Resin composition
A blend of aromatic polyetherketone resin with other resins enhances crystallinity, addressing issues of non-uniformity and inefficiency in molding processes, resulting in improved mechanical properties and productivity.
Patent Information
- Application Number
- JP2024057645
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-03-31
- Filing Date
- 2024-03-29
- Publication Date
- 2024-10-15
AI Technical Summary
Aromatic polyetherketone resins often exhibit insufficient crystallinity, leading to non-uniform molecular states in molded products, rapid deterioration of mechanical properties at high temperatures, and inefficient molding processes due to prolonged cooling times, resulting in poor productivity and moldability.
A blend composition of aromatic polyetherketone resin with other resins such as polyetherketone, polyetheretherketone, or polyetherketoneketone is created, ensuring a high content of aromatic polyetherketone resin and specific thermal properties to enhance crystallinity.
The blend composition promotes crystallization, improving mechanical properties and moldability, thereby enhancing the productivity and physical properties of the resin.
Smart Images

Figure 2024146919000001 
Figure 2024146919000002 
Figure 2024146919000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a resin composition. [Background technology]
[0002] Aromatic polyether ketone resins (hereinafter referred to as "PAEK resins") are so-called super engineering plastics (hereinafter referred to as "super engineering plastics") that have excellent mechanical properties such as heat resistance, chemical resistance, toughness, and dimensional stability, and are widely used in electrical and electronic parts, automotive parts, medical parts, fibers, films, and other applications.
[0003] For example, aromatic polyether ether ketone resin (hereinafter referred to as "PEEK resin"), which is one type of PAEK resin, has two ether moieties and one ketone moiety in the repeating structure of the resin, and is known to exhibit high thermal stability and mechanical properties as a partially crystalline resin due to their high order regularity (Patent Document 1). [Prior art documents] [Patent documents]
[0004] [Patent Document 1] Japanese Patent Application Publication No. 54-90296 Summary of the Invention [Problem to be solved by the invention]
[0005] If the crystallinity of a resin is insufficient, problems due to crystallinity will occur, such as the molecular state of the entire molded product not being uniform when it is made into a molded product, making it difficult for the resin to exhibit sufficient physical properties, and the tendency for mechanical properties to rapidly decrease in high temperature ranges. Also, if a long crystallization time is secured in the molding process in order to increase the crystallinity of a resin with poor crystallinity, the process of cooling the molten resin will become long and expensive, resulting in a resin with poor moldability and productivity.
[0006] Depending on the type, PAEK resin may have insufficient crystallinity, which may cause the above-mentioned problems when used as a material.
[0007] That is, an object of the present invention is to solve the above-mentioned conventional problems, promote the crystallization of an aromatic polyether ketone resin, and provide a highly crystalline resin composition. [Means for solving the problem]
[0008] Therefore, the present inventors have discovered that a highly crystalline resin composition with improved crystallinity can be obtained by blending a PAEK resin, which has insufficient crystallinity, with another resin, and have completed the following invention.
[0009] That is, the gist of the present invention is as follows. [1] A resin composition comprising an aromatic polyetherketone resin X containing a repeating unit represented by the following general formula (1) and at least one resin Y different from the aromatic polyetherketone resin X, wherein the resin Y is any one of polyetherketone, polyetheretherketone, polyetherketoneketone, polyetheretherketoneketone, and polyetherketoneetherketoneketone:
[0010] [ka]
[0011] (In the general formula (1), Structure A is any one selected from the group consisting of the following general formulae (2), (3) and (4), and Structure B is an optionally substituted divalent aromatic hydrocarbon ring.)
[0012] [ka]
[0013] [2] The resin composition according to [1], wherein the structure A is the formula (2).
[0014] [3] The resin composition according to [1] or [2], wherein the mass of the aromatic polyether ketone resin X containing the repeating unit represented by the general formula (1) is 50 mass% or more based on the total mass of the resin composition.
[0015] [4] The resin composition according to any one of [1] to [3], wherein the resin Y is any one of polyether ketone, polyether ether ketone, and polyether ketone ketone. [5] The resin composition according to any one of [1] to [4], wherein Tmc2-Tmc1≧5(°C), where Tmc1 is the melt crystallization temperature of the aromatic polyether ketone resin X containing a repeating unit represented by the general formula (1) and Tmc2 is the melt crystallization temperature of the resin composition.
