Coating material
The coating material with specific resin and curing agent components addresses moisture-induced defects in roofing materials by enhancing crosslinking density and film uniformity, achieving improved initial curing, weather resistance, and followability.
Patent Information
- Application Number
- JP2023074437
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-28
- Publication Date
- 2024-11-08
AI Technical Summary
Existing roofing materials face issues with moisture-induced defects during the drying process, requiring improved initial curing properties and weather resistance while maintaining followability.
A coating material comprising a hydroxyl group-containing resin with a non-aqueous dispersible resin having a hydroxyl value of 30 mgKOH/g or more and a soluble resin with a lower hydroxyl value, along with a curing agent containing a polyisocyanate compound and a silicate compound, enhances crosslinking density and film uniformity.
The coating material improves initial curing properties, suppresses moisture-related defects, and forms a film with excellent weather resistance and followability, ensuring durable and high-quality finishes.
Smart Images

Figure 2024158860000001 
Figure 2024158860000002
Abstract
Description
[Technical field]
[0001] The present invention relates to a coating material. [Background technology]
[0002] Buildings, civil engineering structures, and the like are coated with various coating materials for the purpose of protecting the framework, imparting design, and enhancing aesthetics, etc. Among them, roofing materials are directly exposed to the harsh natural environment, such as rainwater and direct sunlight, and are therefore prone to deterioration, so weather resistance is required. For example, Patent Document 1 describes a coating material that is made of a base agent containing an acrylic polyol and a curing agent containing an isocyanate and a silane coupling agent.
[0003] On the other hand, since the painting of roofing materials is generally carried out outdoors, it is affected by the painting environment (temperature, etc.). For example, moisture may adhere to the coating due to rainwater or condensation during the drying process. Such adhesion of moisture may cause problems with the coating. Furthermore, roofing materials are required to exhibit coating strength (high initial hardening properties) that allows walking on the surface from the day after application, from the viewpoints of workability in the next process (repainting, etc.) and finish quality. A method of blending a hardening catalyst, etc. is known as a means of increasing initial hardening properties, but this may result in reduced conformity to the substrate. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2016-160395 A Summary of the Invention [Problem to be solved by the invention]
[0005] The present invention has been made in consideration of the above-mentioned problems, and has an object to provide a coating material that enhances initial curing properties, suppresses defects caused by moisture during the drying process, and is capable of forming a coating film that is excellent in weather resistance and conformability. [Means for solving the problem]
[0006] In order to solve these problems, the present inventors conducted extensive research and came up with the idea of a coating material containing a specific resin component as an essential component, thereby completing the present invention.
[0007] That is, the present invention has the following features. 1. A coating material having a base agent and a hardener, The base material contains a hydroxyl group-containing resin (A), The curing agent contains a polyisocyanate compound (B) and a silicate compound (C), The coating material further contains a curing catalyst (D), The hydroxyl-containing resin (A) includes a non-aqueous dispersion type resin (a1) having a hydroxyl value of 30 mgKOH / g or more, and a soluble type resin (a2) having a hydroxyl value of 30 mgKOH / g or more, A coating material, wherein the hydroxyl value of the non-aqueous dispersion type resin (a1) is greater than the hydroxyl value of the soluble type resin (a2). 2. The coating material according to 1., wherein the hydroxyl-containing resin (A) contains a silicone component. 3. The coating material according to 1 or 2, wherein the non-aqueous dispersion type resin (a1) contains a silicone component. Effect of the Invention
[0008] The coating material of the present invention can form a coating film that is excellent in weather resistance and conforms to the substrate while improving initial curing properties and suppressing defects caused by moisture during the drying process. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0009] Hereinafter, an embodiment of the present invention will be described.
[0010] The coating material of the present invention has a base agent and a curing agent, the base agent contains a hydroxyl group-containing resin (A), the curing agent contains a polyisocyanate compound (B) and a silicate compound (C), and the coating material further contains a curing catalyst (D).
