, polycarboxylic acid esters, modified polymer compounds, and copolymerized polymer compounds; proteins such as enzymes, antibodies, lectins, and receptors, peptides, amino acids, cytokines, hormones, nucleotides, oligonucleotides, nucleic acids (DNA, RNA, PNA), lipids, bacteria such as Escherichia coli, viruses, and biological molecules such as molecules that constitute cells.

[0072] Examples of the inorganic substances include metals such as sodium, calcium, silicon, aluminum, iron, nickel, manganese, chromium, arsenic, lead, mercury, copper, manganese, tin, antimony, or cadmium; salts such as sodium chloride, sodium acetate, sodium sulfate, or calcium carbonate; inorganic acids such as hydrochloric acid or sulfuric acid; hydroxides such as sodium hydroxide; carbon allotropes such as graphite or diamond; metal complexes such as hexaamminecopper(II) sulfate; non-metallic elements such as boron and compounds thereof; carbon monoxide; or carbon disulfide.

[0073] Examples of mixed gases include air, natural gas, combustion gas, coke oven gas, biogas such as landfill gas generated from landfill sites, and steam reformed methane gas generated and discharged in the petrochemical industry.

[0074] For separation or concentration using molecular sieve membranes, methods called pervaporation and vapor permeation can be used. By utilizing the property of a gas or liquid containing multiple types of molecules, components with high permeance permeate the separation membrane, while components with low permeance have difficulty permeating the separation membrane, it is possible to separate or concentrate specific molecules.

[0075] <Molecular sieve membrane module> A molecular sieve membrane module can be constructed by arranging and integrating one or more molecular sieve membrane elements produced by the production method according to the present invention in a housing.

[0076] In the molecular sieve membrane element produced by the present invention, one end of the first member is connected to the second member, so that the first member can be easily attached to various members of the module via the second member.

[0077] [Embodiment 2] The second embodiment of the present invention will now be described in detail. The second embodiment is the same as the first embodiment in all respects except for the connecting members.

[0078] <Connection parts> The connecting member integrally covers the outer peripheral surface of the end of the first member and at least the surface of the end of the second member, thereby connecting the first member and the second member. The shape of the connecting member is preferably tubular, ring-shaped, or sheet-shaped. In addition, the connecting member has heat shrinkability, and the slope of the stress-strain curve when the strain in a tensile test is 0.75 to 1.0 is 0.69 or more, so that the first member and the second member can be well sealed. From the viewpoint of holding the first member and the second member after shrinkage, the slope is preferably 0.75 or more, more preferably 0.80 or more, even more preferably 0.85 or more, particularly preferably 0.90 or more, and most preferably 0.95 or more. It is preferably 5.0 or less, more preferably 4.0 or less, and even more preferably 3.0 or less. The value at this time is a value obtained by testing the connecting member after heat shrinkage. Furthermore, the connecting member needs to conform to the molecular sieve membrane surface and ensure sealing properties. The sealing property is considered to be due to the softness of the members, and the softness can be expressed as the relatively low tensile strength in the tensile test of the connection member before heat shrinkage. All members are basically harder after heat shrinkage and cooling than before shrinkage. Therefore, a member with a large tensile strength before shrinkage is expected to become harder after shrinkage compared to a member with a small tensile strength, so the sealing member can be selected by checking the tensile strength before shrinkage. The tensile strength is the maximum stress observed in a tensile test performed using a tensile tester. Therefore, the tensile strength of the connection member used is preferably 1.0 MPa or more, more preferably 2.0 MPa or more, even more preferably 3.0 MPa or more, and particularly preferably 6.0 MPa or more. It is preferably 28 MPa or less, more preferably 25 MPa or less, and even more preferably 20 MPa or less. Being within this range makes it suitable for use in gas separation, which is particularly prone to leakage. The tensile strength test is performed in accordance with JIS K 7161. Examples of connection members that exhibit these physical properties include heat-shrinkable silicone and electron beam crosslinked soft polyolefin resin.

