Super-junction silicon carbide semiconductor device and method for manufacturing the super-junction silicon carbide semiconductor device

The superjunction silicon carbide semiconductor device addresses the trade-off between on-resistance and breakdown voltage by using a parallel pn structure with phosphorus and nitrogen ion implantation, enhancing carrier distribution and reducing switching loss for improved performance in power electronics.

JP2024153517APending Publication Date: 2024-10-29NATIONAL INSTITUTE OF ADVANCED INDUSTRIAL SCIENCE & TECHNOLOGY +1

Patent Information

Application Number
JP2023067498
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-17
Publication Date
2024-10-29

AI Technical Summary

Technical Problem

Conventional superjunction silicon carbide semiconductor devices face challenges in achieving a balance between low on-resistance and high breakdown voltage due to the trade-off relationship between the thickness of the n-type drift layer, which affects depletion layer spread and electric field strength, leading to difficulties in improving both characteristics simultaneously.

Method used

The proposed superjunction silicon carbide semiconductor device employs a parallel pn structure with alternating p-type and n-type column regions, utilizing phosphorus and nitrogen ion implantation to form semiconductor layers, which reduces in-plane carrier concentration distribution and increases ion implantation damage, thereby enhancing the balance between on-resistance and breakdown voltage.

Benefits of technology

This approach improves the in-plane carrier concentration distribution and reduces switching loss by minimizing carrier accumulation in the drift layer, allowing for reduced component count and module size in circuits, while maintaining high breakdown voltage and low on-resistance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024153517000001_ABST
    Figure 2024153517000001_ABST
Patent Text Reader

Abstract

To provide a super-junction silicon carbide semiconductor device and a method for manufacturing the super-junction silicon carbide semiconductor device that can reduce the effect of in-plane carrier concentration distribution when forming an n-type semiconductor layer.SOLUTION: A super-junction silicon carbide semiconductor device includes a silicon carbide semiconductor substrate 1, a first semiconductor layer 17 of a first conductivity type, a parallel pn region 21 in which first column regions 4 of the first conductivity type and second column regions 3 of the second conductivity type are repeatedly and alternately arranged, a second semiconductor layer 5 of the first conductivity type, a third semiconductor layer 6 of the second conductivity type, a first semiconductor region 7 of the first conductivity type, a trench 16, a second semiconductor region 14 of the second conductivity type, a third semiconductor region 15 of the second conductivity type, a gate electrode 10, and a first electrode 12. The first column region 4 and the second column region 3 contain phosphorus as an impurity.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a super junction silicon carbide semiconductor device and a method for manufacturing a super junction silicon carbide semiconductor device. [Background technology]

[0002] In conventional silicon carbide MOSFETs (metal oxide semiconductor field effect transistors), a high-quality interface between the gate oxide film and silicon carbide is created by combining epitaxial growth and ion implantation, achieving low resistance. Furthermore, a structure that prevents a high electric field from being applied to the gate oxide film realizes a semiconductor device with high breakdown voltage and high reliability (see, for example, Patent Document 1 below).

[0003] For example, to achieve low resistance, a high-quality interface between the gate oxide film and silicon carbide is created, and the impurity concentration in the JFET (Junction Field Effect Transistor) is increased, thereby achieving low resistance. In addition, a p-type region is formed under the gate electrode to reduce the electric field, achieving high voltage resistance and high reliability. A deep p-type region is formed under the contact region to prevent the avalanche current that occurs when a high voltage exceeding the performance limit is applied to the drain electrode from flowing near the gate electrode, thereby reducing the load on the gate electrode. The deep p-type region under the contact region also prevents large currents from flowing near the gate electrode even when the built-in diode is operating, thereby reducing the load on the gate electrode and improving reliability.

[0004] In a typical n-type channel vertical MOSFET, the n-type conduction layer (drift layer) is the semiconductor layer with the highest resistance among the multiple semiconductor layers formed in the semiconductor substrate. The electrical resistance of this n-type drift layer has a large effect on the on-resistance of the entire vertical MOSFET. In order to reduce the on-resistance of the entire vertical MOSFET, it is possible to reduce the thickness of the n-type drift layer and shorten the current path.

[0005] However, the vertical MOSFET also has a function of maintaining a breakdown voltage by expanding the depletion layer to the high-resistance n-type drift layer in the off state. Therefore, if the n-type drift layer is thinned to reduce the on-resistance, the expansion of the depletion layer in the off state becomes shorter, so that the breakdown field strength is easily reached at a low applied voltage, and the breakdown voltage decreases. On the other hand, in order to increase the breakdown voltage of the vertical MOSFET, it is necessary to increase the thickness of the n-type drift layer, which increases the on-resistance. Such a relationship between the on-resistance and the breakdown voltage is called a trade-off relationship, and it is generally difficult to improve both of them in the trade-off relationship. It is known that this trade-off relationship between the on-resistance and the breakdown voltage also holds true in semiconductor devices such as IGBTs (Insulated Gate Bipolar Transistors), bipolar transistors, and diodes.

[0006] A super junction (SJ) structure is known as a semiconductor device structure that solves the above-mentioned problems (see, for example, Patent Documents 2 and 3 below). Fig. 14 is a cross-sectional view showing the structure of a conventional super junction silicon carbide semiconductor device.

[0007] 14 shows a MOSFET having a super junction structure (hereinafter, SJ-MOSFET) as a super junction silicon carbide semiconductor device. As shown in FIG. 14, the SJ-MOSFET 150 has a high impurity concentration n + The wafer is made of a silicon carbide semiconductor substrate 101 on which an n-type buffer layer 117 and an n-type drift layer 102 are grown. + The p-type column region 103 does not reach the n-type silicon carbide semiconductor substrate 101. In FIG. + The n-type silicon carbide semiconductor substrate 101 is not reached, but + The silicon carbide semiconductor substrate 101 may be formed by the above-mentioned method.

[0008] In addition, the n-type drift layer 102 has a parallel structure (hereinafter referred to as a parallel pn structure 121) in which p-type regions (p-type column regions 103) and n-type regions (portions of the n-type drift layer 102 sandwiched between the p-type column regions 103, hereinafter referred to as n-type column regions 104) that extend in a direction perpendicular to the substrate main surface and have a narrow width in a plane parallel to the substrate main surface are alternately and repeatedly arranged in a plane parallel to the substrate main surface. The p-type column regions 103 and the n-type column regions 104 that constitute the parallel pn structure 121 are regions with a high impurity concentration corresponding to the n-type drift layer 102. In the parallel pn structure 121, the amount of impurities, which is the product of the impurity concentration and the area contained in the p-type column regions 103 and the n-type column regions 104, are approximately equal in charge balance, thereby creating a pseudo non-doped layer in the off state to achieve high voltage resistance.

[0009] In FIG. 14, reference numerals 105, 106, 107, 108, 109, 110, 111, 112, 114, 115, and 116 denote an n-type high concentration region, a p-type base layer, and an n-type + Type source region, p + A contact region, a gate insulating film, a gate electrode, an interlayer insulating film, a source electrode, a first p + Mold base region, 2nd p + The mold base region and trench are shown.

