Substrate

The substrate with alignment marks formed on the substrate itself, using recessed portions and lower transmittance bottom portions, addresses the complexity of existing methods by enabling efficient infrared recognition and alignment without additional patterning steps.

JP2024149729AActive Publication Date: 2024-10-18CANON KK
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2024133380
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-07-12
Filing Date
2024-08-08
Publication Date
2024-10-18
Estimated Expiration
2042-06-10

AI Technical Summary

Technical Problem

Existing methods for forming alignment marks on substrates require additional patterning steps and increase the number of manufacturing steps, and using metal alignment marks on substrates that transmit infrared rays complicates recognition with infrared cameras.

Method used

A substrate with alignment marks that are formed on the substrate itself, utilizing a recessed portion and a bottom portion with lower infrared transmittance than the substrate surfaces, allowing recognition via transmitted infrared light without penetrating the substrate.

Benefits of technology

Enables efficient formation of alignment marks on substrates that can be recognized using infrared cameras, reducing the number of manufacturing steps and ensuring accurate alignment without additional patterning.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024149729000001_ABST
    Figure 2024149729000001_ABST
Patent Text Reader

Abstract

To provide a method for producing a substrate formed with an alignment mark on the substrate itself.SOLUTION: A substrate including an alignment mark has formed therein: an alignment mark that does not penetrate the substrate and has a bottom part having an infrared transmittance lower than those of a first surface and a second surface when arranging predetermined places of the first surface and the second surface of the substrate, and an infrared camera orthogonally; and a concavity.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a substrate. [Background technology]

[0002] Technology for aligning a substrate based on an alignment mark formed on the substrate is used in many fields. In Patent Document 1, a metal that does not transmit infrared rays is used as the material for the alignment mark. This makes it possible to form an alignment mark of a metal layer on a silicon substrate, and the alignment mark can be recognized by transmitted infrared light, allowing the substrate to be aligned. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2019-64272 A Summary of the Invention [Problem to be solved by the invention]

[0004] However, the method of Patent Document 1 requires a process of forming a metal layer on a substrate and then patterning the metal layer into the shape of an alignment mark, and forming all alignment marks from metal increases the number of steps.

[0005] SUMMARY OF THE PRESENT DISCLOSURE In view of the above, an object of the present invention is to provide a method for manufacturing a substrate in which an alignment mark is formed on the substrate itself. [Means for solving the problem]

[0006] A substrate according to one embodiment of the present invention is a substrate having an alignment mark, and is characterized in that when predetermined positions on a first surface and a second surface of the substrate are arranged perpendicular to an infrared camera, the substrate has a bottom having a lower infrared transmittance than the first surface and the second surface, and a non-penetrating alignment mark and a recess are formed in the substrate. Effect of the Invention

[0007] According to the present invention, it is possible to provide a method for manufacturing a substrate in which an alignment mark is formed on the substrate itself. [Brief description of the drawings]

[0008] [Figure 1] 1 is a schematic cross-sectional view of a substrate having an alignment mark. [Diagram 2] FIG. 2 is a schematic cross-sectional view during alignment. [Diagram 3] FIG. 2 is a schematic plan view of a substrate. [Figure 4] FIG. 2 is a schematic plan view of a substrate. [Diagram 5] FIG. 2 is a schematic cross-sectional view of a substrate. [Figure 6] FIG. 2 is a schematic cross-sectional view of a substrate. [Figure 7] FIG. 2 is a schematic plan view of a substrate. [Figure 8] 5A to 5C are schematic cross-sectional views showing a method for manufacturing a substrate. [Figure 9] 5A to 5C are schematic cross-sectional views showing a method for manufacturing a substrate. [Figure 10] 1 is a plan view of an example of an alignment mark; [Figure 11] 1 is a plan view of an example of an alignment mark; [Figure 12] 1 is a plan view of an example of an alignment mark; [Figure 13] 1A and 1B are examples of a plan view and a cross-sectional view of an alignment mark. [Figure 14] 1 is a plan view of an example of an alignment mark; DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0009] Hereinafter, some embodiments of the present invention will be described with reference to the drawings. However, the following description does not limit the scope of the present invention.

[0010] The substrate having the alignment mark described in this embodiment is assumed to be applied to a liquid ejection head using a thermal method, a piezoelectric method, or any other liquid ejection method, but is not limited to this. For example, the substrate having the alignment mark of this embodiment can be applied to a printer, a copier, a facsimile having a communication system, a word processor having a printer unit, a portable device, or an industrial device combined with various processing devices.

[0011] As described above, forming an alignment mark on a metal layer increases the number of steps. In addition, if it is desired to omit the process of forming the metal layer, it is necessary to pattern the alignment mark shape on the substrate itself. However, even if an alignment mark is formed on a material that transmits infrared rays, such as a silicon substrate, there is a risk that the alignment mark cannot be recognized by the transmitted infrared light. Therefore, in the following embodiment, a method for manufacturing a substrate having an alignment mark that allows the alignment mark to be recognized by the transmitted infrared light even if the alignment mark is formed on the substrate itself that transmits infrared rays will be described.

[0012] <<First embodiment>> 1 shows a schematic cross-sectional view of a substrate 1 having an alignment mark according to this embodiment. That is, the substrate 1 is a substrate having an alignment mark manufactured according to this embodiment.

[0013] As shown in FIG. 1, the substrate 1 having the alignment mark has a first substrate 2 and a second substrate 3 bonded to the first substrate 2 via an adhesive. The first substrate 2 has an alignment mark 4 and a recess 5 formed therein, which do not penetrate the first substrate 2. The recess 5 may function as a liquid supply path. A liquid ejection port communicating with the recess 5 may be formed in the second surface 2b of the first substrate 2. The second surface 2b side of the first substrate 2 may be thinned until the recess 5 penetrates the first substrate 2, and processed into a liquid supply path penetrating the first substrate 2. That is, the recess 5 is a through or non-through depression formed in the first substrate 2.