[0079] Here, the term "heat shrinkable" refers to the property of shrinking when heated. For example, when a heat shrinkable member shaped into a tube is heated, its inner diameter shrinks and becomes smaller than before heating. When a heat shrinkable member is used, it is used for a member with a diameter larger than when it is shrunk to the maximum in order to ensure adhesion after shrinkage. Therefore, whether or not a material has heat shrinkability can be determined by peeling off the member used and heating it with a heat gun or oven to see if it shrinks further. Whether or not a material has shrunk can be determined, for example, by measuring the dimensions of the longest part of the material with a micrometer or laser microscope.

[0080] "Heat-shrinkable silicone" refers to silicone that has heat-shrinkability. That is, a heat-shrinkable silicone connection member shaped into a tube has heat-shrinkability that shrinks to the inside of the connection member, and also has sealing properties with respect to the first and second members, for example, by adhering to the outer peripheral surface of the end of the first member and at least the surface of the end of the second member. Because of its good sealing properties, it can be suitably used for gas separation.

[0081] "Electron beam cross-linked soft polyolefin resin" refers to a polyolefin resin having heat shrinkability. That is, a connection member made of electron beam cross-linked soft polyolefin resin formed into a tube shape has heat shrinkability to shrink inside the connection member, and also has sealing properties with respect to the first member and the second member, for example, by adhering to the outer peripheral surface of the end of the first member and at least the surface of the end of the second member. Since it has good sealing properties, it can be suitably used for gas separation.

[0082] The thickness and length of the connecting member (the length along the axial direction of the first and second members) can be changed as appropriate. For example, the second member may be covered entirely on its outer circumferential surface by a connecting member that is longer than the first member. When the diameter D of the first and second members is 9 to 20 mm, the thickness of the connecting member is preferably 0.2 to 3.5 mm, and more preferably 0.3 to 0.8 mm. In this case, the overlap length (axial length) between the connecting member and the first member and the overlap length (axial length) between the connecting member and the second member are preferably 540 times D, and more preferably 10 to 30 times D.

[0083] The shrinkage rate of the connecting member can be appropriately selected according to the other members, but the inner diameter of the connecting member before heating must be larger than the diameters of the first and second members, and the inner diameter of the connecting member after sufficient heating must be smaller than the diameters of the first and second members. For example, when the diameter D of the first and second members is 0.5 to 280 mm, it is preferable to use a heat-shrinkable silicone or electron beam cross-linked soft polyolefin resin tube or the like having an inner diameter d before heating of 0.9 to 285 mm and a shrinkage rate of 40-50% as the connecting member. Here, the term "shrinkage rate" refers to the ratio of the inner diameter after sufficient heating to the inner diameter before heating for a heat-shrinkable member shaped into a tube or ring.

[0084] Examples of heat-shrinkable silicone connection members having the above-mentioned characteristics include ST-65DG manufactured by Shin-Etsu Chemical Co., Ltd., SRFR-15 / 9.6-8-SP manufactured by Tyco Electronics, and SST12-030S manufactured by Nissei Electric Co., Ltd.

[0085] As connecting members made of electron beam crosslinked soft polyolefin resin having the above-mentioned properties, Sumitube A and Sumitube B manufactured by Sumitomo Electric Industries, Ltd., THT-14.0 manufactured by Denka Electron Co., Ltd., and the like can be used.

[0086] To provide the connection member around the outer peripheral surfaces of the ends of the first member and the second member, for example, when the connection member is tubular, the end of the first member may be inserted from one end of the connection member and the second member may be inserted from the other end. When the connection member is sheet-shaped, the connection member may be wrapped around the outer peripheral surface of the end of the first member and the surface of the end of the second member so as to integrally cover them.

[0087] As described above, the first member has a porous substrate and a molecular sieve membrane, and therefore has minute irregularities on its outer peripheral surface. For this reason, in order to connect the first member and the second member while ensuring sealing performance with materials such as fluororesin that have been conventionally used, it was necessary to use additives such as grease and silicone rubber to deal with the irregularities on the outer peripheral surface. By using the connecting member according to the present invention to connect the first member and the second member, the connecting member itself adheres closely to the irregularities on the outer peripheral surface of the first member, ensuring sealing performance, and the process of using additives is not required.

