Peeling detection label and peeling detection method
The peel detection label with a permanent adhesive and brittle film base material, along with a removable adhesive, addresses the issue of unauthorized peeling by ensuring the first label remains on the adherend, facilitating easy detection and preventing reuse.
Patent Information
- Application Number
- JP2023063307
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-10
- Publication Date
- 2024-10-23
AI Technical Summary
Existing peel-off detection labels cannot effectively prevent unauthorized peeling and reuse, as they can be cleanly detached from the adherend, making it difficult to determine if the label was originally attached.
A peel detection label comprising a first label with a permanent adhesive and brittle film base material, and a second label with a removable adhesive, where the second label peels off upon detachment, revealing a pattern or color change, ensuring the first label remains on the adherend, thus preventing reuse.
The label provides easy detection of unauthorized peeling and prevents the first label from being easily removed, maintaining security and integrity by ensuring the first label remains on the adherend, indicating tampering.
Smart Images

Figure 2024150075000002 
Figure 2024150075000003 
Figure 2024150075000004
Abstract
Description
[Technical field]
[0001] The present invention relates to a peeling detection label and a peeling detection method. [Background technology]
[0002] Label materials that can impart security capabilities when affixed to products are widely known as VOID labels. For example, a character transfer type tamper-evident label is known, which is a tamper-evident label consisting of an adhesive layer having a character pattern and a base sheet, and when the adhesive layer side is attached to an adherend and the label is peeled off, the characters on the adhesive layer are transferred to the adherend. This type of tamper-evident label is used as a caution label or seal for expensive electronic devices and precision machine parts. Non-transferable tamper-evident labels are also known in which the characters stand out on the label when the label is peeled off, leaving no trace on the substrate. This type of tamper-evident label cannot be reused because the characters stand out on the label, and is therefore used to prevent unauthorized opening of medicines, cosmetic boxes, etc., and to prevent the label from being used as a counterfeiting method by peeling off the label of a genuine product and sticking it on another product. This type of tamper-evident label is also useful when it is desired to reuse expensive containers, since the label does not remain on the substrate. Furthermore, for stickers bearing bar codes and the like, tamper-evident labels whose base material is easily destroyed are used in order to prevent counterfeiting by peeling off the bar code label from a genuine product and sticking it on another product.
[0003] Patent Document 1 discloses a peel detection label that is intended to be able to detect unauthorized peeling from an adherend while also being able to peel cleanly from the adherend after use. This peel detection label is a peel detection label in which a first sheet and a second sheet are attached to an adherend by an adhesive layer laminated on the surface of the second sheet opposite to the surface attached to the first sheet, and then the first sheet and the second sheet are peeled off, so that peeling from the adherend can be detected, and the second sheet is divided into two regions by a division line, and each of the two regions has a region along at least a part of the division line on the surface attached to the adherend that is a non-adhered portion that is not attached to the adherend. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] Patent Application No. 2014-215350 Summary of the Invention [Problem to be solved by the invention]
[0005] In the case of a peel-off detection label as described in Patent Document 1, the sheet attached to the substrate peels off cleanly from the substrate, making it impossible to determine whether the tamper-evident label itself was originally attached or not. The present invention has been made in consideration of the above-mentioned circumstances, and aims to provide a peeling detection label and a peeling detection method which make it easy to detect when it has been peeled off, and which cannot be easily peeled off from the substrate once peeled off. [Means for solving the problem]
[0006] As a result of extensive research, the inventors have discovered that the above-mentioned problems can be solved by providing a second label that allows characters or the like to appear on the peeled sheet when the upper sheet is peeled off, thereby making it possible to detect that the sheet has been peeled off, and a first label that can be attached to an object, but has a highly adhesive and brittle base material so that the second label does not peel off from the object when it is peeled off, and have thus arrived at the present invention.
[0007] That is, the present invention is a peel detection label comprising a first label and a second label provided on the first label, the surface of the first label forming the first main surface and the surface of the second label forming the second main surface, the first label comprising, from the first main surface side, a permanent adhesive type adhesive layer and a brittle film substrate, in that order, and the second label comprising, from the second main surface side, at least a support, a pattern layer formed on a part of the surface of the support, a substrate layer (Y), and a removable adhesive layer (X), in that order.
[0008] The brittle film substrate preferably has a tensile elongation at break of 20% or less in the film formation direction (MD) as measured in accordance with JIS Z0237:2009.
[0009] The brittle film substrate preferably has a tensile breaking strength of 100 N / 15 mm or less in the film forming direction (MD) as measured in accordance with JIS Z0237:2009.
[0010] The adhesive strength of the permanent adhesive layer is 5 N / 25 mm or more and 40.0 N / 25 mm or less, and the adhesive strength of the removable adhesive layer (X) is 0.1 N / 25 mm or more and 30.0 N / 25 mm or less, and it is preferable that the adhesive strength of the permanent adhesive layer is greater than the adhesive strength of the removable adhesive layer (X).
[0011] The second label has a first adhesive layer between the pattern layer and the base layer (Y), and the adhesive strength of the permanent adhesive layer is 5 N / 25 mm or more and 40.0 N / 25 mm or less, and the adhesive strength of the removable adhesive layer (X) is 0.1 N / 25 mm or more and 30.0 N / 25 mm or less, and it is preferable that the adhesive strength of the permanent adhesive layer is greater than that of the removable adhesive layer (X) and that the adhesive strength of the first adhesive layer is greater than that of the removable adhesive layer (X).
[0012] The first label preferably has a first solid print layer on the second label side of the brittle film substrate, and the second label preferably has a second solid print layer between the support and the removable adhesive layer (X).
[0013] It is preferable that the first label has a release material on the first main surface side.
[0014] The second label preferably has a print coat layer on the second main surface side.
[0015] The peel detection method of the present invention is a method for detecting peeling of a peel detection label, the peel detection label comprising a first label and a second label provided on the first label, the surface of the first label side constituting the first main surface and the surface of the second label side constituting the second main surface, the first label comprising, from the first main surface side, a permanent adhesive type adhesive layer and a brittle film substrate, in this order, and the second label comprising, from the second main surface side, a support, a pattern layer formed on a part of the surface of the support, a substrate layer (Y) and a removable adhesive layer (X), in this order, the peel detection label is attached to an adherend with the first main surface of the first label, and when an attempt is made to peel the peel detection label, only the second label is peeled off, and before and after the peeling of the second label, the pattern of the pattern layer appears in the second label, while the first label remains on the adherend, thereby detecting unauthorized peeling of the peel detection label.