[0014] <Alignment mark> FIG. 2 shows a schematic cross-sectional view when aligning the first substrate 2 in this embodiment. As shown in FIG. 2, the first substrate 2 is aligned by image recognition of the alignment mark 4 by infrared transmitted light 7 irradiated from an infrared camera 8 installed either above or below. The material of the first substrate 2 and the second substrate 3 is preferably a silicon substrate from the viewpoint of processability, but may be other materials as long as the infrared transmitted light 7 can penetrate the substrate and recognize the alignment mark 4. In addition, the alignment mark 4 can be easily recognized by making the alignment mark 4 easily visible by making the predetermined parts of the first surface 2a of the first substrate 2, the second surface 2b of the first substrate 2, the first surface 3a of the second substrate 3, and the second surface 3b of the second substrate 3 mirror-finished so as to easily transmit the infrared transmitted light 7. In addition, the parts of the surfaces of the substrates that are outside the horizontal movable range of the infrared camera 8 are not reflected by the infrared camera 8, so there is no need to make them mirror-finished. In other words, the above-mentioned predetermined parts are the parts of the surfaces of the substrates that are within the horizontal movable range of the infrared camera 8.

[0015] The opening shape of the alignment mark 4 may be, for example, a cross, a V-shape, a U-shape, a C-shape, a U-shape, a W-shape, an E-shape, a square, a polygon, a parallelogram, or a circle, as long as it can be identified as an alignment mark. As shown in FIG. 2, the alignment mark 4 must be located within the first substrate 2, which is the target of alignment, so the alignment mark 4 is formed at a depth that does not penetrate the first substrate 2. The bottom 6 of the alignment mark 4 preferably has a characteristic shape. By having a characteristic shape, when the first surface 2a and the second surface 2b of the first substrate 2 and the infrared camera 8 are arranged orthogonally, the infrared transmittance of the bottom 6 becomes lower than the infrared transmittance of the first surface 2a and the second surface 2b of the first substrate 2. This makes it possible to increase the contrast of the alignment mark 4, and makes it easier to image-recognize the alignment mark 4 by the transmitted infrared light 7. Furthermore, when the first surface 2a and the second surface 2b of the first substrate 2 and the infrared camera 8 are arranged perpendicular to each other, it is preferable that the infrared transmittance of the bottom 6 having a characteristic shape be half or less of the infrared transmittance of the first surface 2a and the second surface 2b of the first substrate 2.

[0016] The bottom 6 may have any shape that can reduce the transmittance of infrared rays. For example, the bottom 6 may have any shape, such as a curved surface, an inclined surface, or an uneven surface. In the case of a curved surface, it is preferable that the arrow height of the curved surface is 6 percent or more of the chord length when the opening width of the alignment mark 4 is taken as the chord length. In the case of an inclined surface, it is preferable that the bottom surface of the bottom 6 is inclined at an angle of 3° or more and less than 90° from the first surface 2a of the first substrate 2 to the second surface 2b of the first substrate 2 when the first surface 2a of the first substrate 2 is taken as a surface with an angle of 0°. In this case, the orientation of the inclined surface with respect to the first surface 2a of the first substrate 2 may be inclined in one direction from the first surface 2a to the second surface 2b, or may be inclined in a V-shape from the first surface 2a to the second surface 2b. It may also be inclined following the crystal orientation of the silicon substrate. In the case of an uneven surface, it is preferable that the bottom surface of the bottom 6 is an uneven surface with an average surface roughness of 1 μm or more. The bottom 6 may have a protrusion 21 to facilitate image recognition of the alignment mark 4. The protrusion 21 will be described in the embodiment described later.

[0017] 3 shows schematic plan views of the first substrate 2 in each of the cases (a) to (d). The alignment marks 4 and the recesses 5 can be formed by dry etching, which is a technique for processing a silicon surface using gas. From the viewpoint of omitting processes, the alignment marks 4 formed on the first substrate 2 are preferably formed simultaneously with the recesses 5.

[0018] As shown in FIG. 3(a), when the alignment mark 4 and the recess 5 are simultaneously formed on the first substrate 2 by dry etching, it is preferable to make the opening width L1 of the alignment mark 4 narrower than the opening width L2 of the recess 5. This can be expected to produce a microloading effect. The microloading effect is that as the opening width of the pattern becomes smaller, the etching rate (etching speed) decreases because ion components and radical components that contribute to etching become less likely to enter the opening pattern. By decreasing the etching rate of the opening width L1, the alignment mark 4 is formed at a position shallower than the recess 5, and it is possible to suppress the alignment mark 4 from penetrating. In addition, it is possible to simultaneously form the alignment mark and the recess 5. If it is desired to form the alignment mark 4 at a position clearly shallower than the recess 5, it is preferable to make the opening width L2 of the recess 5 five times or more larger than the opening width L1 of the alignment mark 4.

[0019] <Modification of the first embodiment> 3(b) and (c) show schematic plan views of the first substrate 2 when the shape of the alignment mark 4 in this embodiment is modified. In FIG. 3(b), the alignment mark 4 is formed as an aggregate of a plurality of holes 9. When the alignment mark 4 and the recess 5 are simultaneously formed on the first substrate 2 by dry etching, the alignment mark 4 is divided into a plurality of holes 9 each having a narrow opening width, and a microloading effect can be expected. In addition, since the opening width in FIG. 3(b) is narrower than that in FIG. 3(a), the depth of the alignment mark 4 can be made shallower, and the alignment mark 4 and the recess 5 can be easily formed simultaneously. The opening shape of the hole 9 may be any shape such as a square, a rectangle, a polygon, a parallelogram, or a circle, as long as the microloading effect can be expected and the hole 9 can be identified as an alignment mark. As an example, the alignment mark 4 may be formed as an aggregate of a plurality of holes 9 and a linear opening 10, as shown in FIG. 3(c).

[0020] FIG. 3(d) shows a modified example of the arrangement of alignment marks 4 which differs from those shown in FIGS. 3(b) and (c) above.

