N-vinyl methyl oxazolidinone-containing composition and method for manufacturing the same

By removing impurities through distillation, the N-vinylmethyloxazolidinone composition achieves stable and transparent formulations for radiation-curable applications, addressing viscosity and coloration issues.

JP2024147482APending Publication Date: 2024-10-16WAKOU KAGAKU CO

Patent Information

Application Number
JP2023179104
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-03
Filing Date
2023-10-17
Publication Date
2024-10-16

AI Technical Summary

Technical Problem

N-vinylmethyloxazolidinone-containing compositions used as reactive diluents in radiation-curable compositions exhibit increased viscosity over time, poor storage stability, and coloration issues due to unavoidable impurities, which affect their performance and applications.

Method used

The composition is produced by removing specific impurities such as 6-ethoxy-2,2,4-trimethyl-1,2-dihydroquinoline and 4-methylproline to less than 1% by mass through distillation, ensuring high transparency and stability.

Benefits of technology

The resulting composition maintains low viscosity, excellent storage stability, and high transparency, suitable for use in radiation-curable applications like inkjet inks and coatings.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024147482000001_ABST
    Figure 2024147482000001_ABST
Patent Text Reader

Abstract

To provide a N-vinyl methyl oxazolidinone-containing composition capable of suppressing viscosity increase due to product aging to impart excellent storage stability and having high transparency, where N-vinyl methyl oxazolidinone is used as a reactive diluent for a radiation curable composition due to its liquid state at the room temperature, and low viscosity and toxicity, and almost odorless properties.SOLUTION: A N-vinyl methyl oxazolidinone-containing composition includes 1 mass% or less of 6-ethoxy-2,2,4-trimethyl-1,2-dihydro quinoline and 4-methyl proline.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to an N-vinylmethyloxazolidinone-containing composition and a method for producing the same. [Background technology]

[0002] N-vinylmethyloxazolidinone is liquid at room temperature, has low viscosity and toxicity, and is virtually odorless, and therefore is widely used as a reactive diluent for radiation curable compositions, particularly in inkjet inks (see Patent Document 1 below), coating formulations, paints, etc. As described in the following Patent Documents 1 and 2, N-vinylmethyloxazolidinone can be produced by a process of pyrolyzing N-(1-hydroxyalkyl)-2-oxazolidinone, or by a process of reacting acetylene with oxazolidinone according to the Reppe method. On the other hand, N-vinylmethyloxazolidinone is commercially available from BASF Societas Europea under the trade name VMOX.

[0003] The N-vinylmethyloxazolidinone obtained through the above-mentioned production process, or the currently commercially available N-vinylmethyloxazolidinone, further contains 3-ethenyl-4-methyl-1,3-oxazolidin-2-one, 3-ethyl-5-methyl-1,3-oxazolidin-2-one, 5-methyl-1,3-oxazolidin-2-one, and 3-(1-ethoxyethyl)-5-methyl-1,3-oxazolidin-2-one as inevitable impurities. Therefore, N-vinylmethyloxazolidinone is supplied to the market as a composition containing other compounds as described above (hereinafter, sometimes referred to as N-vinylmethyloxazolidinone-containing composition).

[0004] However, in the industry where N-vinylmethyloxazolidinone is used as a reactive diluent for radiation curable compositions, the composition and formulations containing the same have problems with storage stability due to increased viscosity over time (a phenomenon in which impurities act as nucleating agents and crystallize). In addition, the composition is colored yellow to brown and has an APHA of 200 or more, which can be problematic depending on the application. [Prior art documents] [Patent documents]

[0005] [Patent Document 1] Special Publication No. 2016-529360 [Patent Document 2] U.S. Pat. No. 4,831,153 Summary of the Invention [Problem to be solved by the invention]

[0006] Therefore, an object of the present invention is to provide an N-vinylmethyloxazolidinone-containing composition which inhibits an increase in viscosity over time of the product, imparts excellent storage stability, and has high transparency, and a method for producing the same. [Means for solving the problem]

[0007] The present inventors have found that conventional N-vinylmethyloxazolidinone-containing compositions contain unavoidable impurities that are not understood by the prior art, and have discovered that the above-mentioned problems can be solved by removing these impurities from the composition, thereby completing the present invention.

[0008] That is, the present invention provides (1) a composition containing N-vinylmethyloxazolidinone represented by the following formula I, in which 6-ethoxy-2,2,4-trimethyl-1,2-dihydroquinoline and 4-methylproline are contained in an amount of 1 mass % or less.

[0009] [ka]

[0010] The present invention also provides (2) a method for producing the composition described in (1) above, which comprises preparing a mixture containing N-vinylmethyloxazolidinone represented by formula I, 3-ethenyl-4-methyl-1,3-oxazolidin-2-one, 3-ethyl-5-methyl-1,3-oxazolidin-2-one, 5-methyl-1,3-oxazolidin-2-one, and 3-(1-ethoxyethyl)-5-methyl-1,3-oxazolidin-2-one, and distilling the mixture to adjust the contents of 6-ethoxy-2,2,4-trimethyl-1,2-dihydroquinoline and 4-methylproline to 1 mass% or less, thereby obtaining an N-vinylmethyloxazolidinone-containing composition represented by formula I. Effect of the Invention