[0016] In the peeling detection method of the present invention, the unauthorized peeling of the peeling detection label may be detected by the appearance of colors unique to the first and second labels from the color of the entire peeling detection label before and after the second label is peeled off. Effect of the Invention
[0017] According to the present invention, it is possible to obtain a peel detection label and peel detection method which are easy to detect when they have been peeled off and which, once peeled off, cannot be easily peeled off from the adherend. [Brief description of the drawings]
[0018] [Figure 1] 1 is a schematic cross-sectional view showing one embodiment of a peel detection label of the present invention. [Diagram 2] 1 is a schematic cross-sectional view showing a state in which a peel detection label of one embodiment of the present invention is in the middle of being peeled from an adherend. [Diagram 3] FIG. 4 is a schematic cross-sectional view showing another embodiment of the peel detection label of the present invention. [Figure 4] 10 is a schematic cross-sectional view showing still another embodiment of the peel detection label of the present invention. FIG. [Diagram 5] 1 is a schematic cross-sectional view showing one embodiment of a peel-off detection label having a release material. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0019] In this specification, the range "X to Y" means "X or more and Y or less". Furthermore, unless otherwise specified, operations and measurements of physical properties are performed under the conditions of room temperature (20 to 25°C) and relative humidity 45 to 55% RH. Furthermore, in this specification, (meth)acrylic acid means both acrylic acid and methacrylic acid. The same applies to other similar terms.
[0020] In the present invention, the determination of whether a target resin belongs to a "tacky resin" or a "non-tacky resin" is made based on the following steps (1) to (4). Procedure (1): A 20 μm thick resin layer made only from the target resin is placed on a 50 μm thick polyethylene terephthalate (PET) film, and a test piece measuring 300 mm long and 25 mm wide is prepared by cutting the film into pieces. Procedure (2): In an environment of 23°C and 50% RH (relative humidity), attach the surface of the test piece on which the resin layer is exposed to a stainless steel plate (SUS304, polished #360) and leave it in the same environment for 24 hours. Step (3): After leaving it to stand, measure the adhesive strength at 23°C and 50% RH (relative humidity) using the 180° peel method at a tensile speed of 300 mm / min based on JIS Z0237:2000. Step (4): If the measured adhesive strength is 0.1N / 25mm or more, the resin is judged to be an "adhesive resin." On the other hand, if the measured adhesive strength is less than 0.1N / 25mm, the resin is judged to be a "non-adhesive resin."
[0021] In the present invention, the term "active ingredient" refers to the components contained in the target composition excluding the dilution solvent. In the present invention, the term "visually detectable" means that a change in the peel detection label before and after re-peeling can be confirmed by the human eye. The weight average molecular weight (Mw) is a value calculated as standard polystyrene by gel permeation chromatography (GPC), specifically, a value measured based on the method described in the examples. In addition, for a preferred numerical range (e.g., range of content, etc.), the lower limit and upper limit described in stages can be combined independently. For example, from the description "preferably 10 to 90, more preferably 30 to 60", the "preferable lower limit (10)" and the "more preferable upper limit (60)" can be combined to form "10 to 60". Similarly, from the description "preferably 10 or more, more preferably 30 or more, and preferably 90 or less, more preferably 60 or less", the preferred range can be selected as "10 or more and 60 or less", or the range can simply be selected as "60 or less".
[0022] [Peel detection label] A peel detection label 100 according to one embodiment of the present invention will be described with reference to FIG. 1, the peeling detection label 100 comprises a first label 10 and a second label 20 provided on the first label 10, with a surface 10a on the first label 10 side constituting a first main surface and a surface 20a on the second label 20 side constituting a second main surface. Hereinafter, the surface 10a on the first label 10 side may be referred to as the "first main surface 10a" and the surface 20a on the second label 20 side may be referred to as the "second main surface 20a". The first label 10 comprises, from the first main surface 10a side, a permanent adhesive type adhesive layer 11 and a brittle film substrate 12, in that order, and the second label 20 comprises, from the second main surface 20a side, a support 31, a pattern layer 32 formed on a part of the surface 31a of the support 31, a substrate layer (Y) 34, and a removable adhesive layer (X) 33, in that order.
[0023] As shown in Fig. 2, the peel detection label 100 is used by attaching the permanent adhesive layer 11 to an adherend 200. When an attempt is made to peel the peel detection label 100, once attached, from the adherend 200, the second label 20 is peeled off because the adhesive strength of the permanent adhesive layer 11 is greater than that of the removable adhesive layer (X) 33. At the same time, interfacial peeling occurs between the support 31 and the pattern layer 32, and a gap 40 is generated, causing a pattern to appear in the second label 20, making it possible to visually detect whether the peel detection label 100 has been peeled off from the adherend 200. Moreover, in the peel detection label 100, a first label 10 comprising a permanent adhesive type adhesive layer 11 and a brittle film substrate 12 is affixed to an adherend 200. Even if an attempt is made to peel the first label 10 from the adherend 200 after the second label 20 has been peeled off, the first label 10 is destroyed and cannot be peeled off, so evidence that the first label 10 has been peeled off remains on the adherend 200. Because the first label 10 is destroyed, the first label 10 cannot be reattached or reused. As described above, the peel detection label 100 of the present invention has a double peel detection function with the first label 10 and the second label 20, and has excellent anti-tampering and anti-opening effects, making it a highly secure peel detection label.
[0024] (Other embodiments) A peel detection label 110 according to another embodiment of the present invention will be described with reference to FIG. 3, the peel detection label 110 differs from the peel detection label 100 in that it includes a first adhesive layer (X1) (hereinafter also simply referred to as "adhesive layer (X1)") 33A between a pattern layer 32 formed on a part of the surface 31a of the support 31 and a base layer (Y) 34. This embodiment includes the base layer (Y) 34 between the first adhesive layer (X1) 33A and the removable adhesive layer (X) 33, which makes it easier for the pattern layer 32 to appear, and is a more preferred embodiment of the second label 20.
[0025] (Further Other Embodiments) A peel detection label 120 according to still another embodiment of the present invention will be described with reference to FIG. 4, in the peel detection label 120, the first label 10 comprises, from the first main surface side 10a, a permanent adhesive type adhesive layer 11, a brittle film substrate 12, and a first solid print layer 15, in this order. The second label 20 comprises, from the second main surface side 20a, a print coat layer 50, a support 31, a pattern layer 32 formed on a part of the surface 31a of the support 31, a second solid print layer 35, an adhesive layer (X1) 33A, a substrate layer (Y) 34, and a removable adhesive layer (X) 33, in this order.
[0026] In this embodiment, the peeling detection label 120 makes it possible to detect unauthorized peeling of the peeling detection label 120 by revealing colors unique to the first label 10 and the second label 20 from the color of the entire peeling detection label 120 before and after the second label 20 is peeled off. Details will be provided below.
[0027] The first label and the second label will be described in detail below. 1. First label The first label 10 includes a permanent adhesive layer 11 and a brittle film substrate 12 in this order from the first main surface 10a side.
[0028] 1.1.Permanent adhesive layer The first label 10 is attached to the adherend 200 by means of a permanent adhesive layer 11 . The adhesive that can be used for the permanent adhesive layer 11 is not particularly limited, and any known adhesive can be used alone or in combination of two or more kinds. The adhesive of the permanent adhesive layer 11 is not particularly limited, but examples thereof include adhesives mainly composed of acrylic adhesives, rubber adhesives, polyester adhesives, or silicone adhesives. Among these, it is preferable to use acrylic adhesives. Acrylic adhesives have excellent weather resistance and can be obtained relatively inexpensively.