[0010] Also, a superjunction semiconductor element is described that includes a parallel pn layer in which first-conductivity-type drift regions and second-conductivity-type partition regions are alternately arranged, and in which the impurity in the first-conductivity-type drift region is phosphorus (see, for example, Patent Document 4 below). [Prior art documents] [Patent documents]

[0011] [Patent Document 1] International Publication No. 2017 / 064949 [Patent Document 2] International Publication No. 2013 / 0179820 [Patent Document 3] JP 2009-130106 A [Patent Document 4] JP 2006-100862 A Summary of the Invention [Problem to be solved by the invention]

[0012] In the method of manufacturing a super junction silicon carbide semiconductor device, since impurity elements are hardly diffused into silicon carbide (SiC), parallel pn structure 121 is formed by combining epitaxial growth and ion implantation. For example, SJ-MOSFET 150 is manufactured as follows. Figures 15 to 18 are cross-sectional views showing states during the manufacturing process of a conventional super junction silicon carbide semiconductor device.

[0013] First, we will use n-type single crystal 4H-SiC (four-layer hexagonal silicon carbide). + A silicon carbide substrate 101 is prepared. + An n-type buffer layer 117 and a first n-type drift layer 102a are epitaxially grown on the first main surface of the silicon carbide substrate 101. The state up to this point is shown in FIG.

[0014] Next, an ion implantation mask 122 having a predetermined opening is formed on the surface of the first n-type drift layer 102a by photolithography using a material such as SiO 2 A film (hereinafter referred to as an oxide film) is formed. Then, aluminum ions (hereinafter referred to as Al ions) are implanted into the openings of the oxide film to form the first p-type column region 103a. The state up to this point is shown in FIG.

[0015] Next, the second n-type drift layer 102b made of silicon carbide is epitaxially grown on the front surface side of the first n-type drift layer 102a while being doped with nitrogen atoms. The state up to this point is shown in FIG.

[0016] Next, an ion implantation mask 122 having a predetermined opening is formed on the surface of the second n-type drift layer 102b by photolithography. Then, Al ions are implanted into the opening of the oxide film to form the second p-type column region 103b. The state up to this point is shown in FIG.

[0017] 17 and the ion implantation process in FIG. 18 are repeated a predetermined number of times to form p-type column regions 103 and n-type column regions 104. Thereafter, n-type high concentration regions 105 are formed by epitaxial growth, and first p + The mold base region 114 and the second p + The first p-type column region 103a and the second p-type column region 103b become part of the p-type column region 103, and the first n-type drift layer 102a and the second n-type drift layer 102b become part of the n-type column region 104.

[0018] Next, a p-type base layer 106 doped with a p-type impurity such as aluminum is formed on the surface of the n-type high concentration region 105. Next, n + type source region 107 and p + This forms a mold contact region 108. Next, an annealing process is performed on the region where the ions have been implanted, and an activation process is performed.

[0019] Next, a trench 116, a gate insulating film 109, a gate electrode 110, an interlayer insulating film 111, a source electrode 112, a source electrode pad (not shown), a back electrode (not shown), and a drain electrode pad (not shown) are formed. In this manner, an SJ-MOSFET 150 shown in FIG. 14 is completed.

[0020] In this manner, conventional super junction silicon carbide semiconductor devices are fabricated (manufactured) by periodically implanting p-type dopants such as Al ions to a constant depth into a portion of n-type drift layer 102 of n-type single crystal 4H—SiC to form p-type column regions 103 and n-type column regions 104.

[0021] However, when a SiC epitaxial film in which the carrier concentration is controlled by doping with n-type impurities is used for the n-type semiconductor layers (first n-type drift layer 102a, second n-type drift layer 102b), there is a problem that the carrier concentration distribution becomes large due to the influence of substrate warpage, temperature distribution, gas flow rate distribution, and the like during epitaxial growth.

[0022] An object of the present invention is to provide a super junction silicon carbide semiconductor device and a method for manufacturing a super junction silicon carbide semiconductor device that can reduce the effect of in-plane carrier concentration distribution when forming an n-type semiconductor layer, in order to solve the problems associated with the conventional techniques described above. [Means for solving the problem]

[0023] In order to solve the above-mentioned problems and achieve the object of the present invention, a super junction silicon carbide semiconductor device according to the present invention has the following features. A first semiconductor layer of a first conductivity type is provided on a front surface of a silicon carbide semiconductor substrate of a first conductivity type. A parallel pn region in which first column regions of a first conductivity type and second column regions of a second conductivity type are repeatedly and alternately arranged in a plane parallel to the front surface is provided on a surface of the first semiconductor layer opposite to the silicon carbide semiconductor substrate. A second semiconductor layer of a first conductivity type is provided on a surface of the parallel pn region opposite to the silicon carbide semiconductor substrate. A third semiconductor layer of a second conductivity type is provided on a surface of the second semiconductor layer opposite to the silicon carbide semiconductor substrate. A first semiconductor region of a first conductivity type having an impurity concentration higher than that of the first semiconductor layer is selectively provided within the third semiconductor layer. A trench is provided penetrating the first semiconductor region and the third semiconductor layer to reach the second semiconductor layer. A second semiconductor region of a second conductivity type is provided in the second semiconductor layer in contact with a bottom of the trench. A third semiconductor region of a second conductivity type is provided in a surface layer of the second semiconductor layer between the trenches. A gate electrode is provided inside the trench via a gate insulating film. A first electrode is provided in contact with the first semiconductor region and the third semiconductor layer. The first column region and the second column region contain phosphorus as an impurity.

[0024] Moreover, the super junction silicon carbide semiconductor device according to the present invention is characterized in that, in the above-mentioned invention, the first column region is composed of a lower first column region on the silicon carbide semiconductor substrate side and an upper first column region on the second semiconductor layer side, the lower first column region containing nitrogen as an impurity, and the upper first column region and the second column region containing phosphorus as impurities.

[0025] In addition, in the super junction silicon carbide semiconductor device according to the present invention, in the above-mentioned invention, the first semiconductor layer contains phosphorus as an impurity.

[0026] In order to solve the above-mentioned problems and achieve the object of the present invention, a method for manufacturing a superjunction silicon carbide semiconductor device according to the present invention has the following features. First, a first step is performed to form a first semiconductor layer of a first conductivity type on a front surface of a silicon carbide semiconductor substrate of a first conductivity type. Next, a second step is performed to form a parallel pn region in which first column regions of a first conductivity type and second column regions of a second conductivity type are repeatedly and alternately arranged in a plane parallel to the front surface on a surface of the first semiconductor layer opposite to the silicon carbide semiconductor substrate side. Next, a third step is performed to form a second semiconductor layer of a first conductivity type on a surface of the parallel pn region opposite to the silicon carbide semiconductor substrate side. Next, a fourth step is performed to form a third semiconductor layer of a second conductivity type on a surface of the second semiconductor layer opposite to the silicon carbide semiconductor substrate side. Next, a fifth step is performed to form a second semiconductor region of a second conductivity type in the second semiconductor layer. Next, a sixth step is performed to form a third semiconductor region of a second conductivity type in a surface layer of the second semiconductor layer. Next, a seventh step is performed in which a first semiconductor region of a first conductivity type having a higher impurity concentration than the first semiconductor layer is selectively formed inside the third semiconductor layer. Next, an eighth step is performed in which a trench is formed that penetrates the first semiconductor region and the third semiconductor layer to reach the second semiconductor layer and whose bottom surface is in contact with the second semiconductor region. Next, a ninth step is performed in which a gate electrode is formed inside the trench via a gate insulating film. Next, a tenth step is performed in which a first electrode is formed in contact with the first semiconductor region and the third semiconductor layer. In the second step, an epitaxial film made of silicon carbide is formed on the front surface of the first semiconductor layer, phosphorus ions are injected from the surface of the epitaxial film to the entire surface to form a semiconductor region of a first conductivity type, and impurity ions of a second conductivity type are selectively injected into the semiconductor region to form a semiconductor region of a second conductivity type. This is repeated multiple times to form the parallel pn structure.

