Towel cloth and manufacturing method thereof

The use of silospan spun yarn with opposite-direction secondary twist addresses pile raising and texture issues in towel fabrics, providing softness, puffiness, and enhanced water absorbency, with reduced environmental and production costs.

JP2024157230AActive Publication Date: 2024-11-07IZAWA TOWEL CO LTD
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
JP2023071472
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-25
Publication Date
2024-11-07
Estimated Expiration
2043-04-25

AI Technical Summary

Technical Problem

Conventional towel fabrics face issues with pile raising property and soft, puffy texture, and there is a need for improved water absorbency.

Method used

The towel fabric uses silospan spun yarn as warp pile yarn, which is non-twisted or lightly twisted with a secondary twist in the opposite direction to the primary twist, anchored to warp and weft yarns, enhancing napping properties and water absorbency.

Benefits of technology

The fabric achieves good pile standing, soft and plump texture, and improved water absorbency, with reduced environmental impact and cost, while maintaining texture durability through fiber intertwining and absence of water-soluble fibers.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024157230000001_ABST
    Figure 2024157230000001_ABST
Patent Text Reader

Abstract

To provide a towel cloth having a good pile napping property, a soft and bulky texture and a water absorbing property, and to provide a manufacturing method of the towel cloth.SOLUTION: There is provided a towel cloth having a warp pile yarn locked to a warp ground yarn and a weft ground yarn, in which the warp pile yarn is a siro spun yarn 19 and is a twistless or loosely twisted spun yarn having secondary twisting applied in a direction opposite to a primary twisting direction of a plurality of rovings 12a and 12b, that is, in an untwisting direction. Since fibers in the pile yarn are entangled with each other due to the twisting habit of the primary twisting and migration caused by the primary twisting, and the pile yarn is the twistless or the loosely twisted yarn, each fiber constituting the pile yarn is present in a free state, which results in the pile yarn having a good napping property and a soft and bulky texture.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a towel fabric using siro spun yarn for the pile yarn, and a method for producing the same. [Background technology]

[0002] Traditionally, towel fabrics have been made by weaving warp pile yarns, warp yarns, and weft yarns into pile fabric. To improve water absorption, towel fabrics have a relatively high basis weight (mass per unit area) and are made of thick, fine yarns. Patent Document 1 proposes using synthetic sirospun yarn to make a heathered yarn for pile fabric. Patent Documents 2 and 3 propose using loosely twisted sirospun yarn to make a pile fabric. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Japanese Patent Application Publication No. 10-088440 [Patent Document 2] JP 2019-137941 A [Patent Document 3] JP 2019-137942 A Summary of the Invention [Problem to be solved by the invention]

[0004] However, the above-mentioned conventional techniques have problems with respect to pile standing and soft, fluffy feel, and further improvements are required.

[0005] The present invention is the result of extensive research aimed at making the most of the characteristics of towel fabric, and provides a towel fabric having good pile standing, a soft and fluffy feel, and water absorbency, and a manufacturing method thereof. [Means for solving the problem]

[0006] The towel fabric of the present invention comprises warp yarns, weft yarns, and warp pile yarns, with the warp pile yarns engaged with the warp yarns and weft yarns, and is characterized in that the warp pile yarns are spun spun yarns that are untwisted or loosely twisted spun yarns to which a secondary twist has been applied in the opposite direction to the primary twist direction of multiple roving yarns, i.e., in the untwisting direction.

[0007] The method for producing towel fabric of the present invention is a method for producing towel fabric as described above, characterized in that the warp pile yarn is a sirospun spun yarn, and a secondary twist is applied in the opposite direction to the primary twist direction of multiple roving yarns having the same twist direction to produce a single untwisted or loosely twisted spun yarn. Effect of the Invention

