Method for producing surface-modified fluorine-based resin member

The electron beam grafting method introduces peroxide radicals on fluororesin surfaces for improved adhesion, addressing the adherence challenge and expanding fluororesin applications.

JP2024147161APending Publication Date: 2024-10-16DAI NIPPON PRINTING CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023059999
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-03
Publication Date
2024-10-16

AI Technical Summary

Technical Problem

Fluororesins have low surface energy and are chemically stable, making them difficult to adhere to other materials, limiting their applications.

Method used

A method involving electron beam irradiation to introduce carbon radicals, followed by oxygen exposure to generate peroxide radicals, and then graft polymerization of a radically polymerizable compound onto the fluororesin surface, allowing for improved adhesion.

Benefits of technology

The method enhances the adhesiveness of fluororesin members to other materials, enabling their use in applications where adhesives are undesirable or restricted, such as packaging and medical devices.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024147161000001_ABST
    Figure 2024147161000001_ABST
Patent Text Reader

Abstract

To provide a new method for producing a surface-modified fluorine-based resin member by an electron beam grafting method.SOLUTION: A method for producing a surface-modified fluorine-based resin member is provided, having: an electron beam irradiating step of irradiating the surface of a fluorine-based resin member 1 with electron beam 11; an oxygen exposure step of exposing the surface of the fluorine-based resin member irradiated with the electron beam to an oxygen-containing atmosphere 12; a radical polymerizable compound arranging step of, after the oxygen exposure step, arranging a radical polymerizable compound 2 on the surface of the fluorine-based resin member or the surface of a covering member 3; a laminating step of laminating the fluorine-based resin member and the covering member with the radical polymerizable compound laid between the members; and a graft polymerization step of graft polymerizing the radical polymerizable compound on the surface of the fluorine-based resin member by heating a laminate having the fluorine-based resin member, the radical polymerizable compound and the covering member in this order.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a method for producing a surface-modified fluorine-based resin member. [Background technology]

[0002] Fluorine-based resins are widely used in various fields as high-performance resins because they have excellent chemical resistance, heat resistance, electrical properties, releasability, weather resistance, low friction, water repellency, etc. On the other hand, fluororesins have a problem in that they are difficult to adhere to other materials because they have low surface energy and are chemically stable.

[0003] Therefore, various surface modification methods for fluororesin members have been proposed. For example, chemical etching using metallic sodium and plasma treatment methods are known. Patent Document 1 discloses a surface modification method for fluororesin materials, which includes an underwater plasma treatment step in which a fluororesin material is exposed to plasma generated in water to introduce a porous structure into the surface layer and roughen the surface, an atmospheric pressure plasma treatment step in which the roughened surface of the fluororesin material is exposed to atmospheric pressure plasma to defluorinate it and then introduce a peroxide radical group during exposure to the atmosphere, and a grafting step in which an organic compound solution having a functional group reactive with an adhesive in the molecule is applied to the peroxide radical group-introduced surface of the fluororesin material, and the organic compound is spontaneously covalently bonded to the peroxide radical group as a reaction point to perform graft polymerization at a high density. Non-Patent Document 1 discloses a surface modification method for fluororesin by radiation grafting. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] Patent No. 5645163 [Non-patent literature]

[0005] [Non-Patent Document 1] Akihiro Oshima, "Surface Modification and Adhesion Improvement of Fluoropolymers Using Quantum Beam-Induced Chemical Reactions", Journal of the Adhesion Society of Japan, Vol. 49, No. 11, 2013, pp. 433-438 Summary of the Invention [Problem to be solved by the invention]

[0006] Non-Patent Document 1 describes a method in which a fluororesin film is irradiated with an electron beam, and then the fluororesin film irradiated with the electron beam is immersed in a monomer solution to graft polymerize the monomer by a liquid phase method.

[0007] The present disclosure has been made in view of the above-mentioned circumstances, and has an object to provide a novel method for modifying the surface of a fluorine-based resin member by electron beam grafting. [Means for solving the problem]

[0008] One embodiment of the present disclosure provides a method for producing a surface-modified fluororesin member, comprising: an electron beam irradiation step of irradiating a surface of a fluororesin member with an electron beam; an oxygen exposure step of exposing the surface of the fluororesin member irradiated with the electron beam to an oxygen-containing atmosphere; a radical polymerizable compound arrangement step of arranging a radical polymerizable compound on the surface of the fluororesin member or the surface of a coating member after the oxygen exposure step; a lamination step of laminating the fluororesin member and the coating member with the radical polymerizable compound sandwiched between them; and a graft polymerization step of graft polymerizing the radical polymerizable compound onto the surface of the fluororesin member by heating a laminate having the fluororesin member, the radical polymerizable compound, and the coating member in this order. Effect of the Invention

[0009] The present disclosure provides a novel method for modifying the surface of a fluorine-based resin member by electron beam grafting. [Brief description of the drawings]

[0010] [Figure 1]1A to 1C are process diagrams illustrating a method for producing a surface-modified fluorine-based resin member according to the present disclosure. [Diagram 2] 1A to 1C are process diagrams illustrating a method for producing a surface-modified fluorine-based resin member according to the present disclosure. [Diagram 3] 1A to 1C are process diagrams illustrating a method for producing a surface-modified fluorine-based resin member according to the present disclosure. [Figure 4] 1A to 1C are process diagrams illustrating a method for producing a surface-modified fluorine-based resin member according to the present disclosure. [Diagram 5] FIG. 2 is a process diagram illustrating a radical polymerizable compound arrangement step and a lamination step in the method for producing a surface-modified fluorine-based resin member according to the present disclosure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] The manufacturing method of the surface-modified fluororesin member in the present disclosure will be described below. However, the present disclosure can be implemented in many different embodiments, and is not limited to the description of the embodiments exemplified below. In addition, in order to make the explanation clearer, the drawings may be schematic in terms of the width, thickness, shape, etc. of each member compared to the embodiment, but these are merely examples and do not limit the interpretation of the present disclosure. In addition, in this specification and each figure, elements similar to those described above with respect to the previously mentioned figures may be given the same reference numerals, and detailed explanations may be omitted as appropriate.

