Grinding method

The grinding method addresses the issue of uneven surfaces by monitoring and controlling the grinding process to minimize material removal, reducing costs and enhancing productivity.

JP2024154134APending Publication Date: 2024-10-30DISCO CORP
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2023067787
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-18
Publication Date
2024-10-30

AI Technical Summary

Technical Problem

The existing methods for peeling wafers from ingots result in uneven surfaces that require excessive grinding to remove the separation layer, increasing productivity costs.

Method used

A grinding method that monitors the presence or absence of a separation layer during the grinding process, using sensors to detect changes in thickness, load, and load current, allowing precise control of the grinding process to minimize the amount of material removed.

Benefits of technology

Reduces the amount of grinding required to remove the separation layer, thereby minimizing productivity costs and improving efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024154134000001_ABST
    Figure 2024154134000001_ABST
Patent Text Reader

Abstract

To provide a grinding method capable of reducing a grinding amount in order to remove a separation layer formed onto a peeling surface of a wafer or an ingot after the peeling.SOLUTION: A grinding method of a wafer for grinding a separation layer from the wafer in which a separation layer remains onto a front surface side in a peeling surface that is peeled from an ingot by using the separation layer as an initial point by forming the separation layer by irradiating a laser beam into an inner part of the ingot, comprises: a holding step 1001 of holding a back surface of the wafer by a chuck table; and a grinding step 1002 of grinding the wafer held by the chuck table with a grinding wheel. The grinding step 1002 executes a grinding while monitoring the presence / absence of the separation layer formed onto the front surface side of the wafer, and terminates the grinding if the separation layer is removed.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a grinding method. [Background technology]

[0002] A technique is known in which a laser beam having a wavelength that is transparent to the ingot is irradiated to a single crystal ingot at a focal point thereof, forming a modified layer and a separation layer including cracks on the intended cutting surface, and then applying an external force to split the wafer along the intended cutting surface on which the separation layer has been formed, thereby separating the wafer from the ingot (see, for example, Patent Document 1). [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2016-111143 A Summary of the Invention [Problem to be solved by the invention]

[0004] When a wafer is peeled from an ingot, the peeled surface of the wafer or ingot becomes uneven, and therefore the wafer or ingot after peeling is ground to remove the unevenness, i.e., to remove the separation layer formed on the peeled surface of the wafer or ingot. In this grinding, it is essential to completely remove the separation layer formed on the peeled surface of the wafer or ingot, but there is a problem in that the wafer or ingot after peeling is required to be ground as little as possible in order to reduce production costs.

[0005] The present invention has been made in consideration of the above problems, and an object of the present invention is to provide a grinding method that reduces the amount of grinding required to remove a separation layer formed on the peeled surface of a wafer or ingot after peeling. [Means for solving the problem]

[0006] In order to solve the above-mentioned problems and achieve the object, the grinding method of the present invention is a wafer grinding method in which a separation layer is formed by irradiating a laser beam inside an ingot, and the separation layer is ground from a wafer that is peeled from the ingot using the separation layer as a starting point and leaves the separation layer on the front side of the peeled surface, the method comprising a holding step of holding the back side of the wafer on a chuck table, and a grinding step of grinding the wafer held on the chuck table with a grinding wheel, the grinding step being characterized in that grinding is performed while monitoring the presence or absence of a separation layer formed on the front side of the wafer, and grinding is terminated when the separation layer is gone.

[0007] The grinding step may include a pre-grinding step in which the predicted thickness of the separation layer is set as the movement amount of the grinding wheel, the movement amount is monitored, and the separation layer is ground to the predicted thickness, and an end point grinding step in which grinding is performed while monitoring the presence or absence of the separation layer.

[0008] The grinding step may involve performing grinding while measuring the thickness of the wafer, calculating the wear rate of the grinding wheel from the amount of change in thickness of the wafer and the amount of movement of a spindle to which the grinding wheel is attached, and detecting the presence or absence of the separation layer based on the change in the wear rate.

[0009] The grinding step may be performed while monitoring a grinding load applied to a chuck table that holds the wafer or a spindle to which a grinding wheel is attached, and the presence or absence of the separation layer may be detected based on a change in the grinding load.

[0010] The grinding step may include performing grinding while monitoring a load current value of a spindle to which a grinding wheel is attached, and detecting the presence or absence of the separation layer based on a change in the load current value. Effect of the Invention

[0011] In the present invention, grinding is performed while monitoring the presence or absence of a separation layer formed on the delamination surface (front surface side) of the wafer or ingot in the grinding step, and grinding is terminated when the separation layer is no longer present, thereby reducing the amount of grinding required to remove the separation layer formed on the delamination surface (front surface side) of the wafer or ingot after delamination. [Brief description of the drawings]

[0012] [Figure 1] FIG. 1 is a flowchart showing an example of a processing procedure of a grinding method according to an embodiment. [Diagram 2] FIG. 2 is a perspective view showing a configuration example of a grinding device for carrying out the grinding method according to the embodiment of FIG. [Diagram 3] FIG. 3 is a cross-sectional view showing a main part of the grinding apparatus of FIG. [Figure 4] FIG. 4 is an exploded cross-sectional view showing a part of the main part of the grinding device of FIG. [Diagram 5] FIG. 5 is a diagram illustrating the grinding step of FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0013] The form (embodiment) for carrying out the present invention will be described in detail with reference to the drawings. The present invention is not limited to the contents described in the following embodiment. Furthermore, the components described below include those that a person skilled in the art can easily imagine and those that are substantially the same. Furthermore, the configurations described below can be appropriately combined. Furthermore, various omissions, substitutions, or modifications of the configurations can be made without departing from the gist of the present invention.