[0021] 3(d) shows a schematic plan view of the first substrate 2 in the case where the alignment mark 4 is disposed so as to be close to the recess 5. With such an arrangement, the radical components that contribute to etching are consumed in the etching of the recess 5 adjacent to the alignment mark 4, and a loading effect can be expected due to a decrease in the etching rate of the alignment mark 4. Therefore, it is possible to form the alignment mark 4 at a shallower position than in the form of FIG. 3(a), which makes it easier to form the alignment mark 4 and the recess 5 simultaneously.

[0022] <<Second embodiment>> FIG. 4 shows a plan view that shows a schematic diagram of the first substrate 2 having an alignment mark in this embodiment. In this embodiment, the positions of the alignment mark 4 and the recessed portion 5 are determined depending on the difference in the distribution of plasma density in the first substrate 2. In the first substrate 2 shown in FIG. 4, the region 15 has a low plasma density and the region 19 has a high plasma density, with the broken line as the boundary. In such a case, it is preferable to form the alignment mark 4 in the region 15 with low plasma density. This is because forming the alignment mark 4 in the region 15 with low plasma density reduces the etching rate of the alignment mark 4, and the alignment mark 4 can be formed at a shallower position. On the other hand, the recessed portion 5 is formed in the region 19 with high plasma density. By forming the recessed portion 5 in the region 19 with high plasma density, it is possible to prevent the alignment mark 4 from being formed at a deeper position than the recessed portion 5, and therefore the alignment mark 4 and the recessed portion 5 can be easily formed simultaneously. As a result, the alignment mark 4 in this embodiment is provided close to the outermost periphery of the first substrate 2. When the region 15 of low plasma density is in the vicinity of the center of the first substrate 2, the alignment mark 4 may be provided in the vicinity of the center of the first substrate 2.

[0023] <<Third embodiment>> FIG. 5 shows a schematic cross-sectional view of the first substrate 2 in this embodiment. The first substrate 2 in this embodiment is not a substrate of a single silicon layer, but an SOI (Silicon On Insulator) substrate in which a first silicon layer 12, an oxide layer 13, and a second silicon layer 20 are laminated. In the first substrate 2, a recess 5 and an alignment mark 4 that does not penetrate the first substrate 2 are simultaneously formed by dry etching. The bottom surface of the recess 5 is a smooth bottom surface 14 with the oxide layer 13 exposed. The reason why the bottom surface of the recess 5 is made smooth is that there is an advantage in that the volume of the liquid supply flow path can be increased when the recess 5 is used as a liquid supply path.

[0024] This embodiment is effective when it is desired to maintain the bottom 6 of the alignment mark 4 with a characteristic shape and to make the bottom surface of the recess a smooth bottom surface 14. However, when etching is performed until the bottom surface of the recess 5 becomes a smooth bottom surface 14, the etching time is longer than that of the first embodiment. Therefore, unless the opening width of the alignment mark 4 is narrower than that of the first embodiment, there is a concern that the bottom surface of the alignment mark 4 will also become a smooth bottom surface 14 or will penetrate the first substrate 2. Since the alignment mark 4 with the smooth bottom surface 14 transmits infrared rays, image recognition by the transmitted light 7 of infrared rays is not possible, and the first substrate 2 cannot be aligned. Also, when the alignment mark 4 penetrates the first substrate 2, image recognition by the transmitted light 7 of infrared rays is not possible, and the first substrate 2 cannot be aligned. Therefore, in this embodiment, it is preferable to narrow the opening width of the alignment mark 4 compared to the case of applying the first embodiment.

[0025] <<Fourth embodiment>> FIG. 6 shows a schematic cross-sectional view of the first substrate 2 in this embodiment. The first substrate 2 in this embodiment is an SOI substrate, as in the third embodiment. In addition to the recess 5 and the alignment mark 4 formed at a position not penetrating the first substrate 2, the first substrate 2 is formed with a frame-shaped groove 11. The bottom surfaces of the recess 5 and the frame-shaped groove 11 are smooth bottom surfaces 14 with the oxide layer 13 exposed. The frame-shaped groove 11, the alignment mark 4, and the recess 5 are simultaneously formed by dry etching. This can be expected to produce a loading effect in which the etching rate of the alignment mark 4 is reduced by the radical components contributing to etching being consumed in the etching of the frame-shaped groove 11 adjacent to the alignment mark 4. This makes it easier to simultaneously form the alignment mark 4 and the recess 5.

[0026] FIG. 7 shows a schematic plan view of the first substrate 2 in this embodiment. As shown in FIG. 6, the etching of the frame-shaped groove 11 can be stopped at the oxide layer 13. As a result, as shown in FIG. 7, the opening width L3 of the frame-shaped groove 11 can be made wider than the opening width L2 of the recess 5, and the recess 5 can be prevented from being formed at a position deeper than the frame-shaped groove 11. By widening the opening width L3 of the frame-shaped groove 11, the depth of the alignment mark 4 can be made shallower than in the third embodiment due to the above-mentioned loading effect, making it easier to simultaneously form the alignment mark 4 and the recess 5. The shape of the frame-shaped groove 11 may be any shape that can be expected to have a loading effect, and may be any of a frame-shaped circle, a frame-shaped square, a frame-shaped rectangle, a frame-shaped polygon, or a frame-shaped parallelogram that surrounds the alignment mark 4.

[0027] <<Fifth embodiment>> Figure 10 shows an example of the planar shape of a non-penetrating alignment mark processed by dry etching on a silicon substrate, and the mark outline shape (recognized outline 52) actually recognized on the alignment software. The dimensions measured by an electron beam microscope are also shown in the figure. The shaded area is the non-penetrating hole 51 processed by dry etching.

[0028] 10(a) is composed of two U-shaped marks. The hatched hole 51 looks dark against the background. The recognized outline of the mark also almost coincides with the outer periphery of the two marks.

[0029] Figure 10(b) shows a modified shape of the mark shown in Figure 10(a) in order to reduce the dry etching depth and prevent the substrate from being penetrated further. Compared to Figure 10(a), the U-shaped portion is divided into three parts, each part being separated from the others. Figure 10(d) shows the recognition contour of the mark corresponding to Figure 10(a). As shown in Figure 10(b), it can be seen that the recognition contour 52 corresponding to Figure 10(a) is also the outer periphery shape of the small pieced part.

