Electrophotographic receptor, process cartridge, and electrophotographic device

By using polymers with specific structural units in the undercoat layer, the electrophotographic photoreceptor stabilizes potential fluctuations, ensuring consistent image quality during mass and high-speed printing.

JP2024152028APending Publication Date: 2024-10-25CANON KK
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
JP2023065927
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-13
Publication Date
2024-10-25

AI Technical Summary

Technical Problem

Conventional electrophotographic photoreceptors experience significant potential fluctuations during mass printing and high-speed printing, leading to deteriorated image quality due to insufficient electron transport ability and charge accumulation.

Method used

Incorporation of specific polymers with structural units represented by formulas (1) and (2) in the undercoat layer to enhance electron mobility, preventing aggregation of perylene imide and naphthalene imide molecules, thereby stabilizing potential fluctuations.

Benefits of technology

The solution effectively suppresses potential fluctuations, maintaining image quality and stability during high-volume and high-speed printing by improving electron transport efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

To provide an electrophotographic receptor capable of suppressing a potential variation.SOLUTION: An electrophotographic receptor includes a support, an undercoat layer, and a photosensitive layer in this order. The undercoat layer includes at least one kind of polymer selected among a group composed of a polymer having a structural unit represented by the following formula (1) and a polymer having a structural unit represented by a specific formula (2).SELECTED DRAWING: None
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to an electrophotographic photosensitive member, a process cartridge, and an electrophotographic apparatus. [Background technology]

[0002] In recent years, there has been a demand for electrophotographic apparatuses capable of forming higher quality images, and there is a demand for apparatuses that can output highly stable image quality even when used repeatedly. In electrophotographic photoreceptors used in electrophotographic processes, a technique is known in which an undercoat layer containing an electron transport material is provided between the support and the photosensitive layer in order to suppress charge injection from the support side to the photosensitive layer side and to suppress the occurrence of image defects such as black spots. Patent Document 1 describes an undercoat layer containing a cured product of a composition containing an electron transport material having a polymerizable functional group, a crosslinking agent, and a resin. Patent Document 2 describes an intermediate layer containing a polymer obtained by polymerizing a diphenoquinone derivative. Patent Document 3 describes an aqueous coating liquid for forming an intermediate layer, which contains a composition containing an electron transport material having a carboxyl group, a dispersant, and a resin. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2014-029479 A [Patent Document 2] Japanese Patent Application Publication No. 11-228675 [Patent Document 3] JP 2012-032458 A Summary of the Invention [Problem to be solved by the invention]

[0004] In recent years, there has been a demand for large-volume and high-speed printing in electrophotographic processes. According to studies by the present inventors, it has been found that in the electrophotographic photoreceptors described in Patent Documents 1, 2, and 3, potential fluctuations may become large when large-volume and high-speed printing is performed. SUMMARY OF THE PRESENT EMBODIMENT An object of the present invention is to provide an electrophotographic photoreceptor capable of suppressing potential fluctuations. [Means for solving the problem]

[0005] The above object can be achieved by the present invention, which is described below. That is, the electrophotographic photoreceptor according to the present invention is an electrophotographic photoreceptor having a support, an undercoat layer, and a photosensitive layer in this order, The undercoat layer is characterized in that it contains at least one polymer selected from the group consisting of polymers having a structural unit represented by the following formula (1) and polymers having a structural unit represented by the following formula (2). [ka] [ka] (In formulas (1) and (2), α, β, and γ represent structures represented by the following formulae (α), (β), and (γ), respectively. R 11 , R 12 , R 13 , R 14 , R 15 , R 16 , R 17 , R 18 , R 21 ,R 22 , R 23 , and R 24 each independently represents a hydrogen atom, a halogen atom, a nitro group, a cyano group, a trifluoromethyl group, a substituted or unsubstituted alkoxy group, a substituted or unsubstituted thiol group, a substituted or unsubstituted amino group, a substituted or unsubstituted alkyl group, a substituted or unsubstituted alkynyl group, or a substituted or unsubstituted aryl group. [ka] [ka] [ka] (In formulas (α), (β), and (γ), R 60 , R 61 , R 70 , R 71 , R 80 , and R 81 each independently represents a hydrogen atom, a substituted or unsubstituted alkyl group, or a substituted or unsubstituted aryl group, Z a , Z b , and Z c each independently represents a single bond, an imino group, an oxygen atom, or a sulfur atom, l a , l b , and l c each independently represents an integer of 0 or more, m a is an integer equal to or greater than 1, m b and m c each independently represents an integer of 0 or more, Z a When represents a single bond, R 60 represents a substituted or unsubstituted alkyl group, Z a represents an imino group or a sulfur atom, R 60 represents a hydrogen atom or a substituted or unsubstituted alkyl group, Z a represents an oxygen atom, and R 60 When represents a hydrogen atom, m a indicates an integer of 2 or more, Z a represents an oxygen atom, and R 60 When m represents a substituted or unsubstituted alkyl group, a indicates an integer of 1 or greater.) Effect of the Invention

[0006] According to the present invention, it is possible to provide an electrophotographic photoreceptor capable of suppressing potential fluctuations. [Brief description of the drawings]

[0007] [Figure 1] FIG. 2 is a diagram showing an example of a layer structure of an electrophotographic photoreceptor according to the present invention. [Diagram 2] 1 is a diagram showing an example of a schematic configuration of an electrophotographic apparatus provided with a process cartridge having an electrophotographic photosensitive member according to the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0008] The present invention will be described in detail below with reference to preferred embodiments. When performing large-volume and high-speed printing, the potential fluctuation may become large in a conventional electrophotographic photoreceptor. The following is considered to be the cause of this. Electrophotographic photoreceptors are required to have high sensitivity and high durability in order to handle large-volume and high-speed printing, and therefore, charge generating substances having higher sensitivity are used as the charge generating substances contained in electrophotographic photoreceptors. As the charge generating material becomes more sensitive, the amount of generated charge increases, but in conventional electrophotographic photoreceptors, the electron transport capacity is insufficient, and it is considered that when images are repeatedly output, charges are retained in the exposed parts of the photosensitive layer, causing potential fluctuations. When the potential fluctuations in the exposed parts of the electrophotographic photoreceptor become large, the density of the image becomes lighter after repeated use than at the beginning, and the image quality deteriorates.

[0009] The present inventors have investigated the inclusion of highly π-conjugated perylene imide and naphthalene imide at high concentrations in order to increase the mobility of electrons in order to suppress potential fluctuations. However, there are cases where the mobility of electrons is not sufficiently increased by merely forming a film containing perylene imide and naphthalene imide at high concentrations. One of the reasons for this is the rigid planar structure of perylene imide and naphthalene imide. Perylene imide and naphthalene imide have a rigid planar structure, so that the molecules tend to stack closely together, and are distributed unevenly by forming aggregation sites in the film, which is thought to be a hindrance to the improvement of the mobility of electrons. Therefore, the present inventors have further studied and found that the above problem can be solved by using a polymer having a specific film-forming unit in addition to perylene imide and naphthalene imide as an electron transport material. That is, by using the above polymer as an electron transport material, perylene imide and naphthalene imide can be present in the film with an appropriate distance from each other, and the formation of aggregation sites can be suppressed. In addition, by using the above polymer as an electron transport material, the mobility of electrons was improved. As a result of the above mechanism, the present inventors have achieved the suppression of potential fluctuation.

[0010] Specifically, an undercoat layer containing, as an electron transport material, at least one polymer selected from the group consisting of a polymer having a repeating structural unit represented by formula (1) described below and a polymer having a repeating structural unit represented by formula (2) described below is used. The present inventors have found that the problems in the conventional technology can be solved by using an electrophotographic photoreceptor provided with such an undercoat layer.

[0011] The configuration of the electrophotographic photoreceptor according to the present invention will be described in detail below. [Electrophotographic photoreceptor] The electrophotographic photoreceptor according to the present invention has a support, an undercoat layer, and a photosensitive layer in this order. Fig. 1 is a diagram showing an example of the layer structure of an electrophotographic photoreceptor. In the layer structure shown in Fig. 1, an undercoat layer 102, and a photosensitive layer (laminated photosensitive layer) 105 consisting of a charge generating layer 103 and a charge transport layer 104 are laminated in this order on a support 101.

[0012] The method for producing the electrophotographic photoreceptor according to the present invention includes a method in which the coating liquid for each layer described below is prepared, coated in the desired order, and dried. In this case, the coating liquid can be applied by dip coating, spray coating, inkjet coating, roll coating, die coating, blade coating, curtain coating, wire bar coating, ring coating, etc. Among these, dip coating is preferred from the viewpoint of efficiency and productivity. The support and each layer will be described below.