[0029] Furthermore, the permanent adhesive layer 11 may contain various known additives, such as tackifiers, fillers, antioxidants, heat stabilizers, UV absorbers, light stabilizers, colorants, flame retardants, and antistatic agents, as necessary.
[0030] (Adhesive strength of permanent adhesive layer) The adhesive strength of the permanent adhesive layer 11 in the first label 10 is preferably 5 N / 25 mm or more, more preferably 8 N / 25 mm or more, as measured by the adhesive strength test described below. The upper limit of the adhesive strength of the permanent adhesive layer 11 is not particularly limited, but is preferably 40.0 N / 25 mm or less, more preferably 35.0 N / 25 mm or less. When the adhesive strength of the permanent adhesive layer 11 is within the above range, the adhesive strength to the adherend 200 is good, and the first label 10 is more likely to be destroyed when peeled off from the adherend 200.
[0031] <Adhesive strength test for permanent adhesive layer> The adhesive strength test is performed in accordance with ISO 29862:2007 (JIS Z0237:2009), in which a test piece of the first label 10 is attached to a SUS304 steel plate (test plate) by pressing it with a 2 kg roller going back and forth once, and then the test piece is peeled off at an angle of 180° to the test plate at a peeling speed of 300 mm / min. The test piece of the first label 10 is reinforced with a 25 μm thick adhesive tape based on polyethylene terephthalate to prevent the label from breaking during testing. The size of the test piece is 25 mm wide and 100 mm long or more.
[0032] (Permanent adhesive layer thickness) The thickness of the permanent adhesive layer 11 is preferably 10 μm to 50 μm, more preferably 15 μm to 40 μm, so that the first label 10 has sufficient adhesiveness (tack) and adhesive strength, and prevents the adhesive from spilling out from the label edge when the label is attached to the adherend 200, and prevents dirt from adhering to the adhesive exposed at the label edge.
[0033] 1.2. Brittle film substrate The brittle film substrate 12 is preferably made of a material that is relatively brittle and easily torn. For example, suitable materials for use include papers such as glassine paper and transparent paper, and sheets made of polyvinyl chloride resin, ABS resin, polyvinyl alcohol resin, acrylic resin, polystyrene resin, polylactic acid resin, cellophane film, and the like.
[0034] The film-forming direction (hereinafter also referred to as machine direction: MD) of the brittle film substrate 12 described below corresponds to the film-forming direction when the brittle film substrate 12 is formed, and also corresponds to the longitudinal direction of the film. The direction at 90° to the film-forming direction of the brittle film substrate 12 (hereinafter also referred to as cross machine direction: CD) corresponds to the direction at 90° to the film-forming direction when the brittle film substrate 12 is formed, and also corresponds to the width direction of the film. A person skilled in the art can easily determine the film formation direction of the brittle film substrate 12 by checking the film properties.
[0035] The brittle film substrate 12 preferably has a tensile breaking elongation of 20% or less, more preferably 1% to 10%, and even more preferably 3% to 7% in the film-forming direction (MD) as measured in accordance with JIS Z0237:2009. When the tensile breaking elongation of the brittle film substrate 12 in the film-forming direction is within the above range, the manufactured label has good brittleness. That is, when a force is applied to the brittle film substrate 12 to peel off the label, the brittle film substrate 12 is not easily stretched, and the brittle film substrate 12 is easily broken.
[0036] The brittle film substrate 12 preferably has a tensile breaking strength in the film-forming direction (MD) measured in accordance with JIS Z0237:2009 of 100 N / 15 mm or less, more preferably 15 N / 15 mm or more and 50 N / 15 mm or less, and even more preferably 28 N / 15 mm or more and 35 N / 15 mm or less. When the tensile breaking strength in the film-forming direction of the brittle film substrate 12 is within the above range, the produced label has good brittleness. That is, when a force is applied to the brittle film substrate 12 in an attempt to peel the label off the adherend, the brittle film substrate 12 becomes easily torn.
[0037] (Thickness of brittle film substrate) The thickness of the brittle film substrate 12 is preferably 10 μm or more and 120 μm or less, more preferably 25 μm or more and 100 μm or less, and even more preferably 40 μm or more and 80 μm or less. This provides the first label 10 with appropriate rigidity. Furthermore, a label manufactured using the first label 10 is suitably prevented from trapping air bubbles or wrinkling when attached to the housing of an office automation device or the like. Furthermore, when the manufactured strip-shaped first label 10 is wound up, lifting between the adhesive and the release liner is reliably prevented.
[0038] In this specification, the "thickness" is a value represented by the average thickness measured at five randomly selected points, and can be obtained using a constant pressure thickness gauge in accordance with JIS K7130. JIS K7130 here is a Japanese Industrial Standard that was created by translating ISO 4593, Plastics-Film and sheeting-Determination of thickness by mechanical scanning without changing the technical content. Here, the thickness of the substrate or layer means the total thickness of the substrate or layer. For example, when the brittle film substrate 12 is composed of multiple layers, the thickness means the total thickness of all layers that make up the main body of the brittle film substrate 12.
[0039] 1.3.Release material As shown in FIG. 5, the first label 10 may have a release material 60 on the first main surface 10a. Examples of the base material for the release material 60 include papers such as fine paper, glassine paper, and craft paper; polyester resin films such as polyethylene terephthalate resin, polybutylene terephthalate resin, and polyethylene naphthalate resin; and plastic films such as olefin resin films such as polypropylene resin and polyethylene resin.
[0040] Examples of release treatment agents for performing release treatment include rubber-based elastomers such as silicone-based resins, olefin-based resins, isoprene-based resins, and butadiene-based resins, long-chain alkyl-based resins, alkyd-based resins, and fluorine-based resins.
[0041] (Thickness of release material) The thickness of the release material 60 is not particularly limited, but is preferably 10 μm or more and 200 μm or less, more preferably 25 μm or more and 170 μm or less, even more preferably 30 μm or more and 125 μm or less, and even more preferably 50 μm or more and 100 μm or less.
[0042] The thickness of the first label 10 excluding the release material 60 can be appropriately selected depending on the purpose, but is preferably 20 μm or more and 200 μm or less, more preferably 60 μm or more and 150 μm or less, and particularly preferably 70 μm or more and 90 μm or less. The thickness of the first label 10 can be measured by the method described below.