[0016] [6] The resin composition according to any one of [1] to [5], wherein an estimated value of the heat of melt crystallization originating from aromatic polyether ketone resin X in the resin composition, which is obtained by multiplying the heat of melt crystallization of aromatic polyether ketone resin X containing a repeating unit represented by general formula (1) by mass fraction, is ΔHmc(est), and the heat of melt crystallization corresponding to a peak originating from the crystallization of aromatic polyether ketone resin X in the resin composition is ΔHmc(exp) / ΔHmc(est)≧1.1.
[0017] The "heat of melting and crystallization corresponding to the peak derived from the crystallization of the aromatic polyether ketone resin X in the resin composition" refers to the heat of melting and crystallization corresponding to the peak derived from the crystallization of the aromatic polyether ketone resin X detected when the resin composition is analyzed by DSC.
[0018] [7] The resin composition according to any one of [1] to [6], wherein an estimated value of the heat of fusion originating from aromatic polyether ketone resin X in the resin composition, which is obtained by multiplying the heat of fusion of aromatic polyether ketone resin X containing a repeating unit represented by general formula (1) by mass fraction, is ΔHm(est), and a heat of fusion corresponding to a peak originating from crystalline melting of aromatic polyether ketone resin X in the resin composition is ΔHm(exp) / ΔHm(est)≧1.1.
[0019] The "heat of fusion corresponding to the peak derived from the crystalline melting of the aromatic polyether ketone resin X in the resin composition" refers to the heat of fusion corresponding to the peak derived from the crystalline melting of the aromatic polyether ketone resin X detected when the resin composition is analyzed by DSC. Effect of the Invention
[0020] According to the present invention, by preparing a resin composition containing a predetermined aromatic polyetherketone resin X and a resin Y different from the resin X, where the resin Y is a polyetherketone resin, crystallization of the aromatic polyetherketone resin X is promoted, and a highly crystalline resin composition can be obtained. By forming a highly crystalline resin composition, the above-mentioned problems in terms of the resin properties and the problems of poor moldability and productivity can be solved. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0021] The present invention will be described in detail below, but the present invention is not limited to the following description, and can be modified in any manner without departing from the gist of the present invention. In this specification, when "A to B" is used with a numerical value or a physical property value between the two sides (A and B represent numerical values or physical property values), this means "greater than or equal to A and less than or equal to B."
[0022] Furthermore, the term "aromatic" encompasses "heteroaromatic" and also encompasses forms containing a heteroatom, which is an element other than carbon, in the ring structure.
[0023] The following describes in detail an embodiment of the present invention. The description of the components described below is an example (representative example) of an embodiment of the present invention, and the present invention is not limited to the following content as long as it does not exceed the gist of the present invention.
[0024] <Resin composition> The resin composition of the present invention is a resin composition comprising a predetermined aromatic polyetherketone resin X and at least one polyetherketone resin different from said resin X (resin Y).
[0025] (Aromatic polyether ketone resin X) The predetermined aromatic polyether ketone resin X in the present invention is an aromatic polyether ketone resin X containing a repeating unit represented by the following general formula (1). Here, the term "polyetherketone" is not limited to polyetherketone in the narrow sense, which contains one ether bond and one ketone bond in one repeating unit, but refers to polyetherketone in the broad sense. The broad sense of polyetherketone means that it may include a resin skeleton that may have multiple ether bonds and multiple ketone bonds in one repeating unit, such as polyetherketone (PEK), polyetheretherketone (PEEK), polyetherketoneketone (PEKK), polyetheretherketoneketone (PEEKK), and polyetherketoneetherketoneketone (PEKEKK).
[0026] [ka]
[0027] In the formula (1), the structure A is any one selected from the group consisting of the following formulae (2), (3) and (4), and the structure B is an optionally substituted divalent aromatic hydrocarbon ring. In the figure, * indicates a binding site.
[0028] [ka]
[0029] Specific examples of the structure A include the following.
[0030] [ka]
[0031] The structure A is preferably any one of the above general formula (2), i.e., A-1 to A-4, and more preferably A-1. In this way, by using PAEK (FDCA-PAEK) having furandicarboxylic acid (FDCA) as a structural unit as a component of the resin composition, it is expected that the environmental load can be reduced because FDCA is obtained from bio-derived raw materials.
