Pyrolytic boron nitride-containing substrate, and insulation substrate of semiconductor device

The pyrolytic boron nitride-containing substrate with alternating pyrolytic boron nitride and carbon layers addresses the challenge of high insulation and heat dissipation in power semiconductor devices, providing enhanced performance for high-voltage applications.

JP2024154710AActive Publication Date: 2024-10-31SHIN ETSU CHEMICAL CO LTD

Patent Information

Application Number
JP2023068688
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-19
Publication Date
2024-10-31
Estimated Expiration
2043-04-19

AI Technical Summary

Technical Problem

Existing insulating substrates for power semiconductor devices face challenges in maintaining high insulation and heat dissipation properties, particularly at high voltages, with common materials exhibiting anisotropy and reduced thermal conductivity.

Method used

A pyrolytic boron nitride-containing substrate is developed with alternating layers of pyrolytic boron nitride and pyrolytic carbon, leveraging the anisotropy of pyrolytic boron nitride for improved insulation in the vertical direction and incorporating pyrolytic carbon layers to enhance thermal conductivity and withstand voltage.

Benefits of technology

The substrate achieves a thin insulating layer with excellent insulation properties and improved thermal conductivity, suitable for high-voltage applications, while minimizing layer separation and maintaining structural integrity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024154710000001_ABST
    Figure 2024154710000001_ABST
Patent Text Reader

Abstract

To provide a pyrolytic boron nitride-containing substrate for a power module that achieves a thinner insulator layer and excellent insulation properties.SOLUTION: A pyrolytic boron nitride-containing substrate is an insulation substrate used as a heat radiation material of a semiconductor device and is mainly composed of pyrolytic boron nitride. It is preferable that the inside of the pyrolytic boron nitride-containing substrate includes pyrolytic carbon layers in a range of one layer or more to 10 layers or less. It is preferable that the pyrolytic carbon layers are mainly composed of carbon and contain boron in a concentration ranging from 0.1% or more to 45% or less by weight. It is preferable that the thickness of each of the pyrolytic carbon layers is 0.1 μm or more and 100 μm or less.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to pyrolytic boron nitride-containing substrates for use as heat dissipation materials in semiconductor devices. [Background technology]

[0002] Power conversion devices using switching power semiconductor elements have high conversion efficiency and are widely used in consumer, automotive, railway, and substation equipment. Among them, power semiconductor elements made of SiC, GaN, or Ga2O3 generate heat when current is passed through them, so high heat dissipation is required. Usually, a metal heat dissipation structure with fins is used for heat dissipation, and the structure is grounded to the ground (GND) to stabilize the potential and prevent electric shock. For this reason, the insulating material placed between the power semiconductor element and the heat dissipation structure must have excellent thermal conductivity. Typical insulating layers include ceramic substrates made of AlN, Al2O3, Si3N4, SiC, etc., and resin materials.

[0003] However, with the recent spread of electric vehicles, the use of on-board power modules at high voltages of over 800 V is also increasing. When the voltage to be converted is high, it becomes necessary to make the insulating material thicker in order to improve insulation, which deteriorates heat dissipation.

[0004] Known methods for improving heat dissipation include, for example, providing an intermediate conductor in an insulating layer to share the voltage, as shown in Patent Document 1, and using an insulating substrate made of Si3N4 particles with high thermal conductivity, as shown in Patent Document 2.

[0005] Another material that can be used as an insulating substrate is hexagonal boron nitride (h-BN). Hexagonal boron nitride has a layered structure like graphite, and has anisotropy in heat dissipation (thermal conductivity) and insulation (electrical conductivity). For this reason, when using hexagonal boron nitride for an insulating substrate, as shown in Patent Document 3, the anisotropy is suppressed by solidifying the particulate sintered body with a resin or the like. [Prior art documents] [Patent documents]

[0006] [Patent Document 1] Patent No. 6200871 [Patent Document 2] Patent No. 5773330 [Patent Document 3] International Publication No. 2022 / 149553 Summary of the Invention [Problem to be solved by the invention]

[0007] As described above, various insulating substrates have been proposed as heat dissipation materials for power semiconductor elements. However, in recent years, applications of high voltage have been increasing, and insulating substrates with higher insulation and heat dissipation properties are required.