[0043] 1.4. First solid printing layer As shown in FIG. 4, the first label 10 may have a first solid print layer 15 on the second label 20 side of the brittle film substrate 12 . Examples of the first solid print layer 15 include those formed using water-based ink, solvent-based ink, and ultraviolet-curable ink. The color of the first solid print layer 15 is preferably different from the color of the second solid print layer 35 described below. The first solid print layer 15 is provided with a second solid print layer 35 on the second label 20 described below, and by making the two different colors, when an attempt is made to peel off the peel detection label 100 and only the second label 20 is peeled off, the color of the label changes before and after the peeling of the second label 20, making it possible to detect that the label has been improperly peeled off. For example, by making the first solid print layer 15 blue and the second solid print layer 35 yellow, the entire peel detection label 120 will be green. When an attempt is made to peel off the peel detection label 120, the second label 20 is peeled off and the blue first label 10 remains on the adherend, causing the color of the entire label to change from green to blue, making it possible to detect that the label has been improperly peeled off. Moreover, the peeled second label 20 exhibits a transparent yellow color specific to the second label 20, and it is clear that the label has been peeled off illegally. Furthermore, the pattern of the pattern layer 32 appears on the second label 20, so that a trace of the peeling remains. The colors of the first solid print layer and the second solid print layer 35 are not limited to those mentioned above, and various combinations are possible.
[0044] 2. Second label As shown in FIG. 1, the second label 20 comprises, from the second main surface 20a side, a support 31, a pattern layer 32 formed on a part of the surface 31a of the support 31, a base layer (Y) 34, and a removable adhesive layer (X) 33, in this order. As shown in Figure 2, when an attempt is made to peel the peel detection label 100 from the substrate 200, the second label 20 is peeled off, and interfacial peeling occurs between the support 31 and the pattern layer 32, resulting in the creation of a gap 40, which causes a pattern to appear on the second label 20, making it possible to visually detect whether the peel detection label 100 has been peeled off from the substrate 200.
[0045] In another embodiment of the second label 20, an adhesive layer (Xn) formed from a composition that is a different material may be laminated on the attachment surface of the removable adhesive layer (X) 33 (not shown). n is an integer of 3 or more. Furthermore, as another embodiment of the second label 20, an intermediate layer (M) (e.g., a primer layer, a metal-based vapor deposition film, a colored layer, etc.) formed from a composition that is a different forming material may be laminated between the base material layer (Y) 34 and the removable adhesive layer (X) 33 (not shown).
[0046] 2.1.Support The support 31 is not particularly limited, but is preferably a support whose surface 32a on the side on which the pattern layer 32 is formed is textured. The textured surface treatment here refers to a process for processing the surface 31a of the support 31 into a surface on which fine irregularities are formed, and a textured surface is generally a rough surface like the surface of a pear. In this specification, the "textured surface" may be a surface with fine irregularities having an irregular shape or a regular shape. It is preferable that the surface 31a of the support 31 on which the pattern layer 32 is formed is a matte-finished surface, since this improves the interfacial adhesion with the base layer (Y) 34 or the removable adhesive layer (X) 33, and more effectively prevents interfacial peeling at these interfaces. Furthermore, for example, when one side of the support 31 is matte-finished, if interfacial peeling occurs between the support 31 and the pattern layer 32, creating a gap 40 in the peeled portion, light is diffusely reflected on the matte surface exposed in the gap 40, and the peeled portion changes from transparent to translucent or opaque before and after peeling, or a matte pattern can be formed. This is preferable because it improves visibility when detecting peeling of the peel detection label 100.
[0047] Therefore, it is preferable that the support 31 has a transparency such that, when the support 31 is incorporated into the peel detection label 100, the support 31 is transparent and any object present on at least the surface 31a side of the support 31 can be visually seen from the second main surface 20a side.
[0048] For these reasons, it is more preferable that the support 31 has transparency that allows the presence or absence of peeling of the peel detection label 100 to be visually detected, and that the surface 31a on the side on which the pattern layer 32 is formed has a matte finish. Specifically, the support 31 preferably has a total light transmittance of 80% or more as measured in accordance with JIS K 7361-1:1997.
[0049] For example, a transparent plastic film is preferably used as the support 31. Examples of materials for the plastic film include acrylic resins such as poly(meth)acrylate; polyamides such as fully aromatic polyamide, nylon 6, nylon 66, and nylon copolymers; polyester resins such as polyethylene terephthalate, polybutylene terephthalate, polyethylene naphthalate, and polyarylate; polyurethane resins such as polyurethane acrylate; polyethylene resins; polypropylene resins; poly(4-methylpentene-1); polyvinyl chloride resins; polyvinylidene chloride resins; polyvinyl alcohol resins; ethylene-vinyl acetate copolymers; polystyrene resins; polycarbonate resins; norbornene resins; and cycloolefin resins. Among these, polyamide and polyester resins are preferred from the viewpoints of transparency, cost, and versatility, and polyethylene terephthalate is more preferred.
[0050] Examples of the matte finish include embossing using an embossing roll having a matte finish, sandblasting (sand matte finish), plasma treatment, chemical etching using a solvent, kneading with transparent fine resin particles, coating with a matte material, etc. Among these, from the viewpoints of cost and versatility, preferred are embossing using an embossing roll having a matte finish or sandblasting, and more preferred is sandblasting. Therefore, as the support 31, a polyamide film or a film made of a polyester resin having a matte finish on the surface 31a of the support 31 on the side on which the pattern layer 32 is formed is more preferable, and a polyethylene terephthalate film having a matte finish on the surface 31a of the support 31 on the side on which the pattern layer 32 is formed is even more preferable.
[0051] The thickness of the support 31 is preferably 1 μm or more and 150 μm or less, more preferably 5 μm or more and 130 μm or less, even more preferably 10 μm or more and 80 μm or less, even more preferably 20 μm or more and 60 μm or less, and even more preferably 30 μm or more and 50 μm or less. The thickness of the support 31 can be measured by the method described below.
[0052] 2.2.Pattern Layer The pattern layer 32 is a layer required to make it possible to visually detect that the second label 20 has been peeled off when the peel detection label 100 is peeled off. The pattern layer 32 is preferably a transparent layer since it is preferable that the pattern is latent before the peeling of the second label 20. By making the pattern layer 32 transparent, the change before and after the peeling of the second label 20 becomes clearer, and when the peeling detection label 100 is affixed to the adherend 200, information such as characters and patterns on the surface of the adherend 200 can be confirmed through the peeling detection label 100, or the peeling detection label itself becomes transparent, making the label less noticeable.
[0053] The pattern layer 32 is not particularly limited, but is preferably a layer formed from a composition containing one or more selected from the group consisting of cellulose-based resins such as methyl cellulose, carboxymethyl cellulose, hydroxyethyl cellulose, etc.; acrylic-based resins such as poly(meth)acrylate, polymethyl (meth)acrylate, etc.; urethane-based resins; acrylic urethane-based resins; polyester-based resins such as polyethylene terephthalate, polybutylene terephthalate, polyethylene naphthalate, polyarylate, etc.; and epoxy-based resins, more preferably a layer formed from a composition containing one or more selected from the group consisting of acrylic resins, urethane-based resins, acrylic urethane-based resins, and polyester-based resins, even more preferably a layer formed from a composition containing one or more selected from the group consisting of acrylic resins and acrylic urethane-based resins, and even more preferably a layer formed from a composition containing an acrylic resin.