[0011] According to the present invention, it is possible to provide an N-vinylmethyloxazolidinone-containing composition that inhibits an increase in viscosity of the product over time, imparts excellent storage stability, and has high transparency, and a method for producing the same. [Brief description of the drawings]

[0012] [Figure 1] 1 is a GC chart of an N-vinylmethyloxazolidinone-containing composition of the present invention. [Diagram 2] This is the VMOX GC chart. [Diagram 3] This is a GC-MS chart of the components remaining in the still after distillation under specific distillation conditions. [Figure 4] 1 is a photograph showing the appearance of the N-vinylmethyloxazolidinone-containing composition (a) of the present invention and VMOX (b) prepared in the examples. [Diagram 5] FIG. 2 shows the results of GC / MS analysis in an example. [Figure 6] FIG. 2 is a diagram showing an ion chromatogram in an example. [Figure 7]FIG. 1 shows MS spectra in an example. [Figure 8A] FIG. 2 is a diagram showing the results of 1H-NMR analysis in an example. [Figure 8B] FIG. 2 is a diagram showing the results of 13C-NMR analysis in an example. [Figure 9A] FIG. 2 is a diagram showing the results of 1H-NMR analysis in an example. [Figure 9B] FIG. 2 is a diagram showing the results of 13C-NMR analysis in an example. [Figure 10] This is a photograph of a sample of 6-ethoxy-2,2,4-trimethyl-1,2-dihydroquinoline. [Figure 11] This is a photograph of a 4-methylproline preparation. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0013] Hereinafter, the embodiments of the present invention will be described in further detail. The N-vinylmethyloxazolidinone-containing composition of the present invention is characterized by containing N-vinylmethyloxazolidinone represented by the following formula I, and containing 1 mass % or less of 6-ethoxy-2,2,4-trimethyl-1,2-dihydroquinoline and 4-methylproline.

[0014] [ka]

[0015] As described above, the present inventors have found that conventional N-vinylmethyloxazolidinone-containing compositions contain unavoidable impurities that are not known in the prior art, and have found that removing these impurities from the composition can suppress the increase in viscosity of the product over time, impart excellent storage stability, and provide an N-vinylmethyloxazolidinone-containing composition with high transparency. The unavoidable impurities are 6-ethoxy-2,2,4-trimethyl-1,2-dihydroquinoline, which is a chemical substance that is liquid at room temperature (Figure 10), and 4-methylproline, which is a chemical substance that is solid at room temperature (Figure 11). These compounds have an adverse effect on the storage stability and adhesion of the composition, and also cause coloring (e.g., yellow, reddish brown, or black).

[0016] A method for producing the N-vinylmethyloxazolidinone-containing composition of the present invention will now be described. First, a mixture containing N-vinylmethyloxazolidinone is prepared according to the conventional technique. This mixture is obtained, as in the conventional technique, through a step of pyrolyzing N-(1-hydroxyalkyl)-2-oxazolidinone or a step of reacting acetylene with oxazolidinone according to the Reppe method. The above two steps are known and can be carried out by a conventional method. For example, the former step of pyrolyzing N-(1-hydroxyalkyl)-2-oxazolidinone can be exemplified by a step of pyrolyzing N-(1-hydroxyalkyl)-2-oxazolidinone or N-(1-hydrocarbyloxyalkyl)-2-oxazolidinone at a temperature range of 200 to 500° C. and a pH range of about 6 to 7, as described in the above Patent Document 2. Alternatively, the mixture containing N-vinylmethyloxazolidinone may be a commercially available product available under the trade name VMOX from BASF Societas Europea. These mixtures contain N-vinylmethyloxazolidinone represented by formula I and have a Hazen color unit number (APHA) of 200 or more.

[0017] In this specification, the Hazen color unit number (APHA) is measured in accordance with JIS K0071-1.

[0018] The mixture is then distilled to adjust the content of 6-ethoxy-2,2,4-trimethyl-1,2-dihydroquinoline and 4-methylproline to 1% by mass or less. The resulting N-vinylmethyloxazolidinone-containing composition has a Hazen color number (APHA) of 150 or less. The N-vinylmethyloxazolidinone-containing composition of the present invention has a 6-ethoxy-2,2,4-trimethyl-1,2-dihydroquinoline and 4-methylproline content of 1% by mass or less, preferably 0.5% by mass or less, more preferably 0.3% by mass or less, even more preferably 0.1% by mass or less, particularly preferably 0.05% by mass or less, and most preferably 0.01% by mass or less.

[0019] As a distillation method, simple distillation can be mentioned. Simple distillation is a method in which a certain amount of raw liquid is charged into a distillation vessel, heated to boiling, and the generated steam is condensed in a condenser to concentrate impurities and purify the liquid.

[0020] The distillation conditions are important for obtaining the N-vinylmethyloxazolidinone-containing composition of the present invention, and examples thereof include the following distillation condition 1. Distillation conditions 1: Bath temperature: 130-140℃ (specifically 135℃) Top temperature: 97-101℃ Decompression level: 1~10hPa (specifically 5 hPa) First cut: None Yield: 97% A small amount of a polymerization inhibitor (preferably butylhydroxytoluene) may be added to the mixture.

