Artificial wood and production method therefor

The described method enhances the reproducibility and natural appearance of artificial wood by using multiple coating layers and embossing techniques to mimic wood grain patterns, addressing the issues of previous resin-based products.

JP2024147782APending Publication Date: 2024-10-16TAICANG ASAHI LINE AUTOMATIC SYST
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2024118788
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2024-07-24
Publication Date
2024-10-16

AI Technical Summary

Technical Problem

Existing artificial wood products lack high reproducibility of wood grain patterns and often have an unnatural appearance due to variations in resin mixing methods and conditions, leading to an easily recognizable resin feel.

Method used

A manufacturing method involving multiple coating layers, embossing, and polishing to create a wood grain pattern by exploiting color differences between layers, with controlled thickness and embossing techniques to mimic natural wood grain.

Benefits of technology

The method achieves artificial wood with high reproducibility and a less unnatural appearance, resembling natural wood grain effectively.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024147782000001_ABST
    Figure 2024147782000001_ABST
Patent Text Reader

Abstract

To provide artificial wood with excellent reproductivity of a wood texture that allows little discomfort on its appearance to be felt, and a production method therefor.SOLUTION: A production method for artificial wood 1 according to an aspect of the present invention is provided with: a firs coating layer forming step for forming a first coating layer 3 on a substrate 2; a second coating layer forming step for forming a second coating layer 4 on the first coating layer; an embossing step for embossing irregularity of a wood texture with an embossing roller 5 from over the second coating layer; and a wood texture forming step for forming a wood texture through color difference between the first coating layer and the second coating layer by exposing a part of the first coating layer through polishing of the second coating layer. An artificial wood according to another aspect of the present invention is provided with: a substrate including substrate resin; a first coating layer including first resin and formed on the substrate; and a second coating layer including second resin and formed on the first coating layer, wherein the wood texture is formed through color difference between the first coating layer and the second coating layer by embossing irregularity of the wood texture from over the second layer with the embossing roller, and exposing a part of the first resin by polishing the second coating layer.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to an artificial wood material and a method for producing the same. [Background technology]

[0002] Due to its moderate hardness and ease of processing, wood has been extremely useful since ancient times as a building and civil engineering material, and also as a material for everyday items such as furniture, tableware, etc. Wood also has distinctive grain on its cross section, and is often used to create a sense of luxury and security.

[0003] On the other hand, in recent years, resin materials are increasingly being used instead of wood due to their moderate hardness and ease of molding. In particular, resin materials can be colored in various colors and given a glossy finish by mixing pigments, etc., and these characteristics can be used to create features that wood does not have.

[0004] However, even when a resin material is used, there is a certain demand for an appearance similar to that of wood to obtain the sense of luxury and security that is associated with wood.

[0005] As an example of this prior art, Patent Document 1 below discloses an artificial wood material that has an appearance similar to that of wood, which is made by appropriately kneading a plurality of resins. [Prior art documents] [Patent documents]

[0006] [Patent Document 1] Japanese Patent Application Publication No. 8-197514 Summary of the Invention [Problem to be solved by the invention]

[0007] However, in the above-mentioned Patent Document 1, while it is necessary to mix multiple resins, there are problems in that the appearance varies greatly depending on the mixing method and conditions, and the reproducibility is not high. In addition, such artificial wood has a smooth surface, which is unnatural in feel and appearance, and is immediately recognizable as being resin.

[0008] In view of the above problems, the present invention has an object to provide an artificial wood material having a high reproducibility of wood grain pattern and a less unnatural appearance, and a manufacturing method thereof. [Means for solving the problem]

[0009] A method for manufacturing artificial wood that solves the above problems includes a first coating layer forming step of forming a first coating layer on a base layer, a second coating layer forming step of forming a second coating layer on the first coating layer, an embossing step of pressing the unevenness of the wood grain from above the second coating layer with an embossing roller, and a wood grain pattern forming step of polishing the second coating layer to expose a portion of the first coating layer and forming a wood grain pattern by the difference in color between the first coating layer and the second coating layer.