[0054] The pattern layer 32 is preferably a layer formed from a resin having an adhesive strength lower than that of the removable adhesive layer (X) 33, and more preferably a layer formed from a non-adhesive resin. Therefore, the layer formed from the composition containing the acrylic resin is preferably a layer formed from an acrylic resin that can form a layer with lower adhesive strength than the resin used in the removable pressure-sensitive adhesive layer (X) 33, among the acrylic resins described below, and is even more preferably a layer formed from a composition containing an acrylic polymer whose main monomer is methyl (meth)acrylate. Here, the "main monomer" refers to the monomer component that is contained (used) in the largest amount among the monomer components that form the polymer.
[0055] Furthermore, when an attempt is made to peel off the peel detection label 100, the second label 20 is peeled off, making interfacial peeling between the support 31 and the pattern layer 32 more likely to occur. Therefore, for example, when the pattern layer 32 is covered with the base material layer (Y) 34, it is preferable that the adhesive strength between the pattern layer 32 and the support 31 is lower than the adhesive strength between the base material layer (Y) 34 and the support 31, and it is more preferable that the adhesive strength between the pattern layer 32 and the support 31 is lower than the adhesive strength between the base material layer (Y) 34 and the support 31, and is also lower than the adhesive strength between the pattern layer 32 and the base material layer (Y) 34. Furthermore, from a similar viewpoint, in the case of a peel detection label 110 as shown in FIG. 3, it is preferable that the adhesive strength between the pattern layer 32 and the support 31 is lower than the adhesive strength between the adhesive layer (X1) 33A and the support 31, and it is more preferable that the adhesive strength between the pattern layer 32 and the support 31 is lower than the adhesive strength between the adhesive layer (X1) 33A and the support 31 and is also lower than the adhesive strength between the pattern layer 32 and the adhesive layer (X1) 33A. Furthermore, in this embodiment, for example, peeling at interfaces other than the interface between the support 31 and the pattern layer 32 can be more effectively prevented.
[0056] In the pattern layer 32, the total content of the aforementioned resins is preferably 50% by mass or more, more preferably 70% by mass or more, even more preferably 80% by mass or more, even more preferably 90% by mass or more, and particularly preferably 100% by mass or less.
[0057] In addition, the pattern layer 32 is formed on a portion of the surface of the support 31 . Here, "formed on a part of the surface of the support 31" means that, in the size of the peel detection label 100 when it is actually affixed, or in the peel detection label 100 after it has been cut out to a predetermined size for use, the area on the surface of the support 31 on which the pattern layer 32 is formed is less than 100%, and is preferably 1% or more and 99% or less, more preferably 2% or more and 95% or less, even more preferably 3% or more and 90% or less, still more preferably 5% or more and 80% or less, still more preferably 8% or more and 70% or less, still more preferably 10% or more and 60% or less, and still more preferably 12% or more and 45% or less.
[0058] The method for forming the pattern layer 32 is not particularly limited as long as it is a method capable of forming the pattern layer 32 on the support 31. For example, it can be formed by a general printing method such as gravure printing, screen printing, offset printing, or flexographic printing using an ink containing a resin and a solvent. Furthermore, the shape of the pattern to be formed is not particularly limited as long as it is possible to detect whether the second label 20 has been peeled off, and it may be a geometric pattern or design, or may be a character pattern. The pattern is not necessarily limited to one "arranged" based on a certain regularity, but also includes irregular (random) shapes. For example, when a specific regular shape is not printed using a printing method, but a pattern layer material is simply sprayed onto a support to form an irregular (random) shape, even if the color tone or light transmittance of the label randomly changes in some places and can be visually recognized, the places formed from the pattern layer material formed on the support 31 are included in the pattern layer 32. However, from the standpoint of manufacturing and product quality, such as more reliably and clearly detecting whether or not the second label 20 has peeled off, and from the standpoint of being able to form a pattern layer 32 suitable for any label size when processed, it is preferable that the interface between the support 31 and the pattern layer 32 exists over a certain area or more, and therefore it is preferable to form a predetermined regular pattern.
[0059] As described above, since the pattern layer itself can form a predetermined pattern, when the pattern layer 32 is a transparent layer, the pattern can be formed as a hidden pattern such as hidden characters. Here, the "hidden pattern" refers to a pattern that is transparent and therefore visible and cannot be visually detected before the second label 20 is peeled off, but becomes visible and visually detectable after the second label 20 is peeled off.
[0060] As described above, the pattern layer 32 used in the present invention has the advantage that the pattern layer 32 itself is peeled off at the interface from the support 31, and therefore it is not necessary to provide layers with separate functions, such as a peeling layer and a printing layer, as the pattern layer 32. Furthermore, by configuring the second label 20 as described above, interfacial peeling can be caused between the support 31 and the pattern layer 32, while interfacial peeling in other locations can be effectively suppressed. Therefore, even if the pattern layer 32 itself forms a relatively intricate pattern, such as letters, it is possible to display the pattern to a degree that can be visually detected when the second label 20 is peeled off.
[0061] The thickness of the pattern layer 32 is preferably less than the thickness of the base layer (Y) 34 when the support 31 is in contact with the base layer (Y) 34 as in Fig. 1, and is preferably less than the thickness of the pressure-sensitive adhesive layer (X1) 33A when in the embodiment of Fig. 3. The thickness of the pattern layer 32 is, for example, preferably 0.05 to 16 µm, more preferably 0.1 to 12 µm, and even more preferably 0.5 to 8 µm. The thickness of the pattern layer 32 can be measured by the method described below.
[0062] 2.3.1. Removable adhesive layer (X) and first adhesive layer (X1) The adhesive of the removable adhesive layer (X) 33 and the first adhesive layer (X1) 33A is not particularly limited, and examples thereof include acrylic adhesives, urethane adhesives, polyisobutylene adhesives, olefin adhesives, acrylic urethane adhesives, polyester adhesives, rubber adhesives, silicone adhesives, and adhesives mainly made of vinyl ether adhesives. These adhesives may be used alone or in combination of two or more. From the viewpoint of further improving the interfacial adhesion between the removable adhesive layer (X) 33, the first adhesive layer (X1) 33A, and the base layer (Y) 34, the removable adhesive layer (X) 33 and the first adhesive layer (X1) 33A are preferably formed from an acrylic resin. Furthermore, the removable pressure-sensitive adhesive layer (X) 33 and the first pressure-sensitive adhesive layer (X1) 33A may contain various known additives, such as a tackifier, a filler, an antioxidant, a heat stabilizer, an ultraviolet absorber, a light stabilizer, a colorant, a flame retardant, and an antistatic agent, as necessary. The removable adhesive layer (X) 33 and the first adhesive layer (X1) 33A may be a single layer or multiple layers. The second label 20 used in the present invention may be, for example, a material disclosed in JP2019 / 039306A.