[0021] Furthermore, in the N-vinylmethyloxazolidinone-containing composition of the present invention, in addition to having 1 mass % or less of 6-ethoxy-2,2,4-trimethyl-1,2-dihydroquinoline and 4-methylproline, from the viewpoint of improving the effects of the present invention, it is preferable that the content of impurities having a retention time of 14 minutes or more under the GC-MS measurement conditions described below (impurities not identified in the above-mentioned conventional techniques) is 1 mass % or less, preferably 0.5 mass % or less, more preferably 0.3 mass % or less, even more preferably 0.1 mass % or less, particularly preferably 0.05 mass % or less, and most preferably 0.01 mass % or less. GC / MS: QP-2010Plus (manufactured by Shimadzu Corporation) Column: DB-5 ms (0.25φ×40m 0.25μm) GC oven temperature: 40℃(3.0 min)~(heating rate 10℃ / min) ~310℃(15minHold) Injection volume: 1.0μl Injection mode: Split injection Split ratio: 1 / 30

[0022] Under the above GC-MS measurement conditions, the GC oven temperature is ultimately 150° C. or higher, and the above impurities are effectively detected under these heating conditions. Specific examples of impurity compounds with a retention time of 14 minutes or longer under the above GC-MS measurement conditions include, in addition to 6-ethoxy-2,2,4-trimethyl-1,2-dihydroquinoline and 4-methylproline, the following compounds: 3-t-Butyl-1,3-oxazolidin-2-one Iridomirmecin

[0023] Furthermore, the N-vinylmethyloxazolidinone-containing composition of the present invention preferably has a Hazen color scale (APHA) of 100 or less, and more preferably 80 or less.

[0024] The N-vinylmethyloxazolidinone-containing composition of the present invention is useful as a radiation-curable composition, particularly as an inkjet ink, a hard coat film, or an adhesive film, and is also useful as various coating formulations and paints.

[0025] Hereinafter, a radiation-curable composition used in ink-jet inks will be described as a suitable application of the N-vinylmethyloxazolidinone-containing composition of the present invention.

[0026] The radiation-curable composition may contain the composition of the present invention in an amount of 0.5 to 80% by mass.

[0027] The radiation curable composition may also contain a stabilizer to prevent premature polymerization.

[0028] Suitable stabilizers may be known stabilizers that prevent premature polymerization of N-vinylmethyloxazolidinone represented by formula I. Stabilizers may include, for example, nitroxyl compounds, such as 1-oxyl-2,2,6,6-tetramethylpiperidine, 4-hydroxy-1-oxyl-2,2,6,6-tetramethylpiperidine, phenol derivatives having at least one substituent at the α-position relative to the phenol group, such as 2,6-di-tert-butyl-4-methylphenol, tocopherol, quinones and hydroquinones, such as hydroquinone monomethyl ether, N-oxyl compounds, aromatic amines and phenylenediamines, imines, sulfonamides, oximes, hydroxylamines, urea derivatives, phosphorus-containing compounds, sulfur-containing compounds, complexing agents based on tetraazaannulenes (TAA) and / or metal salts, and mixtures thereof, if appropriate. The phosphorus-containing compound is, for example, triphenylphosphine, triphenylphosphite, hypophosphorous acid, trinonylphosphite, triethylphosphite or diphenylisopropylphosphine.

[0029] The radiation curable composition may contain further components, such as further radiation curable compounds or additives, such as stabilizers, photoinitiators, and the like.

[0030] Further radiation-curable compounds can be compounds which have polymerizable ethylenically unsaturated groups, for example as vinyl groups, for example as vinyl ether groups, vinyl ester groups or N-vinyl groups, allyl groups or (meth)acryloyl groups.

[0031] The expression "(meth)acryloyl group" refers to an acryloyl group or a methacryloyl group, preferably an acryloyl group.

[0032] A compound having at least one (meth)acryloyl group is hereinafter referred to as a (meth)acryloyl compound for short. The (meth)acryloyl compound may be present in the radiation curable composition in an amount of, for example, 90% by mass or less.

[0033] Such further radiation curable compounds may be monomeric or oligomeric.

[0034] monomer A monomer is defined herein as a compound having one polymerizable ethylenically unsaturated group. The monomer preferably has a molecular weight of less than 300 g / mol, in particular less than 200 g / mol. It acts in particular as a reactive diluent. Possible monomers are, for example, C1-C 20 - selected from alkyl (meth)acrylates, vinyl esters of carboxylic acids containing up to 20 carbon atoms, vinyl aromatic compounds containing up to 20 carbon atoms, ethylenically unsaturated nitriles, vinyl ethers of alcohols containing 1 to 10 carbon atoms.

[0035] Vinyl esters of carboxylic acids having 1 to 20 carbon atoms are, for example, vinyl laurate, vinyl stearate, vinyl propionate, vinyl versatate and vinyl acetate.

[0036] Suitable vinyl aromatic compounds are vinyl toluene, alpha- and p-methyl styrene, alpha-butyl styrene, 4-n-butyl styrene, 4-n-decyl styrene, preferably styrene.

[0037] Examples of nitriles are acrylonitrile and methacrylonitrile.

[0038] Vinyl ethers include vinyl methyl ether or vinyl isobutyl ether. Vinyl ethers of alcohols having 1 to 4 carbon atoms are preferred.

[0039] Suitable (meth)acrylates are in particular C1-C 10 -alkyl acrylates and methacrylates, in particular C1-C8-alkyl acrylates and methacrylates.

[0040] Particularly preferred are methyl acrylate, ethyl acrylate, n-butyl acrylate, n-hexyl acrylate, octyl acrylate, 2-ethylhexyl acrylate and mixtures of these monomers.

