Imprinting device, and imprinting method
The imprint apparatus uses a conductive heating film to improve resist fluidity during pattern transfer, addressing inaccuracies in existing methods by preventing voids and thermal expansion, thus ensuring precise pattern formation.
Patent Information
- Application Number
- JP2023068594
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-19
- Publication Date
- 2024-10-31
AI Technical Summary
Existing imprint methods using thermoplastic polymers with organic solvents face challenges in maintaining resist fluidity at room temperature, leading to pattern transfer inaccuracies due to void formation and thermal expansion issues.
An imprint apparatus with a conductive heating film on the imprint mold generates heat during pressing to increase resist fluidity, ensuring accurate pattern transfer without thermal expansion.
The conductive heating film enhances resist fluidity, preventing voids and thermal expansion, enabling precise pattern transfer and reducing manufacturing time.
Smart Images

Figure 2024154653000001_ABST
Abstract
Description
[Technical field]
[0001] The present disclosure relates to an imprint apparatus and an imprint method. [Background technology]
[0002] 2. Description of the Related Art In the manufacture of semiconductor devices and the like, known methods for forming protruding electrodes on the surface of a substrate include an exposure method, an imprint method, and the like.
[0003] In the exposure method, first, a resist is applied to the surface of the substrate, and then the resist is partially removed by exposure and development using a mask, forming a resist pattern and exposing a part of the base material. Next, the openings in the resist pattern are filled with metal, for example by electrolytic plating, to form protruding electrodes on the exposed substrate. After that, the resist pattern is removed.
[0004] In the imprint method, resist is first applied to the surface of a substrate, and an imprint mold with a concave-convex pattern is pressed against the resist. In this state, the resist is exposed through the imprint mold or heated to harden, forming a resist pattern. Next, metal is filled into the openings of the resist pattern to form protruding electrodes. The resist pattern is then removed.
[0005] The imprint method can reduce the number of steps significantly compared to the exposure method, as it can eliminate the development process, etc. In addition, since it is possible to create an imprint mold having a very fine concave-convex pattern using a semiconductor process, it is possible to form a fine resist pattern.
[0006] In the imprinting method, thermoplastic polymers such as polymethyl methacrylate (PMMA) have been used as the resist. For this reason, it is necessary to press the imprinting mold while heating the resist to a temperature at which it can be deformed. If the heating is insufficient, the fluidity of the resist decreases, and the convex pattern of the imprinting mold is not filled with resist, making it impossible to transfer the pattern accurately. On the other hand, if the heating is excessive, the imprinting mold and imprinting device will thermally expand, deteriorating the positioning accuracy of pattern formation.
[0007] In view of this, an imprint method capable of forming a resist pattern at room temperature has been proposed (Patent Document 1). In this method, a resist containing an organic solvent is used to increase the fluidity of the resist even at room temperature. [Prior art documents] [Patent documents]
[0008] [Patent Document 1] JP 2007-258669 A Summary of the Invention [Problem to be solved by the invention]
[0009] When using a resist containing an organic solvent, in the case of an imprint type and a resist pattern that are becoming finer, it is necessary to increase the ratio of the organic solvent in order to further improve the fluidity of the resist. However, if this is done, the organic solvent will volatilize during pressing, and voids will easily occur, particularly at the base of the convex pattern of the imprint type. As a result, it becomes difficult to transfer the pattern accurately.
[0010] The present disclosure provides an imprinting apparatus and an imprinting mold that are capable of transferring a pattern accurately even when using a resist made of a thermoplastic polymer or a resist with a low ratio of organic solvent. [Means for solving the problem]
[0011] The imprinting apparatus of the present disclosure includes a stage unit on which a substrate is placed, and a head unit that holds an imprinting mold. The imprinting mold has a base and a protruding pattern provided on the base. The imprinting mold is pressed against a resist provided on the substrate to transfer the pattern. A conductive heating film that generates heat when supplied with electricity is formed on a surface of the imprinting mold that contacts the resist.