[0030] In Fig. 10(b), although there is an advantage that the depth of the mark can be made shallow, each part of the mark is fragmented and small. Therefore, as shown in Fig. 10(e), the mark recognition outline corresponding to Fig. 10(b) is a collection of small shapes. Such a mark may have poor recognizability.

[0031] An example of a decrease in recognizability is when an adhesive is applied to one of the substrates and the substrates are bonded, the contrast (10μm to 500μm periodic waviness) caused by the unevenness on the adhesive surface can cause disturbances, resulting in a decrease in recognizability. Other disturbances include the unevenness of the adhesive not being completely eliminated when the substrates are bonded, leaving voids, or minute structures that originally existed on the substrate. It is believed that the smaller the fragmented mark components become, the less distinctive the features become, which causes a decrease in recognizability.

[0032] FIG. 10(c) shows a configuration in which the mark is composed of a group of holes, and the group portion composed of the most adjacent holes is the mark assembly. Each of the two U-shapes is a mark assembly composed of a group of holes. The holes (outermost holes) 51 at the outermost side of the mark assembly extend in one direction in the substrate plane direction. When the holes 51 constitute the side (outermost side) arranged on the outermost side of the mark assembly, the one direction is, for example, the longitudinal direction of the outermost side. The recognition contour 52 is a closed curve that includes the outermost sides and the mark assembly. That is, the connection between the adjacent outermost sides becomes the contour of the alignment mark. In the example of FIG. 10(c), the actual shape is a large number of holes, but as shown in FIG. 10(f), the recognition contour corresponding to FIG. 10(c) is two large U-shapes as a recognition shape.

[0033] 10(c), the distance between the holes 51 in the mark assembly is designed to be small. In this embodiment, a mark similar to that in FIG. 10(a) is constructed by arranging a plurality of holes 51, each 6 μm wide on a side, with the average distance between the holes 51 being 4 μm. Because the average distance between the holes 51 is narrow at 4 μm, on the image sensor that recognizes the alignment mark, the black portion extends outside the actual dimensions of the hole due to blurring caused by scattering from the sidewalls and bottom of the hole.

[0034] As a result, the area between the nearest adjacent holes 51 (hole spacing area) is a 4 μm wide area without holes, but it appears black on the image, so the collection of holes (U-shaped area) can be recognized as a single black mark. The recognized outline 52 of the mark is the same as that shown in Figure 10(d).

[0035] Next, we consider the distance between holes that allows images of multiple holes to be joined together without separation, as the inter-hole areas are covered with blur caused by scattering from the side walls and bottom of the holes. If the actual distance between holes is greater than 15 μm, the images of the holes will be separated. For example, in Figure 10(b), the actual distance between holes is 20 μm, but they are recognized as individual holes.

[0036] Moreover, since FIG. 10(c) is composed of minute holes with a width of 6 μm, the dry etching depth is likely to be shallower due to the microloading effect. This has the advantage of making it more difficult to penetrate the substrate. In addition, the recognition contour can be freely designed to be large, which has the advantage of improving mark recognition. Taking the above results into consideration, it is more preferable for the actual distance between holes to be 10 μm or less, as this allows the images of the holes to be stably connected. It can also be said that even if the actual distance between holes is 15 μm or less, it is still possible to connect the images to a certain extent, making it suitable.

[0037] Here, we prepare two pairs of 625μm thick double-sided polished silicon substrates, and consider processing the alignment marks shown in Fig. 10(a)-(c) non-penetratingly on one of the bonding surfaces by dry etching. Specifically, benzocyclobutene resin is transferred to the surface with the alignment mark at a thickness of 2μm as an adhesive, and the other silicon substrate is bonded to it. As a result of constantly observing and measuring the alignment marks with an infrared microscope during bonding, the mark in Fig. 10(b) had poor stability in mark recognition before and after bonding, and the mark center coordinates were not stable, or the mark could not be detected sometimes. The cause is presumed to be the occurrence of disturbance factors that hinder mark recognition near the alignment mark (surface unevenness of the adhesive, and some of the unevenness of the adhesive that was not crushed and remained as voids).

[0038] On the other hand, the marks in Figures 10(a) and 10(c) are always stable in recognition before and during bonding, and their central coordinates do not move. In Figure 10(a), the inside of the mark is blackened due to the non-penetration, and the recognition outline is large, so recognition is stable, but it was shown that a mark formed by arranging many microholes, such as in Figure 10(c), can also have the same recognition stability.

[0039] The mark composed of a collection of micro-apertures shown in Fig. 10(c) can be configured in a shape other than a dot such as a square. An example is shown in Fig. 11. For either mark, it is preferable to make the actual distance between adjacent micro-apertures sufficiently small. It is also preferable to make the blurred areas near the ends of the micro-marks close enough to be in contact with each other.

[0040] The blur width may be controlled by adjusting the optical system of the infrared microscope. When adjusting, it is preferable to set the alignment mark observation optical system so that the image contrast corresponding to the part sandwiched between adjacent holes in the optical image of the alignment mark is darker than the part outside the range of the alignment mark and the background part where there is no structure. It is preferable to reduce the numerical aperture of the infrared lens, slightly shift the distance between the workpiece and the sensor from the focal position, or lengthen the wavelength of the infrared light to increase the blur width. However, there is a disadvantage that the stability or clarity of the image itself is reduced, so it is preferable to adjust it within the range allowed by the alignment accuracy.

[0041] FIG. 11(a) is composed of a collection of long grooves extending in the substrate plane direction, and these long grooves are arranged on the contour of the alignment mark. By making the holes long, the hole depth becomes deeper than the dots. However, compared to the liquid supply flow path processed in the same etching process, the holes are sufficiently shallow, so even if the liquid flow path is penetrated, the long grooves do not penetrate through them. The long grooves are deeper than the dots, and the unevenness at the bottom increases, making them more likely to scatter, so the inside of the mark becomes darker than the dots. As a result, the visibility of the mark increases and the recognition stability improves.