[0011] (Main ingredient) The base material contains a hydroxyl-containing resin (A) (hereinafter also referred to as "component (A)"), and as component (A), it contains a non-aqueous dispersion type resin (a1) having a hydroxyl value of 30 mgKOH / g or more, and a soluble type resin (a2) having a hydroxyl value of 30 mgKOH / g or more, and the hydroxyl value of the non-aqueous dispersion type resin (a1) is larger than the hydroxyl value of the soluble type resin (a2). In such a case, a coating having a strong crosslinked structure is formed by reaction with a curing agent described later, and excellent effects can be exhibited in terms of weather resistance, stain resistance, conformability to the substrate, and adhesion. Although the mechanism of action is not limited, the soluble resin (a2) contributes to the dispersion effect of the non-aqueous dispersion resin (a1) and is likely to be present around the non-aqueous dispersion resin (a1), and the crosslinking reaction proceeds in such a state, which makes it difficult for the crosslink density in the coating to become uneven. It is presumed that this results in the formation of a uniform coating with a high crosslink density, which improves weather resistance, stain resistance, followability, etc. On the other hand, if the hydroxyl value of the (A) component [non-aqueous dispersion resin (a1) and soluble resin (a2)] is less than 30 mgKOH / g, the crosslink density is low, the coating properties, etc. are reduced, and the above-mentioned effects are difficult to obtain sufficiently. The hydroxyl value mentioned above is the hydroxyl value of the solid content of component (A), and is a value expressed as the number of milligrams of potassium hydroxide equivalent to the moles of hydroxyl groups contained in 1 g of sample.
[0012] Specifically, the hydroxyl value of the non-aqueous dispersion type resin (a1) is 30 mgKOH / g or more (preferably 35 to 200 mgKOH / g, more preferably 40 to 150 mgKOH / g), and the hydroxyl value of the soluble type resin (a2) is 30 mgKOH / g or more (preferably 31 to 150 mgKOH / g, more preferably 35 to 100 mgKOH / g). In such a case, the crosslink density of the coating increases, and excellent effects can be exhibited in weather resistance, stain resistance, followability, etc. In the present invention, "α to β" is synonymous with "α or more and β or less".
[0013] In the present invention, the hydroxyl value of the non-aqueous dispersion type resin (a1) is larger than that of the soluble type resin (a2), and the difference in hydroxyl value is preferably 1 to 50 KOHmg / g (more preferably 2 to 40 KOHmg / g). In such a case, the effect of the present invention can be further enhanced.
[0014] Furthermore, the mixing weight ratio of the non-aqueous dispersion type resin (a1) to the soluble type resin (a2) [(a1) / (a2)] is preferably 99 / 1 to 50 / 50 (more preferably 98 / 2 to 60 / 40), which can further enhance the above-mentioned effects.
[0015] In the present invention, the non-aqueous dispersion type resin (a1) in component (A) is a hydroxyl-containing resin (A) dispersed as resin particles in a non-aqueous solvent, while the soluble type resin (a2) is a hydroxyl-containing resin (A) dissolved in a non-aqueous solvent.
[0016] The non-aqueous solvent preferably contains an aliphatic hydrocarbon-containing non-aqueous solvent (so-called weak solvent). The aliphatic hydrocarbon-containing non-aqueous solvent is a non-aqueous solvent that is less toxic than toluene, xylene, etc., has high operational safety, and has little impact on air pollution. Examples of aliphatic hydrocarbons include n-hexane, n-pentane, n-octane, n-nonane, n-decane, n-undecane, and n-dodecane. These can be used alone or in combination of two or more. In the present invention, aliphatic hydrocarbons can also be introduced by using a mixed solvent such as mineral spirits. The aliphatic hydrocarbon is preferably contained in an amount of 5% by weight or more, more preferably 10 to 80% by weight, based on the total amount of the non-aqueous solvent.
[0017] The non-aqueous solvent may contain a solvent that can be mixed with aliphatic hydrocarbons. Examples of such solvents include petroleum-based solvents such as petroleum ether, petroleum naphtha, and solvent naphtha, as well as ethyl acetate, butyl acetate, methyl ethyl ketone, and methyl isobutyl ketone. Examples of suitable solvents include petroleum-based solvents (aromatic hydrocarbon-containing petroleum mixed solvents) having a mixed aniline point or aniline point of 12 to 70°C. The mixed aniline point or aniline point is a value measured by the method of JIS K2256:2013.