[0014] [Embodiment] A grinding method according to an embodiment of the present invention will be described with reference to the drawings. FIG. 1 is a flowchart showing an example of a processing procedure of the grinding method according to the embodiment. FIG. 2 is a perspective view showing an example of the configuration of a grinding device 1 that performs the grinding method according to the embodiment of FIG. 1. As shown in FIG. 1, the grinding method according to the embodiment includes a holding step 1001 and a grinding step 1002. Both the holding step 1001 and the grinding step 1002 of the grinding method according to the embodiment are performed using, for example, the grinding device 1 shown in FIG. 2.

[0015] In this embodiment, the workpiece 100 to be ground in the grinding method according to the embodiment is, as shown in FIG. 2, a wafer such as a disk-shaped semiconductor wafer or an optical device wafer having a substrate made of silicon, sapphire, silicon carbide (SiC), gallium arsenide, or the like, or an ingot such as a single crystal semiconductor ingot having a base material made of a similar material such as silicon, sapphire, silicon carbide (SiC), gallium arsenide, or the like.

[0016] The workpiece 100 is a single crystal ingot in which a modified layer is formed by irradiating a laser beam that is transparent to the ingot, and further a separation layer including the modified layer and the cracks is formed by forming cracks extending from both sides of the modified layer, and a wafer is peeled from the ingot starting from this separation layer, or an ingot in which a wafer is peeled from the separation layer. The modified layer is, for example, a region in which the density, refractive index, mechanical strength, and other physical properties are different from those of the surrounding area.

[0017] When the workpiece 100 is a wafer peeled from an ingot, a separation layer having irregularities remains on the peeled surface peeled from the ingot. When the workpiece 100 is an ingot peeled from a wafer, a separation layer having irregularities remains on the peeled surface peeled from the wafer. In this specification, the peeled surface side of the workpiece 100 on which the separation layer remains is referred to as the front side, and the surface side of the workpiece 100 opposite to the peeled surface on which the separation layer remains is referred to as the back side.

[0018] When the workpiece 100 is a wafer peeled off from an ingot, the separation layer is removed from the front side by the grinding method according to the embodiment, and then, for example, dividing lines that intersect (orthogonally) are formed on one side, chip-shaped devices are formed in each area partitioned by the dividing lines, and individual semiconductor device chips are manufactured by dividing along the dividing lines by a cutting device or the like. When the workpiece 100 is an ingot peeled off from a wafer, the separation layer is removed from the front side by the grinding method according to the embodiment, and then, as described above, a modified layer is formed by irradiating the ingot with a laser beam that is transparent to the ingot again, and further, cracks extending from both sides of the modified layer are formed, thereby forming a separation layer including the modified layer and the cracks, and the wafer is peeled off from the ingot starting from this separation layer.

[0019] 2, a grinding device 1 that performs the holding step 1001 and the grinding step 1002 of the grinding method according to the embodiment includes a chuck table 10, a grinding unit 20, a contact type thickness measurement unit 30, and a control unit 40. Note that, in this embodiment, a so-called single-axis type grinding device 1 provided with one grinding unit 20 (spindle 21) is used, but the present invention is not limited to this, and a so-called two-axis type grinding device provided with two grinding units 20 (spindle 21) or a grinding device provided with three or more grinding units 20 (spindle 21) may also be used.

[0020] Fig. 3 is a cross-sectional view showing a main part of the grinding device 1 in Fig. 2. Fig. 4 is an exploded cross-sectional view showing a part of the main part of the grinding device 1 in Fig. 3. The chuck table 10 holds the workpiece 100 from the back side. The chuck table 10 is provided so as to be freely movable in the X-axis direction parallel to the horizontal direction by a moving unit (not shown) between a carry-in / carry-out position located on the left front side of Fig. 2 and a grinding position close to the grinding unit 20 located on the right rear side of Fig. 2.

[0021] As shown in Figs. 3 and 4, the chuck table 10 includes a disk-shaped frame 11 having a recess formed therein, and a disk-shaped suction portion 12 fitted into the recess. The suction portion 12 of the chuck table 10 is made of porous ceramics or the like having a large number of porous holes, and is connected to a vacuum suction source (not shown) via a vacuum suction path (not shown). The upper surface of the suction portion 12 of the chuck table 10 is a holding surface 13 that suction-holds the placed workpiece 100 from below. In this embodiment, the upper surface of the frame 11 and the holding surface 13 are formed into a cone-like shape with a slightly lower outer periphery, with the center 13-1 of the holding surface 13 of the chuck table 10 as the apex, as shown in Fig. 2. Note that the holding surface 13 is not limited to this in the present invention, and may be formed flat.

[0022] 3 and 4, an annular bearing 14 that supports the chuck table 10 is provided below the chuck table 10, and an annular support plate 15 is fixed below the annular bearing 14. The bearing 14 supports the chuck table 10 rotatably relative to the support plate 15. An annular table base 16 is provided below the support plate 15.