[0012] The imprinting method of the present disclosure includes a step of pressing an imprint mold against a resist applied on a substrate by using the imprinting apparatus of the present disclosure, wherein the conductive heating film is caused to generate heat during pressing. Effect of the Invention
[0013] According to the imprinting apparatus of the present disclosure, by generating heat from the conductive heating film, the fluidity of the resist can be sufficiently increased, enabling accurate pattern transfer. [Brief description of the drawings]
[0014] [Figure 1] FIG. 1 is a schematic cross-sectional view showing an imprint apparatus according to a first embodiment of the present disclosure. [Diagram 2] FIG. 2 is a plan view of the imprint apparatus in FIG. 1 as viewed from the stage unit side. [Figure 3A] FIG. 3A is a diagram illustrating the imprint method according to the first embodiment of the present disclosure. [Figure 3B] FIG. 3B is a diagram illustrating the imprint method following FIG. 3A. [Figure 3C] FIG. 3C is a diagram illustrating the imprint method following FIG. 3B. [Figure 3D] FIG. 3D is a diagram illustrating the imprint method following FIG. 3C. [Figure 3E] FIG. 3E is a diagram illustrating the imprint method following FIG. 3D. [Figure 3F] FIG. 3F is a diagram illustrating the imprint method following FIG. 3E. [Figure 3G]FIG. 3G is a diagram illustrating the imprint method following FIG. 3F. [Figure 4] FIG. 4 is a schematic cross-sectional view showing an imprint apparatus according to the second embodiment of the present disclosure. [Figure 5A] FIG. 5A is a diagram illustrating an imprint method according to a second embodiment of the present disclosure. [Figure 5B] FIG. 5B is a diagram illustrating the imprint method following FIG. 5A. [Figure 5C] FIG. 5C is a diagram illustrating the imprint method following FIG. 5B. [Figure 5D] FIG. 5D is a diagram illustrating the imprint method following FIG. 5C. [Figure 5E] FIG. 5E is a diagram illustrating the imprint method following FIG. 5D. [Figure 6] FIG. 6 is a schematic cross-sectional view showing an imprint apparatus according to a third embodiment of the present disclosure. [Figure 7A] FIG. 7A is a diagram illustrating an imprint method according to a third embodiment of the present disclosure. [Figure 7B] FIG. 7B is a diagram illustrating the imprint method following FIG. 7A. [Figure 7C] FIG. 7C is a diagram illustrating the imprint method following FIG. 7B. [Figure 8] FIG. 8 is a schematic cross-sectional view showing an imprint apparatus according to another embodiment of the present disclosure. [Figure 9] FIG. 8 is a schematic plan view showing an imprint apparatus according to another embodiment of the present disclosure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0015] Hereinafter, an embodiment will be described with reference to the drawings. Note that the following description is merely an example and is not intended to be limiting. In addition, the present invention can be modified as appropriate within the scope of the present invention.
[0016] (First embodiment) --Imprint device-- FIG 1 is a cross-sectional view showing a schematic diagram of an imprint apparatus 10 according to a first embodiment of the present disclosure. The imprint apparatus 10 includes a stage unit 2 and a head unit 1. A substrate 22 (not shown in FIG 1) is placed on the stage unit 2. The head unit 1 includes an imprint mold 25. The imprint mold 25 includes a base unit 25b and a protruding pattern 25a provided on the base unit 25b. The imprint mold 25 is held by the head unit 1 with the protruding pattern 25a facing the stage unit 2 side.
[0017] The imprint mold 25 includes a conductive heating film 4 that generates heat when supplied with electricity. As will be described in detail later, when the imprint mold 25 is pressed against the resist, the conductive heating film 4 is heated, thereby softening the resist in the vicinity of the protruding patterns 25a of the imprint mold 25 and improving its fluidity. This allows the resist to be filled even at the base of the protruding patterns 25a, enabling the pattern to be transferred accurately.
[0018] It is preferable that the through wiring 3 is provided so as to penetrate the imprint mold 25 and be electrically connected to the conductive heating film 4. The through wiring 3 may further penetrate the head portion 1. Note that the through wiring 3 may be provided in each of the head portion 1 and the imprint mold 25, and the through wirings 3 may be connected to each other when the head portion 1 holds the imprint mold 25.
