Carbon fiber reinforced plastic sheet
The CFRP board with specific carbon fiber and resin ratios and lengths addresses dispersion issues, achieving lightweight, high-strength materials for tools and machinery, with reduced waste and improved safety.
Patent Information
- Application Number
- JP2023080436
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-24
- Publication Date
- 2024-11-06
AI Technical Summary
Existing carbon fiber reinforced plastic (CFRP) products face challenges in achieving uniform dispersion and stable quality, particularly in papermaking methods, leading to inconsistent bending strength and weight reduction, while also generating significant waste that needs to be recycled.
A CFRP board composed of 40 to 60 wt% carbon fiber, 60 to 40 wt% phenolic resin, and 5 to 8 wt% aramid fiber, with carbon fibers of 14 to 15 mm length, is produced using a papermaking method to ensure uniform dispersion and strength, enabling weight reduction and comparable tensile load strength to steel.
The CFRP board achieves a lightweight, high-strength material suitable for tools and machinery, with a specific gravity one-fifth that of iron, providing stability and safety in explosive environments, and reducing waste through recycling.
Smart Images

Figure 2024156587000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a carbon fiber reinforced plastic plate (hereinafter abbreviated as CFRP plate) that can be expected to have bending strength equivalent to that of iron or stainless steel and is one-fifth the weight of iron, and relates to improving quality and stable production. [Background technology] [Background technology]
[0002] Conventionally, as an example, Utility Model Registration No. 3233300 (Patent Document 1) has a tensile load strength almost equivalent to that of a hand-held tool made of iron, and it is possible to provide a hand-held tool that is 1 / 4 to 1 / 7 the weight, which is useful for explosion prevention and ensuring safety when working at height. In actual measurements, a comparison of a 3 mm thick recycled carbon fiber and phenolic resin with a 1 mm thick SUS tool showed a bending strength of 502 MPa and 578 MPa, and a tensile load strength of 6433 N and 6400 MPa. Almost equal strength was confirmed. To explain an embodiment of the present invention, carbon fiber cut to a length of 6 mm and phenolic resin are kneaded in a large amount of water in a ratio of 6:4, and then dehydrated to form a raw material. After that, the mixture is dried at 80°C for 3 hours, and then pressurized and heated for molding. The above drying is performed with a moisture content of about 10%, a heating temperature of 140°C, and a 150-ton press is used for 5 minutes to obtain a 5 mm thick molded product. Furthermore, as an invention to maximize strength, a carbon fiber reinforced plastic plate was developed using a paperboard material containing phenolic resin, a thermosetting resin, one or more types of carbon fiber with fiber lengths in the range of 10 mm to 15 mm, and aramid fiber as a binder.The plate achieved a maximum bending strength of 672 MPa and was confirmed to be usable as a substitute for steel. Although this was possible because of the use of the papermaking method, there is a demand for even greater uniformity in dispersion and stability in quality, which is also a difficulty associated with the papermaking method.
[0003] Furthermore, one domestic aircraft manufacturer produces 70 tons of carbon fiber waste per year, making the development of ways to utilize this waste an urgent task. However, the problems of stable production and recycling of waste materials have yet to be solved.
[0004] The problem of weight reduction by using resin instead of metal has been solved by the invention of Utility Model Registration No. 3225768 (Patent Document 2), which is useful as a solution to the above problem. In summary, it is made of carbon fiber reinforced thermoplastic resin and is extremely useful, but from a molding standpoint, it is necessary to use thermoplastic resin. Also, a thermosetting resin on glass fiber has been proposed in Patent No. 2907679 (Patent Document 3). As a conventional example of this proposal, a method of covering the tool surface with carbon fiber epoxy cloth has also been disclosed, but since the strength is only 40% or less of the torque of similar metal products, its use is limited.