[0042] As another example, as shown in Fig. 11(b), the direction of the long groove may be rotated 90 degrees from that of Fig. 11(a), or as shown in Fig. 11(c), the long groove may be extended obliquely. Note that if the width of the hole 53 (length of the short side of the hole) is too wide, the etching rate increases and there is a risk of the hole penetrating the substrate, which is not preferable. Also, if the groove is narrow, etching does not proceed easily. A preferable width is 0.1 to 10 μm.

[0043] In the case of the long grooves in Fig. 11(a), when the interval between adjacent long grooves widens, the interval between the long grooves becomes thinner on the image and they become separated. Fig. 12(a) shows the recognized contour at that time. As the separation between the long grooves progresses, the edge of the recognized contour at the interval between the long grooves becomes recessed, and the shape stability decreases slightly.

[0044] In contrast, if the outermost periphery of the mark assembly is processed as a continuous closed space long groove as shown in Fig. 11(d), it is possible to prevent the occurrence of a recess in the recognition outline. As a result, a recognition outline 52 without a recess as shown in Fig. 12(b) is obtained. In Fig. 11(d), the outer periphery of the mark assembly is made into a continuous groove, and dots are arranged inside it.

[0045] Furthermore, as shown in FIG. 11(e), it is preferable to make the outer periphery of the mark assembly a continuous groove and arrange multiple grooves on closed curves inside, or to arrange multiple long grooves inside as shown in FIG. 11(f), because this makes the inside of the mark more black.

[0046] 11(d) to (f), the continuous groove surrounding the outermost periphery of the mark assembly may be partially discontinuous. It may also be interrupted in multiple places. In addition, if the groove width is too wide, the etching rate increases and there is a risk of the substrate being penetrated, which is not preferable. Also, if the groove is narrow, etching does not proceed easily. A suitable width is 0.1 to 10 μm.

[0047] Furthermore, regarding the hole density of the microhole assembly (ratio of the opening area of ​​the microholes to the total area of ​​the mark assembly), if it is 30 to 50%, the inside of the mark assembly is blackened and the mark can be stably recognized, which is preferable. Note that the mark can be recognized even if the hole density is lower than 30 to 50%, and in order to obtain a recognizable black contrast, the hole density is preferably 10% or more. Furthermore, it is preferable that the density of the microhole assembly is higher toward the outside of the mark assembly. This is because the outermost boundary of the mark assembly is the recognition outline, and the higher the density and the blacker the area near the outermost part of the mark, the more stable it becomes.

[0048] <<Sixth embodiment>> Next, an example of forming an alignment mark using wet etching will be described. When a silicon substrate is subjected to crystal anisotropic wet etching using a strong alkaline etching solution, the etching rate differs depending on the crystal plane, and therefore various etching hole shapes can be obtained depending on the type of substrate.

[0049] Examples of the substrate include a Si(001) substrate, a Si(110) substrate, and a Si(112) substrate. Examples of the wet etching solution include potassium hydroxide and tetramethylammonium hydroxide. It is preferable to heat the substrate to a temperature of 40 to 90°C.

[0050] When the mark pattern becomes fine, the (111) surface is exposed in a large part of the inside of the mark hole as the etching progresses. The etching rate is slow on the (111) surface, and wet etching stops, so the cross-sectional shape of the hole becomes stable.

[0051] Figure 13(a) shows a shape 61 formed on a Si(001) substrate by processing using wet etching. Figure 13(b) shows a depth profile of the A-A' cross section of Figure 13(a). In Figure 13(b), a stable microhole is processed by exposing the (111) surface 62 to the side wall of the mark hole. The unetched portion is the (001) surface 63.

[0052] By processing a large number of such microholes and narrowing the intervals between the multiple holes, a recognition contour of any shape can be obtained, as in the fifth embodiment (a microhole aggregate processed by dry etching). The preferred arrangement method for the holes in this embodiment is the same as in the fifth embodiment. In particular, when crystal anisotropic wet etching is used, the mark shapes that can be stabilized are limited, and the planar shape cannot be freely designed in some cases. By forming the mark with such an aggregate of multiple microholes, there is an advantage that a recognition contour of any shape can be obtained.

[0053] Figure 13(c) shows a shape 63 formed on a Si(110) substrate by processing using wet etching. Figure 13(d) shows a depth profile of the cross section B-B' of Figure 13(c). In Figure 13(d), the (111) surface 62 is similarly exposed on the side wall of the mark hole, and a stable microhole has been processed.

[0054] <<Seventh embodiment>> Another method for decreasing the rate of dry etching of the alignment mark while enlarging the recognition contour of the mark is to form the outer periphery of the mark with a narrow groove.

[0055] An example is shown in Figure 14(a). For a U-shaped mark shape, a narrow closed groove 57 is formed warping against the mark contour. The narrow groove width causes a microloading effect, which reduces the dry etching rate, allowing groove 57 to be made shallow. The outermost continuous side of groove 57 becomes the recognition contour as it is, and a recognition contour of any size and shape can be obtained. Therefore, the groove can be made shallow while still controlling its shape as desired.

[0056] Moreover, if the groove width of the groove 57 is too wide, the etching rate increases and there is a risk of the substrate being penetrated, which is not preferable. Also, if the groove is narrow, etching does not proceed easily. A preferable width is 0.1 to 10 μm.

[0057] Furthermore, as shown in FIG. 14(b), a part of the mark outline may be formed by a groove. The recognition outline is composed of multiple grooves 58 that are not closed spaces. This has the advantage of reducing the etching rate because the length of the grooves can be shortened. In addition, it is preferable to narrow the gap between multiple grooves, and the gap distance can be set to the same distance as in the fifth embodiment.

[0058] <First manufacturing method> 8(a) to 8(h) are cross-sectional views showing a method for manufacturing the substrate 1, as viewed from the same direction as in FIG. 1. A first method for manufacturing the substrate 1 having an alignment mark will be described with reference to FIG.

