Pattern forming apparatus and pattern forming method
The pattern forming apparatus and method address residual film issues by using a mold roll with light shielding to prevent curing, enabling easy uncured resin removal and reducing manufacturing complexity and costs.
Patent Information
- Application Number
- JP2023064508
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-11
- Publication Date
- 2024-10-24
AI Technical Summary
Existing pattern forming methods result in residual films on base materials due to the curing of resin between the transfer roll and the base material, requiring time-consuming and costly ashing processes to remove.
A pattern forming apparatus and method that includes a mold roll with a light shielding portion at the tip of its convex parts to prevent curing of resin between the mold roll and the base material, allowing for easy removal of uncured resin, thereby reducing residual films.
The apparatus effectively suppresses the formation of residual films by ensuring uncured resin can be easily removed, reducing manufacturing steps and costs by eliminating the need for ashing processes.
Smart Images

Figure 2024151261000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a pattern forming apparatus and a pattern forming method. [Background technology]
[0002] Patent Document 1 discloses an imprinting technology for forming a pattern on the surface of a substrate, which includes a coating step of coating a resin material on a film substrate to form a coating film, and a transfer step of pressing a transfer roll against the coating film of the resin material formed on the substrate to transfer the concave-convex pattern of the transfer roll to the coating film and curing the coating film. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2015-85659 A Summary of the Invention [Problem to be solved by the invention]
[0004] The pattern forming method disclosed in Patent Document 1 is configured to transfer a pattern to a substrate by pressing a transfer roll against a film of a roughness-forming material (curable resin) that has been applied to the substrate in advance, causing the curable resin to flow. As a result, a residual film is generated when the resin material sandwiched between the convex parts of the transfer roll and the substrate remains on the substrate in a cured state. When a residual film is generated, an ashing process or the like is required to remove the residual film, which requires a lot of labor and costs. Therefore, in imprint technology, it is desirable to reduce the residual film.
[0005] The present invention has been made in consideration of the above problems, and has an object to provide a pattern forming apparatus and a pattern forming method that can reduce the amount of film remaining on a substrate. [Means for solving the problem]
[0006] According to one aspect of the present invention, a pattern forming apparatus includes a conveying section having a pay-out roll that pays out a substrate and a take-up roll that takes up the substrate, a resin supplying section that supplies a curable resin to the surface of the substrate conveyed by the conveying section, a mold roll having recesses and protrusions that constitute a pattern formed on its outer periphery and that transfers a pattern to the substrate by contacting the surface of the substrate to which the curable resin has been supplied, a curing section that is provided inside the mold roll and irradiates the substrate with light through the mold roll to cure the curable resin, and a removal section that removes from the substrate any curable resin remaining in an uncured state, and a light-shielding section that blocks light is provided at the tip of the protrusions of the mold roll.
[0007] According to one aspect of the present invention, the pattern forming method includes a supplying step of supplying a curable resin onto the surface of the substrate transported from a pay-out roll to a take-up roll; a transfer step of rotating a mold roll having recesses and protrusions on its outer periphery that constitute a pattern, and sequentially pressing the mold roll against the surface of the substrate to transfer the pattern to the substrate; a curing step of irradiating light through the mold roll toward the curable resin on the substrate against which the mold roll is pressed, thereby curing the curable resin on the substrate; and a removal step of removing the curable resin remaining in an uncured state on the substrate from the substrate, wherein in the curing step, a light-shielding portion provided at the tip of the protrusion of the mold roll blocks light irradiation of the curable resin against which the protrusion is pressed. Effect of the Invention
[0008] According to these aspects, since the light-shielding portion is provided at the tip of the convex portion, even if the curable resin remains between the convex portion of the mold roll and the substrate when the pattern is transferred, the light irradiated from the inside of the mold roll is blocked by the light-shielding portion and is not irradiated to the curable resin. Therefore, the curable resin between the convex portion of the mold roll and the substrate remains on the substrate in an uncured state. Since the uncured curable resin can be easily removed compared to the cured state, the generation of a residual film on the substrate can be suppressed by removing the uncured curable resin on the substrate. [Brief description of the drawings]
[0009] [Figure 1] 1 is a configuration diagram of a pattern forming device according to a first embodiment of the present invention. [Diagram 2] 1 is a block diagram of a pattern forming device according to a first embodiment of the present invention. [Diagram 3] 2 is an enlarged view showing the periphery of a convex portion of a mold roll of the pattern forming device according to the first embodiment of the present invention. FIG. [Figure 4] 5A to 5C are diagrams illustrating a procedure of a first method for forming a light-shielding portion according to the first embodiment of the present invention. [Diagram 5] 5A to 5C are diagrams illustrating a procedure of a second method for forming a light-shielding portion according to the first embodiment of the present invention. [Figure 6] FIG. 4 is a configuration diagram showing a first modified example of a removal unit according to the first embodiment of the present invention. [Figure 7] FIG. 11 is a configuration diagram showing a second modified example of the removal unit according to the first embodiment of the present invention. [Figure 8] FIG. 5 is a configuration diagram of a pattern forming device according to a second embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] (First embodiment) Hereinafter, a pattern forming device 100 and a pattern forming method according to a first embodiment of the present invention will be described with reference to the drawings. Note that in each drawing, the scale of each component is appropriately changed for convenience of explanation, and is not necessarily strictly illustrated.
[0011] First, the configuration of a pattern forming apparatus 100 will be described with reference to FIG.
[0012] As shown in Fig. 1, the pattern forming apparatus 100 is of the so-called roll-to-roll type, and is an apparatus that forms a pattern 2 with an ultraviolet (UV) curable resin (hereinafter also simply referred to as "resin") 5 on one surface (film surface) of a base film 1 as a sheet-like substrate. In the following, the pattern forming apparatus 100 will be described assuming that the up-down direction in Fig. 1 is the vertical direction. In the following description, unless otherwise specified, "up" and "down" refer to up and down in the vertical direction, that is, the up-down direction in the drawing.