[0008] In view of the above circumstances, the technical problem to be solved by the present invention, that is, the object of the present invention, is to provide a pyrolytic boron nitride-containing substrate for a power module which has a thin insulating layer and excellent insulating properties. [Means for solving the problem]

[0009] In order to achieve the above object, the present inventors have conducted extensive research, and the present invention proposes the following means. That is, a substrate containing pyrolytic boron nitride (PBN) in which hexagonal boron nitride is laminated is produced by a thermal CVD reaction. A pyrolytic boron nitride-containing substrate has anisotropy in that the insulating property in the height direction (c direction) of the substrate is higher than that in the planar direction (ab direction), but the thermal conductivity is low. Therefore, in the present invention, the substrate itself is processed to be thin, while taking advantage of the anisotropy of the high insulating property in the height direction (c direction) of the substrate, thereby improving the drawback of the low thermal conductivity in the height direction (c direction) of the substrate. Furthermore, a layer of pyrolytic carbon (PG) is introduced between the layers of PBN, thereby achieving further improvement in insulating property. Specifically, the present invention has the following characteristics.

[0010] A pyrolytic boron nitride-containing substrate according to one embodiment of the present invention is an insulating substrate used as a heat dissipation material for semiconductor devices, characterized in that the main component of this insulating substrate is pyrolytic boron nitride.

[0011] In the present invention, the pyrolytic boron nitride-containing substrate may include one or more and ten or less pyrolytic carbon layers. The pyrolytic carbon layer may be mainly composed of carbon and may include boron at a weight ratio of 0.1% to 45%. The thickness of the pyrolytic carbon layer may be 0.1 μm to 100 μm.

[0012] In the present invention, the thickness of the pyrolytic boron nitride-containing substrate is preferably 0.01 mm to 4 mm, and the arithmetic mean roughness Ra of the surface of the pyrolytic boron nitride-containing substrate is preferably 10 μm or less.

[0013] In the present invention, the semiconductor device may be a SiC, GaN, or Ga2O3 power device.

[0014] An insulating substrate for a semiconductor device according to one embodiment of the present invention is characterized in that it has a structure in which any of the above-mentioned pyrolytic boron nitride-containing substrates is embedded in an insulating resin. Effect of the Invention

[0015] According to the pyrolytic boron nitride-containing substrate of the present invention, it is possible to provide a pyrolytic boron nitride-containing substrate for a power module which has a thin insulating layer and excellent insulating properties. [Brief description of the drawings]

[0016] [Figure 1] FIG. 1 is a schematic diagram illustrating a pyrolytic boron nitride-containing substrate according to one embodiment of the present invention. [Diagram 2] FIG. 2 illustrates the flexibility of a pyrolytic boron nitride-containing substrate according to one embodiment of the present invention. [Diagram 3] FIG. 1 is a schematic cross-sectional view of a power module in which a pyrolytic boron nitride-containing substrate according to one embodiment of the present invention is covered with an insulating resin to form an insulating layer. [Figure 4] FIG. 1 is a schematic cross-sectional view of a power module in which only a pyrolytic boron nitride-containing substrate according to one embodiment of the present invention is used as an insulating layer. [Diagram 5] This is a schematic diagram of an experimental system in which a DC voltage is applied to an insulating layer portion having one intermediate conductor. [Figure 6] FIG. 1 is a schematic diagram of an experimental system in which an AC voltage is applied to an insulating layer portion having one intermediate conductor. [Figure 7] FIG. 2 is a schematic diagram showing the configuration of a test system when performing a dielectric breakdown test. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0017] Hereinafter, an embodiment of the present invention will be described with reference to the drawings.

[0018] 1 is a schematic diagram showing a pyrolytic boron nitride (PBN)-containing substrate 10 according to one embodiment of the present invention. The pyrolytic boron nitride-containing substrate 10 is an insulating substrate used as a heat dissipation material for semiconductor devices. The main component of the pyrolytic boron nitride-containing substrate 10 is pyrolytic boron nitride.

[0019] The pyrolytic boron nitride-containing substrate 10 comprises at least one pyrolytic boron nitride layer 11 (hereinafter referred to as PBN layer 11) and zero or more pyrolytic carbon layers 12 (hereinafter referred to as PG layers 12). In the example shown in FIG. 1, the pyrolytic boron nitride-containing substrate 10 has three PBN layers 11 and two PG layers 12.