[0012] In this specification, when describing an aspect in which another component is placed on top of another component, the term "above" or "below" is used, unless otherwise specified, it includes both a case in which another component is placed directly above or below a certain component so as to be in contact with the certain component, and a case in which another component is placed above or below a certain component with another component in between.

[0013] In addition, in this specification, the terms "film," "sheet," "plate," and the like are not distinguished from one another solely on the basis of differences in name. For example, the term "film" is used to include members also known as sheets and plates.

[0014] The method for producing a surface-modified fluororesin member in the present disclosure includes an electron beam irradiation step of irradiating a surface of a fluororesin member with an electron beam; an oxygen exposure step of exposing the surface of the fluororesin member irradiated with the electron beam to an oxygen-containing atmosphere; a radical polymerizable compound arrangement step of arranging a radical polymerizable compound on the surface of the fluororesin member or the surface of a coating member after the oxygen exposure step; a lamination step of laminating the fluororesin member and the coating member with the radical polymerizable compound sandwiched between them; and a graft polymerization step of graft polymerizing the radical polymerizable compound onto the surface of the fluororesin member by heating a laminate having the fluororesin member, the radical polymerizable compound, and the coating member in this order.

[0015] 1(a) to 1(f) are process diagrams showing an example of a method for producing a surface-modified fluororesin member according to the present disclosure. First, as shown in FIG. 1(a), an electron beam irradiation step is performed in which an electron beam 11 is irradiated onto a surface S1 of a fluororesin member 1. Next, as shown in FIG. 1(b), an oxygen exposure step is performed in which the surface S1 of the fluororesin member 1 irradiated with the electron beam is exposed to an oxygen-containing atmosphere 12. Next, as shown in FIG. 1(c), after the oxygen exposure step, a radical polymerizable compound disposing step is performed in which a radical polymerizable compound 2 is disposed on the surface S1 of the fluororesin member 1. Next, as shown in FIG. 1(d), a lamination step is performed in which a covering member 3 is disposed so as to cover the surface of the fluororesin member 1 on which the radical polymerizable compound 2 is disposed, and the fluororesin member 1 and the covering member 3 are laminated with the radical polymerizable compound 2 sandwiched therebetween. Next, as shown in Fig. 1(e), a graft polymerization step is performed in which heat 13 is applied to the laminate 5 having the fluororesin member 1, the radically polymerizable compound 2, and the coating member 3 in this order, thereby graft polymerizing the radically polymerizable compound 2 onto the surface S1 of the fluororesin member 1. Subsequently, as shown in Fig. 1(f), a peeling step may be performed in which the coating member 3 is peeled off. In this way, a surface-modified fluororesin member 10 is obtained.

[0016] 2(a)-(f) are process diagrams showing another example of the method for producing a surface-modified fluororesin member according to the present disclosure. FIG. 2(a)-(b) are the same as FIG. 1(a)-(b) above. Next, as shown in FIG. 2(c), after the oxygen exposure step, a radical polymerizable compound disposing step is performed in which a radical polymerizable compound 2 is disposed on the surface S3 of the covering member 3. Next, as shown in FIG. 2(d), a lamination step is performed in which a fluororesin member 1 is disposed on the surface of the covering member 3 on which the radical polymerizable compound 2 is disposed, and the fluororesin member 1 and the covering member 3 are laminated with the radical polymerizable compound 2 sandwiched therebetween. FIG. 2(e)-(f) are the same as FIG. 1(e)-(f) above. As a result, a surface-modified fluororesin member 10 is obtained.

[0017] In the present disclosure, radicals can be introduced to the surface of a fluororesin member by irradiating the surface of the fluororesin member with an electron beam and then exposing the surface to an oxygen-containing atmosphere. Specifically, when the fluororesin member is irradiated with an electron beam, fluorine atoms are released from the C-F bonds on the surface of the fluororesin member to generate carbon radicals. In addition, when C-H bonds are also present on the surface of the fluororesin member, when the fluororesin member is irradiated with an electron beam, hydrogen atoms are released from the C-H bonds on the surface of the fluororesin member to generate carbon radicals. The generated carbon radicals then react with oxygen in the oxygen-containing atmosphere to generate peroxide radicals. In this way, it is believed that the peroxide radicals are introduced to the surface of the fluororesin member. Then, the radical polymerizable compound is graft-polymerized starting from the peroxide radicals introduced to the surface of the fluororesin member.

[0018] In the present disclosure, during graft polymerization, the fluororesin member and the coating member are heated in a laminated state with the radical polymerizable compound sandwiched between them. This allows the surface of the fluororesin member and the radical polymerizable compound to be maintained in contact with each other. Furthermore, heating can prevent the radical polymerizable compound from evaporating. Thus, the radical polymerizable compound can be uniformly graft polymerized onto the surface of the fluororesin member. Furthermore, the coating member can prevent the surface of the fluororesin member and the radical polymerizable compound from coming into contact with oxygen in the atmosphere, thereby preventing oxygen from interfering with the graft reaction of the radical polymerizable compound.

[0019] In this manner, in the present disclosure, it is possible to modify the surface of a fluororesin member by utilizing the electron beam grafting method, and to obtain a fluororesin member having excellent adhesiveness to other members.

[0020] Figures 3(a) to (f) are process diagrams showing another example of the method for producing a surface-modified fluororesin member according to the present disclosure. Figures 3(a) to (e) are similar to the above-mentioned Figures 1(a) to (e). As shown in Figure 3(f), the covering member 3 does not need to be peeled off after the graft polymerization step. In this case, a laminate having the surface-modified fluororesin member 10 and the covering member 3 is obtained.

