Printed circuit board and manufacturing method thereof
By configuring printed circuit boards with conductor layers as the outermost layer and adhering to specific relational expressions, the impedance change rate is kept below 5%, enabling the use of high-performance adhesive layers without redesign, thus maintaining circuit pattern stability.
Patent Information
- Application Number
- JP2024146861
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2024-08-28
- Publication Date
- 2024-10-31
- Estimated Expiration
- 2039-11-06
AI Technical Summary
Changing the material of the adhesive layer in a printed circuit board to improve high frequency characteristics alters the dielectric constant of the entire board, necessitating redesign of the circuit pattern to compensate for impedance changes.
The printed circuit board is configured with conductor layers as the outermost layer, laminated via adhesive and dielectric layers, adhering to specific relational expressions to maintain impedance change rates below 5%, allowing the use of high-performance adhesive layers without redesign.
This configuration enables the use of adhesive layers with excellent high frequency characteristics while maintaining impedance stability, allowing reuse of existing circuit patterns without redesign.
Smart Images

Figure 2024156031000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a printed circuit board and a method for manufacturing a printed circuit board. [Background technology]
[0002] Patent Document 1 discloses a technique for providing a printed circuit board with good high-frequency characteristics by using a material with excellent high-frequency characteristics for an adhesive layer of a multi-layer structure. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] International Publication WO2017 / 130945 Summary of the Invention [Problem to be solved by the invention]
[0004] By the way, high frequency characteristics can be improved by using the technology disclosed in Patent Document 1 and by improving the performance of the adhesive layer. However, changing the material of the adhesive layer changes the dielectric constant of the entire printed circuit board.
[0005] For example, if a circuit pattern designed for a conventional printed circuit board that does not use a high-performance adhesive layer is used in a printed circuit board that uses a high-performance adhesive layer, the characteristic impedance at high frequencies will change and reflection loss due to impedance mismatch will increase, resulting in the need to redesign the circuit pattern.
[0006] An object of the present invention is to provide a printed circuit board and a method for manufacturing the printed circuit board that can utilize an adhesive layer having excellent high-frequency characteristics without requiring redesign. [Means for solving the problem]
[0007] In order to solve the above problems, in a printed circuit board formed by laminating at least one dielectric layer and at least two conductor layers, with the conductor layer located in the outermost layer, the conductor layer located in the outermost layer is laminated to the dielectric layer via an adhesive layer, and the relative permittivity Y of the dielectric layer, the relative permittivity X of the adhesive layer, the thickness t (μm) of the adhesive layer, and the impedance change rate p of the circuit formed in the conductor layer when compared with the case where t = 0 (μm) satisfy the following relational expressions 1 to 3, and the impedance change rate p satisfies 0% < p ≤ 5%. (Relational expression 1) X < Y < AX + B (Relational expression 2) A = (0.19t 2 - 5.25t + 43.5)p / 100 + 1 (Relational expression 3) B = (-0.8t + 22)p / 100, which is characterized by this. According to such a configuration, an adhesive layer with excellent high-frequency characteristics can be used without redesign.
[0008] Further, in the present invention, in a printed circuit board formed by laminating at least two dielectric layers and at least three conductor layers, with the conductor layer located in the outermost layer, the conductor layer located between the two dielectric layers is laminated to either one of the two dielectric layers via an adhesive layer, and the relative permittivity Y of the dielectric layer, the relative permittivity X of the adhesive layer, the thickness t (μm) of the adhesive layer, and the impedance change rate p of the circuit formed in the conductor layer when compared with the case where t = 0 (μm) satisfy the following relational expressions 1 to 3, and the impedance change rate p satisfies 0% < p ≤ 5%. (Relational expression 1) X < Y < AX + B (Relational expression 2) A = (0.44t 2 - 12.8t + 108)p / 100 + 1 (Relational expression 3) B = (-0.2t + 26)p / 100, which is characterized by this. According to such a configuration, an adhesive layer with excellent high-frequency characteristics can be used without redesign.
[0009] Further, the present invention is configured by laminating at least two dielectric layers and at least three conductor layers, and in a printed circuit board where the conductor layer is located in the outermost layer, two of the conductor layers located in the outermost layer are respectively laminated via an adhesive layer with respect to the dielectric layer, and the conductor layer located between the two dielectric layers is laminated via an adhesive layer with respect to either one of the two dielectric layers, and the relative permittivity Y of the dielectric layer, the relative permittivity X of the adhesive layer, the thickness t (μm) of the adhesive layer, and the impedance change rate p when the impedance of the circuit formed in the conductor layer is compared with the case of t = 0 (μm) satisfy the following relational expressions 1 to 3, and the impedance change rate p satisfies 0% < p ≦ 5%, (Relational expression 1) X < Y < AX + B (Relational expression 2) A = (0.3t 2 - 8.7t + 78)p / 100 + 1 (Relational expression 3) B = (-0.2t + 10)p / 100, which is characterized in that. According to such a configuration, it is possible to use an adhesive layer with excellent high-frequency characteristics without performing redesign.
[0010] Further, the present invention is characterized in that the impedance change rate p is 3.5% or less. According to such a configuration, by further suppressing the impedance change rate, the necessity for redesign can be further reduced.
[0011] Further, the present invention is characterized in that the impedance change rate p is 2.5% or less. According to such a configuration, by further suppressing the impedance change rate, the necessity for redesign can be further reduced.
[0012] Further, the present invention is characterized in that the impedance change rate p is 2.0% or less. According to such a configuration, by making the impedance change rate extremely small, the necessity for redesign can be made extremely small.
[0013] Further, the present invention is characterized in that the t (μm) is 15 (μm) or less. According to such a configuration, the adhesive strength between the dielectric layer and the conductor layer can be ensured.
[0014] Further, the present invention is characterized in that the t (μm) is 10 (μm) or less. According to such a configuration, the adhesive strength between the dielectric layer and the conductor layer can be ensured.
[0015] Further, the present invention is characterized in that the t (μm) is 5 (μm) or less. According to such a configuration, the adhesive strength between the dielectric layer and the conductor layer can be ensured.
[0016] Further, the present invention is characterized in that the Rz value indicating the surface roughness of the conductor layer is 1 μm or less. According to such a configuration, even when a conductor layer with a small surface roughness and good high-frequency characteristics is used, the need for redesign can be reduced.
[0017] Further, the present invention is characterized in that when the relative permittivity of the dielectric layer is Y and the relative permittivity of the adhesive layer is X, Y = 3.35 or more and 3.85 or less, and X = 2.25 or more and 2.75 or less. According to such a configuration, the impedance change rate can be suppressed, and the need for redesign can be surely reduced.
[0018] Further, the present invention provides a printed circuit board manufacturing method for manufacturing a printed circuit board in which at least one dielectric layer and at least two conductor layers are laminated and the conductor layer is located in the outermost layer. The conductor layer located in the outermost layer is laminated on the dielectric layer via an adhesive layer, and the relative permittivity Y of the dielectric layer, the relative permittivity X of the adhesive layer, the thickness t (μm) of the adhesive layer, and the impedance change rate p of the circuit formed on the conductor layer satisfy the following relational expressions 1 to 3, and the printed circuit board is manufactured so that the impedance change rate p satisfies 0% < p ≤ 5%. (Relational expression 1) X < Y < AX + B (Relational expression 2) A = (0.19t 2It is characterized in that B = ((-5.25t + 43.5)p / 100 + 1) (Relationship 3). According to such a method, an adhesive layer with excellent high-frequency characteristics can be utilized without redesign.