[0005] As an example of the use of a papermaking method, there is Patent Application Publication No. 2021-55717 (Patent Document 4), which describes an invention using carbon fiber and resin as a wet papermaking method (corresponding to the papermaking method of the present invention). However, it is described that the length of the carbon fiber used in the wet papermaking method is 1 mm to 50 mm before use, and 1 mm to 3 mm as short fibers at the time of papermaking, and while this achieves abrasion resistance, the bending strength of the present invention cannot be expected. [Prior art documents] [Patent documents]
[0006] [Patent Document 1] Utility Model Registration No. 3233300 [Patent Document 2] Utility Model Registration No. 3225768 [Patent Document 3] Patent Number 2907679 [Patent Document 4] Patent Application Publication No. 2021-55717 Summary of the Invention [Problem to be solved by the invention]
[0007] The present invention is a CFRP plate devised in consideration of the above, which makes it possible to provide products that require strength and lightness by using a molding die.The CFRP plate is characterized in that the component ratio is 40 to 60 wt% of carbon fiber and 60 to 40 wt% of phenolic resin, which is a thermosetting resin, the concentration of aramid fiber as a fixing material is 5 to 8 wt% in the whole, and the fiber length of the carbon fiber is 14 mm to 15 mm. [Means for solving the problem]
[0008] The CFRP plate of the present invention achieves weight reduction by using resin and improved strength by using a papermaking method to provide a CFRP plate of stable quality that is lightweight and has a tensile load strength comparable to that of steel. In addition, considering mass production, the dispersion of carbon fibers is important, and therefore, since it is a papermaking method, it is important that the difference between the maximum and minimum bending strength is small as a criterion for the dispersion of carbon fibers. The present invention specifies the carbon fiber length that can be made uniform by dispersion.
[0009] An example of the CFRP plate of the present invention is a carbon plate shown in FIG. 1, and a tool such as a wrench or spanner shown in FIG.
[0010] The heat insulating member portion of the present invention utilizes a papermaking method, which is a commonly known method and its purpose is to enable efficient fixation of resin to the fibers.
[0011] The CFRP plate of the present invention is made into a 2 mm thick plate by the papermaking method, by kneading 50 wt% carbon fiber, 45 wt% thermosetting phenolic resin, and 5 wt% fixing agent, and forming it into a 50 mm thick base material. It is then dried and molded by hot pressing at 140°C into a 2 mm thick plate. The shape can be determined by measuring the shape of the mold.
[0012] In carrying out the above, the important thing is the fiber length of the carbon fibers. In order to obtain uniform strength, the fiber length is important, and ensuring dispersibility and strength is important in terms of production. As is clear from Fig. 4, only when the fiber length is 14mm and 15mm, the minimum and maximum values of bending strength are large and the difference between them is small, which indicates that dispersion is favorably performed. In the embodiment, the maximum value of bending strength in the case of a fiber length of 14mm is 609.37MPa, the minimum value is 433.21MPa, and those in the case of a fiber length of 15mm are 636MPa and 450.11MPa. The difference between the maximum and minimum is 176.16MPa in the case of a fiber length of 14mm, and 186.78MPa in the case of a fiber length of 15mm. This is an extremely small value compared to the other fiber lengths of 367.25MPa in the case of a fiber length of 12mm and 232.75MPa in the case of a fiber length of 9mm. The maximum value is 609.37MPa in the case of 14mm and 636.89MPa in the case of 15mm, which maintains a strength almost comparable to that of metal, and since the minimum value is large, the difference is small and the variation in strength is small, and stable quality can be maintained.
[0013] In the above embodiment, a 2 mm thick molded product is exemplified, but if the thickness of the hand-held tool is to be 8 mm to 10 mm, the base material is molded to about 100 mm, and after press molding in the same manner as above, it is molded to a thickness of 8 mm to 10 mm. Effect of the Invention
[0014] This makes it possible to provide hand-held tools that have a tensile load strength roughly equivalent to that of iron hand-held tools, but weigh one-quarter to one-seventh as much, which is beneficial for explosion prevention and ensuring safety when working at heights. In terms of actual measurements, the carbon fiber reinforced plastic plate of this invention, made from recycled carbon and phenolic resin, has a bending strength equivalent of 650 MPa for S55C steel and 520 MPa for SUS304, which is roughly equivalent. In addition, the specific gravity of a carbon fiber reinforced plastic plate is 1.5, which is about one-fifth the weight of steel, which is 7.9. [Brief description of the drawings]
[0015] [Figure 1] FIG. 2 is a perspective view of a photograph substituting a drawing, showing an example of a CFRP plate of the present invention. [Diagram 2] 1 is a photograph substituted for a drawing showing another embodiment of a CFRP plate according to the present invention. [Diagram 3] FIG. 1 is a diagram showing a flow of a papermaking method for carrying out the present invention. [Figure 4] 1 is a table showing the results of bending strength tests carried out by changing the fiber length of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0016] To explain an embodiment of the present invention, carbon fiber cut to 15 mm length and phenolic resin are kneaded in a large amount of water at a ratio of 45 wt% to 50 wt% and 5 wt% fixing agent, and then dehydrated to form a base material. After that, it is dried at 80°C for 3 hours and then pressurized and heated for molding. The drying is performed with a moisture content of about 10%, heating temperature is 140°C, and pressing and molding is performed for 5 minutes in a 150 ton press to obtain a 5 mm thick molded product.
