Synthetic resin container and manufacturing method
Patent Information
- Application Number
- JP2023191724
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-04
- Filing Date
- 2023-11-09
- Publication Date
- 2024-10-17
Smart Images

Figure 2024148134000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a synthetic resin container and a manufacturing method thereof. [Background technology]
[0002] Conventionally, synthetic resin containers have been widely used for various purposes. In recent years, in response to social demand, recycling techniques have been considered for collecting used and discarded containers and reusing them as recycled materials to manufacture new synthetic resin containers.
[0003] For example, Patent Document 1 discloses a technology for reusing (recycling) discarded plastic packaging containers, which includes a process of crushing or coarsely crushing discarded thermoplastic resin packaging containers into small pieces, applying an impact frictional force to the resulting small pieces to separate the resin material from the attached matter, and granulating the resin material. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] Japanese Patent Application Publication No. 09-220721 Summary of the Invention [Problem to be solved by the invention]
[0005] However, in a circulatory recycling technology in which discarded containers are collected and new recycled containers are manufactured from resin materials made from the collected products, a deterioration in physical properties specific to the recycled containers is observed due to the mixture of various collected products. In addition, even recycled resin materials that have been collected and subjected to a separation process and a washing process may be contaminated with foreign matter remaining in the recycled raw materials, such as deteriorated resin or burnt resin, as well as metal, sand, pigments, fillers, etc. Therefore, various problems may occur in the regenerated recycled containers, such as a decrease in the adhesion (sealing property) of the fitting parts and a decrease in impact strength, making them more likely to break when dropped. On the other hand, there is a demand for manufacturing recycled containers using a high content of recycled materials.
[0006] Therefore, the inventors conducted extensive research to solve the above-mentioned problems when turning collected synthetic resin containers into raw materials and reusing them to manufacture new synthetic resin containers (recycled containers), and as a result, they have completed the present invention. [Means for solving the problem]
[0007] The method for manufacturing a synthetic resin container according to the present invention includes sandwiching a parison extruded from an extruder through a die head between a pair of split dies, and blowing air into the parison to blow it into a predetermined container shape having a mouth portion and a storage portion, wherein recycled resin material obtained from recovered synthetic resin containers is discharged from a die head outlet for recycled resin provided in the die head to form a parison, and in a predetermined region, reinforcing resin material is discharged from a die head outlet for reinforcing resin provided in the die head so as to be discharged onto the inner side of the resin material discharged from the die head outlet for recycled resin, thereby partially forming a layer made of reinforcing resin on the inner side of the parison, and blow molding is performed by sandwiching the parison between the split dies so that the mouth portion is formed in a portion corresponding to the layer made of reinforcing resin, and the inner surface of the mouth portion is formed by the reinforcing resin.
[0008] In addition, the method for producing a synthetic resin container according to the present invention includes a step of sandwiching a parison extruded from an extruder through a die head between a pair of split dies, blowing air into the parison to blow the parison into a predetermined container shape having a mouth portion and a storage portion, ejecting recycled resin material obtained from recovered synthetic resin containers from a die head outlet for recycled resin provided in the die head to form a parison, and ejecting a reinforcing resin material in a predetermined region from a die head outlet for reinforcing resin provided in the die head so as to be ejected on the outer circumferential side of the resin material ejected from the die head outlet for recycled resin, thereby partially forming a layer made of reinforcing resin on the outer circumferential side of the parison, sandwiching the parison between the split dies to perform blow molding so that the mouth portion is formed in a portion corresponding to the layer made of reinforcing resin, and then cutting the inner circumferential surface side of the mouth portion to expose at least a portion of the layer made of reinforcing resin to the inner circumferential surface of the mouth portion, and forming at least a portion of the inner circumferential surface of the mouth portion with the reinforcing resin.
[0009] In addition, the synthetic resin container of the present invention is a synthetic resin container made of recycled resin material obtained from collected synthetic resin containers, and includes a mouth portion which serves as an outlet for pouring the contents, and a storage portion, and the mouth portion is configured to be sealed when a lid body is attached by close contact between the inner surface of the mouth portion and the sealing surface of an inner ring provided on the lid body, and a layer made of reinforcing resin is provided on the mouth portion. Effect of the Invention
[0010] According to the present invention, it is possible to provide a synthetic resin container having stable physical properties in specific areas and a method for manufacturing the same, by using collected synthetic resin containers as raw materials and reusing these to manufacture new synthetic resin containers. [Brief description of the drawings]
[0011] [Figure 1] 1 is an explanatory diagram showing an outline of a synthetic resin container according to an example of this embodiment; [Diagram 2] 1 is an enlarged cross-sectional view of a main portion of a synthetic resin container according to an example of this embodiment. [Diagram 3] 1 is an enlarged cross-sectional view of a main portion of a parison for blow molding a synthetic resin container according to an example of this embodiment. FIG. [Figure 4] 1 is an explanatory diagram showing an outline of an example of a parison molding device for carrying out a method for manufacturing a synthetic resin container according to the present invention. FIG. [Diagram 5] FIG. 11 is an explanatory diagram showing an outline of a synthetic resin container according to another example of the present embodiment. [Figure 6] FIG. 11 is an enlarged cross-sectional view of a main portion of a synthetic resin container according to yet another example of the present embodiment. [Figure 7] 10 is an enlarged cross-sectional view of a main portion of a parison for blow molding a synthetic resin container according to yet another example of the present embodiment. FIG. [Figure 8] 1 is an explanatory diagram showing an outline of another example of a parison molding device for carrying out the method for manufacturing a synthetic resin container according to the present invention. FIG. [Figure 9] 1 is an explanatory diagram showing an outline of yet another example of a parison molding device for carrying out the method for manufacturing a synthetic resin container according to the present invention. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] Hereinafter, preferred embodiments of the present invention will be described with reference to the drawings.