[0013] <Support> In the present invention, the electrophotographic photoreceptor has a support. In the present invention, the support is preferably a conductive support having electrical conductivity. The shape of the support may be a cylinder, a belt, a sheet, or the like. Among them, a cylindrical support is preferable. The surface of the support may be subjected to electrochemical treatment such as anodization, blasting, cutting, or the like. The support is preferably made of a metal, a resin, or a glass. Examples of the metal include aluminum, iron, nickel, copper, gold, stainless steel, and alloys thereof. Among them, an aluminum support using aluminum is preferable. Furthermore, the resin or glass may be made conductive by a process such as mixing with or coating with a conductive material.

[0014] <Conductive layer> In the present invention, a conductive layer may be provided on the support. By providing the conductive layer, scratches and irregularities on the surface of the support can be concealed and light reflection on the surface of the support can be controlled. The conductive layer preferably contains conductive particles and a resin. The conductive particles may be made of a material such as metal oxide, metal, or carbon black. Examples of metal oxides include zinc oxide, aluminum oxide, indium oxide, silicon oxide, zirconium oxide, tin oxide, titanium oxide, magnesium oxide, antimony oxide, bismuth oxide, etc. Examples of metals include aluminum, nickel, iron, nichrome, copper, zinc, silver, etc. Among these, it is preferable to use metal oxides as the conductive particles, and it is particularly preferable to use titanium oxide, tin oxide, or zinc oxide. When a metal oxide is used as the conductive particles, the surface of the metal oxide may be treated with a silane coupling agent or the like, or the metal oxide may be doped with an element such as phosphorus or aluminum or an oxide thereof. The conductive particles may have a laminated structure having a core particle and a coating layer that covers the core particle. Examples of the core particle include titanium oxide, barium sulfate, zinc oxide, etc. Examples of the coating layer include metal oxides such as tin oxide. When a metal oxide is used as the conductive particles, the volume average particle size is preferably 1 nm or more and 500 nm or less, and more preferably 3 nm or more and 400 nm or less. Examples of the resin include polyester resin, polycarbonate resin, polyvinyl acetal resin, acrylic resin, silicone resin, epoxy resin, melamine resin, polyurethane resin, phenol resin, and alkyd resin. The conductive layer may further contain silicone oil, resin particles, a masking agent such as titanium oxide, and the like. The thickness of the conductive layer is preferably from 1 μm to 50 μm, and particularly preferably from 3 μm to 40 μm. The conductive layer can be formed by preparing a coating solution for the conductive layer containing the above-mentioned materials and solvent, forming a coating film of this, and drying it. Examples of the solvent used in the coating solution include alcohol-based solvents, sulfoxide-based solvents, ketone-based solvents, ether-based solvents, ester-based solvents, and aromatic hydrocarbon-based solvents. Examples of the dispersion method for dispersing the conductive particles in the coating solution for the conductive layer include a method using a paint shaker, a sand mill, a ball mill, and a liquid collision type high-speed disperser.

[0015] <Undercoat layer> The electrophotographic photoreceptor according to the present invention has an undercoat layer on the support or the conductive layer. In the present invention, the undercoat layer is obtained by forming a coating film of a coating solution for the undercoat layer containing a specific polymer, and then heating and drying the coating film. The specific polymer is at least one polymer selected from the group consisting of polymers having a structural unit represented by the following formula (1) and polymers having a structural unit represented by the following formula (2). The temperature at which the coating film is heated and dried is preferably 50 to 200°C.

[0016] In the present invention, the undercoat layer contains, as an electron transport material, at least one polymer selected from the group consisting of a polymer having a structural unit represented by the following formula (1) and a polymer having a structural unit represented by the following formula (2): [ka] [ka] (In formulas (1) and (2), α, β, and γ represent structures represented by the following formulae (α), (β), and (γ), respectively. R 11 , R 12 , R 13 , R 14 , R 15 , R 16 , R 17 , R 18 , R 21 ,R 22 , R 23, and R 24 each independently represents a hydrogen atom, a halogen atom, a nitro group, a cyano group, a trifluoromethyl group, a substituted or unsubstituted alkoxy group, a substituted or unsubstituted thiol group, a substituted or unsubstituted amino group, a substituted or unsubstituted alkyl group, a substituted or unsubstituted alkynyl group, or a substituted or unsubstituted aryl group. [ka] [ka] [ka] (In the formulas (α), (β), and (γ), R 60 , R 61 , R 70 , R 71 , R 80 , and R 81 each independently represents a hydrogen atom, a substituted or unsubstituted alkyl group, or a substituted or unsubstituted aryl group, Z a , Z b , and Z c each independently represents a single bond, an imino group, an oxygen atom, or a sulfur atom, l a , l b , and l c each independently represents an integer of 0 or more, m a is an integer equal to or greater than 1, m b and m c each independently represents an integer of 0 or more, Z a When represents a single bond, R 60 represents a substituted or unsubstituted alkyl group, Z a represents an imino group or a sulfur atom, R 60 represents a hydrogen atom or a substituted or unsubstituted alkyl group, Z a represents an oxygen atom, and R 60When represents a hydrogen atom, m a indicates an integer of 2 or more, Z a represents an oxygen atom, and R 60 When m represents a substituted or unsubstituted alkyl group, a indicates an integer of 1 or greater.)

[0017] In the structural unit represented by formula (1) and the structural unit represented by formula (2), examples of the substituent that the substituted alkyl group has include an aryl group, a halogen atom, a nitro group, and a cyano group. Examples of the substituent on the substituted aryl group include a halogen atom, a nitro group, a cyano group, a trifluoromethyl group, an alkyl group, a halogen-substituted alkyl group, and an alkoxy group. Examples of the substituent on the substituted alkoxy group include a halogen atom, a nitro group, a cyano group, a trifluoromethyl group, an alkyl group, a halogen-substituted alkyl group, and an alkoxy group. Examples of the substituent that the substituted thiol group has include a halogen atom, a nitro group, a cyano group, a trifluoromethyl group, an alkyl group, a halogen-substituted alkyl group, and an alkoxy group. Examples of the substituent on the substituted amino group include a halogen atom, a nitro group, a cyano group, a trifluoromethyl group, an alkyl group, a halogen-substituted alkyl group, a hydroxyalkyl group, an aryl group, and an alkoxy group. Furthermore, examples of the substituent that the substituted alkynyl group may have include a halogen atom, a nitro group, a cyano group, a trifluoromethyl group, an alkyl group, a halogen-substituted alkyl group, and an alkoxy group.

[0018] In the structural unit represented by formula (1) and the structural unit represented by formula (2), specific examples of the substituted or unsubstituted alkyl group include a methyl group, an ethyl group, an n-propyl group, an isopropyl group, an n-butyl group, an isobutyl group, a sec-butyl group, a tert-butyl group, an n-pentyl group, an isopentyl group, a neopentyl group, a tert-pentyl group, a cyclopentyl group, an n-hexyl group, a 1-methylpentyl group, a 4-methyl-2-pentyl group, a 3,3-dimethylbutyl group, a 2-ethylbutyl group, a cyclohexyl group, a hexyl group, an isohexyl group, a heptyl group, an octyl group, a nonyl group, a decyl group, an undecyl group, a dodecyl group, a tridecyl group, a tetradecyl group, a hexadecyl group, a heptadecyl group, an octadecyl group, a nonadecyl group, an icosyl group, a henicosyl group, a triacontyl group, a benzyl group, and a trityl group. Specific examples of the substituted or unsubstituted alkynyl group include an ethynyl group, a propynyl group, a butynyl group, a pentynyl group, a hexynyl group, a heptynyl group, and an octynyl group. Specific examples of the substituted or unsubstituted aryl group include a phenyl group, a biphenylyl group, a fluorenyl group, a 1-naphthyl group, a 2-naphthyl group, and a tolyl group. Specific examples of the substituted or unsubstituted alkoxy group include a methoxy group, an ethoxy group, a propoxy group, a tert-butoxy group, a phenoxy group, a pentyloxy group, a cyclohexyloxy group, a benzyloxy group, an allyloxy group, and a 1-naphthyloxy group. Specific examples of the substituted or unsubstituted thiol group include a thiol group (sulfanyl group), a methylthio group, an ethylthio group, a propylthio group, a butylthio group, a pentylthio group, a hexylthio group, a heptylthio group, an octylthio group, and a phenylthio group. Specific examples of the substituted or unsubstituted amino group include an amino group, a methylamino group, a dimethylamino group, a trimethylamino group, an ethylamino group, a diethylamino group, a propylamino group, an isopropylamino group, a butylamino group, a pentylamino group, a hexylamino group, a heptylamino group, an octylamino group, a phenylamino group, and a pyrrolidinyl group.