[0020] The PBN layer 11 is formed of pyrolytic boron nitride (PBN). PBN is boron nitride (BN) produced by chemical vapor deposition (CVD) and has a layered crystal structure like graphite. Therefore, PBN has characteristics such as excellent insulation (breakdown voltage > 400 AC kV / mm), high thermal conductivity (50-100 W / m·K (ab direction), 1.8 W / m·K (c direction)), high heat resistance, thermal shock resistance, chemical inertness, and high bending strength (150-230 MPa). Compared with ceramics such as AlN, Al2O3, and SiC, PBN has the characteristic of being highly flexible and easy to form into a thin film. FIG. 2 is a diagram showing the flexibility of the pyrolytic boron nitride-containing substrate 10, showing the state in which the pyrolytic boron nitride-containing substrate 10 is bent by hand. The thickness of the PBN that becomes the PBN layer 11 can be controlled by adjusting the supply amount of the raw material gas, so that it is possible to form the PBN into a thin film as necessary.

[0021] The PG layer 12 is formed of pyrolytic carbon (Pyrolytic Graphite: PG) or boron-doped pyrolytic carbon (Boron-doped Pyrolytic Graphite: BPG). In this specification, the PG layer 12 is a general term for both PG and BPG. The PG and BPG layers constituting the PG layer 12 are conductive. Pyrolytic carbon (Pyrolytic Graphite: PG) and boron-doped pyrolytic carbon (Boron-doped Pyrolytic Graphite: BPG) can be formed by changing the film formation conditions (type of supply gas, etc.) during the vapor phase growth of PBN. For example, as shown in FIG. 1, the PG layer 12 can be laminated between the PBN layers 11. When the PG layer 12 serving as an intermediate conductor is introduced between the PBN layers 11 as in the structure shown in FIG. 1, the DC and AC voltages are shared, making it possible to thin the PBN layer 11 and improve its withstand voltage characteristics.

[0022] The number of PG layers 12 included in the pyrolytic boron nitride-containing substrate 10 is preferably in the range of 10 layers or less. In this way, the PBN layer 11 can be thinned while improving the voltage resistance characteristics. Even if the pyrolytic boron nitride-containing substrate 10 does not include the pyrolytic carbon PG layer 12, it is possible to use a pyrolytic boron nitride-containing substrate as the PBN layer 11. However, as the number of conductive layers increases, the voltage distribution rate when an AC voltage is applied decreases, so the pyrolytic boron nitride-containing substrate 10 preferably has one or more PG layers 12. On the other hand, if 10 or more PG layers 12 are laminated, the influence of the difference in thermal expansion coefficient with the PBN layer 11 becomes large, which causes layer separation. Therefore, the number of PG layers 12 included in the pyrolytic boron nitride-containing substrate 10 is preferably in the range of 0 layers or more and 10 layers or less, more preferably in the range of 1 layer or more and 5 layers or less, and even more preferably in the range of 1 layer or more and 3 layers or less.

[0023] The PG layer 12 is a pyrolytic carbon layer whose main component is carbon. The PG layer 12 does not need to contain boron, but it is preferable that it contains boron in a weight ratio range of 0.1% to 45%. The thermal expansion coefficient of pyrolytic carbon varies depending on the boron concentration. Pyrolytic carbon that is not doped with boron has a thermal expansion coefficient of approximately 1.9×10 -6 / ℃, and the thermal expansion coefficient of pyrolytic boron nitride is 2.8~3.5×10 -6 / °C (in the planar direction). In contrast, when boron is doped in the above weight ratio range, the thermal expansion coefficient of the pyrolytic carbon constituting the PG layer 12 is increased to about 4.0×10 -6 / ° C., thereby reducing the difference in thermal expansion coefficient between the PG layer 12 and the pyrolytic boron nitride constituting the PBN layer 11. This allows up to about 10 PG layers 12 to be laminated.

[0024] The thickness of the pyrolytic carbon constituting each layer of the PG layer 12 is preferably 0.1 μm or more and 100 μm or less. If the thickness is 0.1 mm or less, the resistivity of the pyrolytic carbon becomes large, and it may not be possible to fully exhibit the performance as an intermediate conductor. On the other hand, if the thickness is 100 μm or more, the strength of the pyrolytic boron nitride-containing substrate 10 may decrease or peel off. For the above reasons, the thickness of each layer of the PG layer 12 is preferably in the range of 0.1 μm or more and 100 μm or less, more preferably in the range of 0.5 μm or more and 75 μm or less, and even more preferably in the range of 1 μm or more and 50 μm or less.