[0018] The component (A) of the present invention may be any resin containing a hydroxyl group, such as polyether polyol, polyester polyol, acrylic polyol, fluorine-containing polyol, etc., and may also be used, such as phenol resin polyol, epoxy polyol, polybutadiene polyol, polyisoprene polyol, polyester-polyether polyol, urea-dispersed polyol, carbonate polyol, etc. One or more of these may be used as the component (A). It is particularly preferable that the component (A) of the present invention contains an acrylic polyol.
[0019] The acrylic polyol may be a copolymer of a hydroxyl group-containing monomer, an alkyl (meth)acrylate ester, and, if necessary, other monomers. Examples of hydroxyl group-containing monomers include hydroxyalkyl esters of (meth)acrylic acid, such as 2-hydroxyethyl (meth)acrylate, 2-hydroxypropyl (meth)acrylate, 3-hydroxypropyl (meth)acrylate, 2-hydroxybutyl (meth)acrylate, and 4-hydroxybutyl (meth)acrylate; hydroxyalkyl vinyl ethers, such as hydroxyethyl vinyl ether, hydroxypropyl vinyl ether, hydroxybutyl vinyl ether, and hydroxypentyl vinyl ether; and hydroxyallyl ethers, such as ethylene glycol monoallyl ether, diethylene glycol monoallyl ether, and triethylene glycol monoallyl ether. One or more of these can be used.
[0020] Examples of (meth)acrylic acid alkyl esters include methyl (meth)acrylate, ethyl (meth)acrylate, isopropyl (meth)acrylate, n-butyl (meth)acrylate, isobutyl (meth)acrylate, n-amyl (meth)acrylate, isoamyl (meth)acrylate, n-hexyl (meth)acrylate, 2-ethylhexyl (meth)acrylate, octyl (meth)acrylate, decyl (meth)acrylate, dodecyl (meth)acrylate, octadecyl (meth)acrylate, cyclohexyl (meth)acrylate, and the like. One or more of these can be used.
[0021] Examples of other monomers include amino group-containing monomers such as dimethylaminoethyl (meth)acrylate, dimethylaminopropyl (meth)acrylate, dimethylamino (meth)acrylate, aminoethyl (meth)acrylate, and diethylaminoethyl (meth)acrylate; carboxyl group-containing monomers such as acrylic acid, methacrylic acid, crotonic acid, maleic acid or its monoalkyl ester, itaconic acid or its monoalkyl ester, and fumaric acid or its monoalkyl ester; amide-containing monomers such as (meth)acrylamide and ethyl (meth)acrylamide; nitrile group-containing monomers such as (meth)acrylonitrile; and glycidyl Examples of the monomer include epoxy group-containing monomers such as (meth)acrylates; alkoxysilyl group-containing monomers such as vinyltrimethoxysilane, vinyltriethoxysilane, γ-(meth)acryloyloxypropyltrimethoxysilane, γ-(meth)acryloyloxypropyltriethoxysilane, γ-(meth)acryloyloxypropylmethyldimethoxysilane, or silicone compounds having a polymerizable double bond; aromatic hydrocarbon monomers such as styrene, methylstyrene, chlorostyrene, vinyltoluene, and the like; and vinyl esters such as vinyl acetate, vinyl propionate, vinyl butyrate, and vinyl pivalate, and one or more of these can be used as necessary.
[0022] Furthermore, it is preferable that the component (A) contains a silicone component as a constituent. In particular, it is preferable that the non-aqueous dispersion type resin (a1) contains a silicone component. By including a silicone component in the non-aqueous dispersion type resin (a1) having a large hydroxyl value, a silicone coating having an increased crosslinking density is formed, and the effect of improving long-term weather resistance can be further enhanced. The form of such a silicone component may be linear, branched, cyclic, or the like. The content of the silicone component is determined by the ratio of SiO to the resin solids. 2In terms of conversion, the content is preferably 0.1 to 20% by weight (more preferably 0.5 to 10% by weight). Within the above range, it is possible to obtain an effect of improving long-term weather resistance and ensure conformability to the substrate. In addition, the soluble resin (a2) may be in an embodiment that does not contain a silicone component, taking into consideration conformability to the substrate, adhesion, flexibility, etc.