[0013] [First embodiment] A first embodiment of the present invention will be described. FIG. 1 is an explanatory diagram showing an outline of a synthetic resin container 1 according to this embodiment. The container 1 of this embodiment is a so-called recycled bottle made of recycled resin material obtained from collected synthetic resin containers.
[0014] Container 1 shown in Fig. 1 includes a mouth 2 which serves as an inlet / outlet for pouring the contents, and a storage section 3 in which the contents are stored. Storage section 3 has a body 4 whose upper end in the height direction tapers in diameter toward mouth 2 and connects to the lower end of mouth 2, and a bottom 5 which closes the lower end side in the height direction of body 4. In the example shown in the figure, container 1 is formed to have a generally cylindrical container shape, but the shape of container 1 is not limited thereto.
[0015] Here, the height direction refers to the direction perpendicular to the horizontal plane when container 1 is placed upright on the horizontal plane with mouth 2 facing up, and the up-down, left-right and length-width directions of container 1 are defined as shown in Figure 1 when container 1 is placed upright with mouth 2 facing up.
[0016] In the illustrated example, the outer circumferential surface of the cylindrical mouth portion 2 is provided with threads 21 for screwing in the lid 6 (not shown in Fig. 1), but the means for attaching the lid 6 is not limited to this. An engaging protrusion may be provided instead of the threads 21 so that the lid 6 can be attached by tapping.
[0017] Fig. 2 is an enlarged cross-sectional view of a main portion of the container 1, showing the mouth 2 of the container 1 together with a part of the lid 6 for sealing the container 1. Note that the thicknesses of the members shown in the cross sections of Fig. 2 and the following drawings are exaggerated and depicted diagrammatically. In this embodiment, the mouth 2 of the container 1 is configured to be sealed when the lid body 6 is attached by close contact between the inner surface 22 of the mouth 2 and the sealing surface 62 of the sealing inner ring 61 provided on the lid body 6.
[0018] Here, when using recycled resin material obtained from collected synthetic resin containers as the molding material for the container 1, there is a problem that the sealing property is reduced. That is, the recycled resin material obtained by cleaning and pelletizing a wide variety of collected products may have deteriorated physical properties or may contain a large amount of foreign matter remaining in the recycled raw material. Foreign matter mixed into the recycled resin material may include deteriorated resin, burnt resin, metal, sand, pigment, filler, etc. It has been confirmed that the largest of these foreign matter has a major diameter of about 0.5 mm. As a result, when the mouth part 2 of the container 1 is composed of a layer 1a made of recycled resin formed from recycled resin material, there is a risk that the adhesion between the seal surface 62 of the inner ring 61 of the lid body 6 and the inner peripheral surface 22 of the mouth part 2 may be insufficient. Furthermore, if foreign matter contained in the layer 1a made of recycled resin is exposed to the inner surface 22, i.e., the surface, of the mouth 2, not only will the adhesion be poor when the lid body 6 is fitted to the mouth 2, but the sealing surface 62 of the inner ring 61 with which the foreign matter comes into contact will be scratched, which may lead to constant leakage of the contents of the container 1.
[0019] Therefore, in the container 1 according to this embodiment, a layer 1b made of a reinforcing resin formed from a reinforcing resin material is provided on the inner peripheral surface 22 side of the mouth portion 2 of the container 1. The presence of not only the layer 1a made of recycled resin but also the layer 1b made of reinforcing resin in the mouth portion 2 can reduce the deterioration of physical properties caused by using recycled resin materials in that portion. In addition, since the layer 1a made of recycled resin does not directly contact the inner ring 61 of the lid body 6, the seal surface 62 of the inner ring 61 of the lid body 6 and the inner circumferential surface 22 of the mouth portion 2 can be sufficiently kept in close contact. In addition, the seal surface 62 of the inner ring 61 of the lid body 6 can be prevented from being scratched by foreign matter contained in the layer 1a made of recycled resin. Furthermore, by providing layer 1b made of reinforcing resin only in a part of mouth portion 2, it is possible to avoid a decrease in the proportion of recycled resin material used, compared to when layer 1b made of reinforcing resin is provided over the entire or most part of the container 1.