[0063] In addition, in the case of the configuration of the second label 20 as shown in Fig. 3, it is preferable that the pattern layer 32 and the first adhesive layer (X1) 33A contain the same type of resin, and for example, in the case where the pattern layer 32 is a layer formed of an acrylic resin, it is preferable that the first adhesive layer (X1) 33A is also an acrylic resin described later. By adopting such an embodiment, the interfacial adhesion between the first adhesive layer (X1) 33A and the pattern layer 32 is improved, and when an attempt is made to peel the peel detection label 110 from the adherend 200, the second label 20 is peeled off, and interfacial peeling occurs between the support 31 and the pattern layer 32, generating a gap 40, so that a pattern appears on the second label 20, and it becomes possible to visually detect whether the second label 20 has been peeled off or not.
[0064] (Adhesive strength of removable adhesive layer (X) and adhesive strength of first adhesive layer (X1)) The adhesive strength of the removable pressure-sensitive adhesive layer (X) 33 is preferably 0.1 N / 25 mm or more, more preferably 0.5 N / 25 mm or more, and even more preferably 1.0 N / 25 mm or more. The upper limit of the adhesive strength of the removable pressure-sensitive adhesive layer (X) 33 is not particularly limited, but is preferably 300 N / 25 mm or less, more preferably 20.0 N / 25 mm or less, and even more preferably 10.0 N / 25 mm or less. When the adhesive strength of the removable adhesive layer (X) 33 satisfies the above range, for example, when the second label 20 has a release material, it is preferable because it is possible to more easily realize the function of preventing a pattern from appearing when the peel detection label is peeled off from the release material, and allowing a pattern to appear when the second label 20 is peeled off.
[0065] In the case where the second label 20 has a first adhesive layer (X1) 33A and a removable adhesive layer (X) 33 as shown in Fig. 3, the adhesive strength of the adhesive layer (X1) 33A is preferably 5.0 N / 25 mm or more, more preferably 10.0 N / 25 mm or more. The upper limit of the adhesive strength of the first adhesive layer (X1) 33A is not particularly limited, but is preferably 40.0 N / 25 mm or less, more preferably 30.0 N / 25 mm or less. When the adhesive strength of the first adhesive layer (X1) 33A satisfies the above range, peeling is less likely to occur at the interface between the support and / or pattern layer and the first adhesive layer (X1) 33A when the peel detection label is re-peeled, and the first adhesive layer (X1) 33A itself is less likely to break, which is preferable.
[0066] In addition, in the case where the second label 20 has the first adhesive layer (X1) 33A and the removable adhesive layer (X) 33, the adhesive strength of the first adhesive layer (X1) 33A is preferably equal to or greater than that of the removable adhesive layer (X) 33. By having the adhesive strength of the first adhesive layer (X1) 33A equal to or greater than that of the removable adhesive layer (X) 33, it is possible to more effectively prevent the following problem: "When the second label 20 is peeled off, before the removable adhesive layer (X) 33 is peeled off from the first label 10, peeling occurs at the interface between the support 31 and / or pattern layer 32 and the first adhesive layer (X1) 33A, and the removable adhesive layer (X) 33 remains on the first label 10, causing adhesive residue." This is preferable. In addition, it is preferable that the adhesive strength of the first adhesive layer (X1) 33A is equal to or greater than the adhesive strength of the removable adhesive layer (X) 33, because this more effectively prevents interfacial peeling from occurring in situations other than those originally intended, such as during production or storage, such as punching the second label 20 or winding or unwinding the second label 20 into a roll, and when peeling the peel detection label 100 from the release material 60 immediately before use.
[0067] <Method of measuring adhesive strength> The adhesive strength of the pressure-sensitive adhesive layer (X1) 33A and the removable pressure-sensitive adhesive layer (X) 33 can be measured by the following method. Procedure (1): A 25 μm thick adhesive layer made from the same composition as the adhesive layer to be measured is placed on a 25 μm thick polyethylene terephthalate (PET) film, and a test piece measuring 300 mm long x 25 mm wide is prepared by cutting the film into pieces. Procedure (2): In an environment of 23°C and 50% RH (relative humidity), attach the exposed surface of the adhesive layer of the test piece to a stainless steel plate (SUS304, polished #360) and leave it in the same environment for 24 hours. Step (3): After step (2), measure the adhesive strength of the adhesive layer at a tension speed (peel speed) of 300 mm / min using the 180° peel method based on JIS Z0237:2000 under an environment of 23°C and 50% RH (relative humidity). The measurement result is the adhesive strength of the adhesive layer.
[0068] 2.3.2. Base material layer (Y) The base material layer (Y) 34 used in the second label 20 preferably has an elastic modulus of 10 MPa or more and 800 MPa or less. When the base material layer (Y) 34 satisfies the above requirements, a peel detection label is obtained that does not leave adhesive residue on the first label. In addition, from the viewpoint of achieving both prevention of adhesive transfer onto the first label and better pattern expression, the elastic modulus of the base material layer (Y) 34 is preferably 15 MPa or more, more preferably 18 MPa or more, even more preferably 50 MPa or more, even more preferably 100 MPa or more, even more preferably 200 MPa or more, and is preferably 700 MPa or less, more preferably 600 MPa or less, even more preferably 500 MPa or less, even more preferably 400 MPa or less, and even more preferably 300 MPa or less. In addition, from the viewpoint of obtaining better pattern expression, the base material layer (Y) 34 is preferably a layer having a lower elastic modulus than the support 31, and more preferably a layer having a lower elastic modulus than the support 31 and a higher elastic modulus than the pressure-sensitive adhesive layer (X) 33. When the value of the elastic modulus of the base layer (Y) 34 is 100 MPa or less, it means the value of the storage elastic modulus E' at 23° C. measured by a torsional shear method, and when the value exceeds 100 MPa, it means the value of the storage elastic modulus E' at 23° C. measured by a tensile method. The elastic modulus can be measured by the following method.
[0069] <Method of measuring elastic modulus> The elastic modulus of the base layer (Y) 34 can be measured by the following method. A test sample with a diameter of 8 mm and a thickness of 3 mm is prepared from the same composition as the composition forming the layer to be measured. Using a viscoelasticity measuring device (manufactured by Anton Paar, device name "MCR300"), the storage shear modulus G' of the test sample at 23°C is measured by a torsional shear method under the following conditions: test start temperature: -20°C, test end temperature: 150°C, heating rate: 3°C / min, frequency: 1Hz. The storage modulus E' is calculated from the storage shear modulus G' using the approximate formula "E'=3G'". For samples that cannot be measured using the above-mentioned viscoelasticity measuring device, such as samples with values exceeding 100 MPa, a dynamic viscoelasticity automatic measuring device (manufactured by Orientec Co., Ltd., product name "Leovibron (registered trademark) DDV-01FD") is used to measure the storage modulus E' of the test sample at 23°C using a tensile method under the following conditions: test start temperature: -50°C, test end temperature: 200°C, heating rate: 3°C / min, amplitude: 5μm, frequency: 1Hz, for a test sample formed from the same composition as the composition that forms the layer to be measured and cut to a size of 30 mm in MD x 5 mm in TD x 200μm in thickness.
