Base material with coat and manufacturing method of the same

A coated base material with a peelable film and longitudinal recesses addresses the issue of packaging detachment and waste by providing effective protection and enabling reuse, enhancing manufacturing efficiency.

JP2024154041APending Publication Date: 2024-10-30INOAC HOUSING & CONSTR MATERIALS
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023067636
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-18
Publication Date
2024-10-30

AI Technical Summary

Technical Problem

Existing flexible tube packaging solutions are prone to falling off or becoming misaligned during transportation, leading to exposure of the outer surface to dust and dirt, and generate waste due to separate packaging materials.

Method used

A coated base material with a peelable film laminated on its outer surface, featuring recesses along the longitudinal direction to prevent detachment and facilitate easy peeling, allowing for reuse and reduced environmental impact.

Benefits of technology

The coated base material effectively protects against scratches and dirt while minimizing waste by allowing the coating to be peeled off and reused, reducing manufacturing costs through continuous production processes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024154041000001_ABST
    Figure 2024154041000001_ABST
Patent Text Reader

Abstract

To provide a base material with a coat which makes the coat on an outer peripheral surface of the base material less likely to fall and is formed separably, and to provide a manufacturing method of the base material with the coat.SOLUTION: A base material 1 with a coat includes: a base material 2 which may be wound in an annular form; and a peelable coat 3 laminated on an outer peripheral surface 2a of the base material 2. The coat 3 has a recessed part 4 formed along a longitudinal direction of the base material 2. The base material 2 and the coat 3 may be formed of the same kind of resin material. Further, the base material 2 may be a pipe 12.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a coated substrate in which the outer peripheral surface of a substrate that can be wrapped around an annular shape is coated, and a method for producing the coated substrate. [Background technology]

[0002] Conventionally, proposals have been made to prevent foreign matter such as dust and dirt from adhering to the outer surface of a long flexible tube or the like, or to prevent scratches. For example, Patent Document 1 describes the following: A packaging form for flexible tubes in which long flexible tubes are stocked as an inventory and desired lengths of the flexible tubes are cut and sold from the inventory, the packaging form comprises the flexible tube made of a deformable soft material and a cylindrical packaging body provided along the periphery of the flexible tube, the packaging body being made of a cuttable and deformable material and covering the flexible tube so as to be deformable in response to bending and deformation of the flexible tube.

[0003] According to this, when a desired length of flexible tube is cut from an inventory of flexible tube, the packaging is cut together with the flexible tube while the flexible tube is still covered with the packaging without removing the packaging from the flexible tube, so that the outer surface of the inventory of flexible tube is not exposed, and the flexible tube to be sold is separated without exposing the outer surface of the inventory of flexible tube. The inventory of flexible tube is stored with its outer surface covered with the packaging, and the cut flexible tube can be carried with its outer surface covered with the packaging.

[0004] Therefore, the outer surface of the flexible tube can be kept from being exposed to the outside air during inventory management, cutting, and after cutting. As a result, it is possible to prevent foreign matter such as dust and dirt from adhering to the outer surface of the flexible tube and to prevent discoloration, and the outer surface of the flexible tube can be kept hygienic. It is described that this is particularly effective when the flexible tube is made of a material that has adhesiveness and high electrical insulation properties, such as silicone rubber, and foreign matter such as dust and dirt is likely to adhere to the outer surface due to static electricity, etc. [Prior art documents] [Patent documents]

[0005] [Patent Document 1] Patent No. 5771863 Summary of the Invention [Problem to be solved by the invention]

[0006] However, the conventional example described in Patent Document 1 is expected to have the following problems. According to Patent Document 1, the flexible tube is simply covered by the packaging body. It is described that the packaging body is preferably formed into a cylindrical shape with a diameter larger than the outer diameter of the flexible tube, and that the packaging body can be wrapped around the flexible tube so that a space is formed between the outer surface of the flexible tube and the inner surface of the packaging body, thereby maintaining a constant distance between the outer surface of the flexible tube and the inner surface of the packaging body. In this case, since there is a space between the packaging body and the outer surface of the flexible tube, there is a risk that the packaging body may fall off the flexible tube or become displaced during transportation, etc.