[0020] The recycled resin material is obtained by cleaning and pelletizing collected synthetic resin containers to turn them into raw materials, and is not particularly limited as long as it is a thermoplastic resin that can be extruded. Examples of such thermoplastic resins include olefin-based resins such as low-density polyethylene, high-density polyethylene, polypropylene, poly1-butene, poly4-methyl-1-pentene, random or block copolymers of α-olefins such as ethylene, propylene, 1-butene, and 4-methyl-1-pentene, and cyclic olefin copolymers; ethylene-vinyl copolymers such as ethylene-vinyl acetate copolymer, ethylene-vinyl alcohol copolymer, and ethylene-vinyl chloride copolymer; and styrene-based resins such as polystyrene, acrylonitrile-styrene copolymer, ABS, and α-methylstyrene-styrene copolymer. Examples include vinyl resins such as polyvinyl chloride, polyvinylidene chloride, vinyl chloride-vinylidene chloride copolymers, polymethyl acrylate, and polymethyl methacrylate; polyamide resins such as nylon 6, nylon 6-6, nylon 6-10, nylon 11, and nylon 12; polyester resins such as polyethylene terephthalate (PET), polybutylene terephthalate, polyethylene naphthalate, and copolymer polyesters thereof; polycarbonate resins; polyphenylene oxide resins; and biodegradable resins such as polylactic acid. All of these have extrusion grade melt flow rates. In general, olefin resins and polyester resins that are widely used in the packaging field are preferably used, and olefin resins obtained mainly by mechanical recycling as recycled resin materials are most preferably used.
[0021] The reinforcing resin material is preferably a resin material (virgin material) that is the above-mentioned thermoplastic resin and has not been subjected to a recycling process. From the viewpoint of container molding, the layer 1a made of recycled resin and the layer 1b made of reinforcing resin of the container 1 are preferably formed of the same type of resin, but are not necessarily limited to the same type of resin as long as blow molding is possible. Other resin materials having specific physical properties may also be used.
[0022] Such a synthetic resin container 1 can be manufactured by so-called direct blow molding, in which a parison 10 extruded into a cylindrical shape from an extruder through a die head 110 is sandwiched between a pair of split dies and blown into the parison 10 to blow it into a desired container shape. The parison 10 according to this embodiment is configured to include a layer 10a made of recycled resin formed from a recycled resin material, and to partially include a layer 10b made of reinforcing resin formed from a reinforcing resin material in a predetermined region on the inner periphery of the parison 10. 3 is an enlarged cross-sectional view of a main portion of a parison 10 suitable for blow molding the container 1 according to this embodiment, and shows a schematic cross-section of the parison 10 near a region including a layer 10b made of a reinforcing resin. In FIG. 3, the right side corresponds to the inner periphery of the parison 10. The thicknesses of the members shown in the cross-section of FIG. 3 are exaggerated and shown schematic. In this embodiment, the layer 10b (FIG. 3) made of reinforcing resin of the parison 10 becomes the layer 1b (FIG. 2) made of reinforcing resin of the container 1 by blow molding.
[0023] When the container 1 is formed by direct blow molding, the parison 10 partially provided with the layer 10b made of a reinforcing resin on its inner periphery side can be formed as follows.
[0024] FIG. 4 is an explanatory diagram showing an outline of a parison molding apparatus 100 for molding a parison 10 for blow molding the container 1 according to the first embodiment. The illustrated parison molding apparatus 100 is equipped with a die head 110 having a die head outlet 111 for recycled resin from which recycled resin material is extruded in an annular shape, and a die head outlet 112 for reinforced resin from which reinforcing resin material is extruded in an annular shape. In this embodiment, the reinforcing resin die head outlet 112 is positioned so that the reinforcing resin material discharged therefrom is discharged on the inner peripheral side of the resin material discharged from the recycled resin die head outlet 111.
[0025] In this embodiment, such a parison molding apparatus 100 is used to extrude recycled resin material from the die head outlet 111 for recycled resin using an extruder not shown in the figure to form a parison 10 including a layer 10a made of recycled resin, and a predetermined amount of reinforcing resin material is extruded from the die head outlet 112 for reinforcing resin in a desired area, and then the extrusion of the reinforcing resin material is stopped to form a parison 10 including a layer 10b made of reinforcing resin in some areas. The discharge of the recycled resin material from the die head outlet 111 for recycled resin can be constant regardless of the discharge of the reinforcing resin material from the die head outlet 112 for reinforcing resin. Alternatively, the discharge amount of the recycled resin material from the die head outlet 111 for recycled resin may be controlled to increase or decrease depending on the discharge of the reinforcing resin material from the die head outlet 112 for reinforcing resin. For example, the discharge of the recycled resin material from the die head outlet 111 for recycled resin may be reduced while a predetermined amount of reinforcing resin material is discharged from the die head outlet 112 for reinforcing resin, and then the discharge of the reinforcing resin material may be stopped while the discharge of the recycled resin material is increased to form a parison 10 including a layer 10b made of reinforcing resin in a partial region.
[0026] When the discharge of the reinforcing resin material is stopped, it is preferable to perform suck-back control. That is, when the reinforcing resin material is discharged from the reinforcing resin die head discharge port 112 by the reinforcing resin extruder 122 to be merged with the recycled resin material, the resin pressure in the supply path of the reinforcing resin material supplied from the reinforcing resin extruder 122 to the reinforcing resin die head discharge port 112, i.e., the communication path 140, is adjusted at any timing to perform suck-back control to pull back the reinforcing resin material from the reinforcing resin die head discharge port 112. By controlling the suck-back when the discharge of the reinforcing resin material is stopped, the partial discharge of the reinforcing resin material can be appropriately controlled, and excessive discharge of the reinforcing resin material can be prevented. As a result, the thickness and the formation area of the layer 10b made of the reinforcing resin can be easily adjusted.