[0019] Here, if wiring for supplying electricity to the conductive heating film 4 is provided on the side surface of the head unit 1 or the surface in contact with the imprint mold 25, the flatness of the portion of the head unit 1 in contact with the imprint mold 25 may deteriorate. In addition, if a material of the wiring different from that of the head unit 1 comes into contact with the imprint mold 25, it is possible that variation will occur in the in-plane distribution of the load during pressing. Furthermore, if the wiring becomes too long, electrical noise may be generated, causing variation in the amount of heat generated. In order to avoid these, it is preferable to use the through wiring 3 that penetrates the imprint mold 25.
[0020] Next, a further description will be given of the configuration of the conductive heating film 4. As shown in Fig. 1, the conductive heating film 4 is provided on the base portions of the side surfaces of the protruding patterns 25a and on the surface of the base portion 25b of the imprint mold 25.
[0021] 2 is a schematic plan view of the imprint mold 25 of FIG 1, seen from the side of the protruding pattern 25a. Regarding the configurations of the protruding pattern 25a and the conductive heating film 4, the cross section taken along line II in FIG 2 corresponds to FIG 1.
[0022] As shown in FIG. 2, the convex pattern 25a is cylindrical and arranged on the base 25b. The conductive heating film 4 includes a base film 4a provided at least at the base of the side of the convex pattern 25a, a peripheral film 4b provided at the peripheral portion of the convex pattern 25a on the surface of the base 25b, and a connection film 4c connecting the peripheral films 4b. The connection film 4c connects the peripheral films 4b to each other, thereby forming a continuous electrical path. In the example of FIG. 2, the upper right and lower right convex patterns 25a are both ends, forming one meandering electrical path without branching. When the through wiring 3 is electrically connected to the convex patterns 25a at both ends, electricity can be supplied to the electrical path formed by the conductive heating film 4.
[0023] Such an electrical path may be a single path extending over the entire surface of the imprint mold 25. Alternatively, the entire surface of the imprint mold 25 may be divided into a plurality of regions, and an electrical path may be provided in each of the regions. When a plurality of electrical paths are formed, electrical connection is made from the through wiring 3 to each path so that electricity can be supplied to each path.
[0024] It is preferable that the width W1 of the connection film 4c is smaller than the width W2 of the peripheral film 4b. Since current has the property of flowing along the shortest path, the narrow width W1 of the connection film 4c improves the current density in the peripheral film 4b near the base of the protruding pattern 25a. As a result, the heat generation near the base of the protruding pattern 25a can be increased.
[0025] The imprint mold 25 is made of, for example, Si, Ni, glass, etc. The conductive heating film 4 is made of, for example, Ag, ITO (indium tin oxide), etc., and is formed on the surface of the imprint mold 25 by a sputtering method, a vapor deposition method, etc. The through wiring 3 is made of a good conductor such as copper, a copper alloy, or aluminum. The connection film 4c can be provided as a metal film such as Au, Cu, Al, Ag, etc., or may be made of the same material as the base film 4a and the peripheral film 4b. The head part 1 and the stage part 2 may be made of stainless steel, ceramic, etc.
[0026] --Imprint method-- Next, an imprint method using the imprint apparatus 10 will be described with reference to FIGS. 3A to 3G.
[0027] 3A, a resist 21 is formed on the surface of a substrate 22. For example, a liquid material is dropped onto the substrate 22 and formed into a film by using a spin coating method.
[0028] 3B, the resist 21 is heated to volatilize the solvent, thereby forming a film. Furthermore, if a thermosetting resist is used, the resist 21 is thermally cured and solidified.
[0029] 3C, the substrate 22 on which the resist 21 is provided is placed on the stage unit 2 of the imprint apparatus 10. The imprint mold 25 is held in the head unit 1, and a current is supplied to the conductive heating film 4 through the through wiring 3, causing the conductive heating film 4 to generate heat.
[0030] Next, as shown in FIG. 3D, the head unit 1 is lowered toward the stage unit 2 to press the imprint mold 25 against the resist 21.
[0031] At this time, the convex pattern 25a is heated in advance by heating the conductive heating film 4. Therefore, the resist 21 that comes into contact with the tip of the convex pattern 25a during pressing is also heated, improving the fluidity. As a result, when the imprint mold 25 is inserted into the resist 21, the convex pattern 25a is prevented from buckling. In addition, since it takes a certain amount of time for the conductive heating film 4 to generate heat, it is preferable to heat the conductive heating film 4 before pressing in order to shorten the time required for the manufacturing process. Furthermore, the conductive heating film 4 may be heated and kept on standby before the substrate 22 is placed. However, it is possible to use a method in which the conductive heating film 4 is heated after pressing is started.