[0010] In addition, in this aspect, although not limited thereto, it is preferable that the grain pattern forming step varies the polishing depth depending on the position on the surface of the first coating layer.

[0011] In addition, in this respect, although not limited thereto, the thickness of the first coating layer is preferably in the range of 0.2 mm or more and 1.0 mm or less.

[0012] In addition, in this respect, although not limited thereto, the thickness of the second coating layer is preferably in the range of 0.05 mm or more and 0.4 mm or less.

[0013] Also, in this respect, although not limited thereto, it is preferable that the wood grain pattern forming step comprises polishing the second coating layer so that the boundary between the first coating layer and the second coating layer extends in one direction while being curved.

[0014] In addition, an artificial wood material according to another aspect of the present invention comprises a base layer containing a base layer resin, a first coating layer containing a first resin and formed on the base layer, and a second coating layer containing a second resin and formed on the first coating layer, in which an embossing roller is used to create a wood grain pattern on top of the second coating layer, and the second coating layer is further polished to expose a portion of the first resin, and a wood grain pattern is formed by the difference in color between the first coating layer and the second coating layer. Effect of the Invention

[0015] As described above, the present invention can provide an artificial wood material having a high degree of reproducibility of wood grain patterns and a natural appearance, and a method for manufacturing the same. [Brief description of the drawings]

[0016] [Figure 1] FIG. 2 is a flow chart showing the process flow of the manufacturing method for artificial wood according to the embodiment. [Diagram 2] 1 is a diagram showing an outline of an artificial wood manufacturing system for manufacturing artificial wood according to an embodiment. [Diagram 3] 1 is a schematic perspective view of an artificial wood member according to an embodiment of the present invention; [Figure 4] 1 is a schematic diagram of a cross section of an artificial wood member according to an embodiment of the present invention. [Diagram 5] 1 is a schematic perspective view of a base layer of an artificial wood according to an embodiment of the present invention; [Figure 6] 1 is a schematic oblique view of an artificial wood according to an embodiment of the present invention when a first coating layer is formed on a base layer thereof. [Figure 7] FIG. 2 is a schematic perspective view of an artificial wood according to an embodiment in which a first coating layer is formed on a base layer, and a second coating layer is further formed thereon (unsanded wood). [Figure 8] 3 is a schematic diagram of an embossing roller for creating uneven wood grain on the second coating layer of the artificial wood according to the embodiment. FIG. [Figure 9] 1 is a schematic diagram of a polishing roller in an artificial wood manufacturing system according to an embodiment. [Figure 10]FIG. 2 is a photograph of an artificial wood material produced according to an embodiment. BEST MODE FOR CARRYING OUT THEINVENTION

[0017] Hereinafter, the embodiments of the present invention will be described in detail with reference to the drawings. However, the present invention can be embodied in many different forms, and is not limited to the specific examples described in the following embodiments and examples.

[0018] Fig. 1 is a flow diagram showing the process flow of the method for producing artificial wood according to this embodiment (hereinafter referred to as "this method"). As shown in this figure, this method includes a step of forming a base layer (S0), a step of forming a first coating layer on the base layer (S1), a step of forming a second coating layer on the first coating layer (S2), a step of forming a second coating layer on the first coating layer (S3), a step of pressing the unevenness of the wood grain from above the second coating layer with an embossing roller, and a step of forming a wood grain pattern by polishing the second coating layer to expose a part of the first coating layer and forming a wood grain pattern by the difference in color between the first coating layer and the second coating layer (S4).