[0027] Such partial discharge and suck-back control of the resin material can be performed, for example, by a gear pump 130 capable of irregular forward and reverse rotation as shown in Fig. 4. The extruder 122 that supplies the reinforcing resin material is connected to the gear pump 130, and the reinforcing resin material is supplied to the reinforcing resin die head discharge port 112 of the die head through a communication passage 140 by the forward rotation of the gear pump 130. Also, suck-back control is possible by reversing the rotation of the gear pump 130. More specifically, the gear pump 130 includes a gear case 131 and two gears 132a and 133a. The gears 132a and 133a rotate while meshing in the direction indicated by the arrows in the figure. When the two gears 132a and 133a disengage from each other in the inflow section 134, the reinforcing resin material supplied from the extruder 122 enters the tooth grooves 132b and 133b. The reinforcing resin material that has entered the tooth grooves 132b and 133b is held between the gear case 131 and the tooth grooves 132b and 133b, and is transported to the outflow section 135 by the rotation of the gears 132a and 133a in the direction of their rotation, i.e., the direction indicated by the arrows in the figure. When the teeth of the gears 132a, 133a mesh again in the outflow section 135, the reinforcing resin material in the tooth grooves 132b, 133b is extruded and sequentially supplied to the outflow section 135. By using such a gear pump 130, it is possible to supply a predetermined amount of reinforcing resin material while controlling the flow rate of the reinforcing resin material supplied to the die head 110 by appropriately adjusting the extrusion amount of the reinforcing resin material from the extruder 122 and the rotation speed of the gears 132a, 133a. Then, by rotating the gears 132a, 133a of such a gear pump 130 in the reverse direction (rotating them in the opposite direction to the direction indicated by the arrow in the figure), suck-back control can be performed.
[0028] Furthermore, in cases where the communication passage 140 for supplying the reinforcing resin material to the die head 110 is long, even if the gear pump 130 is made to function as a suck-back mechanism, it may take some time to pull back the reinforcing resin material from the reinforcing resin die head discharge port 112, making it difficult to instantly obtain the effect of suck-back control. In such cases, a second suck-back mechanism 150 may be provided at a position closer to the die head 110, as shown in FIG. There are no limitations on the specific configuration of this second suck back mechanism 150, so long as it can suck the reinforcing resin material in the communicating passage 140 and adjust the resin pressure in the communicating passage 140. For example, as shown in the figure, it may be configured to suck the reinforcing resin material in the communicating passage 140 by operating a piston 150b in the direction of the arrow in the figure using a cylinder 150a. The closer the second suck-back mechanism 150 is provided to the reinforcing resin die head outlet 112, the more sensitive the suck-back control becomes. However, this increases the rate of decrease in the resin pressure in the communication passage 140, which may result in more reinforcing resin material being pulled back than necessary from the reinforcing resin die head outlet 112. In such a case, the thickness of the reinforcing resin material may decrease. For this reason, in this embodiment, the suck back control may be performed by using both the gear pump 130 and the second suck back mechanism 150. By combining the insensitive suck back control by the gear pump 130 and the sensitive suck back control by the second suck back mechanism 150, minute adjustments of the discharge of the reinforcing resin material from the reinforcing resin die head discharge port 112 can be made more easily.
[0029] The parison 10 thus formed is sandwiched between a pair of split dies, the leading end side of the parison 10 in the extrusion direction is pinched off and fused, and then blow air is blown into the parison 10 to perform blow molding, thereby manufacturing the container 1. In this embodiment, the parison 10 is sandwiched between the split dies and blow molded so that the inner circumferential surface 22 of the mouth portion 2 of the container 1 is formed in a portion of the parison 10 corresponding to the layer 10b made of reinforcing resin.
[0030] Also, a step of making the inner peripheral surface 22 of the mouth part 2 of the container 1 into a smooth surface by cutting using a rotary blade or the like may be carried out. For example, when the mouth part 2 of the container 1 is formed by extrusion molding such as rotary blow molding, and the inner peripheral surface 22 of the mouth part 2 is not in contact with the mold surface of the molding die, the inner peripheral surface 22 of the mouth part 2 may lack smoothness. In such a case, by cutting the inner peripheral surface 22 of the mouth part 2 to increase the smoothness, the adhesion between the seal surface 62 of the inner ring 61 of the lid body 6 and the inner peripheral surface 22 of the mouth part 2 of the container 1 can be improved, and good sealing can be ensured. Even when the inner surface 22 of the mouth portion 2 is cut in this manner, according to the manufacturing method of this embodiment, the extrusion of the reinforcing resin material is controlled as described above, so that the layer 1b made of reinforcing resin provided on the inner surface 22 side of the mouth portion 2 is formed partially in a specified area with its thickness adjusted, and it is possible to appropriately prevent the layer 1b made of reinforcing resin from being scraped off by the cutting process, thereby exposing the layer 1a made of recycled resin to the surface.