[0023] The chuck table 10 is provided so as to be rotatable by a rotary drive source 17 about a predetermined rotation axis that passes through the center 13-1 of the holding surface 13 and is perpendicular to the bottom surface of the cone that forms the holding surface 13. As shown in Figures 3 and 4, the rotary drive source 17 is positioned in openings provided in the centers of the bearing 14, the support plate 15, and the table base 16, and is connected to the lower side of the frame 11 of the chuck table 10.

[0024] 3 and 4, a load sensor 18 is provided between the support plate 15 and the table base 16. The load sensors 18 are provided at a plurality of locations (e.g., three locations) at equal intervals (e.g., 120 degrees) along the circumferential direction of the holding surface 13 of the chuck table 10. The load sensor 18 measures the load applied to the chuck table 10 and outputs the measured load to the control unit 40. The load sensor 18 measures the grinding load applied to the chuck table 10 during grinding by the grinding unit 20 and outputs the measured grinding load to the control unit 40.

[0025] 3 and 4, a rotation axis adjustment unit 19 that tilts the rotation axis of the chuck table 10 with respect to the Z-axis direction parallel to the vertical direction is provided below the table base 16. The rotation axis adjustment unit 19 allows the rotation axis of the chuck table 10 to be tilted by an inclination angle within a predetermined range with respect to the Z-axis direction parallel to the vertical direction, and accordingly, the holding surface 13 can be tilted by the same inclination angle with respect to a horizontal plane parallel to the XY plane, in which the bottom surface of the cone that forms the holding surface 13 is formed.

[0026] As shown in Fig. 2 and Fig. 3, the grinding unit 20 includes a spindle 21, a grinding wheel 22, a grinding feed unit 24, a grinding fluid supply unit 25, a load current value detection sensor 26, and a load sensor 28. The spindle 21 is provided rotatably around an axis parallel to the vertical direction (Z-axis direction) and supports the grinding wheel 22 detachably attached to the lower end so as to be rotatable around an axis parallel to the vertical direction. The grinding wheel 22 has a grinding wheel 23 arranged in an annular shape on its lower surface. In this embodiment, the grinding wheel 23 arranged in an annular shape on the grinding wheel 22 is formed by fixing abrasive grains such as diamond, cBN (cubic boron nitride), etc., with a bond material (binding material) such as a metal bond, a resin bond, or a vitrified bond.

[0027] The grinding unit 20 is disposed so that the spindle 21 faces the holding surface 13 of the chuck table 10 positioned at the grinding position in the vertical direction. In the grinding device 1 in this embodiment, as shown in Fig. 2 and Fig. 3, the rotation axis of the chuck table 10 positioned at the grinding position and the rotation axes of the spindle 21 and grinding wheel 22 of the grinding unit 20 are arranged to be shifted in the horizontal direction, and when the grinding unit 20 grinds the grinding surface of the workpiece 100 held on the chuck table 10, a part of the grinding surface of the workpiece 100 held on the chuck table 10 is exposed upward.

[0028] The grinding feed unit 24 performs grinding feed in which the spindle 21 of the grinding unit 20 and the grinding wheel 22 attached to the spindle 21 are moved relatively along the grinding feed direction (the Z-axis direction parallel to the vertical direction) relative to the chuck table 10 positioned at the grinding position, thereby moving the spindle 21 and the grinding wheel 22 closer to and farther away from the chuck table 10 positioned at the grinding position relative to the grinding feed direction.

[0029] The grinding feed unit 24 is a known ball screw mechanism having a motor, a ball screw, and a guide. The grinding feed unit 24 is configured to have a ball screw provided so as to be rotatable around the axis of the Z axis, a motor for rotating the ball screw around the axis, and a guide for supporting the spindle 21 so as to be movable in the Z axis direction. The grinding feed unit 24 has a feed speed and a movement amount controlled by the control unit 40 controlling the driving of the motor. Here, the feed speed refers to a speed at which the grinding feed unit 24 moves the spindle 21 and the grinding wheel 22 relatively close to and away from the chuck table 10 positioned at the grinding position along the Z axis direction. The movement amount refers to an amount (height) at which the grinding feed unit 24 moves the spindle 21 and the grinding wheel 22 relatively close to and away from the chuck table 10 positioned at the grinding position along the Z axis direction. The feed speed is the movement amount per unit time.

[0030] The grinding feed unit 24 includes an encoder that reads the rotational position of the motor, and detects the relative position in the Z-axis direction with respect to the chuck table 10 positioned at the grinding position of the spindle 21 based on the rotational position of the motor read by the encoder, and outputs the detected relative position to the control unit 40. Here, for the relative position in the Z-axis direction, an apparatus orthogonal coordinate system (XYZ coordinates) provided in the grinding apparatus 1 is used. For example, the center of the chuck table 10 positioned at the grinding position is set as the origin of the apparatus orthogonal coordinate system. In addition, the grinding feed unit 24 detects the relative position in the Z-axis direction with respect to the chuck table 10 positioned at the grinding position of the spindle 21 at regular time intervals (for example, every second) before the start of grinding, during grinding, and after the end of grinding, for example, to detect the feed speed and the movement amount, and output the detected feed speed and the movement amount to the control unit 40. In addition, the grinding feed unit 24 is not limited to a configuration in which an encoder detects the relative position in the Z-axis direction with respect to the chuck table 10 positioned at the grinding position of the spindle 21, but may also be configured with a linear scale parallel to the Z-axis direction and a reading head that is freely movable in the Z-axis direction by the grinding feed unit 24 and reads the graduations of the linear scale.