[0013] The base film 1 is a resin film having a flat film surface that is continuous over a predetermined length. In the following, the base film 1 integrated with the resin 5 that forms the pattern 2 is also referred to as a "pattern film 3."
[0014] As shown in FIG. 1, the pattern forming apparatus 100 includes a conveying section 10 that conveys the base film 1 in the longitudinal direction, a mold roll 20 having recesses 21 and protrusions 22 formed on its outer periphery that constitute a predetermined pattern 2, an electric motor 23 as a drive section that drives the mold roll 20 to rotate, a pressing roll 25 into which the base film 1 is inserted between the mold roll 20, a peeling roll 26 that peels the pattern film 3 from the mold roll 20, a coating die 30 as a resin supplying section that supplies resin 5 to the film surface of the base film 1, a lamp 35 as a curing section that is supplied to the recesses 21 of the mold roll 20 and hardens the resin 5 on the base film 1 as the mold roll 20 rotates, thereby integrating it with the base film 1, and a controller 70 (see FIG. 2) that controls the pattern forming apparatus 100.
[0015] The conveying section 10 has a pay-out roll 11 that pays out the base film 1, a take-up roll 12 that winds up the base film 1 paid out from the pay-out roll 11, and a number of guide rolls 13 that support the base film 1 being conveyed between the pay-out roll 11 and the take-up roll 12.
[0016] The payout roll 11 and the take-up roll 12 are each driven to rotate around a central axis by an electric motor (not shown) (see the arrow in the figure). The central axis of the payout roll 11 and the central axis of the take-up roll 12 are arranged parallel to each other. The base film 1 paid out from the payout roll 11 is wound by the take-up roll 12, so that the base film 1 is transported in the longitudinal direction between the payout roll 11 and the take-up roll 12. The electric motor that rotates the payout roll 11 and the take-up roll 12 is controlled by a controller 70 so as to transport the base film 1 at a constant speed while applying a predetermined tension so as not to cause bending. In the following description, the payout roll 11 side is referred to as the "upstream" in the transport direction, and the take-up roll 12 side is referred to as the "downstream" in the transport direction.
[0017] The base film 1 transported between the pay-out roll 11 and the take-up roll 12 is wound around the multiple guide rolls 13. The multiple guide rolls 13 are rotated in accordance with the transport of the base film 1. A transport path for the base film 1 is formed by the multiple guide rolls 13.
[0018] The central axis of the mold roll 20 is set parallel to the central axes of the pay-out roll 11 and the take-up roll 12. Recesses 21 and protrusions 22 constituting the pattern 2 to be molded in the base film 1 are formed on the cylindrical outer circumferential surface of the mold roll 20. The base film 1 transported from the pay-out roll 11 to the take-up roll 12 is wound around the lower part of the mold roll 20.
[0019] The mold roll 20 is formed of a material having light transmission (translucency), more specifically, ultraviolet transmission. The mold roll 20 is formed with an accommodation hole 20a for accommodating a lamp 35. Light (ultraviolet rays) emitted by the lamp 35 provided inside the mold roll 20 passes through the mold roll 20 and is irradiated from the inside to the outside of the mold roll 20.
[0020] As shown in Fig. 3, a recessed portion 22a recessed toward the inside in the radial direction of the mold roll 20 (upper side in Fig. 3) is formed at the tip of the protruding portion 22 of the mold roll 20. The recessed portion 22a is formed over the entire area of the protruding portion 22 in the axial direction of the mold roll 20. The recessed portion 22a is also formed over the entire area of the protruding portion 22 in the circumferential direction of the mold roll 20.
[0021] A light-shielding portion 24 having a light-shielding property for blocking light irradiated by a lamp 35 is provided in the recess 22a of the protrusion 22. The light-shielding portion 24 blocks ultraviolet light from the lamp 35 to the resin 5 sandwiched between the tip of the protrusion 22 and the base film 1.
[0022] The light-shielding portion 24 is formed by applying (filling) a raw material such as silver (Ag) nano-ink or silver paste into the recessed portion 22a formed in the protruding portion 22 of the mold roll 20 and then solidifying it to be integrated with the mold roll 20 as a solid film.
[0023] The recessed portion 22a is formed in a substantially semicircular shape (cone-shaped) in a cross section perpendicular to the central axis of the mold roll 20. In other words, the recessed portion 22a is formed by a curved surface. As a result, even if a force (shear force) in the circumferential direction (left and right direction in FIG. 3) of the mold roll 20 acts on the light-shielding portion 24 when the roll cleaning unit 50 described later wipes off the resin 5, the shear force is dispersed by the curved surface. Therefore, according to this embodiment, it is possible to suppress the detachment of the light-shielding portion 24 from the recessed portion 22a, compared to a case where the tip of the protrusion 22 is flat without the recessed portion 22a. Note that the recessed portion 22a is not essential, and the tip of the protrusion 22 may be formed substantially flat without the recessed portion 22a.
[0024] 4 and 5, a method for forming the light shielding portion 24 will be described. For example, the light shielding portion 24 can be formed by a first method shown in FIG. 4 or a second method shown in FIG.
[0025] In the first method shown in Fig. 4, first, raw material M1 of the light-shielding portion 24 is applied to a base member B1 such as a film (Fig. 4(a)). Next, the protrusions 22 at the tip of a mold roll 20 on which a pattern has been formed in advance are brought into contact with the raw material M1 applied to the base member B1, and the raw material M1 is adhered to the protrusions 22 (Fig. 4(b)). Then, the raw material M1 at the tip of the protrusions 22 is dried or baked to solidify, forming the light-shielding portion 24 fixed to the tip of the mold roll 20 (Fig. 4(c)).