[0032] The head unit 1 is lowered to press the imprint mold 25, whereby the concave-convex pattern of the convex pattern 25a is transferred to the resist 21, forming a resist pattern 21a. At this time, the conductive heating film 4 is heated, improving the fluidity of the resist 21, and the resist 21 is sufficiently filled in the vicinity of the base of the convex pattern 25a. As a result, the occurrence of voids is suppressed, and the pattern can be transferred accurately.
[0033] 3E, the head unit 1 is raised together with the imprint mold 25 to separate the imprint mold 25 from the resist pattern 21a. At this time, it is preferable to heat the conductive heating film 4. This improves the fluidity of the surface of the resist pattern 21a, thereby reducing the stress generated in the imprint mold 25 during the mold release, and thus preventing the imprint mold 25 from breaking.
[0034] The imprint method for forming the resist pattern 21a is now complete. After this, the resist pattern 21a may be exposed to light.
[0035] After the resist pattern 21a is formed, the protruding electrodes 24 are formed as shown in Figures 3F and 3G. For this purpose, the openings of the resist pattern 21a are filled with metal by, for example, electrolytic plating. Thereafter, the resist pattern 21a is removed by a process using a resist remover or the like, thereby forming the protruding electrodes 24 on the base material 22.
[0036] As described above, the imprinting apparatus 10 of this embodiment and the imprinting method using the same enable accurate pattern transfer by improving the fluidity of the resist 21 by generating heat from the conductive heating film 4. In particular, to address the difficulty of filling the resist 21 near the base of the protruding pattern 25a, the conductive heating film 4 is provided near the base.
[0037] Furthermore, if the resist 21 is heated in areas other than the vicinity of the base of the protruding pattern 25a, the fluidity of the entire resist pattern 21a is high even after the imprint mold 25 is released, and the pattern may collapse. This can also be suppressed by heating only the vicinity of the base of the protruding pattern 25a.
[0038] As shown in FIG. 2, on the surface of the base 25b of the imprint mold 25, the range (dimension) D1 where the conductive heating film 4 is provided around the protruding patterns 25a is preferably about 1 / 5 to 1 / 3 of the distance D2 between the protruding patterns 25a.
[0039] Also, with regard to the height direction of the protruding patterns 25a, since heating near the base is important, it is preferable to provide the conductive heating film 4 near the base. For example, it is preferable that the height of the base film 4a is 1 / 3 or less of the height of the protruding patterns 25a. However, it is also possible to provide the conductive heating film 4 over the entire height direction. In this case, the vicinity of the tip of the protruding patterns 25a is also heated, so that the resistance can be reduced when the protruding patterns 25a are inserted into the resist 21.
[0040] Moreover, according to the imprinting apparatus 10 of this embodiment, only the conductive heating film 4 is heated to press the imprinting mold 25 at room temperature and normal pressure. This suppresses thermal expansion of the head unit 1 and the stage unit 2, and as a result, suppresses deviation of the transfer position of the imprinting mold 25. Therefore, the resist pattern 21a can be formed in an accurate position.
[0041] Second embodiment The second embodiment will be described below, focusing mainly on the differences from the first embodiment, and the description of similar configurations (which are designated by the same reference numerals in the drawings) may be simplified.
[0042] --Imprint device-- 4 is a cross-sectional view showing a schematic diagram of an imprint apparatus 10a according to a second embodiment of the present disclosure. In addition to the configuration of the imprint apparatus 10 of the first embodiment, the imprint apparatus 10a includes an exposure mechanism 11 above the head unit 1. The head unit 1 and the imprint mold 25 are formed of a transparent rigid body such as glass or acrylic resin, and transmit the exposure light generated by the exposure mechanism 11. The conductive heating film 4 is also made of a material such as ITO that transmits the exposure light. The stage unit 2 and the through wiring 3 are the same as those in the first embodiment.
