Laminate and package
A polyolefin resin laminate with integrated laser-absorbing materials allows for easy cutting and tearing of monomaterial packages, addressing recyclability and opening challenges in single-resin polyethylene containers.
Patent Information
- Application Number
- JP2024135575
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2024-08-15
- Publication Date
- 2024-11-06
- Estimated Expiration
- 2041-09-21
AI Technical Summary
Plastic containers and packaging made from multiple types of resins are difficult to recycle, and single-resin polyethylene containers have low laser absorption, making it challenging to form half-cut lines for easy opening.
A laminate composed of a polyolefin resin sealant layer and base material layer, with laser-absorbing materials integrated into the base layer, allowing cuts to be formed by laser irradiation without penetrating the sealant layer, enhancing manual tearability.
The laminate and package achieve excellent manual tearability while being made of monomaterial, facilitating recycling and easy opening without the need for knives.
Smart Images

Figure 2024156998000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a laminate and a package. [Background technology]
[0002] Paragraph 0010 of Patent Document 1 describes a laminated film, which is a film conventionally used for packaging bags, in which a polyolefin resin such as low-density polyethylene, linear low-density polyethylene, ethylene-vinyl acetate copolymer, polypropylene, etc. is laminated as a sealant layer on a base film such as biaxially oriented polypropylene, biaxially oriented polyamide, biaxially oriented polyester, etc. Furthermore, paragraph 0014 of Patent Document 1 describes forming a half-cut line by a laser. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2013-39932 A Summary of the Invention [Problem to be solved by the invention]
[0004] In recent years, there has been a problem with the recovery of plastic containers and packaging after use, in that packaging bags containing two or more types of resin are difficult to recycle as plastic containers and packaging. To facilitate recycling, mono-material containers and packaging using a single resin have been proposed. As a single resin, polyethylene resin is inexpensive and easy to process, but it has low absorption of energy rays, so it is difficult to form a half-cut line even when irradiated with a laser.
[0005] The present invention has been made in consideration of the above circumstances, and an object of the present invention is to provide a laminate and a package that are monomaterial yet have excellent hand-tearability. [Means for solving the problem]
[0006] In order to solve the above-mentioned problems, the present invention provides a laminate having a sealant layer formed from a polyolefin-based resin and a base layer formed from a polyolefin-based resin, characterized in that a cut is formed by removing at least a portion of the base layer in the thickness direction by laser irradiation without penetrating the laminate in the thickness direction.
[0007] The polyolefin resin may be a polyethylene resin. The cut may be formed from the side of the base layer to a part of the layer adjacent to the sealant layer in the thickness direction. The laminate may have a stretched polyethylene resin layer, and the cut may be formed from the side of the base layer to the stretched polyethylene resin layer. At least a portion of the sealant layer may contain an absorber for the laser. At least a portion of the base layer may contain an absorbent for the laser. A coating layer or printing layer containing the laser absorbent may be formed on at least the location where the cut is to be formed on the outermost surface of the laminate, which is the opposite side to when the sealant layer becomes the innermost layer of the laminate. The layer adjacent to the sealant layer may be a stretched polyethylene resin layer. In the base layer, the polyethylene resin layer may be laminated with the ethylene-vinyl alcohol copolymer layer by coextrusion.
[0008] A metal vapor deposition layer may be formed on the surface of the base layer facing the sealant layer. The substrate layer may have a first substrate layer disposed on a side closer to the sealant layer in the thickness direction of the laminate, and a second substrate layer disposed on a side farther from the sealant layer, the first substrate layer being a stretched polyethylene resin layer, and a metal vapor deposition layer may be formed on a surface of the first substrate layer facing the second substrate layer. The oriented polyethylene resin layer of the first base material layer may be a biaxially oriented polyethylene resin layer. The first base layer may have a thickness of 40 μm or less. The sealant layer and the base layer may be laminated via an adhesive layer that absorbs the laser.
[0009] The present invention also provides a package formed from the laminate. The package may be a refill pouch. Effect of the Invention
[0010] According to the present invention, it is possible to provide a laminate and a package that are excellent in hand tearability despite being a mono-material. [Brief description of the drawings]
[0011] [Figure 1] 1 is a cross-sectional view illustrating a laminate according to a first embodiment. [Diagram 2] FIG. 11 is a cross-sectional view illustrating a laminate according to a second embodiment. [Diagram 3] FIG. 11 is a cross-sectional view illustrating a laminate according to a third embodiment. [Figure 4] FIG. 13 is a cross-sectional view illustrating a laminate according to a fourth embodiment. [Diagram 5] FIG. 13 is a cross-sectional view illustrating a laminate according to a fifth embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] Hereinafter, the present invention will be described based on preferred embodiments. The laminate of the embodiment has a sealant layer formed of a polyolefin resin and a base layer formed of a polyolefin resin. A cut is formed by removing at least a part of the base layer in the thickness direction by irradiating a laser without penetrating the laminate in the thickness direction.