[0088] <Method of tensile test for connection members> The physical properties of the connection member after heat shrinkage are calculated from the stress-strain curve obtained in the tensile test. The test pieces used in this case are prepared as follows. The connection member cut to 6-7 cm is placed around the first member and heat-shrunk using a heat gun until it is in close contact with the first member. After that, a cut is made in the axial direction to peel off the material into a sheet, and the short side is cut so that it is smaller than the width of the manual fixed-position wedge-shaped grip of the tensile tester. The thickness and length of the short side of the rectangular test piece are measured at three points using a vernier caliper, and the arithmetic average is taken, and then the cross-sectional area is calculated. The thickness is measured at three points on the center line of the test piece in the longitudinal direction, 1 cm from both ends and at equidistant points from both ends, and the arithmetic average is taken. The length of the short side is the arithmetic average of three straight lines parallel to the short side that intersect with the point where the thickness was measured. Three test pieces are prepared for each connection member. A tensile tester is used for the tensile test. The test specimen was gripped by a manual fixed-position wedge grip at least 1 cm in the longitudinal direction, and the tensile test was performed at a tensile speed of 1 mm / min. The software used for data processing was Shimadzu Corporation's TRAPEZIUM X (version 1.5.2) or a successor software capable of equivalent processing. The stress-strain curve was obtained by dividing the obtained test force by the cross-sectional area on the Y-axis and dividing the travel distance of the grip by the distance between the tips of the initial grips on the X-axis.

[0089] <Analysis of stress-strain curve> The slope of the change in stress was calculated from the difference in the stress values ​​between 0.75 and 1.0 on the obtained stress-strain curve. The calculation method is as follows. Slope = ((stress at 0.75 strain) - (stress at 1.0 strain)) / (1.0 - 0.75) The above-mentioned slope was calculated from the test results of three samples, and the average value was used for the evaluation.

[0090] The slope of the stress change within the above-mentioned range of strain is a value indicating the magnitude of the stress after the connecting member has been stretched to a certain extent, which can be said to be a value related to the strength of the connecting member to hold the first and second members together when used in a molecular sieve membrane element.

[0091] The following examples are provided to specifically explain the embodiments of the present invention. Of course, the present invention is not limited to the following examples, and various modifications are possible in detail. EXAMPLES

[0092] (Method of tensile test for connection members) The physical properties of the connection member after heat shrinkage were calculated from the stress-strain curve obtained in the tensile test. The test pieces used were prepared as follows. The connection member cut to 6-7 cm was placed around the first member and heat-shrunk using a heat gun until it was in close contact with the first member. After that, a cut was made in the axial direction to peel off the connection member into a sheet, and the short side was cut so that it was smaller than the width of the manual fixed-position wedge-shaped grip of the tensile tester. The thickness and length of the short side of the rectangular test piece were measured at three points using a vernier caliper, and the arithmetic average was taken, and then the cross-sectional area was calculated. The thickness was measured at three points on the center line of the test piece in the longitudinal direction, 1 cm from both ends and at an equal distance from both ends, and the arithmetic average was taken. The length of the short side was determined as the arithmetic average of three straight lines parallel to the short side that intersected with the point where the thickness was measured. Three test pieces were prepared for each connection member. A Shimadzu AGS-X10kN was used for the tensile tests. The test pieces were gripped at least 1cm in the longitudinal direction using a manual fixed-position wedge-shaped grip, and the tensile tests were performed at a tensile speed of 1mm / min. The software used for data processing was Shimadzu TRAPEZIUM X (version 1.5.2). A stress-strain curve was obtained by dividing the obtained test force by the cross-sectional area (stress) on the Y-axis and dividing the movement distance of the grip by the initial distance between the tips of the grips (strain) on the X-axis.

[0093] <Analysis of stress-strain curve> The slope of the change in stress was calculated from the difference in the stress values ​​between 0.75 and 1.0 on the obtained stress-strain curve. The calculation method is as follows. Slope = ((stress at 0.75 strain) - (stress at 1.0 strain)) / (1.0 - 0.75) The above-mentioned slope was calculated from the test results of three samples, and the average value was used for the evaluation.