[0019] 2 is a schematic diagram of an actual artificial wood manufacturing system (hereinafter referred to as "this system") S relating to one example for realizing this method. As shown in this figure, this system S includes a base layer forming device M1 for forming a base layer 2, a first coating layer forming device M2 for forming a first coating layer 3 on the base layer 2, a second coating layer forming device M3 for forming a second coating layer 4 on the first coating layer 3, and a conveying mechanism M4 for conveying the base layer 2 sequentially from the base layer forming device M1 to the first coating layer forming device M2 and the second coating layer forming device M3. Furthermore, the conveying mechanism M4 is further configured to convey the base layer 2 formed up to the second coating layer 4 to at least one, preferably a plurality of polishing rollers 6 as shown in this figure, and polish it.

[0020] Fig. 3 is a schematic perspective view of artificial wood (hereinafter referred to as "real wood") 1 produced by the present method, and Fig. 4 is a schematic cross-sectional view of the real wood 1. The real wood 1 comprises a base layer 2, a first coating layer 3 covering the base layer 2, and a second coating layer 4 covering the first coating layer 3, and the second coating layer 4 is polished to expose a part of the first coating layer 3, and a wood grain pattern is formed by the difference in color between the first coating layer 3 and the second coating layer 4.

[0021] The above-mentioned treatment makes it possible to provide artificial wood with a highly reproducible grain pattern and a natural appearance, as will be described in detail later.

[0022] This method first includes a step of forming a base layer (S0). In this step, the "base layer" refers to a layer that serves as a foundation for forming a first coating layer 3 and a second coating layer 4, which will be described in detail later. It is preferable that the base layer is made of a material containing a basic resin, but it is also possible to use a metal such as aluminum.

[0023] In addition, the "basic resin" in this step means the resin contained in the base layer, and "basic" is a prefix used to distinguish it from the resin in the first coating layer and the second coating layer described below, and does not have any technical meaning in itself.

[0024] The resin in this step is not limited, but is preferably at least one of polyethylene, polypropylene, and ionomer resin.

[0025] In this step, the base layer 2 may contain wood flour in addition to the basic resin. "Wood flour" refers to wood obtained by finely grinding compatible wood into a powder form.

[0026] In addition, the size of the wood flour is not limited, but the average size of the wood flour measured by the mesh passing rate is preferably 20 mesh or more and 100 mesh or less, and more preferably 40 mesh or more and 80 mesh or less. By making it 40 mesh or more, there is an advantage that the water absorption rate can be reduced, and by making it 80 mesh or less, there is an advantage that the blending efficiency with the resin can be maintained high.

[0027] The blending ratio of wood flour and resin in the base layer 2 in this step is not limited as long as it can function as the base layer 2, but when the weight of the entire base layer 2 is taken as 100, it is preferable that the base wood flour content is in the range of 50 to 70, and more preferably in the range of 55 to 65. A ratio of 55 or more has the advantage of being able to reduce the shrinkage rate, and a ratio of 65 or less has the advantage of being able to increase the strength.

[0028] In this step, the base layer 2 may contain additives in addition to the wood flour and resin. Examples of additives include, but are not limited to, a compatibilizer, a lubricant, etc. The use of a compatibilizer has the advantage that even when a plurality of different materials are mixed, the materials can be mixed uniformly. The use of a lubricant has the advantage that friction between the resin and the metal surface of the molding machine and between resins can be reduced, and fluidity and releasability can be improved, thereby improving processability. Examples of compatibilizers include, but are not limited to, maleic anhydride compatibilizers, acrylic acid compatibilizers, and butyl acrylate compatibilizers. Examples of lubricants include zinc stearate, polyethylene wax, etc.

[0029] The amount of the compatibilizer added is not limited as long as the function of the base layer 2 can be ensured, but it is preferable that the amount is in the range of 1 to 7, and more preferably 3 to 5, based on the total weight of the base layer 2 being 100.

[0030] The amount of lubricant added is not limited as long as the function of the base layer 2 can be ensured, but it is preferable that the amount of lubricant added is in the range of 1 to 5, and more preferably 1 to 2, based on the total weight of the base layer 2 being 100.