[0008] The towel of the present invention is a towel fabric including warp yarns, weft yarns, and warp pile yarns, the warp pile yarns being engaged with the warp yarns and weft yarns, the warp pile yarns being spun spun yarns of sirospun yarns, and being untwisted or loosely twisted spun yarns to which a secondary twist has been applied in the opposite direction (untwisting direction) to the primary twist direction of the multiple roving yarns, thereby providing a towel fabric with good pile standing, a soft and fluffy texture, and water absorption, and a manufacturing method thereof. That is, in combination with the yarn structure in which a secondary twist has been applied in the opposite direction (untwisting direction) to the primary twist direction of the multiple roving yarns, the twisting tendency of the primary twist and migration of the primary twist (phenomenon in which single fibers are twisted inward or outward) remain, there is entanglement between the fibers, the yarn is untwisted or loosely twisted, and each constituent fiber exists in a free state, resulting in a pile yarn with good pile standing and a soft and fluffy texture. [Brief description of the drawings]

[0009] [Figure 1] FIG. 1 is a schematic perspective view of a sirospun spinning device according to one embodiment of the present invention. [Diagram 2] FIG. 2 is a schematic explanatory diagram of a towel cloth according to one embodiment of the present invention. [Diagram 3]Figure 3 is a diagram of the weave of the fiber towel fabric. [Figure 4] FIG. 4 is a side photograph (magnification: 50 times) of the pile portion of the towel fabric in Example 1 of the present invention. [Diagram 5] FIG. 5 is a plan view photograph (magnification: 10 times) of the towel fabric of Example 1 of the present invention. [Figure 6] FIG. 6 is a side photograph (magnification: 50 times) of the pile portion of the towel fabric in Example 2 of the present invention. [Figure 7] FIG. 7 is a plan view photograph (magnification: 10 times) of the towel fabric of Example 2 of the present invention. [Figure 8] FIG. 8 is a side photograph (magnification: 50 times) of the pile portion of the ol fabric of Comparative Example 1. [Figure 9] FIG. 9 is a plan view photograph (magnification: 10 times) of the towel fabric of Comparative Example 1. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0010] The present invention focuses on the fact that warp pile yarns (hereinafter also referred to as pile yarns), which account for approximately 70% of the constituent yarns of a towel fabric, are important yarns that determine the pile standing property, the texture of the towel fabric, and functionality such as fuzz shedding, and has conducted further research and obtained the following findings. That is, the towel fabric of the present invention is a towel fabric that includes warp yarns, weft yarns, and warp pile yarns, in which the warp pile yarns are engaged with the warp yarns and weft yarns, and the warp pile yarns are sirospun spun yarns, and a secondary twist is applied in the opposite direction to the primary twist direction of multiple rovings, i.e., in the untwisting direction, and the warp pile yarns are made of untwisted or loosely twisted spun yarns. It has been found that this has the following advantages. (1) The warp pile yarn is a sirospun yarn, and a secondary twist is added in the opposite direction to the primary twist direction of the multiple roving yarns, with the same or more twists than the primary twist. As a result, a secondary twist is applied, but the twist tendency of the primary twist remains, migration of the primary twist (the phenomenon in which single fibers are twisted inward or outward) also remains, and there is entanglement between the fibers. Since the yarn is either untwisted or loosely twisted, each component fiber exists in a free state, the pile standing property is good, and the pile yarn has a soft and fluffy texture. Because of its soft and fluffy texture, it can be gently touched against the skin and can efficiently wipe away sweat and moisture (texture effect, wiping effect). (2) Since pile yarn is either untwisted or loosely twisted, the constituent fibers are more likely to absorb moisture, and at the same time, this swelling promotes air movement, improving breathability (water absorption effect, ventilation effect). (3) The intertwining of the constituent fibers reduces pilling (impact of reduced pilling), reduces changes in texture after washing, and maintains the original soft, fluffy texture (effect of durability of texture after washing). (4) When producing spun yarn, there is no need to use water-soluble fibers (such as water-soluble vinylon), glue, etc., which reduces costs. However, if water-soluble fibers (such as water-soluble vinylon), glue, etc. are used and then removed after the fabric is made, voids are generated, which reduces the fluffiness (volume) and increases the amount of fluff that falls off. (5) Since there is no need to use water-soluble fibers (such as water-soluble vinylon) or glue when producing spun yarn, the environmental impact of factory wastewater containing these materials can be reduced.