[0031] [Second embodiment] Next, a second embodiment of the present invention will be described. FIG. 5 is an explanatory diagram showing the outline of a synthetic resin container 1 according to this embodiment, with a left portion of the container 1 cut away to show its cross section. In the container 1 according to the first embodiment described above, the layer 1b made of a reinforcing resin is provided on the inner circumferential surface 22 of the mouth portion 2. In contrast, the container 1 according to the present embodiment is configured to partially include the layer 1b made of a reinforcing resin not only on the inner circumferential surface 22 of the mouth portion 2 but also on the outer circumferential surface of the storage portion 3 of the container 1.
[0032] According to such a container 1, the layer 1b made of reinforcing resin is provided in at least a partial region of the storage section 3 of the container 1, thereby improving the physical properties such as impact resistance of the part. In the illustrated example, the layer 1b made of reinforcing resin is provided in the lower part of the body 4, but the position where the layer 1b made of reinforcing resin is provided is not limited to the illustrated example. For example, the layer 1b may be provided in the grounding part or pinch-off part of the bottom 5 of the container 1. Furthermore, with such a container 1, it is possible to avoid a decrease in the proportion of recycled resin material used, compared to when the entire or most of the area of the container 1 is provided with a layer 1b made of a reinforcing resin.
[0033] The reinforcing resin material forming the layer 1b made of reinforcing resin provided on the outer peripheral surface of the storage portion 3 of the container 1 may be the same as or different from the reinforcing resin material forming the layer 1b made of reinforcing resin provided on the inner peripheral surface 22 of the mouth portion 2. A recycled resin material adjusted to have specific physical properties may be used.
[0034] The container 1 in the second embodiment can be manufactured by forming a parison 10 having a layer 10a made of recycled resin, a layer 10b made of reinforcing resin in a specified region on the inner side, and a layer 10b made of reinforcing resin in a specified region on the outer side, sandwiching the formed parison 10 between a pair of split molds, and blowing air into the parison 10 to blow mold it into the desired container shape. The parison 10 for manufacturing the container 1 according to the second embodiment can be manufactured by the parison molding apparatus 100 described in the first embodiment, which further includes a third die head outlet 113 from which the reinforcing resin material is extruded in an annular shape in addition to the die head outlet 111 for recycled resin and the die head outlet 112 for reinforcing resin. The third die head outlet 113 is arranged so that the reinforcing resin material discharged therefrom is discharged on the outer periphery of the recycled resin material discharged from the die head outlet 111 for recycled resin. The discharge of the reinforcing resin material from the third die head outlet 113 can be controlled in the same manner as the discharge of the reinforcing resin material from the die head outlet 112 for reinforcing resin. Using a parison molding apparatus 100 further equipped with a die head discharge port 113, a parison 10 can be formed in the same manner as the manufacturing method of the first embodiment, except that a layer 10b made of reinforcing resin is further partially provided on the outer circumferential side of the parison 10. The manufacturing method of this embodiment differs from that of the first embodiment in the above points, but other configurations are similar to those of the first embodiment, so duplicated explanations will be omitted.
[0035] [Third embodiment] Next, a third embodiment of the present invention will be described. Fig. 6 is an enlarged cross-sectional view of a main part of the container 1 according to this embodiment, showing the mouth 2 of the container 1 together with a part of the lid 6 for sealing the container 1. Fig. 7 is an enlarged cross-sectional view of a main part of a parison 10 suitable for blow molding the container 1 according to this embodiment, showing a schematic cross-section of the parison 10 near a region including a layer 10b made of a reinforcing resin. In Fig. 7, the right side is the inner peripheral side of the parison 10. Note that the thicknesses of the members shown in the cross-sections of Figs. 6 and 7 are exaggerated and depicted schematic.
[0036] In the container 1 according to the first embodiment described above, the layer 10b made of reinforcing resin is partially formed on the inner periphery side of the parison 10, the parison 10 is sandwiched between split dies and blow molded so that the mouth portion 2 is formed at a portion corresponding to the layer 10b made of reinforcing resin, and the inner periphery surface 22 of the mouth portion 2 is formed from the reinforcing resin. In contrast, the container 1 according to the present embodiment is configured such that the layer 10b made of reinforcing resin is partially formed on the outer periphery side of the parison 10, the parison 10 is sandwiched between split dies and blow molded so that the mouth portion 2 is formed at a portion corresponding to the layer 10b made of reinforcing resin, and then the inner periphery surface 22 side of the mouth portion 2 is cut to expose at least a portion of the layer 1b made of reinforcing resin to the inner periphery surface 22 of the mouth portion 2, and at least a portion of the inner periphery surface 22 of the mouth portion 2 is formed from the reinforcing resin.