[0025] The thickness of the pyrolytic boron nitride-containing substrate 10 is preferably in the range of 0.01 mm or more and 4 mm or less. If the thickness is 0.01 mm or less, the strength of pyrolytic boron nitride decreases and it becomes easy to peel off due to impact, etc. On the other hand, if the thickness is 4 mm or more, the thermal conductivity of pyrolytic boron nitride in the vertical direction (c-axis direction) is low at 1.8 W / m·K, so that when used as an insulating material for a power module, the heat dissipation is poor. For the above reasons, the thickness of the pyrolytic boron nitride-containing substrate is preferably in the range of 0.01 mm or more and 4 mm or less, more preferably in the range of 0.02 mm or more and 1 mm or less, and even more preferably in the range of 0.03 mm or more and 0.6 mm or less.

[0026] In order to improve the bondability with Al-Si or Al-Ge brazing materials and Ag-containing pastes used when bonding the pyrolytic boron nitride-containing substrate 10 to components such as conductive layers and heat sinks, it is desirable for the arithmetic mean roughness Ra of the surface of the pyrolytic boron nitride-containing substrate 10 to be 10 μm or less. More preferably, Ra should be 2 μm or less, and even more preferably, 0.5 μm or less.

[0027] The pyrolytic boron nitride-containing substrate 10 according to this embodiment can be used in power modules (20, 30) as shown in Fig. 3 and Fig. 4. In Fig. 3, the pyrolytic boron nitride-containing substrate 10 is covered with insulating resin 24, which serves as an insulating layer disposed between a power semiconductor element and a heat dissipation structure. That is, the pyrolytic boron nitride-containing substrate 10 is covered with insulating resin 24, a metal plate 23 for a circuit layer that serves as a circuit layer is laminated on the front side, and a metal plate 25 for a heat conduction layer that serves as a heat conduction layer for heat dissipation is laminated on the back side. For example, the metal plate 23 for a circuit layer and the metal plate 25 for a heat conduction layer are formed of pure Al.

[0028] In Fig. 4, only the pyrolytic boron nitride-containing substrate 10 is used as an insulating layer disposed between the power semiconductor element and the heat dissipation structure. That is, the pyrolytic boron nitride-containing substrate 10 is covered with brazing material layers 36 and 37, a circuit layer metal plate 23 is laminated on the front side to become a circuit layer, and a heat conduction layer metal plate 25 is laminated on the back side to become a heat conduction layer for heat dissipation. For example, the circuit layer metal plate 23 and the heat conduction layer metal plate 25 are formed of pure Al. The brazing material layers 36 and 37 are formed of, for example, an Al-Si (silicon)-based (e.g., Al: 93 wt%, Si: 7 wt%, thickness 10 μm to 15 μm) or an Al-Ge (germanium)-based brazing material.

[0029] 3 and 4, an electronic component 21 is fixed to the upper surface of the circuit layer metal plate 23 by a solder layer 22. Here, the electronic component 21 may be, for example, a semiconductor chip, and an example of the semiconductor chip is a power device such as an IGBT (Insulated Gate Bipolar Transistor).

[0030] 3 and 4, the heat conduction layer metal plate 25 is made of a metal having high thermal conductivity such as Al (aluminum), and is bonded and fixed to the pyrolytic boron nitride-containing substrate 10 by brazing layers (36, 37). Here, the heat conduction layer metal plate 25 has a thickness of, for example, 0.6 mm. The heat conduction layer metal plate 25 may be formed into a shape having a large surface area, such as a heat dissipation fin, for high heat dissipation properties, as necessary.

[0031] <Principle of voltage sharing by intermediate conductor> 5 and 6 are schematic diagrams of an experimental system in which DC and AC voltages are applied to an insulating layer portion having one intermediate conductor. FIG. 5 shows a voltage sharing model 50 in an insulating layer of a power module to which a DC voltage is applied. FIG. 6 shows a voltage sharing model 60 in an insulating layer of a power module to which an AC voltage is applied. The electrode 52 in FIG. 5 and FIG. 6 corresponds to the metal plate 23 for the circuit layer in FIG. 3, the intermediate conductor 54 in FIG. 5 and FIG. 6 corresponds to the PG layer 12 in the pyrolytic boron nitride-containing substrate 10, the insulating layers 53 and 55 correspond to the PBN layer 11 in the pyrolytic boron nitride-containing substrate 10, and the electrode 56 in FIG. 5 and FIG. 6 corresponds to the metal plate 25 for the heat conduction layer in FIG. 3. Reference numeral 51 in FIG. 5 denotes a DC power source 51, and reference numeral 61 in FIG. 6 denotes an AC power source 61.