[0011] In the present invention, sirospun spun yarn is used as the warp pile yarn. Sirospun is a yarn in a state similar to a two-ply yarn, which is made by drafting a plurality of rovings separately at a certain interval and then twisting them together. Compared to a two-ply yarn made by twisting a plurality of yarns together, the fibers of the sirospun spun yarn are regularly arranged on the yarn surface, and there is little fuzz. For this reason, it can be used as a warp pile yarn in a single yarn. In addition, due to the yarn structure unique to the sirospun spun yarn, even if it is a non-twisted yarn or a loosely twisted yarn, the fibers are entangled with each other, so there is no problem with winding, and thread breakage during weaving is unlikely to occur, and the weaving process is also good. The multiple rovings referred to above refer to two or more rovings, and it is known to use two or three rovings. An example of two rovings will be described below.

[0012] The spun spun yarn of the present invention preferably has a twist factor K of 0 to 3.5, more preferably 0 to 3.3, and even more preferably 0 to 3.0. The twist factor (K) is calculated by the following formula (Math 1).

number

[0013] It is preferable that the sirospun yarn has a secondary twist in the opposite direction to the primary twist direction of the two rovings, the number of twists being equal to or greater than the number of twists in the primary twist. For example, if the primary twist directions of the two rovings are both Z-directions, the secondary twist is S-direction, and the number of twists in the secondary twist is equal to or greater than the number of twists in the primary twist. This allows each component fiber to exist in a more free state, resulting in good pile standing and a pile yarn with a soft, fluffy feel.

[0014] The spun spun yarn is preferably 100% cotton. If it is 100% cotton, it has a soft and fluffy texture and can also absorb water. In addition, natural fibers including hemp and wool, regenerated fibers including rayon, acetate, and polyester, semi-synthetic fibers, and chemical fibers may be blended as long as these properties are not impaired. The blending rate of these fibers other than cotton is preferably 30% by mass or less. There are no particular limitations on the yarn count of the spun spun yarn, but thin ones with counts of 100 to 40 are preferably applied for thin fabrics, 30 to 16 for medium-weight fabrics, and thick ones with counts of 12 to 8 for heavy fabrics.

[0015] The silospun spun yarn is preferably mercerized. The mercerization process improves firmness, stiffness, shape memory, luster, strength, shrink resistance, and dyeability by immersing the yarn in an aqueous solution of caustic soda (sodium hydroxide) and tensioning it. This is thought to be because part of the crystalline structure of cotton changes from type I to type II via alkali cellulose, and the structure around the crystals is also rearranged. The mercerization process itself has been well known for a long time, as described in the fiber dictionary. When the silospun spun yarn of the present invention that is untwisted or loosely twisted in the untwisting direction is mercerized, the pile standing property, soft and fluffy texture, water absorption, etc. are synergistically improved and shape memory is achieved, resulting in a high-quality towel fabric. The concentration of caustic soda (sodium hydroxide) in the aqueous solution is preferably 15% by mass or more, more preferably 20% by mass or more. The tension treatment is preferably carried out by setting the speed ratio of the supply roller to the take-up roller at about 1 to 1.1 and immersing the material in an aqueous solution of caustic soda (sodium hydroxide) in a tensioned state.

[0016] The method for producing the towel fabric of the present invention includes the following steps. (1) Two rovings with the same twist direction are twisted in the opposite direction (untwisting direction) to the primary twist direction to produce a non-twisted or loosely twisted spun yarn. Preferably, a secondary twist is added that is equal to or greater than the number of twists in the primary twist. This produces a single sirospun yarn, which is then used as a warp pile yarn to produce towel fabric. (2) The warp and weft yarns of the towel fabric may be any type of yarn, such as open-end spun yarn, air spun yarn, ring spun yarn, filament composite spun yarn, or bonded spun yarn. (3) After the towel fabric is woven, it is bleached, scoured, dyed, etc. in the usual way to make towel fabric.