[0007] The object of the present invention is to solve the problems of the conventional art by providing a coated substrate in which the coating on the outer peripheral surface of the substrate does not easily fall off and is formed so as to be separable, and a method for producing a coated substrate. [Means for solving the problem]

[0008] A coated substrate according to a first aspect of the present invention comprises a substrate that can be wrapped around a ring shape, and a coating that is laminated on the outer peripheral surface of the substrate and can be peeled off, the coating having a recess formed along the longitudinal direction of the substrate.

[0009] According to this, the coating is laminated on the outer peripheral surface of the substrate and does not easily fall off, so that the outer peripheral surface of the substrate can be protected from scratches, dirt, etc. Also, since the recesses are formed along the longitudinal direction of the substrate and the coating can be peeled off from the outer peripheral surface of the substrate, the coating can be peeled off from the substrate by tearing the recesses.

[0010] The coated substrate may be formed such that the substrate and the coating are made of the same type of resin material. In this case, the substrate and the coating are made of the same type of resin material, so that separation is not required when disposing of the coated substrate. Therefore, the substrate and the coating can be reused together when recycling materials, thereby reducing the environmental load.

[0011] The coated substrate may be a tube. In this case, the substrate is applicable to pipes and the like, and there is no limit to the length.

[0012] A coated substrate manufacturing method according to a second aspect of the present invention is a method for manufacturing a coated substrate, comprising a first step of shaping the substrate, a second step of cooling the substrate shaped by the first step, and a third step of forming the coating on an outer peripheral surface of the substrate cooled by the second step.

[0013] According to this, the first to third steps can be continuously performed by a series of manufacturing equipment, so that the manufacturing cost can be reduced. Also, the outer peripheral surface of the substrate can be stably coated. [Brief description of the drawings]

[0014] [Figure 1] FIG. 1 is a plan view showing a coated substrate 1a according to a first embodiment of the present invention. [Diagram 2] 2 is a partial enlarged view of cross section II in FIG. 1, illustrating the cross-sectional shape of a first recess 4a. FIG. [Diagram 3] 2, and is a diagram illustrating the cross-sectional shape of a first recess 14a. FIG. [Figure 4] 1A is a perspective view showing a coated substrate 1a, where (a) shows the state before the coating 3 is peeled off at the first recess 4a, and (b) shows the state after a portion of the first recess 4a is separated to peel off the coating 3 from the substrate 2. [Diagram 5] 1A is a perspective view showing a coated substrate 1a, in which (a) shows a state in which the coating 3 has been peeled off and cut in a predetermined range in the longitudinal direction from an end of the substrate 2, and (b) shows a state in which a joint 27 has been attached to (a). [Figure 6] 1A is a perspective view showing a coated substrate 1a, in which (a) shows a state in which the coating 3 has been peeled off and rolled up in a predetermined range in the longitudinal direction from an end of the substrate 2, (b) shows a state in which a joint 27 has been attached to (a), and (c) shows a state in which the coating 3 has been further applied to the joint 27 from (b). [Figure 7] FIG. 2 is a plan view showing a coated substrate 1b according to a second embodiment of the present invention. [Figure 8] 8 is a partial enlarged view of the cross section II-II in FIG. 7, illustrating the cross-sectional shape of a second recess 4b. [Figure 9] 9 is another example of the configuration of FIG. 8, illustrating the cross-sectional shape of a second recess 14b. [Figure 10] 1A is a perspective view showing a coated substrate 1b, in which (a) shows the state before the coating 3 is peeled off at the second recess 4b, (b) shows the state in which a part of the second recess 4b is separated and the coating 3 is peeled off from the substrate 2, (c) shows the state in which the coating 3 has been peeled off and cut in a predetermined range in the longitudinal direction from the end of the substrate 2, and (d) shows the state in which the coating 3 has been peeled off and rolled up in a predetermined range in the longitudinal direction from the end of the substrate 2. [Figure 11] FIG. 11 is a plan view showing a coated substrate 1c according to a third embodiment of the present invention. [Figure 12] FIG. 12 is a partial enlarged view of the cross section III-III in FIG. 11, illustrating the cross-sectional shape of a third recess 4c and the cross-sectional shape of a band-shaped portion 3c. [Figure 13] 1A is a perspective view showing a coated substrate 1c, where (a) shows the state before peeling off the coating 3 at the third recess 4c, and (b) shows the state after a portion of the third recess 4c has been separated to peel off the band-shaped portion 3c from the substrate 2, and then the coating 3 has been peeled off. [Figure 14] 1A and 1B are perspective views showing a coated substrate 1c, where (c) shows a state in which the coating 3 has been peeled off and cut in a predetermined range in the longitudinal direction from an end of the substrate 2, and (b) shows a state in which a joint 27 has been attached to (a). [Figure 15]1A is a perspective view showing a coated substrate 1c, in which (a) shows a state in which the coating 3 has been peeled off and rolled up in a predetermined range in the longitudinal direction from the end of the substrate 2, (b) shows a state in which a joint 27 has been attached to (a), and (c) shows a state in which the coating 3 has been further applied to the joint 27 from (b). [Figure 16] FIG. 2 is a plan view showing the manufacturing apparatus 20 of the present invention. [Figure 17] FIG. 1 is a diagram showing an example of a conventional gaiter-wrapped package. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0015] Hereinafter, a coated substrate 1 and a method for manufacturing a coated substrate embodying the present invention will be described with reference to the drawings. Note that the description of the embodiment of the invention and the drawings referred to are used to explain technical features that may be adopted by the present invention. The present invention is not limited thereto. The configurations shown in the drawings are merely illustrative examples and are not intended to limit the present invention.