[0013] The laser is not particularly limited as long as it is a laser used for resin processing of films, etc., and examples thereof include solid-state lasers, gas lasers, fiber lasers, semiconductor lasers, excimer lasers, etc. The wavelength of the laser may be any of the infrared region, the visible light region, and the ultraviolet region. For example, a CO2 laser is preferable because it has an output wavelength of about 9 to 11 μm, which is a relatively long wavelength in the infrared region, and has excellent resin processability.
[0014] When a film is irradiated with a long-wavelength laser, the film heats up locally at the irradiated area, removing part of the resin. By removing a narrow width of resin, a linear cut is formed. The cut may be a continuous line in the length direction, or a broken or dotted line that is discontinuous in the length direction. The cut may be linear in the length direction, or it may be curved or bent.
[0015] Polyolefin resins such as polyethylene resins have a relatively simple molecular structure, and therefore have a limited infrared absorption wavelength band, making it difficult to absorb laser energy. However, since polyolefin resins have a relatively low melting point, once energy is absorbed into the material, it is relatively easy to process, such as melting and cutting. Therefore, by disposing a laser-absorbing material in or near the polyethylene resin layer, the polyethylene resin layer can be easily processed.
[0016] Conventional laminated films use PET film or the like as a base layer, so the PET film absorbs the laser, making it easy to form cuts such as half-cut lines in the laminated film. However, in the case of mono-material materials that mainly consist of polyolefin resin layers, it is necessary to arrange a material that absorbs the laser depending on the position and depth of the cut.
[0017] Next, a laminate 10 of a first embodiment will be described with reference to Fig. 1. This laminate 10 is formed by laminating a sealant layer 11 made of a polyolefin resin and a base layer 12 made of a polyolefin resin via an adhesive layer 13, and the base layer 12 has a slit 14 formed by removing at least a part of the base layer 12 in the thickness direction by laser irradiation. The slit 14 may be open on the outer surface of the base layer 12.
[0018] At least a portion of the base layer 12 contains a laser-absorbing agent, so that a slit 14 can be formed in the base layer 12. The resin layer containing the laser-absorbing agent in the base layer 12 can be formed from a polyolefin resin such as a polyethylene resin or a polypropylene resin. When the base layer 12 has two or more polyolefin resin layers, at least one of the layers should be a polyolefin resin layer containing a laser-absorbing agent. By providing the slit 14, it is possible to impart easy cutting by tearing and hand cutting properties without using a blade.
[0019] The laser absorbing agent is not particularly limited, but examples thereof include carbon-based materials such as carbon black, inorganic materials such as titanium oxide and iron oxide, coloring materials such as pigments and dyes, and resin materials such as acrylic resins and polyester resins. When a laser absorbing agent is blended into the polyolefin resin layer, the laser absorbing agent may be in a powder form and melt-kneaded.
[0020] The depth of the cut 14 can be adjusted as appropriate, and the cut 14 may be formed only in a portion of the thickness direction of the base material layer 12, or the cut 14 may reach the adhesive layer 13. The sealant layer 11 may be formed of a polyethylene resin layer that does not contain a laser absorbent so that the cut 14 does not penetrate the sealant layer 11. In this case, when the cut 14 reaches the sealant layer 11 by laser irradiation, the laser passes through the sealant layer 11, so that processing of the sealant layer 11 can be suppressed.
[0021] In order to suppress the laser from passing through the sealant layer 11, at least a part of the sealant layer 11 may contain a laser absorbing agent. The resin layer containing the laser absorbing agent in the sealant layer 11 can be formed from a polyolefin resin such as a polyethylene resin or a polypropylene resin. When the sealant layer 11 has two or more polyolefin resin layers, at least one of the layers may be a polyolefin resin layer containing a laser absorbing agent. This can prevent the laser irradiated from the substrate layer 12 side from passing through the sealant layer 11 and acting on unintended locations.
[0022] The sealant layer 11 is preferably formed from a sealant resin. Examples of the sealant resin include polyethylene-based resins having relatively low density, such as linear low-density polyethylene (LLDPE) and low-density polyethylene (LDPE), non-oriented polyethylene-based resins, polypropylene-based resins, etc. The sealant layer 11 may be formed from one type of polyolefin-based resin, or may contain two or more types of polyolefin-based resins.