[0019] From the viewpoint of forming a uniform film state of perylene imide and naphthalene imide in the undercoat layer and from the viewpoint of improving the mobility of electrons, R 11 , R 12 , R 13 , R 14 , R 15 , R 16 , R 17 , and R 18 At least one of R in formula (2) 21 ,R 22 , R 23 , and R 24 It is preferable that at least one of the above is a halogen atom, a nitro group, a cyano group, a trifluoromethyl group, a substituted or unsubstituted alkoxy group having 20 carbon atoms or less, a substituted or unsubstituted thiol group having 20 carbon atoms or less, a substituted or unsubstituted amino group having 20 carbon atoms or less, a substituted or unsubstituted alkyl group having 20 carbon atoms or less, a substituted or unsubstituted alkynyl group having 20 carbon atoms or less, or a substituted or unsubstituted aryl group having 20 carbon atoms or less.

[0020] From the viewpoint of forming a uniform film state of perylene imide and naphthalene imide in the undercoat layer and from the viewpoint of improving the electron mobility, R 60 and R 61 R in formula (β) 70 and R 71 , and R in formula (γ) 80 and R 81 At least one of R in formula (α) is preferably a substituted or unsubstituted alkyl group having 20 or less carbon atoms or a substituted or unsubstituted aryl group having 20 or less carbon atoms. 60However, it is more preferable that the alkyl group is a substituted or unsubstituted alkyl group having 20 or less carbon atoms.

[0021] In order to form a uniform film state of perylene imide and naphthalene imide in the undercoat layer and to improve the electron mobility, the formula (α) a , l in formula (β) b , and l in formula (γ) c are each preferably an integer of 0 or more and 10 or less.

[0022] From the viewpoint of forming a uniform film state of perylene imide and naphthalene imide in the undercoat layer and from the viewpoint of improving the mobility of electrons, m a is an integer of 1 to 40, and m in formula (β) b and m in formula (γ) c Each of m in formula (α) is preferably an integer of 0 to 40. a is an integer of 2 to 30, and m in formula (α) a and m in formula (β) b and m in formula (γ) c The sum of is more preferably 3 or more and 30 or less.

[0023] Specific examples of polymers having a structural unit represented by formula (1) and polymers having a structural unit represented by formula (2) are shown below. Detailed example compounds (P-1) to (P-549) and (N-1) to (N549) are shown in Tables 1 to 22. In Tables 1 to 22, (SB) represents a single bond, and the bond represented by a dashed line represents a bond bonded to the main skeleton of the compound. [ka] [ka] [ka]

[0024] [Table 1]

[0025]

Table 2

[0026]

Table 3

[0027]

Table 4

[0028]

Table 5

[0029]

Table 6

[0030]

Table 7

[0031]

Table 8

[0032]

Table 9

[0033]

Table 10

[0034]

Table 11

[0035]

change

change

change

[0036]

Table 12

[0037]

Table 13

[0038]

Table 14

[0039]

Table 15

[0040]

Table 16

[0041]

Table 17

[0042]

Table 18

[0043]

Table 19

[0044] [Table 20]

[0045] [Table 21]

[0046] [Table 22]

[0047] At least one polymer selected from the group consisting of polymers having a structural unit represented by formula (1) and polymers having a structural unit represented by formula (2) preferably has a weight average molecular weight of 30,000 or less. In the present invention, the content of at least one polymer selected from the group consisting of polymers having a structural unit represented by formula (1) and polymers having a structural unit represented by formula (2) relative to the total mass of the undercoat layer is preferably 30 mass% or more, and from the viewpoint of improving the electron mobility in the undercoat layer, more preferably 50 mass% or more.

[0048] The thickness of the undercoat layer is preferably from 0.1 μm to 10 μm, and more preferably from 0.5 μm to 5 μm.

[0049] The undercoat layer controls charge injection at the interface and also functions as an adhesive layer. The undercoat layer in the present invention has a function of transporting charges of the same polarity as the charge polarity of the surface of the electrophotographic photoreceptor. Specifically, the charge polarity of the electrophotographic photoreceptor is negative, and the undercoat layer has a negative charge transport function, i.e., an electron transport function, and its electron mobility is 10 -7 cm 2 / V·sec or more is preferable, and 10 -6 cm 2 / V·sec or more. In order to maintain the surface potential of the electrophotographic photoreceptor, the volume resistivity of the undercoat layer is 1×10 10 It is preferable that the resistivity is Ω·cm or more, and more preferably 1×10 12Ω·cm or more.

[0050] The coating liquid for forming the undercoat layer according to the present invention may contain a crosslinking agent in addition to the electron transport material. As the crosslinking agent, any known material can be used, specifically, the compounds described in "Crosslinking Agent Handbook" edited by Shinzo Yamashita and Tosuke Kaneko, published by Taiseisha (1981) can be mentioned. In the present invention, the crosslinking agent is preferably an isocyanate compound having an isocyanate group or a blocked isocyanate group, or an amine compound having an N-methylol group or an alkyl-etherified N-methylol group. An isocyanate compound having 2 to 6 isocyanate groups or blocked isocyanate groups is preferred.

[0051] Examples of the isocyanate compound as the crosslinking agent include the isocyanate compounds shown below, but the present invention is not limited thereto. In addition, the isocyanate compounds shown below may be used in combination. Examples of the isocyanate compound include isocyanurate modified products, biuret modified products, allophanate modified products, and adduct modified products with trimethylolpropane or pentaerythritol of diisocyanates such as triisocyanate benzene, triisocyanate methylbenzene, triphenylmethane triisocyanate, lysine triisocyanate, tolylene diisocyanate, hexamethylene diisocyanate, dicyclohexylmethane diisocyanate, naphthalene diisocyanate, diphenylmethane diisocyanate, isophorone diisocyanate, xylylene diisocyanate, 2,2,4-trimethylhexamethylene diisocyanate, methyl-2,6-diisocyanate hexanoate, and norbornane diisocyanate. The blocked isocyanate group is -NHCOX 1 (X 1 X is a protecting group). 1 may be any protecting group that can be introduced into an isocyanate group.

[0052] Examples of commercially available isocyanate compounds include isocyanate-based crosslinking agents such as Duranate MFK-60B, SBA-70B, 17B-60P, SBN-70D, and SBB-70P manufactured by Asahi Kasei Corporation, and Desmodur BL3175 and BL3475 manufactured by Sumika Bayer Urethane Co., Ltd.

[0053] The amine compound as the crosslinking agent preferably has an N-methylol group or an alkyl-etherified N-methylol group.More preferably, the amine compound has a plurality (two or more) of N-methylol groups or alkyl-etherified N-methylol groups.For example, the amine compound may include methylolated melamine, methylolated guanamine, methylolated urea derivatives, methylolated ethylene urea derivatives, methylolated glycoluril, and compounds in which the methylol moiety is alkyl-etherified, and derivatives thereof.

[0054] Examples of commercially available amine compounds (crosslinking agents) include Super Melami No. 90 (manufactured by NOF Corp. (formerly Nippon Oil & Fats)), Super Bekkamin® TD-139-60, L-105-60, L127-60, L110-60, J-820-60, and G-821-60 (manufactured by DIC Corp.), U-Ban 2020 (Mitsui Chemicals), Sumitex Resin M-3 (manufactured by Sumitomo Chemical Co., Ltd. (formerly Sumitomo Chemical Co., Ltd.)), and Ni Examples of such compounds include Karac MW-30, MW-390, and MX-750LM (manufactured by Sanwa Chemical Co., Ltd.), Super Beckamin(R) L-148-55, 13-535, L-145-60, and TD-126 (manufactured by DIC Corporation), Nikalac BL-60 and BX-4000 (manufactured by Sanwa Chemical Co., Ltd.), Nikalac MX-280, Nikalac MX-270, and Nikalac MX-290 (manufactured by Sanwa Chemical Co., Ltd.).

[0055] The coating liquid for forming the undercoat layer according to the present invention may contain a thermoplastic resin having a polymerizable functional group in addition to the electron transport material and the crosslinking agent. Examples of the thermoplastic resin include polyacetal resin, polyolefin resin, polyester resin, polyether resin, polyamide resin, etc. Examples of the polymerizable functional group of the thermoplastic resin include a hydroxyl group, a thiol group, an amino group, and a methoxy group. Furthermore, the thermoplastic resin is preferably a thermoplastic resin having a repeating unit consisting of -(CH2-CH2-O)n- (n is an integer of 2 or more and 200 or less), -(CH2-CH3CH-O)n- (n is an integer of 2 or more and 200 or less), or -(CH2-CH2-O-CH2-CH2-SS)n- (n is an integer of 2 or more and 50 or less).