[0059] First, as shown in Fig. 8(a), a silicon substrate with a thickness of about 725 µm and a diameter of about 200 mm is prepared as the first substrate 2. The first surface 2a and the second surface 2b of the first substrate 2 are mirror surfaces. Next, as shown in Fig. 8(b), a positive resist is applied to the first surface 2a of the first substrate 2 by a spin coat method, and then baked to form a resist layer 16.

[0060] 8(c), a cross-shaped alignment mark processing pattern 17 with an opening width of about 10 μm and a recess processing pattern 18 with an opening width of about 100 μm were formed in the resist layer 16 by photolithography. Since the opening width of the alignment mark processing pattern 17 is narrower than the opening width of the recess processing pattern 18, it is possible to reduce the etching rate of the alignment mark 4 to be lower than the etching rate of the recess 5 in the dry etching process described later. In addition, it is possible to form the alignment mark 4 at a position shallower than the recess 5.

[0061] Next, as shown in FIG. 8(d), alignment marks 4 and recesses 5 were simultaneously formed on the first substrate 2 by a Bosch process using reactive ion etching, a type of dry etching. The Bosch process is a technique for anisotropically etching silicon by alternately repeating the formation of a protective film (not shown) mainly composed of carbon and etching with SF6 gas or the like. SF6 gas was used when etching the alignment marks 4 and the recesses 5. C4F8 gas was used when forming a protective film on the side surfaces of the alignment marks 4 and the recesses 5.

[0062] In the case of this embodiment, in order to make it easier to image-recognize the alignment mark 4 with the infrared transmitted light 7, it is preferable to perform dry etching under conditions in which the silicon protrusion 21 is likely to occur on the bottom 6 and the bottom 6 is likely to become a curved surface. The protrusion 21 is formed by etching the silicon, leaving a protective film partially on the bottom 6, and the protective film serves as an etching mask, and the silicon remains. The presence of the protrusion 21 makes it easier to image-recognize using the infrared transmitted light 7. In this embodiment, in order to create conditions in which the silicon protrusion 21 is likely to occur on the bottom 6, the flow rate of SF6 gas is reduced to favor the formation of the protective film. In addition, in order to create conditions in which the bottom 6 is likely to become a curved surface, the output of the bias that attracts ions and plays a role in favoring anisotropy is reduced, and isotropy is favored. At this time, the bottom 6 has a characteristic shape having the silicon protrusion 21 and a curved surface. In addition, in order to keep the infrared transmittance low, it is preferable to form the alignment mark 4 so as not to penetrate the first substrate 2.

[0063] The depth of the formed alignment mark 4 was about 400 μm, and the depth of the formed recess 5 was about 600 μm. In this embodiment, the bottom 6 of the alignment mark 4 is formed by the silicon protrusion 21 and a curved surface, but the shape of the bottom 6 is not limited to this. In this embodiment, reactive ion etching is used, but the alignment mark 4 may be formed by chemical etching, wet etching, laser processing, or sandblasting. In addition, the silicon protrusion 21 formed in the recess 5 is unnecessary in this embodiment, so it may be removed after processing the alignment mark 4 and the recess 5 by dry etching.

[0064] Next, as shown in Fig. 8(e), the protective film in the Bosch process is removed with hydrofluoroether, and then the resist layer 16 is removed with an alkaline stripping solution. Next, as shown in Fig. 8(f), a silicon substrate with a thickness of about 725 μm and a diameter of about 200 mm is prepared as the second substrate 3. The first surface 3a and the second surface 3b of the second substrate 3 are mirror surfaces.

[0065] Next, as shown in FIG. 8(g), the first surface 2a of the first substrate 2 and the second surface 3b of the second substrate 3 are opposed to each other, and the first surface 2a of the first substrate 2, the second surface 2b of the first substrate 2, and an infrared camera 8 used for recognizing the alignment mark 4 are disposed orthogonally. The infrared transmitted light 7 may be irradiated from the first surface 2a side of the first substrate 2, or may be irradiated from the second surface 2b side of the first substrate 2. Next, the alignment mark 4 formed on the first substrate 2 is image-recognized by the infrared transmitted light 7 irradiated from the infrared camera 8. When aligning the first substrate 2, the contrast of the alignment mark 4 reflected by the infrared camera 8 is increased, so that the alignment mark 4 can be image-recognized by the infrared transmitted light 7. This shows that the infrared transmittance of the bottom 6, which has a characteristic shape due to dry etching, is lower than the infrared transmittance of the first surface 2a of the first substrate 2. It is also understood that even if the alignment mark 4 is formed on a silicon substrate that transmits infrared rays, it is possible to perform image recognition of the alignment mark 4 using the transmitted infrared light 7. Next, the first substrate 2 is aligned based on the alignment mark 4.

[0066] Next, as shown in FIG. 8(h), the aligned first surface 2a of the first substrate 2 and the second surface 3b of the second substrate 3 are bonded via an adhesive (not shown) and then cured by heat treatment. The adhesive is spin-coated on a dry film before aligning the first substrate 2, and transferred to the first surface 2a of the first substrate 2. At this time, the adhesive is not transferred onto the alignment marks 4 and the openings of the recesses 5. The adhesive may be applied by screen printing or patterning by photolithography using a photosensitive adhesive. The bonding method may be direct bonding such as diffusion bonding without using an adhesive.

[0067] As described above, according to this embodiment, it is possible to manufacture a silicon substrate having an alignment mark formed on the substrate itself. Furthermore, in the substrate 1 having an alignment mark manufactured in this manner, it is possible to align the first substrate 2 by image-recognizing the alignment mark 4 using transmitted infrared light 7.

[0068] <Second manufacturing method> Figure 9 is a cross-sectional view showing a manufacturing method for the first substrate 2 shown in Figure 4. That is, this figure is a cross-sectional view of the first substrate 2 shown in Figure 4 when viewed from the same direction as Figure 1. The second manufacturing method shows an example in which the first substrate 2 having an alignment mark is manufactured by a method different from the first manufacturing method.

[0069] The difference between the second manufacturing method and the above-mentioned first manufacturing method is Fig. 8(d) in Fig. 8. Therefore, only a part corresponding to Fig. 8(d) will be explained below.