[0023] The thickness of the sealant layer 11 is not particularly limited, but may be, for example, about 50 to 180 μm. The sealant layer 11 may be a single-layer sealant film or a multi-layer sealant film. The multi-layer sealant film can be formed by laminating two or more layers of film-like sealant resin by co-extrusion, extrusion lamination, sandwich lamination, thermal lamination, or the like. The multi-layer sealant film may also include a resin layer such as EVOH.
[0024] The base layer 12 may be a polyolefin resin layer stretched by biaxial stretching, uniaxial stretching, or the like, or may be a non-stretched polyolefin resin layer. Examples of the base layer 12 include polyethylene resins having relatively high density, such as medium density polyethylene (MDPE) and high density polyethylene (HDPE), and polypropylene resins. The base layer 12 may be formed from one type of polyolefin resin, or may contain two or more types of polyolefin resins. The thickness of the base layer 12 is not particularly limited, but may be, for example, about 10 to 50 μm. The base layer 12 may have a multilayer structure. The multilayer base layer 12 can be formed by laminating two or more resin layers by a coextrusion method, an extrusion lamination method, a sandwich lamination method, a thermal lamination method, or the like, without using an adhesive. The structure in which a plurality of base layers are laminated via an adhesive layer will be described later.
[0025] The polyethylene-based resin used in the sealant layer 11 or the base layer 12 may be a homopolymer of ethylene or a copolymer mainly composed of ethylene. Examples of monomers (comonomers) other than ethylene include one or more of α-olefins such as 1-butene, 1-hexene, and 1-octene, cyclic olefins such as norbornene, and vinyl monomers such as vinyl acetate, vinyl chloride, and acrylic acid. When a comonomer is used in the polyethylene-based resin, the comonomer may be one or two or more.
[0026] The proportion of ethylene in the constituent monomers of the polyethylene resin is preferably 50% by weight or more, and may be, for example, 80 to 100% by weight. The ethylene or comonomer used in the polyethylene resin may be a compound derived from a fossil resource such as petroleum, or a compound derived from biomass such as plants. The material forming the polyethylene resin layer may be one type of polyethylene resin, or a blend of two or more types of polyethylene resins. The polyethylene resin layer may contain recycled polyethylene.
[0027] A polypropylene (PP)-based resin may be used for the sealant layer 11 or the base layer 12. The polypropylene-based resin may be a homopolymer of propylene (homo PP), or a random copolymer (random PP) or block copolymer (block PP) of a propylene-ethylene copolymer or the like. Examples of monomers (comonomers) other than propylene include one or more of α-olefins such as ethylene, 1-butene, 1-hexene, and 1-octene, and vinyl monomers such as vinyl acetate, vinyl chloride, and acrylic acid. When a comonomer is used in the polypropylene-based resin, the comonomer may be one or more of the following: The proportion of propylene in the constituent monomers of the polypropylene-based resin is preferably 50% by weight or more, and may be, for example, 80 to 100% by weight. The polypropylene-based resin layer may contain recycled polypropylene.
[0028] The resin contained in the sealant layer 11 or the base layer 12 may be only a polyolefin-based resin, only a polyethylene-based resin, or only a polypropylene-based resin. The sealant layer 11 or the base layer 12 may contain additives other than resin. The additives are not particularly limited, but examples thereof include antioxidants, lubricants, antiblocking agents, flame retardants, ultraviolet absorbers, light stabilizers, antistatic agents, colorants, crosslinking agents, and the like. The additives may be components that are compatible with the resin, or components that are not compatible with the resin.
[0029] The sealant layer 11 and the base layer 12 may be bonded together via an adhesive layer 13 by dry lamination or the like. Although not particularly shown, extrusion lamination, thermal lamination, or the like may be used without interposing the adhesive layer 13 between the sealant layer 11 and the base layer 12. At least one of the sealant layer 11 and the base layer 12 may be subjected to a surface treatment such as ozone treatment, plasma treatment, corona treatment, discharge treatment, flame treatment, or the like.
[0030] The adhesive layer 13 may be formed from an adhesive or an anchor coating agent. The material for forming the adhesive layer 13 is not particularly limited, but may include urethane compounds, epoxy compounds, isocyanate compounds, polyethyleneimine, and organic titanium compounds such as titanium alkoxide. The thickness of the adhesive layer 13 may be, for example, about 0.1 to 10 μm, about 1 to 6 μm, or about 3 to 4 μm. The adhesive layer 13 may contain a resin, or may be an adhesive layer that does not contain a resin.