[0056] Thermoplastic resins having a polymerizable functional group that are commercially available include, for example, polyether polyol resins such as AQD-457, AQD-473 (all manufactured by Nippon Polyurethane Industry Co., Ltd.), GP-400, and GP-700 (all manufactured by Sanyo Chemical Industries, Ltd. and Sannix); Phthalkid W2343 (manufactured by Hitachi Chemical Co., Ltd.), Watersol S-118, CD-520, Beckolite M-6402-50, and M-6201-40IM (all manufactured by DIC), Haridip WH-1188 (manufactured by Harima Chemical Co., Ltd.), ES3604, and ES6538 (all manufactured by Nippon Polyurethane Industry Co., Ltd.); Examples of such resins include polyester polyol resins such as those manufactured by U-PICA; polyacrylic polyol resins such as Burnock WE-300 and WE-304 (both manufactured by DIC); polyvinyl alcohol resins such as Kuraray Poval PVA-203 (manufactured by Kuraray); polyvinyl acetal resins such as BX-1, BM-1, and KS-5 (both manufactured by Sekisui Chemical Co., Ltd.); polyamide resins such as Toresin FS-350 (manufactured by Nagase Chemtex); polyamine resins such as Luccamide (manufactured by DIC); and polythiol resins such as QE-340M (manufactured by Toray). Among these, polyvinyl acetal resins having a polymerizable functional group and polyester polyol resins having a polymerizable functional group are preferred from the viewpoint of polymerizability.

[0057] The undercoat layer can be formed by preparing a coating solution for the undercoat layer containing the above-mentioned materials and solvent, forming a coating film from the coating solution, and drying and / or curing the coating solution. Examples of the solvent used in the coating solution include alcohol-based solvents, ketone-based solvents, ether-based solvents, ester-based solvents, and aromatic hydrocarbon-based solvents.

[0058] <Photosensitive layer> The photosensitive layer of an electrophotographic photoreceptor is mainly classified into (1) a multi-layer type photosensitive layer and (2) a single-layer type photosensitive layer. (1) The multi-layer type photosensitive layer has a charge generation layer containing a charge generation material and a charge transport layer containing a charge transport material. (2) The single-layer type photosensitive layer has a photosensitive layer containing both a charge generation material and a charge transport material.

[0059] (1) Laminated photosensitive layer The laminated type photosensitive layer has a charge generating layer and a charge transport layer.

[0060] (1-1) Charge generation layer The charge generating layer preferably contains a charge generating material and a resin. Examples of the charge generating material include azo pigments, perylene pigments, polycyclic quinone pigments, indigo pigments, and phthalocyanine pigments. Among these, azo pigments and phthalocyanine pigments are preferred. Among phthalocyanine pigments, oxytitanium phthalocyanine pigments, chlorogallium phthalocyanine pigments, and hydroxygallium phthalocyanine pigments are preferred. The content of the charge generating material in the charge generating layer is preferably from 40% by mass to 85% by mass, and more preferably from 60% by mass to 80% by mass, based on the total mass of the charge generating layer. Examples of the resin include polyester resin, polycarbonate resin, polyvinyl acetal resin, polyvinyl butyral resin, acrylic resin, silicone resin, epoxy resin, melamine resin, polyurethane resin, phenol resin, polyvinyl alcohol resin, cellulose resin, polystyrene resin, polyvinyl acetate resin, polyvinyl chloride resin, etc. Among these, polyvinyl butyral resin is more preferable.

[0061] The charge generating layer may further contain additives such as an antioxidant and an ultraviolet absorbing agent, etc. Specific examples of such additives include hindered phenol compounds, hindered amine compounds, sulfur compounds, phosphorus compounds, and benzophenone compounds. The thickness of the charge generating layer is preferably from 0.1 μm to 1 μm, and more preferably from 0.15 μm to 0.4 μm. The charge generating layer can be formed by preparing a coating solution for the charge generating layer containing the above-mentioned materials and solvent, forming a coating film of this, and drying it. Examples of the solvent used in the coating solution include alcohol-based solvents, sulfoxide-based solvents, ketone-based solvents, ether-based solvents, ester-based solvents, and aromatic hydrocarbon-based solvents.

[0062] (1-2) Charge transport layer The charge transport layer preferably contains a charge transport material and a resin. Examples of the charge transport material include polycyclic aromatic compounds, heterocyclic compounds, hydrazone compounds, styryl compounds, enamine compounds, benzidine compounds, triarylamine compounds, and resins having groups derived from these materials. Among these, triarylamine compounds and benzidine compounds are preferred.

[0063] The content of the charge transport material in the charge transport layer is preferably from 25% by weight to 70% by weight, and more preferably from 30% by weight to 55% by weight, based on the total weight of the charge transport layer. Examples of the resin include polyester resin, polycarbonate resin, acrylic resin, polystyrene resin, etc. Among these, polycarbonate resin and polyester resin are preferable. As the polyester resin, polyarylate resin is particularly preferable. The content ratio (mass ratio) of the charge transport material to the resin is preferably from 4:10 to 20:10, and more preferably from 5:10 to 12:10. The charge transport layer may also contain additives such as antioxidants, ultraviolet absorbers, plasticizers, leveling agents, slipping agents, and abrasion resistance improvers. Specific examples of such additives include hindered phenol compounds, hindered amine compounds, sulfur compounds, phosphorus compounds, benzophenone compounds, siloxane-modified resins, silicone oils, fluororesin particles, polystyrene resin particles, polyethylene resin particles, silica particles, alumina particles, and boron nitride particles. The thickness of the charge transport layer is preferably from 5 μm to 50 μm, more preferably from 8 μm to 40 μm, and particularly preferably from 10 μm to 30 μm. The charge transport layer can be formed by preparing a coating solution for the charge transport layer containing the above-mentioned materials and solvent, forming a coating film of this, and drying it. Examples of the solvent used in the coating solution include alcohol-based solvents, ketone-based solvents, ether-based solvents, ester-based solvents, and aromatic hydrocarbon-based solvents. Among these solvents, ether-based solvents or aromatic hydrocarbon-based solvents are preferred.

[0064] (2) Single-layer photosensitive layer The single-layer type photosensitive layer can be formed by preparing a coating solution for the photosensitive layer containing a charge generating material, a charge transporting material, a resin and a solvent, forming a coating film of this, and drying it. The charge generating material, the charge transporting material and the resin are the same as the examples of materials in "(1) Multi-layer type photosensitive layer" above.

[0065] <Protective layer> In the present invention, a protective layer may be provided on the photosensitive layer. By providing the protective layer, durability can be improved. The protective layer preferably contains conductive particles and / or a charge transport material, and a resin. The conductive particles include particles of metal oxides such as titanium oxide, zinc oxide, tin oxide, and indium oxide. Examples of the charge transport material include polycyclic aromatic compounds, heterocyclic compounds, hydrazone compounds, styryl compounds, enamine compounds, benzidine compounds, triarylamine compounds, and resins having groups derived from these materials. Among these, triarylamine compounds and benzidine compounds are preferred. Examples of the resin include polyester resin, acrylic resin, phenoxy resin, polycarbonate resin, polystyrene resin, phenol resin, melamine resin, epoxy resin, etc. Among them, polycarbonate resin, polyester resin, and acrylic resin are preferable.

[0066] The protective layer may be formed as a cured film by polymerizing a composition containing a monomer having a polymerizable functional group. Examples of the reaction include thermal polymerization, photopolymerization, and radiation polymerization. Examples of the polymerizable functional group of the monomer having a polymerizable functional group include an acrylic group and a methacrylic group. A material having a charge transport function may be used as the monomer having a polymerizable functional group. The protective layer may contain additives such as antioxidants, ultraviolet absorbers, plasticizers, leveling agents, slipping agents, abrasion resistance improvers, etc. Specific examples of the additives include hindered phenol compounds, hindered amine compounds, sulfur compounds, phosphorus compounds, benzophenone compounds, siloxane-modified resins, silicone oils, fluororesin particles, polystyrene resin particles, polyethylene resin particles, silica particles, alumina particles, and boron nitride particles. The thickness of the protective layer is preferably from 0.5 μm to 10 μm, and more preferably from 1 μm to 7 μm. The protective layer can be formed by preparing a coating solution for the protective layer containing the above-mentioned materials and solvent, forming a coating film from the coating solution, and drying and / or curing the coating solution. Examples of the solvent used in the coating solution include alcohol-based solvents, ketone-based solvents, ether-based solvents, sulfoxide-based solvents, ester-based solvents, and aromatic hydrocarbon-based solvents.