[0019] Further, the present invention relates to a printed circuit board manufacturing method for manufacturing a printed circuit board in which at least two dielectric layers and at least three conductor layers are laminated and the conductor layer is located in the outermost layer. The conductor layer located between the two dielectric layers is laminated via an adhesive layer with respect to either one of the two dielectric layers. The relative permittivity Y of the dielectric layer, the relative permittivity X of the adhesive layer, the thickness t (μm) of the adhesive layer, and the impedance change rate p when the impedance of the circuit formed in the conductor layer is compared with the case of t = 0 (μm) satisfy the following relational expressions 1 to 4, and the printed circuit board is manufactured so that the impedance change rate p satisfies 0% < p ≤ 5%. (Relational expression 1) X < Y < AX + B (Relational expression 2) A = (0.44t 2 It is characterized in that B = ((-12.8t + 108)p / 100 + 1) (Relationship 3). According to such a method, an adhesive layer with excellent high-frequency characteristics can be utilized without redesign.
[0020] Further, the present invention relates to a printed circuit board manufacturing method for manufacturing a printed circuit board in which at least two dielectric layers and at least three conductor layers are laminated and the conductor layer is located in the outermost layer. The two conductor layers located in the outermost layer are each laminated via an adhesive layer with respect to the dielectric layer, and the conductor layer located between the two dielectric layers is laminated via an adhesive layer with respect to either one of the two dielectric layers. The relative permittivity Y of the dielectric layer, the relative permittivity X of the adhesive layer, the thickness t (μm) of the adhesive layer, and the impedance change rate p when the impedance of the circuit formed in the conductor layer is compared with the case of t = 0 (μm) satisfy the following relational expressions 1 to 3, and the printed circuit board is manufactured so that the impedance change rate p satisfies 0% < p ≤ 5%. (Relational expression 1) X < Y < AX + B (Relational expression 2) A = (0.3t 2-8.7t+78)p / 100+1 (relationship 3) B=(-0.2t+10)p / 100. According to this method, an adhesive layer with excellent high frequency characteristics can be used without redesign. Effect of the Invention
[0021] According to the present invention, it is possible to provide a printed circuit board and a method for manufacturing a printed circuit board that can utilize an adhesive layer with excellent high-frequency characteristics without redesigning the circuit board. [Brief description of the drawings]
[0022] [Figure 1] 1 is a cross-sectional view showing an example of the configuration of a printed circuit board according to a first embodiment of the present invention. [Diagram 2] FIG. 2 is a diagram showing an example of a simulation configuration for investigating an impedance change rate of the first embodiment shown in FIG. [Diagram 3] FIG. 3 is a diagram showing an example of a TDR waveform in FIG. 2. [Figure 4] FIG. 11 is a diagram illustrating an example of a method for determining Ta and Tb. [Diagram 5] FIG. 3 is a diagram showing a simulation result in FIG. 2. [Figure 6] FIG. 13 is a diagram for explaining an error in a printed circuit board. [Figure 7] FIG. 3 is a diagram showing a simulation result in FIG. 2. [Figure 8] FIG. 5 is a cross-sectional view showing an example of the configuration of a printed circuit board according to a second embodiment of the present invention. [Figure 9] FIG. 9 is a diagram showing an example of a configuration for simulation for investigating an impedance change rate of the second embodiment shown in FIG. 8. [Figure 10] FIG. 10 is a diagram showing a simulation result in FIG. [Figure 11] FIG. 10 is a diagram showing a simulation result in FIG. [Figure 12] FIG. 10 is a diagram showing a simulation result in FIG. [Figure 13] FIG. 11 is a cross-sectional view showing an example of the configuration of a printed circuit board according to a third embodiment of the present invention. [Figure 14] FIG. 14 is a diagram showing an example of a simulation configuration for investigating an impedance change rate of the third embodiment shown in FIG. [Figure 15] FIG. 15 is a diagram showing an example of a TDR waveform in FIG. 14. [Figure 16] FIG. 11 is a diagram illustrating an example of a method for determining Ta and Tb. [Figure 17] FIG. 15 is a diagram showing a simulation result in FIG. 14. [Figure 18] FIG. 15 is a diagram showing a simulation result in FIG. 14. [Figure 19] FIG. 15 is a diagram showing a simulation result in FIG. 14. [Figure 20] FIG. 15 is a diagram showing a simulation result in FIG. 14. [Figure 21] FIG. 11 is a cross-sectional view showing an example of the configuration of a printed circuit board according to a fourth embodiment of the present invention. [Figure 22] FIG. 13 is a diagram showing a simulation result of a modified embodiment of the present invention. [Diagram 23] FIG. 13 is a diagram showing a simulation result of a modified embodiment of the present invention. [Figure 24] FIG. 13 is a diagram showing a simulation result of a modified embodiment of the present invention. [Diagram 25] FIG. 13 is a diagram showing a simulation result of a modified embodiment of the present invention. [Figure 26] FIG. 4 is a cross-sectional view of a substrate when impedance is actually measured. [Figure 27] FIG. 4 is a cross-sectional view of a substrate when impedance is actually measured. [Figure 28] 1 shows an example of the configuration of a measurement device for actually measuring impedance. [Figure 29] FIG. 29 is a diagram showing the results of actual measurements in FIG. 28. [Diagram 30] FIG. 13 is a diagram showing a simulation result of a modified embodiment of the present invention. [Diagram 31]This is an SEM image of the substrate when measuring the thickness of the adhesive layer. [Diagram 32] FIG. 13 is a diagram showing a simulation result of a modified embodiment of the present invention. [Diagram 33] FIG. 13 is a diagram showing a simulation result of a modified embodiment of the present invention. [Diagram 34] FIG. 13 is a diagram showing a simulation result of a modified embodiment of the present invention. [Diagram 35] FIG. 13 is a diagram showing a simulation result of a modified embodiment of the present invention. [Diagram 36] FIG. 13 is a diagram showing a simulation result of a modified embodiment of the present invention. [Figure 37] FIG. 13 is a diagram showing a simulation result of a modified embodiment of the present invention. [Figure 38] FIG. 13 is a diagram showing a simulation result of a modified embodiment of the present invention. [Figure 39] FIG. 13 is a diagram showing a simulation result of a modified embodiment of the present invention. [Diagram 40] FIG. 13 is a diagram showing a simulation result of a modified embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0023] Next, an embodiment of the present invention will be described.
[0024] (A) Description of the First Embodiment of the Invention Fig. 1 is a cross-sectional view showing a configuration example of a printed circuit board according to a first embodiment of the present invention. In the configuration example shown in Fig. 1, a printed circuit board 10 has a ground layer 11, a dielectric layer 12, an adhesive layer 13, and a conductor layer 14. The first embodiment is an embodiment having a microstrip line.
[0025] Here, the ground layer 11 is made of a highly conductive metal such as copper, and functions as a ground for the circuit.
[0026] The dielectric layer 12 may be made of, for example, epoxy resin, polyamideimide resin, fluororesin, polyimide resin, polyphenylene ether resin, Teflon (registered trademark) resin, or a resin obtained by mixing these with glass fiber. Furthermore, these materials may be appropriately mixed. Of course, materials other than these may also be used.
[0027] The adhesive layer 13 is made of, for example, an epoxy resin, a polyamide resin polymer, a polyethersulfone resin, a polyolefin resin, or a polyphenylene ether resin, and has the function of adhering the conductor layer 14 to the dielectric layer 12 .
[0028] The conductor layer 14 is made of a highly conductive metal such as copper, and various wiring patterns are formed thereon.