[0031] The adhesive layer 13 may absorb the laser in order to form a slit 14 in the base layer 12 and suppress transmission of the laser through the sealant layer 11. The material such as the adhesive may have a structure that absorbs the laser, or the above-mentioned laser absorbing agent may be added to the material such as the adhesive. It is preferable that the laminate 10 has at least one laser absorbing layer selected from the sealant layer 11 that absorbs the laser, the base layer 12 that absorbs the laser, and the adhesive layer 13 that absorbs the laser.
[0032] Next, a laminate 20 of a second embodiment will be described with reference to Fig. 2. In this laminate 20, a sealant layer 21, a first base material layer 22, and a second base material layer 23, each made of a polyolefin resin, are laminated via adhesive layers 24, 25, and a cut 26 is formed by removing at least a part of the thickness direction from the second base material layer 23 to the first base material layer 22 by laser irradiation. In the thickness direction of the laminate 20, the first base material layer 22 is disposed on the side closer to the sealant layer 21, and the second base material layer 23 is disposed on the side farther from the sealant layer 21.
[0033] At least one of the first base material layer 22 and the second base material layer 23 has a polyolefin resin layer containing a laser absorbent, so that the cut 26 can be formed in the base material layers 22 and 23. The cut 26 may be formed continuously in the adhesive layer 25 between the first base material layer 22 and the second base material layer 23. The depth of the cut 26 can be appropriately adjusted, and the cut 26 may be formed only in a part of the thickness direction of the first base material layer 22, or the cut 14 may reach the adhesive layer 24. It is preferable that the cut 26 penetrates the second base material layer 23. In the illustrated example, the cut 26 is formed from the second base material layer 23 side to a part of the thickness direction of the first base material layer 22, which is a resin layer adjacent to the sealant layer 11. As in the first embodiment, the cut 26 may not penetrate the sealant layer 21, or the laser may not pass through the sealant layer 21.
[0034] The laminate 20 of the second embodiment can be manufactured in the same manner as the laminate 10 of the first embodiment, except that it has two each of the base layers 22, 23 and the adhesive layers 24, 25. The material of the sealant layer 21 may be the same as that of the sealant layer 11 of the first embodiment. The material of the base layers 22, 23 may be the same as that of the base layer 12 of the first embodiment. The material of the adhesive layers 24, 25 may be the same as that of the adhesive layer 13 of the first embodiment.
[0035] Although not particularly shown, in the laminate 10, 20 of the first or second embodiment, a printed layer may be provided on one or both sides of the base layer 12, 22, 23. The printed layer can be formed by printing ink in a solid or patterned manner using a printing method such as gravure printing, letterpress printing, offset printing, screen printing, inkjet printing, etc. The thickness of the printed layer is not particularly limited, but may be about 0.5 to 10 μm. The printed layer may be formed on the entire surface of the base layer 12, 22, 23, or may be formed on a part of the surface. Two or more printed layers may be overlapped. The printed layer may be omitted.
[0036] It is preferable that the total of the specific resins is 80% by weight or more and the total of the materials other than the specific resins is 20% by weight or less, and it is more preferable that the total of the specific resins is 90% by weight or more and the total of the materials other than the specific resins is 10% by weight or less, based on the total weight of the laminate 10, 20 of the first or second embodiment. This makes it possible to realize a mono-material material of the specific resin even if a laser absorbent, adhesive, etc. is used in the laminate 10, 20. Examples of the specific resin include polyolefin resin, polyethylene resin, or polypropylene resin. The laminate 10, 20 may use two or more resins that correspond to the specific resin.
[0037] Next, a laminate 30 of a third embodiment will be described with reference to Fig. 3. In this laminate 30, a sealant layer 31 formed from a polyolefin resin and a base layer 32 formed from a polyolefin resin are laminated via an adhesive layer 33. A laser absorbing layer 34 containing a laser absorbing agent is formed on the outer surface of the base layer 32, and a cut 35 is formed in the base layer 32 by removing at least a part of the base layer 32 in the thickness direction by laser irradiation. The outer surface of the base layer 32 is the outermost surface of the laminate 30 when the sealant layer 31 is the innermost layer.
[0038] The laser absorbing layer 34 may be a coating layer formed from a varnish or the like. A heat-resistant varnish capable of forming the laser absorbing layer 34 by drying, curing, etc. after coating is preferred. The varnish may contain a resin and a solvent, or may contain a solventless resin. The solvent of the varnish may be appropriately selected in consideration of the performance when applied to a polyethylene resin. A powdered laser absorbent may be blended into the varnish. The resin forming the varnish is not particularly limited, but examples thereof include one or more of urethane resin, acrylic resin, epoxy resin, polymethylpentene resin, cyclic olefin resin, unsaturated polyester resin, alkyd resin, polyimide resin, polyamideimide resin, polyamide resin, etc.