[0016] <Common configuration of the coated substrate 1 in each embodiment> 1 to 6 are used as representative examples to explain the configuration common to each embodiment of the coated substrate 1 according to the first aspect of the present invention. The coated substrate 1 comprises a substrate 2 that can be wrapped around in an annular shape, and a peelable coating 3 that is laminated on the outer peripheral surface 2a of the substrate 2. The coating 3 has a recess 4 formed along the longitudinal direction of the substrate 2.

[0017] As shown in FIG. 2 etc., the coating 3 is attached to the outer peripheral surface 2a of the substrate 2 in a non-adhesive state. The recesses 4 are formed along the longitudinal direction of the substrate 2, and are recessed from the outer peripheral surface 3a of the coating 3 toward the outer peripheral surface 2a of the substrate 2. The recesses 4 along the longitudinal direction may extend at a predetermined angle to the central axis C, may extend in a spiral shape, or may extend in a meandering state, in addition to the case where the substrate 2 is a cylindrical member, in addition to the case where the recesses 4 are parallel to the central axis C, in the case where the substrate 2 is a cylindrical member. The substrate 2 can be wrapped around in a ring shape, for example, a pipe, and the like, and there is no limit to the length. The substrate 2 can be applied in various forms, and may be a cylindrical member, a square tube member, a columnar member, a square column member, or the like.

[0018] The substrate 2 and the coating 3 may be made of the same type of resin material. Furthermore, the substrate 2 and the coating 3 may be made of a thermoplastic resin. For example, the substrate 2 and the coating 3 may be made of low-density polyethylene. Alternatively, high-density polyethylene, cross-linked polyethylene, polybutene, polypropylene, or polyvinyl chloride may be used. It is preferable to select a so-called pipe grade polyethylene.