[0032] The optionally substituted divalent aromatic hydrocarbon ring of structure B is preferably a substituted or unsubstituted aromatic hydrocarbon ring having 6 to 30 carbon atoms. A structure in which a plurality of aromatic hydrocarbon rings are linked may also be used, but the linkage of the aromatic hydrocarbon rings is preferably a direct linkage of the aromatic rings, or when the linkage is via a substituent, the substituent preferably does not contain an ether group. Moreover, it is more preferable that the aromatic hydrocarbon ring is unsubstituted.
[0033] Specifically, the structure B is preferably any one selected from the group consisting of the following general formulae (5) to (14).
[0034] [ka]
[0035] In formula (7), n1 is preferably 0 or 1. In formula (12), R 1 , R 2 are hydrocarbon groups which may be the same or different, each of which may have an alicyclic skeleton or an aromatic skeleton and may have a substituent.
[0036] More specifically, the structure B includes the following formulae B-1 to B-17.
[0037] [ka]
[0038] As the structure B, B-1, B-5, B-6, B-7, B-8, B-9, B-13, B-14, B-15, B-16, and B-17 are preferred, and among them, B-1, B-5, and B-6 are more preferred. The aromatic polyether ketone resin X containing the repeating unit represented by formula (1) may have two or more types of structures B, and among these, preferably, the aromatic polyether ketone resin X may contain two or more types selected from B-1, B-5, B-6, B-7, B-8, B-9, B-13, B-14, B-15, B-16, and B-17, and more preferably, the aromatic polyether ketone resin X may contain two or more types selected from B-1, B-5, and B-6.
[0039] Specific examples of the repeating unit represented by formula (1) are given below.
[0040] [ka]
[0041] [ka]
[0042] [ka]
[0043] [ka]
[0044] [ka]
[0045] [ka]
[0046] [ka]
[0047] [ka]
[0048] [ka]
[0049] [ka]
[0050] [ka]
[0051] [ka]
[0052] [ka]
[0053] Among the above specific examples, from the viewpoint of easily obtaining a crystallinity improving effect by forming the resin composition of the present invention, it is preferable that Resin X has a repeating unit represented by (1)-1, (1)-2, or (1)-4, and among these, it is particularly preferable that Resin X has a repeating unit represented by (1)-1 or both repeating units represented by (1)-1 and (1)-2.
[0054] The aromatic polyether ketone resin X is preferably crystalline. The melting point of the aromatic polyether ketone resin X is preferably 250° C. or higher, more preferably 280° C. or higher, further preferably 300° C. or higher, and particularly preferably 320° C. or higher.
[0055] The reduced viscosity of the aromatic polyether ketone resin X of the present invention is usually 0.6 dL / g or more. Also, it is preferably 0.8 dL / g or more, and particularly preferably 0.9 dL / g or more. On the other hand, the reduced viscosity of the aromatic polyether ketone resin X of the present invention is usually 3.5 dL / g or less, preferably 3.0 dL / g or less, more preferably 2.5 dL / g or less, even more preferably 2.0 dL / g or less, particularly preferably 1.9 dL / g or less, particularly preferably 1.8 dL / g or less, particularly preferably 1.7 dL / g or less, and most preferably 1.6 dL / g or less. The reduced viscosity (ηsp / c) of aromatic polyetherketone resin X in the present invention is calculated by dissolving the resin in concentrated sulfuric acid at a concentration c=0.1 g / dL, measuring the specific viscosity (ηsp) at 25°C using an Ubbelohde viscometer, and dividing the measured value by the concentration c. It is known that the reduced viscosity correlates with the molecular weight of the resin, and it is common to compare the molecular weight of aromatic polyetherketone resin X relatively using the reduced viscosity value. In other words, if the reduced viscosity of aromatic polyetherketone resin X is 0.6 dL / g or more, it can be said that the molecular weight is sufficiently high to the extent that the properties do not change significantly due to molding processing.
[0056] (Resin Y) Examples of the resin Y constituting the resin composition of the present invention include polyether ketone (PEK), polyether ether ketone (PEEK), polyether ketone ketone (PEKK), polyether ether ketone ketone (PEEKK), polyether ketone ether ketone ketone (PEKEKK), etc. Among these, PEK, PEEK, and PEKK are preferred, and PEEK is the most preferred.