[0029] In addition, as a method for manufacturing the printed circuit board 10 shown in FIG. 1, first, a conductor layer 14 having an adhesive layer 13 is formed. More specifically, the adhesive layer 13 is formed by coating or spraying on one side of an electrolytic copper foil or rolled copper foil having an Rz value indicating surface roughness of 1 μm or less. Here, the Rz value means a value expressed in micrometers (μm) obtained by cutting out a reference length from a roughness curve in the direction of its average line, measuring the distance between the crest line and the valley line of the cutout portion in the direction of the longitudinal magnification of the roughness curve, based on JIS standard B0601. The reason why an electrolytic copper foil or rolled copper foil having an Rz value of 1 μm or less is used is that an electrolytic copper foil or rolled copper foil having a small Rz value has better high-frequency characteristics than one having a large Rz value. Specifically, a copper foil having a small Rz value has a reduced signal transmission loss due to the skin effect compared to one having a large Rz value.
[0030] Next, a ground layer 11 made of electrolytic copper foil or rolled copper foil, a dielectric layer 12 made of a dielectric material, and a conductor layer 14 on which an adhesive layer 13 is formed are laminated in this order, and then bonded together by pressing or the like.
[0031] Next, a photoresist layer (not shown) is formed on the conductor layer 14, and is irradiated with ultraviolet light by, for example, an exposure device in accordance with the circuit pattern, thereby allowing the photoresist layer to harden in accordance with the circuit pattern.
[0032] Next, the printed circuit board 10 with the cured photoresist layer is placed in a solvent to remove the uncured photoresist layer, thereby forming a photoresist layer on the conductor layer 14 according to the circuit pattern.
[0033] Next, the printed circuit board 10 is placed in an etching solution. As a result, the areas where the photoresist layer does not exist are corroded and removed by the etching solution, forming a conductor layer 14 according to the circuit pattern. In the example of FIG. 1, a microstrip line is formed.
[0034] Next, the remaining hardened photoresist layer is peeled off using a solvent, etc. In this way, the printed circuit board 10 shown in FIG.
[0035] Next, the first embodiment of the present invention will be described in detail.
[0036] As shown in Fig. 1, the thickness of the adhesive layer 13 is 15 µm, and the total thickness of the adhesive layer 13 and the dielectric layer 12 is 150 µm. In this case, a simulation is performed by an electromagnetic field simulator using the finite element method, such as HFSS (High Frequency Structure Simulator) manufactured by ANSYS, Inc., using a circuit as shown in Fig. 2 having a dielectric layer 12, adhesive layer 13, and conductor layer 14 having similar thicknesses.
[0037] More specifically, in the example shown in Figure 2, a ground layer 11 (not shown) with a length in the y-axis direction of 10 mm is placed on the xy plane with its longitudinal center aligned along the y-axis, and a dielectric layer 12 with a length in the y-axis direction of 10 mm is placed above it (above the z-axis direction), and an adhesive layer 13 with a length in the y-axis direction of 6 mm is placed on top of that, and a conductor layer 14 with a length in the y-axis direction of 10 mm is placed on top of that along the y-axis.
[0038] Then, a pulse signal with a rise time of 25 ps is applied and the TDR (Time Domain Reflectometry) waveform is measured.
[0039] FIG. 3 is a diagram showing the results of the simulation. More specifically, FIG. 3 shows the reflected wave of a signal input from near the origin of the coordinate system. The horizontal axis of FIG. 3 shows time (ps), and the vertical axis shows impedance (Ω). Ta shows the reception time of the reflected wave from point A, and Tb shows the reception time of the reflected wave from point B. As a way of taking Ta and Tb, for example, Ta can be set to near the origin (near Ta=0). For Tb, a point where the slope of the TDR waveform is generally small in common between materials with high and low relative dielectric constants in the vicinity of the peak of the TDR waveform can be selected. As an example, in this embodiment, as shown in FIG. 4, an arbitrary point in a flat region common to the TDR waveform (dashed curve) of the main substrate of the dielectric layer 12 with the highest relative dielectric constant (Y=5) and the TDR waveform (solid curve) of the lowest relative dielectric constant (Y=2) within the analysis range is set as Tb. The flat region can be a region where the curve (dash-dotted curve) showing the slope (Ω / ns) of the TDR waveform of the main substrate with the highest relative dielectric constant (Y=5) and the curve (dash-dotted curve) showing the slope (Ω / ns) of the TDR waveform of the main substrate with the lowest relative dielectric constant (Y=2) are both, for example, 10Ω / ns or less. For example, Tb can be set to 0.062ns, which is in the range of 0.56 to 0.63ns shown in FIG. 4. In the example shown in FIG. 3, Ta=0ns, Tb=0.062ns, and the impedance at time Ta is Za and the impedance at time Tb is Zb, so that Za can be treated as the impedance of the reflected wave from point A and Zb can be treated as the impedance of the reflected wave from point B. Note that the above-mentioned method of taking Za and Zb is one example, and Za and Zb may be obtained by individually selecting flat regions according to the value of Y, for example. Alternatively, the impedance of a printed circuit board may be obtained by actually measuring the impedance of the printed circuit board and using a TDR waveform obtained by the above-mentioned procedure.
[0040] For these simulation results, the impedance change rate [%] is defined as follows:
[0041] Impedance change rate = (Zb - Za) / Za × 100 (1)
[0042] More specifically, equation (1) shows the rate of change in impedance between the part without adhesive layer 13 (point A) where the impedance is Za and the part with adhesive layer 13 (point B) where the impedance is Zb.
[0043] Fig. 5 is a diagram showing the rate of change in impedance when the dielectric constant of the dielectric layer 12 and the dielectric constant of the adhesive layer 13 are changed in Fig. 2. In Fig. 5, the horizontal axis represents the dielectric constant of the primer constituting the adhesive layer 13, and the vertical axis represents the dielectric constant of the main substrate constituting the dielectric layer 12.
[0044] 5, the thin curved lines indicate the boundary lines that divide the regions in which the impedance change rate falls within a predetermined range. For example, the second curved line from the top left is the boundary line that divides the region of the relative dielectric constant in which the impedance change rate is 20.0% or more.
[0045] The thick line L1 is a line segment indicating the position where the relative dielectric constants of the primer and the main substrate are equal. The thick line L2 is a line segment indicating the position where the impedance change rate is 5%. The thick line L3 is a line segment indicating the position where the relative dielectric constant of the main substrate is 3.00.
[0046] If the relative dielectric constant of the primer constituting the adhesive layer 13 is X and the relative dielectric constant of the dielectric material constituting the dielectric layer 12 is Y, then these must satisfy the following two relational expressions (2) and (3).
[0047] Y>X (2)
[0048] In other words, if a material is selected so that the relative dielectric constant of adhesive layer 13 is greater than the relative dielectric constant of dielectric layer 12, the delay of signals passing through conductor layer 14 will be large, so it is necessary to select a material so as to satisfy equation (2).
[0049] Y<1.38X+0.50 (3)
[0050] The right-hand side of equation (3) represents the bold straight line L2 in Figure 5. By setting equation (3) to be satisfied, the rate of change in characteristic impedance can be kept to 5% or less. The characteristic impedance of typical high-frequency circuit boards is controlled to ±5%, and as long as the change is within 5%, transmission with little reflection loss is possible even when using circuit patterns designed for conventional printed circuit boards.
[0051] In order to suppress the reflected noise to 5% or less of the signal amplitude, it is necessary to suppress the change in characteristic impedance to within 10%. Therefore, the impedance adjustment specification of the board is set to ±10% as the standard (Eric Bogatin, High-Speed Digital Signal Transmission Technology: Introduction to Signal Integrity (2010), supervised translation by Toshio Sudo, p.271).
[0052] Due to etching accuracy, the line width generally varies by about twice the copper foil thickness, which causes the line impedance to vary by about ±5%. As mentioned above, in order to keep the change in characteristic impedance within ±10%, it is necessary to keep the change within 5%. For example, in Figure 6, if the design is such that the impedance is 50 Ω when w = 0.324 mm, and there is a variation of w ± 0.012 mm x 2 of the copper foil thickness, then the impedance will vary by about ±5%, with w = 0.324 + 0.024 mm being 47.9 Ω, and with w = 0.324 - 0.024 mm being about 52.4 Ω.