[0070] The base layer (Y) 34 may be any layer that satisfies the elastic modulus, and for example, among the plastic films described in the section on the support, those that satisfy the elastic modulus can be used as the base layer (Y) 34. From the viewpoints of transparency, cost, and versatility, the base layer (Y) 34 is preferably formed from an acrylic urethane resin, an olefin resin, a polyamide, or a polyester resin.
[0071] The base layer (Y) 34 may contain a colorant. By including a colorant in the base layer (Y) 34, the visibility of the peel detection pattern is further improved, and it becomes easier to detect whether or not the peel detection label has been peeled again.
[0072] The thickness (Xt) of the removable pressure-sensitive adhesive layer (X) 33 is preferably 0.5 μm or more and 50.0 μm or less, more preferably 1.0 μm or more and 30.0 μm or less, even more preferably 2.0 μm or more and 20.0 μm or less, still more preferably 3.0 μm or more and 15.0 μm or less, and even more preferably 4.0 μm or more and 12.0 μm or less.
[0073] The thickness (Yt) of the base layer (Y) 34 is preferably 0.5 μm or more and 50.0 μm or less, more preferably 1.0 μm or more and 30.0 μm or less, even more preferably 2.0 μm or more and 20.0 μm or less, still more preferably 2.5 μm or more and 15.0 μm or less, and even more preferably 3.0 μm or more and 12.0 μm or less.
[0074] 2.4. Second solid printing layer The second label 20 may have a second solid print layer 35 between the support 31 and the removable adhesive layer (X) 33, as shown in FIG. The second solid print layer 35, like the first solid print layer 15, may be formed from a water-based ink, a solvent-based ink, or an ultraviolet-curable ink. When the peel detection label 120 is affixed to the adherend 200, it is preferable that the peel detection label has a transparency that allows at least the changes due to interfacial peeling to be visually recognized from the support 31 side of the peel detection label 120, and it is more preferable that the peel detection label has a transparency that allows the information on the adherend 200 to be visually recognized. That is, it is more preferable that any object present on the other surface side of the first label 10 be visible from the surface (second main surface 20a) of the second label 20 facing the support 31.
[0075] 2.5.Printed Coating Layer The second label 20 may have a printed coating layer 50 on the outermost surface, as shown in Fig. 5. The printed coating layer 50 preferably contains a polyester resin or an acrylic resin. The print coat layer 50 can be formed in the desired area by applying a printing coating agent containing each of the components that make up the print coat layer 50 and a dilution medium to the surface on which the print coat layer 50 is to be formed, and then drying it as necessary to volatilize the dilution medium. The amount of the printing coating agent applied to the second label 20 is preferably such that the thickness of the printing coating layer 50 after drying is 0.05 μm or more and 9 μm or less, more preferably 0.5 μm or more and 7 μm or less, and even more preferably 2 μm or more and 5 μm or less.
[0076] The thickness of the second label 20 is preferably 5 μm or more and 150 μm or less, more preferably 10 μm or more and 100 μm or less, even more preferably 20 μm or more and 80 μm or less, and even more preferably 30 μm or more and 70 μm or less. The thickness of the second label 20 can be measured by the method described below.
[0077] [Manufacturing method of peel detection labels] There is no particular limitation on the method for producing the peel detection label. As an example, the peel detection label of the present invention can be produced by producing the first label 10 and the second label 20 by a known method, respectively, and laminating them.
[0078] [Use of peel detection labels] The peeling detection label of the present invention can be used, for example, as a label to prevent tampering with the display content of automobile parts, electrical and electronic parts, precision machinery parts, etc.; to prevent improper packaging or opening of goods when they are consigned or packaged; a sealing label to guarantee the virginity of the contents of medicines, cosmetics, food, etc.; to prevent improper opening and closing of various openings on various passenger cars, airplanes, trains, ships, etc. (for example, to prevent the improper introduction of foreign objects into transport entrances or fuel tanks, etc.); to prevent peeling or tampering with identification or certification labels on various certificates such as passports and product certifications; and as a security measure to prevent improper intrusion into various passenger cars, airplanes, trains, ships, etc. and into various buildings.
[0079] [Peeling detection method] The peel detection method of the present invention is a method for detecting peeling of a peel detection label. As described above, referring to FIG. 1, a peel detection label 100 comprises a first label 10 and a second label 20 provided on the first label 10, with a surface 10a on the first label 10 side constituting a first main surface and a surface 20a on the second label 20 side constituting a second main surface, the first label 10 comprising, from the first main surface 10a side, a permanent adhesive type pressure-sensitive adhesive layer 11 and a brittle film substrate 12 in this order, and the second label 20 comprising, from the second main surface 20a side, a support 31, a palladium film formed on a part of a surface 31a of the support 31, and a palladium film formed on a part of a surface 31a of the support 31. The peel detection label 100 comprises, in this order, a turn layer 32, a base material layer (Y) 34, and a removable adhesive layer (X) 33. The first main surface 10a of the first label 10 is affixed to an adherend 200, and when an attempt is made to peel the peel detection label 100, only the second label 20 is peeled off, and before and after the peeling of the second label 20, the pattern of the pattern layer 32 appears in the second label 20, while the first label 10 remains on the adherend 200, thereby detecting the unauthorized peeling of the peel detection label.
[0080] In addition, it is preferable that the peeling detection method of the present invention is a method for detecting unauthorized peeling of the peeling detection label 100 by the emergence of colors unique to the first label 10 and the second label 20 from the color of the entire peeling detection label 100 before and after the peeling of the second label 20. The peeling detection method of the present invention, having the above-mentioned configuration, has a double peeling detection function with first label 10 and first label 20, and has an excellent effect of preventing tampering and unauthorized opening. EXAMPLES
[0081] The present invention will be described below with reference to examples and comparative examples. In the examples, the term "parts" or "%" may be used, but unless otherwise specified, it means "parts by mass" or "% by mass". Furthermore, unless otherwise specified, each operation is carried out at room temperature (25°C).
[0082] [First label] The first label used in the examples and comparative examples is described below.
[0083] [Label 1 (fragile label)] An adhesive product (manufactured by Lintec Corporation, product name "FP1102B PAT1 11HLDF") that has a permanent adhesive layer and a brittle film substrate (polyvinyl chloride film (white) 50 μm) in that order, adhesive strength: 15.5 N / 25 mm
[0084] [Label 2 (easily destructible label)] An adhesive product (manufactured by Lintec Corporation, product name "TE80WPAT1 8K") that has a permanent adhesive layer and a destructible film base material (special polypropylene film (white) 80μm) in that order, adhesive strength: 15.5N / 25mm
[0085] [Second label] The second labels used in the examples and comparative examples are described below.
[0086] [Label 3] An adhesive product having a support and a removable adhesive layer in that order (manufactured by Lintec Corporation, product name "RE5054"), adhesive strength: 9.4 N / 25 mm, no letter pattern layer.