[0039] The laser absorbing layer 34 may be a printing layer formed from a printing ink or the like. The ink for forming the printing layer may contain a coloring material such as a pigment or a dye, and a binder. Examples of the binder include, but are not limited to, polyamide, polyurethane, polyester, polyvinyl chloride, polyvinyl acetate, vinyl chloride-vinyl acetate copolymer, acrylic polymer, polybutadiene, cyclized rubber, and the like. The ink may contain a solvent such as water, an organic solvent, or vegetable oil. After printing, the ink can be dried by volatilization of the solvent, hardening of the ink, and the like. Heating, ultraviolet irradiation, and the like may be performed to promote drying of the ink.
[0040] The laminate 30 of the third embodiment can be produced in the same manner as the laminate 10 of the first embodiment, except that it has a laser absorbing layer 34. The configurations of the sealant layer 31, the base layer 32, and the adhesive layer 33 may be the same as those of the sealant layer 11, the base layer 12, and the adhesive layer 13 of the first embodiment, respectively.
[0041] In the laminate 30 of the third embodiment, the sealant layer 31 and the base layer 32 may or may not contain a laser absorbing agent. When the laser absorbing layer 34 generates heat by laser irradiation, at least a part of the base layer 32 is removed to form a gap 35. When the base layer 32 contains a laser absorbing agent, the base layer 32 is also heated and removed by laser irradiation to form a gap 35.
[0042] The substrate layer 32 may be two or more layers, but when the substrate layer 32 does not contain a laser absorbing agent, it is preferable that the substrate layer 32 is one layer and is a resin layer stretched by biaxial stretching, uniaxial stretching, or the like. In the illustrated example, a slit 35 is formed up to a part of the thickness direction of the substrate layer 32, which is a resin layer adjacent to the sealant layer 31. Since the slit 35 is formed by heat generation of the laser absorbing layer 34, the substrate layer 32 does not need to contain a laser absorbing agent, and therefore the substrate layer 32 can be easily stretched. By using a resin film stretched by biaxial stretching, uniaxial stretching, or the like, which has high dimensional stability, for the substrate layer 32, it becomes easy to form the laser absorbing layer 34 on the substrate layer 32 by coating or printing.
[0043] The laser absorbing layer 34 may be formed in a pattern in the area where the cut 35 is formed in the plane of the laminate 30. For example, when the cut 35 is formed in a line, the laser absorbing layer 34 may be formed in a line or strip including the width and length of the cut 35. The pattern of the laser absorbing layer 34 is not particularly limited, and may be the entire surface of the laminate 30 or a partial area such as a line, strip, zigzag, polygonal, or circular shape. The pattern coating or printing may be performed by gravure printing. When the laser absorbing layer 34 is visible due to coloring or the like, an indication regarding the cut 35 may be created together with characters or a design.
[0044] Next, a laminate 40 of a fourth embodiment will be described with reference to Fig. 4. This laminate 40 includes a sealant layer 41, a first resin layer 42, and a second resin layer 43, each of which is made of a polyolefin resin, laminated together, and a cut 46 is formed by removing at least a part of the thickness direction from the second resin layer 43 to the first resin layer 42 by laser irradiation. The sealant layer 41 and the first resin layer 42 are laminated together with an adhesive layer 44 interposed therebetween. The first resin layer 42 and the second resin layer 43 are laminated together with a laser absorbing layer 45 interposed therebetween.
[0045] At least one of the resin layers 42 and 43 may be a base material layer. The first resin layer 42 may be a first base material layer, and the second resin layer 43 may be a second base material layer. The second resin layer 43 may be a base material layer, and the first resin layer 42 may be an intermediate resin layer interposed between the base material layer and the sealant layer.
[0046] The laser absorbing layer 45 may be formed from a resin that can be co-extruded with the polyethylene resin of the resin layers 42 and 43 and has laser absorbing properties. An example of such a resin is ethylene-vinyl alcohol copolymer (EVOH). When the polyethylene resin and the EVOH resin layer are laminated by co-extrusion, the EVOH resin layer can be formed thin, and the recyclability of the polyethylene resin can be maintained. In addition, the EVOH resin layer can impart barrier properties. In this case, the substrate may be a substrate in which three layers, the resin layers 42 and 43 and the laser absorbing layer 45, are co-extruded.