[0032] Intermediate conductor 54 is disposed between electrode 52 and electrode 56. Insulating layer 53 is disposed between electrode 52 and intermediate conductor 54. Insulating layer 55 is disposed between electrode 56 and intermediate conductor 54. If the voltage between intermediate conductor 54 and electrode 52 is V1 and the voltage between electrode 52 and electrode 56 is V, the voltage sharing of the capacitance circuit when an AC voltage is applied can be calculated by the following formula. Pyrolytic carbon layer V1=V C1 / (C1+C2)...(1) Here, C1 represents the capacitance between the electrode 52 and the intermediate conductor 54, and C2 represents the capacitance between the intermediate conductor 54 and the electrode 56.

[0033] Here, by adjusting the structure of the voltage sharing model and the material of the insulating layer, it is possible to make C1 = C2. In this case, from formula (1), the voltage sharing rate obtained by dividing V1 by V is 50%. In this model, C1 = C2. V1 / V=50% (2) EXAMPLES

[0034] Examples and comparative examples are shown below.

[0035] <Preparation of pyrolytic boron nitride-containing substrate 10> (Examples 1 to 6) First, ammonia (NH3) and boron trichloride (BCl3) were reacted at 1900°C under a pressure of 100 Torr by a CVD method to produce a pyrolytic boron nitride-containing substrate 10 having the thickness shown in Table 1. This was then cut into a size of 50 mm x 50 mm.

[0036] (Surface roughness) The arithmetic mean roughness Ra of the surface of the cut pyrolytic boron nitride-containing substrate 10 was measured using a Surftest SJ-210 manufactured by Mitutoyo Corp. The results are shown in Table 1.

[0037] [Table 1]

[0038] (Dielectric breakdown testing of pyrolytic boron nitride-containing substrates) The dielectric breakdown test was performed using a method based on JIS C 2110-1 "Solid electrical insulating materials - Test method for dielectric breakdown strength - Part 1: Test by application of commercial frequency AC voltage". Specifically, as shown in FIG. 7, dielectric breakdown test equipment 40 is placed in oil tank 41 with insulating oil 42, a test piece of pyrolytic boron nitride-containing substrate 10 is placed therein, and the approximate center of the test piece is sandwiched between upper electrode 44 and lower electrode 45, and lead wires are connected to the electrodes. Thereafter, the value of power supply voltage 43 is increased at a constant rate, and the dielectric breakdown voltage is measured. The dielectric breakdown strength is calculated by dividing the obtained dielectric breakdown voltage by the thickness of the sample.

[0039] The conditions for carrying out the above dielectric breakdown test are as follows: Sample size: 50mm x 50mm x 0.1~10mm Electrode shape: Upper electrode: Φ25.4mm×20mm / edge 1.6mmR Lower electrode: Φ25.4mm×10mm / edge 1.6mmR Voltage rise speed: 0.5 kV / sec (applying DC and AC, frequency of AC is 50 Hz) Pretreatment: C-90h / 22±1℃ / 60±5% Measurement atmosphere: 25°C, in silicone oil (JIS C2320 insulating oil compliant) Number of measurements: n=l

[0040] (Examples 7 to 10) A pyrolytic boron nitride (PBN) layer 11 was formed in the same manner as in Example 1. The temperature was lowered to 1500°C, and methane gas (CH4) and BCl3 were changed and pyrolyzed under the condition of 50 Torr to form a pyrolytic carbon (PG) layer 12. Then, ammonia (NH3) and boron trichloride (BCl3) were reacted again by the CVD method at 1900°C under a pressure of 100 Torr to form a PBC layer 11, and a pyrolytic boron nitride-containing substrate 10 with the thickness shown in Table 1 was produced. This was cut into a size of 50 mm x 50 mm. Then, the dielectric breakdown voltage was measured in the same manner as in Example 1. The results are shown in Table 1.