[0031] The grinding fluid supply unit 25 supplies a grinding fluid such as pure water to the workpiece 100 held on the chuck table 10 positioned at the grinding position. The load current value detection sensor 26 is connected to the spindle motor provided in the spindle 21, and detects the load current value of the spindle 21, which is the value of the current flowing through the spindle motor provided in the spindle 21. The load current value of the spindle 21 tends to increase as the grinding load and grinding resistance increase when the workpiece 100 is ground with the grinding wheel 22.

[0032] 3, a load sensor 28 is provided below the spindle 21 between the spindle 21 and a cover member covering the outer periphery of the spindle 21. The load sensor 28 is provided at a plurality of locations (e.g., three locations) at equal intervals (e.g., 120 degrees) along the circumferential direction of the grinding wheel 22 attached to the spindle 21. The load sensor 28 measures the load applied to the spindle 21 to which the grinding wheel 22 is attached, and outputs the measured load to the control unit 40. The load sensor 28 measures the grinding load applied to the spindle 21 to which the grinding wheel 22 is attached during grinding by the grinding unit 20, and outputs the measured grinding load to the control unit 40.

[0033] In the grinding unit 20, the spindle 21 is rotated around an axis parallel to the vertical direction, thereby rotating the grinding wheel 22 attached to the lower end of the spindle 21 around an axis parallel to the vertical direction, and the chuck table 10, which is positioned at the grinding position and disposed opposite the spindle 21 and holds the workpiece 100, is rotated around the rotation axis, and while a grinding fluid supply unit 25 supplies a grinding fluid to the workpiece 100 held on the rotated chuck table 10, the grinding feed unit 24 presses the rotating grinding wheel 22 along the grinding feed direction, thereby grinding the workpiece 100 with the grinding stone 23 of the grinding wheel 22. The grinding wheel 22 grinds the workpiece 100 along the grinding surface, forming the grinding surface of the workpiece 100 parallel to the grinding surface.

[0034] In this embodiment, the contact type thickness measurement unit 30 is provided near the grinding position as shown in Fig. 2. As shown in Fig. 2, the contact type thickness measurement unit 30 includes a first probe 31 and a second probe 32. In this embodiment, the first probe 31 and the second probe 32 are both contact type probes that measure the height of the position of contact.

[0035] The first probe 31 comes into contact with the outside of the workpiece 100 on the holding surface 13 of the chuck table 10 holding the workpiece 100, thereby measuring the position of the holding surface 13 in the Z-axis direction, i.e., the height of the holding surface 13. The second probe 32 comes into contact with the top surface (surface to be ground) of the workpiece 100 held on the holding surface 13 of the chuck table 10, thereby measuring the position (top surface position) of the top surface of the workpiece 100 in the Z-axis direction, i.e., the height (top surface height) of the top surface of the workpiece 100. Both the first probe 31 and the second probe 32 output the measured position (height) results to the control unit 40. In addition, both the first probe 31 and the second probe 32 detect the height of the holding surface 13 of the chuck table 10 and the height of the top surface of the workpiece 100 before grinding begins, during grinding, and after grinding is completed, for example at regular intervals (for example, every second), to obtain the time changes in the height of the holding surface 13 and the time changes in the height of the top surface of the workpiece 100, and output these obtained time changes to the control unit 40.

[0036] The control unit 40 controls the operation of various components of the grinding device 1, and causes the grinding device 1 to perform a grinding process of the workpiece 100, including the grinding method according to the embodiment. During grinding of the workpiece 100 by the grinding unit 20, the control unit 40 acquires the grinding load applied to the chuck table 10 by the load sensor 18 provided on the chuck table 10 positioned at the grinding position, acquires the feed speed and movement amount of the spindle 21 by the grinding feed unit 24, acquires the load current value of the spindle 21 by the load current value detection sensor 26, acquires the grinding load applied to the spindle 21 to which the grinding wheel 22 is attached by the load sensor 28, and acquires the time change in the height of the holding surface 13 and the time change in the height of the upper surface of the workpiece 100 by the contact type thickness measurement unit 30. The control unit 40 controls the feed speed and movement amount of the spindle 21 by the grinding feed unit 24.

[0037] The control unit 40 calculates the thickness of the workpiece 100 by subtracting the height of the holding surface 13 from the height of the upper surface of the workpiece 100 based on the height of the holding surface 13 and the height of the upper surface of the workpiece 100 acquired by the contact thickness measurement unit 30. The control unit 40 calculates the time change in the thickness of the workpiece 100 and the amount of change in the thickness of the workpiece 100 based on the time change in the height of the holding surface 13 and the time change in the height of the upper surface of the workpiece 100 acquired by the contact thickness measurement unit 30, and calculates the grinding amount of the workpiece 100 ground by the grinding wheel 22 based on the calculated time change in the thickness of the workpiece 100 and the amount of change in the thickness of the workpiece 100. In this way, the control unit 40 can substantially measure the thickness of the workpiece 100, the time change in the thickness of the workpiece 100, and the amount of change in the thickness of the workpiece 100 by the contact thickness measurement unit 30.