[0019] The substrate 2 may also be a tube 12. As exemplified in FIG. 2 and the like, the tube 12 may be a cylindrical tube whose outer shape includes an ellipse in a cross section perpendicular to the longitudinal direction. The thickness t3 of the coating 3 is formed to be thinner than the thickness t2 of the substrate 2. For example, the tube 12 has an outer diameter of 27 mm, the thickness t2 of the substrate 2 is 4 mm, and the thickness t3 of the coating 3 is in the range of 0.15 to 0.25 mm. Even if the outer diameter dimension of the tube 12 changes, the thickness t3 of the coating 3 is appropriate within the above range. The thicker the thickness t3 of the coating 3, the higher the material cost becomes, and the more difficult it becomes to tear. Furthermore, the thickness t4 of the thin-walled portion of the recess 4 shown in FIG. 2 and the like is, for example, 0.05 mm. It is desirable that the thickness t4 of the thin-walled portion of the recess 4 is as thin as possible while having a predetermined tensile strength. The tube 12 is not limited to a cylindrical tube, and may be a square tube.

[0020] 2 and other figures, the coating 3 may be continuous over the entire circumferential direction of the outer circumferential surface 2a of the substrate 2 and in close contact with the outer circumferential surface 2a of the substrate 2.

[0021] <Effects of the configuration common to each embodiment of the coated substrate 1> The configuration common to each embodiment of the coated substrate 1 described above provides the following effects. The coating 3 is laminated on the outer peripheral surface 2a of the substrate 2 and does not easily fall off. This makes it possible to protect the outer peripheral surface 2a of the substrate 2 from scratches, dirt, and the like. In addition, the recesses 4 are formed along the longitudinal direction of the substrate 2, and the coating 3 and the outer peripheral surface 2a of the substrate 2 are peelable from each other, so that the coating 3 can be peeled off from the substrate 2 by tearing the recesses 4.

[0022] As shown in FIG. 17, in the past, for example, a long pipe product 32 was continuously manufactured at a predetermined length, and was wound and bundled at a constant diameter. The packaging film 30 was wound around the pipe product 32 in a so-called gaiter, and the pipe product 32 was shipped in a continuously spirally wound state. At the site where the pipe product 32 is used, the pipe product 32 is cut to a required length for use, and at that time, the packaging film 30 is entirely peeled off. At that time, the remaining pipe product 32 is moved or stored with the packaging film 30 peeled off. Then, the remaining pipe product 32 has a problem that dust adheres to the outer circumferential surface or is scratched. Furthermore, since the packaging film 30 is entirely peeled off, a large amount of waste is generated at the work site.

[0023] In contrast, the coated substrate 1 of the present invention solves this problem. The coating 3 also functions as a packaging material for the substrate 2. It is possible to peel off the entire coating 3, but as shown in FIG. 5(a) and other figures, it is also possible to peel off and cut only a certain area from the end of the substrate 2, leaving the coating 3 on the remaining part. In other words, at the work site, only the coating 3 peeled off from the end of the substrate 2 in a certain area becomes waste. When cutting the coating 3, it may be torn from the recess 4 in the circumferential direction, or a cutting tool may be used if it is difficult to cut.

[0024] Alternatively, as shown in FIG. 6(a) and the like, only a certain range from the end of the substrate 2 may be peeled off, and the peeled off portion may be left. When the joint 27 is connected to the coated substrate 1, as shown in FIG. 6(b) and the like, the coating 3 may be turned up and connected. Alternatively, as shown in FIG. 6(c) and the like, it is also possible to cover the peeled off portion on the joint 27 side. In this case, the peeled off portion is left without being cut off, so that waste can be reduced to zero. In the case of a pipe or the like that is buried underground, the coated substrate 1 may be left without cutting the coating 3. In addition, when the coated substrate 1 is used above ground where it can be seen, the coating 3 may be cut off to improve the appearance.

[0025] The coating 3 remaining on the coated substrate 1 can continue to serve as a packaging material to protect the outer peripheral surface 2a of the substrate 2 from dust or scratches. The coating 3 is expected to provide a certain level of protection not only during storage of the coated substrate 1, but also against dust or scratches that may occur when the substrate is dragged during construction or transportation on site. Thus, the coated substrate 1 can be cut to the required length for use at multiple work sites, and the remainder can be transported or stored.