[0057] PEEK has the following structure:
[0058] [ka]
[0059] n means the degree of polymerization of the repeating unit.
[0060] The polyetherketone resin is preferably crystalline. The melting point of the polyetherketone resin is preferably higher than the melting point of the aromatic polyetherketone resin X represented by the general formula (1) above. The melting point of the polyetherketone resin is preferably 300°C or higher, more preferably 320°C or higher, further preferably 330°C or higher, and particularly preferably 335°C or higher.
[0061] The polyether ketone resin has a melt viscosity at 400° C., measured in accordance with ISO 11443, of preferably 80 to 700 Pa·s, more preferably 200 to 600 Pa·s, and further preferably 300 to 500 Pa·s.
[0062] In addition, the polyetherketone resin preferably has good dispersibility in the aromatic polyetherketone resin X, and from this point of view, it is preferable that the polyetherketone resin has the above-mentioned crystallinity, preferable melting point, and melt viscosity. In the present invention, it is preferable that the polyetherketone resin has good dispersibility in the aromatic polyetherketone resin X, but that they are not completely miscible with each other.
[0063] (Composition of Resin Composition) In the resin composition of the present invention, the proportion of the aromatic polyether ketone resin X containing a repeating unit represented by general formula (1) is preferably 50 mass % or more, more preferably 60 mass % or more, even more preferably 70 mass % or more, particularly preferably 80 mass % or more, and most preferably 90 mass % or more, based on the entire resin composition.
[0064] In the resin composition of the present invention, the greater the proportion of aromatic polyetherketone resin X containing a repeating unit represented by general formula (1), the greater the crystallinity improving effect of the blended polyetherketone resin. Furthermore, since the aromatic polyetherketone resin X can be contained in a high content in the resulting resin composition, it becomes possible to improve the crystallinity of the entire resin composition while enjoying the properties of the aromatic polyetherketone resin X itself.
[0065] From the viewpoint of reducing the overall cost of the resin composition by increasing the content of inexpensive polyetherketone resin while containing a certain amount of the aromatic polyetherketone resin X, and obtaining a highly crystalline resin composition, the proportion of the aromatic polyetherketone resin X containing a repeating unit represented by general formula (1) is preferably 50 mass % or less, more preferably 40 mass % or less, further preferably 30 mass % or less, particularly preferably 20 mass % or less, and most preferably 10 mass % or less, based on the entire resin composition.
[0066] (Thermal properties of resin composition) The thermal properties of the resin composition of the present invention were measured using a differential scanning calorimeter "DSC7020" (manufactured by Hitachi High-Tech Science Corporation) by heating about 2 mg of the resin composition from 30°C to 360°C at a rate of 10°C / min (1st heating), then cooling from 360°C to 30°C at a rate of 10°C / min (1st cooling), and further heating from 30°C to 360°C at a rate of 10°C / min (2nd heating). The results are shown below.
[0067] In addition, in the evaluation of the thermal properties of the resin composition by DSC, signals derived from both a phase mainly containing aromatic polyether ketone resin X having a repeating structure of general formula (1) in the composition and a phase mainly containing polyether ketone resin may be observed, but each value below means a value of the phase mainly containing aromatic polyether ketone resin X having a repeating structure of general formula (1) (when values are described in two rows in the examples, the value in the upper row is used).
[0068] 1st heating The glass transition temperature (Tg) in the first heating is preferably 130 to 170°C, and more preferably 140 to 160°C. The cold crystallization temperature (Tcc) in the first heating is preferably 160 to 200°C, and more preferably 180 to 195°C. The heat of cold crystallization (ΔHcc) in the first heating is preferably 5 to 40 J / g, and more preferably 25 to 35 J / g. The melting point (Tm) in the first heating is preferably 250 to 330°C, and more preferably 270 to 300°C. The heat of fusion (ΔHm) in the first heating is preferably 5 to 40 J / g, and more preferably 20 to 38 J / g.
[0069] 1st cooling The melt crystallization temperature (Tmc) in the first cooling is preferably from 210 to 250°C, and more preferably from 220 to 240°C. The heat of melting and crystallization (ΔHmc) at the 1st cooling is preferably from 5 to 40 J / g, and more preferably from 20 to 35 J / g.