[0067] [Process cartridges, electrophotographic devices] The process cartridge according to the present invention is characterized in that it integrally supports the electrophotographic photosensitive member described above and at least one means selected from the group consisting of a charging means, a developing means and a cleaning means, and is detachably attachable to the main body of the electrophotographic apparatus. The electrophotographic apparatus according to the present invention is characterized by comprising the electrophotographic photosensitive member described above, as well as a charging means, an exposing means, a developing means and a transferring means.

[0068] FIG. 2 shows an example of a schematic configuration of an electrophotographic apparatus having a process cartridge equipped with an electrophotographic photosensitive member. A cylindrical electrophotographic photoreceptor 1 is driven to rotate around an axis 2 at a predetermined peripheral speed in the direction of the arrow. The surface of the electrophotographic photoreceptor 1 is charged to a predetermined positive or negative potential by a charging means 3. Although the figure shows a roller charging method using a roller-type charging member, a corona charging method, a proximity charging method, an injection charging method, or other charging methods may be adopted. Exposure light 4 is irradiated from an exposure means (not shown) onto the charged surface of the electrophotographic photoreceptor 1, and an electrostatic latent image corresponding to the target image information is formed. The electrostatic latent image formed on the surface of the electrophotographic photoreceptor 1 is developed with toner contained in a developing means 5, and a toner image is formed on the surface of the electrophotographic photoreceptor 1. The toner image formed on the surface of the electrophotographic photoreceptor 1 is transferred to a transfer material 7 by a transfer means 6. The transfer material 7 to which the toner image has been transferred is transported to a fixing means 8, where the toner image is fixed, and the transfer material is printed out outside the electrophotographic device. The electrophotographic device may have a cleaning means 9 for removing deposits such as toner remaining on the surface of the electrophotographic photoreceptor 1 after transfer. Also, a so-called cleanerless system may be used in which the deposits are removed by the developing means 5 or the like without separately providing the cleaning means 9. The electrophotographic apparatus may have a charge eliminating mechanism that eliminates charge on the surface of the electrophotographic photoreceptor 1 by pre-exposure light 10 from a pre-exposure means (not shown). Also, in order to mount and remove the process cartridge 11 according to the present invention to the main body of the electrophotographic apparatus, a guide means 12 such as a rail may be provided.

[0069] The electrophotographic photoreceptor of the present invention can be used in laser beam printers, LED printers, copiers, facsimiles, and combination machines thereof. EXAMPLES

[0070] The present invention will be described in more detail below using examples and comparative examples. The present invention is not limited to the following examples without departing from the gist of the present invention. In the following description of the examples, "parts" are based on mass unless otherwise specified. First, examples of the synthesis of a polymer (electron transport material) having a structural unit represented by formula (1) and a polymer (electron transport material) having a structural unit represented by formula (2) will be shown.

[0071] [Synthesis example of a polymer having a structural unit represented by formula (1) (example of compound: P-3)] The following materials were prepared: 50 parts N-methylpyrrolidone 1.96 parts of 3,4,9,10-perylenetetracarboxylic dianhydride (Tokyo Chemical Industry Co., Ltd.) Poly(propylene glycol) bis(2-aminopropyl ether) (Mn230, Sigma-Aldrich) 1.38 parts These were mixed and heated to 180°C while stirring, and reacted for 48 hours, after which the mixture was cooled. Then, the mixture was poured into 50 ml of water, and the precipitate was filtered off. The precipitate obtained was washed with hot water and then dried to obtain 3.0 parts of a polymer (P-3) having a structural unit represented by formula (1). The obtained compound was identified by NMR. For identification, measurement was performed using 1H-NMR (400 MHz, JMN-EX400, JEOL) using CDCl3 as a solvent. As a result, the target product was confirmed to have the following peak positions. δ8.6-7.8ppm (broad m, perylene site) δ4.3-4.1ppm (broad m, alkyl moiety linked to imide nitrogen) δ4.0-3.2ppm (broad m, ether portion) δ1.60-1.11ppm (broad s, methyl group) The weight average molecular weight of the obtained polymer is shown in Table 23. The weight average molecular weight (Mw) was measured by GPC (gel permeation chromatography) using HLC-8220 manufactured by Tosoh Corporation, and expressed as a polystyrene equivalent value.

[0072] [Synthesis example of a polymer having a structural unit represented by formula (2) (example of compound: N-3)] The following materials were prepared: 50 parts N,N-dimethylacetamide 1,4,5,8-naphthalenetetracarboxylic dianhydride (Tokyo Chemical Industry Co., Ltd.) 1.34 parts Poly(propylene glycol) bis(2-aminopropyl ether) (Mn230, Sigma-Aldrich) 1.38 parts These were mixed and heated to 100°C while stirring, and reacted for 24 hours, after which the mixture was cooled. Then, the mixture was poured into 50 ml of water, and the precipitate was filtered off. The precipitate obtained was washed with hot water and then dried to obtain 3.0 parts of a polymer (N-3) having a structural unit represented by the naphthalene diformula (2). The obtained compound was identified by NMR. For identification, measurement was performed using 1H-NMR (400 MHz, JMN-EX400, JEOL) using CDCl3 as a solvent. As a result, the target product was confirmed to have the following peak positions. δ8.72ppm (s, naphthalene portion) δ5.44ppm (m, proton of carbon adjacent to imide nitrogen) δ4.17ppm (broad m, ether portion) δ2.02 (broad m, alkyl moiety) δ1.52-1.10ppm (broad s, methyl group) The weight average molecular weight of the obtained polymer is shown in Table 32. The weight average molecular weight (Mw) was measured by GPC (gel permeation chromatography) using HLC-8220 manufactured by Tosoh Corporation, and expressed as a polystyrene equivalent value.

[0073] A synthesis example of an electron transport material used in a comparative example will be described below. [Synthesis example of electron transport material (D01)] The following materials were prepared: 1.96 parts of 3,4,9,10-perylenetetracarboxylic dianhydride (Tokyo Chemical Industry Co., Ltd.) DL-2-amino-1-butanol (Tokyo Chemical Industry Co., Ltd.) 0.89 parts These were mixed with 100 parts of dimethylacetamide under a nitrogen atmosphere and stirred at room temperature for 1 hour to prepare a suspension. The resulting suspension was then refluxed for 8 hours, and the precipitate was filtered off and recrystallized with ethyl acetate to obtain 2.67 parts of an electron transport material (D01). The obtained compound was identified by NMR. For identification, 1H-NMR (400MHz, JMN-EX400, JEOL) was measured using CDCl3 as a solvent. As a result, the target compound was confirmed to have the following peak positions. δ9.0ppm (s, hydroxyl group) δ8.64ppm (dd, perylene site) δ5.03ppm (m, proton on the carbon adjacent to the imide nitrogen) δ4.08-3.78ppm (m, ether portion) δ1.90-1.70ppm (m, methylene group) δ0.95ppm (dd, methyl group)

[0074] [Synthesis example of electron transport material (D06)] 4.65 parts of 2,2'-dihydroxybiphenyl was dissolved in 1000 parts of chloroform, 50 parts of Fetizon reagent (ferrite-supported silver carbonate) was added, and the mixture was heated under reflux for 40 hours. After heating, the reaction solution was returned to room temperature, the Fetizon reagent was filtered, the solvent in the filtrate was removed, and the residue was dispersed and washed with 500 parts of methanol. Dispersion washing was repeated three times to obtain a brown solid. The yield was 0.85 parts, and the weight average molecular weight (Mw) measured by GPC was 5300.

[0075] [Synthesis example of electron transport material (D07)] To 100 parts of dimethylacetamide, 5.4 parts of 1,4,5,8-naphthalenetetracarboxylic dianhydride (Tokyo Chemical Industry Co., Ltd.) and 3.0 parts of 3,5-diaminobenzoic acid (Tokyo Chemical Industry Co., Ltd.) were added under a nitrogen atmosphere. After stirring at room temperature for 1 hour, the mixture was refluxed for 8 hours, and the precipitate was filtered off. The precipitate was washed with acetone to obtain 6.2 parts of electron transport material (D07). The product obtained was in the form of particles.