[0021] Figures 4(a) to (f) are process diagrams showing another example of the method for producing a surface-modified fluororesin member according to the present disclosure. Figures 4(a) to (e) are similar to the above-mentioned Figures 2(a) to (e). As shown in Figure 4(f), the covering member 3 does not need to be peeled off after the graft polymerization step. In this case, a laminate having a surface-modified fluororesin member 10 and a covering member 3 is obtained.

[0022] In the present disclosure, by appropriately selecting and using a radically polymerizable compound, it is also possible to obtain a laminate in which a surface-modified fluorine-based resin member and a coated member are bonded together without the use of an adhesive.

[0023] Hereinafter, each step of the method for producing a surface-modified fluororesin member according to the present disclosure will be described.

[0024] 1. Fluorine resin components The fluorine-based resin member in the present disclosure contains a fluorine-based resin. Examples of the fluorine-based resin include polytetrafluoroethylene resin (PTFE), perfluoroalkoxy resin (PFA), copolymer resin of tetrafluoroethylene and hexafluoropropylene (FEP), copolymer resin of tetrafluoroethylene, perfluoroalkyl vinyl ether, and hexafluoropropylene (EPE), copolymer resin of tetrafluoroethylene and ethylene (ETFE), polychlorotrifluoroethylene resin (PCTFE), copolymer resin of ethylene and chlorotrifluoroethylene (ECTFE), vinylidene fluoride resin (PVDF), and vinyl fluoride resin (PVF). Among them, polytetrafluoroethylene resin (PTFE) is preferable. This is because PTFE is highly versatile.

[0025] Furthermore, the fluororesin member may contain various additives, such as a light stabilizer, an ultraviolet absorber, an antioxidant, a filler, and a lubricant, as necessary.

[0026] The form of the fluororesin member is not particularly limited, and may be, for example, a film or sheet, or a molded product.

[0027] When the fluororesin member is a film or sheet, it may be uniaxially or biaxially stretched.

[0028] 2.Electron beam irradiation process In the electron beam irradiation step in the present disclosure, the surface of the fluororesin member is irradiated with an electron beam.

[0029] When the fluororesin member is a film or sheet, or is flat, only one side of the fluororesin member may be irradiated with an electron beam, or both sides of the fluororesin member may be irradiated with an electron beam. When both sides of the fluororesin member are irradiated with an electron beam, each side is irradiated with an electron beam in the electron beam irradiation step, but both sides can be treated simultaneously from the radical polymerizable compound arrangement step to the graft polymerization step described below, and both sides of the fluororesin member can be surface modified.

[0030] The irradiation energy of the electron beam is appropriately adjusted depending on the type of fluororesin contained in the fluororesin member, etc. In particular, it is preferable that the irradiation energy of the electron beam is low. By using a low irradiation energy, deterioration of the fluororesin member can be suppressed, and radical generation on the surface of the fluororesin member occurs more efficiently, thereby increasing the graft ratio.

[0031] The acceleration voltage of the electron beam may be, for example, 50 kV to 70 kV, so that the electron beam can be irradiated only onto the surface of the fluororesin member. The absorbed dose of the electron beam may be, for example, 50 kGy to 900 kGy, so that the electron beam can be irradiated only onto the surface of the fluororesin member.

[0032] The electron beam irradiation device may be a conventionally known device, such as a curtain-type electron irradiation device (LB1023, manufactured by I-Electron Beam Co., Ltd.) or a line-type low-energy electron beam irradiation device (EB-ENGINE, manufactured by Hamamatsu Photonics KK).

[0033] The atmosphere in the electron beam irradiation step is preferably a vacuum or an inert gas atmosphere. In the above atmosphere, the oxygen concentration is preferably 100 ppm or less. When electron beams are irradiated in the presence of oxygen, ozone is generated, which has a negative effect on the environment and may cause the surface of the fluororesin member to react with the ozone and change its characteristics. Examples of inert gases include nitrogen and argon. For example, an oxygen concentration of 100 ppm or less can be achieved by filling the inside of an electron beam irradiation device with an inert gas.

[0034] 3.Oxygen exposure process In the oxygen exposure step according to the present disclosure, the surface of the fluororesin member irradiated with the electron beam is exposed to an oxygen-containing atmosphere.

[0035] As described above, when the surface of a fluororesin member is irradiated with an electron beam, carbon radicals are generated on the surface of the fluororesin member. The generated carbon radicals then react with oxygen in an oxygen-containing atmosphere to generate peroxide radicals. In the graft polymerization process described below, the peroxide radicals are used as a starting point to graft polymerize a radically polymerizable compound described below. Specifically, the peroxide radicals on the surface of the fluororesin member are bonded to the radically polymerizable compound to form a covalent bond. For three-dimensional structural reasons, the peroxide radicals are considered to have a higher reactivity with the radically polymerizable compound than the carbon radicals. Therefore, in the present disclosure, in order to generate peroxide radicals, oxygen exposure is performed after irradiation with an electron beam.

[0036] The oxygen-containing atmosphere is not particularly limited as long as it contains oxygen, and examples thereof include an air atmosphere, an atmosphere containing ozone, and a mixed atmosphere containing oxygen and an inert gas such as nitrogen, argon, helium, carbon dioxide, etc. If the atmosphere is an air atmosphere, atmospheric adjustment is unnecessary and it is simple.

[0037] The exposure time may be any time that can generate peroxide radicals and does not disappear the generated peroxide radicals, and is appropriately adjusted according to the types of fluororesin and radical polymerizable compound contained in the fluororesin member, the oxygen-containing atmosphere, and the like. Specifically, the exposure time is, for example, 2 hours or more, may be 6 hours or more, or may be 12 hours or more. The exposure time is, for example, 1 week or less, may be 48 hours or less, or may be 24 hours or less. If the exposure time is too short, it may be difficult to generate peroxide radicals sufficiently. On the other hand, if the exposure time is too long, the peroxide radicals may disappear.