[0041] Furthermore, polar monomers which are substituted with isocyanate, amino, amide, epoxy, hydroxyl or acid groups are also suitable.

[0042] Examples include monomers having a carboxyl group, a sulfo group, or a phosphonic acid group (e.g., vinylphosphonic acid). Carboxylic groups are preferred. Examples include acrylic acid, methacrylic acid, itaconic acid, maleic acid, fumaric acid, or acryloyloxypropionic acid.

[0043] Further monomers are, for example, monomers containing hydroxyl groups, in particular C1-C 10 - hydroxyalkyl (meth)acrylates, (meth)acrylamides and monomers containing a ureido group, such as ureido (meth)acrylates.

[0044] Mono(meth)acrylates of di- or polyhydric alcohols, such as the monoacrylates or monomethacrylates of ethylene glycol or propylene glycol, also come into consideration as further monomers.

[0045] Also suitable are reaction products of (meth)acrylic acid with monoepoxides, such as phenyl glycidyl ether or glycidyl versatate.

[0046] Phenyloxyethylene glycol mono(meth)acrylate, glycidyl acrylate, glycidyl methacrylate, amino(meth)acrylate, such as 2-aminoethyl(meth)acrylate, or N-vinylpyrrolidone, or N-vinyl-N-methylacetamide, may also be mentioned as further monomers. In a preferred embodiment, the monomer is a compound having a (meth)acryloyl group.

[0047] Oligomers In this specification, an oligomer is defined as a compound having 2 to 10 polymerizable ethylenically unsaturated groups. Compounds having an average of 1.5 to 6, and particularly 2 to 5, polymerizable groups are preferred.

[0048] The weight average molecular weight Mw of the oligomer is preferably at least 300 g / mol, more preferably at least 500 g / mol. Preferably, Mw is less than 5000 g / mol, particularly preferably less than 3000 g / mol (measured by gel permeation chromatography using polystyrene as standard and tetrahydrofuran as eluent). The oligomers are in particular (meth)acryloyl compounds.

[0049] The oligomers are in particular (meth)acrylates of polyfunctional alcohols or alkoxylated polyfunctional alcohols.Examples of such alcohols are difunctional alcohols such as ethylene glycol, diethylene glycol, triethylene glycol, propylene glycol, dipropylene glycol, tripropylene glycol, butanediol, pentanediol, hexanediol, neopentyl glycol, alkoxylated phenolic compounds such as ethoxylated or propoxylated bisphenols, cyclohexanedimethanol, trifunctional and polyfunctional alcohols such as glycerol, trimethylolpropane, butanetriol, trimethylolethane, pentaerythritol, ditrimethylolpropane, dipentaerythritol, sorbitol, mannitol and the corresponding alkoxylated, in particular ethoxylated and propoxylated alcohols.

[0050] The alkoxylated alcohols are obtained in a known manner by reaction of said alcohols with alkylene oxides, in particular ethylene oxide or propylene oxide. The degree of alkoxylation of the hydroxyl groups is preferably between 0 and 10, i.e. 1 mole of hydroxyl groups may preferably be alkoxylated with up to 10 moles of alkylene oxide. (Meth)acrylates of polyesterols may also be mentioned as oligomers.

[0051] Suitable polyesterols are, for example, polyesterols that can be prepared by esterification of polycarboxylic acids, preferably dicarboxylic acids, with polyols, preferably diols. Starting materials for such hydroxyl-containing polyesters are known to those skilled in the art. Dicarboxylic acids preferably used are succinic acid, glutaric acid, adipic acid, sebacic acid, o-phthalic acid, its isomers and its hydrogenation products, as well as esterifiable derivatives, such as anhydrides or dialkyl esters of said acids. Maleic acid, fumaric acid, tetrahydrophthalic acid or its anhydrides are also suitable. Suitable polyols are the abovementioned alcohols, preferably ethylene glycol, 1,2- and 1,3-propylene glycol, butane-1,4-diol, hexane-1,6-diol, neopentyl glycol, cyclohexanedimethanol, and polyglycols based on ethylene glycol and propylene glycol.

[0052] The (meth)acrylates of polyesterols can be prepared in multiple stages or in a single stage from acrylic acid, polycarboxylic acids and polyols, as described, for example, in EP 279303.

[0053] Epoxide (meth)acrylates or urethane (meth)acrylates may also be suitable oligomers.

[0054] Epoxide (meth)acrylates are, for example, those obtainable by reaction of epoxidized olefins or poly- or mono- or diglycidyl ethers, such as bisphenol A diglycidyl ether, with (meth)acrylic acid.

[0055] Said reactions are known to those skilled in the art and are described, for example, in R. Holmann, UV and EB Curing Formulation for Printing Inks and Paints, London 1984.

[0056] Urethane (meth)acrylates are in particular reaction products of hydroxyalkyl (meth)acrylates with poly- or diisocyanates (see also R. Holmann, UV and EB Curing Formulation for Printing Inks and Paints, London 1984). Urethane (meth)acrylates can be present in the radiation-curable composition in a proportion of, for example, 1 to 30% by weight.

[0057] The compounds may contain further functional groups, for example hydroxyl groups that are not esterified with (meth)acrylic acid.

[0058] Further oligomers are low molecular weight unsaturated polyesters which contain double bonds, in particular as a result of a content of maleic or fumaric acid, and which are copolymerizable.