[0038] The control unit 40 calculates the wear rate of the grinding wheel 22 attached to the spindle 21 by subtracting the change in thickness of the workpiece 100 from the movement amount of the spindle 21 based on the movement amount of the spindle 21 acquired by the grinding feed unit 24 and the change in thickness of the workpiece 100 acquired by actual measurement using the contact type thickness measurement unit 30. The control unit 40 also calculates the wear rate of the grinding wheel 22 attached to the spindle 21 in a predetermined unit time by subtracting the change in thickness of the workpiece 100 per predetermined unit time (e.g., 1 second) from the movement amount of the spindle 21 per predetermined unit time (e.g., 1 second) based on the movement amount of the spindle 21 acquired by the grinding feed unit 24 and the change in thickness of the workpiece 100 acquired by actual measurement using the contact type thickness measurement unit 30, and dividing the subtracted value by the change in thickness of the workpiece 100 per predetermined unit time. Furthermore, the control unit 40 calculates a moving average of the wear rate of the grinding wheel 22 per predetermined time (for example, 10 seconds) based on data on the time change of the wear rate of the grinding wheel 22 in a predetermined unit time.

[0039] The control unit 40 calculates a moving average of the grinding loads applied to the chuck table 10 and the spindle 21 per predetermined time (e.g., 10 seconds) based on data on the change over time of the grinding loads applied to the chuck table 10 and the spindle 21. The control unit 40 calculates a moving average of the load current value of the spindle 21 per predetermined time (e.g., 10 seconds) based on data on the change over time of the load current value of the spindle 21.

[0040] In this embodiment, the control unit 40 includes a computer system. The computer system included in the control unit 40 includes an arithmetic processing device having a microprocessor such as a CPU (Central Processing Unit), a storage device having a memory such as a ROM (Read Only Memory) or a RAM (Random Access Memory), and an input / output interface device. The arithmetic processing device of the control unit 40 performs arithmetic processing according to a computer program stored in the storage device of the control unit 40, and outputs control signals for controlling the grinding device 1 to each component of the grinding device 1 via the input / output interface device of the control unit 40.

[0041] The grinding device 1 may include a cassette, an alignment unit, a carry-in unit, an unloading unit, a cleaning unit, and a carry-in / out unit (not shown) in the vicinity of the carry-in / out position of the chuck table 10. The cassette is a container for storing a plurality of workpieces 100. The alignment unit is a table on which the workpieces 100 removed from the cassette are temporarily placed and their center alignment is performed. The carry-in unit has a suction pad, and adsorbs and holds the workpiece 100 before grinding aligned by the alignment unit, and carries it onto the chuck table 10 positioned at the carry-in / out position. The carry-out unit adsorbs and holds the workpiece 100 after grinding held on the chuck table 10 positioned at the carry-in / out position, and carries it out to the cleaning unit. The cleaning unit cleans the workpiece 100 after grinding, and removes contamination such as grinding chips attached to the ground surface. The carry-in / out unit carries the workpiece 100 before grinding out of the cassette to the alignment unit, and carries the workpiece 100 after grinding out of the cleaning unit into the cassette. The carry-in / out unit is, for example, a robot pick equipped with a U-shaped hand, and transports the workpiece 100 by suction-holding it with the U-shaped hand.

[0042] A grinding method according to an embodiment will be described below. In the present specification, a wafer grinding method for grinding a wafer as a workpiece 100 and removing a separation layer formed on the peeled surface (front surface side) of the wafer will be described below, but the present invention is not limited thereto and also includes an ingot grinding method for grinding an ingot as a workpiece 100 and removing a separation layer formed on the peeled surface (front surface side) of the ingot.

[0043] The holding step 1001 is a step in which the back surface of the wafer, which is the workpiece 100, is held by the chuck table 10. In the holding step 1001, first, a carry-in / out unit (not shown) carries out the workpiece 100 (wafer) accommodated in a cassette (not shown) and transports it to an alignment unit (not shown), and the alignment unit aligns the center of the transported workpiece 100 (wafer), and then, a carry-in unit (not shown) carries the workpiece 100 (wafer) centered by the alignment unit onto the holding surface 13 of the chuck table 10 positioned at the carry-in / carry-out position. In the holding step 1001, the back surface of the workpiece 100 (wafer) loaded onto the holding surface 13 is then suction-held by the holding surface 13 of the chuck table 10, and then the chuck table 10, with the workpiece 100 (wafer) being suction-held by the holding surface 13, is moved from the loading / unloading position to the grinding position by a moving unit not shown.

[0044] The grinding step 1002 is a step in which the workpiece 100, which is a wafer, held on the chuck table 10 is ground by the grinding wheel 22. In the grinding step 1002, first, the spindle 21 is rotated around an axis parallel to the vertical direction, thereby rotating the grinding wheel 22 attached to the lower end of the spindle 21 around an axis parallel to the vertical direction, and the chuck table 10, which is positioned at the grinding position and opposed to the spindle 21 and holds the workpiece 100 (wafer), is rotated around the rotation axis. In the grinding step 1002, next, the grinding fluid is supplied to the workpiece 100 (wafer) held on the rotated chuck table 10 by the grinding feed unit 24, while the grinding fluid supply unit 25 supplies grinding fluid to the workpiece 100 (wafer) held on the rotated chuck table 10, and the grinding wheel 23 of the grinding wheel 22 is pressed along the grinding feed direction.