[0026] In the second method shown in FIG. 5, the light shielding portion 24 is formed together with the mold roll 20. Specifically, as shown in FIG. 5(a), a raw material M1 of the light shielding portion 24 is provided only on the bottom of the recess of a mold type Mo (for example, a Ni electroforming mold type) on which a pattern corresponding to the pattern of the mold roll 20 is formed. Then, a roll raw material M2, which is an ultraviolet curing resin constituting the mold roll 20, is applied to a roll base member B2 (for example, a film) which is the base of the mold roll 20 (FIG. 5(b)), and the roll raw material M2 is pressed against the mold type Mo to transfer the pattern (FIG. 5(c)). In this state, the roll raw material M2 is irradiated with ultraviolet light to be cured, and the mold roll 20 is formed. As the roll raw material M2 is cured to form the mold roll 20, the raw material M1 at the bottom of the recess of the mold type Mo is fixed to the mold roll 20. Then, the mold roll 20 is released from the mold die Mo, and the raw material M1 attached to the tip of the convex portion 22 of the mold roll 20 is dried or baked (FIG. 5(d)). As the raw material M1 solidifies, the light-shielding portion 24 is fixed to the tip of the mold roll 20. In this method, the adhesion of the light-shielding portion 24 to the raw material M1 increases when the mold roll 20 is cured by ultraviolet light, so that the light-shielding portion 24 is less likely to come off the mold roll 20, and the durability of the light-shielding portion 24 can be increased.
[0027] By the method as described above, the light-shielding portion 24 can be formed at the tip of the mold roll 20. Note that the method for forming the light-shielding portion 24 is not limited to the above, and it can be formed by any method.
[0028] As shown in Fig. 1, the electric motor 23 drives the mold roll 20 to rotate around the central axis. The electric motor 23 is controlled by the controller 70 so that the rotation speed of the mold roll 20 is synchronized with the conveying speed of the base film 1 by the conveying unit 10. The electric motor 23 rotates the mold roll 20, thereby sequentially bringing the convex portions 22 and concave portions 21 on the outer periphery of the mold roll 20 into contact with the film surface of the base film 1. As a result, the pattern on the outer periphery of the mold roll 20 is transferred to the resin 5 on the film surface of the base film 1.
[0029] The pressing roll 25 is provided adjacent to the mold roll 20 so that its central axis is parallel to that of the mold roll 20. The pressing roll 25 is provided rotatably about its central axis, and the base film 1 located on the upstream side of the mold roll 20 is wound around its outer circumferential surface. The base film 1 is inserted between the pressing roll 25 and the mold roll 20, and the outer circumferential surface of the pressing roll 25 faces the outer circumferential surface of the mold roll 20 with the base film 1 sandwiched between them. Therefore, the pressing roll 25 rotates freely due to the transport (movement) of the base film 1 wound around it.
[0030] The pressing roll 25 is configured to move forward and backward with respect to the mold roll 20 by an actuator (not shown). That is, the distance between the central axes of the pressing roll 25 and the mold roll 20 can be adjusted by the actuator. In this embodiment, the pressing roll 25 can be moved in the left-right direction in FIG. 1 by the actuator. This allows the adhesion force of the mold roll 20 to the base film 1 to be adjusted. The operation of the actuator is controlled by a controller 70.
[0031] The peeling roll 26 is provided adjacent to the mold roll 20 so that its central axis is parallel to that of the mold roll 20. The peeling roll 26 is provided rotatably about its central axis, and the base film 1 located downstream of the mold roll 20 is wound around its outer circumferential surface. The base film 1 is inserted between the peeling roll 26 and the mold roll 20, and the outer circumferential surface of the peeling roll 26 faces the outer circumferential surface of the mold roll 20 with the base film 1 sandwiched between them. The peeling roll 26 rotates freely due to the transport (movement) of the base film 1 around which it is wound.
[0032] The peeling roll 26 is configured to move forward and backward with respect to the mold roll 20 by an actuator (not shown). That is, the distance between the central axes of the peeling roll 26 and the mold roll 20 can be adjusted by the actuator. In this embodiment, the peeling roll 26 can be moved in the left-right direction in FIG. 1 by the actuator. The pattern film 3 is guided by the peeling roll 26 and peeled off from the mold roll 20 together with the resin 5.
[0033] The lamp 35 is a light source capable of emitting ultraviolet rays, and for example, an LED lamp is used. The operation of the lamp 35 is controlled by the controller 70. The lamp 35 is provided in the mold roll 20 so as to emit ultraviolet rays toward the contact portion between the mold roll 20 and the base film 1 (the lower part of the mold roll 20 in FIG. 1). The ultraviolet rays emitted from the lamp 35 are irradiated through the mold roll 20 having translucency to the resin 5 on the base film 1 to which the convex portions 22 and the concave portions 21 of the mold roll 20 are transferred. As a result, the resin 5 on the base film 1 is cured and integrated (fixed) with the base film 1. The lamp 35 is not limited to an LED lamp, and may be any other lamp capable of emitting ultraviolet rays.
[0034] The coating die 30 is disposed at a position upstream of the mold roll 20 where the resin 5 can be coated onto the base film 1. The coating die 30 ejects uncured resin 5 to be supplied onto the film surface of the base film 1, forming a film of the resin 5 on the film surface of the base film 1. Since the coating die 30 can have a known configuration, detailed illustrations and specific descriptions are omitted. The operation of the coating die 30 is controlled by a controller 70.
[0035] In addition, the pattern forming apparatus 100 further includes a removal section 40 that removes the resin 5 remaining in an uncured state on the pattern film 3 from the pattern film 3, and a roll cleaning section 50 that removes the uncured resin 5 adhering to the convex portions 22 of the mold roll 20 that have transferred the pattern to the surface of the base film 1 from the mold roll 20.