[0087] [Label 4] An adhesive product (manufactured by Lintec Corporation, product name "RE505S") having a support and a removable adhesive layer in that order, adhesive strength: 0.1 N / 25 mm, no letter pattern layer.
[0088] [Label 5] An adhesive product (manufactured by Lintec Corporation, product name "TP Seal B (NT) VOID") that includes, in this order, a support, a pattern layer formed on a portion of the surface of the support, a second solid print layer (blue), a base layer, and a removable adhesive layer. Adhesive strength: 3.6 N / 25 mm
[0089] [Label 6] An adhesive product (manufactured by Lintec Corporation, product name "TP Seal R (NT) VOID") that includes, in this order, a support, a pattern layer formed on a portion of the surface of the support, a second solid print layer (red), a base layer, and a removable adhesive layer. Adhesive strength: 3.6 N / 25 mm
[0090] [Label 7] Lintec tamper-proof label, character transfer type, product name "TE Keshi 50 VOID PAT1 8LK", adhesive strength: 11.0N / 25mm
[0091] [Examples 1 to 3 and Comparisons 1 to 7] A peel detection label was produced by bonding the first label and the second label in the combination shown in Table 1. In Example 1, a first solid print layer (yellow) was applied on the brittle film substrate of label 1.
[0092] [evaluation] The following evaluations were carried out for the above-mentioned Examples and Comparative Examples. Table 1 shows the evaluation results.
[0093] (Color before removing the second label) The color of the peel detection label before the second label was peeled off was visually judged from above.
[0094] (Color after removing the second label) After the second label was removed, the color was visually judged from above.
[0095] (Ease of detecting label removal: color change) When the label was peeled off, a change in color occurred and it was judged by visual inspection whether peeling was easily detected. <Evaluation criteria for color change> A: There was a change in color and it was easy to detect. B: There was no change in color and it was difficult to detect.
[0096] (Traces of peeling off the second label: Visibility of characters) When the second label was peeled off, a visual inspection was performed to determine whether any traces, such as letters standing out, remained on the base material. <Evaluation criteria for character expression> A: Traces such as embossed letters remained. B: No trace was left.
[0097] (Difficulty of removing the first label: security) It was determined whether the first label could be removed from the substrate. <Security evaluation criteria> A: The first label was difficult to remove. B: The first label was easily removed.
[0098] [Table 1]
[0099] Examples 1 to 3, which used the first label having a brittle film substrate, were good in all evaluation items. On the other hand, in Comparative Examples 1 and 2, labels 5 and 6 were used as the second labels, which reveal characters when peeled off, but a destructible label was used as the first label. Therefore, when attempting to peel off the entire label, the base material of the first label was destroyed and the characters did not reveal themselves. In Comparative Examples 3 to 6, a white brittle film and a fragile label were used for the first label, and a transparent label was used for the second label, so there was no color change. In addition, the second labels, Labels 3 and 4, were labels without character patterns, so no characters were visible. However, because the first label was made of a brittle film or a fragile label, it was not easy to peel off the first label, so security was maintained. In Comparative Example 7, a transfer-type label in which characters are transferred to an adherend is used as the second label. In other words, the adhesive strength of the second label was so high that the second label alone could not be peeled off. [Explanation of symbols]
[0100] 10 First Label 10a: Surface of first label (first main surface) 11 Permanent adhesive layer 12 Brittle film substrate 15 1st solid printing layer 20 Second Label 20a: Surface (second main surface) of second label 20 31 Support 31a Surface of the support 32 Pattern Layer 32a Pattern layer surface 33 Removable adhesive layer (X) 33A Adhesive layer (X1) 34 Base material layer (Y) 35 Second solid printing layer 40 void 50 Printing Coat Layers 60 Release material 100, 110, 120 Peel detection label 200 Adherent
Claims
1. A peel detection label, A packaging material according to the present invention includes a first label and a second label provided on the first label, the surface of the first label side being a first main surface and the surface of the second label side being a second main surface, The first label includes, from the first main surface side, a permanent adhesive type pressure-sensitive adhesive layer and a brittle film substrate in this order, A peel detection label in which the second label comprises, from the second main surface side, at least a support, a pattern layer formed on a portion of the surface of the support, a base material layer (Y), and a removable adhesive layer (X), in that order.
2. The peel detection label according to claim 1, wherein the brittle film substrate has a tensile breaking elongation of 20% or less in the film formation direction (MD) as measured in accordance with JIS Z0237:2009.
3. The peel detection label according to claim 1, wherein the brittle film substrate has a tensile breaking strength of 100 N / 15 mm or less in the film formation direction (MD) as measured in accordance with JIS Z0237:2009.
4. The adhesive strength of the permanent adhesive layer is 5 N / 25 mm or more and 40.0 N / 25 mm or less, The adhesive strength of the removable pressure-sensitive adhesive layer (X) is 0.1 N / 25 mm or more and 30.0 N / 25 mm or less, 2. The peel detection label according to claim 1, wherein the adhesive strength of the permanent adhesive layer is greater than the adhesive strength of the removable adhesive layer (X).
5. the second label has a first pressure-sensitive adhesive layer between the pattern layer and the base layer (Y), The adhesive strength of the permanent adhesive layer is 5 N / 25 mm or more and 40.0 N / 25 mm or less, The adhesive strength of the removable pressure-sensitive adhesive layer (X) is 0.1 N / 25 mm or more and 30.0 N / 25 mm or less, The peel detection label of claim 1, wherein the adhesive strength of the permanent adhesive layer is greater than the adhesive strength of the removable adhesive layer (X), and the adhesive strength of the first adhesive layer is greater than the adhesive strength of the removable adhesive layer (X).
6. The first label has a first solid print layer on the second label side of the brittle film substrate, The peel detection label according to claim 1, wherein the second label has a second solid print layer between the support and the removable adhesive layer (X).
7. The peel detection label according to claim 1 , further comprising a release material on the first main surface side of the first label.
8. The peel detection label according to claim 1 , further comprising a print coating layer on the second main surface side of the second label.
9. A method for detecting that a peel detection label has been peeled, comprising the steps of: the peel detection label comprises a first label and a second label provided on the first label, a surface of the first label side constitutes a first main surface, and a surface of the second label side constitutes a second main surface; The first label includes, from the first main surface side, a permanent adhesive type pressure-sensitive adhesive layer and a brittle film substrate in this order, the second label comprises, from the second main surface side, a support, a pattern layer formed on a part of the surface of the support, a base layer (Y), and a removable pressure-sensitive adhesive layer (X), in this order; The peel detection label is attached to an adherend by the first main surface of the first label, When an attempt is made to peel off the peel detection label, only the second label is peeled off, and the pattern of the pattern layer appears in the second label before and after the peeling of the second label, while the first label remains on the substrate, thereby detecting the unauthorized peeling of the peel detection label.
10. The peel detection method according to claim 9, wherein the unauthorized peeling of the peel detection label is detected by the emergence of colors unique to the first label and the second label from the color of the entire peel detection label before and after the second label is peeled off.