[0027] Furthermore, in the manufacturing method of a super junction silicon carbide semiconductor device according to the present invention, in the above-mentioned invention, the second step comprises forming an epitaxial film made of silicon carbide on the front surface of the first semiconductor layer, implanting nitrogen ions into a lower region on the silicon carbide semiconductor substrate side from the surface of the epitaxial film over the entire surface, and implanting phosphorus ions over the entire surface of the epitaxial film to form a semiconductor region of a first conductivity type, and selectively implanting impurity ions of a second conductivity type into the semiconductor region to form a semiconductor region of a second conductivity type, by repeating this process once or a plurality of times, thereby forming the parallel pn structure.

[0028] Moreover, in the method for manufacturing a super junction silicon carbide semiconductor device according to the present invention, in the above-mentioned invention, in the first step, the epitaxial film is formed on the front surface of the silicon carbide semiconductor substrate, and phosphorus ions are implanted over the entire surface of the epitaxial film to form the first semiconductor layer.

[0029] In addition, the present invention provides a method for manufacturing a super-junction silicon carbide semiconductor device according to the above-mentioned invention, wherein the epitaxial film is a non-doped film made of silicon carbide or a film containing 1×10 nitrogen atoms. 13 ~10 15 / cm 3 The present invention is characterized by being an ultra-low concentration film made of silicon carbide doped with .

[0030] In addition, in the method for manufacturing a super junction silicon carbide semiconductor device according to the present invention, the first semiconductor layer contains phosphorus and nitrogen as impurities.

[0031] According to the above-mentioned invention, by using P ion implantation when forming an n-type semiconductor layer, the carrier concentration distribution in the surface can be improved compared to the case of forming the n-type semiconductor layer by epitaxial growth. In addition, the total amount of ion implantation damage to the n-type column region can be increased. In addition, by ion implanting P ions, which have a heavier mass than N ions or Al ions, the total amount of ion implantation damage increases and the lifetime is further shortened. As a result, when the body diode of the SiC SJ-MOSFET is used as a freewheeling diode in a circuit such as an inverter to reduce the number of parts and the module size, the effect of reducing switching loss by reducing the amount of carrier accumulation in the drift layer and the effect of suppressing current degradation by reducing the electron / hole density in the drift layer can be obtained. Effect of the Invention

[0032] ADVANTAGEOUS EFFECTS OF THE PRESENT DISCLOSURE The super junction silicon carbide semiconductor device and the method for manufacturing the super junction silicon carbide semiconductor device according to the present invention have the advantage that the influence of in-plane carrier concentration distribution can be reduced when an n-type semiconductor layer is formed. [Brief description of the drawings]

[0033] [Figure 1] 1 is a cross-sectional view showing a structure of a super junction silicon carbide semiconductor device according to a first embodiment. [Diagram 2] 1 is a cross-sectional view (part 1) showing a state during the manufacture of the super junction silicon carbide semiconductor device according to the first embodiment. [Diagram 3] 4 is a cross-sectional view (part 2) showing a state during the manufacture of the super junction silicon carbide semiconductor device according to the first embodiment. FIG. [Figure 4] 4 is a cross-sectional view (part 3) showing a state during the manufacture of the super junction silicon carbide semiconductor device according to the first embodiment. FIG. [Diagram 5] 4 is a cross-sectional view showing a state during the manufacture of the super junction silicon carbide semiconductor device according to the first embodiment (part 4). FIG. [Figure 6] 5 is a cross-sectional view showing a state during the manufacture of the super junction silicon carbide semiconductor device according to the first embodiment (part 5). FIG. [Figure 7]FIG. 6 is a cross-sectional view showing a state during the manufacture of the super junction silicon carbide semiconductor device according to the first embodiment (part 6). [Figure 8] FIG. 7 is a cross-sectional view showing a state during the manufacture of the super junction silicon carbide semiconductor device according to the first embodiment; [Figure 9] FIG. 8 is a cross-sectional view showing a state during the manufacture of the super junction silicon carbide semiconductor device according to the first embodiment (part 8). [Figure 10] 4 is a graph showing P and Al concentrations in a region into which P ions and Al ions are implanted in the method for manufacturing the super junction silicon carbide semiconductor device according to the first embodiment. [Figure 11] 13 is a graph showing a simulation result of the average ranges of N ions, Al ions, and P ions in SiC according to the second embodiment. [Figure 12] FIG. 11 is a cross-sectional view showing a structure of a super junction silicon carbide semiconductor device according to a second embodiment. [Figure 13] 13 shows a simulation result of a dopant concentration profile of the parallel pn structure according to the second embodiment. [Figure 14] FIG. 1 is a cross-sectional view showing a structure of a conventional super junction silicon carbide semiconductor device. [Figure 15] 1A to 1C are cross-sectional views showing a conventional super junction silicon carbide semiconductor device in the middle of its manufacture (part 1). [Figure 16] 1A and 1B are cross-sectional views showing a conventional super junction silicon carbide semiconductor device in the middle of its manufacture (part 2). [Figure 17] 1A to 1C are cross-sectional views showing a conventional super junction silicon carbide semiconductor device in the middle of its manufacture (part 3). [Figure 18] 4 is a cross-sectional view showing a conventional super junction silicon carbide semiconductor device in the middle of its manufacture (part 4). DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0034] A preferred embodiment of the superjunction silicon carbide semiconductor device and the method of manufacturing the superjunction silicon carbide semiconductor device according to the present invention will be described in detail below with reference to the attached drawings. In this specification and the attached drawings, in a layer or region prefixed with n or p, electrons or holes are the majority carriers, respectively. In addition, + and - attached to n or p mean that the impurity concentration is higher and lower than that of a layer or region not prefixed with n or p, respectively. When the notations of n and p including + and - are the same, it indicates that the concentration is close including the variation, and the concentration is not necessarily the same. The English lowercase letters n and p are used to indicate the conductivity type of a semiconductor. Although nitrogen (N) and phosphorus (P) are discussed as impurity elements, the elements are distinguished by expressing them in English capital letters. In the following description of the embodiment and the attached drawings, the same reference numerals are attached to similar configurations, and duplicated explanations are omitted. In addition, the description of the same or equivalent should include within 5% in consideration of the variation in manufacturing.

[0035] (Embodiment 1) FIG. 1 is a cross-sectional view showing a structure of a super junction silicon carbide semiconductor device according to a first embodiment. The super junction silicon carbide semiconductor device according to the present invention will be described taking an SJ-MOSFET 50 as an example. The SJ-MOSFET 50 shown in FIG. 1 is an SJ-MOSFET 50 having a MOS (Metal Oxide Semiconductor) gate on a front surface (surface on a p-type base region 6 side described later) of a semiconductor substrate (silicon carbide substrate: semiconductor chip) made of silicon carbide. In FIG. 1, only two unit cells (functional units of an element) are shown, and other unit cells adjacent to these are not shown.