[0036] The removal section 40 has a storage section 41 that stores cleaning liquid L in which the pattern film 3 is immersed, an air knife 43 that blows air onto the pattern film 3 that has been immersed in the cleaning liquid L in the storage section 41 and removed from the storage section 41, and a drying section 44 that dries the pattern film 3 that has been blown with air by the air knife 43.
[0037] The conveying path of the pattern film 3 is formed by the guide roll 13 so that the pattern film 3 is immersed in the cleaning liquid L in the reservoir 41 after the resin 5 is fixed. The cleaning liquid L stored in the reservoir 41 is water or a solvent. Examples of the solvent that can be used include hydrocarbon solvents (cyclohexane, etc.), glycol ether solvents (PGME, etc.), alcohol solvents (ethanol, IPA, etc.), ketone solvents (acetone, MEK, MIBK, etc.), and ester solvents (methyl acetate, ethyl acetate, etc.). By immersing the pattern film 3 with the uncured resin 5 remaining in the cleaning liquid L, the uncured resin 5 is dissolved in the cleaning liquid L and removed, or can be softened by the cleaning liquid L. By softening the uncured resin 5, it becomes easier to remove the resin 5 using the air knife 43 later.
[0038] The air knife 43 is a nozzle that ejects compressed air supplied from a gas supply source (not shown). In this embodiment, a pair of air knives 43 are provided to sandwich the base film 1. This allows air to be sprayed onto both the front and back sides of the base film 1. By spraying air from the air knife 43 onto the pattern film 3 after it has been immersed in the cleaning liquid L in the reservoir 41, the resin 5 remaining on the base film 1 and the cleaning liquid L adhering to the base film 1 are removed. The number and positions of the air knives 43 are not limited to those in this embodiment. For example, two or more pairs of air knives 43 may be provided.
[0039] The drying section 44 is a drying furnace that evaporates the cleaning liquid L on the base film 1 that has not been completely removed by the air knife 43. The drying section 44 has a heating chamber (not shown) in which the interior atmosphere is heated, and evaporates and removes the cleaning liquid L by passing the base film 1 through it. Alternatively, the drying section 44 may be configured to blow heated air onto the base film 1 to remove the cleaning liquid L. Also, the drying section 44 does not have to be provided.
[0040] The roll cleaning section 50 has a sheet-shaped roll cleaner 51 that sequentially contacts the convex portions 22 of the mold roll 20 as the mold roll 20 rotates, a nip roll 52 around which the roll cleaner 51 is wrapped, and a cleaner pay-out roll 53 and a cleaner take-up roll 54 that transport the roll cleaner 51.
[0041] The roll cleaner 51 is a sheet-like nonwoven fabric extending in the longitudinal direction. The width of the roll cleaner 51 is set to be equal to or greater than the width (dimension in the axial direction) of the mold roll 20.
[0042] The nip roll 52 faces the mold roll 20 with the roll cleaner 51 in between, and is provided so as to sandwich the roll cleaner 51 together with the mold roll 20. The roll cleaner 51 is wrapped around the nip roll 52, so that the convex parts 22 of the mold roll 20 come into contact with the roll cleaner 51 as it rotates. As a result, the resin 5 that is pressed against the uncured resin 5 and adheres to the convex parts 22 of the mold roll 20 can be wiped off (removed) by the roll cleaner 51.
[0043] The cleaner pay-out roll 53 and the cleaner take-up roll 54 are each driven to rotate about a central axis by an electric motor (not shown), similar to the pay-out roll 11 and the take-up roll 12 in the transport section 10. The central axis of the cleaner pay-out roll 53 and the central axis of the cleaner take-up roll 54 are parallel to each other and are provided parallel to the pay-out roll 11 and the take-up roll 12. By taking up the roll cleaner 51 paid out from the cleaner pay-out roll 53 by the cleaner take-up roll 54, the contact portion (contact surface) of the roll cleaner 51 that comes into contact with the mold roll 20 is renewed. This makes it possible to suppress a decrease in the performance of the roll cleaner 51 in removing the resin 5.
[0044] The cleaner pay-out roll 53 and the cleaner take-up roll 54 are controlled by the controller 70 so as not to cause bending of the roll cleaner 51. The cleaner pay-out roll 53 and the cleaner take-up roll 54 may be controlled so as to transport the roll cleaner 51 continuously, or may be controlled so as to repeatedly transport and stop (transport intermittently).
[0045] In this embodiment, the conveying direction of the roll cleaner 51 is along the rotation direction of the mold roll 20. If the roll cleaner 51 is conveyed in a direction against the rotation direction of the mold roll 20, the roll cleaner 51 is likely to wear out due to friction with the mold roll 20 during conveyance. In this case, the motor capacity of the electric motor that drives the pay-out roll 11 and the take-up roll 12 must also be increased. By making the conveying direction of the roll cleaner 51 along the rotation direction of the mold roll 20, wear on the roll cleaner 51 can be suppressed and the motor capacity of the electric motor can be suppressed.
[0046] The nip roll 52 is provided so that its central axis is parallel to the cleaner pay-out roll 53 and the cleaner take-up roll 54. The nip roll 52 is rotated in accordance with the conveyance of the roll cleaner 51.
[0047] The controller 70 is composed of a microcomputer equipped with a CPU (Central Processing Unit), a ROM (Read Only Memory), a RAM (Random Access Memory), and an I / O interface (Input / Output Interface). The RAM stores data for CPU processing, the ROM stores control programs and the like for the CPU in advance, and the I / O interface is used for inputting and outputting information to and from connected devices. The controller 70 may be composed of multiple microcomputers. The controller 70 is programmed to be capable of executing at least the processes required for executing the control according to each embodiment and modified example. The controller 70 may be configured as a single device, or may be divided into multiple devices and configured to distribute the processes of each control among the multiple devices.