[0043] In this embodiment, a UV (ultraviolet) curable resist is used as the resist 21. The exposure mechanism 11 generates UV light for curing the UV curable resist. The UV light passes through the head unit 1 and the imprint mold 25, and is irradiated onto the resist 21 on the substrate 22. Therefore, the resist can be cured in a state where the imprint mold 25 is pressed against the resist.
[0044] The exposure mechanism 11 includes a light source that emits the necessary light (ultraviolet light). A UV light emitting diode or the like may be provided on the head unit 1 as the light source, or light may be guided from a light source provided elsewhere using an optical fiber or the like.
[0045] --Imprint method-- Next, an imprint method using the imprint apparatus 10a will be described with reference to FIGS. 5A to 5E.
[0046] 5A, a resist 21 is formed on the surface of a substrate 22. Here, a UV-curable resist is used, and is dropped onto the substrate 22 and spin-coated.
[0047] 5B, the substrate 22 on which the resist 21 is provided is placed on the stage unit 2 of the imprint apparatus 10. Electricity is supplied to the conductive heating film 4 of the imprint mold 25 held by the head unit 1 to generate heat.
[0048] 5C, the head unit 1 is lowered toward the stage unit 2 to press the imprint mold 25 against the resist 21. As a result, the concave-convex pattern of the convex pattern 25a is transferred to the resist 21, and a resist pattern 21b is formed.
[0049] In this way, the imprint mold 25 is pressed against the resist 21 before it is hardened by exposure, and the fluidity of the resist 21 is more efficiently improved by generating heat in the conductive heating film 4. As a result, the resist 21 is sufficiently filled up to the base of the protruding patterns 25a, and the occurrence of voids can be suppressed.
[0050] 5D, UV light 14 is applied using the exposure mechanism 11. The UV light passes through the head unit 1, the imprint mold 25, and the conductive heating film 4, which are made of a transparent material, and hardens the resist pattern 21b. Therefore, the resist pattern 21a, which is reliably filled up to the base of the protruding pattern 25a, is hardened, enabling accurate transfer.
[0051] Thereafter, as shown in FIG. 5E, the head unit 1 is raised, the imprint mold 25 is released from the resist pattern 21b, and the resist pattern 21a is completed on the substrate 22.
[0052] Here, if the resist pattern 21b is released after being hardened by exposure, the protruding pattern 25a and the resist pattern 21b may adhere to each other, causing the base of the protruding pattern 25a to break. In response to this, the conductive heating film 4 is heated to soften the surface of the resist pattern 21b near the base of the protruding pattern 25a, which is most likely to adhere. By releasing the resist pattern 21b in this state, adhesion and breakage of the protruding pattern 25a can be suppressed.
[0053] After that, the resist pattern 21b may be cured by heating.
[0054] (Third embodiment) The third embodiment will be described below, focusing mainly on the differences from the first embodiment, and the description of similar configurations (the same reference numerals are used in the drawings) may be simplified.
[0055] --Imprint device-- 6 is a cross-sectional view showing a schematic diagram of an imprint apparatus 10b according to a third embodiment of the present disclosure. In addition to the configuration of the imprint apparatus 10 of the first embodiment, the imprint apparatus 10a further includes a head temperature adjustment mechanism 12 that heats or cools the head unit 1, and a stage temperature adjustment mechanism 13 that heats or cools the stage unit 2.
[0056] Use of such an imprint apparatus 10b makes it possible to suppress buckling of the convex pattern 25a, collapse of the resist pattern, and deviation of the transfer position of the pattern, as described below.
[0057] --Imprint method-- Next, an imprint method using the imprint apparatus 10b will be described with reference to FIGS. 7A to 7C.
[0058] First, in a process similar to that shown in FIGS. 3A and 3B in the first embodiment, a resist 21 made of a thermosetting resin is applied onto a substrate 22 and thermally cured to form a film.
[0059] 7A, the substrate 22 on which the resist 21 is provided is placed on the stage unit 2 of the imprint apparatus 10. In addition, the resist 21 is heated by the stage unit temperature adjustment mechanism 13 to improve the fluidity of the resist 21.