[0059] Preferred oligomers are fluid at 20° C. and 1 bar.

[0060] In a preferred embodiment, the oligomer is a (meth)acryloyl compound, in particular a (meth)acrylate of a polyfunctional alcohol, in particular a (meth)acryloyl compound having no other functional groups besides hydroxyl or ether groups.

[0061] The most preferred oligomers are (meth)acryloyl compounds which are fluid at 20° C. and 1 bar and have 2 to 5 (meth)acryloyl groups.

[0062] polymer In addition to the above monomers and / or oligomers, the radiation-curable composition may contain polymers that already have a high molecular weight, such polymers having a molecular weight Mw of more than 3000, in particular more than 5000 (measured by gel permeation chromatography using polystyrene as standard and tetrahydrofuran as eluent).

[0063] Suitable polymers may have reactive groups, such as polymerizable ethylenically unsaturated groups, or other functional groups that react with corresponding groups of any monomer or oligomer, thereby resulting in bonding to said monomer or oligomer during curing, but also suitable are polymers that do not have such groups, which subsequently form a separate continuous phase or an interpenetrating network in the resulting coating.

[0064] Suitable polymers are, for example, polyesters, polyadducts, especially polyurethanes, or polymers obtained by free radical polymerization. Polymers obtained by free radical polymerization are particularly suitable, preferably C1-C 20 Suitable are those which contain at least 40% by weight, particularly preferably at least 60% by weight and very particularly preferably at least 80% by weight of so-called main monomers selected from alkyl (meth)acrylates, vinyl esters of carboxylic acids containing up to 20 carbon atoms, vinyl ethers of monoalcohols containing up to 20 carbon atoms, vinyl aromatic compounds containing up to 20 carbon atoms and / or ethylenically unsaturated nitriles.

[0065] In a preferred embodiment, the radiation curable composition used as an ink-jet ink contains a (meth)acryloyl compound.

[0066] In a particularly preferred embodiment, the radiation curable composition used as an inkjet ink contains a monomer having a (meth)acryloyl group (hereinafter, for short, referred to as a (meth)acryloyl monomer) and / or an oligomer having a (meth)acryloyl compound (hereinafter, for short, referred to as a (meth)acryloyl oligomer).

[0067] In a particularly preferred embodiment, the radiation curable composition used as an inkjet ink contains a (meth)acryloyl oligomer, and preferably contains a (meth)acryloyl oligomer having 2 to 5 (meth)acryloyl groups.

[0068] In a preferred embodiment, at least 70% by weight of all radiation curable compounds of said radiation curable composition are (meth)acryloyl compounds and N-vinyloxazolidinones.

[0069] In addition to the radiation curable compounds, the radiation curable compositions may contain additives, such as pigments, e.g. effect pigments, dyes, fillers, stabilizers, e.g. UV absorbers, antioxidants or biocides, leveling agents, defoamers, wetting agents, antistatic agents, etc.

[0070] The radiation curable composition may contain water or organic solvents. Preferably, the radiation curable composition contains little or no water or organic solvents (compounds that are non-reactive at 20° C. and 1 bar).

[0071] In a preferred embodiment, the radiation-curable composition contains less than 20% by weight, particularly preferably less than 10 parts by weight and in particular less than 5 parts by weight, of water or organic solvent, based on 100 parts by weight of printing ink. Very particularly preferably, the radiation-curable composition contains substantially no or less than 1% by weight of water or organic solvent.

[0072] Preferably, the radiation curable composition contains at least one photoinitiator, which can for example be a so-called alpha-cleavage agent, i.e. a photoinitiator in which a chemical bond is cleaved to generate two free radicals which start further crosslinking or polymerization reactions.

[0073] For example, acylphosphine oxides (Lucirin (registered trademark) from BASF), hydroxyalkylphenones (e.g., Irgacure (registered trademark) 184), benzoin derivatives, benzyl derivatives, and dialkyloxyacetophenones are included.

[0074] In particular, the photoinitiator may be a so-called H-abstraction agent which removes a hydrogen atom from the polymer chain, for example a photoinitiator which has a carbonyl group which is transferred to a C-H bond with the formation of a CCOH group.

[0075] In particular, mention may be made here of acetophenone, benzophenone and their derivatives.

[0076] Mention may also be made of benzoin or benzoin ethers.

[0077] The photoinitiators may be used alone or as mixtures, with mixtures of photoinitiators having different modes of action being particularly suitable.

[0078] When present, the photoinitiator may be attached to the polymer or oligomer.

[0079] In the case of thermal curing or in the case of a combination of radiation and thermal curing, one or more thermally activatable initiators may be added, such as peroxides, azo compounds, etc.

[0080] The radiation curable compositions generally contain at least one dye or pigment.

[0081] The radiation curable compositions can be prepared in any desired manner by adding and mixing the individual components in any order.

[0082] The radiation curable compositions are used as printing inks in ink jet printing.

[0083] The radiation curable composition is printed onto a substrate and preferably then cured by radiation.

[0084] Printing onto a variety of substrates is possible, for example paper, metal foils or polymeric films such as polyethylene terephthalate, polyamide, polystyrene, polyvinyl chloride, polycarbonate, polyolefins such as polyethylene, polypropylene or aluminum, in particular polyolefin substrates such as polyethylene or polypropylene substrates, even if such substrates have not been corona pretreated.