[0070] As shown in FIG. 9, alignment marks 4 and recesses 5 were simultaneously formed in first substrate 2 by the Bosch process using reactive ion etching, which is a type of dry etching.

[0071] SF6 gas is used when etching the alignment mark 4 and the recess 5. C4F8 gas is used when forming a protective film on the side of the alignment mark 4 and the recess 5. At this time, the alignment mark 4 is formed in the region 15 of the first surface 2a of the first substrate 2 where the plasma density is low, and the recess 5 is formed in the region 19 of the first surface 2a of the first substrate 2 where the plasma density is high, so that a microloading effect can be expected. That is, the alignment mark 4 can be formed at a position shallower than the recess 5. The depth of the formed alignment mark 4 was about 360 μm, and the depth of the formed recess 5 was about 600 μm. The following description is omitted because it is the same as FIG. 8(e) to FIG. 8(h).

[0072] Even in the case of substrate 1 having alignment marks manufactured as described above, it is possible to perform image recognition of alignment mark 4 using transmitted infrared light 7, thereby enabling alignment of first substrate 2.

[0073] <<Other embodiments>> The above-described embodiments can be combined as appropriate. For example, the alignment mark 4 surrounded by the frame-shaped groove 11 described with reference to Figures 6 and 7 can be formed in a shallower portion of the substrate 2 by forming the alignment mark 4 with a collection of a plurality of holes 9 as described with reference to Figure 3(b).

[0074] In addition, for example, the forms described in (c) and (d) of Figure 3 may be combined. The alignment mark 4 can be formed in a shallower portion of the substrate 2 by forming the alignment mark 4 at a position close to the recess 5 and as a collection of a plurality of holes 9 and linear openings 10. In addition, the embodiments described above may be appropriately combined.

[0075] The present invention also includes the following configurations.

[0076] (Configuration 1) A method for manufacturing a substrate having an alignment mark, comprising the steps of: a forming step of forming an alignment mark and a recess in the substrate, the alignment mark having a bottom portion with a lower infrared transmittance than the first surface and the second surface of the substrate and not penetrating the substrate; an alignment step of aligning the substrate by orthogonally arranging an infrared camera and predetermined positions in the horizontal direction of the first surface and the second surface of the substrate, and recognizing the image of the alignment mark formed on the substrate by the transmitted light of infrared light irradiated from the infrared camera, and aligning the substrate; A method for manufacturing a substrate, comprising:

[0077] (Configuration 2) 2. The method for manufacturing a substrate according to claim 1, wherein the predetermined position is a position where the alignment mark formed on the substrate can be image-recognized by the transmitted light irradiated from the infrared camera.

[0078] (Configuration 3) 3. The method for manufacturing a substrate according to configuration 1 or 2, wherein in the forming step, the alignment mark and the recess are simultaneously formed by dry etching.

[0079] (Configuration 4) 4. The method for manufacturing a substrate according to any one of configurations 1 to 3, wherein in the forming step, an etching rate of the alignment mark is made slower than an etching rate of the recess.

[0080] (Configuration 5) 5. The method of claim 1, wherein the forming step forms the alignment mark so that an opening width of the alignment mark is narrower than an opening width of the recess.

[0081] (Configuration 6) 6. The method for manufacturing a substrate according to any one of configurations 1 to 5, wherein the forming step forms the alignment mark in an area of ​​the substrate where plasma density is low.

[0082] (Configuration 7) 7. The method for manufacturing a substrate according to any one of configurations 1 to 6, wherein the forming step forms the alignment mark at a position adjacent to the recess.

[0083] (Configuration 8) 8. The method for manufacturing a substrate according to any one of configurations 1 to 7, wherein the forming step forms a frame-shaped groove so as to surround a periphery of the alignment mark.

[0084] (Configuration 9) 8. The method for manufacturing a substrate according to any one of configurations 1 to 7, wherein in the forming step, the alignment mark is formed as a plurality of holes that do not penetrate the substrate.

[0085] (Configuration 10) a group of the plurality of holes that is closest to each other is defined as a mark assembly, a hole that is located most outside of the mark assembly is defined as an outermost hole, and a side of the outermost hole that is located most outside of the mark assembly is defined as an outermost side, A method for manufacturing a substrate according to configuration 9, further comprising aligning a closed curve including the mark assembly and including a plurality of the outermost sides as part of a recognition shape of the alignment mark.

[0086] (Configuration 11) Among the plurality of groups of holes, a group portion consisting of holes closest to each other is defined as a mark group, and the mark group is The method for manufacturing a substrate according to configuration 9, wherein an alignment mark observation optical system is set so that, in an optical image of the alignment mark, the image contrast corresponding to the portion sandwiched between adjacent holes is darker than the image contrast outside the alignment mark and in the background portion where no structures are present.

[0087] (Configuration 12) A substrate having an alignment mark, an alignment mark that does not penetrate the substrate and has a bottom portion that has a lower infrared transmittance than the first surface and the second surface when predetermined positions on the first surface and the second surface of the substrate and an infrared camera are disposed perpendicular to each other; A recess; A substrate, comprising:

[0088] (Configuration 13) 13. The substrate according to configuration 12, wherein the opening width of the alignment mark is narrower than the opening width of the recess.

[0089] (Configuration 14) 14. The substrate according to claim 12 or 13, wherein the alignment mark is formed at a position shallower than the recess.

[0090] (Configuration 15) 15. The substrate of any one of configurations 12 to 14, wherein the alignment mark is a collection of a plurality of holes.

[0091] (Configuration 16) 15. The substrate of any one of configurations 12 to 14, wherein the alignment mark is formed by a collection of a plurality of holes and a linear opening.

[0092] (Configuration 17) 17. The substrate of any one of claims 12 to 16, wherein the substrate is a silicon substrate.

[0093] (Configuration 18) 18. The substrate of any one of configurations 12 to 17, wherein at least a portion of the first and second surfaces of the substrate are mirror surfaces.

[0094] (Configuration 19) 19. The substrate according to any one of configurations 12 to 18, wherein the substrate is a silicon on insulator (SOI) substrate.