[0026] Furthermore, if the substrate 2 and the coating 3 are made of the same resin material, the substrate 2 and the coating 3 of the coated substrate 1 do not need to be separated when they are disposed of. Therefore, they can be reused as a single unit when recycling materials, thereby reducing the environmental load.

[0027] Furthermore, if the substrate 2 and the coating 3 are made of a thermoplastic resin, they can be manufactured in a single manufacturing process, thereby reducing production costs.

[0028] 2 and other figures, when the substrate 2 is a pipe 12, it can be applied to a pipe or the like, and there is no limit to the length. For example, in the substrate 2, that is, the pipe 12, if the thickness t3 of the coating 3 is formed to be thinner than the thickness t2 of the substrate 2, the material cost of the coating 3 can be reduced. Also, the amount of the coating 3 that is peeled off and discarded can be reduced, thereby suppressing the environmental load.

[0029] Moreover, the coating 3 is continuous around the entire circumferential direction of the outer peripheral surface 2a of the substrate 2, and therefore can better protect the outer peripheral surface 2a of the substrate 2. Furthermore, if the coating 3 is in close contact with the outer peripheral surface 2a of the substrate 2, it is less likely to fall off or become displaced from the substrate 2.

[0030] <Description of the Configuration of the Film-Coated Substrate 1a of the First Embodiment> Next, with reference to FIG. 1 to FIG. 6, a coated substrate 1a of a first embodiment according to the first aspect of the present invention will be described. In the coated substrate 1a, the first recess 4a, which is a recess 4, is recessed between the outer peripheral surface 3a of the coating 3 and the outer peripheral surface 2a of the substrate 2, and is formed continuously along the longitudinal direction of the substrate 2. The cross-sectional shape of the recess 4 is not limited. For example, as in the first recess 4a shown in FIG. 2, the cross-sectional shape of the recess 4 may have a thin-walled portion with a thickness t4 within a circumferential width w1, and may be recessed in a trapezoidal shape from the outer peripheral surface 3a of the coating 3 toward the outer peripheral surface 2a of the substrate 2. Also, as in the first recess 14a shown in FIG. 3, the recess may be recessed in a V-shape from the outer peripheral surface 3a of the coating 3 toward the outer peripheral surface 2a of the substrate 2. The thickness t4 of the thin-walled portion of the first recess 4a in FIG. 2 and the first recess 14a in FIG. 3 is, for example, 0.05 mm. Also, the width w1 in the circumferential direction of the first recess 4a is, for example, 1.5 mm.

[0031] Next, referring to FIG. 4, a method of tearing the first recess 4a and peeling off the coating 3 will be described. From the state of FIG. 4(a), as shown in FIG. 4(b), an operator tears the thin portion of the first recess 4a by hand to peel off the coating 3. After the state of FIG. 4(b), a number of treatment methods can be selected for the coating 3. First, as shown in FIG. 5(a), the coating 3 peeled off from the substrate 2 is cut along the circumferential direction. Second, as shown in FIG. 6(a), the coating 3 peeled off from the substrate 2 is rolled up without being cut. Note that the first recess 4a may be formed in multiple rows to make it easier to roll up the coating 3. Similarly, the coated substrate 1b of the second embodiment described later may be formed with multiple rows of second recesses 4b.

[0032] The coated substrate 1a may be connected to a joint 27. When connecting a joint 27 to the coated substrate 1a in the state shown in Fig. 5(a), the coating 3 is peeled off and cut, and the exposed portion of the substrate 2 is inserted into the joint 27, as shown in Fig. 5(b).

[0033] Furthermore, there are two methods for connecting a joint 27 to a coated substrate 1a in the state shown in Fig. 6(a). As shown in Fig. 6(b), one method involves peeling the substrate 2 off and peeling the coating 3, and then inserting the exposed substrate 2 into the joint 27. The state shown in Fig. 6(b) is acceptable, but as shown in Fig. 6(c), after inserting the substrate 2 into the joint 27, the peeled-over portion of the coating 3 may be placed over the joint 27.