[0094] [Example 1] <First component> A first member (11) having a zeolite membrane as a molecular sieve membrane on the outer peripheral surface of a porous substrate was produced with reference to WO2013 / 125660. That is, a porous alumina tube (outer diameter 12 mm, inner diameter 9 mm) was used as the inorganic porous support.

[0095] <Second member> As the second member (12), a cylindrical member made of SUS304 having an outer diameter of φ12 mm and a length of 16 mm was produced.

[0096] <Connection using connecting parts> A heat-shrinkable silicone tube (13) (ST-65DG manufactured by Shin-Etsu Chemical Co., Ltd.) having a length of 20 mm and an inner diameter of 11.0 to 14.0 mm was prepared as a connecting member. Next, one end of the first member (11) was inserted from one end side of the connecting member (13), one end of the second member (12) was inserted from the other end side of the connecting member (13), and the connecting member (13) was provided around the end of the first member (11) and the end of the second member (12) by a method of coaxially butting the end face of the first member (11) and the end face of the second member (12) in the connecting member (13).

[0097] Next, the first member (11), the second member (12), and the connecting member (13) were heated as a whole while rotating with a heat gun, whereby the connecting member (13) was thermally shrunk and brought into close contact with an end of the first member (11) and an end of the second member (12), thereby obtaining a molecular sieve membrane element (1). In this molecular sieve membrane element (1), the heat-shrinkable silicone tube (13) is brought into close contact, thereby fixing and sealing the connecting portion between the first member (11) and the second member (12).

[0098] As the further covering member, a piece of fluororesin heat-shrinkable tube (14) (Junflon NF120 manufactured by Junkosha) having a length of 30 mm and an inner diameter of 13 mm was prepared. The molecular sieve membrane element (1) was inserted into the further covering member (14), and the further covering member (14) was arranged so as to cover the entire connecting member (13) and the outer peripheral surface of the first member (11) and the outer peripheral surface of the second member (12) within a range of 10 mm on both sides of the connecting member (13). Next, the further covering member (14) was heat-shrunk by heating with a heat gun, and was brought into close contact with the outer peripheral surfaces of the first member (11), the second member (12), and the connecting member (13).

[0099] A tensile test was carried out on a heat-shrinkable silicone tube (ST-65DG manufactured by Shin-Etsu Chemical Co., Ltd.) under the above conditions. The results are shown in Figure 2. The slope of the stress at a strain of 0.75-1.0 obtained under the above analysis conditions was 1.22. The tensile strength of the heat-shrinkable silicone tube used was 6.0 MPa.

[0100] [Example 2] Except for using an electron beam cross-linked soft polyolefin resin tube (Sumitomo Electric Industries, Sumitube A, inner diameter 13.0 mm) as the connecting member, the first member and the second member were connected in the same manner as in Example 1. The tensile strength of the electron beam cross-linked soft polyolefin resin tube used was 19.2. A tensile test was carried out on the electron beam cross-linked soft polyolefin resin tube in the same manner as in Example 1. The results are shown in Figure 3. The gradient of the stress at a strain of 0.75-1.0 obtained under the above analysis conditions was 0.99.

[0101] [Comparative Example 1] The first member (11), the second member (12) and the further covering member (14) were the same as those in Example 1.

[0102] An addition reaction type silicone rubber precursor (KE-1885 manufactured by Shin-Etsu Chemical Co., Ltd.) was applied to the outer peripheral surface of one end of the first member (11) and one end of the second member (12). Specifically, the addition reaction type silicone rubber precursor was applied to a thickness of 0.2 mm over the entire outer peripheral surface of one end of the first member (11) within a range of about 24 mm in width, and over the entire outer peripheral surface of one end of the second member (12) within a range of about 16 mm in width.

[0103] Next, one end of the first member (11) was inserted into one end of a heat-shrinkable tube (14) serving as a covering material, and one end of the second member (12) was inserted into the other end of the heat-shrinkable tube (14), and the first member (11) and the second member (12) were butted together coaxially within the heat-shrinkable tube (14) and positioned so that the entire applied addition reaction type silicone rubber precursor was covered with the heat-shrinkable tube (14). Next, the heat-shrinkable tube (14) was heated with a heat gun to thermally shrink the heat-shrinkable tube (14) and bring it into close contact with the silicone rubber precursor.