[0036] As shown in FIG. 1, the SJ-MOSFET 50 according to the first embodiment has n + An n-type buffer layer (first semiconductor layer of first conductivity type) 17 is deposited on a first main surface (front surface), for example, a (0001) surface (Si surface), of a silicon carbide substrate (silicon carbide semiconductor substrate of first conductivity type) 1, and a parallel pn structure 21 is provided on the surface of the n-type buffer layer.

[0037] n +The silicon carbide substrate 1 is, for example, a silicon carbide single crystal substrate doped with nitrogen (N). The parallel pn structure 21 includes a p-type column region 3 and an n-type column region 4. The n-type column region 4 can also be called an n-type drift layer 2 because it conducts electrons of the majority carriers of the element. + An n-type high concentration region (second semiconductor layer of the first conductivity type) 5 is selectively provided in a surface layer on the opposite side to the silicon carbide substrate 1 side. The n-type high concentration region 5 is + The n-type high-concentration drift layer has an impurity concentration lower than that of the silicon carbide substrate 1 and higher than that of the n-type column region 4. The n-type high-concentration region 5 is a so-called current spreading layer (CSL) that reduces the spreading resistance of carriers.

[0038] Parallel pn structure 21, n + A p-type base layer (a third semiconductor layer of a second conductivity type) 6 is provided on the surface side opposite to the n-type silicon carbide substrate 1 side. + The silicon carbide substrate 1, n-type buffer layer 17, parallel pn structure 21, n-type high concentration region 5, and p-type base layer 6 together constitute a silicon carbide semiconductor base. The portion above the parallel pn structure 21 is an element structure, and FIG. 1 illustrates a trench MOSFET element.

[0039] The n-type buffer layer 17 is + The n-type buffer layer 17 is a buffer layer having an impurity concentration similar to that of the n-type silicon carbide substrate 1. The n-type buffer layer 17 is non-doped or has an extremely low impurity concentration (1×10 13 ~10 15 / cm 3 The n-type buffer layer 17 is formed by implanting P (phosphorus) ions to become n-type into the epitaxial film 22 (see FIG. 2) doped with nitrogen (about 1000 Å). Therefore, the n-type buffer layer 17 contains phosphorus as an impurity. By using P ion implantation when forming the n-type buffer layer 17, the carrier concentration distribution in the surface can be improved compared to the case where the n-type buffer layer 17 is formed by doping with nitrogen and growing epitaxially. The recombination of electrons and holes is promoted in the n-type buffer layer 17, and the n +By suppressing the density of holes injected into the silicon carbide substrate 1, the occurrence of triangular / band-shaped stacking faults can be effectively suppressed.

[0040] The SJ-MOSFET 50 is provided with a parallel pn structure 21. The parallel pn structure 21 includes an n-type column region (first column of a first conductivity type) 4 and a p-type column region (second column of a second conductivity type) 3. + The n-type column regions 4 are alternately and repeatedly arranged in a plane parallel to the front surface of the silicon carbide substrate 1. The n-type column regions 4 are provided from the surface of the n-type buffer layer 17 to reach the n-type high concentration region 5.

[0041] In addition, as a charge balance of the parallel pn structure 21, the product (amount of impurities) of the width of the p-type column region 3 and the impurity concentration of the p-type column region 3 is almost equal to the product (amount of impurities) of the width of the n-type column region 4 and the impurity concentration of the n-type column region 4. Specifically, this is within ±5%. For this reason, the parallel pn structure 21 is known as a structure that can simultaneously obtain both low on-resistance and high withstand voltage characteristics. In FIG. 1, a dotted line is drawn in the center of the parallel pn structure 21, but this is to indicate that it is formed in, for example, two layers, as will be described later in FIG. 9. Of course, the parallel pn structure 21 may be formed in one layer, or in two or more layers.

[0042] As shown in Figure 1, + A back electrode (not shown) is provided on a second main surface (back surface, i.e., the back surface of the silicon carbide semiconductor base) of the silicon carbide substrate 1. The back electrode constitutes a drain electrode. A drain electrode pad (not shown) is provided on the surface of the back electrode.

[0043] A trench structure is formed on the first main surface side (p-type base layer 6 side) of the silicon carbide semiconductor substrate. +The gate electrode 10 extends from the surface opposite to the silicon carbide substrate 1 (the first main surface side of the silicon carbide semiconductor base) through the p-type base layer 6 to reach the n-type high concentration region 5. A gate insulating film 9 is formed along the inner wall of the trench 16 on the bottom and side walls of the trench 16, and a gate electrode 10 is formed inside the gate insulating film 9 in the trench 16. The gate electrode 10 is insulated from the n-type high concentration region 5 and the p-type base layer 6 by the gate insulating film 9. A part of the gate electrode 10 may protrude from above the trench 16 towards the source electrode 12 described later.

[0044] The n-type high concentration region 5 includes a first p + A second semiconductor region of a second conductivity type (a base region of a second conductivity type) 14 and a second p + A first p-type base region (a third semiconductor region of a second conductivity type) 15 is selectively provided. + The mold base region 14 covers at least the bottom surface of the trench 16. The bottom corner portion of the trench 16 is the boundary between the bottom surface and the sidewall of the trench 16. + The n-type base region 15 is provided between the trenches 16 and extends from the surface of the n-type high concentration region 5 on the p-type base layer 6 side to the first p + It is provided to the same depth as the mold base region 14 .

[0045] 1st p. + The mold base region 14 and the second p + The pn junction between the n-type base region 15 and the n-type column region 4 is formed at a position deeper on the drain side than the bottom surface of the trench 16. + The mold base region 14 and the second p + The depth position of the drain side end of the base region 15 is the first p + The mold base region 14 and the second p + It is sufficient that the pn junction between the first base region 15 and the n-type column region 4 is located deeper on the drain side than the bottom surface of the trench 16, and this can be changed in various ways according to design conditions. + The mold base region 14 and the second p +The mold base region 15 can prevent a high electric field from being applied to the gate insulating film 9 along the bottom surface of the trench 16 .

[0046] The surface layer of the p-type base layer 6 has n + A p-type source region (first semiconductor region of a first conductivity type) 7 is selectively provided. + A contact region 8 may be provided. + The n-type source region 7 is in contact with the trench 16. + Type source region 7 and p + The contact regions 8 are in contact with each other. + "Provided on the surface of the semiconductor layer" means that a semiconductor region / semiconductor layer is provided above the surface of the semiconductor layer, and "provided on the surface layer of the semiconductor layer" means that a semiconductor region / semiconductor layer is provided inside the semiconductor layer and is exposed on the surface of the semiconductor layer.