[0045] FIG. 5 is a diagram for explaining the grinding step 1002 in FIG. 1. FIG. 5 shows a graph of the change in wear rate of the grinding wheel 22 with respect to the amount of grinding of the workpiece 100 (wafer) when the grinding wheel 22 grinds the peeled surface (front surface side) of the workpiece 100 (wafer) on which a separation layer having a thickness of about 15 μm is formed, while maintaining the feed rate of the spindle 21 constant at, for example, 0.4 μm / s, and maintaining the same grinding conditions for grinding the workpiece 100 (wafer) with the other grinding wheels 22, as in the grinding step 1002. Here, as shown in FIG. 5, the calculated wear rate of the grinding wheel 22 may vary greatly depending on the timing of calculation. Therefore, in this embodiment, taking into consideration the variation in the wear rate of the grinding wheel 22, a moving average of the wear rate of the grinding wheel 22 per predetermined time (for example, 10 seconds) calculated based on the time change of the wear rate of the grinding wheel 22 is used. In addition, in this embodiment, similar to the wear rate of the grinding wheel 22, the moving average of the grinding load applied to the chuck table 10 and the spindle 21, and the load current value of the spindle 21 per a predetermined period of time (e.g., 10 seconds) is used.

[0046] The graph in Figure 5 shows that in the region where the amount of workpiece 100 (wafer) ground is about 15 μm or less, the moving average of the wear rate of the grinding wheel 22 becomes larger than a predetermined threshold value (0.7% in the example shown in Figure 5), and as the amount of workpiece 100 (wafer) ground increases, the moving average of the wear rate of the grinding wheel 22 gradually decreases, and in the region where the amount of workpiece 100 (wafer) ground is more than about 15 μm, the moving average of the wear rate of the grinding wheel 22 settles at a low value below the predetermined threshold value. Here, in FIG. 5, the area of ​​the workpiece 100 (wafer) where the amount of grinding is about 15 μm or less is the area where the separation layer of the workpiece 100 (wafer) is being ground by the grinding wheel 22, and in FIG. 5, the area of ​​the workpiece 100 (wafer) where the amount of grinding is more than about 15 μm is the area where the grinding wheel 22 has finished grinding the separation layer of the workpiece 100 (wafer) and is grinding the portion that is not the separation layer.

[0047] In this way, when the grinding conditions for grinding the workpiece 100 (wafer) with the grinding wheel 22 are maintained the same, when the grinding wheel 22 grinds the separation layer of the workpiece 100 (wafer), the moving average of the wear rate of the grinding wheel 22 is larger than when the grinding wheel 22 grinds the portion of the workpiece 100 (wafer) that is not the separation layer, and therefore it can be seen that the grinding load on the grinding wheel 22 is larger. Furthermore, when the grinding conditions for grinding the workpiece 100 (wafer) with the grinding wheel 22 are maintained the same, when the separation layer of the workpiece 100 (wafer) is ground with the grinding wheel 22, the grinding load applied to the chuck table 10 that holds the workpiece 100 (wafer) to be ground and the spindle 21 to which the grinding wheel 22 that grinds the workpiece 100 (wafer) is attached is smaller than when the grinding wheel 22 is used to grind an area of ​​the workpiece 100 (wafer) that is not the separation layer, and the load current value of the spindle 21 to which the grinding wheel 22 that grinds the workpiece 100 (wafer) is attached is lower.

[0048] For this reason, in the grinding step 1002, the presence or absence of a separation layer can be monitored by the following methods of the first, second, and third examples. In this embodiment, the grinding step 1002 performs grinding while monitoring the presence or absence of a separation layer formed on the peeled surface (front surface side) of the workpiece 100 (wafer), and ends grinding when the separation layer disappears, that is, when it is detected that the separation layer does not exist.

[0049] In a first example of the grinding step 1002, the control unit 40 performs grinding while measuring the thickness of the workpiece 100 (wafer), calculates the wear rate of the grinding wheel 22 from the amount of change in the thickness of the workpiece 100 (wafer) and the amount of movement of the spindle 21 on which the grinding wheel 22 is attached, and detects the presence or absence of a separation layer based on the change in the wear rate.

[0050] In the first example of the grinding step 1002, specifically, the control unit 40 calculates the wear rate of the grinding wheel 22 attached to the spindle 21 by subtracting the time change in the thickness of the workpiece 100 (wafer) from the feed rate of the spindle 21 based on the feed rate of the spindle 21 acquired by the grinding feed unit 24 and the time change in the thickness of the workpiece 100 (wafer) acquired by substantially measuring it by the contact type thickness measuring unit 30, and calculates the moving average of the wear rate of the grinding wheel 22 per predetermined time based on the time change in the wear rate of the grinding wheel 22. In the first example of the grinding step 1002, if the moving average of the wear rate of the grinding wheel 22 per predetermined time becomes larger than a predetermined threshold, it detects that the separation layer still remains, and if the moving average of the wear rate of the grinding wheel 22 per predetermined time becomes equal to or less than a predetermined threshold within a predetermined time, for example, it detects that the separation layer has disappeared and grinding of the separation layer has been completed.