[0060] In addition, the conductive heating film 4 of the imprint mold 25 held by the head unit 1 is heated. This is for the purpose of increasing the fluidity of the resist 21, as in the first and second embodiments, but at this time, there is a risk that the entire head unit 1 will thermally expand and the positional accuracy of the pattern transfer will decrease. To address this, the head unit 1 is cooled by the head temperature adjustment mechanism 12. This makes it possible to prevent thermal expansion of the entire head unit 1 and also to prevent a decrease in positional accuracy.
[0061] On the other hand, when a material with a small thermal expansion coefficient such as ceramic is used for the head unit 1, the pattern transfer position accuracy is unlikely to decrease due to thermal expansion. In this case, the head unit 1 can be heated by the head temperature adjustment mechanism 12 to help improve the fluidity of the resist 21 by the heat generated by the conductive heating film 4. Therefore, the head unit 1 is heated or cooled according to the purpose.
[0062] 7B, the head unit 1 is lowered toward the stage unit 2, and the imprint mold 25 is pressed against the resist 21. As a result, the concave-convex pattern of the convex pattern 25a is transferred to the resist 21, and a resist pattern 21c is formed. At this time, the fluidity of the resist 21 can be improved by the heating by the stage unit temperature adjustment mechanism 13 in addition to the heat generated by the conductive heating film 4, and the pattern can be accurately transferred.
[0063] Thereafter, as shown in FIG. 7C, the head unit 1 is raised, the imprint mold 25 is released from the resist pattern 21c, and the resist pattern 21c is completed on the substrate 22.
[0064] At this time, it is preferable to cool the stage part temperature adjustment mechanism 13. This reduces the fluidity of the resist pattern 21c, and prevents the resist pattern 21c from losing its shape after demolding.
[0065] In addition, it is preferable that the head temperature adjustment mechanism 12 is heated. This helps improve the fluidity of the resist pattern 21c due to the heat generated by the conductive heating film 4, and prevents the protruding pattern 25a from breaking during demolding. Even if the head part 1 is heated during or before demolding, the position is already regulated by the resist pattern 21c, so that the transfer position of the pattern is unlikely to shift. Therefore, heating the head part 1 after pressing it is unlikely to cause any problems.
[0066] In order to prevent both the breakage of the protruding pattern 25a and the deformation of the resist pattern 21c during demolding, it is preferable to control the temperature of the resist pattern 21c so that the portion near the protruding pattern 25a is higher than the glass transition temperature and the other portion is lower than the glass transition temperature. This can be achieved by using the head temperature adjustment mechanism 12, the stage temperature adjustment mechanism 13, and the conductive heating film 4.
[0067] In the above, both the head temperature adjustment mechanism 12 and the stage temperature adjustment mechanism 13 are provided, and heating and cooling for each have been described. However, it is also possible to provide only one of the head temperature adjustment mechanism 12 and the stage temperature adjustment mechanism 13, or to perform only one of heating and cooling. By providing mechanisms as needed, the cost of the imprint apparatus can be reduced.
[0068] (Other embodiments) Next, as other embodiments, examples of other shapes of the convex pattern 25a of the imprint mold 25 and the resist pattern 21d formed thereby will be described.
[0069] Fig. 8 is a cross-sectional view showing a schematic diagram of an imprinting apparatus 10c. The imprinting apparatus 10c has a different shape of the protruding patterns 25a from the imprinting apparatus 10 of the first embodiment. In the imprinting apparatus 10 of Figs. 1 and 2, the protruding patterns 25a are cylindrical and extend from the base with the same shape and size. In contrast, in the imprinting apparatus 10c of Fig. 8, the protruding patterns 25a have a pointed shape that tapers from the base side toward the tip side, for example, a cone shape.
[0070] In the imprint apparatus 10 of the first embodiment, the protruding pattern 25a has a circular shape in a plan view seen from the stage unit 2 side, as shown in Fig. 2. However, this is not limited to this. Fig. 9 shows an example of another shape of the protruding pattern 25a, which is a rectangular shape extending to a certain length.
[0071] In these cases as well, a conductive heating film 4 is provided, which includes a base film 4a of the rectangular convex pattern 25a, a peripheral film 4b of the convex pattern 25a on the surface of the base 25b, and a connecting film 4c that connects the peripheral films 4b together.