[0048] The controller 70 controls the operation of each component of the pattern forming device 100 so as to enable the pattern forming method described below to be performed.
[0049] Next, a pattern forming method executed by the pattern forming apparatus 100 will be described.
[0050] The pattern forming method according to the present embodiment includes a supplying step of supplying resin 5 to the surface of the base film 1 being transported from the pay-out roll 11 to the take-up roll 12, a transfer step of pressing a mold roll 20, which has recesses 21 and protrusions 22 forming a pattern on its outer periphery, against the surface of the base film 1 while rotating to transfer the pattern to the base film 1, a curing step of irradiating ultraviolet light through the mold roll 20 toward the resin 5 on the base film 1 pressed by the mold roll 20 to cure the resin 5 on the base film 1, a peeling step of peeling the base film 1 from the mold roll 20, a removal step of removing the resin 5 remaining on the base film 1 in an uncured state from the base film 1, and a roll cleaning step of removing the uncured resin 5 attached to the protrusions 22 of the mold roll 20. Each step will be specifically described below.
[0051] [Supply process] In the supply process, the electric motors that drive the payout roll 11 and the take-up roll 12 of the conveying section 10 are rotated at a predetermined speed in a predetermined direction to convey the base film 1 at a predetermined conveying speed. Also, the electric motor 23 is rotated to rotate the mold roll 20 at a predetermined speed in a predetermined rotation direction. The rotation speed of the mold roll 20 is set to a speed that corresponds to the conveying speed of the base film 1 by the conveying section 10. In other words, the electric motor that drives the mold roll 20 is controlled to be synchronized with the conveying section 10 so as to correspond to the conveying speed of the base film 1.
[0052] In addition, the resin 5 is continuously applied by the coating die 30 to the film surface (the surface facing the mold roll 20) of the base film 1 being conveyed by the conveying section 10. As a result, a film of the resin 5 having a predetermined thickness is formed on the surface of the base film 1 facing the mold roll 20.
[0053] [Transfer process] The base film 1 coated with the resin 5 in the supplying step passes between the pressing roll 25 and the mold roll 20. At this time, the outer periphery of the mold roll 20 is pressed against the resin 5 on the base film 1. As a result, the resin 5 sandwiched between the base film 1 and the convex parts 22 of the mold roll 20 flows so as to fill the concave parts 21 of the mold roll 20. In this way, a pattern corresponding to the convex parts 22 and concave parts 21 on the outer periphery of the mold roll 20 is transferred to the resin 5 on the base film 1. As the outer periphery of the mold roll 20 is pressed against the resin 5 on the base film 1 in sequence with the rotation, a pattern that is continuous in the longitudinal direction is formed on the base film 1.
[0054] [Curing process] In the curing step, first, the lamp 35 is turned on. When the base film 1 to which the pattern has been transferred moves to a position facing the lamp 35 across the mold roll 20, the resin 5 on the base film 1 is irradiated with ultraviolet light from the lamp 35 and cured, and is fixed to the base film 1. In this way, the resin 5 on the base film 1 transported around the outer periphery of the mold roll 20 is successively integrated with the base film 1.
[0055] Here, in the transfer step, the resin 5 may remain on the base film 1 while being sandwiched between the base film 1 and the protruding portion 22 of the mold roll 20 without being filled in the recessed portion 21 of the mold roll 20 (see FIG. 3). In contrast, in this embodiment, a light-shielding portion 24 that blocks ultraviolet rays from the lamp 35 is provided at the tip of the protruding portion 22 of the mold roll 20. Therefore, the light-shielding portion 24 blocks ultraviolet rays from the lamp 35 and does not irradiate the resin 5 remaining between the base film 1 and the protruding portion 22 of the mold roll 20 (the resin 5 at the position that becomes the recessed portion 21 in the pattern on the base film 1). Therefore, in the curing step, only the resin 5 filled in the recessed portion 21 of the mold roll 20 (the resin 5 that becomes the protruding portion 22 in the pattern on the base film 1) is irradiated with ultraviolet rays from the lamp 35 and cured on the base film 1. The resin 5 between the base film 1 and the protruding portion 22 of the mold roll 20 remains on the base film 1 in an uncured state because the irradiation of ultraviolet rays is blocked.
[0056] [Peeling process] The base film 1 (pattern film 3 ) to which the resin 5 has been fixed in the curing process is peeled off from the outer periphery of the mold roll 20 by being guided (redirected) away from the mold roll 20 by the peeling roll 26 .
[0057] [Removal process] The pattern film 3 peeled off from the mold roll 20 is transported toward the reservoir 41 and immersed in the cleaning liquid L. By being immersed in the cleaning liquid L, the uncured resin 5 remaining on the pattern film 3 is removed or softened.
[0058] Air is discharged from the air knife 43 onto the pattern film 3 that has been taken out of the cleaning liquid L. As a result, the resin 5 softened by the cleaning liquid L and the cleaning liquid L adhering thereto are removed by the air.
[0059] In this manner, the uncured resin 5 remaining on the pattern film 3 is removed. The pattern film 3 from which the uncured resin 5 has been removed is wound up by the winding roll 12 after the cleaning liquid L has been reliably removed by the drying section 44.
[0060] [Roll cleaning process] When the base film 1 is peeled off, the mold roll 20 comes into contact with the roll cleaner 51 as it rotates. The uncured resin 5 adhering to the mold roll 20 as the base film 1 is peeled off is removed from the protruding parts 22 of the mold roll 20 by the roll cleaner 51. The protruding parts 22 from which the uncured resin 5 has been removed are pressed against the resin 5 on the base film 1 again as the mold roll 20 rotates, transferring the pattern.