[0031] As described above, the base layer 2 is a layer that serves as a base for forming the first coating layer 3 and the second coating layer 4. The base layer 2 itself may be a layer formed on the surface of another material, but it is also preferable that the base layer 2 itself is an important member that forms the skeleton of the artificial wood. In addition, from the viewpoint of easily forming the first coating layer 3 and the second coating layer 4 with a uniform thickness, at least a part of the base layer 2 preferably has a flat surface, specifically, a plate-shaped member or a columnar member. If it has a flat surface, it is possible to form the first coating layer 3 and the second coating layer 4 uniformly as described above, and by polishing the second coating layer 4, it is possible to expose a part of the first coating layer 3 to have a desired shape and form a desired wood grain pattern. FIG. 5 shows a perspective schematic diagram of the base layer 2 in the real wood 1.

[0032] Next, the method includes a first coating layer forming step (S1) of forming a first coating layer containing a first resin on the base layer.

[0033] As is clear from the above description, the "first coating layer" in this step refers to a coating layer that covers the base layer, and is configured to contain a first resin.

[0034] In addition, the "first resin" in this step refers to the resin contained in the first coating layer, and "first" is a prefix used to distinguish it from the resin in the base layer described above and the second coating layer described below, and does not have any technical meaning in itself. The "resin" may be the same as the above-mentioned basic resin, and is preferably at least one of polyethylene, polypropylene, ionomer resin, and Surlyn resin, for example.

[0035] In addition to the resin, the first coating layer 3 in this step may contain an appropriate additive. Examples of the additive include, but are not limited to, a compatibilizer, a colorant, an adhesive, and an antioxidant.

[0036] The use of a compatibilizer has the advantage that, even when a plurality of different materials are mixed, the materials can be mixed uniformly. Examples of the compatibilizer include, but are not limited to, maleic anhydride compatibilizer, acrylic acid compatibilizer, butyl acrylate compatibilizer, etc.

[0037] In addition, the amount of compatibilizer added is not limited as long as the function of the first coating layer 3 can be ensured, but it is preferable that the amount is in the range of 1 to 7, and more preferably 3 to 5, when the total weight of the first coating layer 3 is 100.

[0038] Furthermore, by adding a colorant to the first coating layer 3, the first coating layer 3 can be colored in a desired color. The color of the colorant is not particularly limited, but it is preferable that the color or concentration of the colorant in the second coating layer 4, which will be described in detail later, is different. Examples of the colorant include a carbon black colorant, an oak colorant, a gold colorant, a gray colorant, a dark teak colorant, and a dark walnut colorant.

[0039] In addition, the amount of colorant added is not limited as long as the function of the first coating layer 3 is ensured, but it is preferable that the amount of colorant added is in the range of 1 to 6, and more preferably 3 to 4, when the total weight of the first coating layer 3 is 100.

[0040] Furthermore, by using an adhesive for the first covering layer 3, there is an advantage that it can be reliably adhered to the base layer 2. Furthermore, examples of the adhesive include an epoxy resin adhesive and a urethane adhesive.

[0041] In addition, the amount of adhesive added is not limited as long as it can ensure its function as the first coating layer 3, but it is preferable that the amount of adhesive added be in the range of 1 to 7, and more preferably 3 to 5, when the total weight of the first coating layer 3 is 100.

[0042] In addition, there is an advantage that oxidation can be prevented and quality deterioration can be prevented by using an antioxidant in the first coating layer 3. In addition, examples of the antioxidant include organic antioxidants and phosphorus-based antioxidants.

[0043] In addition, the amount of antioxidant added is not limited as long as the function of the first coating layer 3 is ensured, but it is preferable that the amount is in the range of 0.1 to 3, and more preferably 0.5 to 1, when the total weight of the first coating layer 3 is 100.