[0076] [Example 1] [Manufacturing of electrophotographic photoreceptors] <Support> An aluminum cylinder with a length of 260.5 mm and a diameter of 30 mm was prepared. This aluminum cylinder was machined (JIS B 0601:2014, ten-point average roughness Rzjis: 0.8 μm), and the machined aluminum cylinder was used as a support (conductive support).

[0077] <Undercoat layer> Next, 5 parts of exemplary compound (P-1) as an electron transport material was dissolved in a mixed solvent of 48 parts of chloroform and 24 parts of o-xylene. The obtained coating solution for undercoat layer was dip-coated on a support, and the obtained coating film was heated at 170° C. for 40 minutes and dried to form an undercoat layer with a thickness of 1.5 μm.

[0078] <Charge generation layer> Next, hydroxygallium phthalocyanine crystals (charge generating material) having peaks at Bragg angles (2θ±0.2°) of 7.5°, 9.9°, 12.5°, 16.3°, 18.6°, 25.1°, and 28.3° in CuKα characteristic X-ray diffraction were prepared. 10 parts of this hydroxygallium phthalocyanine crystal, 5 parts of polyvinyl butyral resin (trade name: S-LEC BX-1, manufactured by Sekisui Chemical Co., Ltd.), and 250 parts of cyclohexanone were placed in a sand mill using glass beads with a diameter of 1 mm, and dispersed for 2 hours. Next, 250 parts of ethyl acetate were added to this to prepare a coating liquid for a charge generating layer. This coating liquid for a charge generating layer was applied by dip coating on the undercoat layer to form a coating film, and the resulting coating film was dried at a temperature of 95° C. for 10 minutes to form a charge generating layer having a thickness of 0.15 μm.

[0079] <Charge transport layer> The following materials were prepared: As a charge transport material, 5 parts of a charge transport material represented by the following formula: [ka] 5 parts of a charge transport material compound represented by the following formula: [ka] Polycarbonate (product name: Iupilon Z-400, manufactured by Mitsubishi Engineering Plastics) 10 parts These were dissolved in a mixed solvent of 25 parts of orthoxylene / 25 parts of methyl benzoate / 25 parts of dimethoxymethane to prepare a coating solution for the charge transport layer. The charge transport layer coating liquid thus prepared was dip-coated onto the charge generation layer to form a coating film, and the coating film was dried by heating at a temperature of 120° C. for 30 minutes to form a charge transport layer having a thickness of 25 μm.

[0080] [evaluation] Evaluation of potential fluctuations A laser beam printer (product name: Laser Jet Enterprise M609dn) manufactured by Hewlett-Packard was prepared for the evaluation of potential fluctuations. For the evaluation, the laser beam printer was modified so that it could operate at a process speed of 370 mm / s, with variable charging conditions, and variable laser exposure. The potential fluctuation was evaluated as follows. The manufactured electrophotographic photoreceptor was mounted in the above-mentioned laser beam printer manufactured by Hewlett-Packard Co., Ltd., and placed in an environment of normal temperature and normal humidity (23° C. / 50% RH). The surface potential of the electrophotographic photoreceptor was initially −500 V for the non-exposed area potential and 0.3 μJ / cm for the exposure light amount. 2 The potential of the exposed portion was measured after 10,000 sheets were passed through (hereinafter also referred to as after durability). The surface potential was measured by modifying the cartridge, attaching a potential probe (model 6000B-8, Trek Japan Co., Ltd.) to the development position, and measuring the potential at the center of the drum using a surface potential meter (model 344, Trek Japan Co., Ltd.). During paper passing, a character image with a print rate of 1% was printed on A4-sized plain paper, and 10,000 sheets of image output were performed. That is, as described above, in the present invention, the potential fluctuation was evaluated as a value calculated from the amount of fluctuation between the initial state and after durability. The results are shown in Table 23.

[0081] Evaluation of Electron Mobility The electron mobility was determined by the time of flight method. It is known that the electron mobility depends on the electric field strength. 7 The values ​​used were those in V / m. The specific measurement method is as follows. First, for the evaluation of electron mobility, the undercoat layer coating liquid was applied to an aluminum sheet with a wire bar and dried at 160°C for 10 minutes to form an undercoat layer with a thickness of 5.0 μm. Thereafter, the charge generation layer coating liquid was applied to the aluminum sheet with a wire bar and dried at 100°C for 10 minutes to form a charge generation layer with a thickness of 0.2 μm to prepare a measurement sample. The measurement sample thus prepared was sandwiched between glass transparent electrodes coated with a conductive material such as ITO coating to form a circuit consisting of a power source and a resistor for measuring current. Next, an electric field of 3.0×10 7 After applying a voltage adjusted to V / m, the sample was irradiated with light from the transparent electrode side. At this time, electrons generated in the charge generation layer were injected into the undercoat layer, and the current waveform when they travel through the undercoat layer by hopping conduction was observed with an oscilloscope to obtain the travel time (t) of the carriers traveling within the sample. The speed (v=d / t) was calculated from this travel time (t) and the thickness (d) of the sample. Since the speed (v) is the product (v=μE) of the electron mobility (μ) and the electric field strength (E), the electron mobility (μ) in the sample was calculated by dividing the speed (v) by the electric field strength (E).

[0082] The mobilities obtained are shown in Table 23. The volume resistivity was also measured using the measurement samples prepared in the same manner. The results are shown in Table 23.

[0083] [Examples 2 to 6, 11 to 39, 44 to 417] Electrophotographic photoreceptors were produced and evaluated in the same manner as in Example 1, except that the electron transporting substance in Example 1 was changed to one shown in Tables 23 to 31. The results are shown in Tables 23 to 31.

[0084] [Example 7] An electrophotographic photoreceptor was produced and evaluated in the same manner as in Example 1, except that the undercoat layer was formed as follows. The results are shown in Table 23. <Undercoat layer> The following materials were prepared: 8 parts of exemplary compound (P-3) as an electron transport material 4.01 parts of a blocked isocyanate compound (product name: SBB-70P (solid content 70%, isocyanate:blocking group=6.7:3.3 (mass ratio), manufactured by Asahi Kasei)) as an isocyanate compound 0.12 parts of styrene-acrylic resin (product name: UC-3920, manufactured by Toagosei) These were dissolved in a mixed solvent consisting of 48 parts of 1-butanol and 24 parts of acetone. The obtained coating liquid for the undercoat layer was dip-coated onto a support, and the obtained coating film was heated at 170° C. for 40 minutes to be cured (polymerized) to form an undercoat layer with a thickness of 1.5 μm.

[0085] [Examples 8 to 10, 40 to 43] In Example 7, the amount of the electron transport material was changed to the amount shown in Table 23. The content ratio of the electron transport material, the isocyanate compound, and the resin in the undercoat layer was changed so that the content ratio (mass%) of the electron transport material in the undercoat layer became the value shown in Table 23. The ratio between the isocyanate compound and the resin was kept constant. Except for that, an electrophotographic photoreceptor was produced in the same manner as in Example 7 and evaluated in the same manner. The results are shown in Table 23.

[0086] [Examples 501 to 506, 511 to 539, 544 to 917] Electrophotographic photoreceptors were produced and evaluated in the same manner as in Example 1, except that the electron transporting substance in Example 1 was changed to one shown in Tables 32 to 40. The results are shown in Tables 32 to 40.

[0087] [Examples 507 to 510, 540 to 543] In Example 7, the amount of the electron transport material was changed to the amount shown in Table 32. The content ratio of the electron transport material, the isocyanate compound, and the resin in the undercoat layer was changed so that the content ratio (mass%) of the electron transport material in the undercoat layer became the value shown in Table 32. The ratio between the isocyanate compound and the resin was kept constant. Except for that, an electrophotographic photoreceptor was produced in the same manner as in Example 7, and evaluated in the same manner. The results are shown in Table 32.

[0088] [Examples 418, 918] The support was changed to the one described below, a conductive layer was formed on the support as described below, and an undercoat layer, a charge generating layer, and a charge transport layer were formed on the conductive layer in the same manner as in Examples 1 and 501, to produce and evaluate electrophotographic photoreceptors. The results are shown in Tables 31 and 40.

[0089] <Support> An aluminum cylinder having a diameter of 30 mm and a length of 260.5 mm was used as a support (cylindrical support).