[0085] A preferred embodiment of the present invention is inkjet printing onto a polypropylene or polyethylene substrate, the most preferred substrate being polyethylene. EXAMPLES

[0086] The present invention will be specifically described below with reference to examples, but the present invention is not limited to these.

[0087] An N-vinylmethyloxazolidinone-containing composition of the present invention was prepared as follows. (Preparation of mixtures with Hazen unit color number (APHA) of 200 or more) A commercially available N-vinylmethyloxazolidinone-containing composition (product name: VMOX, manufactured by BASF Societas Europea) was prepared. Figure 2 shows the GC chart of VMOX. The GC measurement conditions are as follows: <Measurement conditions> Device name: Shimadzu GC-2025 Column: DB-1 (Agilent, length: 30 m, inner diameter: 0.25 mm, film thickness: 0.25 μm) Column temperature profile: 70-300 °C (10 °C / min, hold at 70 °C for 2 minutes, heat to 300 °C and hold for 5 minutes, total 30 minutes) Carrier gas: He

[0088] Commercially available VMOX has, for example, the following composition (% by mass) (excluding impurities described below): N-vinylmethyloxazolidinone 96.2% 3-Ethenyl-4-methyl-1,3-oxazolidin-2-one 3.1% 3-Ethyl-5-methyl-1,3-oxazolidin-2-one 0.2% 5-Methyl-1,3-oxazolidin-2-one 0.0% (or trace amount) 3-(1-ethoxyethyl)-5-methyl-1,3-oxazolidin-2-one 0.1%

[0089] Next, the mixture was distilled under the following distillation condition 1 to obtain a composition containing N-vinylmethyloxazolidinone represented by the above formula I having a Hazen color number (APHA) of 66. Distillation conditions 1: Bath temperature: 135℃ Top temperature: 97-101℃ Decompression level: 5 hPa First cut: None Yield: 97%

[0090] Fig. 1 is a GC chart of the obtained N-vinylmethyloxazolidinone-containing composition of the present invention. The GC measurement conditions are the same as those in Fig. 2.

[0091] Referring to Figure 1, the main peak was confirmed at a retention time of 8.471 minutes, and this fraction is N-vinylmethyloxazolidinone. The other peaks indicate the above-mentioned other unavoidable impurities. Referring to Figure 2, the same tendency as Figure 1 is seen. Comparing Figures 1 and 2, a small peak is confirmed at a retention time of 19.852 minutes in VMOX in Figure 2, but no such peak is confirmed in Figure 1. Therefore, in order to identify the component corresponding to the retention time of 19.852 minutes, GC-MS analysis was performed under the following measurement conditions for the components remaining in the still after distillation under the distillation condition 1. In addition, the NIST Spectral Mass Library (software names NIST08, 08S, 05, 05s) or the WILEY Mass Library (software name WILEY 139) was used as the library for compound identification.

[0092] GC / MS: QP-2010Plus (manufactured by Shimadzu Corporation) Column: DB-5 ms (0.25φ×40m 0.25μm) GC oven temperature: 40℃(3.0 min)~(heating rate 10℃ / min) ~310℃(15minHold) Injection volume: 1.0μl Injection mode: Split injection Split ratio: 1 / 30

[0093] Figure 3 is a GC-MS chart of the components remaining in the still after distillation under the distillation condition 1 under the GC-MS measurement conditions. The peak numbers and retention times (RT) of 14 minutes or more in Figure 3, as well as compound names based on library search, are shown in Tables 1 and 2 below. It is assumed that compounds with retention times (RT) of less than 14 minutes contain 3-ethenyl-4-methyl-1,3-oxazolidin-2-one, 3-ethyl-5-methyl-1,3-oxazolidin-2-one, 5-methyl-1,3-oxazolidin-2-one, and 3-(1-ethoxyethyl)-5-methyl-1,3-oxazolidin-2-one contained in VMOX.

[0094] [Table 1]

[0095] [Table 2]

[0096] From the results of Tables 1 and 2, the content of impurities having a retention time of 14 minutes or more under the GC-MS measurement conditions contained in the N-vinylmethyloxazolidinone-containing composition of the present invention can be calculated, and was 0 mass% in the N-vinylmethyloxazolidinone-containing composition of the present invention.

[0097] The N-vinylmethyloxazolidinone-containing composition of the present invention obtained after distillation had almost the same composition as VMOX.

[0098] Figure 4 shows the appearance photographs of the N-vinylmethyloxazolidinone-containing composition (a) of the present invention and VMOX (b) prepared in this example. While coloring was observed in VMOX (b), the N-vinylmethyloxazolidinone-containing composition (a) of the present invention had a transparent appearance.

[0099] The present inventors have investigated the group of compounds picked up based on FIG. 3 and the library search, and have found that compounds with retention times (RT) of 14 minutes or more, particularly those with retention times (RT) of about 20 minutes (specifically, 20.137 minutes in FIG. 3) are 6-ethoxy-2,2,4-trimethyl-1,2-dihydroquinoline and those with retention times of about 21 minutes (specifically, 21.504 minutes in FIG. 3) are 4-methylproline, which are present in VMOX, and that 6-ethoxy-2,2,4-trimethyl-1,2-dihydroquinoline is a reddish brown to black liquid at room temperature, and 4-methylproline is a yellowish brown to reddish brown crystalline solid chemical substance at room temperature, and that these compounds have adverse effects on the storage stability and adhesion of the composition, as well as the transparency of the composition.