[0017] The spun spun yarn is preferably cotton with a micronaire of 4 to 7 and an average fiber length of 28 to 45 mm. Here, micronaire refers to mass micrograms (μg) per inch (25.4 mm). Cotton with a micronaire of 4 to 7 and an average fiber length of 28 to 45 mm has a lot of crimp and high crimp strength, so when applied to the spun spun yarn of the present invention, the twist tendency of the first twist and migration of the first twist (the phenomenon in which single fibers are twisted inward or outward) tend to remain, the fibers tend to be entangled, and since it is a non-twisted yarn or a loosely twisted yarn, each component fiber exists in a free state. Therefore, the pile yarn has good nap standing property and has a soft and fluffy texture. Specific examples are preferably those shown in Table 1 below. Among these, Shankar 6 from India is more preferable.

[0018] [Table 1]

[0019] The towel of the present invention is suitable for bath towels (towels after a bath), bath towels, face towels, towel handkerchiefs (towel squares), hand towels, wash towels, hand towels, bath mats, sports towels, beach towels (body towels), etc. The fabric blend ratio, yarn type, yarn usage, mass per unit (bath weight), etc. are appropriately set according to the required properties such as fluff shedding and water absorbency. The basis weight can be controlled by changing the pile length (long to short) of the pile yarn to control the basis weight (large to small). Here, examples of preferable basis weights that can exert the effects of the present invention include a basis weight of 100 to 250 g / m for thin fabrics. 2 The medium-weight fabric has a basis weight of 250 to 500 g / m 2 The thickness is 500~1000g / m 2 In addition, 100 g / m2 Those that are less than 1000g / m are thin and have no bulk. 2 Anything over that is too thick and heavy, and neither is recommended.

[0020] In the present invention, cotton is the most excellent in terms of texture, water absorption, hygroscopicity, and ease of handling as a towel, but cotton may be blended with small amounts of linen, rayon, cupra, acetate, or wool. Blends of rayon, cupra, and acetate provide hygroscopicity, while wool provides heat retention. The woven fabric is desized in a jet dyeing machine in accordance with the cotton processing process, and then scoured under standard cotton scouring conditions (constant temperature of 95-98°C, hold time of 50 minutes, dilute caustic soda solution, alcohol ethoxylate added bath). After scouring, it is bleached under standard conditions (98°C, 50 minutes, hydrogen peroxide solution). It is then dehydrated and finished by setting in a tenter (off-white finish). This bleaching process also involves hot water treatment. If it is desired to include synthetic fiber crimped yarn, the false twisted yarn is crimped by the above scouring, and then the fabric is finished as is.

[0021] Next, when dyeing is performed after scouring and bleaching, cotton is dyed with reactive dyes (60 to 80°C, 40 minutes). Polyester fibers are dyed with disperse dyes (130°C, 40 minutes). When dyeing fabrics containing cotton and polyester, in addition to plain dyeing in this two-bath process, disperse dyes and reactive dyes can be used separately to dye different colors or chambray (shades). In addition, printing can be performed on off-white fabrics that have been scoured and bleached. In the case of yarn-dyed polyester yarns, shrinkage can be expressed at the same time as scouring, and the yarns can be bleached and dyed, and then woven to obtain yarn-dyed towel fabrics. In the case of yarn-dyed cotton yarns, the yarns can be scoured, bleached, dyed, and then woven to obtain yarn-dyed towel fabrics. In this way, the present invention allows commercialization of products with excellent color and design properties through a variety of dyeing methods.

[0022] The following description will be given with reference to the drawings. In the following drawings, the same reference numerals denote the same parts. Fig. 1 is a schematic perspective view of a sirospun spinning device according to one embodiment of the present invention. In this sirospun spinning device 10, two roving bobbins 11a, 11b are hung from one spindle on a creel (roving supplying tool), and rovings 12a, 12b supplied from the two roving bobbins 11a, 11b are sent in parallel to a draft device 15 through a two-mouth trumpet guide 13 provided on the upstream side (roving bobbin side) of a back roller 14. The rovings 12a, 12b are then drafted at a predetermined interval between the back roller 14 and an apron 16, and between the apron 16 and a front roller 17, respectively, to form fleeces 18a, 18b. The fleeces 18a, 18b are spun from the front roller 17 and twisted downstream of the front roller 17 by a twisting mechanism caused by the rotation of the spindle 21 to form one spun yarn 19, which is then taken up onto a bobbin 22 via a snail wire 20 and a traveler 21. For example, the twist directions of the primary twist of the two rovings 12a, 12b are both in the Z direction, the twist direction by the spindle 21 is in the S direction, and the rovings are twisted in the untwisting direction. The number of twists by the spindle 21 (secondary twist number) is set to be the same as or greater than the number of twists in the primary twist.