[0061] In this manner, the pattern 2 is formed on the film surface of the base film 1, and a patterned film 3 is obtained.
[0062] Furthermore, in this embodiment, since the ultraviolet rays from the lamps 35 are blocked by the light-shielding portion 24, the resin 5 sandwiched between the convex portions 22 of the mold roll 20 and the base film 1 remains on the base film 1 in an uncured state. Since the resin 5 remains in an uncured state, it can be relatively easily removed from the base film 1 by immersion in the cleaning liquid L or by air injection using the air knife 43. Therefore, the generation of a residual film on the pattern film 3 can be suppressed, and the subsequent ashing process is not required, thereby reducing the number of manufacturing steps and costs.
[0063] From another perspective, since the uncured resin 5 remaining on the base film 1 can be removed by a configuration (removal section 40) within the pattern forming apparatus 100, an ashing device separate from the pattern forming apparatus 100 is not required, thereby reducing manufacturing labor and costs.
[0064] In this embodiment, the light shielding portion 24 is provided as a solid film in the recessed portion 22a provided at the tip of the protruding portion 22 of the mold roll 20. As a result, the light shielding portion 24 is engaged with the recessed portion 22a in the circumferential direction of the mold roll 20, so that durability against a shear force along the circumferential direction of the mold roll 20 can be ensured when the remover 40 wipes off the uncured resin 5 from the protruding portion 22 of the mold roll 20. Therefore, it is possible to suppress the light shielding portion 24 from falling off (peeling off) from the recessed portion 22a.
[0065] Next, modified examples of this embodiment will be described. The following modified examples are also within the scope of the present invention, and it is possible to combine the following modified examples with each configuration of the above embodiment, to combine the following modified examples with each other, or to combine the following modified examples with other embodiments. In each modified example, the same components as those in the above embodiment are denoted by the same reference numerals, and the description thereof will be omitted.
[0066] In the above embodiment, the removal unit 40 includes a storage unit 41 in which the cleaning liquid L is stored, and an air knife 43 that ejects air.
[0067] 6, the removal unit 40 may have an ultrasonic cleaner 45 that is immersed in the cleaning liquid L. This allows the uncured resin 5 remaining on the base film 1 to be efficiently removed. This also shortens the time the base film 1 is immersed in the cleaning liquid L, thereby improving the production speed and reducing the space required by making the storage unit 41 smaller.
[0068] 7, the removal unit 40 may include a liquid nozzle 46 that sprays the cleaning liquid L toward the base film 1 and a tray 47 that receives the sprayed cleaning liquid L, instead of immersing the base film 1 in the cleaning liquid L. In this case, it is possible to reduce the space required for the device compared to the case where the base film 1 is immersed in the cleaning liquid L. Note that the configuration of the ultrasonic cleaner 45 shown in FIG. 6 may be applied to the modified example shown in FIG. 7.
[0069] It is also preferable that the air knife 43 injects air onto the pattern film 3 immediately after it is taken out of the cleaning liquid L. For this reason, it is also preferable to provide an adjustment mechanism for adjusting the position and injection angle of the air knife 43.
[0070] Second embodiment Next, a pattern forming apparatus 200 and a pattern forming method according to a second embodiment will be described with reference to Fig. 8. In the following, differences from the first embodiment will be mainly described, and the same components as those in the first embodiment will be denoted by the same reference numerals and descriptions thereof will be omitted as appropriate.
[0071] In the pattern forming apparatus 100 according to the first embodiment, the light shielding portion 24 is provided in advance at the tip of the convex portion 22 of the mold roll 20. In the first embodiment, the light shielding portion 24 is integrated with the mold roll 20 so that the light shielding portion 24 is not removed when the uncured resin 5 adhering to the convex portion 22 of the mold roll 20 is removed.
[0072] In contrast, in the second embodiment, the light-shielding portion is not provided in advance at the tip of the convex portion 22 of the mold roll 20, but is provided on the outer periphery of the mold roll 20 by repeatedly applying and removing the light-shielding portion as the mold roll 20 rotates. A specific description will be given below.
[0073] 8, the pattern forming apparatus 200 according to the second embodiment includes, in addition to the configuration of the first embodiment except for the light shielding unit, a light shielding unit supplying unit 60 that sequentially applies a light shielding unit to the tips of the convex portions 22 of the mold roll 20 as the mold roll 20 rotates. The operation of the light shielding unit supplying unit 60 is also controlled by the controller 70.
[0074] In this embodiment, the light-shielding portion is not baked into a solid film as in the first embodiment, but is supplied to the outer periphery of the mold roll 20 in a liquid state before becoming solid (hereinafter, the light-shielding portion is also referred to as "light-shielding liquid 24a"). The light-shielding portion supply unit 60 has a dispenser 61 that discharges the light-shielding liquid 24a as the light-shielding portion, a supply roll 62 that receives the light-shielding liquid 24a discharged by the dispenser 61 and applies the light-shielding liquid 24a to the outer periphery of the mold roll 20, and a doctor blade 63 that removes excess light-shielding liquid 24a on the outer periphery of the supply roll 62.
[0075] The dispenser 61 is configured to continuously drip the light-shielding liquid 24a toward the outer periphery of the supply roll 62. The dispenser 61 is disposed shifted to the right in the drawing from a position directly above the central axis of the supply roll 62, and is configured to drip the resin 5 to a position shifted in the circumferential direction from the top of the supply roll 62 to the forward side in the rotation direction of the mold roll 20 (to the right in the drawing).