[0038] 4. Radical polymerizable compound placement process In the radical polymerizable compound disposing step in the present disclosure, after the oxygen exposure step, a radical polymerizable compound is disposed on the surface of the fluorine-based resin member or the surface of the coated member.

[0039] (1) Radical polymerizable compound The radical polymerizable compound has a radical polymerizable functional group. Examples of the radical polymerizable functional group include a functional group having an ethylenically unsaturated double bond. Examples of the functional group having an ethylenically unsaturated double bond include a vinyl group, a (meth)acryloyl group, an allyl group, and a styryl group.

[0040] In addition, when the surface-modified fluorine-based resin member and another member are bonded via an adhesive, the radical polymerizable compound may further have a functional group reactive with the adhesive or a functional group having affinity with the adhesive. Such functional groups are appropriately selected according to the type of adhesive. Examples of such functional groups include hydroxyl groups, carboxyl groups, carboxylate groups, aldehyde groups, ketone groups, isocyanate groups, amino groups, dialkylamino groups, trialkylammonium groups, amide groups, formamide groups, epoxy groups, sulfonic acid groups, and halogen-substituted alkyl groups.

[0041] In addition, when the surface-modified fluororesin member and the coated member are bonded together without the aid of an adhesive, the radical polymerizable compound may further have a functional group reactive with the coated member. Such a functional group is appropriately selected according to the material of the coated member. For example, when the coated member is a metal member, the functional group may be a hydroxyl group, a carbonyl group, a lactone group, a carboxyl group, an acid anhydride group, a phosphonic acid group, an epoxy group, or a sulfur-containing functional group. Specific examples of the sulfur-containing functional group include =S, a mercapto group, a sulfide group, and an epithio group. It is believed that the hydroxyl group, the carbonyl group, the lactone group, the carboxyl group, the acid anhydride group, and the phosphonic acid group form a hydrogen bond or a chelate bond with the hydroxyl group present on the metal surface. In addition, since the acid anhydride group has a strong basicity, it is believed to form an ionic bond with the hydroxyl group present on the metal surface. In addition, it is believed that the epoxy group forms a hydroxyl group by a ring-opening reaction, and this hydroxyl group forms a hydrogen bond with the hydroxyl group present on the metal surface. Additionally, sulfur-containing functional groups can bond with metal atoms such as platinum, palladium, and silver.

[0042] The radical polymerizable compound may further have an epoxy group. Even if the radical compound does not have a desired functional group, a step of reacting the radical polymerizable compound graft-polymerized on the surface of the fluorine-based resin member with an organic compound having a desired functional group is carried out after the peeling step described below, and the desired functional group can be introduced on the surface of the fluorine-based resin member by ring-opening reaction of the epoxy group of the radical polymerizable compound.

[0043] The radical polymerizable compound is not particularly limited. When the surface-modified fluorine-based resin member is bonded to another member via an adhesive, examples of the radical polymerizable compound include acrylic acids, methacrylic acids, acrylic acid esters, methacrylic acid esters, acrylamides, methacrylamides, styrenes, vinylformamides, vinylbiphenyls, vinylnaphthalenes, vinylanthracenes, vinylpyrrolidones, acrylonitriles, maleic acids, maleimides, divinyl compounds, and trivinyl compounds.

[0044] The acrylic acids include acrylic acid, and the methacrylic acids include methacrylic acid.

[0045] Examples of acrylic acid esters include alkyl acrylates, aryl acrylates, alkoxy acrylates, hydroxyalkyl acrylates, aminoalkyl acrylates, alkenyl acrylates, epoxy group-containing acrylates, and isocyanate group-containing acrylates.

[0046] Examples of methacrylic acid esters include alkyl methacrylates, aryl methacrylates, alkoxy methacrylates, hydroxyalkyl methacrylates, aminoalkyl methacrylates, alkenyl methacrylates, epoxy group-containing methacrylates, and isocyanate group-containing methacrylates.

[0047] Examples of alkyl acrylates include methyl acrylate, ethyl acrylate, n-propyl acrylate, isopropyl acrylate, n-butyl acrylate, isobutyl acrylate, tert-butyl acrylate, n-pentyl acrylate, n-hexyl acrylate, cyclohexyl acrylate, n-heptyl acrylate, n-octyl acrylate, 2-ethylhexyl acrylate, nonyl acrylate, decyl acrylate, dodecyl acrylate, and stearyl acrylate. Examples of alkyl methacrylates include methyl methacrylate, ethyl methacrylate, n-propyl methacrylate, isopropyl methacrylate, n-butyl methacrylate, isobutyl methacrylate, tert-butyl methacrylate, n-pentyl methacrylate, n-hexyl methacrylate, cyclohexyl methacrylate, n-heptyl methacrylate, n-octyl methacrylate, 2-ethylhexyl methacrylate, nonyl methacrylate, decyl methacrylate, dodecyl methacrylate, and stearyl methacrylate.

[0048] Examples of the aryl acrylate include phenyl acrylate, toluyl acrylate, benzyl acrylate, etc. Examples of the aryl methacrylate include phenyl methacrylate, toluyl methacrylate, benzyl methacrylate, etc.

[0049] Examples of the alkoxy acrylate include 2-methoxyethyl acrylate, 3-methoxybutyl acrylate, etc. Examples of the alkoxy methacrylate include 2-methoxyethyl methacrylate, 3-methoxybutyl methacrylate, etc.

[0050] Examples of the hydroxyalkyl acrylate include 2-hydroxyethyl acrylate, 2-hydroxypropyl acrylate, etc. Examples of the hydroxyalkyl methacrylate include 2-hydroxyethyl methacrylate, 2-hydroxypropyl methacrylate, etc.

[0051] Examples of the aminoalkyl acrylate include dimethylaminoethyl acrylate, etc. Examples of the aminoalkyl methacrylate include dimethylaminoethyl methacrylate, etc.