[0037] In this way, as in the first embodiment, not only the layer 1a made of recycled resin but also the layer 1b made of reinforcing resin is present in a part of the mouth part 2, and the deterioration of physical properties due to the use of recycled resin material in this part can be reduced. In addition, at least a part of the layer 1b made of reinforcing resin is exposed to the inner peripheral surface 22 of the mouth part 2, so that the adhesion between the seal surface 62 of the inner ring 61 of the lid body 6 and the inner peripheral surface 22 of the mouth part 2 can be sufficiently maintained. In addition, since the area where the layer 1a made of recycled resin directly contacts the inner ring 61 of the lid body 6 is at least reduced, it is possible to reduce the damage to the seal surface 62 of the inner ring 61 of the lid body 6 caused by foreign matter contained in the layer 1a made of recycled resin. Furthermore, by partially providing layer 1b made of reinforcing resin at mouth portion 2, it is possible to avoid a decrease in the proportion of recycled resin material used, compared to when layer 1b made of reinforcing resin is provided over the entire or most part of the container 1.
[0038] The method for producing the container 1 according to the third embodiment will be described in detail below.
[0039] FIG. 8 is an explanatory diagram showing an outline of a parison molding apparatus 200 for molding a parison 10 for blow molding a container 1 according to the third embodiment. The illustrated parison molding apparatus 200 includes a die head 210 having a die head outlet 211 for recycled resin from which recycled resin material is extruded in an annular shape, and a die head outlet 212 for reinforced resin from which reinforcing resin material is extruded in an annular shape. In this embodiment, the die head outlet 212 for reinforced resin is disposed so that the reinforcing resin material extruded therefrom is discharged on the outer periphery of the resin material extruded from the die head outlet 211 for recycled resin.
[0040] In this embodiment, such a parison molding apparatus 200 is used to extrude recycled resin material from the die head outlet 211 for recycled resin using an extruder not shown in the figure to form a parison 10 including a layer 10a made of recycled resin, and a predetermined amount of reinforcing resin material is extruded from the die head outlet 212 for reinforcing resin in a desired area, and then the extrusion of the reinforcing resin material is stopped to form a parison 10 including a layer 10b made of reinforcing resin in some areas.
[0041] The parison 10 thus formed is sandwiched between split dies and blow molded so that the mouth portion 2 is formed at a location corresponding to the layer 10b made of reinforcing resin, and is molded into a container 1 having the layer 1b made of reinforcing resin on the outer peripheral surface side of the mouth portion 2. In this embodiment, the layer 1a made of recycled resin on the inner peripheral surface 22 side of the mouth portion 2 is then cut to expose at least a part of the layer 1b made of reinforcing resin on the inner peripheral surface 22 of the mouth portion 2. In this way, the container 1 is manufactured in which at least a part of the inner peripheral surface 22 of the mouth portion 2 is formed of the reinforcing resin. To cut the inner circumferential surface 22 side of the mouth portion 2 to expose the reinforcing resin at the inner circumferential surface 22 of the mouth portion, cutting using a rotary blade or the like can be performed as described in the first embodiment.
[0042] Using a parison molding device 200 arranged so that the resin material extruded from the die head outlet 212 for reinforcing resin is extruded more outer than the resin material extruded from the die head outlet 211 for recycled resin, a layer 10b made of reinforcing resin is partially provided on the outer periphery of the parison 10, and the container 1 can be manufactured in the same manner as the manufacturing method of the first embodiment, except that the inner periphery 22 side of the mouth portion 2 is cut after the parison 10 is blow molded. The manufacturing method of this embodiment differs from that of the first embodiment in the above points, but other configurations are similar to those of the first embodiment, so duplicated explanations will be omitted.
[0043] According to the manufacturing method of this embodiment, even when the inner surface 22 of the mouth portion 2 is cut, the extrusion of the reinforcing resin material can be controlled as described in the first embodiment, so that the layer 1b made of reinforcing resin provided at the mouth portion 2 is formed in a specified area with its thickness adjusted partially, and it is possible to appropriately prevent a situation in which part of the layer 1a made of recycled resin is scraped off by the cutting process, making it impossible to maintain the thickness of the mouth portion 2.
[0044] According to the present invention, when a new synthetic resin container 1 is manufactured using recycled resin material obtained from collected synthetic resin containers, a layer 1b made of reinforcing resin formed by a reinforcing resin material is partially provided in the region, so that the deterioration of physical properties due to the use of the recycled resin material can be reduced in the region. In particular, by providing such a layer 1b made of reinforcing resin in the mouth portion 2 and forming at least a part of the inner peripheral surface 22 of the mouth portion 2 with the reinforcing resin, it is possible to increase the adhesion with the sealing surface 62 of the inner ring 61 of the lid body 6 without excessively reducing the proportion of recycled resin material used, and to increase the sealing ability of the container 1. In addition, by further providing a layer 1b made of reinforcing resin in a part of the outer peripheral surface of the container 1, it is possible to improve the physical properties such as impact resistance of the part without excessively reducing the proportion of recycled resin material used.
[0045] Although the present invention has been described above by showing preferred embodiments, it goes without saying that the present invention is not limited to the above-described embodiments, and various modifications can be made within the scope of the present invention.