[0076] The supply roll 62 is a cylindrical roll (so-called anilox roll) with a central axis parallel to the mold roll 20. The supply roll 62 is controlled by the controller 70 so as to rotate at a constant speed. The supply roll 62 is provided so as to apply the light-shielding liquid 24a applied to the outer periphery to the tip of the convex portion 22 of the mold roll 20 located at a position separated from the base film 1. In this embodiment, the supply roll 62 is provided vertically above the mold roll 20, and is configured to apply the light-shielding liquid 24a to the convex portion 22 of the mold roll 20 from which the uncured resin 5 has been removed by the roll cleaning unit 50.
[0077] The doctor blade 63 is provided so that its tip is in contact with or has a small gap with the outer circumferential surface of the supply roll 62. The light-shielding liquid 24a is supplied from the dispenser 61 to the space formed between the outer periphery of the supply roll 62 and the doctor blade 63. Excess of the light-shielding liquid 24a discharged from the dispenser 61 is scraped off from the outer periphery of the supply roll 62 by the dispenser 61, and the outer periphery of the supply roll 62 is coated with the applicable light-shielding liquid 24a.
[0078] Next, a pattern forming method according to a second embodiment will be described.
[0079] The pattern forming method of the second embodiment further includes a light-shielding portion supplying step of supplying a light-shielding liquid 24 a to the convex portions 22 of the mold roll 20 in addition to the pattern forming method of the first embodiment.
[0080] In the light-shielding portion supplying process, the light-shielding liquid 24a is continuously dropped from the dispenser 61 into the space between the outer periphery of the supply roll 62 and the doctor blade 63. Excess of the dropped light-shielding liquid 24a is scraped off by the doctor blade 63, and an appropriate amount of the light-shielding liquid 24a is applied to the outer periphery of the supply roll 62.
[0081] As the supply roll 62 rotates, the light-shielding liquid 24 a applied to the outer periphery of the supply roll 62 comes into contact with the convex portions 22 of the mold roll 20 , and the light-shielding liquid 24 a is applied to the tips of the convex portions 22 .
[0082] The mold roll 20 having the light-shielding liquid 24a applied to the tips of the convex portions 22 in this manner is pressed against the resin 5 on the base film 1 in the transfer process, and the pattern is transferred to the resin 5 on the base film 1 in the same manner as in the above embodiment.
[0083] The light-shielding liquid 24a applied to the convex parts 22 of the mold roll 20 may be dried and solidified when pressed against the base film 1, or may remain liquid. In either case, the light-shielding liquid 24a can block ultraviolet rays from the lamps 35 to the resin 5 sandwiched between the convex parts 22 of the mold roll 20 and the base film 1, so that the same effect as the light-shielding part of the first embodiment is achieved.
[0084] The light-shielding liquid 24a applied to the convex portions 22 of the mold roll 20 is removed together with the uncured resin 5 attached to the convex portions 22 in the roll cleaning process after the mold roll 20 and the base film 1 are peeled off in the peeling process. Thereafter, new light-shielding liquid 24a is supplied to the convex portions 22 of the mold roll 20 by the light-shielding supply unit 60 as the mold roll 20 rotates. Furthermore, even if the light-shielding liquid 24a remains on the base film 1, it is removed from the base film 1 together with the uncured resin 5 by the removal unit 40 in the removal process.
[0085] In this way, by repeating the application and removal of the light-shielding liquid 24a to the mold roll 20, a constant amount (constant thickness) of the light-shielding liquid 24a can be constantly supplied to the outer periphery of the mold roll 20. This blocks ultraviolet rays from reaching the uncured resin 5 between the convex parts 22 of the mold roll 20 and the base film 1, and also prevents the light-shielding liquid 24a from remaining on the base film 1 (pattern film 3) due to an excessive amount of the light-shielding liquid 24a being unable to be completely removed by the removal unit 40.
[0086] In this embodiment, similarly to the first embodiment, ultraviolet light from the lamps 35 is blocked by the light-shielding portion 24, and the resin 5 sandwiched between the convex portions 22 of the mold roll 20 and the base film 1 remains on the base film 1 in an uncured state. Since the resin 5 remains in an uncured state, it can be relatively easily removed from the base film 1 by immersion in a cleaning liquid L or by air injection using an air knife 43. Therefore, the generation of a residual film on the pattern film 3 can be suppressed, and the subsequent ashing process is not required, thereby reducing the number of manufacturing steps and costs.
[0087] Furthermore, in this embodiment, the application and removal of the light-shielding liquid 24a is repeated as the mold roll 20 rotates, so that a predetermined amount of the light-shielding liquid 24a can be more reliably supplied to the outer periphery of the mold roll 20, and a pattern film 3 in which the generation of residual film is suppressed can be stably produced.
[0088] Although detailed illustration is omitted, the molding roll 20 of the second embodiment may also have the recessed portions 22a as in the first embodiment, or may not have the recessed portions 22a.
[0089] The effects of each embodiment will be described below.
[0090] A pattern forming device 100, 200 which forms a pattern on a sheet-like base film 1 comprises a conveying section 10 having a pay-out roll 11 which pays out the base film 1 and a take-up roll 12 which takes up the base film 1, a resin supplying section which supplies resin 5 to the surface of the base film 1 conveyed by the conveying section 10, a mold roll 20 which has recesses 21 and protrusions 22 which constitute the pattern formed on its outer periphery and which transfers the pattern to the base film 1 by contacting the surface of the base film 1 to which the resin 5 has been supplied, a lamp 35 which is provided inside the mold roll 20 and irradiates light through the mold roll 20 to the base film 1 to harden the resin 5, and a removal section 40 which removes the resin 5 remaining in an unhardened state on the base film 1 from the base film 1, and a light-shielding section 24, 24a which blocks light is provided at the tip of the protrusion 22 of the mold roll 20.