[0044] In addition, in this step, although not limited thereto, the thickness of the first coating layer 3 is preferably in the range of 0.2 mm to 1.0 mm, more preferably in the range of 0.4 mm to 0.8 mm. If it is 0.4 mm or more, the effect is more remarkable. On the other hand, if it is 1.0 mm or less, it is possible to obtain the effect without unnecessary thickness and to save costs, so it is more preferable to make it 0.8 mm or less. Note that FIG. 6 shows an image of a cross section when the first coating layer 3 is formed on the base layer 2 of the wood 1.

[0045] This method also includes a second coating layer forming step (S2) of forming a second coating layer containing a second resin on the first coating layer.

[0046] As is clear from the above description, the "second coating layer" in this step refers to a coating layer that covers the first coating layer. The second coating layer also contains a second resin. Here, "second" is an ordinal number used to distinguish the first coating layer from the first coating layer, since the second coating layer covers the same base layer, and has no other technical meaning.

[0047] Furthermore, in this step, it is preferable that the second coating layer 4 covers at least a part, and preferably the entirety, of the first coating layer 3. In this way, a part of the first coating layer 3 can be exposed in a later step, and the boundary between them can be used as a wood grain pattern. Note that Fig. 7 shows an image of a cross section of real wood 1 in an unpolished state in which the first coating layer 3 is formed on the base layer 2 of the real wood 1 and the second coating layer 4 is further formed on top of that (hereinafter referred to as "unpolished wood").

[0048] In addition, the "second resin" in this step means the resin contained in the second coating layer, and "second" is an ordinal number used to distinguish it from the resin in the base layer and the first coating layer, just like the "second" in the second coating layer, and does not have any technical meaning in itself. Also, the "resin" is the same as the above-mentioned basic resin, and is not limited thereto.

[0049] The type of the second resin in this step may be the same as the above-mentioned basic resin, and is preferably at least one of polyethylene, polypropylene, ionomer resin, and Surlyn resin, for example.

[0050] In addition to the above resin, the second coating layer 4 in this step may contain an appropriate additive. Examples of the additive include, but are not limited to, a compatibilizer, a colorant, an adhesive, and an antioxidant.

[0051] The use of a compatibilizer has the advantage that, even when a plurality of different materials are mixed, the materials can be mixed uniformly. Examples of the compatibilizer include, but are not limited to, maleic anhydride compatibilizer, acrylic acid compatibilizer, butyl acrylate compatibilizer, etc.

[0052] In addition, the amount of compatibilizer added is not limited as long as the function of the second coating layer 4 is ensured, but it is preferable that the amount is in the range of 1 to 7, and more preferably 3 to 5, when the total weight of the second coating layer 4 is 100.

[0053] Furthermore, by adding a colorant to the second coating layer 4, the second coating layer 4 can be colored in a desired color. The color of the colorant is not particularly limited, but it is preferable that the color or concentration of the colorant in the first coating layer 3 is different from that of the colorant in the first coating layer 3. Specific examples of the colorant are not limited, but include, for example, a carbon black colorant, an oak colorant, a gold colorant, a gray colorant, a dark teak colorant, and a dark walnut colorant.

[0054] In addition, the amount of colorant added is not limited as long as the function of the second coating layer 4 is ensured, but it is preferable that the amount of colorant added is in the range of 1 to 6, and more preferably 3 to 4, when the total weight of the second coating layer 4 is 100.

[0055] Furthermore, by using an adhesive for the second covering layer 4, there is an advantage that it can be reliably adhered to the first covering layer 3. Furthermore, examples of the adhesive include an epoxy resin adhesive, a urethane adhesive, and the like.

[0056] In addition, the amount of adhesive added is not limited as long as the function of the second coating layer 4 is ensured, but it is preferable that the amount of adhesive added is in the range of 1 to 7, and more preferably 3 to 5, when the total weight of the second coating layer 4 is 100.

[0057] In addition, there is an advantage that oxidation can be prevented and quality deterioration can be prevented by using an antioxidant in the second coating layer 4. In addition, examples of the antioxidant include organic antioxidants and phosphorus-based antioxidants.