[0090] <Conductive layer> An anatase-type titanium oxide having an average primary particle size of 200 nm was used as the substrate, and a titanium niobium sulfate solution containing 33.7 parts of titanium in terms of TiO2 and 2.9 parts of niobium in terms of Nb2O5 was prepared. 100 parts of the substrate was dispersed in pure water to prepare a suspension of 1000 parts, which was then heated to 60°C. The titanium niobium sulfate solution and 10 mol / L sodium hydroxide were dropped into the suspension over 3 hours so that the pH of the suspension was 2 to 3. After the entire amount was dropped, the pH was adjusted to near neutral, and a polyacrylamide-based flocculant was added to precipitate the solids. The supernatant was removed, filtered, washed, and dried at 110°C to obtain an intermediate containing 0.1 mass% of organic matter derived from the flocculant in terms of C. This intermediate was calcined in nitrogen at 750°C for 1 hour, and then calcined in air at 450°C to produce titanium oxide particles. The obtained particles had an average particle size (average primary particle size) of 220 nm as determined by a particle size measurement method using a scanning electron microscope. Next, a phenolic resin (phenolic resin monomer / oligomer) was used as a binder (product name: Plyofen J-325, manufactured by DIC, resin solid content: 60%, density after curing: 1.3 g / cm 2 50 parts of this phenol resin were dissolved in 35 parts of 1-methoxy-2-propanol as a solvent to obtain a solution. To this solution, 60 parts of titanium oxide particles were added, and the mixture was placed in a vertical sand mill using 120 parts of glass beads with an average particle size of 1.0 mm as a dispersion medium, and dispersion treatment was carried out for 4 hours under conditions of a dispersion temperature of 23±3°C and a rotation speed of 1500 rpm (circumferential speed of 5.5 m / s) to obtain a dispersion. The glass beads were removed from this dispersion using a mesh. Next, the following materials were prepared: 0.01 part silicone oil as a leveling agent (product name: SH28 PAINT ADDITIVE, manufactured by Toray Dow Corning) Silicone resin particles (product name: KMP-590, manufactured by Shin-Etsu Chemical Co., Ltd., average particle size: 2 μm, density: 1.3 g / cm) were used as a surface roughening agent. 3 ) 8 copies These were added to the dispersion liquid after removing the glass beads, stirred, and filtered under pressure using PTFE filter paper (product name: PF060, manufactured by Advantec Toyo) to prepare a coating liquid for the conductive layer. The conductive layer coating liquid thus prepared was dip-coated onto the above-mentioned support to form a coating film, and the coating film was heated at 150° C. for 20 minutes to be cured, thereby forming a conductive layer having a thickness of 25 μm.

[0091] [Comparative Example 1] An electrophotographic photoreceptor was produced and evaluated in the same manner as in Example 1, except that the electron transporting material (P-1) in Example 1 was changed to the electron transporting material (D01). The results are shown in Table 41. In Table 41, "Nd" indicates that the value was not determined because it was not possible to measure. The reason for this is thought to be that after the undercoat layer was formed, the sample was immersed in the charge generating layer coating liquid, and then a part of the undercoat layer was dissolved. [ka]

[0092] [Comparative Examples 2 to 5] In Example 7, the electron transport material (P-3) was changed to the amount of electron transport material shown in Table 41. The content ratio of the electron transport material, the isocyanate compound, and the resin in the undercoat layer was changed so that the content ratio (mass%) of the electron transport material in the undercoat layer became the value shown in Table 41. The ratio between the isocyanate compound and the resin was kept constant. Except for that, an electrophotographic photoreceptor was produced in the same manner as in Example 7 and evaluated in the same manner. The results are shown in Table 41.

[0093] [Comparative Example 6] An electrophotographic photoreceptor was produced and evaluated in the same manner as in Comparative Example 3, except that the electron transporting material (D01) in Comparative Example 3 was changed to the electron transporting material (D04). The results are shown in Table 41. [ka]

[0094] [Comparative Example 7] An electrophotographic photoreceptor was produced and evaluated in the same manner as in Comparative Example 3, except that the electron transporting material (D01) in Comparative Example 3 was changed to the electron transporting material (D05). The results are shown in Table 41. [ka]

[0095] [Comparative Example 8] In Example 1, the electron transport material (P-1) was changed to the electron transport material (D06). In addition, an electrophotographic photoreceptor was produced and evaluated in the same manner as in Example 1, except that the undercoat layer was formed as follows. The results are shown in Table 41. <Undercoat layer> 8 parts of the electron transport material (D06) was dissolved in 80 parts of chloroform. The obtained coating solution for the undercoat layer was dip-coated on a support, and the obtained coating film was heated at 100° C. for 15 minutes and dried to form an undercoat layer with a thickness of 1.5 μm. [ka]

[0096] [Comparative Example 9] In Example 506, the electron transport material (N-3) was changed to the electron transport material (D07). In addition, an electrophotographic photoreceptor was produced and evaluated in the same manner as in Example 506, except that the undercoat layer was formed as follows. The results are shown in Table 41. [ka] <Undercoat layer> 40 parts of the electron transport material (D07) and 500 parts of distilled water, 300 parts of methanol, and 8 parts of triethylamine as a dispersion medium were mixed and dispersed for 2 hours in a sand mill using glass beads with a diameter of 1 mm to prepare a coating solution for an undercoat layer. The obtained coating solution for an undercoat layer was dip-coated on a support, and the obtained coating film was heated at 120°C for 10 minutes and dried to form an undercoat layer with a thickness of 1.5 μm.

[0097] [Comparative Example 10] In Example 506, the electron transport material (N-3) was changed to the electron transport material (D08). In addition, an electrophotographic photoreceptor was produced and evaluated in the same manner as in Example 506, except that the undercoat layer was formed as follows. The results are shown in Table 41. [ka] In the structure of the electron transport material (D08), the ratio of the repeating units is indicated by mole percent. <Undercoat layer> 40 parts of the electron transport material (D08) and 300 parts of distilled water, 500 parts of methanol, and 8 parts of triethylamine as a dispersion medium were mixed and dispersed for 2 hours in a sand mill using glass beads with a diameter of 1 mm to prepare a coating solution for an undercoat layer. The obtained coating solution for an undercoat layer was dip-coated on a support, and the obtained coating film was heated at 120°C for 10 minutes and dried to form an undercoat layer with a thickness of 1.5 μm.

[0098] [Table 23]

[0099]

Table 24

[0100]

Table 25

[0101]

Table 26

[0102]

Table 27

[0103]

Table 28

[0104]

Table 29

[0105]

Table 30

[0106]

Table 31

[0107]

Table 32

[0108]

Table 33

[0109]

Table 34

[0110] [Table 35]

[0111] [Table 36]

[0112] [Table 37]

[0113] [Table 38]

[0114] [Table 39]

[0115] [Table 40]

[0116] [Table 41]