[0053] In addition, since an epoxy-based base material is assumed to be used as the main base material constituting the dielectric layer 12, the relative dielectric constant thereof falls within the range of the following formula (4). Of course, when a base material other than an epoxy-based base material is used, the relative dielectric constant may fall outside this range.
[0054] 3≦Y≦5 (4)
[0055] Fig. 7 is a diagram showing the relationship between the impedance change rate, signal delay, and ease of application to existing designs when the relative dielectric constant of the main substrate constituting the dielectric layer 12 in Fig. 2 is set to 3 or 5, and the relative dielectric constant of the primer constituting the adhesive layer 13 is changed. In Fig. 5, "Example" shows the results according to the first embodiment of the present invention, and "Comparative Example" shows an embodiment different from the first embodiment.
[0056] As shown in FIG. 7 , in the “Examples” that satisfy formulas (2) to (4), all signal delays are “none,” and the ease of application to existing designs is evaluated as either “◯” for an impedance change rate of “3.5 to 5%” that indicates that a circuit pattern designed for a conventional printed circuit board can be applied, “◎” for an impedance change rate of “2.5 to 3.5%” that indicates that a circuit pattern designed for a conventional printed circuit board is easily applicable, “◎◎” for an impedance change rate of “2 to 2.5%” that indicates that a circuit pattern designed for a conventional printed circuit board is even easier to apply, or “◎◎◎” for an impedance change rate of “up to 2%” that indicates that a circuit pattern designed for a conventional printed circuit board is particularly easily applicable.
[0057] On the other hand, in the comparative examples, for example, in the example of sample number "293", the relative dielectric constant Y of the main substrate is 3, while the relative dielectric constant X of the primer is 3.5, so formula (2) is not satisfied. In this case, the ease of application to existing designs is "◎◎◎", but the signal delay is "present", which is not preferable.
[0058] In addition, sample numbers "378" to "387" satisfy formula (2) but do not satisfy formula (3), so there is "no" signal delay, but the ease of application to existing designs is either "△" for an impedance change rate of "5 to 7.5%" and indicating that it is difficult to apply a circuit pattern designed for a conventional printed circuit board, "×" for an impedance change rate of "7.5 to 10%" and indicating that it is difficult to apply a circuit pattern designed for a conventional printed circuit board, or "XX" for an impedance change rate of "10% or more" and indicating that it is particularly difficult to apply a circuit pattern designed for a conventional printed circuit board. For this reason, it is difficult to apply these to existing designs, so there is a high possibility that redesign will be required.
[0059] As described above, in the first embodiment of the present invention, in the configuration shown in Fig. 1, when the relative dielectric constant of the primer constituting the adhesive layer 13 is X and the dielectric constant of the dielectric constituting the dielectric layer 12 is Y, the rate of change in impedance can be made 5% or less by selecting materials such that X and Y satisfy the above-mentioned formulas (2) to (4). As a result, when using a conductor layer 14 having good high-frequency characteristics and an Rz value of 1 µm or less, it becomes necessary to use the adhesive layer 13 to increase the bonding strength. Even in such a case, however, by selecting materials such that the above-mentioned formulas (2) to (4) are satisfied, the previous circuit pattern can be reused without making design changes.
[0060] (B) Description of the second embodiment of the present invention Fig. 8 is a diagram showing an example of the configuration of a printed circuit board according to a second embodiment of the present invention. In the first embodiment shown in Fig. 1, the adhesive layer 13 is fixed at 15 μm, but in the example of Fig. 8, the adhesive layer 13 is set to t μm. In addition, the impedance change rate is set to p%, and the relationship between X, Y, t, and p is obtained.
[0061] FIG. 9 shows a configuration example that is the subject of the simulation used in the second embodiment. In the example of FIG. 9, compared with FIG. 2, the thickness of the adhesive layer 13 is changed from 15 μm to t μm. That is, in the second embodiment, the simulation was performed while changing the thickness t of the adhesive layer 13.
[0062] FIG. 10 shows the simulation results when t = 15 μm. Further, FIG. 11 shows the simulation results when t = 10 μm. Furthermore, FIG. 12 shows the simulation results when t = 5 μm. From these comparisons, as the thickness t of the adhesive layer 13 becomes thinner, the thin line curve indicating the boundary line of the impedance change rate moves toward the upper left point (1.00, 5.00) and the interval between the curves widens. As a result, the thinner the thickness t of the adhesive layer 13, the wider the region where the impedance change rate falls within the desired range (for example, the range where the impedance change rate p is 0% < p ≤ 5%, that is, exceeding 0% and less than or equal to 5%), and the range of material selection that can eliminate the need for design changes can be widened. From this perspective, t = 10 μm or less is more preferable, and t = 5 μm or less is even more preferable.
[0063] Also, based on FIGS. 10 to 12, when obtaining the relationships of X, Y, t, and p, the following equations (5) to (7) are obtained.
[0064] X < Y < AX + B ···(5)
[0065] A = (0.19t 2 -5.25t + 43.5)p / 100 + 1 ···(6)
[0066] B = (-0.8t + 22)p / 100 ···(7)
[0067] The boundaries within a predetermined range of the impedance change rate p calculated by the above formula are shown as thick straight lines in Figures 10 to 12. The thick straight lines showing the calculation results in these figures closely match the thin curved lines showing the results obtained by simulation. Therefore, by substituting the thickness t of adhesive layer 13 and the desired impedance change rate p into formulas (5) to (7) above for calculation, the range of the relative dielectric constant X of adhesive layer 13 and the relative dielectric constant Y of dielectric layer 12 can be calculated.
[0068] As described above, in the second embodiment of the present invention, in the configuration shown in Fig. 8, when the relative dielectric constant of the primer constituting the adhesive layer 13 is X, the dielectric constant of the dielectric material constituting the dielectric layer 12 is Y, the thickness of the adhesive layer 13 is t, and the impedance change rate is p, by selecting materials so that X, Y, and t satisfy the above-mentioned formulas (5) to (7), the impedance change rate p can be kept within a desired range. Therefore, when using a conductor layer 14 with good high-frequency characteristics, particularly an Rz value of 1 µm or less, it becomes necessary to use the adhesive layer 13 to increase the bonding strength, but even in such a case, by selecting materials so as to satisfy the above-mentioned formulas (5) to (7), it is possible to reuse the previous circuit pattern without making design changes.
[0069] (C) Description of the third embodiment of the present invention Fig. 13 is a diagram showing a configuration example of a printed circuit board according to a third embodiment of the present invention. In the configuration example shown in Fig. 13, compared to Fig. 8, a dielectric layer 15 and a ground layer 16 are newly added on the conductor layer 14 and the adhesive layer 13. The other configurations are the same as those in Fig. 8. Note that the third embodiment is an embodiment having a strip line.
[0070] Here, the dielectric layer 15 is made of the same material as the dielectric layer 12. That is, for the dielectric layer 15, for example, epoxy resin, polyamideimide resin, fluororesin, polyimide resin, polyphenylene ether resin, Teflon (registered trademark) resin, and resins obtained by mixing these with glass fiber can be used. Furthermore, these materials may be appropriately mixed and used. Of course, materials other than these may also be used.
[0071] The ground layer 16 is made of a highly conductive metal such as copper, and functions as a ground, similar to the ground layer 11. Note that the ground layer 16 may be configured as a power layer that supplies positive power, instead of a ground layer.
[0072] The printed circuit board 10 shown in FIG. 13 can be manufactured by laminating the dielectric layer 15 and the ground layer 16 on the printed circuit board of FIG. 8 described above by a press process.