[0052] Examples of the alkenyl acrylate include allyl acrylate, etc. Examples of the alkenyl methacrylate include allyl methacrylate, etc.

[0053] Examples of epoxy group-containing acrylates include glycidyl acrylate. Examples of epoxy group-containing methacrylates include glycidyl methacrylate.

[0054] Examples of the isocyanate group-containing acrylate include isocyanate acrylate, etc. Examples of the isocyanate group-containing methacrylate include isocyanate methacrylate, etc.

[0055] Examples of the acrylamides include acrylamide. Examples of the methacrylamides include methacrylamide.

[0056] Examples of styrenes include vinylbenzyltrimethylammonium chloride, chloromethylstyrene, and sodium p-styrenesulfonate.

[0057] The vinylformamides include N-vinylformamide.

[0058] In addition, when the surface-modified fluororesin member and the coated member are joined without an adhesive and the coated member is a metal member, examples of the radical polymerizable compound include carboxylic acid monomers, phosphate ester monomers, and nitrogen-containing monomers.

[0059] Examples of carboxylic acid monomers include 1,4-cyclohexanedimethanol acrylate, γ-butyrolactone acrylate, γ-butyrolactone methacrylate, 4-methacryloxyethyltrimellitic anhydride (4-META), 4-methacryloxyethyltrimellitic acid (4-AET), and 11-(meth)acryloyloxy-1,1-undecanedicarboxylic acid (MAC-10).

[0060] An example of the phosphate monomer is 10-methacryloyloxydecyl dihydrogen phosphate (MDP).

[0061] Examples of the nitrogen-containing monomer include triazinethiol monomers, thiouracil monomers, epithio monomers, and thiophosphate monomers. Examples of the triazinethiol monomers include 6-(4-vinylbenzyl-n-propyl)amino-1,3,5-triazine-2,4-dithiol (VBATDT). Examples of the thiouracil monomers include 6-methacryloyloxyhexyl 2-thiouracil-5-carboxylate (MTU-6). Examples of the epithio monomers include 2,3-epithiopropyl methacrylate (EP1MA), 4,5-epithiopentyl methacrylate (EP3MA), 9,10-epithiodecyl methacrylate (EP8MA), and 10,11-epithioundecyl methacrylate (EP9MA).

[0062] The radical polymerizable compound may be used alone or in combination of two or more kinds.

[0063] (2) Covering material The covering member in the present disclosure is not particularly limited as long as it is a member that can cover the surface of the fluororesin member to be modified.

[0064] The covering member preferably has oxygen barrier properties. In the graft polymerization step described later, the covering member can prevent the surface of the fluorine-based resin member and the radical polymerizable compound from coming into contact with oxygen in the atmosphere. This can prevent oxygen from inhibiting the graft reaction of the radical polymerizable compound. Therefore, the graft polymerization step can be performed in an air atmosphere. A general barrier film can be used as the covering member having oxygen barrier properties. Examples of the barrier film include metal foil, metal deposition film, inorganic deposition film, barrier resin film, and barrier resin coated film. In addition, as described later, even when the covering member is a metal member, it can have oxygen barrier properties.

[0065] The covering member may be flexible or may be rigid. When the covering member is flexible, it is easy to suppress the inclusion of air bubbles when laminating the fluorine-based resin member and the covering member via the radical polymerizable compound. On the other hand, when the covering member is rigid, not only can the occurrence of wrinkles in the covering member be suppressed when laminating the fluorine-based resin member and the covering member via the radical polymerizable compound, but also the occurrence of wrinkles in the covering member due to the graft reaction in the graft polymerization process can be suppressed. In addition, when an inert gas is flowed to create an inert gas atmosphere in the graft polymerization process, the covering member has rigidity, so that the displacement and peeling of the covering member due to the gas flow can be suppressed. Among them, it is preferable that the covering member has flexibility. In addition, when the covering member has flexibility, as described later, by placing a weight on a laminate having a fluorine-based resin member, a radical polymerizable compound, and a covering member in this order, or by applying pressure to a laminate having a fluorine-based resin member, a radical polymerizable compound, and a covering member in this order, the wrinkles, displacement, and peeling of the covering member can be suppressed.

[0066] In the present disclosure, when a peeling step described later is performed, it is preferable that the covering member has releasability. This is because the covering member can be easily peeled off in the peeling step. An example of a covering member having releasability is a release-treated resin member. As described above, the release-treated resin member is preferably flexible, and a release-treated resin film is preferable. An example of a release-treated resin film is a release-treated polyester film or a release-treated polyolefin film.

[0067] On the other hand, when a peeling step is carried out, the surface of the coated member may be previously subjected to a surface treatment in order to increase adhesion to the radical polymerizable compound.

[0068] The material of the covering member is not particularly limited, and examples thereof include metal materials, resin materials, rubber materials, and inorganic materials.

[0069] When the peeling step is performed, the covering member preferably contains a resin material, and as described above, is preferably a resin member that has been subjected to a release treatment.

[0070] On the other hand, when the peeling step is not performed, the coated member preferably contains a metal material, that is, is a metal member. A laminate in which the surface-modified fluororesin member and the metal member are bonded without the use of an adhesive can be obtained. Examples of the metal material include metals, alloys, and metal compounds.

[0071] In addition, when the peeling step is not performed, it is also preferable that the covering member contains a rubber material, that is, is a rubber member. Examples of the rubber material include butyl-based rubber, isoprene rubber, isoprene-isobutylene rubber, butadiene rubber, styrene-butadiene rubber, ethylene-propylene rubber, and nitrile rubber. Examples of the butyl-based rubber include butyl rubber, chlorinated butyl rubber, brominated butyl rubber, and divinylbenzene copolymerized butyl rubber.

[0072] The size of the coating member is not particularly limited as long as it is large enough to cover the surface of the fluororesin member to be modified. When a peeling step is performed, the size of the coating member may be larger than the size of the fluororesin member. In this case, the end of the fluororesin member can also be covered with the coating member, and the intrusion of oxygen in the atmosphere can be suppressed.