[0023] SiO in the present invention 2 The conversion is the amount of silica (SiO 2 ) and is expressed as the weight fraction remaining. In general, alkoxysilanes, silicates, silicones, etc. react with water to undergo hydrolysis to become silanols, which then undergo condensation reactions between silanols or between silanols and alkoxy. When this reaction is carried to its ultimate state, silica (SiO 2 ) These reactions are RO(Si(OR) 2 O)nR+(n+1)H 2 O→nSiO 2 +(2n+2)ROH (R represents an alkyl group. n is an integer.) The reaction formula is as follows: 2 The conversion was made based on the amount of remaining silica component according to this reaction formula.
[0024] The method for introducing silicone into component (A) is not particularly limited and various methods can be used. For example, (1) A method for copolymerizing a silicone compound having a polymerizable double bond, (2) A method of reacting a functional group in a resin with a silicone compound having a functional group capable of reacting with the functional group; (3) A method of reacting a resin copolymerized with a reactive silyl group-containing monomer with a reactive silyl group-containing compound; (4) A method in which a functional group in a resin is reacted with a coupling agent having a functional group capable of reacting with the functional group, and then a reactive silyl group-containing compound is reacted therewith.
[0025] Examples of the combinations of functional groups in (2) and (4) above include a hydroxyl group and an isocyanate group, a hydroxyl group and a carboxylic anhydride group, an amino group and an isocyanate group, a carboxyl group and an epoxy group, an amino group and an epoxy group, and an alkoxysilyl group and an alkoxysilyl group.
[0026] The reactive silyl group in (3) and (4) above is a group in which an alkoxyl group, a phenoxy group, a mercapto group, an amino group, a halogen, or the like is bonded to a silicon atom. The reactive silyl group-containing compound is one having two or more reactive silyl groups in one molecule, and examples thereof include tetrafunctional alkoxysilanes such as tetraethoxysilane, tetramethoxysilane, and tetrabutoxysilane; trifunctional alkoxysilanes such as methyltrimethoxysilane, methyltriethoxysilane, methyltributoxysilane, ethyltrimethoxysilane, ethyltriethoxysilane, ethyltributoxysilane, propyltrimethoxysilane, propyltriethoxysilane, butyltrimethoxysilane, butyltriethoxysilane, phenyltrimethoxysilane, phenyltriethoxysilane, and phenyltributoxysilane; dimethyldimethoxysilane, dimethyldiethoxysilane, dimethyldibutoxysilane, diethyldimethoxysilane, diethyldiethoxysilane, dipropyldimethoxysilane, and dipropyl Examples of the alkoxysilanes include diethoxysilane, dibutyldimethoxysilane, dibutyldiethoxysilane, diphenyldimethoxysilane, diphenyldiethoxysilane, diphenyldibutoxysilane, methylphenyldimethoxysilane, and methylphenyldiethoxysilane; chlorosilanes such as tetrachlorosilane, methyltrichlorosilane, ethyltrichlorosilane, propyltrichlorosilane, phenyltrichlorosilane, vinyltrichlorosilane, dimethyldichlorosilane, diethyldichlorosilane, diphenyldichlorosilane, and methylphenyldichlorosilane; acetoxysilanes such as tetraacetoxysilane, methyltriacetoxysilane, phenyltriacetoxysilane, dimethyldiacetoxysilane, and diphenyldiacetoxysilane, and the like. One or more of these can be used. Also, a compound having one reactive silyl group in one molecule can be used in combination.
[0027] The reactive silyl group-containing monomer in (3) above is a compound containing a reactive silyl group and a polymerizable double bond, and examples thereof include vinyltrimethoxysilane, vinyltriethoxysilane, vinyltri-n-butoxysilane, vinyltris(β-methoxyethoxy)silane, allyltrimethoxysilane, trimethoxysilylethyl vinyl ether, triethoxysilylethyl vinyl ether, trimethoxysilylpropyl vinyl ether, triethoxysilylpropyl vinyl ether, γ-(meth)acryloyloxypropyltrimethoxysilane, γ-(meth)acryloyloxypropyltriethoxysilane, γ-(meth)acryloyloxypropylmethyldimethoxysilane, vinylmethyldimethoxysilane, methyldimethoxysilylethyl vinyl ether, methyldimethoxysilylpropyl vinyl ether, and the like. One or more of these may be used.
