Target

A specific In1+xM1-xO3(ZnO)y oxide semiconductor film composition addresses the issue of spinel-type crystal structure formation in In-Ga-Zn-based films, enhancing electrical characteristics and reliability through sputtering with a polycrystalline target, achieving high-performance semiconductor devices.

JP2024152756AActive Publication Date: 2024-10-25SEMICON ENERGY LAB CO LTD
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
JP2024129712
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2015-11-02
Filing Date
2024-08-06
Publication Date
2024-10-25
Estimated Expiration
2036-02-11

AI Technical Summary

Technical Problem

The formation of a spinel-type crystal structure in In-Ga-Zn-based oxide semiconductor films can adversely affect the electrical characteristics and reliability of transistors, leading to potential variations in crystallinity and electrical properties.

Method used

The development of an oxide semiconductor film with a specific composition of In1+xM1-xO3(ZnO)y, where x is between 0 and 0.5, and y is approximately 1, formed using a sputtering device with a polycrystalline metal oxide target, ensuring a single-phase homologous phase and c-axis orientation, and maintaining low hydrogen and impurity concentrations.

Benefits of technology

This approach enhances the electrical characteristics and reliability of semiconductor devices by providing a novel oxide semiconductor film with improved carrier mobility and reduced impurity and defect levels, resulting in high-performance semiconductor devices.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024152756000001_ABST
    Figure 2024152756000001_ABST
Patent Text Reader

Abstract

To provide a novel oxide semiconductor film.SOLUTION: An oxide semiconductor film includes In, M (M represents Al, Ga, Y, or Sn), and Zn. The oxide semiconductor film has a composition near a solid solution range of a structure of In1+xM1-xO3(ZnO)y (x is a number that satisfies 0<x<0.5, and y approximately represents 1). In particular, the ratio of the number of atoms of In, M, and Zn in the oxide semiconductor film is around In:M:Zn=4:2:3, and when In is 4, M is 1.5 or more and 2.5 or less, and Zn is 2 or more and 4 or less.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Citation Information

Patent Citations

  • Oxide semiconductor film and semiconductor device

    JP2012134475A

  • Method of manufacturing semiconductor device

    JP2013157359A

  • Semiconductor device

    JP2014007399A

  • Semiconductor device

    JP2014030001A

  • Manufacturing method of sputtering target, deposition method of oxide film, and transistor

    JP2014194076A