[0073] The form of the covering member is not particularly limited, and may be, for example, a film or sheet, or a molded product.

[0074] (3) Arrangement method of radical polymerizable compound In this step, the radical polymerizable compound is placed on the surface of the fluororesin member or the surface of the coated member. The radical polymerizable compound may be placed on the surface of the fluororesin member or the surface of the coated member.

[0075] The method for disposing the radical polymerizable compound on the surface of the fluororesin member is not particularly limited as long as it is a method that can dispose the radical polymerizable compound on the surface of the fluororesin member having low surface energy, and examples of the method include a dropping method and a spray coating method. In the case of the dropping method, the radical polymerizable compound may be dropped at one location on the surface of the fluororesin member, or may be dropped at multiple locations.

[0076] The method for disposing the radical polymerizable compound on the surface of the coated member is not particularly limited as long as it is a method that can dispose the radical polymerizable compound on the surface of a fluororesin member having low surface energy, and for example, a dropping method or various coating methods can be used. Examples of the coating method include a bar coating method and a spray coating method.

[0077] When the radical polymerizable compound is disposed on the surface of the fluorine-based resin member or the surface of the coated member, the radical polymerizable compound may be used as it is, or may be diluted or dissolved in a solvent. When the radical polymerizable compound has high reactivity, it is preferable to dilute the radical polymerizable compound with a solvent. The solvent is appropriately selected depending on the type of the radical polymerizable compound, the disposition method, etc. Furthermore, in the radical polymerizable compound solution, the concentration of the radical polymerizable compound is appropriately adjusted depending on the disposition method, the desired graft ratio, etc.

[0078] The radical polymerizable compound solution may be degassed to remove dissolved oxygen before being placed on the surface of the fluorine-based resin member or the surface of the coated member, or may not be degassed. When the reactivity of the radical polymerizable compound is high, the reaction time is short, so degassing may be performed, or may not be performed. When degassing is not performed, the manufacturing cost can be reduced. Furthermore, when the reactivity of the radical polymerizable compound is low, degassing is preferably performed. Oxygen inhibition of the graft reaction of the radical polymerizable compound can be suppressed.

[0079] The atmosphere in the radical polymerizable compound arrangement step is not particularly limited, and may be an air atmosphere or an inert gas atmosphere. The inert gas atmosphere is the same as the inert gas atmosphere in the electron beam irradiation step. When the reactivity of the radical polymerizable compound is high, the reaction time is short, so an air atmosphere or an inert gas atmosphere may be used. In the case of an air atmosphere, the production cost can be reduced. Furthermore, when the reactivity of the radical polymerizable compound is low, an inert gas atmosphere is preferable. Oxygen inhibition of the graft reaction of the radical polymerizable compound can be suppressed.

[0080] 5.Lamination process In the lamination step of the present disclosure, the fluororesin member and the covering member are laminated with the radical polymerizable compound sandwiched therebetween.

[0081] In the above radical polymerizable compound disposing step, when the radical polymerizable compound is disposed on the surface of the fluororesin member, a covering member is laminated on the surface of the fluororesin member on which the radical polymerizable compound is disposed. On the other hand, in the above radical polymerizable compound disposing step, when the radical polymerizable compound is disposed on the surface of the covering member, a fluororesin member is laminated on the surface of the covering member on which the radical polymerizable compound is disposed.

[0082] In addition, when surface-modifying both sides of a fluororesin member, for example, as shown in Fig. 5(a), in the radical-polymerizable compound disposing step, the radical-polymerizable compound 2 is disposed on the surface S1 of the fluororesin member 1, and the radical-polymerizable compound 2 is disposed on the surface of the covering member 3b, and in the laminating step, as shown in Fig. 5(b), for example, the fluororesin member 1 is laminated on the surface of the covering member 3b on which the radical-polymerizable compound 2 is disposed, and the covering member 3a is laminated on the surface of the fluororesin member 1 on which the radical-polymerizable compound 2 is disposed. This allows the surface of both sides S1 and S2 of the fluororesin member 1 to be modified.

[0083] When laminating a fluororesin member and a coating member with a radical polymerizable compound sandwiched therebetween, it is preferable to laminate the fluororesin member and the coating member so as to prevent air bubbles from being mixed in. For example, the incorporation of air bubbles can be suppressed by laminating the fluororesin member and the coating member while applying pressure with a roll.

[0084] After laminating the fluorine-based resin member and the covering member with the radical polymerizable compound sandwiched therebetween, pressure may be applied to the laminate having the fluorine-based resin member, the radical polymerizable compound, and the covering member in this order. Wrinkling, misalignment, and peeling of the covering member can be suppressed. In addition, wrinkles, misalignment, and peeling of the fluorine-based resin member can also be suppressed. Examples of methods for applying pressure to the laminate include a method of placing a weight on the laminate, a method of using a blocking tester, and a method of using a press. The weight is not particularly limited, and an example of the weight is a metal plate. Since the metal plate usually has oxygen barrier properties, by placing the metal plate on the laminate, it is possible to suppress the surface of the fluorine-based resin member and the radical polymerizable compound from coming into contact with oxygen in the graft polymerization process. The size of the metal plate is preferably equal to or larger than the size of the fluorine-based resin member. It is possible to suppress the permeation of oxygen and to apply pressure evenly to the entire surface of the fluorine-based resin member.

[0085] The atmosphere in the lamination step is not particularly limited, and may be an air atmosphere or an inert gas atmosphere. The inert gas atmosphere is the same as the inert gas atmosphere in the electron beam irradiation step. When the covering member has oxygen barrier properties, or when a weight is placed on the laminate and the weight has oxygen barrier properties, the atmosphere can be an air atmosphere.