[0046] For example, in the first embodiment described above, a manufacturing method for manufacturing a container 1 having a layer 1b made of a reinforcing resin on the inner surface 22 of the mouth portion 2 was exemplified, but it is also possible for layer 1b made of a reinforcing resin to be further provided on other regions of the inner surface of the container 1, such as the inner surface of the storage portion 3. To form a layer 10b made of reinforcing resin partially in two or more places on the inner side of the parison 10, when forming the parison 10, reinforcing resin material is ejected multiple times from the die head outlet 112 for reinforcing resin provided in the die head 110 to form a parison having a layer 10b made of reinforcing resin in a predetermined area, and the formed parison is sandwiched in a mold and blow molded to produce a container 1 having a layer 1b made of reinforcing resin in a predetermined area. With such a container, by further providing a layer 1b made of reinforcing resin on a portion of the inner surface of the container 1, it is possible to improve the physical properties such as impact resistance of that portion without excessively reducing the proportion of recycled resin material used.
[0047] In addition, in the third embodiment, a manufacturing method for manufacturing a container 1 having a layer 1b made of a reinforcing resin in a part of the mouth portion 2 has been exemplified, but the layer 1b made of a reinforcing resin can also be further provided in other regions of the outer surface of the container 1, for example, the outer surface of the storage portion 3. To form a layer 10b made of reinforcing resin partially in two or more places on the outer periphery of the parison 10, when forming the parison 10, reinforcing resin material is ejected multiple times from the die head outlet 212 for reinforcing resin provided in the die head 210 to form a parison having a layer 10b made of reinforcing resin in a predetermined area, and the formed parison is sandwiched in a mold and blow molded to produce a container 1 having a layer 1b made of reinforcing resin in a predetermined area. With such a container, by further providing a layer 1b made of a reinforcing resin on a portion of the outer peripheral surface of the container 1, it is possible to improve the physical properties such as impact resistance of that portion without excessively reducing the proportion of recycled resin material used.
[0048] In the third embodiment described above, a layer 10b made of reinforcing resin formed from the reinforcing resin material discharged from the third die head discharge port 113 may be further provided on the outer periphery of the parison 10 by using the parison molding device 200 further provided with the third die head discharge port 113 as described in the second embodiment. In this case, the resin material discharged from the reinforcing resin die head discharge port 212 and the resin material discharged from the third die head discharge port 113 may be different. A recycled resin material adjusted to have specific physical properties may be used.
[0049] The parison 10 for manufacturing the container 1 according to the third embodiment can also be manufactured by the parison molding device 100 equipped with the third die head outlet 113 described in the second embodiment. In this case, when the recycled resin material is discharged from the die head outlet 111 for recycled resin to form the parison 10 including the layer 1a made of recycled resin, a predetermined amount of reinforcing resin material is discharged from the third die head outlet 113 in a desired area, and then the discharge of the reinforcing resin material is stopped, thereby forming the parison 10 for manufacturing the container 1 according to the third embodiment. In this case, it is preferable that the third die head outlet 113 stops discharging the reinforcing resin material by suck-back control. The container 1 can also be formed such that the layer 1b made of reinforcing resin is partially provided on the inner peripheral surface of the container 1 by discharging the reinforcing resin material from the die head outlet 112 provided in the parison molding device 100 so as to be discharged on the inner peripheral side of the resin material discharged from the die head outlet 111 for recycled resin.
[0050] In addition, in the above-described first embodiment, a configuration is exemplified in which, when forming the parison 10, the resin material is partially discharged by the gear pump 130 and suck-back control is performed when the discharge is stopped, but the partial discharge of the resin material and the suck-back control are not limited to this form. For example, a configuration may be adopted in which partial discharge and suck-back control of the resin material is performed by an accumulator. Specific embodiments of this configuration will be described below.
[0051] FIG. 9 is an explanatory diagram showing an outline of yet another example of the parison molding apparatus 100 for carrying out the method for manufacturing the synthetic resin container 1 according to the present invention. In this embodiment, the extruder 122 that supplies the reinforcing resin material is connected to a switching unit 161, and can intermittently extrude a predetermined amount of molten reinforcing resin material. The switching unit 161 constitutes a part of the storage unit 160, and switches between storing and supplying the reinforcing resin material by a switching valve 165. The reinforcing resin material extruded from the extruder 122 is temporarily stored in the storage unit 160 that includes two accumulators 162 and 163. The switching valve 165 of the switching unit 161 alternately connects and disconnects between the extruder 122 and the accumulators 162 and 163, and between the accumulators 162 and 163 and the communication passage 140. The communication passage 140 connects the storage section 160 and the die head 110, and the reinforcing resin material stored in the storage section 160 is supplied to the die head outlet 112 for reinforcing resin of the die head through the communication passage 140. At this time, the reinforcing resin material is supplied intermittently from two accumulators 162, 163 alternately. Specifically, the reinforcing resin material melt-extruded from the extruder 122 is filled into one of the accumulators 162 through a switching valve 165. Then, when discharging the reinforcing resin material, the switching valve 165 is switched and the accumulator 162 is operated, and the reinforcing resin material filled in the accumulator 162 is supplied to the die head outlet 112 for reinforcing resin of the die head through the communication passage 140. At this time, the switching valve 165 connects one accumulator 162 to the communication passage 140, and simultaneously connects the other accumulator 163 to the extruder 122 (the state shown in FIG. 9). As a result, the reinforcing resin material extruded from the extruder 122 is filled into the accumulator 163. In this manner, the reinforcing resin material is stored alternately in the two accumulators 162, 163 from the extruder 122, and a predetermined amount of reinforcing resin material is alternately supplied from the accumulators 162, 163 to the die head outlet 112 for reinforcing resin of the die head.