[0100] Specifically, the components (sample) remaining in the still after distillation under the above-mentioned distillation condition 1 were taken out, and the compounds contained therein were identified. (1) 6-Ethoxy-2,2,4-trimethyl-1,2-dihydroquinoline Analysis conditions: GC / MS: QP-2010Plus (manufactured by Shimadzu Corporation) Column: DB-5 ms (0.25φ×40m 0.25μm) GC oven temperature: 40℃(3.0 min)~10℃ / min ~310℃(15minHold) Injection volume: 1.0μl Injection mode: Split injection Split ratio: 1 / 30

[0101] 10.3 mg of the above sample was dissolved in 1.0 ml of CHCl3 to prepare the analytical sample. Meanwhile, 1.5 mg of 6-ethoxy-2,2,4-trimethyl-1,2-dihydroquinoline standard was dissolved in 1.5 ml of CHCl3 to prepare the analytical sample. The TIC obtained by GC / MS analysis according to the above analytical conditions is shown in Figure 5. FIG. 5(a) shows the analysis result of a 6-ethoxy-2,2,4-trimethyl-1,2-dihydroquinoline standard, and FIG. 5(b) shows the analysis result of the above analytical sample.

[0102] The retention time (RT) of the 6-ethoxy-2,2,4-trimethyl-1,2-dihydroquinoline standard detected in Figure 5(a) is 19.980 min, and a peak is also detected in Figure 5(b) at a retention time (RT) of around 19.55 min. Therefore, to confirm whether this peak is 6-ethoxy-2,2,4-trimethyl-1,2-dihydroquinoline, we redrawn the ion chromatogram using the base ion (M / Z: 202) of the MS fragment of 6-ethoxy-2,2,4-trimethyl-1,2-dihydroquinoline. The chromatogram is shown in Figure 6. Comparing M / Z: 202, the two peaks match.

[0103] The MS spectra of the samples shown in Figures 5(a) and (b) are shown in Figure 7. Since the two MS spectra are almost identical, it was found that the target peak shown in Figures 5(a) and (b) is 6-ethoxy-2,2,4-trimethyl-1,2-dihydroquinoline.

[0104] (2) 4-Methylproline Since 4-methylproline has a complex molecular structure, the samples were analyzed under the following NMR analysis conditions. Analysis conditions: Fractionation conditions: The components remaining in the still after distillation under the above distillation condition 1 were dissolved in methanol, passed through an ODS column at 6 ml / min, and fractionated using a UV detector and an RI detector. NMR measurement conditions: Deuterium oxide was used. 1 H-NMR, 13 Measurements were performed by C-NMR. NMR equipment: Varian UNITY INOVA Measurement frequency: 1 H-NMR 500MHz, 13 C-NMR 125MHz

[0105] The analytical results are shown in Figures 8 and 9. Figure 8A shows the results of the above-mentioned sample. 1 1H-NMR analysis results. 13 The C-NMR analysis results are shown in Figure 9A. 1 1H-NMR analysis results. FIG. 9B shows the results of a standard sample of 4-methylproline. 13 8 and 9 show the results of C-NMR analysis. It was confirmed that the component (sample) remaining in the still after distillation under the above-mentioned distillation condition 1 contained 4-methylproline.

[0106] Photographs of authentic 6-ethoxy-2,2,4-trimethyl-1,2-dihydroquinoline and authentic 4-methylproline are shown in Figures 10 and 11, respectively. The 6-ethoxy-2,2,4-trimethyl-1,2-dihydroquinoline specimen shown in FIG. 10 is black-brown in color, and the 4-methylproline specimen shown in FIG. 11 is yellow-brown in color.

[0107] (Inkjet ink creation) The components according to the formulation shown in Table 3 below were mixed to prepare an inkjet ink.

[0108] [Table 3]

[0109] Pigment: Pigment Blue 15:3 (PB15:3) Urethane acrylate: BASF Laromer PR9000 Isobornyl acrylate: IBXA manufactured by Osaka Organic Chemical Industry Ltd. Multifunctional acrylate VEEA: 2-(2-vinyloxyethoxy)ethyl acrylate manufactured by Nippon Shokubai Co., Ltd. Irgacure TPO: BASF acylphosphine oxide polymerization initiator, 2,4,6-trimethylbenzoyldiphenylphosphine oxide Irgacure 819: BASF acylphosphine oxide polymerization initiator, bis(2,4,6-trimethylbenzoyl)phenylphosphine oxide

[0110] The resulting ink-jet ink was subjected to the following tests. <Creating the hardened product> Each composition was applied to a PVC film "Transparent PVC RE-137" (manufactured by Mimaki Engineering Co., Ltd.) using a bar coater, and ultraviolet light was irradiated using an LED light source ultraviolet ray irradiator [model number: E075Sd HD, manufactured by Ushio Inc., irradiation wavelength 365 nm] at an irradiation intensity of 80 mW / cm. 2 The resulting cured product was obtained.