[0023] 2 is a schematic diagram of a towel fabric 1 according to one embodiment of the present invention. This towel fabric 1 is composed of warp pile yarns 2a, 2b, weft ground yarns 3, and warp ground yarns 4a, 4b, and the warp pile yarns 2a, 2b form loop piles while being fixed to the ground structure composed of the weft ground yarns 3 and the warp ground yarns 4a, 4b. The obtained towel fabric 1 is cut to a predetermined size and the ends are processed to make a towel.

[0024] Figure 3 is a weave diagram of a towel fabric according to one embodiment of the present invention. This weave is a three-pick terry motion weave. The warp pile yarns cross once for every three weft ground yarns. The warp ground yarns G and the warp pile yarns P are arranged alternately. The weft yarns 1 to 3 indicate the order. In Figure 3, as viewed from the warp yarns, black and x indicate floating yarns, and white indicates sinking yarns. EXAMPLES

[0025] The present invention will be described in more detail below with reference to examples, but the present invention is not limited to the following examples. <Evaluation of the texture of finished towel fabric> (1) Evaluation of soft texture The softness of the texture is expressed as the volume per gram of towel fabric and is calculated using the following bulk height formula. The higher the value, the softer and better the texture. The thickness was measured according to JIS L-1096 (2010) 8.5 Bulkiness Test, and the basis weight was measured by precisely weighing the weight of a 1m square. Measurements were taken at five points, and the average value was used. Umbrella height (cm 3 / g) = Thickness (mm) / Weight (g / m 2 ) x 1000 (2) Evaluation of fluffy texture The towel fabric is compressed at a constant speed using a compression measuring device: KES-G5 (manufactured by Kato Tech Co., Ltd.) and the compression work: WC = (gf.cm 2 The measurements were taken at five locations, and the average value was calculated. The WC value is the amount of energy required to compress the fabric; the higher the value, the better the towel is compressed, the more fluffier it is, and the fluffier it is. (3) Evaluation of wash durability of texture The towel fabric was washed 20 times in a washing machine according to JIS L-0217 (1995), Method 103. After drying, the compression work: WC = (gf.cm 2 ) was measured at five locations and the average value was expressed. The smaller the difference in WC value before and after washing, the less the loss of fluffy texture due to washing, and the more durable and good the product is. (4) Evaluation of drainage during washing A 35cm wide piece of towel fabric was cut to a length so that it weighed 80g, the weight was accurately measured to one decimal place, and the piece was soaked in water for 20 minutes. The wet towel fabric was then taken out and centrifugally dehydrated in the spin tub of a washing machine for 4 minutes, the weight was accurately measured, and the residual moisture content (%) of the towel fabric was calculated using the following formula. The smaller the value, the better the drainage. Better drainage tends to lead to a faster subsequent drying speed. Three measurements were taken and the average value was used. Residual moisture content of fabric (%) = (Weight of fabric after soaking in water and dehydrating (W1)) - (Weight of fabric before soaking in water (W0)) / (Weight of fabric before soaking in water (W0)) x 100 (5) Evaluation of pilling of towel fabric after washing The amount of shedding due to washing was measured according to JIS L0217 (1995), method 103. The percentage of shedding (%) was calculated using the following formula. The smaller the value, the less shedding and the better the result. The number of measurements was 5, and the average value was used. Lint shedding rate (%) = (weight of lint that fell off after washing (g1)) / (weight of towel before washing (g0)) x 100 (6) Water absorption evaluation (modified Larose method) The measurement was performed five times according to the modified Larose method of JIS L 1907 (2010), and the average value was calculated. The Larose index (water absorption index) was calculated according to the following formula. Larose index (water absorption index)=2545V×1411W+79 V: Maximum water absorption rate (ml / s), W: Water absorption amount at the maximum water absorption rate (ml) The higher the value, the faster and larger the amount of moisture absorbed from the skin, which is preferable. (7) Water absorption rate (dropping method) The water absorption rate of the terry cloth was measured and evaluated based on the Vuillet method, a drop method in JIS L 1907 (2010). The test outline was to drop a single drop of water onto the terry cloth from a height of 10 cm, measure the water absorption time (seconds) until the mirror-like surface of the drop disappeared three times, and calculate the average value. The shorter the time, the faster and better the water absorption. <Rewetting rate test method> The water-rewet rate is described in Patent Publication No. 6991633 proposed by the applicant, and is a test method in which water droplets are dropped onto a test specimen of the fabric, the water is absorbed, and the fabric is evaluated as the property of not releasing the water, i.e., the water-rewet rate, which coincides with the evaluation of the water absorbency felt by people when using a fiber fabric such as a towel. The lower the water-rewet rate, the greater the water absorbency of the fabric, and the better it can be evaluated to be. (1) Test environment and other conditions The test environment was standard, with a temperature of 20±4°C and a relative humidity of 65±4%. The filter papers were stored for at least 24 hours under standard conditions (temperature 20±4℃, relative humidity 65±4% RH). The test specimens were stored for at least 24 hours under standard conditions at a temperature of 20±4℃ and a relative humidity of 65±4%RH. The temperature of the water used for dripping was 20±15℃ (5~35℃). (2) Operation procedure The size of the test specimen 1 of the fiber towel fabric was 10 cm long and 10 cm wide. The test specimen 1 was placed on a sample stand (not shown). The filter paper used was made of α-cellulose, conforming to the JIS P 3801 Class 1 standard, with a diameter of 110 mm and a thickness of 0.22 mm, and the weight of the filter paper was measured. The filter paper used was Advantec's product name "Circular Qualitative Filter Paper No. 1." Measure 0.8 ml of water into a pipette, drop it into test specimen 1, and wait 5 seconds to allow test specimen 1 to absorb the water. A filter paper was placed on top and a load of 1.3 kg (1274 Pa) was placed on top of it. Wait 5 seconds and then remove the load. The weight of the filter paper after absorbing water was measured. (3) Calculation of water rewetting rate Calculation was made using the following formula. W = [(BA) / A] × 100 Where W: Water rewetting rate (%) A: Weight of filter paper before measurement (g) B: Weight of filter paper after absorbing water (g) <Pile standing property> The pile portion of the towel fabric was observed using an optical microscope, with side photographs (magnification 50x).