[0058] In addition, the amount of antioxidant added is not limited as long as the function of the second coating layer 4 is ensured, but it is preferable that the amount is in the range of 0.1 to 3, and more preferably 0.5 to 1, when the total weight of the second coating layer 4 is 100.

[0059] In this step, although not limited thereto, the thickness of the second coating layer 4 is preferably in the range of 0.05 mm to 0.4 mm, more preferably in the range of 0.2 mm or less. A thickness of 0.05 mm or more provides a coating effect of being able to sufficiently cover the first coating layer 3, while a thickness of 0.4 mm or less provides an advantage of being able to easily expose the first coating layer 3 by polishing, and a thickness of 0.2 mm or less makes this effect more pronounced.

[0060] This method also includes an embossing step (S3) in which an embossing roller is used to press the unevenness of the wood grain onto the second coating layer. By forming the unevenness to form the wood grain, it is possible to distinguish between positions that are easy to cut and positions that are difficult to cut in the subsequent polishing step, which is advantageous in that it makes it easier to form a wood grain that is closer to the real thing. It is particularly effective to add the unevenness while the wood is still soft. Figure 8 shows a schematic diagram of the embossing roller 5 used in this step.

[0061] In addition, this method may include a cutting step after this step. According to this method, after the base layer 2, the first coating layer 3, and the second coating layer 4 are formed, they can be cut into a desired product size, making them easier to handle. In addition, after the above step, the product can be cured (cooled and solidified) for about one day to stabilize its quality.

[0062] This method also includes a grain pattern forming step (S4) of polishing the second coating layer to expose a part of the first coating layer, and forming a grain pattern by the difference in color between the first coating layer and the second coating layer. As is clear from the above description, in this step, the entire first coating layer 3 is first covered, the first coating layer 3 is hidden, and then unevenness is formed, and the second coating layer 4 is polished to expose a part of the first coating layer 3. As a result, the boundary between these two layers is expressed as a grain pattern. Note that the "grain pattern" here refers to a pattern that is not a real grain, but looks like a grain. In addition, the "grain" includes not only the grain that appears when wood is cut perpendicular to its growth direction, but also the grain (wood grain) that appears when wood is cut along its growth direction. The image of the real wood 1 produced by this method is as shown in Figure 3 above.

[0063] In addition, in this step, it is preferable to vary the polishing depth depending on the position on the surface of the first coating layer 3. This has the advantage that it is possible to create a pattern that is not regular but resembles natural wood grain. In particular, this polishing depth, in addition to the previous unevenness pressing step, can form unevenness and patterns similar to the feel of natural wood, which has the advantage of reducing the sense of incongruity for those who touch the wood 1.

[0064] Furthermore, in this step, it is preferable to further polish the second coating layer 4 so that the boundary between the first coating layer 3 and the second coating layer 4 is curved while extending in one direction. By forming the boundary between the first coating layer 3 and the second coating layer 4 so that it is curved while extending in one direction in this way, there is an advantage that a pattern that more closely resembles natural wood grain can be obtained, as described above. Of course, in this case, it is preferable to form multiple boundaries.

[0065] In this step, a part of the first coating layer 3 can be ground off, but it is preferable not to expose the base layer 2. By setting the depth of grinding to a range that does not expose the base layer 2, it is possible to ensure the strength of the wood 1 itself. In other words, the depth of grinding in this step is less than the total thickness of the first coating layer 3 and the second coating layer 4.