[0073] Fig. 14 shows the configuration of the simulation target used in the third embodiment. In the example of Fig. 14, on the xy plane, a ground layer 11 (not shown) having a length in the y-axis direction of 20 mm is arranged so that the center in the longitudinal direction is along the y-axis, a dielectric layer 12 having a length in the y-axis direction of 20 mm is arranged above it (z-axis direction), an adhesive layer 13 having a length in the y-axis direction of 10 mm is arranged on it in the lower half of the figure, a conductor layer 14 having a length in the x-axis direction of 0.09 to 0.29 mm and a length in the y-axis direction of 20 mm is arranged on it, a dielectric layer 15 having a length in the y-axis direction of 20 mm is arranged on it, and a ground layer 16 having a length in the y-axis direction of 20 mm is arranged on it.
[0074] The bottom of Figure 14 shows cross-sectional views of points A and B. At point A, the dielectric layer 12 and the dielectric layer 15 are integrally configured. On the other hand, at point B, an adhesive layer 13 having a thickness of t μm is interposed between the dielectric layer 12 and the dielectric layer 15. The thicknesses of the dielectric layer 12, the adhesive layer 13, and the dielectric layer 15 are 318 μm, and the ground layer 16 is 18 μm. The impedance of the area where the adhesive layer 13 does not exist is adjusted to 50 Ω.
[0075] For the configuration shown in FIG. 14, a pulse signal with a rise time of 25 ps is applied and the TDR waveform is measured.
[0076] Fig. 15 is a diagram showing the TDR waveform of the simulation result. Fig. 15 shows the reflected wave of a signal input from near the origin of the coordinate system. The horizontal axis of this diagram indicates time, and the vertical axis indicates impedance. Furthermore, Ta indicates the reception time of the reflected wave from point A, and Tb indicates the reception time of the reflected wave from point B. In order to determine Ta and Tb, it is possible to select a point in the TDR waveform where the slope of the TDR waveform is generally small in both materials with high and low relative dielectric constants. In this embodiment, as an example, as shown in Fig. 16, any point in the first region where the TDR waveform (dashed curve) of the main substrate of the dielectric layer 12 with the highest relative dielectric constant (Y = 5) and the TDR waveform (solid curve) of the main substrate of the dielectric layer 12 with the lowest relative dielectric constant (Y = 2) are both flat within the analysis range can be Ta, and any point in the first region where the TDR waveform (dashed curve) of the main substrate of the dielectric layer 12 with the highest relative dielectric constant (Y = 5) and the TDR waveform of the main substrate of the dielectric layer 12 with the lowest relative dielectric constant (Y = 2) rise together and then become flat within the analysis range can be Tb. The flat region can be, for example, a region where the curve (double-dotted curve) showing the slope (Ω / ns) of the TDR waveform of the main substrate with the highest relative dielectric constant (Y = 5) and the curve (single-dotted curve) showing the slope (Ω / ns) of the TDR waveform of the main substrate with the lowest relative dielectric constant (Y = 2) are both 10Ω / ns or less. For example, Ta can be set to 0.050 ns, which is in the range of 0.026 to 0.088 ns in FIG. 16. Also, Tb can be set to 0.180 ns, which is in the range of 0.180 to 0.188 ns in FIG. 16. In the example shown in FIG. 15, Ta=0.050 ns, Tb=0.180 ns, and the impedance at time Ta is Za, and the impedance at time Tb is Zb, so that Za can be treated as the impedance of the reflected wave from point A, and Zb can be treated as the impedance of the reflected wave from point B. Note that the above-mentioned method of taking Za and Zb is one example, and Za and Zb may be obtained by selecting flat regions individually according to the value of Y, for example. Also, the impedance of the printed circuit board may be obtained by using a TDR waveform obtained by actually measuring the impedance of the printed circuit board, according to the above-mentioned procedure.
[0077] FIG. 17 shows the simulation results of FIG. 14 when the thickness t of the adhesive layer 13 is set to 15 μm. In FIG. 17, the thin-line curve indicates the boundary that divides the region where the impedance change rate falls within a predetermined range. For example, the second thin line from the upper left indicates the boundary where the impedance change rate is 7.5% or more.
[0078] FIG. 18 shows the simulation results of FIG. 14 when the thickness t of the adhesive layer 13 is set to 10 μm. In FIG. 18, the thin-line curve indicates the boundary line that divides the region where the impedance change rate falls within a predetermined range. For example, the second thin line from the upper left indicates the boundary where the impedance change rate is 5.0% or more.
[0079] FIG. 19 shows the simulation results of FIG. 14 when the thickness t of the adhesive layer 13 is set to 5 μm. In FIG. 19, the thin-line curve indicates the boundary line that divides the region where the impedance change rate falls within a predetermined range. For example, the upper left thin line indicates the boundary where the impedance change rate is 2.5% or more.
[0080] From these comparisons, as the thickness t of the adhesive layer 13 decreases, the curve indicating the range of the impedance change rate moves toward the upper left point (1.00, 5.00) and the interval between the curves widens. As a result, the thinner the thickness t of the adhesive layer 13, the wider the region where the impedance change rate falls within the desired range (for example, the range where the impedance change rate p is 0% < p ≤ 5%, that is, the range exceeding 0% and being 5% or less). From this perspective, t = 10 μm or less is more preferable, and t = 5 μm or less is even more preferable.
[0081] Also, based on FIGS. 17 to 19, when obtaining the relationships of X, Y, t, and p, the following equations (8) to (10) are obtained.
[0082] X < Y < AX + B ···(8)
[0083] A = (0.44t 2 -12.8t + 108)p / 100 + 1 ···(9)
[0084] B = (-0.2t + 26)p / 100 (10)
[0085] The boundaries of the impedance change rate p obtained by the above formula are shown as thick straight lines in Figures 17 to 19. The thick straight lines showing the calculation results in these figures and the thin curved lines showing the results obtained by simulation are in good agreement. Therefore, by substituting the thickness t of the adhesive layer 13 and the desired impedance change rate p into the above formulas (8) to (10) and performing calculations, it is possible to obtain the range of the relative dielectric constant X of the adhesive layer 13 and the relative dielectric constant Y of the dielectric layer 12. This allows the impedance change rate to be suppressed, allowing the existing design to be reused without modification.
[0086] Fig. 20 is a diagram showing the relationship between the impedance change rate, signal delay, and ease of application to existing designs when the relative dielectric constant of the main substrate constituting the dielectric layer 12 is set to 3 or 5 and the relative dielectric constant of the primer constituting the adhesive layer 13 is changed in Fig. 14. In Fig. 20, "Example" shows the results according to the third embodiment of the present invention, and "Comparative Example" shows an embodiment different from the third embodiment.
[0087] As shown in FIG. 20, in the “Examples” that satisfy equations (8) to (10), all signal delays are “none,” and the ease of application to existing designs is evaluated as either “◯” for an impedance change rate of “3.5 to 5%” indicating that a circuit pattern designed for a conventional printed circuit board can be applied, “◎” for an impedance change rate of “2.5 to 3.5%” indicating that a circuit pattern designed for a conventional printed circuit board is easily applicable, “◎◎” for an impedance change rate of “2 to 2.5%” indicating that a circuit pattern designed for a conventional printed circuit board is even easier to apply, or “◎◎◎” for an impedance change rate of “up to 2%” indicating that a circuit pattern designed for a conventional printed circuit board is particularly easy to apply.
[0088] On the other hand, in the comparative example, for example, in the case of the sample number "686", the relative permittivity Y of the main base material is 3, while the relative permittivity X of the primer is 3.5, so X < Y is not satisfied. In this case, the ease of application to the existing design is "◎◎◎", but since the signal delay is "present", it is not preferable.