[0047] EVOH can be obtained by copolymerizing ethylene with a vinyl ester monomer, saponifying the resulting copolymer, and converting the vinyl ester units to vinyl alcohol units. Examples of the vinyl ester monomer include vinyl carboxylates such as vinyl formate, vinyl acetate, vinyl butyrate, and vinyl benzoate. The greater the proportion of vinyl alcohol units in EVOH, the more improved the barrier properties are, but the lower the moisture resistance is. Therefore, it is preferable that EVOH has an appropriate ethylene content. Examples of the ethylene content of EVOH include 20 to 60 mol%. The degree of saponification of EVOH is not limited to 100 mol%, but is preferably 80 mol% or more, for example.
[0048] The laser absorbing layer 45 between the first resin layer 42 and the second resin layer 43 may be a printed layer formed from a printing ink, similar to the laser absorbing layer 34 of the third embodiment. A printed layer may be formed on the outer surface of the first resin layer 42, and the printed layer on the first resin layer 42 side and the second resin layer 43 may be bonded with an adhesive layer (not shown). A printed layer may be formed on the inner surface of the second resin layer 43, and the printed layer on the second resin layer 43 side and the first resin layer 42 may be bonded with an adhesive layer (not shown). The resin layers 42 and 43 on which the printed layer is formed are preferably base material layers.
[0049] The laminate 40 of the fourth embodiment can be manufactured in the same manner as the laminate 20 of the second embodiment, except that it has a laser absorbing layer 45. The sealant layer 41, the first resin layer 42, the second resin layer 43, and the adhesive layer 44 may have the same configurations as the sealant layer 21, the first base material layer 22, the second base material layer 23, and the adhesive layers 24 and 25 of the second embodiment, respectively.
[0050] A further resin layer may be provided between the first resin layer 42 and the sealant layer 41. For example, in order to improve the hand-cuttability of the laminate 40, it is preferable to provide a stretched polyethylene-based resin layer stretched by biaxial stretching, uniaxial stretching, or the like. The second resin layer 43 may be a base layer, and the first resin layer 42 may be a stretched polyethylene-based resin layer. It is preferable that a slit is formed from the base layer side to the stretched polyethylene-based resin layer. A resin layer such as a non-stretched polyethylene-based resin layer may be laminated between the stretched polyethylene-based resin layer having the slit 46 and the sealant layer 41 by extrusion or the like. In this case, the slit 46 may not reach the resin layer such as the non-stretched polyethylene-based resin layer. The resin layer included in the laminate 40 may include four types of layers in order: a base layer, a stretched polyethylene-based resin layer, a non-stretched polyethylene-based resin layer, and a sealant layer. The adhesive layer 44 may be omitted, and a laminate may be formed in the order of the second resin layer 43 of the base material layer, the laser absorbing layer 45, the first resin layer 42 of the stretched polyethylene-based resin, the unstretched polyethylene-based resin layer, and the sealant layer 41. When the base material layer or the stretched polyethylene-based resin layer contains a laser absorbing agent, the laser absorbing layer 45 between the layers may be omitted.
[0051] In addition, a stretched polyethylene resin layer stretched by biaxial stretching, uniaxial stretching, or the like may be used as the first resin layer 42 adjacent to the sealant layer 41, and a laminate may be formed in which the second resin layer 43 of the base material layer / laser absorbing layer 45 / first resin layer 42 of stretched polyethylene resin / adhesive layer 44 / sealant layer 41 are laminated in this order. In addition, the adhesive layer 44 may be omitted, and a laminate may be formed in which the second resin layer 43 of the base material layer / laser absorbing layer 45 / first resin layer 42 of stretched polyethylene resin / sealant layer 41 are laminated in this order. In these examples, the resin layer adjacent to the sealant layer 41 is a single layer stretched polyethylene resin layer. In the illustrated example, a cut 46 is formed from the second resin layer 43 side of the base material layer to a part of the first resin layer 42 adjacent to the sealant layer 41 in the thickness direction.
[0052] Next, a laminate 50 of a fifth embodiment will be described with reference to Fig. 5. This laminate 50 has a sealant layer 51, a first base material layer 52, and a second base material layer 53, each formed from a polyolefin resin. The sealant layer 51 and the first base material layer 52 are laminated with an adhesive layer 54 interposed between them. A metal vapor deposition layer 55 is formed on the outer surface of the first base material layer 52, and the metal vapor deposition layer 55 and the second base material layer 53 are laminated with an adhesive layer 56 interposed between them.