[0026] Example 1 (1) Warp pile yarn The warp pile yarn was produced using a sirospun spinning device shown in Figure 1. Shankar 6 cotton from India was used. The two rovings 12a and 12b were twisted in the Z direction for the primary twist, and the twisting direction by the spindle 21 was the S direction, and they were twisted in the untwisting direction. The fineness of the roving was 5g / 6 yards (9113 decitex), and the Z-directional twist number of the roving was 5 turns / inch (twist factor K=1 in terms of cotton count). The obtained spun yarn had a cotton count of 20 and a twist number of 11.7 turns / inch (twist factor K=2.6). (2) Warp threads The warp yarns used Indian cotton filling and ring-spun yarn No. 40 two-ply yarn with a twist coefficient of 3.8 for the first twist and 2.2 for the second twist. (3) Weft threads The weft yarn used Indian cotton filling, ring spun yarn No. 20 single yarn, twist factor: 4.0. (4) Towel fabric weaving The warp pile yarns and warp ground yarns were sized, and the fabric shown in Figure 2 was woven using a pile loom with the weave shown in Figure 3. The warp density was 34 threads / inch, the weft density was 56 threads / inch, and the weight was 463g / m 2 The fabric composition is 100% cotton. (5) Towel fabric refining and finishing process Next, this grey fabric was desized in a liquid jet dyeing machine in the usual manner similar to cotton processing (55°C x 20 minutes, amylase, surfactant-added bath), and then scoured in the same machine at 98°C for 50 minutes in a dilute caustic soda, alcohol ethoxylate-added bath. It was then bleached in a conventional hydrogen peroxide bath at 98°C for 50 minutes, tentered at 135°C, and finished (off-white finish). The pile length was 1.15 cm.