[0017] The CFRP plate in Example 1 is a thick plate with a thickness of 5 mm and dimensions of 180 mm x 60 mm, as shown in Figure 1. The shape of the CFRP plate can be changed to tools such as a spanner or ratchet wrench (Figure 2) by changing the shape of the mold. Larger tools can also be manufactured by changing the mold and press machine. The manufacturing method for the CFRP plate uses a papermaking method, as shown in Figure 3.
[0018] This manufacturing method includes 1. a crushing process, 2. a mixing process, 3. a papermaking process, 4. a dehydration press process, 5. a drying process, 6. a punching process, and 7. a press molding process. In the 1. crushing process, carbon fibers are cut to a predetermined fiber length. In the 2. mixing process, the carbon fibers, phenolic resin, and aramid fibers are placed in a container filled with water and dispersed and mixed. In the 3. papermaking process, the mixed liquid is made into a papermaking frame. In the 4. dehydration press process, the mixed liquid made in the papermaking frame is dehydrated, and a base material is formed by a dehydration press. In the 5. drying process, the base material is dried. In the 6. punching process, the dried base material is punched into a desired shape, for example, a plate or a tool shape, with a Thomson blade. In the 7. press molding process, the moisture of the punched base material is adjusted, and the material is pressed by a press machine to complete the molding. The materials of the CFRP plate are phenolic resin, carbon fibers, and aramid fibers. The papermaking method in the papermaking process is a generally known method. The purpose of the papermaking process is to efficiently fix the resin to the fibers. The details of the papermaking method are as shown in JP 2001-123386 A. In this papermaking method, a dispersion water in which heat-resistant fibers are dispersed is stored in a water storage tank having a number of openable and closable drainage holes formed in the bottom surface, the drainage holes in the water storage tank are simultaneously opened to release the dispersion water, a papermaking tank arranged below the water storage tank receives the dispersion water that falls from the water storage tank, and then the water is drained from the papermaking tank, and the heat-resistant fibers are separated by a papermaking net arranged in the papermaking tank.
[0019] The carbon fibers are recycled carbon fibers that are defective products produced before roving and before being impregnated with resin. The manufacturing method of the CFRP plate of Example 1 will be described in detail. 1. In the crushing process, the recycled carbon fibers are cut into fiber lengths of 10 mm and 15 mm. 2. In the mixing process, 5 wt% aramid fiber, 50 wt% phenolic resin, which is a thermosetting resin, and 22.5 wt% each of carbon fiber with a fiber length of 10 mm and carbon fiber with a fiber length of 15 mm are dispersed and mixed in a large amount of water in a container. 3. In the papermaking process, the mixed liquid is papermade in a papermaking frame. 4. In the dehydration press process, the paper-made mixed liquid in the papermaking frame is dehydrated to form a base material. 5. In the drying process, the base material is dried at 80°C for 3 hours. 6. In the punching process, the base material is punched out with a Thomson blade in the shape of the plate material. 7. In the press molding process, the base material is molded under pressure and heat. Drying is performed until the moisture content of the raw material is about 10%. The heating temperature is 140°C, and the material is pressed for 5 minutes in a 150-ton press to obtain a 5 mm thick molded product.
[0020] In the above embodiment, a flat carbon fiber reinforced plastic plate and a wrench are used, but the pressing pressure and time are adjusted depending on the size.
[0021] This invention is not only extremely beneficial in that it has succeeded in making CFRP plate materials lightweight and explosion-proof by using a papermaking method and thermoplastic resins, but also because it can use recycled carbon, it can make a significant contribution to reducing carbon dioxide emissions by eliminating the need for melting at temperatures of several thousand degrees to obtain steel or stainless steel plate materials and tools.
[0022] In addition, in the past, tools were held on the waist when working at height, which could cause back pain due to their weight, but the lightweight design is expected to alleviate this and reduce the risk of serious accidents caused by tools falling. Furthermore, the extremely lightweight design also reduces damage caused by collisions with walls and other objects. [Industrial Applicability]
[0023] The present invention is an extremely excellent new material that can be used in the machinery and tool industries as an alternative to metals, allowing the production of products of stable quality, and is also effective as an environmentally friendly measure, as it is explosion-proof and thus fire-preventive, and has significant benefits such as weight reduction.
Claims
[Claim 1] A carbon fiber reinforced plastic plate comprising carbon fiber, a phenolic resin which is a thermosetting resin component, and aramid fiber as a fixing material, the carbon fiber having a fiber length of 14 mm to 15 mm.
Citation Information
Patent Citations
Fiber base material for friction material, and friction material using the same
JP2021055717A
composite hand tools
JP2907679B2
Adjustable wrench
JP3225768U
Hand tools
JP3233300U