[0047] The interlayer insulating film 11 is provided on the entire first main surface side of the silicon carbide semiconductor substrate so as to cover the gate electrode 10 embedded in the trench 16. The source electrode 12 is connected to the n-type + The p-type source region 7 and the p-type base layer 6 are in contact with each other. + When the n-type contact region 8 is provided, + Type source region 7 and p + The source electrode 12 is in contact with the type contact region 8. The source electrode 12 is made of, for example, a NiSi film. The source electrode 12 is electrically insulated from the gate electrode 10 by an interlayer insulating film 11. A source electrode pad (not shown) made of Al or AlSi is provided on the source electrode 12. A barrier metal (not shown) made of, for example, Ti and TiN may be provided between the source electrode 12 and the interlayer insulating film 11 to prevent diffusion of metal atoms from the source electrode 12 to the gate electrode 10 side.

[0048] As described later, the n-type column region 4 is formed by implanting P ions to become n-type into a non-doped or ultra-low concentration epitaxial film 23 (see FIG. 4). Therefore, the n-type column region 4 contains phosphorus as an impurity. Since this ion implantation is performed on the entire surface, the p-type column region 3 also contains phosphorus as an impurity. By using P ion implantation when forming the epitaxial film 23, the carrier concentration distribution within the surface can be improved compared to the case where the epitaxial film is formed by doping nitrogen and growing it epitaxially. In addition, the total amount of ion implantation damage to the n-type column region 4 can be increased.

[0049] Furthermore, by ion implanting P (phosphorus) with a mass number of 31, which is heavier than N (nitrogen) with a mass number of 14 and Al (aluminum) with a mass number of 27, the total amount of ion implantation damage increases and the lifetime is further shortened. As a result, when using the body diode of a SiC SJ-MOSFET as a freewheeling diode in order to reduce the number of components and module size in circuits such as inverters, it is possible to obtain the effect of reducing switching losses by reducing the amount of carrier accumulation in the drift layer and the effect of suppressing degradation due to current flow by reducing the electron and hole density in the drift layer.

[0050] (Method of Manufacturing Super-junction Silicon Carbide Semiconductor Device According to First Embodiment) Next, a description will be given of a method for manufacturing the super junction silicon carbide semiconductor device according to the first embodiment. Figures 2 to 9 are cross-sectional views that typically show states during the manufacturing process of the super junction silicon carbide semiconductor device according to the first embodiment.

[0051] First, we used n-type single crystal 4H-SiC. + A type silicon carbide substrate 1 is prepared. + An epitaxial film 22 is epitaxially grown on the first main surface of the silicon carbide substrate 1. The epitaxial film 22 may be a non-doped film made of silicon carbide that does not contain impurities, or may be a film made of silicon carbide that is doped with n-type impurities, such as nitrogen atoms, at a concentration of 1×10 13 ~10 15 / cm 3Alternatively, the epitaxial film 22 may be an ultra-low concentration film made of silicon carbide doped to a degree of 0.1%. Alternatively, the epitaxial film 22 may be a non-doped film, and then nitrogen ions may be implanted to dope the epitaxial film 22 to a desired degree. The state up to this point is shown in FIG. 2. Next, phosphorus ions are implanted into the entire surface of the epitaxial film 22 to form the n-type buffer layer 17. Next, an annealing process is performed in an inert gas atmosphere at about 1700° C. to activate the n-type buffer layer 17. Note that the annealing process may be performed to activate all the ion-implanted regions at once. The state up to this point is shown in FIG. 3.

[0052] Next, the epitaxial film 23 is epitaxially grown on the surface of the n-type buffer layer 17. The state up to this point is shown in FIG. 4. Next, phosphorus is ion-implanted over the entire surface of the epitaxial film 23 to form the lower n-type drift layer 2a. The acceleration energy when implanting the P ions is set in a range where a desired decrease in lifetime can be obtained and the crystal is not damaged too much to cause deterioration of characteristics. From this viewpoint, the acceleration energy when implanting the P ions is desirably 700 eV or more. The upper limit is 21.5 MeV or less, preferably 5.4 MeV or less, and furthermore, considering the throughput of the ion implantation device, 3.75 MeV or less is preferable. In addition, in order to improve the concentration distribution of the doping concentration in the ion implantation method, it is more preferable to use an ion implantation device that also uses a wafer scan (mechanical scan) method than an ion implantation device that uses only the beam scan method. Next, an annealing process is performed in an inert gas atmosphere at about 1700° C. to activate the lower n-type drift layer 2a. The annealing process may be performed to activate all the ion implanted regions at once. The state up to this point is shown in FIG.

[0053] Next, an ion implantation mask 30 having a predetermined opening is formed on the surface of the lower n-type drift layer 2a by photolithography, for example, using an oxide film. Then, aluminum ions are implanted into the opening of the oxide film to form the lower p-type column region 3a. The region into which the aluminum ions are not implanted becomes the lower n-type column region 4a. The state up to this point is shown in FIG. 6. Next, the ion implantation mask 30 is removed. Next, an annealing process is performed in an inert gas atmosphere at about 1700° C. to activate the lower p-type column region 3a. Note that the annealing process may be performed to activate each ion implantation region together at the end.

[0054] Next, an epitaxial film 24 is epitaxially grown on the surfaces of the lower p-type column region 3a and the lower n-type column region 4a. The state up to this point is shown in FIG. 7. Next, phosphorus ions are implanted into the entire surface of the epitaxial film 24 to form the upper n-type drift layer 2b. Next, an annealing process is performed in an inert gas atmosphere at about 1700° C. to activate the upper n-type drift layer 2b. The annealing process may be performed to activate each ion-implanted region at the same time. The state up to this point is shown in FIG. 8.

[0055] Next, an ion implantation mask (not shown) having a predetermined opening is formed on the surface of the upper n-type drift layer 2b by photolithography, for example, using an oxide film. Aluminum ions are then implanted into the openings of the oxide film to form the upper p-type column region 3b. The region into which the aluminum ions are not implanted becomes the upper n-type column region 4b. Next, the ion implantation mask is removed. Next, an annealing process is performed in an inert gas atmosphere at about 1700°C to activate the upper p-type column region 3b. Note that the annealing process may be performed to activate each ion implantation region at the end. Next, the ion implantation mask is removed. The state up to this point is shown in FIG. 9.

[0056] The lower p-type column region 3a and the upper p-type column region 3b become the p-type column region 3, and the lower n-type column region 4a and the upper n-type column region 4b become the n-type column region 4, forming a parallel pn structure 21. Here, an example has been shown in which the parallel pn structure 21 is formed by stacking epitaxial films 23 and 24 in two stages, but it may also be formed by stacking three or more stages. The above are the manufacturing steps shown in FIGS. 2 to 9, and the n + A silicon carbide substrate 1, an n-type buffer layer 17, and a parallel pn structure 21 are formed.

[0057] 10 is a graph showing the P and Al concentrations in the regions implanted with P ions and Al ions in the structure of FIG. 9, calculated based on the results of a simulation in the method for manufacturing a super-junction silicon carbide semiconductor device according to the first embodiment. In FIG. 10, the vertical axis shows the P and Al concentrations, and the unit is atoms / cm. 3 For example, the notation 1.0E+18 on the vertical axis is 1.0×10 18 means that the concentration of P in the upper n-type column region 4b, the lower n-type column region 4a, and the n-type buffer layer 17 is increased from the origin (0 μm). The thick lines indicate the concentration of Al in the upper p-type column region 3b and the lower p-type column region 3a, from the origin. The thickness of the epitaxial films 23 and 24 was set to 2 μm.