[0070] 2nd calibration The preferred ranges of Tg and Tm in the 2nd heating of the resin composition of the present invention are the same as those in the 1st heating. Since the resin composition of the present invention is sufficiently crystallized in the process of the first cooling, the crystallization peak becomes small in the second heating, and Tcc and ΔHcc tend not to be observed. It should be noted that the larger the values of Tmc, ΔHmc, and ΔHm, the higher the crystallinity.
[0071] Here, when the melt crystallization temperature of the aromatic polyether ketone resin X containing the repeating unit represented by the general formula (1) is Tmc1 and the melt crystallization temperature of the resin composition is Tmc2, it is preferable that Tmc2-Tmc1 ≧ 5 (°C), more preferably Tmc2-Tmc1 ≧ 10 (°C), even more preferably Tmc2-Tmc1 ≧ 18 (°C), and even more preferably Tmc2-Tmc1 ≧ 25 (°C). By being in such a range, it can be said that a composition with excellent crystallinity in which crystallization starts at a higher temperature is obtained.
[0072] In the above, the melt crystallization temperature at 1st cooling of the resin composition may show two types of values, a value corresponding to the aromatic polyetherketone resin X containing a repeating unit of formula (1) and a value corresponding to -polyetherketone resin, as in each composition in the following Examples, but the "melt crystallization temperature (Tmc2) of the resin composition" in the above means the value corresponding to the melt crystallization of the phase mainly containing the aromatic polyetherketone resin X containing a repeating unit of formula (1) (i.e., the value in the upper row in each Example). The melt crystallization temperature Tmc1 of the aromatic polyether ketone resin X means an inherent value (values in Comparative Examples 1 and 2) observed when the aromatic polyether ketone resin X is subjected to thermal analysis alone.
[0073] In addition, when the estimated value of the melt crystallization heat derived from the aromatic polyether ketone resin X in the resin composition, which is obtained by multiplying the melt crystallization heat (ΔHmc) of the aromatic polyether ketone resin X containing the repeating unit represented by the general formula (1) by the mass fraction, is ΔHmc(est), and the measured value of the melt crystallization heat corresponding to the peak derived from the crystallization of the aromatic polyether ketone resin X in the resin composition is ΔHmc(exp), it is preferable that ΔHmc(exp) / ΔHmc(est)≧1.1, more preferably ΔHmc(exp) / ΔHmc(est)≧2.0, even more preferably ΔHmc(exp) / ΔHmc(est)≧3.0, particularly preferably ΔHmc(exp) / ΔHmc(est)≧3.2, and most preferably ΔHmc(exp) / ΔHmc(est)≧3.5. By being in such a range, it can be said that a composition with excellent crystallinity in which melt crystallization proceeds to a higher degree than the original resin X is obtained.
[0074] Furthermore, when the estimated value of the heat of fusion derived from the aromatic polyetherketone resin X in the resin composition, which is obtained by multiplying the heat of fusion (ΔHm) of the aromatic polyetherketone resin X containing the repeating unit represented by the general formula (1) by the mass fraction, is ΔHm(est), and the measured value of the heat of fusion corresponding to the peak derived from the crystal melting of the aromatic polyetherketone resin X in the resin composition is ΔHm(exp), it is preferable that ΔHm(exp) / ΔHm(est)≧1.1, more preferably ΔHm(exp) / ΔHm(est)≧1.2, even more preferably ΔHm(exp) / ΔHm(est)≧1.25, particularly preferably ΔHm(exp) / ΔHm(est)≧1.4, and particularly preferably ΔHm(exp) / ΔHm(est)≧1.5. By being in such a range, it can be said that a composition having excellent crystallinity and improved crystallinity is obtained compared to the original resin X.
[0075] (Additives, etc.) The resin composition of the present invention can be mixed with other resins and additives other than the aromatic polyether ether ketone resin containing the repeating unit of the above general formula (1) or the polyether ketone resin, as long as the effects of the present invention are not impaired, depending on the application, required performance, etc. The other resins and additives used may be used alone or in combination of two or more. Other resins include polyphenylene sulfide resin, polyetherimide resin, LCP (liquid crystal polymer), polyphenylsulfone resin, polyethersulfone resin, polyphthalamide resin, polysulfone resin, polyimide resin, and epoxy resin.