[0089] Also, in the sample numbers "771" to "775", although X < Y is satisfied, X < Y < AX + B is not satisfied. Therefore, although there is no signal delay, the ease of application to the existing design is such that the impedance change rate is "5 to 7.5%", indicating "△" that it is difficult to apply the circuit pattern designed for the conventional printed circuit board, the impedance change rate is "7.5 to 10%", indicating "×" that it is difficult to apply the circuit pattern designed for the conventional printed circuit board, or the impedance change rate is "10% or more", indicating "××" that it is particularly difficult to apply the circuit pattern designed for the conventional printed circuit board. For this reason, since it is difficult to apply these to the existing design, there is a high possibility that a new design will be required.
[0090] As described above, in the third embodiment of the present invention, in the configuration shown in FIG. 13, when the relative permittivity of the primer constituting the adhesive layer 13 is X, the permittivity of the dielectric constituting the dielectric layer 12 is Y, the thickness of the adhesive layer 13 is t, and the impedance change rate is p, by selecting the members so that X, Y, and p satisfy the above-described formulas (8) to (10), the impedance change rate p can be kept within a desired range. Therefore, when using the conductor layer 14 with good high-frequency characteristics and an Rz value of 1 μm or less, it is necessary to use the adhesive layer 13 to increase the bonding strength. Even in such a case, by selecting the materials so as to satisfy the above-described formulas (8) to (10), the conventional circuit pattern can be reused without changing the design.
[0091] (D) Description of the Fourth Embodiment of the Present Invention FIG. 21 is a diagram showing a configuration example of the fourth embodiment of the present invention. In FIG. 21, parts corresponding to those of the third embodiment shown in FIG. 13 are given the same reference numerals, and their description will be omitted. Compared with FIG. 13, FIG. 21 has added adhesive layers 31 and 32. The rest is the same as FIG. 13. Here, adhesive layer 31 is a layer that bonds ground layer 11 and dielectric layer 12. Adhesive layer 32 is a layer that bonds dielectric layer 15 and ground layer 16. Adhesive layers 31 and 32 are made of the same material as adhesive layer 13.
[0092] Fig. 22 shows the simulation results of Fig. 21 when the thickness t of the adhesive layer 13 is set to 15 µm. In Fig. 22, the thin curved lines indicate boundaries that separate regions where the impedance change rate is within a predetermined range. For example, the second thin line from the top left indicates the boundary where the impedance change rate is 15.0% or more.
[0093] Fig. 23 shows the simulation results of Fig. 21 when the thickness t of the adhesive layer 13 is set to 10 μm. In Fig. 23, the thin curved lines indicate the boundary lines dividing the regions where the impedance change rate is within a predetermined range. For example, the second thin line from the top left indicates the boundary where the impedance change rate is 10.0% or more.
[0094] Fig. 24 shows the simulation results of Fig. 21 when the thickness t of the adhesive layer 13 is set to 5 μm. In Fig. 35, the thin curved lines indicate the boundary lines dividing the regions where the impedance change rate is within a predetermined range. For example, the second thin line from the top left indicates the boundary where the impedance change rate is 5.0% or more.
[0095] From these comparisons, as the thickness t of the adhesive layer 13 decreases, the curve showing the range of the impedance change rate moves toward the upper left point (1.00, 5.00) and the interval between the curves widens. As a result, the thinner the thickness t of the adhesive layer 13, the wider the region where the impedance change rate falls within the desired range (for example, the range where the impedance change rate p is 0% < p ≤ 5%, that is, exceeding 0% and less than or equal to 5%). From this perspective, t = 10 μm or less is more preferable, and t = 5 μm or less is even more preferable.
[0096] Also, based on FIGS. 22 to 24, when obtaining the relationships of X, Y, t, and p, the following equations (11) to (13) are obtained.
[0097] X < Y < AX + B ···(11)
[0098] A = (0.3t 2 −8.7t + 78)p / 100 + 1 ···(12)
[0099] B = (−0.2t + 10)p / 100 ···(13)
[0100] The boundaries of the impedance change rate p obtained by the above equations are shown as thick solid lines in FIGS. 22 to 24. The thick solid lines showing the calculation results in these figures are in good agreement with the thin curves showing the results obtained by simulation. Therefore, for the above equations (11) to (13), by substituting the thickness t of the adhesive layer 13 and the desired impedance change rate p and performing the calculation, the ranges of the relative permittivity X of the adhesive layer 13 and the relative permittivity Y of the dielectric layer 12 can be obtained. Thereby, by suppressing the impedance change rate, it is possible to be used without changing the existing design.
[0101] FIG. 25 is a diagram showing the relationship among the impedance change rate, signal delay, and ease of application to an existing design when the relative permittivity of the main base material constituting the dielectric layer 12 is set to 3 or 5 and the relative permittivity of the primer constituting the adhesive layer 13 is changed in FIG. 21. In FIG. 25, "Example" shows the results according to the fourth embodiment of the present invention, and "Comparative Example" shows an embodiment different from the fourth embodiment.
[0102] As shown in FIG. 25, in the "Examples" that satisfy formulas (11) to (13), there is no signal delay in all cases. Also, regarding the ease of application to an existing design, the impedance change rate is "3.5 to 5%", indicating that the circuit pattern designed for a conventional printed circuit board can be applied, marked with "〇"; the impedance change rate is "2.5 to 3.5%", indicating that it is easy to apply the circuit pattern designed for a conventional printed circuit board, marked with "◎"; the impedance change rate is "2 to 2.5%", indicating that it is even easier to apply the circuit pattern designed for a conventional printed circuit board, marked with "◎◎"; the impedance change rate is "~2%", indicating that it is particularly easy to apply the circuit pattern designed for a conventional printed circuit board, marked with "◎◎◎".
[0103] On the other hand, in the comparative example, for example, in the case of sample number "1079", the relative permittivity Y of the main base material is 3, while the relative permittivity X of the primer is 3.5, so X < Y is not satisfied. In this case, although the ease of application to an existing design is "◎◎◎", it is not preferable because there is a signal delay.
[0104] Also, for sample numbers “1164” to “1170”, although X < Y is satisfied, X < Y < AX + B is not satisfied. So, there is no signal delay, but the ease of application to the existing design is as follows: when the impedance change rate is “5 - 7.5%”, it is indicated by “△” that it is difficult to apply the circuit pattern designed for the conventional printed circuit board; when the impedance change rate is “7.5 - 10%”, it is indicated by “×” that it is difficult to apply the circuit pattern designed for the conventional printed circuit board; when the impedance change rate is “10% - ”, it is indicated by “××” that it is particularly difficult to apply the circuit pattern designed for the conventional printed circuit board. Therefore, for these, since it is difficult to apply them to the existing design, there is a high possibility that a re - design will be required.
[0105] As described above, in the fourth embodiment of the present invention, in the configuration shown in FIG. 21, when the relative permittivity of the primer constituting the adhesive layer 13 is X, the permittivity of the dielectric constituting the dielectric layer 12 is Y, the thickness of the adhesive layer 13 is t, and the impedance change rate is p, by selecting the members so that X, Y, and p satisfy the above - mentioned formulas (11) to (13), the impedance change rate p can be kept within a desired range. Therefore, when using the conductor layer 14 with good high - frequency characteristics and an Rz value of 1 μm or less, it is necessary to use the adhesive layer 13 to increase the bonding strength. Even in such a case, by selecting the materials so that the above - mentioned formulas (11) to (13) are satisfied, the conventional circuit pattern can be diverted without making a design change.
[0106] Next, the method for measuring the line impedance will be described.