[0051] Here, the predetermined threshold value in the first example of the grinding step 1002 is predetermined to a value that is sufficiently larger than the moving average of the wear rate of the grinding wheel 22 per predetermined time calculated when grinding the portion that is not the separation layer, and is not sufficiently larger than the moving average of the wear rate of the grinding wheel 22 per predetermined time calculated when grinding the separation layer, and is stored in the control unit 40.

[0052] 5, it can be seen that the moving average of the wear rate of the grinding wheel 22 transitions from a state greater than a predetermined threshold value (0.7% in the example shown in FIG. 5) to a state equal to or less than the predetermined threshold value when the amount of wear of the workpiece 100 (wafer) ground reaches 15 μm (approximately 14 μm in the example shown in FIG. 5). In such a case, when the control unit 40 detects that the calculated moving average of the wear rate of the grinding wheel 22 has become equal to or less than the predetermined threshold value within a predetermined time, the control unit 40 detects that the separation layer has disappeared and grinding of the separation layer has ended, and ends the first example of the grinding step 1002.

[0053] In a second example of the grinding step 1002, the control unit 40 performs grinding while monitoring the grinding load applied to the chuck table 10 holding the workpiece 100 (wafer) to be ground or the spindle 21 on which the grinding wheel 22 is mounted, and detects the presence or absence of a separation layer based on a change in the grinding load.

[0054] In the second example of the grinding step 1002, specifically, the control unit 40 acquires the grinding load applied to the chuck table 10 holding the workpiece 100 (wafer) to be ground by the load sensor 18, acquires the grinding load applied to the spindle 21 to which the grinding wheel 22 is attached by the load sensor 28, and calculates the moving average of the grinding load applied to each of the chuck table 10 and the spindle 21 per predetermined time based on the time change of the grinding load applied to each of the chuck table 10 and the spindle 21. In the second example of the grinding step 1002, if the moving average of the grinding load applied to the chuck table 10 or the spindle 21 per predetermined time becomes smaller than a predetermined threshold, it detects that the separation layer still remains, and if the moving average of the grinding load applied to the chuck table 10 or the spindle 21 per predetermined time becomes equal to or greater than a predetermined threshold within a predetermined time, for example, it detects that the separation layer has disappeared and grinding of the separation layer has been completed. In a second example of the grinding step 1002, when the control unit 40 detects that the calculated moving average of the grinding load applied to the chuck table 10 or the spindle 21 has become equal to or greater than a predetermined threshold within a predetermined time, the control unit 40 detects that the separation layer has disappeared and grinding of the separation layer has been completed, and ends the second example of the grinding step 1002.

[0055] Here, the specified threshold value in the second example of grinding step 1002 is predetermined to a value that is sufficiently smaller than the moving average of the grinding load applied to the chuck table 10 or the spindle 21 calculated when grinding the portion that is not the separation layer, and is not sufficiently smaller than the moving average of the grinding load applied to the chuck table 10 or the spindle 21 calculated when grinding the separation layer, and is stored in the control unit 40.

[0056] In the third example of the grinding step 1002, the control unit 40 performs grinding while monitoring the load current value of the spindle 21 to which the grinding wheel 22 is attached, and detects the presence or absence of a separation layer from a change in the load current value.

[0057] In the third example of the grinding step 1002, specifically, the control unit 40 acquires the load current value of the spindle 21 by the load current value detection sensor 26, and calculates the moving average of the load current value of the spindle 21 per predetermined time based on the time change of the load current value of the spindle 21. In the third example of the grinding step 1002, when the moving average of the load current value of the spindle 21 per predetermined time becomes lower than a predetermined threshold, it detects that the separation layer still remains, and when the moving average of the load current value of the spindle 21 per predetermined time becomes equal to or greater than a predetermined threshold within a predetermined time, for example, it detects that the separation layer has disappeared and grinding of the separation layer has ended. In the third example of the grinding step 1002, the control unit 40 detects that the separation layer has disappeared and grinding of the separation layer has ended at the timing when it detects that the calculated moving average of the load current value of the spindle 21 has become equal to or greater than a predetermined threshold within a predetermined time, for example, and ends the third example of the grinding step 1002.

[0058] Here, the predetermined threshold value in the third example of grinding step 1002 is predetermined to a value that is sufficiently lower than the moving average of the load current value of the spindle 21 calculated when grinding the portion that is not the separation layer, and is not sufficiently lower than the moving average of the load current value of the spindle 21 calculated when grinding the separation layer, and is stored in the control unit 40.

[0059] Also, the thickness of the separation layer formed on the peeled surface (front surface side) of the workpiece 100 (wafer) can be roughly predicted by investigating in advance. For this reason, as shown in FIG. 1, the grinding step 1002 may be provided with a pre-grinding step 1011 in which the predicted thickness of the separation layer is set as the movement amount of the grinding wheel 22 without monitoring the presence or absence of the separation layer, and the movement amount is monitored to grind the separation layer by the predicted thickness, and an end-point grinding step 1012 in which grinding is performed while monitoring the presence or absence of the separation layer and grinding is terminated when the separation layer is gone. By providing the pre-grinding step 1011 and the end-point grinding step 1012 in this way, the grinding step 1002 can reduce the time for grinding while monitoring the presence or absence of the separation layer to the minimum necessary, and can more efficiently reduce the amount of grinding required to remove the separation layer formed on the peeled surface (front surface side) of the wafer or ingot after peeling.