[0058] After the epitaxial film 22 is formed without doping, the n-type buffer layer 17 has an average P ion implantation concentration of about 1.8×10 16 atoms / cm 3 It was assumed that P ion implantation processing would be performed so that

[0059] In addition, in the lower n-type drift layer 2a, after the epitaxial film 23 is formed without doping, the P ion implantation concentration in the box profile portion is about 3.0×10 on average. 16 atoms / cm 3 It was assumed that P ion implantation processing would be performed so that

[0060] In addition, in the lower p-type column region 3a, an ion implantation mask having a predetermined opening is formed of an oxide film by photolithography technology, and the Al ion implantation concentration in the box profile portion is set to an average of about 1.3×10 17 atoms / cm 3 It was assumed that Al ions were implanted into the openings of the oxide film so that

[0061] In addition, after removing the oxide film, the upper n-type drift layer 2b is formed with the epitaxial film 24 without doping, and the P ion implantation concentration in the box profile portion is about 3.0×10 on average. 16 atoms / cm 3 It was assumed that P ion implantation processing would be performed so that

[0062] In addition, in the upper p-type column region 3b, an ion implantation mask having a predetermined opening is formed of an oxide film by photolithography technology, and the Al ion implantation concentration in the box profile portion is set to an average of about 1.3×10 17 atoms / cm 3 It was assumed that Al ions were implanted into the openings of the oxide film so that the following was true: At the junctions of each layer and region, the ion implanted regions overlap, resulting in a peak due to high concentration.

[0063] Returning to the explanation of the manufacturing method of the semiconductor device of Fig. 1, the following manufacturing procedure is well known and therefore is not shown in the figures. After the process of Fig. 9, an n-type high concentration region 5 doped with nitrogen is formed by epitaxial growth on the surfaces of the p-type column region 3 and the n-type column region 4. Next, a first p + The mold base region 14 and the second p + A mold base region 15 is formed by selective ion implantation using a selective mask.

[0064] Next, a p-type base layer 6 doped with p-type impurities such as aluminum is formed by epitaxial growth on the surface of the n-type high concentration region 5. Next, an ion implantation mask having a predetermined opening is formed on the surface of the p-type base layer 6 by photolithography, the mask being made of, for example, an oxide film, a semiconductor film, or a laminated structure of an oxide film / semiconductor film. An n-type impurity such as phosphorus (P) is ion-implanted into this opening, and n is implanted into a part of the surface of the p-type base layer 6. + Next, the n-type source region 7 is formed. + The ion implantation mask used for forming the p-type source region 7 is removed, and a new ion implantation mask having a predetermined opening is formed in the same manner, and p-type impurities such as aluminum are ion-implanted into a portion of the surface of the p-type base layer 6 to form a p + A contact region 8 may be formed. + The impurity concentration of the p-type contact region 8 is set to be higher than the impurity concentration of the p-type base layer 6.

[0065] Next, annealing is performed in an inert gas atmosphere at about 1700° C. to form n-type column regions 4 and + Type source region 7, p + An activation process is then carried out on the mold contact region 8, etc. As described above, the ion implantation regions may be activated all at once by a single annealing process, or activation may be carried out by performing an annealing process each time an ion implantation is performed.

[0066] Next, a trench forming mask having a predetermined opening is formed on the surface of the p-type base layer 6 by photolithography, using, for example, an oxide film. Next, a trench 16 is formed by dry etching, penetrating the p-type base layer 6 and reaching the n-type high concentration region 5. The bottom of the trench 16 is the first p-type impurity formed in the n-type high concentration region 5. + This may extend to the mold base region 14. The trench mask is then removed.

[0067] Next, n +A gate insulating film 9 is formed along the surface of the source region 7 and the bottom and sidewalls of the trench 16. This gate insulating film 9 may be formed by thermal oxidation at a temperature of about 1000° C. in an oxygen atmosphere. Alternatively, this gate insulating film 9 may be formed by a method of deposition by a chemical vapor deposition reaction such as high temperature oxidation (High Temperature Oxide: HTO).

[0068] Next, for example, a phosphorus-doped polycrystalline silicon layer is formed by chemical vapor deposition on the gate insulating film 9. This polycrystalline silicon layer may be formed so as to fill the trench 16. This polycrystalline silicon layer is patterned by photolithography and left inside the trench 16 to form the gate electrode 10.

[0069] Next, for example, phosphorus glass is deposited to a thickness of about 1 μm so as to cover the gate insulating film 9 and the gate electrode 10, forming an interlayer insulating film 11. Next, a barrier metal (not shown) made of titanium (Ti) or titanium nitride (TiN) may be formed so as to cover the interlayer insulating film 11. The interlayer insulating film 11 and the gate insulating film 9 are patterned by photolithography to form a n + A contact hole is formed to expose the source region 7. + When the n-type contact region 8 is formed, + Type source region 7 and n + A contact hole is formed to expose the source region 7. Thereafter, a heat treatment (reflow) is performed to flatten the interlayer insulating film 11.

[0070] Next, a conductive film that will become the source electrode 12 is provided in the contact hole and on the interlayer insulating film 11. This conductive film is selectively removed to leave the source electrode 12 only in the contact hole, and n + The source region 7 is in contact with the source electrode 12. + When the n-type contact region 8 is formed, + Type source region 7 and p +The mold contact region 8 is brought into contact with the source electrode 12. Next, the source electrode 12 other than the contact hole is selectively removed.

[0071] Next, an electrode pad to become a source electrode pad (not shown) is deposited on the source electrode 12 on the front surface of the silicon carbide semiconductor substrate and on the interlayer insulating film 11 by, for example, sputtering.

[0072] Next, n + A back electrode made of nickel or the like is provided on the second main surface of the silicon carbide semiconductor substrate 1. After that, annealing is performed in an inert gas atmosphere at about 1000° C. to form an n-type silicon carbide semiconductor substrate 1. + In the case where the trench 16 is not formed, an n-type well region is formed in a part of the surface region of the p-type base layer 6, the front surface side of the silicon carbide semiconductor substrate is thermally oxidized to form a gate insulating film 9, the p-type base layer 6 and each region formed on the surface of the p-type base layer 6 are covered with the gate insulating film 9, a polycrystalline silicon layer is formed as a gate electrode 10 on the gate insulating film 9, the polycrystalline silicon layer is patterned and selectively removed, and the n-type well region of the p-type base layer 6 is formed. + The polycrystalline silicon layer is left on the portion sandwiched between the n-type source region 7 and the n-type well region, and an interlayer insulating film 11 is formed to cover the gate electrode 7. In this manner, the silicon carbide semiconductor device shown in FIG.

[0073] As described above, according to the superjunction silicon carbide semiconductor device and the method for manufacturing the superjunction silicon carbide semiconductor device according to the first embodiment, by using P ion implantation when forming the n-type semiconductor layer, the carrier concentration distribution in the plane can be improved compared to the case of forming the n-type semiconductor layer by epitaxial growth. In addition, the total amount of ion implantation damage to the n-type column region can be increased. In addition, by ion implanting P ions, which have a heavier mass than N ions and Al ions, the total amount of ion implantation damage increases and the lifetime is further shortened. As a result, when the body diode of the SiC SJ-MOSFET is used as a freewheeling diode in a circuit such as an inverter to reduce the number of components and the module size, the effect of reducing switching loss by reducing the amount of carrier accumulation in the drift layer and the effect of suppressing current degradation by reducing the electron-hole density in the drift layer can be obtained.