[0076] The additive is not particularly limited and can be appropriately selected according to the purpose, and examples thereof include inorganic fillers and organic fillers. The shape of the filler is not particularly limited and examples thereof include particulate, plate-like, fibrous, and other fillers. Among fibrous fillers, carbon fiber and glass fiber are preferred because they have a wide range of industrial applications.
[0077] Furthermore, there are no particular limitations on the additives other than the filler, and additives such as heat stabilizers, antioxidants, lubricants, antiblocking agents, nucleating agents, colorants, pigments, ultraviolet absorbers, light stabilizers, modifiers, crosslinking agents, etc. may be contained.
[0078] <Method of producing resin composition> The method for producing the resin composition of the present invention is not particularly limited, but includes a method of melt-mixing the blended raw material resin chips and additives in the same extruder, a method of melting and then mixing them in separate extruders, and mixing by kneading using a normal kneader such as a single-screw extruder, a twin-screw extruder, a Banbury mixer, a roll mixer, a Brabender plastograph, or a kneader blender. In this case, it is also possible to prepare the composition and obtain a molded product at the same time by directly feeding each raw material chip into a molding machine. In addition, the resin may be dissolved in an appropriate solvent to prepare a homogeneous solution, and then the solvent may be removed to obtain the composition.
[0079] <Molded object, application> The resin composition of the present invention can be molded into a molded article by a melt molding method such as injection molding or extrusion molding, or by a method of handling the resin composition as a solution using an appropriate good solvent, depending on the application and required performance. Specific examples of the shape and application of the molded article include films, fibers, pipes, rods, rings, gears, bearings, coating materials, and in vivo implant materials. As for the form of the molded article, the composition of the present invention alone may be used to construct the molded article, but it may also be combined with other materials in any shape as long as the properties of the composition can be exhibited, and used as a laminate, for example. EXAMPLES
[0080] The following examples of the resin composition of the present invention are given, but the present invention is not limited to these examples as long as the gist of the invention is not exceeded. The methods for measuring the various properties are as follows. <Thermal properties of resin composition or resin> The thermal properties of the resin composition or resin were measured using a differential scanning calorimeter "DSC7020" (manufactured by Hitachi High-Tech Science Corporation) by heating approximately 2 mg of the resin composition or resin from 30°C to 360°C at a rate of 10°C / min (1st heating), then cooling from 360°C to 30°C at a rate of 10°C / min (1st cooling), and further heating from 30°C to 360°C at 10°C / min (2nd heating). In the first and second heating, Tg, Tcc, ΔHcc, Tm, and ΔHm were measured, and in the first cooling, Tmc and ΔHmc were measured. In Table 1, ΔHm in the 1st heating corresponds to ΔHm(exp), and the estimated ΔHm value corresponds to ΔHm(est). In addition, in Table 1, ΔHmc at the 1st cooling corresponds to ΔHmc(exp), and the estimated ΔHmc value in Table 1 corresponds to ΔHmc(est).
[0081] <Synthesis Example 1> In a reaction vessel equipped with an agitator, a nitrogen inlet / vacuum inlet, and a heater, 7.09 parts by mass of bisfluorobenzoylfuran (BFBF), 2.50 parts by mass of hydroquinone (HQ), 3.17 parts by mass of potassium carbonate, 27.2 parts by mass of diphenyl sulfone, and 1.5 parts by mass of triglyme were charged. Nitrogen gas was introduced into the vessel while stirring the contents of the reaction vessel, and the system was placed under a nitrogen atmosphere by vacuum replacement. Next, the temperature was raised to 200°C while stirring the system, and the reaction was carried out at this temperature for 1 hour. Thereafter, the temperature was raised to 280°C over 5 minutes, and polycondensation was continued at this temperature for 2 hours. The polymerization product was removed from the reaction vessel and crushed with a hammer to make it into a powder form, and then washed by solid-liquid extraction with 157 parts by mass of acetone at room temperature for 15 minutes to recover the solid components. Washing with acetone was carried out again under the same conditions. Subsequently, washing by solid-liquid extraction with 200 parts by mass of water at 60°C for 15 minutes was carried out to recover the solid components. The mixture was washed again with water under the same conditions. After that, the mixture was washed by solid-liquid extraction with 103 parts by mass of N-methyl-2-pyrrolidone at 120°C for 30 minutes to recover the solid component. The filtered solid component was vacuum dried at 120°C for 6 hours in a vacuum dryer to obtain the target aromatic polyether ketone resin X1 having the skeleton of formula (1)-1.