[0107] In this embodiment, in order to actually measure the line impedance, a measurement board 10A having a line pattern with an adhesive layer having the layer configuration of Fig. 26 and a measurement board 10B having the same line pattern without an adhesive layer shown in Fig. 27 are created. In the configuration shown in Fig. 26, the thickness of the adhesive layers 13, 31, 32 is t μm, and the thickness of the adhesive layers 13, 31, 32 and the dielectric layers 12, 15 is 318 μm. In the configuration shown in Fig. 27, the thickness of the dielectric layers 12, 15 is 318 μm.
[0108] 28, both ends of the lines formed on such measurement boards 10A, 10B are provided with patterns for inputting and outputting signals from connectors 61, 62. A signal is input to measurement boards 10A, 10B from vector network analyzer 50 via connectors 61, 62 and cables 51, 52, the frequency is swept up to an arbitrary range, and the frequency characteristics of the return loss of measurement boards 10A, 10B are measured.
[0109] In the vector network analyzer 50, a step signal is convolved with the data measured in the frequency domain, and an inverse Fourier transform is performed to obtain a graph of the reflection coefficient, which is step response data in the time domain. In the actual measurement of the line impedance in this embodiment, an E8364C manufactured by Keysight Technologies is used as the vector network analyzer 50. Furthermore, by setting the port impedance of the vector network analyzer 50 as the reference impedance, the impedance is calculated from the reflection coefficient, and a graph is obtained in which the horizontal axis indicates time and the vertical axis indicates impedance, as shown in FIG.
[0110] In the graph shown in Figure 29, there is a flat region with peaks at both ends indicating impedance mismatch due to the contact between connectors 61, 62 and the board. These two peaks are regarded as peaks corresponding to the line ends, and the inside of these peaks can be regarded as the region corresponding to the line section. In this measurement, the impedance of the board can be calculated by averaging the values in a range of 5% of the distance between the peaks corresponding to both line ends, forward and backward from the center of both line ends.
[0111] FIG. 29 shows the results of actual measurements of a substrate in which a dielectric layer 12 is made of a dielectric material with a relative permittivity Y=3.6, an adhesive layer 13 is made of an adhesive with a relative permittivity X=2.2, and the thickness of the adhesive layer 13 is set to 15 μm. The impedance change rate due to the presence or absence of an adhesive layer is about 4.9% (=(50.6-48.2) / 48.2×100). The relative permittivity Y of the dielectric layer 12 and the relative permittivity X of the adhesive layer 13 can be measured in accordance with the Japanese Industrial Standard JIS C2138:2007. FIG. 30 shows the results of simulation when the thickness of the adhesive layer 13 of the measurement substrate 10A having the line pattern with an adhesive layer having the layer structure of FIG. 26 is set to 15 μm. More specifically, FIG. 30 shows the results when the thickness of the adhesive layer 13 is 15 μm, and the squares in the figure show the characteristics when X=2.2 and Y=3.6. The actual measurements are within the range of the squares in these figures. The dielectric constant X of the adhesive layer 13 and the dielectric constant Y of the dielectric layer 12 may change depending on the frequency of the input signal. For this reason, although the measurement results are expressed by square regions in Fig. 30, the dielectric constants at representative frequencies (e.g., median or average) of the frequency band of the signal input as the values of X and Y may be used as the values of X and Y. In this measurement and simulation, a 10 GHz signal is used.
[0112] Next, a method for measuring the thickness of the adhesive layer will be described.
[0113] Figure 31 is a diagram showing the cross section of a sample consisting of a resin layer and copper foil. In the example of Figure 31, the substrate sample is processed into small pieces using an ultramicrotome or the like, and the observation surface is treated by ion milling, after which an SEM image is taken using a SEM (Scanning Electron Microscope). When the resin layer is divided into layers that do not contain filler material or areas of different colors, the layer closest to the copper foil can be defined as the adhesive layer and its thickness can be measured.
[0114] (D) Description of Modified Embodiments The above embodiment is merely an example, and it goes without saying that the present invention is not limited to the above-mentioned cases. For example, although the above embodiment does not show specific examples of the relative dielectric constants X and Y of the dielectric layer 12 and the adhesive layer 13, for example, a material with X=2.5 and Y=3.6 may be used.
[0115] 32 to 34 show simulation results when a dielectric having a relative dielectric constant X=2.5 is used as the dielectric layer 12 of the second embodiment, an adhesive having a relative dielectric constant Y=3.6 is used as the adhesive layer 13, and the thickness of the adhesive layer 13 is set to 15, 10, and 5 μm. More specifically, FIG. 32 shows the results when the thickness of the adhesive layer 13 is 15 μm, and the circle in the figure shows the characteristics when X=2.5 and Y=3.6. In the example of FIG. 32, the impedance change rate is 4.2%. Furthermore, FIG. 33 shows the results when the thickness of the adhesive layer 13 is 10 μm, and the circle in the figure shows the characteristics when X=2.5 and Y=3.6. In the example of FIG. 33, the impedance change rate is 3.0%. Furthermore, FIG. 34 shows the results when the thickness of the adhesive layer 13 is 5 μm, and the circle in the figure shows the characteristics when X=2.5 and Y=3.6. In the example of FIG. 34, the impedance change rate is 2.2%.
[0116] 35 to 37 show simulation results in the case where a dielectric having a relative dielectric constant X=2.5 is used as the dielectric layer 12 of the third embodiment, an adhesive having a relative dielectric constant Y=3.6 is used as the adhesive layer 13, and the thickness of the adhesive layer 13 is set to 15, 10, and 5 μm. More specifically, FIG. 35 shows the results when the thickness of the adhesive layer 13 is 15 μm, and the circle in the figure shows the characteristics when X=2.5 and Y=3.6. In the example of FIG. 35, the impedance change rate is 1.9%. Furthermore, FIG. 36 shows the results when the thickness of the adhesive layer 13 is 10 μm, and the circle in the figure shows the characteristics when X=2.5 and Y=3.6. In the example of FIG. 36, the impedance change rate is 1.2%. Furthermore, FIG. 37 shows the results when the thickness of the adhesive layer 13 is 5 μm, and the circle in the figure shows the characteristics when X=2.5 and Y=3.6. In the example of FIG. 37, the impedance change rate is 0.2%.
[0117] 38 to 40 show simulation results in the case where a dielectric having a relative dielectric constant X=2.5 is used as the dielectric layer 12 of the fourth embodiment, an adhesive having a relative dielectric constant Y=3.6 is used as the adhesive layer 13, and the thickness of the adhesive layer 13 is set to 15, 10, and 5 μm. More specifically, FIG. 38 shows the results when the thickness of the adhesive layer 13 is 15 μm, and the circle in the figure shows the characteristics when X=2.5 and Y=3.6. In the example of FIG. 38, the impedance change rate is 2.5%. Furthermore, FIG. 39 shows the results when the thickness of the adhesive layer 13 is 10 μm, and the circle in the figure shows the characteristics when X=2.5 and Y=3.6. In the example of FIG. 39, the impedance change rate is 1.3%. Furthermore, FIG. 40 shows the results when the thickness of the adhesive layer 13 is 5 μm, and the circle in the figure shows the characteristics when X=2.5 and Y=3.6. In the example of FIG. 40, the impedance change rate is 0.5%.
[0118] From the above, in both the microstrip line and the strip line, if a dielectric with a relative dielectric constant X=2.5 is used as the dielectric layer 12, an adhesive with a relative dielectric constant Y=3.6 is used as the adhesive layer 13, and the thickness of the adhesive layer 13 is set to 15, 10, or 5 μm, the impedance change rate falls within the range of 0.2 to 4.2%. Therefore, by selecting the above-mentioned materials, it is possible to achieve an impedance change rate that does not require design changes. Note that, although X=2.5 and Y=3.6 are set above, materials having a dielectric constant within a predetermined range centered on these values may be used. For example, X=2.25 or more and 2.75 or less, and Y=3.35 or more and 3.85 or less may be set.