[0117] The disclosure according to an embodiment of the present invention includes the following configuration. (Configuration 1) An electrophotographic photoreceptor having a support, an undercoat layer, and a photosensitive layer in this order, The undercoat layer contains at least one polymer selected from the group consisting of a polymer having a structural unit represented by the following formula (1) and a polymer having a structural unit represented by the following formula (2): [ka] [ka] (In formulas (1) and (2), α, β, and γ represent structures represented by the following formulae (α), (β), and (γ), respectively. R 11 , R 12 , R 13 , R 14 , R 15 , R 16 , R 17 , R 18 , R 21 ,R 22 , R 23 , and R 24 each independently represents a hydrogen atom, a halogen atom, a nitro group, a cyano group, a trifluoromethyl group, a substituted or unsubstituted alkoxy group, a substituted or unsubstituted thiol group, a substituted or unsubstituted amino group, a substituted or unsubstituted alkyl group, a substituted or unsubstituted alkynyl group, or a substituted or unsubstituted aryl group. [ka] [ka] [ka] (In the formulas (α), (β), and (γ), R 60 , R 61 , R 70 , R 71 , R 80 , and R 81 each independently represents a hydrogen atom, a substituted or unsubstituted alkyl group, or a substituted or unsubstituted aryl group, Z a , Z b , and Z c each independently represents a single bond, an imino group, an oxygen atom, or a sulfur atom, l a , l b , and l c each independently represents an integer of 0 or more, m a is an integer equal to or greater than 1, m b and m c each independently represents an integer of 0 or more, Z a When represents a single bond, R 60 represents a substituted or unsubstituted alkyl group, Z a represents an imino group or a sulfur atom, R 60 represents a hydrogen atom or a substituted or unsubstituted alkyl group, Z a represents an oxygen atom, and R 60 When represents a hydrogen atom, m a indicates an integer of 2 or more, Z a represents an oxygen atom, and R 60 When m represents a substituted or unsubstituted alkyl group, a indicates an integer of 1 or greater.) (Configuration 2) The electrophotographic photoreceptor according to Configuration 1, wherein the content of at least one polymer selected from the group consisting of the polymer having a structural unit represented by Formula (1) and the polymer having a structural unit represented by Formula (2) is 50% by mass or more relative to the total mass of the undercoat layer. (Configuration 3) R in formula (1) 11 , R 12 , R 13 , R 14 , R 15 , R 16 , R 17 , and R 18 and R in formula (2). 21 ,R 22 , R 23 , and R 24at least one of which is independently a halogen atom, a nitro group, a cyano group, a trifluoromethyl group, a substituted or unsubstituted alkoxy group having 20 carbon atoms or less, a substituted or unsubstituted thiol group having 20 carbon atoms or less, a substituted or unsubstituted amino group having 20 carbon atoms or less, a substituted or unsubstituted alkyl group having 20 carbon atoms or less, a substituted or unsubstituted alkynyl group having 20 carbon atoms or less, or a substituted or unsubstituted aryl group having 20 carbon atoms or less. (Configuration 4) R in formula (α) 60 and R 61 R in formula (β) 70 and R 71 , and R in formula (γ) 80 and R 81 4. The electrophotographic photoreceptor according to any one of configurations 1 to 3, wherein at least one of the groups is a substituted or unsubstituted alkyl group having 20 or less carbon atoms or a substituted or unsubstituted aryl group having 20 or less carbon atoms. (Configuration 5) l in formula (α) a , l in formula (β) b , and l in formula (γ) c and each independently represent an integer of 0 or more and 10 or less. (Configuration 6) m in formula (α) a is an integer between 1 and 40, m in formula (β) b and m in formula (γ) c and each independently represent an integer of 0 or more and 40 or less. (Configuration 7) R in formula (α) 60 7. The electrophotographic photoreceptor according to any one of configurations 1 to 6, wherein represents a substituted or unsubstituted alkyl group having 20 or less carbon atoms. (Configuration 8) m in formula (α) a is an integer between 2 and 30, m in formula (α) a and m in formula (β) b and m in formula (γ) cThe electrophotographic photoreceptor according to any one of Configurations 1 to 7, wherein the sum of and is 3 or more and 30 or less. (Configuration 9) The electrophotographic photoreceptor according to any one of configurations 1 to 8, wherein the weight average molecular weight of at least one polymer selected from the group consisting of a polymer having a structural unit represented by formula (1) and a polymer having a structural unit represented by formula (2) is 30,000 or less. (Configuration 10) The volume resistivity of the undercoat layer is 1×10 10 10. The electrophotographic photoreceptor according to any one of configurations 1 to 9, which has a resistivity of Ω·cm or more. (Configuration 11) A process cartridge which integrally supports the electrophotographic photosensitive member according to any one of configurations 1 to 10 and at least one means selected from the group consisting of a charging means, a developing means and a cleaning means, and is detachably mountable to an electrophotographic apparatus. (Configuration 12) 11. An electrophotographic apparatus comprising: an electrophotographic photoreceptor according to any one of Configurations 1 to 10; a charging means, an exposure means, a developing means, and a transfer means. [Explanation of symbols]

[0118] 101:Support 102: Undercoat layer 103: Charge generating layer 104: Charge transport layer 105: Photosensitive layer 1: Electrophotographic photoreceptor 2: Axis 3: Charging means 4: Image exposure light 5: Developing method 6: Transfer method 7: Transfer material 8: Image fixing means 9: Cleaning means 10: Pre-exposure light 11: Process cartridge 12: Guidance means

Claims

1. An electrophotographic photoreceptor having a support, an undercoat layer, and a photosensitive layer in this order, the undercoat layer contains at least one polymer selected from the group consisting of a polymer having a structural unit represented by the following formula (1) and a polymer having a structural unit represented by the following formula (2): 【Chemistry 1】 【Chemistry 2】 (In formulas (1) and (2), α, β, and γ represent structures represented by the following formulae (α), (β), and (γ), respectively. R 11 , R 12 , R 13 , R 14 , R 15 , R 16 , R 17 , R 18 , R 21 , R 22 , R 23 , and R 24 each independently represents a hydrogen atom, a halogen atom, a nitro group, a cyano group, a trifluoromethyl group, a substituted or unsubstituted alkoxy group, a substituted or unsubstituted thiol group, a substituted or unsubstituted amino group, a substituted or unsubstituted alkyl group, a substituted or unsubstituted alkynyl group, or a substituted or unsubstituted aryl group. 【Chemistry 3】 【Chemistry 4】 【Chemistry 5】 (In the formulas (α), (β), and (γ), R 60 , R 61 , R 70 , R 71 , R 80 , and R 81 each independently represents a hydrogen atom, a substituted or unsubstituted alkyl group, or a substituted or unsubstituted aryl group, Z a , Z b , and Z c each independently represents a single bond, an imino group, an oxygen atom, or a sulfur atom, l a , l b , and l c each independently represents an integer of 0 or more, m a is an integer equal to or greater than 1, m b and m c each independently represents an integer of 0 or more, Z a When represents a single bond, R 60 represents a substituted or unsubstituted alkyl group, Z a represents an imino group or a sulfur atom, R 60 represents a hydrogen atom or a substituted or unsubstituted alkyl group, Z a represents an oxygen atom, and R 60 When represents a hydrogen atom, m a represents an integer of 2 or more, Z a represents an oxygen atom, and R 60 represents a substituted or unsubstituted alkyl group, m a represents an integer of 1 or more.)

2. 2. The electrophotographic photoreceptor according to claim 1, wherein a content ratio of the at least one polymer selected from the group consisting of a polymer having a structural unit represented by formula (1) and a polymer having a structural unit represented by formula (2) relative to a total mass of the undercoat layer is 50 mass% or more.

3. R in formula (1) 11 , R 12 , R 13 , R 14 , R 15 , R 16 , R 17 , and R 18 and R in formula (2) 21 , R 22 , R 23 , and R 24 and at least one of the above is independently a halogen atom, a nitro group, a cyano group, a trifluoromethyl group, a substituted or unsubstituted alkoxy group having 20 or less carbon atoms, a substituted or unsubstituted thiol group having 20 or less carbon atoms, a substituted or unsubstituted amino group having 20 or less carbon atoms, a substituted or unsubstituted alkyl group having 20 or less carbon atoms, a substituted or unsubstituted alkynyl group having 20 or less carbon atoms, or a substituted or unsubstituted aryl group having 20 or less carbon atoms.

4. R in formula (α) 60 and R 61 , R in formula (β) 70 and R 71 and R in formula (γ) 80 and R 81 2. The electrophotographic photoreceptor according to claim 1, wherein at least one of the groups is a substituted or unsubstituted alkyl group having 20 or less carbon atoms or a substituted or unsubstituted aryl group having 20 or less carbon atoms.

5. l in formula (α) a , l in formula (β) b and l in formula (γ) c and each independently represents an integer of 0 or more and 10 or less.

6. m in formula (α) a is an integer between 1 and 40, m in formula (β) b And m in formula (γ) c and each independently represent an integer of 0 or more and 40 or less.

7. R in formula (α) 60 2. The electrophotographic photoreceptor according to claim 1, wherein is a substituted or unsubstituted alkyl group having 20 or less carbon atoms.

8. m in formula (α) a is an integer between 2 and 30, m in formula (α) a and m in formula (β) b and m in formula (γ) c The electrophotographic photoreceptor according to claim 1 , wherein the sum of and is 3 or more and 30 or less.

9. 2. The electrophotographic photoreceptor according to claim 1, wherein the weight average molecular weight of the at least one polymer selected from the group consisting of a polymer having a structural unit represented by formula (1) and a polymer having a structural unit represented by formula (2) is 30,000 or less.

10. The volume resistivity of the undercoat layer is 1×10 10 The electrophotographic photoreceptor according to claim 1 , which has a surface area of ​​Ω·cm or more.

11. 11. A process cartridge which integrally supports the electrophotographic photosensitive member according to any one of claims 1 to 10 and at least one means selected from the group consisting of a charging means, a developing means and a cleaning means, and is detachably mountable to an electrophotographic apparatus.

12. 11. An electrophotographic apparatus comprising: the electrophotographic photoreceptor according to claim 1; a charging unit, an exposing unit, a developing unit, and a transferring unit.

Citation Information

Patent Citations

  • Polymer, electrophotography photoreceptor containing the polymer, process cartridge having the electrophotography photoreceptor and electrophotography device

    JP1999228675A

  • Aqueous coating liquid, method for manufacturing electrophotographic photoreceptor, and electrophotographic photoreceptor

    JP2012032458A

  • Electrophotographic photoreceptor, method for producing electrophotographic photoreceptor, process cartridge, electrophotographic apparatus, and imide compound

    JP2014029479A