[0034] <Effects of the coated substrate 1a of the first embodiment> The above-described configuration of the coated substrate 1a provides the following effects. In the coated substrate 1a, the first recess 4a, which is the recess 4, is recessed between the outer peripheral surface 3a of the coating 3 and the outer peripheral surface 2a of the substrate 2 and is formed continuously along the longitudinal direction of the substrate 2. Thus, the coating 3 has a continuously formed thin-walled portion, so that the coating 3 can be peeled off from the substrate 2 by tearing the first recess 4a or the first recess 14a to any position in the longitudinal direction. The coating 3 can be peeled off from the end of the substrate 2 to any length in the longitudinal direction.

[0035] 5(a), the coating 3 peeled off from the substrate 2 may be cut off. For example, the coating 3 peels off when it is connected to the joint 27, but only a part of it is cut off and discarded, so that the amount of waste can be reduced.

[0036] As shown in Fig. 6(a), the coating 3 peeled off from the substrate 2 may be left rolled up without being cut. In this case, the coating 3 is not cut, so no waste is generated. Furthermore, workers do not need to use cutting tools such as scissors or a utility knife at the construction site. As shown in Fig. 6(c), the coating 3 may be placed over the joint 27 after the joint 27 is connected.

[0037] <Description of the Configuration of the Film-Coated Substrate 1b of the Second Embodiment> Next, a coated substrate 1b according to a second embodiment of the first aspect of the present invention will be described with reference to Fig. 7 to Fig. 10. In the coated substrate 1b, second recesses 4b, which are recesses 4, are formed intermittently along the longitudinal direction of the substrate 2. In the example shown in Fig. 8, the second recesses 4b penetrate from the outer peripheral surface 3a of the coating 3 to the outer peripheral surface 2a of the substrate 2. The second recesses 4b may penetrate in a cylindrical shape, or may penetrate in a conical, prismatic, or pyramidal shape.

[0038] In the example shown in Fig. 9, the second recess 14b is recessed between the outer peripheral surface 3a of the coating 3 and the outer peripheral surface 2a of the substrate 2. The cross-sectional shape of the second recess 14b shown in Fig. 9 is recessed in a truncated cone shape from the outer peripheral surface 3a of the coating 3 toward the outer peripheral surface 2a of the substrate 2, and the thin-walled portion is formed to have a thickness t4 and a diameter w1. The second recess 14b may be formed in a cone shape in addition to the example shown in Fig. 9. Alternatively, the second recess 14b may be formed in a prismatic, cylindrical, conical, or pyramidal shape.

[0039] Next, a method of peeling off the coating 3 by tearing the second recess 4b will be described with reference to FIG. 10. The method of peeling off the coating 3 is the same as that of the coated substrate 1a, and the worker tears the second recess 4b by hand from the state of FIG. 10(a) to that of FIG. 10(b), and peels off the coating 3. After the state of FIG. 10(b), the coating 3 may be cut along the circumferential direction after peeling off from the substrate 2 as shown in FIG. 10(c), or may be rolled up without being cut as shown in FIG. 10(d). The method of connecting the coated substrate 1b and the joint 27 is the same as that of the coated substrate 1a, and a description thereof will be omitted.

[0040] <Effects of the coated substrate 1b of the second embodiment> The above-described configuration of the coated substrate 1b provides the following advantages. In the coated substrate 1b, the second recesses 4b or 14b, which are recesses 4, are formed intermittently along the longitudinal direction of the substrate 2. Therefore, the coating 3 can be peeled off from the substrate 2 by tearing between the second recesses 4b or 14b and between adjacent second recesses 4b or 14b lined up in the longitudinal direction. Furthermore, the coating 3 can be peeled off from the end of the substrate 2 to any desired length in the longitudinal direction.

[0041] Since the second recesses 4b or the second recesses 14b are formed intermittently along the longitudinal direction, the strength of the coating 3 when a circumferential force is applied thereto is stronger than when the second recesses 4b or the second recesses 14b are formed continuously. This makes it possible to reduce the likelihood that the coating 3 will tear and peel off when an external force is applied thereto during transportation or the like.