[0082] <Synthesis Example 2> In a reaction vessel equipped with an agitator, a nitrogen inlet / vacuum inlet, and a heater, 22.7 parts by mass of bisfluorobenzoylfuran (BFBF), 0.80 parts by mass of hydroquinone (HQ), 14.0 parts by mass of 4,4'-dihydroxybenzophenone (DHBP), 10.1 parts by mass of potassium carbonate, 87.0 parts by mass of diphenylsulfone, and 4.8 parts by mass of triglyme were charged. Nitrogen gas was introduced into the vessel while stirring the contents of the reaction vessel, and the system was placed under a nitrogen atmosphere by vacuum replacement. Next, the temperature was raised to 200°C while stirring the system, and the reaction was carried out at this temperature for 1 hour. Thereafter, the temperature was raised to 280°C over 5 minutes, and polycondensation was continued at this temperature for 1 hour. The polymerization product was removed from the reaction vessel and crushed with a hammer to make it into a powder, and then washed by solid-liquid extraction with 784 parts by mass of acetone at room temperature for 15 minutes to recover the solid components. Washing with acetone was carried out again under the same conditions. Next, washing was performed by solid-liquid extraction with 1000 parts by mass of water at 60°C for 15 minutes, and the solid component was recovered. Washing with water was performed again under the same conditions. After that, washing was performed by solid-liquid extraction with 309 parts by mass of N-methyl-2-pyrrolidone at 120°C for 30 minutes, and the solid component was recovered. The filtered solid component was vacuum-dried at 120°C for 6 hours in a vacuum dryer to obtain the target aromatic polyether ketone resin X2 having the skeleton of formula (1)-1 and formula (1)-2.
[0083] <Example 1> As an aromatic polyetherketone resin containing a repeating unit of formula (1), aromatic polyetherketone resin X1 having 2,5-bis(4-fluorobenzoyl)furan (BFBF) and hydroquinone (HQ) as structural units produced in the above Synthesis Example 1 was used, and Victrex PEEK 650G (manufactured by Victrex) was used as the polyetherketone resin. 90 parts by mass of aromatic polyetherketone resin and 10 parts by mass of polyetherketone resin were weighed out and dissolved in 2710 parts by mass of pentafluorophenol (manufactured by Fujifilm Wako Pure Chemical Industries, Ltd.), and then 5500 parts by mass of chloroform (manufactured by Fujifilm Wako Pure Chemical Industries, Ltd.) were added to obtain a uniform resin solution. This resin solution was dropped into a large excess of methanol to recover the precipitated solid resin composition, which was then vacuum dried and subjected to the measurement of the above thermal properties. Table 1 shows the results of the thermal property measurement.
[0084] <Examples 2 and 3> A solid resin composition was obtained and the above thermal properties were measured in the same manner as in Example 1, except that the composition of the resins to be mixed was changed to the ratio shown in Table 1. Table 1 shows the results of the thermal property measurements. <Example 4> A solid resin composition was obtained in the same manner as in Example 1, except that the aromatic polyetherketone resin X1 was changed to the aromatic polyetherketone resin X2 having BFBF, HQ and 4,4'-dihydroxybenzophenone (DHBP) as structural units, which was produced in the above Synthesis Example 2, and the thermal properties were measured. Table 1 shows the results of the thermal property measurement. <Examples 5 and 6> A solid resin composition was obtained and the above thermal properties were measured in the same manner as in Example 4, except that the composition of the resins to be mixed was changed to the ratio shown in Table 1. Table 1 shows the results of the thermal property measurements.
[0085] <Comparative Example 1> The above thermal properties were measured using only the aromatic polyether ketone resin X1. Table 1 shows the results of the thermal property measurement. <Comparative Example 2> The above thermal properties were measured using only the aromatic polyether ketone resin X2. Table 1 shows the results of the thermal property measurement.
[0086] <Comparative Example 3> The thermal properties were measured using only the polyetherketone resin Victrex PEEK 650G. Table 1 shows the results of the thermal property measurements.