[0074] (Embodiment 2) Next, a second embodiment will be described. In the second embodiment, the parallel pn structure 21 in FIG. 1 is modified to form a parallel pn structure 21'. In the first embodiment, the thickness of one layer of the epitaxial film 23 forming the parallel pn structure 21 is set to, for example, about 2 μm, and it is assumed that P ions of the n-type column region can be implanted into the entire thickness as shown in FIG. 10. In contrast, in the second embodiment, it is assumed that the thickness of one layer of the epitaxial film 23 is a thick layer, for example, exceeding about 2.5 μm, and it is difficult to implant P ions into the entire thickness, and a device structure and a manufacturing method thereof are provided. As will be described later, for a thick epitaxial film, the n-type column region is formed by a two-stage structure in which shallow portions are formed by P ion implantation and deep portions are formed by N ion implantation.

[0075] Fig. 11 is a graph showing the simulation results of the average range of N ions, Al ions, and P ions implanted into SiC versus the respective acceleration energies. The density of SiC is 3.21 g / cm 3The average range was calculated as . The crystal structure of SiC was not taken into consideration. In FIG. 11, the vertical axis indicates the average range of N ions, Al ions, and P ions in SiC in μm, and the horizontal axis indicates the acceleration energy of N ions, Al ions, and P ions in MeV. As shown in FIG. 11, since P ions have the heaviest mass, the implantation depth is the shallowest at the same acceleration energy. Furthermore, since N ions have the lightest mass, the implantation depth is the deepest at the same acceleration energy. In other words, it is difficult to implant P ions into a layer deeper than N ions, whereas the second embodiment presents a solution to this problem.

[0076] 12 is a cross-sectional view showing the structure of a super junction silicon carbide semiconductor device according to the second embodiment. In the super junction silicon carbide semiconductor device according to the second embodiment, parallel pn structure 21' is, for example, a single epitaxial layer, and n-type column region 4 is composed of a first n-type column region 4' into which P ions are implanted and a second n-type column region 4'' into which N ions are implanted. As a result, p-type column region 3 is also composed of a first p-type column region 3' into which Al ions and P ions are implanted, and a second p-type column region 3'' into which Al ions and N ions are implanted.

[0077] Fig. 13 shows the results of a simulation of the dopant concentration profile of the parallel pn structure 21' in Fig. 12. It is assumed that an ion implanter capable of accelerating Al ions up to 8000 keV, P ions up to 5400 keV, and N ions up to 6300 keV is used. The p-type column region 3 is implanted with Al ions in 16 stages from 120 keV to 8000 keV, with a set concentration of 1.3 x 10 17 atoms / cm 3 On the other hand, in the n-type column region 4, N ions are implanted in a box profile from 3920 keV to 5780 keV in six steps, and then P ions are implanted in a box profile from 85 keV to 5400 keV in 12 steps, resulting in an average concentration of 3.0 × 10 16 atoms / cm 3This is the target ion implantation profile. As shown in Fig. 13, an overlapping region where both P ions and N ions are implanted occurs in the middle of the n-type column region 4, but this is not shown in Fig. 12. In order to improve the concentration distribution of the doping concentration in the ion implantation method, it is more preferable to use an ion implantation device that also uses the wafer scan (mechanical scan) method rather than an ion implantation device that uses only the beam scan method.

[0078] With this structure, it is possible to form a deeper n-type column region 4 by using N ions, which have a lighter mass and a longer average range than P ions, in regions that are too deep for the performance of the ion implantation device to reach. This makes it possible to make the depth of each layer of the n-type column region 4 and the p-type column region 3 deeper than in the first embodiment.

[0079] (Method of Manufacturing Super-junction Silicon Carbide Semiconductor Device According to Second Embodiment) Next, a manufacturing method of the super junction silicon carbide semiconductor device according to the second embodiment will be described. In the following manufacturing process, the first and second n-type column regions 4', 4'' are first formed as a layer structure, and then a p-type column region is selectively ion-implanted into the layer structure, thereby defining the n-type column region as the remaining portion. In the following description of the manufacturing method, the first and second n-type column regions 4', 4'' refer to either the initial layer structure or the subsequently defined n-type column regions, depending on the stage of the manufacturing process.

[0080] First, similarly to the method for manufacturing the super junction silicon carbide semiconductor device according to the first embodiment, n-type buffer layer 17 is formed, and epitaxial film 23 is epitaxially grown on the surface of n-type buffer layer 17. The steps up to this point are the same as those in FIGS. 2 and 3. Next, while P ions are implanted into the entire epitaxial film 23 in FIG. 5, in the second embodiment, nitrogen ions are implanted into a deep position from the surface of epitaxial film 23 (a region in contact with n-type buffer layer 17) to form second n-type column region 4''.

[0081] Next, P ions are implanted from the surface of the epitaxial film 23 to form the first n-type column region 4' at a shallow position from the surface of the epitaxial film 23. Next, an annealing process is performed in an inert gas atmosphere at about 1700°C to activate the first n-type column region 4' and the second n-type column region 4''. The annealing process may be performed to activate all the ion-implanted regions at once. The carrier concentration of the second n-type column region 4'' may be the same as the carrier concentration of the first n-type column region 4' formed by ion implantation of phosphorus, or it may not be the same.

[0082] Next, an ion implantation mask 30 having a predetermined opening is formed, for example, from an oxide film on the surface of the first n-type column region 4' by photolithography. Then, aluminum ions are implanted into the openings of the oxide film to form the p-type column region 3. The region into which the aluminum ions are not implanted becomes the n-type column region 4. Since Al is implanted into the p-type column region 3 in addition to the n-type column region 4, a structure of the first p-type column region 3' and the second p-type column region 3'' is formed. Next, the ion implantation mask 30 is removed. Next, an annealing process is performed in an inert gas atmosphere at about 1700°C to activate the p-type column region 3. Note that the annealing process may be performed to activate each ion implantation region together at the end. In this way, the parallel pn structure 21' of the second embodiment is formed. Here, an example of forming the parallel pn structure 21' by stacking one layer of the epitaxial film 23 has been shown, but it may be formed by stacking two or more layers. Thereafter, a step of forming n-type high concentration region 5 is carried out in the same manner as in the method for manufacturing a super junction silicon carbide semiconductor device according to the first embodiment, thereby completing the silicon carbide semiconductor device shown in FIG.

[0083] As described above, according to the super junction silicon carbide semiconductor device and the manufacturing method of the super junction silicon carbide semiconductor device of the second embodiment, by using P ion implantation when forming the n-type semiconductor layer, it is possible to obtain the same effect as in the first embodiment. Furthermore, by using N ion implantation, it is possible to form n-type column regions in regions that are too deep for P ions to reach, and it is possible to make the depths of the n-type column regions and the p-type column regions deeper than in the first embodiment. Note that, when the n-type buffer layer has a region that is too deep for P ions to reach, N ion implantation may also be used in the deep region.