[0042] In addition, since the second recesses 4b or the second recesses 14b are formed intermittently, the tearing force required to tear the recesses 4 differs between the portion where the recesses 4 are formed and the portion where the recesses 4 are not formed. That is, the portion where the second recesses 4b or the second recesses 14b are formed is easy to tear, and the portion where the second recesses 4b or the second recesses 14b are not formed is difficult to tear. Therefore, when the coating 3 is torn from the end of the substrate 2, the tearing length can be easily adjusted by the pitch interval at which the second recesses 4b or the second recesses 14b are formed.

[0043] <Description of the Configuration of the Film-Coated Substrate 1c of the Third Embodiment> Next, referring to Fig. 11 to Fig. 13, a coated substrate 1c of a third embodiment according to the first aspect of the present invention will be described. In the coated substrate 1c, a plurality of rows of third recesses 4c, which are recesses 4, are formed along the longitudinal direction of the substrate 2, and a strip-shaped portion 3c is formed between the third recesses 4c. In the example shown in Fig. 11 to Fig. 13, two third recesses 4c are continuously formed along the longitudinal direction of the substrate 2, and a strip-shaped portion 3c is formed between the third recesses 4c. In addition, as in the example of the coated substrate 1b of the second embodiment, the third recesses 4c may be formed intermittently along the longitudinal direction of the substrate 2. The interval between the third recesses 4c and the third recesses 4c in the circumferential direction can be set arbitrarily.

[0044] In the example shown in FIG. 12, the band-shaped portion 3c has a trapezoidal cross-sectional shape with a width of w4 at the bottom, and both sides in the circumferential direction are connected to the third recess 4c. The third recess 4c has a thickness t4, which is the same as that of the coated substrate 1a of the first embodiment and the coated substrate 1b of the second embodiment. In FIG. 12, the radial height of the band-shaped portion 3c is the same as the outer diameter of the coating 3, but may be lower than the outer diameter of the coating 3. In addition, the cross-sectional shape of the band-shaped portion 3c is not limited to a trapezoidal shape, and various shapes can be applied. The third recess 4c has a width w3 in the circumferential direction. The width w3 may be larger or smaller than the width w1 of the coated substrate 1a of the first embodiment and the coated substrate 1b of the second embodiment. The widths of the third recess 4c in the circumferential direction may be different from each other.

[0045] Next, a method of peeling off the coating 3 by tearing the third recess 4c will be described with reference to Fig. 13. The boundary between the band-shaped portion 3c and other portions of the coating 3 is a thin portion. As shown in Fig. 13(b), when an operator pinches the band-shaped portion 3c and pulls it up in a direction away from the substrate 2, the thin portion tears and peels off. The portion of the coating 3 that was connected to the band-shaped portion 3c floats up, and the coating 3 can be easily peeled off from the substrate 2. Note that in order to make it easier to peel off the coating 3, multiple rows of band-shaped portions 3c may be formed, and third recesses 4c may also be formed at the same time.

[0046] As with the coated substrate 1a, a number of treatment methods can be selected for the coating 3 after peeling. The first method is to cut the coating 3 peeled off from the substrate 2 along the circumferential direction as shown in FIG. 14(a). The second method is to leave the coating 3 peeled off from the substrate 2 rolled up without cutting it as shown in FIG. 15(a). The method of connecting the coated substrate 1b and the joint 27 is also the same as that of the coated substrate 1a, and includes a connection method as shown in FIG. 14(b) and a connection method as shown in FIG. 15(b) or FIG. 15(c).

[0047] <Effects of the coated substrate 1c of the third embodiment> The above-described configuration of the coated substrate 1c provides the following effects. In the coated substrate 1c, the strip portion 3c is formed between the third recesses 4c, which are the recesses 4. By tearing the third recesses 4c to separate the strip portion 3c, a claw for peeling the coating 3 from the substrate 2 can be formed. Thus, the coating 3 can be easily peeled from the substrate 2. Furthermore, if the third recesses 4c are shaped like the first recesses 4a or the first recesses 14a of the first embodiment, the effect of the coated substrate 1a can also be achieved. Furthermore, if the third recesses 4c are shaped like the second recesses 4b or the second recesses 14b of the second embodiment, the effect of the coated substrate 1b can also be achieved.