[0041] (Examples 11 and 12) By repeating the method of laminating the PBN layer 11 and the PG layer 12 in Examples 7 to 10, a pyrolytic boron nitride-containing substrate 10 having a plurality of PBN layers 11 and PG layers 12 and having a thickness shown in Table 1 was produced. This was cut into a size of 50 mm x 50 mm. Then, measurements were made in the same manner as in Example 1. The results are shown in Table 1.

[0042] A pyrolytic boron nitride-containing substrate 10 having a PG layer 12 was produced in the same manner as in Example 7. The surface of this pyrolytic boron nitride-containing substrate 10 was roughened by sandblasting, and then cut into a size of 50 mm x 50 mm. Then, measurements were performed in the same manner as in Example 1. The results are shown in Table 1.

[0043] Examples 1 to 6 show that if the thickness of the pyrolytic boron nitride containing substrate 10 is in the range of 0.01 mm to 4.0 mm, the thickness can be reduced while maintaining the insulating performance.

[0044] From Examples 7 to 9, it is possible to fabricate a pyrolytic boron nitride-containing substrate 10 having sufficient insulating performance by setting the boron doping amount within the range of weight ratio of 0% to 45%.

[0045] From Example 10, it is clear that if the number of pyrolytic carbon layers is within the range of 0 to 10, a pyrolytic boron nitride-containing substrate having sufficient insulating performance can be fabricated.

[0046] From Examples 11 and 12, it is clear that if the arithmetic mean roughness Ra of the pyrolytic boron nitride containing substrate is in the range of 10 μm or less, a pyrolytic boron nitride containing substrate having sufficient insulating performance can be produced. [Explanation of symbols]

[0047] 10 Pyrolytic boron nitride-containing substrates 11 Pyrolytic boron nitride (PBN) layer 12 Pyrolytic carbon (PG) layer 20, 30 Power Module 21 Electronic Components 22 Solder layer 23 Metal plate for circuit layer 24 Insulating resin 25 Metal plate for thermal conductive layer 36, 37 Brazing layer 40 Dielectric breakdown test equipment 41 Oil tank 42 Insulating oil 43 Power supply voltage 44 Upper electrode 45 Lower electrode 50 Voltage sharing model when DC is applied 51 DC power supply 52, 56 electrodes 53, 55 Insulating layer 54 Intermediate Conductor 60 Voltage sharing model when AC is applied 61 AC power supply

Claims

1. A pyrolytic boron nitride-containing substrate, which is an insulating substrate used as a heat dissipation material for semiconductor devices, and is characterized in that its main component is pyrolytic boron nitride.

2. 2. The pyrolytic boron nitride-containing substrate according to claim 1, further comprising one or more and ten or less pyrolytic carbon layers therein.

3. 3. The pyrolytic boron nitride-containing substrate according to claim 2, wherein the pyrolytic carbon layer is mainly composed of carbon and contains boron at a concentration ranging from 0.1% to 45% by weight.

4. 4. The pyrolytic boron nitride-containing substrate according to claim 3, wherein the thickness of each layer of said pyrolytic carbon layer is 0.1 [mu]m or more and 100 [mu]m or less.

5. 5. The pyrolytic boron nitride-containing substrate according to claim 1, wherein the pyrolytic boron nitride-containing substrate has a thickness of 0.01 mm or more and 4 mm or less.

6. 5. The pyrolytic boron nitride-containing substrate according to claim 1, wherein the arithmetic mean roughness Ra of the surface of the pyrolytic boron nitride-containing substrate is 10 μm or less.

7. The semiconductor device is made of SiC, GaN, or Ga. 2 O 3 5. The pyrolytic boron nitride-containing substrate according to claim 1, which is a power device.

8. 5. An insulating substrate for a semiconductor device, comprising the pyrolytic boron nitride-containing substrate according to claim 1 embedded in an insulating resin.

Citation Information

Patent Citations

  • Heater and preparation method thereof

    CN110662314A

  • Production of thermally decomposed boron nitride formed article

    JP1992059661A

  • Pyrolytic boron nitride-pyrolytic carbon laminated material

    JP1992170379A

  • Multilayer formed article coated with heat-decomposed boron nitride and its production

    JP1995172963A

  • Production method of pyrolytic boron nitride-coated carbonaceous substrate

    JP2014118600A

Cited By

  • Insulator having excellent insulation properties and capable of miniaturization

    WO2026225731A1