[0066] The polishing method in this step is not limited as long as it can realize the above-mentioned effect, but it is preferable to use a polishing roller 6 to polish the wood (unpolished wood) in which the first coating layer 3 is formed on the base layer 2, the first coating layer 3 is entirely covered with the second coating layer 4, and the unevenness is pressed. This is a simple configuration and is preferable from the viewpoint of being able to mass-produce real wood 1 with a similar pattern. An image of the polishing roller 6 in this case is shown in FIG. 9. In this case, it is preferable that the polishing roller 6 has different conditions such as the amount, thickness, and length of the abrasive material applied to the surface in each of its axial direction and rotation direction. By doing so, there is an advantage that unevenness occurs in the vertical and horizontal directions of the surface of the real wood 1, making it possible to make the wood more close to the natural grain. In addition, the number of polishing rollers used in this step is not particularly limited, and it is also preferable to polish sequentially using multiple polishing rollers. This makes it possible to achieve a more complex polished state.

[0067] As described above, the present embodiment can provide an artificial wood material having a high degree of wood grain reproducibility and a natural appearance, and a method for manufacturing the same. EXAMPLES

[0068] Here, the above-mentioned artificial wood was actually produced and its effects were confirmed.

[0069] First, a mixture of polyethylene and wood powder was formed into a base layer 40 mm high and 219 mm wide (extrusion length 1,830 mm), and then a first coating layer 0.6 mm thick was applied on top of it. This first coating layer was made of polyethylene, polypropylene, and Surlyn resin, and was colored by adding 3.5% by weight of oak coloring agent.

[0070] Next, the entire first coating layer was covered with a 0.05mm second coating layer. As a result, the first coating layer was completely covered, and the wood was left unpolished. This second coating layer was also made of polyethylene, polypropylene, and Surlyn resin, to which 3.5% by weight of dark teak colorant was added as a colorant. In other words, the first coating layer and the second coating layer were made to be different colors.

[0071] The wood grain pattern was then pressed with an embossing roller to create the wood grain pattern, and after cutting and curing, the wood was polished with a polishing roller to expose part of the first coating layer and reveal the wood grain pattern, completing the product. Figure 10 shows a photograph of the product.

[0072] As described above, it has been confirmed that this embodiment can provide an artificial wood material having a high reproducibility of wood grain and a natural appearance, and a manufacturing method thereof. [Industrial Applicability]

[0073] INDUSTRIAL APPLICABILITY The present invention has industrial applicability as an artificial wood material and a manufacturing method thereof. [Explanation of symbols]

[0074] 1…Artificial wood 2...Base layer 3...First coating layer 4...Second coating layer 5…Embossing roller 6...Abrasive roller M1…Base layer forming device M2…first coating layer forming device M3…Second coating layer forming device M4: Transport mechanism

Claims

1. A first coating layer forming step of forming a first coating layer on a base layer; a second coating layer forming step of forming a second coating layer on the first coating layer; an embossing step of pressing the unevenness of the wood grain from above the second coating layer with an embossing roller; A method for manufacturing artificial wood, comprising a wood grain pattern forming step of polishing the second coating layer to expose a portion of the first coating layer, and forming a wood grain pattern by using a difference in color between the first coating layer and the second coating layer.

2. 2. The method for producing artificial wood according to claim 1, wherein said grain pattern forming step varies the polishing depth depending on the position on the surface of the first coating layer.

3. 2. The method for producing artificial wood according to claim 1, wherein the thickness of the first coating layer is in the range of 0.2 mm to 1.0 mm.

4. 2. The method for producing artificial wood according to claim 1, wherein the thickness of the second coating layer is in the range of 0.05 mm to 0.4 mm.

5. The method for manufacturing artificial wood as described in claim 1, wherein the wood grain pattern forming step comprises polishing the second coating layer so that the boundary between the first coating layer and the second coating layer extends in one direction while being curved.

6. A base layer including a base layer resin; a first coating layer formed on the base layer, the first coating layer including a first resin; a second coating layer including a second resin and formed on the first coating layer; The second coating layer is then pressed with an embossing roller to create a grain pattern. The artificial wood is formed by exposing a part of the first resin and forming a wood grain pattern by the difference in color between the first coating layer and the second coating layer.

Citation Information

Patent Citations

  • Manufacture of plate-like artificial wood having straight grain pattern

    JP1996197514A