[0053] The metal deposition layer 55 is a laser reflective layer, and therefore can suppress penetration of the laser into the sealant layer 51 and the first base layer 52. The metal deposition layer 55 can be formed thin to maintain the recyclability of the polyolefin resin. The metal deposition layer 55 can also impart barrier properties. The metal to be deposited is not particularly limited, and examples thereof include metals such as aluminum (Al), titanium (Ti), zinc (Zn), tin (Sn), and chromium (Cr), or alloys thereof.
[0054] When forming the metal vapor deposition layer 55 on the first base layer 52, in order to control the deposition, the first base layer 52 is preferably a stretched polyethylene resin layer. The metal vapor deposition layer 55 may be formed on a single film of the first base layer 52. The metal vapor deposition layer 55 may be formed on the first base layer 52 of a multilayer film laminated with the sealant layer 51 via the adhesive layer 54. The stretched polyethylene resin layer of the first base layer 52 may be a uniaxially stretched resin layer or a biaxially stretched resin layer.
[0055] The stretching direction of the stretched polyethylene-based resin layer in the first base layer 52 and the like is not particularly limited, and may be the machine (MD) direction or the cross (TD) direction. Biaxial stretching in the MD and TD directions is also possible. The stretching ratio may be, for example, about 2 to 10 times. The stretching direction in the uniaxial or biaxial stretching may be an oblique direction crossing the MD and TD directions. The stretched polyethylene-based resin layer is preferably HDPE, MDPE, LLDPE, or LDPE, and more preferably LLDPE.
[0056] The second base layer 53 disposed on the outside of the metal deposition layer 55 may contain a laser absorbing agent. The first base layer 52 disposed on the inside of the metal deposition layer 55 may not contain a laser absorbing agent. The thickness of the first base layer 52 may be 40 μm or less, and more preferably 25 μm or less. This ensures hand-cuttability when the cut 57 does not reach the first base layer 52. When the first base layer 52 is a uniaxially stretched resin layer, the direction of uniaxial stretching can be aligned with the direction of the cut 57 to facilitate breaking along the cut 57.
[0057] The laminate 50 of the fifth embodiment can be produced in the same manner as the laminate 20 of the second embodiment, except that it has a metal vapor deposition layer 55. The sealant layer 51, the first base material layer 52, the second base material layer 53, and the adhesive layers 54 and 56 may have the same configurations as the sealant layer 21, the first base material layer 22, the second base material layer 23, and the adhesive layers 24 and 25 of the second embodiment, respectively.
[0058] Although not particularly shown, in the laminate 50 of the fifth embodiment, the first base material layer 52 and the adhesive layer 56 may be omitted, and the layers may be laminated in the order of sealant layer 51 / adhesive layer 54 / metal vapor deposition layer 55 / base material layer 53. In this manner, by forming the metal vapor deposition layer 55 on the surface of the base material layer 53 facing the sealant layer 51, a cut 57 is formed in the base material layer 53, and it is possible to suppress transmission of the laser through the sealant layer 51. Two or more base material layers 53 may be laminated on the outer side of the metal vapor deposition layer 55. A resin layer may be further provided between the metal vapor deposition layer 55 and the sealant layer 51.
[0059] The laminates 10, 20, 30, 40, 50 of the above-mentioned embodiments are in the form of laminated films mainly made of polyolefin resins, and can be used for various applications. The method of forming the laminated film is not particularly limited, and examples thereof include dry lamination, extrusion lamination, heat lamination, co-extrusion, and coating. Different methods may be used to laminate each layer. The sealant layers 11, 21, 31, 41, 51 can be placed face to face and the laminates 10, 20, 30, 40, 50 can be joined by fusion.
[0060] The laminate of the embodiment can be used to produce a package. At least one member of the package may be formed from the laminate of the embodiment. Examples of the package include packaging bags such as pouches and bags, tubes, containers, sleeve packaging, strip packaging, and lids. Specific examples of packaging bags include three-sided sealed bags, four-sided sealed bags, pillow bags, gusset bags, and standing pouches. When the laminate is a flexible laminate film, a soft packaging package can be formed. Since it is easy to refill and dispose of, it can be suitably used for refill packaging such as refill pouches.
[0061] The package may have a filling port, a pouring port, etc. For example, an opening may be formed between the front and rear body members at the top of the package, which can be used for filling or pouring the contents. After filling the contents, the body members may be joined to seal the package. The pouring port may be formed in a thin protruding shape at the top or corner of the package.
[0062] The non-through cuts 14, 26, 35, 46, and 57 are preferably formed so as to cross the body or the spout of the package. The process of forming the cuts 14, 26, 35, 46, and 57 may be performed on the laminates 10, 20, 30, 40, and 50 before the bag is made, or may be performed on the package after the bag is made.