[0087] [Table 1]
[0088] In Table 1, when values are displayed in two rows, the values in the upper row are derived from the phase in the composition that mainly contains aromatic polyether ketone resin, and the values in the lower row are derived from the phase in the composition that mainly contains PEEK. In the table, "nd" means "not detected," meaning that no measurable signal was observed. In Example 6, the two melting peaks were close to each other and difficult to separate, so that it was not possible to calculate ΔHm at each Tm.
[0089] <Evaluation Results> From Table 1, at the 1st cooling, the Tmc (the value in the upper row) derived from the phase mainly containing the aromatic polyetherketone resin is increased compared to the value inherent to the aromatic polyetherketone resin (Comparative Examples 1 and 2). This means that the crystallinity is improved by blending the polyetherketone resin.
[0090] Furthermore, the actual measured ΔHmc value (ΔHmc(exp)) at 1st cooling of each composition is improved compared to the estimated ΔHmc value (ΔHmc(est)), which is calculated by multiplying the ΔHmc value inherent to the aromatic polyether ketone resin (ΔHmc in Comparative Examples 1 and 2) by the proportion of the aromatic polyether ketone resin in each composition, which also shows that the crystallinity of the composition of the present invention is improved. In addition, ΔHmc(exp) / ΔHmc(est) was 3.56 (Example 1), 3.43 (Example 2), 2.33 (Example 3), 3.40 (Example 4), 3.13 (Example 5), and 1.67 (Example 6).
[0091] Furthermore, compared with the estimated ΔHm value (ΔHm(est)), which is a value calculated by multiplying the ΔHm value inherent to the aromatic polyether ketone resin (ΔHm in Comparative Examples 1 and 2) by the proportion of the aromatic polyether ketone resin in the composition, the actual measured ΔHm value (ΔHm(exp)) in the first heating of each resin composition is improved, which also shows that the crystallinity of the composition of the present invention is improved. In addition, ΔHm(exp) / ΔHm(est) is 1.59 (Example 1), 1.24 (Example 2), 1.14 (Example 3), 1.24 (Example 4), and 1.27 (Example 5).
Claims
1. A resin composition comprising an aromatic polyetherketone resin X containing a repeating unit represented by the following general formula (1) and at least one resin Y different from the aromatic polyetherketone resin X, wherein the resin Y is any one of polyetherketone, polyetheretherketone, polyetherketoneketone, polyetheretherketoneketone, and polyetherketoneetherketoneketone: 【Chemistry 1】 (In the general formula (1), Structure A is any one selected from the group consisting of the following general formulae (2), (3), and (4), and Structure B is an optionally substituted divalent aromatic hydrocarbon ring.) 【Chemistry 2】
2. The resin composition according to claim 1 , wherein the structure A is represented by the formula (2).
3. The resin composition according to claim 1 or 2, wherein the mass of the aromatic polyether ketone resin X containing the repeating unit represented by the general formula (1) is 50 mass% or more based on the entire resin composition.
4. The resin composition according to claim 1 or 2, wherein the resin Y is any one of polyether ketone, polyether ether ketone, and polyether ketone ketone.
5. The resin composition according to claim 1 or 2, wherein Tmc2-Tmc1 is ≧5 (°C), where Tmc1 is the melt crystallization temperature of the aromatic polyether ketone resin X containing the repeating unit represented by the general formula (1) and Tmc2 is the melt crystallization temperature of the resin composition.
6. 3. The resin composition according to claim 1 or 2, wherein an estimated value of the heat of melt crystallization derived from the aromatic polyether ketone resin X in the resin composition, which is obtained by multiplying the heat of melt crystallization of the aromatic polyether ketone resin X containing the repeating unit represented by the general formula (1) by a mass fraction, is ΔHmc(est), and the heat of melt crystallization corresponding to a peak derived from the crystallization of the aromatic polyether ketone resin X in the resin composition is ΔHmc(exp) / ΔHmc(est)≧1.
1.
7. 3. The resin composition according to claim 1 or 2, wherein an estimated value of the heat of fusion derived from the aromatic polyether ketone resin X in the resin composition, which is obtained by multiplying the heat of fusion of the aromatic polyether ketone resin X containing the repeating unit represented by the general formula (1) by a mass fraction, is ΔHm(est), and a heat of fusion corresponding to a peak derived from crystalline melting of the aromatic polyether ketone resin X in the resin composition is ΔHm(exp) / ΔHm(est)≧1.1.