[0027] Example 2 The same procedure as in Example 1 was carried out, except that the warp pile yarns were immersed in an aqueous solution of 200 g / L of caustic soda (sodium hydroxide), tensioned, and mercerized.

[0028] Comparative Example 1 The same procedure as in Example 1 was carried out, except that the twist directions of the primary twist of the two rovings 12a, 12b as the warp pile yarns were both in the Z direction, and the twist direction by the spindle 21 was also in the Z direction. The obtained spun yarn had a cotton count of 20 and a twist number of 14 turns / inch (twist factor K=3.1). The above results are shown in Table 2.

[0029] [Table 2]

[0030] As is clear from Table 2, the towel fabrics of Examples 1 and 2 were better than Comparative Example 1 in bulkiness, total and post-wash compression work WC, fuzz shedding rate, improved Larose method water absorption index, water absorption speed, wet-back rate, and nap standing (Figs. 4, 6, and 8). As a result, it was confirmed that the towel fabric of the present invention is a towel fabric with good pile standing, a soft and fluffy texture, and water absorbency that could not be obtained by conventional technology. Furthermore, the towel fabric of Example 2 (pile yarn is mercerized) had the highest compression work WC and water drainage property: residual moisture rate after 20 washes, and was also good in firmness, stiffness, shape memory, luster, strength, shrink resistance, and dyeability. [Industrial Applicability]

[0031] The towel fabric of the present invention is also suitable for use as fabric for face towels, bath towels, towel handkerchiefs, sports towels, bathrobes, towel blankets, clothing, socks, rugs, bedding, and the like. [Explanation of symbols]

[0032] 1. Towel fabric 2a, 2b warp pile yarn 3 Weft thread 4a, 4b Warp thread 10. Silospun spinning device 11a, 11b roving bobbin 12a,12b roving 13 Trumpet Guide 14 Back roller 15 Draft device 16 Apron 17 Front roller 18a,18b Fleece 19 Spun Yarn 20 Snell Wire 21 Spindle 22 Bobbin

Claims

1. A towel fabric comprising warp yarns, weft yarns, and warp pile yarns, the warp pile yarns being engaged with the warp yarns and the weft yarns, The warp pile yarn is a sirospun yarn, The towel fabric is characterized in that the sirospun yarn is a non-twisted or loosely twisted spun yarn to which a secondary twist has been applied in the opposite direction to the primary twist direction of the multiple roving yarns, i.e., in the untwisting direction.

2. The towel fabric according to claim 1, wherein the spun spun yarn has a twist coefficient K of 0 to 3.

5. The twist factor (K) is calculated using the following formula (1). [0010] Where, t: number of twists (twists / 25.4mm), S: cotton count (British cotton count)

3. The towel fabric according to claim 1, wherein the twist direction of the secondary twist of the sirospun yarn is the same as or greater than the number of twists of the primary twist.

4. The towel fabric according to claim 1, wherein the silospun yarn is 100% cotton.

5. The towel fabric according to claim 1, wherein the silospun yarn is cotton having a micronaire of 4 to 7 and an average fiber length of 28 to 45 mm. Here, micronaire refers to micrograms (μg) of mass per inch (25.4 mm).

6. The towel fabric according to claim 1, wherein the sirospun yarn is mercerized.

7. A method for producing a towel fabric according to any one of claims 1 to 6, The warp pile yarn is a sirospun yarn, This method for producing a towel fabric is characterized in that a plurality of rovings having the same twist direction are subjected to a secondary twist in a direction opposite to the primary twist direction to form a single untwisted or loosely twisted spun yarn.

8. The method for producing a towel fabric according to claim 7, wherein the silo spun yarn is mercerized by immersing the yarn in an alkaline aqueous solution and tensioning it.

Citation Information

Patent Citations

  • Production of raw yarn for pile fabric

    JP1985052638A

  • Fibrous structure containing cotton fiber

    JP2001348776A

  • Modified cotton, cotton yarn and textile product comprising the same, and method for producing modified cotton

    JP2022128926A

  • Towel fabric and production method therefor

    WO2022059487A1

  • Towel fabric and production method therefor

    WO2022220175A1