[0111] (Adhesion test) The test was carried out in accordance with JIS K5600-5-6:1999. The cured product obtained in the above <Preparation of Cured Product>, whose surface was no longer sticky when touched with a finger, was left to stand for 24 hours at room temperature of 25°C and humidity of 50%, and then 1 mm wide cuts were made with a cutter knife to create a grid (5 x 5 pieces). Cellophane adhesive tape was attached to the grid and peeled off at 90 degrees, and the peeling state of the cured product from the polyvinyl chloride substrate was visually observed. The remaining area of ​​the coated surface of the sample was visually evaluated on the following 5-point scale. The higher the score, the better the adhesion. <Evaluation criteria> 5 points: No peeling, or peeling occurs but the peeled area is less than 5% 4 points: Peeling area is 5% or more but less than 10% 3 points: Peeling area is between 10% and 30% 2 points: Peeling area 30% to less than 50% 1 point: Peeling area 50% or more

[0112] (Storage stability test) The prepared composition was placed in a sealed glass container and allowed to stand in a thermostatic chamber at 60° C. for one week, and the storage stability was evaluated from the rate of change in viscosity before and after storage calculated by the following formula (1). Viscosity change rate (%) = ((viscosity after storage for 1 week at 60°C – initial viscosity) / initial viscosity) × 100 (1) <Evaluation criteria> ○: Viscosity change rate is within 10% △: Viscosity change rate is more than 10% and less than 20% ×: Viscosity change rate exceeds 20%

[0113] The results are shown in Table 3. From the results in Table 3, it was found that the N-vinylmethyloxazolidinone-containing composition of the present invention has high transparency and can inhibit the viscosity increase of the product over time, thereby imparting excellent storage stability.

[0114] (Surface curing time) The components according to the formulation shown in Table 4 below were mixed to prepare mixed solutions 1 and 2.

[0115] [Table 4]

[0116] In the presence of a light source emitting weak ultraviolet light (eg, a fluorescent lamp), 3 ml of each of the mixed solutions 1 and 2 shown in Table 4 above was dropped into separate petri dishes, and the time until the surface hardened was measured. As a result, the time until the surface of the mixed liquid 1 hardened was 8 minutes, and the time until the surface of the mixed liquid 2 hardened was 30 minutes.

[0117] (Color change) Mixtures 3 and 4 were prepared by mixing the composition of the present invention and each component prepared separately in the formulation shown in Table 5 below.

[0118] [Table 5]

[0119] 10 g of each of the mixed solutions 3 and 4 shown in Table 5 above was taken and placed in separate 100 ml containers. After heating at 80° C. for 180 minutes, the change in color tone over time was examined. As a result, the APHA of mixed solution 3 before heating was 100, and the APHA after heating was 200. On the other hand, the APHA of mixed solution 4 before heating was 25, and the APHA after heating was 40-50.

Claims

1. A composition containing N-vinylmethyloxazolidinone represented by the following formula I, in which 6-ethoxy-2,2,4-trimethyl-1,2-dihydroquinoline and 4-methylproline are contained in an amount of 1 mass % or less. 【Chemical 1】

2. 2. The composition of claim 1, having a Hazen Color Scale (APHA) of 150 or less.

3. The composition according to claim 1, wherein the content of impurities having a retention time of 14 minutes or more is 1% by mass or less under the following GC-MS measurement conditions: GC / MS: QP-2010Plus (manufactured by Shimadzu Corporation) Column: DB-5 ms (0.25φ×40m 0.25μm) GC oven temperature: 40°C (3.0 min) - (heating rate 10°C / min) - 310°C (15 min hold) Injection volume: 1.0μl Injection mode: Split injection Split ratio: 1 / 30

4. 10. The composition of claim 1 further comprising 3-ethenyl-4-methyl-1,3-oxazolidin-2-one, 3-ethyl-5-methyl-1,3-oxazolidin-2-one, 5-methyl-1,3-oxazolidin-2-one, and 3-(1-ethoxyethyl)-5-methyl-1,3-oxazolidin-2-one.

5. A mixture containing N-vinylmethyloxazolidinone represented by the following formula I, 3-ethenyl-4-methyl-1,3-oxazolidin-2-one, 3-ethyl-5-methyl-1,3-oxazolidin-2-one, 5-methyl-1,3-oxazolidin-2-one, and 3-(1-ethoxyethyl)-5-methyl-1,3-oxazolidin-2-one is provided: The mixture is distilled to adjust the contents of 6-ethoxy-2,2,4-trimethyl-1,2-dihydroquinoline and 4-methylproline to 1 mass % or less, thereby obtaining a composition containing N-vinylmethyloxazolidinone represented by the following formula I: A method for producing the composition of claim 1. 【Chemistry 2】

6. obtaining a composition containing N-vinylmethyloxazolidinone represented by formula I, which has a Hazen color value (APHA) of 150 or less; The method of claim 5.

7. A radiation-curable composition comprising the composition of claim 1.

8. An ink-jet ink comprising the composition of claim 1.

9. A hard coat film comprising the composition according to claim 1.

10. An adhesive film comprising the composition of claim 1.

Citation Information

Patent Citations

  • Inkjet printing ink containing N-vinyloxazolidinone

    JP2016529360A

  • Preparation of N-vinyl-2-oxazolidinone

    US4831153A

Cited By

  • Continuous synthesis method of 3-N-(1-ethoxyethyl)-5-methyl oxazolidine-2-ketone

    CN121085864A

  • A continuous process for the synthesis of 3-n-(1-ethoxyethyl)-5-methyl oxazolidin-2-one

    CN121085864B