[0095] (Configuration 20) 20. The substrate according to any one of configurations 12 to 19, further comprising a frame-shaped groove formed so as to surround the alignment mark.

[0096] (Configuration 21) 21. The substrate of any one of configurations 12 to 20, wherein the substrate is bonded to a second substrate that is a silicon substrate.

[0097] (Configuration 22) 22. The substrate of embodiment 21, wherein at least a portion of the first surface and the second surface of the second substrate are mirror surfaces.

[0098] (Configuration 23) an alignment mark including a plurality of holes, a group of the plurality of holes including holes that are closest to each other is defined as a mark assembly, and holes that are located on the outermost side of the mark assembly are defined as outermost holes; a side of the outermost hole that is disposed on the outermost side of the mark assembly is defined as an outermost side; The substrate according to configuration 12, wherein adjacent outermost edges are connected to each other to form the outline of the alignment mark.

[0099] (Configuration 24) 24. The substrate of claim 23, wherein the average distance between nearest neighboring holes is 15 μm or less.

[0100] (Configuration 25) 25. The substrate according to claim 23 or 24, wherein the plurality of holes extend in one direction in a plane of the substrate.

[0101] (Configuration 26) The one direction is 26. The substrate described in structure 25, characterized in that it includes the mark collection and is in the longitudinal direction of a closed curve including a plurality of the outermost sides.

[0102] (Configuration 27) 25. The substrate according to structure 23 or 24, wherein the outermost hole surrounds a plurality of other holes that constitute the mark assembly.

[0103] (Configuration 28) The substrate according to any one of structures 23 to 27, wherein the substrate is a silicon substrate, the plurality of holes are formed by processing the silicon substrate by anisotropic wet etching, and a portion of a surface forming the interior of the plurality of holes is a (111) surface.

[0104] (Configuration 29) 24. The substrate of claim 23, wherein the alignment mark is comprised of a plurality of slots, the slots being disposed on a contour of the alignment mark.

[0105] (Configuration 30) 24. The substrate according to claim 23, wherein the alignment mark is composed of a long groove hole having a closed space shape, and the long groove hole is disposed on the outline of the alignment mark.

[0106] (Configuration 31) 31. The substrate according to structure 29 or 30, wherein the long groove may be partially discontinuous.

[0107] (Configuration 32) 24. The substrate according to claim 23, wherein the outer periphery of the alignment mark is formed as a groove having a width of 0.1 to 10 μm. [Explanation of symbols]

[0108] 1. Substrate with alignment marks 2 First board 2a: First surface of first substrate 2b Second surface of the first substrate 4 Alignment marks 5. Recess 7. Infrared transmission 8. Infrared Camera

Claims

1. A substrate having an alignment mark, an alignment mark that does not penetrate the substrate and has a bottom portion that has a lower infrared transmittance than the first surface and the second surface when predetermined positions on the first surface and the second surface of the substrate and an infrared camera are disposed perpendicular to each other; A recess; A substrate, comprising:

2. The substrate according to claim 1 , wherein an opening width of the alignment mark is narrower than an opening width of the recess.

3. The substrate according to claim 1 , wherein the alignment mark is formed at a position shallower than the recess.

4. The substrate according to claim 1 , wherein the alignment mark is a collection of a plurality of holes.

5. The substrate of claim 1 , wherein the alignment mark is formed of a collection of a plurality of holes and a linear opening.

6. The substrate of claim 1 , wherein the substrate is a silicon substrate.

7. The substrate of claim 1 , wherein at least a portion of the first surface and the second surface of the substrate are mirror surfaces.

8. The substrate of claim 1 , wherein the substrate is a silicon on insulator (SOI) substrate.

9. The substrate according to claim 1 , further comprising a frame-shaped groove formed so as to surround the alignment mark.

10. The substrate according to claim 1 , further comprising a second substrate bonded to the substrate, the second substrate being a silicon substrate.

11. The substrate of claim 10 , wherein at least a portion of the first surface and the second surface of the second substrate are mirror surfaces.

12. the alignment mark is composed of a plurality of holes, a group of the plurality of holes is defined as a mark assembly consisting of holes that are closest to each other, the outermost hole in the mark assembly is defined as an outermost hole, and the side of the outermost hole that is disposed on the outermost side of the mark assembly is defined as an outermost side, 2. The substrate according to claim 1, wherein adjacent outermost sides of the outermost sides are connected to each other to form the outline of the alignment mark.

13. 13. The substrate of claim 12, wherein the average distance between nearest neighboring pores is 15 [mu]m or less.

14. The substrate according to claim 12 , wherein the plurality of holes extend in one direction in a plane of the substrate.

15. The one direction is 15. The substrate according to claim 14, which is in a longitudinal direction of a closed curve including the mark collection and including a plurality of the outermost sides.

16. 13. The substrate according to claim 12, wherein the outermost hole surrounds a plurality of other holes that form the mark assembly.

17. 13. The substrate according to claim 12, wherein the substrate is a silicon substrate, the plurality of holes are formed by processing the silicon substrate by anisotropic wet etching, and a portion of a surface constituting the interior of the plurality of holes is a (111) surface.

18. 13. The substrate of claim 12, wherein the alignment mark is comprised of a plurality of slots, the slots being arranged on a contour of the alignment mark.

19. 13. The substrate according to claim 12, wherein the alignment mark is constituted by a long groove hole having a closed space shape, and the long groove hole is disposed on a contour portion of the alignment mark.

20. 20. The substrate according to claim 18, wherein the slot may be partially discontinuous.

21. 13. The substrate according to claim 12, wherein the outer periphery of the alignment mark is formed as a groove having a width of 0.1 to 10 μm.

Citation Information

Patent Citations

  • Mark for alignment on semiconductor wafer and manufacture thereof

    JP1983090728A

  • Dust analyzing wafer and manufacture thereof

    JP1991256339A

  • Manufacturing method for electronic device and manufacturing method for ink jet head

    JP2019064272A

  • Electronic device, liquid injection head and method of manufacturing liquid injection head

    JP2020157606A