[0052] Here, the switching operation of the switching valve 165 is performed by a cylinder (not shown), and the operations of the two accumulators 162, 163 are performed by the respective cylinders 162a, 163a, etc. At this time, by adjusting the operating speed of the accumulators 162, 163, it is possible to adjust the supply speed of the reinforcing resin material, that is, the amount of the reinforcing resin material added to the parison 10. This makes it possible to change the thickness of the layer 10b made of reinforcing resin.
[0053] When performing the suck-back control, after the reinforcing resin material is supplied from the accumulators 162, 163, the cylinders 162a, 163a are operated in reverse to pull back the reinforcing resin material in the communication passage 140 into the accumulators 162, 163, thereby making the accumulators 162, 163 function as a suck-back mechanism. Specifically, after the reinforcing resin material is supplied from the accumulator 162, the piston 162b is operated in the direction of the arrow in the figure to pull back the reinforcing resin material into the accumulators 162, 163. Also, as described in the first embodiment, the second suck back control may be provided at a position closer to the die head. The suck back control may be used by using the accumulators 162 and 163 and the second suck back mechanism 150 in combination. [Explanation of symbols]
[0054] 1 container 1a Layer made of recycled resin 1b Layer made of reinforcing resin 2 Mouth 22 Inner surface of mouth 10 Parison 10a Layer made of recycled resin 10b Layer made of reinforcing resin
Claims
1. A parison extruded from an extruder through a die head is sandwiched between a pair of split dies, and blown air is blown into the parison to blow mold it into a predetermined container shape having a mouth portion and a container portion, A recycled resin material obtained from collected synthetic resin containers is discharged from a die head outlet for recycled resin provided in the die head to form a parison; In a predetermined region, a reinforcing resin material is discharged from a die head outlet for reinforcing resin provided in the die head so as to be discharged on the inner peripheral side of the resin material discharged from the die head outlet for recycled resin, thereby partially forming a layer made of reinforcing resin on the inner peripheral side of the parison; A method for manufacturing a synthetic resin container, characterized in that the parison is sandwiched between the split molds and blow molded so that the mouth portion is formed in a portion corresponding to the layer made of the reinforcing resin, and the inner surface of the mouth portion is formed by the reinforcing resin.
2. A parison extruded from an extruder through a die head is sandwiched between a pair of split dies, and blown air is blown into the parison to blow mold it into a predetermined container shape having a mouth portion and a container portion, A recycled resin material obtained from collected synthetic resin containers is discharged from a die head outlet for recycled resin provided in the die head to form a parison; In a predetermined region, a reinforcing resin material is discharged from a die head outlet for reinforcing resin provided in the die head so as to be discharged on the outer peripheral side of the resin material discharged from the die head outlet for recycled resin, thereby partially forming a layer made of reinforcing resin on the outer peripheral side of the parison; A method for manufacturing a synthetic resin container, comprising: sandwiching the parison between the split molds and blow molding the parison so that the mouth is formed in a portion corresponding to the layer of reinforcing resin; cutting the inner surface side of the mouth to expose at least a portion of the layer of reinforcing resin on the inner surface of the mouth; and forming at least a portion of the inner surface of the mouth from the reinforcing resin.
3. 3. The method for producing a synthetic resin container according to claim 1, wherein the reinforcing resin material is a virgin material that has not been subjected to a recycling process.
4. The method for producing a synthetic resin container according to claim 1 or 2, wherein the reinforcing resin material is discharged under suck-back control.
5. 3. The method for producing a synthetic resin container according to claim 1, wherein the reinforcing resin material is also extruded from a third die head outlet provided within the die head and arranged so as to be extruded on the outer periphery of the recycled resin material extruded from the die head outlet for recycled resin, thereby partially forming a layer of reinforcing resin on the outer periphery of the parison.
6. 3. The method for manufacturing a synthetic resin container according to claim 1, wherein the reinforcing resin material is ejected multiple times from the die head ejection port for the reinforcing resin provided in the die head to partially form a layer of reinforcing resin in two or more places on the parison.
7. A synthetic resin container made of recycled resin material obtained from collected synthetic resin containers, The container includes an opening for injecting and dispensing the contents, and a storage section. the mouth portion is configured to be sealed by a seal surface of an inner ring provided on the lid body being brought into close contact with an inner peripheral surface of the mouth portion when the lid body is attached, A synthetic resin container, characterized in that the mouth portion is provided with a layer made of a reinforcing resin.
8. 8. The synthetic resin container according to claim 7, wherein at least a part of the inner circumferential surface of the mouth portion is formed from a reinforcing resin.
9. 9. The synthetic resin container according to claim 7, wherein the layer made of the reinforcing resin is formed from a virgin material that has not been subjected to a recycling process.
10. 9. The synthetic resin container according to claim 7, wherein a layer made of a reinforcing resin is partially provided on an outer peripheral surface of the container portion.
11. 9. The synthetic resin container according to claim 7, wherein a layer made of a reinforcing resin is partially provided on an inner peripheral surface of the container portion.
Citation Information
Patent Citations
Method for recovery and pelletizing of discarded resin packaging container and apparatus therefor