[0072] In this way, even if the convex pattern 25a has a shape different from that shown in Figures 1 and 2, by forming a conductive heating film 4 including a base film 4a, a peripheral film 4b and a connection film 4c, the same effects as those described above can be obtained.
[0073] The convex pattern 25a may be pointed as shown in Fig. 8 and rectangular in plan view as shown in Fig. 9. In this case, the convex pattern 25a has a shape in which the side of a triangular prism is connected to the base 25b. The convex pattern 25a may have various shapes including a quadrangular prism and a quadrangular pyramid, and in any case, the effect of the present disclosure can be obtained by providing the conductive heating film 4.
[0074] The above-described embodiments may be modified in form and detail without departing from the spirit of the claims. Furthermore, the contents of each embodiment may be appropriately combined and substituted as long as the functions of the subject matter of the present disclosure are not impaired. [Industrial Applicability]
[0075] INDUSTRIAL APPLICABILITY The technology disclosed herein is useful as an imprint apparatus and an imprint method since it is possible to accurately transfer a pattern to a resist. [Explanation of symbols]
[0076] 1 Head section 2. Stage section 3 Through Wiring 4. Conductive heating film 4a Base membrane 4b Peripheral membrane 4c Connection membrane 10, 10a to 10c Imprint device 11 Exposure mechanism 12 Head temperature control mechanism 13 Stage temperature control mechanism 14 UV light 21 Resist 21a~21d Resist pattern 22 Base material 24 Protruding electrode 25 Imprint type 25a Convex pattern 25b base
Claims
1. A stage portion on which a substrate is placed; a head portion for holding an imprint mold, the imprint mold has a base and a protruding pattern provided on the base, an imprinting apparatus that transfers a pattern by pressing the imprinting mold against a resist provided on the base material, An imprinting apparatus comprising: a conductive heating film that generates heat when supplied with electricity, the conductive heating film being formed on a surface of the imprint mold that contacts the resist.
2. In claim 1, the conductive heating film includes a base film provided at least at the base of the side surface of the protruding pattern, a peripheral film provided at the peripheral portion of the protruding pattern on the surface of the base, and a connection film connecting the peripheral films together; An imprinting apparatus, characterized in that at least one electrical path is formed on the surface of the base by the connection portion film and the peripheral portion film.
3. In claim 2, An imprinting apparatus, comprising: a connecting portion film of the conductive heating film, the connecting portion film having a width smaller than a width of the peripheral portion film of the conductive heating film.
4. In claim 1 or 2, An imprinting apparatus comprising: a through wiring that passes through the head portion and is electrically connected to the conductive heating film.
5. In claim 1 or 2, The head unit is provided with an exposure mechanism, An imprint apparatus, characterized in that the head unit, the imprint mold, and the conductive heating film transmit light emitted by the exposure mechanism.
6. In claim 1 or 2, An imprint apparatus comprising: at least one of a head temperature adjustment mechanism that adjusts a temperature of the head unit; and a stage temperature adjustment mechanism that adjusts a temperature of the stage unit.
7. 2. An imprint method using the imprint apparatus of claim 1, pressing the imprint mold against a resist applied on the base material; The imprinting method, in which, in the step, the conductive heating film is caused to generate heat when the pressing is performed.
8. 6. An imprint method using the imprint apparatus of claim 5, the resist is a resist that is hardened by exposure to light, pressing the imprint mold against a resist applied on the base material; The imprint method, in which, in this process, after the conductive heating film is heated, the resist is hardened by the exposure mechanism.
9. 7. An imprint method using the imprint apparatus of claim 6, the resist is a resist made of a thermoplastic polymer, pressing the imprint mold against a resist applied on the base material; The imprinting method is characterized in that, in this process, at least one of the head portion and the stage portion is heated before the pressing, and the conductive heating film is caused to generate heat when the pressing is performed.
10. In claim 9, an imprinting method comprising: after the step of pressing the imprint mold, releasing the imprint mold while controlling a temperature of the resist other than the vicinity of the convex pattern to a glass transition temperature or lower using at least one of the head temperature adjustment mechanism and the stage temperature adjustment mechanism.
Citation Information
Patent Citations
Imprint lithography method and imprint lithography apparatus
JP2007258669A