[0048] The method of treating the coating 3 and the method of connecting to the joint 27 described with reference to Figs. 14 and 15 have the same effects as those of the coated substrate 1a.

[0049] <Explanation of the coated substrate manufacturing method> Next, a method for manufacturing a coated substrate will be described. The method for manufacturing a coated substrate is a method for manufacturing a coated substrate 1 by coating an outer peripheral surface 2a of a substrate 2 that can be wrapped around an annular shape. The method for manufacturing a coated substrate includes a first step of forming the substrate 2, a second step of cooling the substrate 2 formed in the first step, and a third step of forming a coating 3 on the outer peripheral surface 2a of the substrate 2 cooled in the second step. The first step to the third step are continuously performed by a series of manufacturing apparatuses 20. Furthermore, the third step may include a fourth step of forming a recess 4 on a part of the outer peripheral surface 3a of the coating 3. The first and third steps are performed by extrusion molding of a resin, for example.

[0050] Next, the manufacturing apparatus 20 will be described with reference to FIG. 16. The manufacturing apparatus 20 is an apparatus in which the manufacturing process proceeds from left to right in the figure. In the first process, the substrate 2 is extruded in the first extruder 21 and passed through the vacuum water tank 22 to be molded. Next, in the second process, the substrate 2 molded in the vacuum water tank 22 is cooled in the first cooling water tank 23. Next, in the second extruder 24, a coating material is extruded onto the outer peripheral surface 2a of the substrate 2 to form the coating 3. The resin, which is the coating material, discharged from the second extruder 24 is pulled by the extrusion molding speed of the substrate 2. The inner and outer diameters of the coating material become smaller than when it left the second extruder 24, and the coating material coats the outer peripheral surface 2a of the substrate 2. After that, the coating material is cooled and contracted in the second cooling water tank 26, and adheres to the outer peripheral surface 2a of the substrate 2.

[0051] The substrate 2 is continuously extruded from the first extruder 21, and the take-up machine 25 takes up the coated substrate 1, so that the process proceeds continuously. The coated substrate 1 is cut when it reaches a predetermined length. Since the coating 3 also serves as a packaging material for the substrate 2, the coated substrate 1 is shipped as a product without going through a further packaging process.

[0052] <Effects of the coating substrate manufacturing method> The coated substrate manufacturing method described above has the following advantages. The coated substrate manufacturing method can reduce manufacturing costs because the first to third steps can be performed continuously using a series of manufacturing apparatuses 20. The coating 3 can be stably applied to the outer peripheral surface 2a of the substrate 2. Furthermore, when the third step, which is the step of forming the coating 3, includes a step of forming recesses 4, the recesses 4 can be stably formed. Furthermore, the need for post-processing can be eliminated, thereby reducing manufacturing costs. [Explanation of symbols]

[0053] 1, 1a, 1b, 1c coated base material 2a Outer surface 3 Coating 3a Outer surface 4 Recess 12 tubes C center axis

Claims

1. A substrate that can be wrapped around an annular shape; A peelable coating is provided on the outer peripheral surface of the substrate, The coating has a recess formed along the longitudinal direction of the substrate.

2. The coated substrate according to claim 1 , wherein the substrate and the coating are made of the same type of resin material.

3. The coated substrate of claim 1 , wherein the substrate is a tube.

4. A method for producing a coated substrate according to any one of claims 1 to 3, comprising the steps of: A first step of forming the substrate; A second step of cooling the substrate formed in the first step; A method for producing a coated substrate, comprising a third step of forming the coating on the outer peripheral surface of the substrate cooled in the second step.

Citation Information

Patent Citations

  • Colored fluorine mica ceramics and manufacture

    JP1982071863A