[0091] The pattern forming method for forming a pattern on a sheet-like base film 1 includes a supplying process of supplying resin 5 onto the surface of the base film 1 being transported from a pay-out roll 11 to a take-up roll 12; a transfer process of pressing a mold roll 20, which has recesses 21 and protrusions 22 that constitute the pattern on its outer periphery, against the surface of the base film 1 while rotating to transfer the pattern to the base film 1; a curing process of irradiating light through the mold roll 20 toward the resin 5 on the base film 1 pressed by the mold roll 20 to harden the resin 5 on the base film 1; and a removal process of removing the resin 5 remaining in an uncured state on the base film 1 from the base film 1. In the curing process, light-shielding portions 24, 24a provided at the tips of the protrusions 22 of the mold roll 20 block the irradiation of light to the resin 5 against which the protrusions 22 are pressed.
[0092] In these configurations, since the light-shielding parts 24, 24a are provided at the tips of the convex parts 22, even if the resin 5 remains between the convex parts 22 of the mold roll 20 and the base film 1 when the pattern is transferred, the light irradiated from the inside of the mold roll 20 is blocked by the light-shielding parts 24, 24a and is not irradiated to the resin 5. Therefore, the resin 5 between the convex parts 22 of the mold roll 20 and the base film 1 remains in an uncured state on the base film 1. Since the uncured resin 5 can be removed more easily than the cured resin 5, the generation of a residual film on the base film 1 can be suppressed by removing the uncured resin 5 on the base film 1.
[0093] Moreover, the pattern forming apparatuses 100 and 200 further include a roll cleaning unit 50 that removes the uncured resin 5 adhering to the protruding portions 22 of the mold roll 20 that has transferred the pattern onto the surface of the base film 1 from the mold roll 20 .
[0094] In this configuration, it is possible to suppress a decrease in molding accuracy in the transfer of the pattern caused by the resin 5 remaining on the mold roll 20.
[0095] In addition, in the pattern forming device 100, a recess 22a that is recessed radially inward of the mold roll 20 is formed at the tip of the convex portion 22 of the mold roll 20, and the light-shielding portion 24 is filled in the recess 22a of the convex portion 22 and is integrated with the mold roll 20.
[0096] In this configuration, the light-shielding portion 24 is formed in advance as an integral part of the mold roll 20, and therefore can be easily introduced into existing equipment by simply replacing the mold roll 20 without having to install new equipment, etc.
[0097] The pattern forming device 200 further includes a light shielding portion supplying section 60 that sequentially applies the light shielding portion 24 to the tips of the protrusions 22 of the mold roll 20 as the mold roll 20 rotates.
[0098] In this configuration, even if the mold roll 20 is repeatedly pressed against the base film 1, the light-shielding portion 24 is sequentially supplied to the tip of the mold roll 20, so that the light-shielding portion 24 can be more reliably supplied to the tip of the convex portion 22.
[0099] Although the embodiments of the present invention have been described above, the above-mentioned embodiments merely show some of the application examples of the present invention, and it is not intended that the technical scope of the present invention be limited to the specific configurations of the above-mentioned embodiments. [Explanation of symbols]
[0100] 100 Pattern forming device 200 Pattern forming device 1. Base film (substrate) 2 Pattern 10. Conveyor 11 Payout roll 12 Winding roll 20 Mold roll 21 Recess 22 Convex 22a Recess 24 Light shielding section 24a Light shielding liquid (light shielding part) 30 Coating die (resin supply section) 35 Lamp (curing part) 40 Removal part 50 Roll Cleaning Section 60 Light shielding supply unit
Claims
1. A pattern forming apparatus for forming a pattern on a sheet-like substrate, comprising: A conveying section including a pay-out roll that pays out the base material and a take-up roll that takes up the base material; a resin supplying section that supplies a curable resin to a surface of the base material transported by the transporting section; a mold roll having an outer periphery on which recesses and protrusions constituting the pattern are formed, the mold roll contacting the surface of the substrate to which the curable resin is supplied to transfer the pattern to the substrate; a curing section provided inside the mold roll and irradiating the base material with light through the mold roll to cure the curable resin; A removal unit that removes the curable resin remaining in an uncured state on the base material from the base material, A light-shielding portion that blocks light is provided at the tip of the convex portion of the mold roll. Pattern forming device.
2. The pattern forming apparatus according to claim 1 , The method further includes a roll cleaning unit that removes the uncured curable resin adhering to the convex portions of the mold roll that have transferred the pattern onto the surface of the base material from the mold roll. Pattern forming device.
3. The pattern forming apparatus according to claim 1 or 2, A recessed portion recessed toward the inside in the radial direction of the mold roll is formed at the tip of the protruding portion of the mold roll, The light-shielding portion is filled in the recessed portion of the protruding portion and is integrated with the mold roll. Pattern forming device.
4. The pattern forming apparatus according to claim 1 or 2, The mold roll further includes a light-shielding portion supplying unit that sequentially applies the light-shielding portion to the tip of the convex portion of the mold roll as the mold roll rotates. Pattern forming device.
5. A pattern forming method for forming a pattern on a sheet-like substrate, comprising the steps of: a supplying step of supplying a curable resin onto a surface of the substrate transported from a feed roll to a take-up roll; a transfer step of pressing a mold roll, the mold roll having recesses and protrusions that constitute the pattern formed on its outer periphery, against the surface of the substrate while rotating the mold roll to transfer the pattern to the substrate; a curing step of irradiating light through the mold roll toward the curable resin on the substrate against which the mold roll is pressed, thereby curing the curable resin on the substrate; A removing step of removing the curable resin remaining in an uncured state on the base material from the base material, In the curing step, a light shielding portion provided at a tip of the protrusion of the mold roll blocks irradiation of light to the curable resin against which the protrusion is pressed. Pattern forming method.
Citation Information
Patent Citations