[0086] 6. Graft polymerization process In the graft polymerization step of the present disclosure, a laminate having the fluorine-based resin member, the radically polymerizable compound, and the coating member in this order is heated, thereby graft polymerizing the radically polymerizable compound onto the surface of the fluorine-based resin member.

[0087] The heating temperature is not particularly limited as long as it is a temperature at which the radical polymerizable compound can be graft-polymerized onto the surface of the fluororesin member, and is appropriately adjusted according to the types of fluororesin and radical polymerizable compound contained in the fluororesin member, the heating time described below, and the like. The heating temperature is, for example, 30°C or higher and 100°C or lower. If the heating temperature is too low, the graft reaction rate is slow, and the graft reaction may take a long time, or a sufficient graft rate may not be obtained. Also, if the heating temperature is too high, the radicals generated on the surface of the fluororesin member may decay, and a sufficient graft rate may not be obtained.

[0088] The heating time is not particularly limited as long as it is a time that allows graft polymerization of the radical polymerizable compound onto the surface of the fluororesin member, and is appropriately adjusted depending on the types of fluororesin and radical polymerizable compound contained in the fluororesin member, the heating temperature, etc. The heating time is, for example, 3 minutes or more and 1 week or less.

[0089] When pressure is applied to the laminate in the lamination step, the laminate is heated in a state in which pressure is applied to the laminate in the graft polymerization step.

[0090] The atmosphere in the graft polymerization step is preferably an inert gas atmosphere. The inert gas atmosphere is the same as the inert gas atmosphere in the electron beam irradiation step. This can suppress oxygen inhibition of the graft reaction of the radical polymerizable compound. In addition, when the reactivity of the radical polymerizable compound is high, the reaction time is short, so the atmosphere may be an air atmosphere.

[0091] The lamination step and the graft polymerization step may be performed in sequence or simultaneously. When the lamination step and the graft polymerization step are performed in sequence, for example, an oven or a hot plate can be used in the graft polymerization step. On the other hand, when the heating time in the graft polymerization step is very short, the lamination step and the graft polymerization step can be performed simultaneously. In this case, in the lamination step and the graft polymerization step, the fluorine-based resin member and the covering member are thermocompressed via a radical polymerizable compound. In such a case, for example, a method using a heated roll or a hot press can be applied.

[0092] Unlike the fluorine-based resin member, the surface of the coated member is not irradiated with an electron beam, and therefore it is considered that the radical polymerizable compound does not undergo graft polymerization on the surface of the coated member.

[0093] 7. Peeling process In the present disclosure, after the graft polymerization step, a peeling step of peeling off the covering member may be performed, in which case a surface-modified fluorine-based resin member is obtained.

[0094] On the other hand, in the present disclosure, the coating member does not need to be peeled off after the graft polymerization step. In this case, a laminate having a surface-modified fluororesin member and a coating member is obtained. By appropriately selecting and using a radical polymerizable compound, a laminate in which the surface-modified fluororesin member and the coating member are bonded without the use of an adhesive can be obtained.

[0095] 8. Cleaning process In the present disclosure, the surface-modified fluororesin member may be washed after the peeling step. This allows the unreacted radical polymerizable compound to be removed. Examples of the washing method include solvent washing and detergent washing. The solvent is appropriately selected depending on the radical polymerizable compound, and examples of the solvent include organic solvents such as alcohol and water. Two or more types of washing methods may be combined.

[0096] After washing, drying may be performed. The drying method is not particularly limited, and may be, for example, hot air drying.

[0097] 9.Plasma treatment process In the present disclosure, a plasma treatment step may be performed before the electron beam irradiation step, in which a plasma treatment is performed on the surface of the fluororesin member. When a radical polymerizable compound is arranged on the surface of the fluororesin member in the radical polymerizable compound arrangement step, the plasma treatment may make it easier for the radical polymerizable compound to spread over the surface of the fluororesin member.

[0098] The gas used in the plasma treatment is appropriately adjusted depending on the type of fluororesin contained in the fluororesin member. Examples of the gas include non-reactive gases such as argon and helium, and reactive gases such as nitrogen, oxygen, and hydrogen. A mixed gas of these may also be used.

[0099] The plasma treatment may be, for example, a low-temperature plasma treatment or a high-temperature plasma treatment, and may be, for example, an atmospheric pressure plasma treatment or a vacuum plasma treatment.

[0100] The conditions of the plasma treatment are appropriately adjusted according to the type of fluororesin contained in the above-mentioned fluororesin member. For example, if the plasma treatment intensity is too low, the effect of improving the wettability of the surface of the fluororesin member may not be sufficiently obtained. Also, if the plasma treatment intensity is too high, the fluororesin member may be damaged, or the fluororesin member may be deformed or discolored, resulting in poor appearance.

[0101] 10. Other processes In the present disclosure, after the peeling step, a step of reacting the radically polymerizable compound graft-polymerized on the surface of the fluororesin member with an organic compound may be performed. When the radically polymerizable compound does not have a desired functional group, the desired functional group can be introduced onto the surface of the fluororesin member by further reacting the radically polymerizable compound with an organic compound having a desired functional group. The organic compound is not particularly limited as long as it has a functional group reactive with the radically polymerizable compound and a functional group to be introduced onto the surface of the fluororesin member, and is appropriately selected.

[0102] The functional group reactive with the radical polymerizable compound is preferably a functional group reactive with the epoxy group of the radical polymerizable compound. Examples of the functional group reactive with the epoxy group of the radical polymerizable compound include an amino group and an NH group constituting a secondary amine.

[0103] Furthermore, in the case where a surface-modified fluororesin member and a coated member are joined without the use of an adhesive and the coated member is a metal member, examples of functional groups to be introduced onto the surface of the fluororesin member include a hydroxyl group, a carbonyl group, a lactone group, a carboxyl group, an acid anhydride group, a phosphonic acid group, and a sulfur-containing functional group.