[0063] In order to facilitate opening of the package, a cutout portion penetrating the laminate, such as a notch, may be formed around the opening portion in addition to the non-penetrating cuts 14, 26, 35, 46, 57 described above in the opening portion. The cutout portion penetrating the laminate is formed in the seal portion where the inner surface of the laminate is joined in order to ensure the hermeticity of the package.
[0064] The dimensions of the package are not particularly limited. For example, when used as a refill container, the height in the vertical direction is about 100 to 500 mm, the width in the horizontal direction is about 70 to 300 mm, and the filling amount is about 100 cm 3 ~5000cm 3 The state of the contents may be a fluid such as a liquid, a powder, or a granule. The type of contents may be, but is not limited to, a detergent, a medicine, a cosmetic, a pharmaceutical, a beverage, a seasoning, an ink, a paint, a fuel, or the like.
[0065] The packaging body may be formed only from the laminate 10, 20, 30, 40, 50 of the embodiment, or may be combined with accessories such as a label, a tag, a straw, an outer box, etc. From the viewpoint of recycling, it is preferable that the accessories can be separated from the packaging body.
[0066] Although the present invention has been described above based on the preferred embodiment, the present invention is not limited to the above embodiment, and various modifications can be made without departing from the spirit of the present invention. Modifications include addition, substitution, omission, and other changes of components. [Explanation of symbols]
[0067] 10, 20, 30, 40, 50...Laminate 11, 21, 31, 41, 51…Sealant layer 12,22,23,32,52,53…Base material layer 13,24,25,33,44,54,56...adhesive layer 14,26,35,46,57...Gap 34,45...Laser absorbing layer 42, 43…Resin layer 55...Metal deposition layer
Claims
1. A laminate having a sealant layer formed from a polyolefin-based resin and a base layer formed from a polyolefin-based resin, characterized in that a cut is formed by removing at least a portion of the base layer in the thickness direction by irradiating the laser without penetrating the laminate in the thickness direction.
2. 2. The laminate according to claim 1, wherein the polyolefin resin is a polyethylene resin.
3. 3. The laminate according to claim 1, wherein the slit is formed from the side of the base material layer to a part of the layer adjacent to the sealant layer in the thickness direction.
4. The laminate according to any one of claims 1 to 3, characterized in that the laminate has a stretched polyethylene-based resin layer, and the slit is formed from the side of the base material layer to the stretched polyethylene-based resin layer.
5. 5. The laminate according to claim 1, wherein at least a portion of the sealant layer contains an absorbent for the laser.
6. 6. The laminate according to claim 1, wherein at least a portion of the base layer contains an absorbent for the laser.
7. The laminate according to any one of claims 1 to 6, characterized in that a coating layer or a printing layer containing the laser absorbent is formed at least at a location where the cut is to be formed on the outermost surface of the laminate, which is opposite to when the sealant layer becomes the innermost layer of the laminate.
8. 8. The laminate according to claim 1, wherein the layer adjacent to the sealant layer is a layer of a stretched polyethylene resin.
9. 9. The laminate according to claim 1, wherein in the base layer, the polyethylene-based resin layer is laminated with the ethylene-vinyl alcohol copolymer layer by coextrusion.
10. 10. The laminate according to claim 1, further comprising a metal vapor deposition layer formed on a surface of the base layer facing the sealant layer.
11. The laminate according to any one of claims 1 to 9, characterized in that the base layer has a first base layer arranged on a side closer to the sealant layer in a thickness direction of the laminate, and a second base layer arranged on a side farther from the sealant layer, the first base layer being a stretched polyethylene-based resin layer, and a metal vapor deposition layer being formed on a surface of the first base layer facing the second base layer.
12. 12. The laminate according to claim 11, wherein the oriented polyethylene resin layer of the first base layer is a biaxially oriented polyethylene resin layer.
13. 13. The laminate according to claim 11, wherein the first base layer has a thickness of 40 μm or less.
14. The laminate according to any one of claims 1 to 13, wherein the sealant layer and the base layer are laminated via an adhesive layer that absorbs the laser.
15. A package formed from the laminate according to any one of claims 1 to 14.
16. 16. The package of claim 15, which is a refill pouch.
Citation Information
Patent Citations
Easily unsealable laminous packaging material
JP1996183133A
Co-extruded multilayer film
JP2002036444A
Method for forming easy unsealing means, and pouch with easily unsealing means
JP2003040285A
Laminate for hand tearable package having sealant layer containing plant-derived polyethylene
JP2020049837A
Film, packaging bag constituted of film, laminate comprising film and packaging bag constituted of laminate
JP2020203408A