[0104] Thereafter, the connection portion of the first member (11) and the second member (12) covered with the heat shrink tube (4) was heated at 155°C for 1 hour to harden the silicone rubber precursor, thereby obtaining a molecular sieve membrane element (1). In this molecular sieve membrane element (1), the first member (11) and the second member (12) were fixed by the heat shrink tube (14) via an intermediate layer made of addition reaction type silicone rubber, and the connected portion was sealed. That is, the intermediate layer made of addition reaction type silicone rubber in Comparative Example 1 corresponds to the connection member (13) in Example 1.

[0105] [Comparative Example 2] Except for using an electron beam cross-linked soft flame-retardant fluoroelastomer resin tube (Sumitomo Electric Industries, Sumitube KH200, inner diameter 12.7 mm) as the connecting member, an attempt was made to connect the first member and the second member in the same manner as in Example 1. However, when using only the electron beam cross-linked soft flame-retardant fluoroelastomer resin tube for the connection, the binding force was so weak that when one of the members was held, the other member would fall, and the connection could not be maintained. A tensile test was carried out on the electron beam cross-linked soft flame-retardant fluoroelastomer resin tube in the same manner as in Example 1. The results are shown in Figure 4. The gradient of the stress at a strain of 0.75-1.0 obtained under the above analysis conditions was 0.68. The tensile strength of the electron beam cross-linked soft flame-retardant fluoroelastomer resin tube used was 28.2.

[0106] The molecular sieve membrane elements prepared in Example 1 and Comparative Example 1 were used to carry out the tests described below. By carrying out the permeation test using relatively large gas molecules that are difficult to permeate through the molecular sieve membrane, the leakage from the sealed connection part can be observed as the flow rate of the gas molecules. Therefore, in the gas permeation test (A) described below, the gas permeation test was carried out using sulfur hexafluoride.

[0107] On the other hand, by comparing the results of a permeation test using gas molecules that easily permeate the molecular sieve membrane with the results of a permeation test using relatively large gas molecules that do not easily permeate the molecular sieve membrane, the performance of the molecular sieve membrane element can be clarified. Therefore, in the gas permeation test (B) described below, a gas permeation test was performed using carbon dioxide.

[0108] [Test: Gas permeability test (A)] The gas permeation test was performed using a separation membrane module (2) as shown in FIG. 1 and sulfur hexafluoride as the gas molecules. The separation membrane module (2) includes a pressure vessel (3), a molecular sieve membrane element (1) disposed in the pressure vessel (3), and a pipe (6) connected to a first member (11) of the molecular sieve membrane element (1) by a connection member (13) and a covering member (14). Specifically, sulfur hexafluoride was introduced into the pressure vessel (3) as the supply gas (4), and the permeated gas (5) that permeated the molecular sieve membrane element (1) was measured by a flow meter (not shown) connected to the pipe (6). In addition, a purging process was performed with the supply gas to be used to remove components such as moisture and air. The permeated gas flow rate was measured after the permeated gas flow rate stabilized while keeping the sample temperature constant and the pressure on the supply gas side at 0.1 MPaG and the pressure on the permeated gas side at 0.00 MPaG.

[0109] [Test: Gas permeability test (B)] A gas permeation test was carried out in the same manner as in Gas Permeation Test (A), except that carbon dioxide was used as the gas molecule.

[0110] <Test Results of Example 1> The molecular sieve membrane element produced in Example 1 had a significantly low sulfur hexafluoride permeation rate of 0.3 sccm. The carbon dioxide permeation rate was 488 sccm, which was sufficiently higher than that of sulfur hexafluoride. The ratio of carbon dioxide permeation rate to sulfur hexafluoride permeation rate was 1627, and it was confirmed that the use of a silicone heat shrink tube ensured sufficient sealing performance.