[0104] 11.Applications The method for producing a surface-modified fluororesin member according to the present disclosure is suitable for use in applications where the use of adhesives is undesirable or limited. Examples of such applications include packaging materials for medicines, medical devices, cosmetics, food, etc., and medical devices such as syringes and tubes. In addition, since fluororesin members have excellent electrical properties, the method is also suitable for use in a method for producing a surface-modified fluororesin member used in a printed wiring board.

[0105] The present disclosure is not limited to the above-described embodiments. The above-described embodiments are merely examples, and anything that has substantially the same configuration as the technical idea described in the claims of the present disclosure and exhibits similar effects is included in the technical scope of the present disclosure. EXAMPLES

[0106] The present disclosure will be described in further detail below with reference to examples and comparative examples.

[0107] [Example 1] A polychlorotrifluoroethylene resin (PTFE) film (V7900 manufactured by Valqua Corp.) was prepared as a fluorine-based resin member. After purging with nitrogen gas so that the oxygen concentration in the chamber of the electron beam irradiation device was 100 ppm or less, the surface of the PTFE film was irradiated with electron beams using an electron beam irradiation device (line irradiation type low energy electron beam irradiation device "EES-L-DP01" manufactured by Hamamatsu Photonics K.K.) at a voltage of 50 kV, an absorbed dose of 300 kGy, and an oxygen concentration in the device of 35 ppm or less.

[0108] After the electron beam irradiation, the PTFE film was exposed to the atmosphere for 24 hours to introduce peroxide radicals onto the surface of the PTFE film. 2 0.1 ml of 2-hydroxyethyl methacrylate (HEMA) was dropped onto the area. The same PTFE film as the fluororesin member was used as the covering member, and the surface of the PTFE film, which is the fluororesin member, on which HEMA was dropped was sealed with the PTFE film, which is the covering member, and a SUS plate was placed on top of the covering member to obtain a laminate. Then, using an oven, the reaction was carried out under nitrogen flow at 60°C for 24 hours. After the reaction, the laminate was removed from the oven, the SUS plate was removed from the laminate, and the covering member was peeled off. Next, the surface of the PTFE film, which is the fluororesin member, on which HEMA was dropped was washed with water and a neutral detergent, wiped off with ethanol, and air-dried.

[0109] [evaluation] (1)X-ray photoelectron spectroscopy (XPS) Using an X-ray photoelectron analyzer (KRATOS' "ESCA-3400"), the elements present on the surface of the PTFE film were detected. The measurement conditions were as follows. The results are shown in Table 1. Note that the unit of the numerical values of the elements in the table is atomic%. <XPS Measurement Conditions> X-ray used: Mg Output: 200 W Angle: 90 degrees

[0110]

Table 1

[0111] (2) Contact Angle Using a fully automatic contact angle meter "DropMaster" manufactured by Kyowa Interface Science Co., Ltd., the contact angle of water on the surface of the PTFE film was measured by the θ / 2 method. Specifically, at 20°C and 50% RH, 1.5 μL of pure water was dropped onto the surface of the PTFE film, and the static contact angle 2 seconds after droplet landing was determined. The contact angle of water was 109.6° for the PTFE film before electron beam irradiation and 80.0° for the PTFE film after the graft reaction of HEMA.

[0112] (3) Interlayer Adhesion Strength A copper foil was laminated on the PTFE film after the graft reaction of HEMA through an adhesive layer containing an epoxy-based thermosetting adhesive. Next, after thermally laminating at a temperature of 120°C and a speed of 1 m / min using a heating roll, a thermal press was performed at a temperature of 180°C and a pressure of 1 MPa to bond the PTFE film and the copper foil to obtain a laminate.

[0113] A test piece with a width of 10 mm was cut out from the above laminate. Using a tensile testing machine ("STB-1225S" manufactured by A&D Company Limited), in accordance with JIS K6854-2, at 23°C, 30% RH, a tensile speed of 50 mm / min, and a peel angle of 180°, the interlayer adhesion strength between the PTFE film and the copper foil was measured. The interlayer adhesion strength between the PTFE film and the copper foil was 12.5 N / 10 mm.

[0114] For comparison, a laminate was similarly produced using the PTFE film before electron beam irradiation, and the interlayer adhesive strength between the PTFE film and the copper foil was measured, but the interlayer adhesive strength was too weak to measure. [Explanation of symbols]

[0115] 1 … Fluorine resin materials 2... Radical polymerizable compounds 3 … Covering material 10 ... Surface-modified fluororesin components 11 … Electron beam 12 … Oxygen-containing atmosphere 13 … fever S1: Surface of fluororesin material

Claims

1. an electron beam irradiation step of irradiating a surface of a fluorine-based resin member with an electron beam; an oxygen exposure step of exposing the surface of the fluororesin member irradiated with the electron beam to an oxygen-containing atmosphere; a radical polymerizable compound disposing step of disposing a radical polymerizable compound on the surface of the fluorine-based resin member or the surface of the coated member after the oxygen exposure step; a lamination step of laminating the fluorine-based resin member and the covering member with the radical polymerizable compound sandwiched between them; a graft polymerization step of graft-polymerizing the radical polymerizable compound onto a surface of the fluorine-based resin member by heating a laminate having the fluorine-based resin member, the radical polymerizable compound, and the coating member in this order; The method for producing a surface-modified fluorine-based resin member comprising the steps of:

2. The method for producing a surface-modified fluorine-based resin member according to claim 1 , further comprising a peeling step of peeling off the coated member after the graft polymerization step.

3. The method for producing a surface-modified fluorine-based resin member according to claim 2 , wherein the coated member has releasability.

4. The method for producing a surface-modified fluorine-based resin member according to claim 1 , wherein the coated member is not peeled off after the graft polymerization step.

5. The method for producing a surface-modified fluorine-based resin member according to claim 4 , wherein the coated member contains a metal material.

6. The method for producing a surface-modified fluorine-based resin member according to any one of claims 1 to 5, wherein the coated member has oxygen barrier properties.

Citation Information