[0084] In the above, the present invention has been described by taking as an example a case where the main surface of a silicon carbide substrate made of silicon carbide is a (0001) surface and a MOS is constructed on the (0001) surface, but the present invention is not limited to this and can be modified in various ways such as a wide band gap semiconductor, a surface orientation of the substrate main surface, etc. Also, in the embodiment of the present invention, a trench type MOSFET has been described by way of example, but the present invention is not limited to this and can be applied to semiconductor devices of various configurations such as MOS type semiconductor devices such as planar type MOSFETs and IGBTs. [Industrial Applicability]

[0085] INDUSTRIAL APPLICABILITY As described above, the super junction silicon carbide semiconductor device and method of manufacturing the super junction silicon carbide semiconductor device according to the present invention are useful for high voltage semiconductor devices used in power conversion devices and power supply devices for various industrial machines and the like. [Explanation of symbols]

[0086] 1, 101 n + Silicon carbide substrate 2, 102 n-type drift layer 2a Lower n-type drift layer 2b Upper n-type drift layer 3, 103 p-type column region 3a Lower p-type column region 3b Upper p-type column region 3' First p-type column region 3'' Second p-type column region 4, 104 n-type column region 4a Lower n-type column region 4b Upper n-type column region 4' First n-type column region 4'' 2nd n-type column region 5, 105 n-type high concentration region 6, 106 p-type base layer 7, 107 n + Type Source Area 8, 108 p. + Mold Contact Area 9, 109 Gate insulating film 10, 110 Gate electrode 11, 111 Interlayer insulating film 12, 112 Source electrode 14, 114 1st p. + Type-based regions 15, 115 2nd p. + Type-based regions 16, 116 Trench 17, 117 n-type buffer layer 21, 21', 121 parallel pn structure 22, 23, 24 Epitaxial film 30, 122 Ion implantation mask 50, 150 SJ-MOSFET 102a First n-type drift layer 102b Second n-type drift layer 103a First p-type column region 103b Second p-type column region

Claims

1. a first conductivity type silicon carbide semiconductor substrate; a first semiconductor layer of a first conductivity type provided on a front surface of the silicon carbide semiconductor substrate; a parallel pn region in which first column regions of a first conductivity type and second column regions of a second conductivity type are repeatedly and alternately arranged in a plane parallel to the front surface, the parallel pn region being provided on a surface of the first semiconductor layer opposite to the silicon carbide semiconductor substrate; a second semiconductor layer of a first conductivity type provided on a surface of the parallel pn region opposite to the silicon carbide semiconductor substrate; a third semiconductor layer of a second conductivity type provided on a surface of the second semiconductor layer opposite to the silicon carbide semiconductor substrate; a first semiconductor region of a first conductivity type selectively provided within the third semiconductor layer and having a higher impurity concentration than the first semiconductor layer; a trench passing through the first semiconductor region and the third semiconductor layer to reach the second semiconductor layer; a second semiconductor region of a second conductivity type provided in the second semiconductor layer and in contact with a bottom of the trench; a third semiconductor region of a second conductivity type provided between the trenches in a surface layer of the second semiconductor layer; a gate electrode provided inside the trench via a gate insulating film; a first electrode in contact with the first semiconductor region and the third semiconductor layer; Equipped with 4. A super junction silicon carbide semiconductor device, wherein the first column region and the second column region contain phosphorus as an impurity.

2. the first column region is composed of a lower first column region on the silicon carbide semiconductor substrate side and an upper first column region on the second semiconductor layer side; 2. The super junction silicon carbide semiconductor device according to claim 1, wherein the lower first column region contains nitrogen as an impurity, and the upper first column region and the second column region contain phosphorus as impurities.

3. 3. The super junction silicon carbide semiconductor device according to claim 1, wherein the first semiconductor layer contains phosphorus as an impurity.

4. a first step of forming a first semiconductor layer of a first conductivity type on a front surface of a silicon carbide semiconductor substrate of a first conductivity type; a second step of forming a parallel pn region in a surface of the first semiconductor layer opposite to the silicon carbide semiconductor substrate, the parallel pn region including first column regions of a first conductivity type and second column regions of a second conductivity type repeatedly and alternately arranged in a plane parallel to the front surface; a third step of forming a second semiconductor layer of a first conductivity type on a surface of the parallel pn region opposite to the silicon carbide semiconductor substrate; A fourth step of forming a third semiconductor layer of a second conductivity type on a surface of the second semiconductor layer opposite to the silicon carbide semiconductor substrate; a fifth step of forming a second semiconductor region of a second conductivity type in the second semiconductor layer; a sixth step of forming a third semiconductor region of a second conductivity type in a surface layer of the second semiconductor layer; a seventh step of selectively forming a first semiconductor region of a first conductivity type having an impurity concentration higher than that of the first semiconductor layer within the third semiconductor layer; an eighth step of forming a trench that penetrates the first semiconductor region and the third semiconductor layer to reach the second semiconductor layer and has a bottom surface in contact with the second semiconductor region; a ninth step of forming a gate electrode inside the trench via a gate insulating film; a tenth step of forming a first electrode in contact with the first semiconductor region and the third semiconductor layer; Including, a first semiconductor layer formed on the first semiconductor layer and an epitaxial film formed on the first semiconductor layer; a first conductivity type semiconductor region formed by injecting phosphorus ions into the entire surface of the epitaxial film; and a second conductivity type semiconductor region formed by selectively injecting impurity ions of a second conductivity type into the semiconductor region. This is repeated a plurality of times to form a parallel pn structure.

5. 5. The method for manufacturing a super junction silicon carbide semiconductor device according to claim 4, wherein in the second step, an epitaxial film made of silicon carbide is formed on the front surface of the first semiconductor layer, nitrogen ions are implanted into the entire surface of the epitaxial film in a lower region on the silicon carbide semiconductor substrate side, and phosphorus ions are implanted into the entire surface of the epitaxial film to form a semiconductor region of a first conductivity type, and impurity ions of a second conductivity type are selectively implanted into the semiconductor region to form a semiconductor region of a second conductivity type, by repeating this process once or a plurality of times, the parallel pn structure is formed.

6. 6. The method for manufacturing a super junction silicon carbide semiconductor device according to claim 4 or 5, wherein in the first step, the epitaxial film is formed on a front surface of the silicon carbide semiconductor substrate, and phosphorus ions are implanted into an entire surface of the epitaxial film to form the first semiconductor layer.

7. The epitaxial film is a non-doped film made of silicon carbide or a film containing 1×10 nitrogen atoms. 13 ~10 15 / cm 3 6. The method for manufacturing a super junction silicon carbide semiconductor device according to claim 4, wherein the super junction silicon carbide is an ultra-low concentration film made of silicon carbide doped with .

8. 6. The method for manufacturing a super junction silicon carbide semiconductor device according to claim 4, wherein the first semiconductor layer contains phosphorus and nitrogen as impurities.

Citation Information

Patent Citations

  • Semiconductor device and manufacturing method therefor

    JP2014236120A

  • Silicon carbide semiconductor device and power conversion device

    WO2023286235A1

  • Super-junction semiconductor element

    JP2006100862A

  • Semiconductor device and manufacturing method thereof

    JP2009130106A

  • Semiconductor device

    WO2013179820A1

Cited By

  • Semiconductor device

    WO2026168261A1