[0111] <Test Results of Example 2> The molecular sieve membrane element produced in Example 2 had a significantly low sulfur hexafluoride permeation rate of 0.43 sccm. The carbon dioxide permeation rate was 492 sccm, which was sufficiently higher than that of sulfur hexafluoride. The ratio of carbon dioxide permeation rate to sulfur hexafluoride permeation rate was 1132, and it was confirmed that the use of the electron beam crosslinked soft polyolefin resin tube ensured sufficient sealing performance. Thus, the molecular sieve membrane elements prepared in Examples 1 and 2 can be used as molecular sieve membrane elements exhibiting sufficiently high separation performance for separating gases.

[0112] [Summary of considerations regarding test results] As can be seen from the test results, the molecular sieve membrane elements obtained in Examples 1 and 2 had excellent sealing properties. This is believed to be because the use of a connecting member with a stress-strain curve slope of 0.69 or more when the strain in the tensile test is 0.75 to 1.0 or less provides high adhesion to the molecular sieve membrane surface and maintains excellent sealing properties. The electron beam cross-linked soft flame-retardant fluoroelastomer resin tube used in Comparative Example 2 was unable to hold the connection target by itself. Although there is a possibility of connection by using an additional covering member, there is a disadvantage in that one process is added to the production of the molecular sieve membrane element. In addition, even if an additional covering member is used, it is questionable whether adhesion to the member can be ensured.

[0113] The molecular sieve membrane elements of Examples 1 and 2, which are excellent as described above, are produced by a simple process of placing a tubular member across the boundary between the first and second members and heating it, and this process time can be significantly reduced compared to the time-consuming sealing process using the addition reaction type silicone rubber of Comparative Example 1. Therefore, the manufacturing workability is good, and further improvement in productivity is expected. [Industrial Applicability]

[0114] INDUSTRIAL APPLICABILITY The molecular sieve membrane element of the present invention is expected to improve productivity and is therefore suitable for use in separating gas or liquid mixtures, and is expected to contribute to the expansion and development of the technical field of said separation. [Explanation of symbols]

[0115] 1. Molecular sieve membrane element 11 First member 12 Second member 13 Connection parts 14 Further covering materials

Claims

1. A first member having a molecular sieve membrane on the inner wall and / or the outer wall of a tubular porous substrate; a second member having an end portion, the second member being disposed coaxially with the first member and connected to at least one end portion of the first member by a connecting member; the connecting member is a covering member made of heat-shrinkable silicone that covers an outer surface of an end of the first member that is parallel to the axial direction of the first member and an outer surface of an end of the second member, the molecular sieve membrane element.

2. The molecular sieve membrane element according to claim 1 , further comprising an additional covering member covering at least a portion of the connecting member.

3. The molecular sieve membrane element according to claim 2 , wherein the further covering member is made of a fluororesin.

4. 2. The molecular sieve membrane element according to claim 1, wherein no filler is present between the connecting member and an outer side surface parallel to the axial direction of the first member and a surface of the end of the second member.

5. The molecular sieve membrane element according to claim 1 , wherein the molecular sieve membrane is a zeolite membrane.

6. A first member having a molecular sieve membrane on the inner wall and / or the outer wall of a tubular porous substrate; a second member having an end portion, the second member being disposed coaxially with the first member and connected to at least one end portion of the first member by a connecting member; the connecting member has a covering member that covers an outer surface of an end of the first member that is parallel to an axial direction of the first member and an outer surface of an end of the second member, The covering member has heat shrinkability, a gradient of a stress-strain curve of 0.69 or more when the strain in a tensile test is 0.75 or more and 1.0 or less, and a tensile strength of 28 MPa or less.

7. A method for producing a molecular sieve membrane element according to any one of claims 1 to 6, disposing the first member and the second member coaxially; a step of circumferentially providing the connection member on an end portion of the first member and an end portion of the second member; a step of heating and shrinking the connection member to cover surfaces of the end portion of the first member and the end portion of the second member with the connection member; A method for producing a molecular sieve membrane element comprising the steps of:

Citation Information

Patent Citations

  • Molecular sieve membrane element and manufacturing method therefor

    JP2022037674A

Cited By

  • Dispersion stabilizer based on at least two types of polyols and method for preparing the same