[0060] In the grinding method according to the embodiment having the above-mentioned configuration, grinding is performed while monitoring the presence or absence of a separation layer formed on the peeled surface (front surface side) of the workpiece 100 (wafer or ingot) in the grinding step 1002, and grinding is terminated when the separation layer disappears, that is, when it is detected that there is no separation layer. Therefore, the grinding method according to the embodiment has an effect of reducing the amount of grinding required to remove the separation layer formed on the peeled surface (front surface side) of the wafer or ingot after peeling.

[0061] Moreover, the grinding method according to the embodiment can be configured to include a pre-grinding step 1011 in which the grinding step 1002 omits monitoring the presence or absence of a separation layer, sets the expected thickness of the separation layer as the movement amount of the grinding wheel 22, monitors the movement amount, and grinds the separation layer by the expected thickness, and an end-point grinding step 1012 in which grinding is performed while monitoring the presence or absence of the separation layer, and ends when the separation layer is gone. Therefore, the grinding method according to the embodiment can more efficiently reduce the amount of grinding required to remove the separation layer formed on the peeled surface (front surface side) of the wafer or ingot after peeling, by reducing the time for grinding while monitoring the presence or absence of the separation layer to the minimum necessary.

[0062] In the first example of the grinding method according to the embodiment, the control unit 40 performs grinding while measuring the thickness of the workpiece 100 (wafer or ingot), calculates the wear rate of the grinding wheel 22 from the change in thickness of the workpiece 100 (wafer or ingot) and the movement amount of the spindle 21 to which the grinding wheel 22 is attached, and detects the presence or absence of a separation layer from the change in the wear rate. In the second example of the grinding method according to the embodiment, the control unit 40 performs grinding while monitoring the grinding load applied to the chuck table 10 that holds the workpiece 100 (wafer or ingot) to be ground or the spindle 21 to which the grinding wheel 22 is attached, and detects the presence or absence of a separation layer from the change in the grinding load. In the third example of the grinding method according to the embodiment, the control unit 40 performs grinding while monitoring the load current value of the spindle 21 to which the grinding wheel 22 is attached, and detects the presence or absence of a separation layer from the change in the load current value. For these reasons, the grinding method according to the embodiment can accurately and appropriately detect the presence or absence of a separation layer.

[0063] It should be noted that the present invention is not limited to the above-described embodiment, and various modifications can be made without departing from the gist of the present invention. [Explanation of symbols]

[0064] 1 Grinding equipment 10 Chuck table 21 Spindle 22 Grinding Wheel 100 Workpiece (corresponding to the wafer according to the present invention) 1001 Hold Step 1002 Grinding step 1011 Pre-grinding step 1012 End point grinding step

Claims

1. A method for grinding a wafer, comprising: forming a separation layer by irradiating an inside of an ingot with a laser beam; and grinding the separation layer from a wafer that is peeled from the ingot starting from the separation layer and has the separation layer remaining on a surface side of the peeled wafer, the method comprising the steps of: a holding step of holding the back surface of the wafer on a chuck table; a grinding step of grinding the wafer held on the chuck table with a grinding wheel, The grinding step includes: A grinding method comprising the steps of: carrying out grinding while monitoring the presence or absence of a separation layer formed on the front surface side of the wafer; and terminating grinding when the separation layer disappears.

2. The grinding step includes: a pre-grinding step of setting a movement amount of a grinding wheel equal to an expected thickness of the separation layer, monitoring the movement amount, and grinding the separation layer by the expected thickness; 2. The grinding method according to claim 1, further comprising an end point grinding step of performing grinding while monitoring the presence or absence of the separation layer.

3. The grinding step includes:

3. The grinding method according to claim 1, further comprising the steps of: measuring the thickness of the wafer while grinding; calculating a wear rate of the grinding wheel from a change in thickness of the wafer and a movement amount of a spindle to which the grinding wheel is attached; and detecting the presence or absence of the separation layer based on a change in the wear rate.

4. The grinding step includes:

3. The grinding method according to claim 1, further comprising the steps of: performing grinding while monitoring a grinding load applied to a chuck table that holds the wafer or a spindle to which a grinding wheel is attached; and detecting the presence or absence of the separation layer based on a change in the grinding load.

5. The grinding step includes:

3. A grinding method according to claim 1, further comprising the steps of: performing grinding while monitoring a load current value of a spindle to which a grinding wheel is attached; and detecting the presence or absence of said separation layer based on a change in said load current value.

Citation Information

Patent Citations

  • Method and apparatus for setting reference chuck table for set-up in grinder

    JP2001001261A

  • Method for grinding workpiece

    JP2011036962A

  • Processing end point detection method and processing end point detection apparatus

    JP2012124419A

  • Detection method of grinding wheel wear amount

    JP2014037045A

  • SiC SUBSTRATE SEPARATING METHOD

    JP2017092314A