[0119] In the first embodiment, there is one dielectric layer 12 and two conductor layers (ground layer 11 and conductor layer 14), and in the third and fourth embodiments, there are two dielectric layers 12, 15 and three conductor layers (ground layers 11, 16 and conductor layer 14), but the number of dielectric layers and conductor layers may be set to other numbers.
[0120] In addition, in each of the above embodiments, the thickness t of the adhesive layer 13 is set to 5≦t≦15, but it may be set to t<5 as necessary.
[0121] In each of the above embodiments, the dielectric constant is adjusted by selecting the materials of the dielectric layers 12 and 15 and the adhesive layer 13, but the dielectric constant may be adjusted by changing the shapes of these layers. For example, the dielectric constant may be adjusted by providing a plurality of air holes.
[0122] In addition, since the above formulas (1) to (16) are approximate formulas, the constants included in them are merely examples and are not limited to these. In addition, since it is expected that the constants may vary to some extent depending on the environment, etc., it is expected that they have a certain range. [Explanation of symbols]
[0123] 10 Printed circuit board 11 Ground Layer 12 Dielectric layer 13 Adhesive layer 14 Conductor layer 15 Dielectric layer 16 Ground Layer
Claims
1. A printed circuit board comprising at least one dielectric layer and at least two conductor layers laminated together, the conductor layers being positioned as outermost layers, the conductor layer located at the outermost layer is laminated on the dielectric layer via an adhesive layer, a relative permittivity Y of the dielectric layer, a relative permittivity X of the adhesive layer, a thickness t (μm) of the adhesive layer, and an impedance change rate p when the impedance of a line formed in the conductor layer is compared with that when t=0 (μm) satisfy the following relational expressions 1 to 3, and the impedance change rate p satisfies 0%<p≦5%. (Relationship 1) X<Y<AX+B (Relationship 2) A = (0.19t 2 -5.25t+43. 5) p / 100+1 (Relationship 3) B = (-0.8t + 22) p / 100 A printed circuit board characterized by:
2. A printed circuit board comprising at least two dielectric layers and at least three conductor layers laminated together, the conductor layers being positioned as outermost layers, the conductor layer located between the two dielectric layers is laminated to one of the two dielectric layers via an adhesive layer; a relative permittivity Y of the dielectric layer, a relative permittivity X of the adhesive layer, a thickness t (μm) of the adhesive layer, and an impedance change rate p when the impedance of a line formed in the conductor layer is compared with that when t=0 (μm) satisfy the following relational expressions 1 to 3, and the impedance change rate p satisfies 0%<p≦5%. (Relationship 1) X<Y<AX+B (Relationship 2) A = (0.44t 2 -12.8t+108)p / 100+1 (Relational expression 3) B=(-0.2t+26)p / 100 A printed circuit board characterized by:
3. A printed circuit board comprising at least two dielectric layers and at least three conductor layers laminated together, the conductor layers being positioned as outermost layers, The two conductor layers located in the outermost layers are laminated on the dielectric layers via adhesive layers, and the conductor layer located between the two dielectric layers is laminated on one of the two dielectric layers via an adhesive layer; a relative permittivity Y of the dielectric layer, a relative permittivity X of the adhesive layer, a thickness t (μm) of the adhesive layer, and an impedance change rate p when the impedance of a line formed in the conductor layer is compared with that when t=0 (μm) satisfy the following relational expressions 1 to 3, and the impedance change rate p satisfies 0%<p≦5%. (Relationship 1) X<Y<AX+B (Relational Expression 2) A = (0.3t 2 - 8.7t + 78)p / 100 + 1 (Relational expression 3) B=(-0.2t+10)p / 100 A printed circuit board characterized by:
4. 4. The printed circuit board according to claim 1, wherein the impedance change rate p is 3.5% or less.
5. 4. The printed circuit board according to claim 1, wherein the impedance change rate p is 2.5% or less.
6. 4. The printed circuit board according to claim 1, wherein the impedance change rate p is 2.0% or less.
7. 7. The printed circuit board according to claim 1, wherein the thickness t (μm) is 15 (μm) or less.
8. 7. The printed circuit board according to claim 1, wherein the thickness t (μm) is 10 (μm) or less.
9. 7. The printed circuit board according to claim 1, wherein the t (μm) is 5 (μm) or less.
10. 10. The printed circuit board according to claim 1, wherein the conductor layer has a surface roughness Rz value of 1 [mu]m or less.
11. 11. The printed circuit board according to claim 1, wherein, when the dielectric constant of the dielectric layer is Y and the dielectric constant of the adhesive layer is X, Y is 3.35 or more and 3.85 or less, and X is 2.25 or more and 2.75 or less.
12. A method for manufacturing a printed circuit board, comprising laminating at least one dielectric layer and at least two conductor layers, the conductor layers being positioned as outermost layers, the method comprising the steps of: The conductor layer located at the outermost layer is laminated on the dielectric layer via an adhesive layer, The printed circuit board is manufactured so that the relative permittivity Y of the dielectric layer, the relative permittivity X of the adhesive layer, the thickness t (μm) of the adhesive layer, and the impedance change rate p of the line formed in the conductor layer satisfy the following relational expressions 1 to 3, and the impedance change rate p satisfies 0%<p≦5%. (Relationship 1) X<Y<AX+B (Relationship 2) A = (0.19t 2 -5.25t+43.5)p / 100+1 (Relationship 3) B = (-0.8t + 22) p / 100 A method for manufacturing a printed circuit board comprising the steps of:
13. A method for manufacturing a printed circuit board, comprising laminating at least two dielectric layers and at least three conductor layers, the conductor layers being positioned as outermost layers, comprising: The conductor layer located between the two dielectric layers is laminated to one of the two dielectric layers via an adhesive layer; The printed circuit board is manufactured so that the relative permittivity Y of the dielectric layer, the relative permittivity X of the adhesive layer, the thickness t (μm) of the adhesive layer, and the impedance change rate p when the impedance of the line formed in the conductor layer is compared with that when t = 0 (μm) satisfy the following relational expressions 1 to 4, and the impedance change rate p satisfies 0% < p ≦ 5%. (Relationship 1) X<Y<AX+B (Relationship 2) A = (0.44t 2 -12.8t+108)p / 100+1 (Relational expression 3) B=(-0.2t+26)p / 100 A method for manufacturing a printed circuit board comprising the steps of:
14. A method for manufacturing a printed circuit board, comprising laminating at least two dielectric layers and at least three conductor layers, the conductor layers being positioned as outermost layers, comprising: The two conductor layers located in the outermost layers are laminated on the dielectric layers via adhesive layers, and the conductor layer located between the two dielectric layers is laminated on one of the two dielectric layers via an adhesive layer; The printed circuit board is manufactured so that the relative permittivity Y of the dielectric layer, the relative permittivity X of the adhesive layer, the thickness t (μm) of the adhesive layer, and the impedance change rate p when the impedance of the line formed in the conductor layer is compared with that when t = 0 (μm) satisfy the following relational expressions 1 to 3, and the impedance change rate p satisfies 0% < p ≦ 5%. (Relationship 1) X<Y<AX+B (Relational Expression 2) A = (0.3t 2 - 8.7t + 78)p / 100 + 1 (Relational expression 3) B=(-0.2t+10)p / 100 A method for manufacturing a printed circuit board comprising the steps of:
Citation Information
Patent Citations
Wiring board and circuit device
JP2006303464A
Microstripline structure and its manufacturing method
JP2009016521A
Metal clad laminated plate, circuit board, and multi-layer circuit board
WO2018163999A1
Multilayer printed circuit board and multilayer metal clad laminated board
WO2017130945A1