[0028] The coupling agent in (4) above is, for example, a compound having at least one or more alkoxysilyl groups and other substituents in one molecule.Specific examples of the coupling agent include β-(3,4 epoxycyclohexyl)ethyltrimethoxysilane, γ-glycidoxypropylmethyldiethoxysilane, γ-glycidoxypropyltriethoxysilane, N-(β-aminoethyl)-γ-aminopropylmethyldimethoxysilane, N-(β-aminoethyl)-γ-aminopropyltrimethoxysilane, γ-aminopropyltriethoxysilane, isocyanate functional silane, γ-methacryloxypropyltrimethoxysilane, γ-methacryloxypropylmethyldiethoxysilane, γ-methacryloxypropyltriethoxysilane, etc., and one or more of these can be used.
[0029] The glass transition temperature of component (A) is preferably -10 to 80°C (more preferably 0 to 60°C). If the glass transition point is within this range, the physical properties of the coating, such as stain resistance, flexibility, and durability, can be improved. The glass transition temperature is a value calculated by Fox's formula based on the vinyl monomer constituting the resin.
[0030] (hardening agent) The curing agent contains a polyisocyanate compound (B) and a silicate compound (C).
[0031] The (B) polyisocyanate compound (hereinafter also referred to as "component (B)") has two or more isocyanate groups in one molecule and reacts with the above-mentioned component (A) to form a coating film. The (B) component is preferably one that can crosslink with the (A) component at room temperature. The room temperature here preferably means -10°C or higher and 50°C or lower, more preferably -5°C or higher and 40°C or lower. The isocyanate group content in the solid content of the (B) component is preferably 2% by weight or higher and 30% by weight or lower.
[0032] Examples of the (B) component include derivatives of at least one diisocyanate selected from aliphatic diisocyanates and alicyclic diisocyanates, an alcohol component, and, if necessary, a polyol component, etc., which have been subjected to alphanation, biuretization, dimerization (uretidione formation), trimerization (isocyanurate formation), adductation, carbodiimide formation reaction, etc., and mixtures thereof. These can be used alone or in combination of two or more.
[0033] Aliphatic diisocyanates are compounds having saturated aliphatic groups in the molecule, such as 1,4-diisocyanatobutane, 1,5-diisocyanatopentane, 1,6-diisocyanatohexane (also known as hexamethylene diisocyanate (HDI)), 1,6-diisocyanato-2,2,4-trimethylhexane, methyl 2,6-diisocyanatohexanoate (lysine diisocyanate), etc. On the other hand, alicyclic diisocyanates are compounds having cyclic aliphatic groups in the molecule, such as 5-isocyanato-1-isocyanatomethyl-1,3,3-trimethylcyclohexane (isophorone diisocyanate), 1,3-bis(isocyanatomethyl)cyclohexane (hydrogenated xylylene diisocyanate), bis(4-isocyanatocyclohexyl)methane (hydrogenated diphenylmethane diisocyanate), 1,4-diisocyanatocyclohexane, etc. Among these, HDI is the most preferable because it has excellent weather resistance and flexibility. (Hereinafter, aliphatic diisocyanates and alicyclic diisocyanates will be collectively referred to as "diisocyanates.")
[0034] Examples of the alcohol component include methanol, ethanol, 1-propanol, 2-propanol, 1-butanol, 2-butanol, isobutanol, 1-pentanol, 2-pentanol, isoamyl alcohol, 1-hexanol, 2-hexanol, 1-heptanol, 1-octanol, 2-ethyl-1-hexanol, 3,3,5-trimethyl-1-hexanol, tridecanol, pentadecanol, palmityl alcohol, stearyl alcohol, cyclopentanol, cyclohexanol, methylcyclohexanol, trimethylcyclohexanol, etc. These can be used alone or in combination of two or more.
[0035] Examples of the polyol component include polyether polyol, polyester polyol, polyolefin polyol, etc. In the present invention, polyether polyols such as polypropylene triol, polypropylene glycol, polytetramethylene glycol, etc. are particularly suitable. These can be used alone or in combination of two or more.
[0036] In the present invention, it is preferable to use a polyisocyanate compound having an isocyanate group content of 5 to 35% by weight (more preferably 8 to 30% by weight, and even more preferably 12 to 28% by weight) in the solid content. In the case of such a range, it is possible to form a coating film having excellent curability (particularly initial curability), sufficient suppression of problems caused by moisture such as condensation during the drying process, and excellent finishing properties (gloss, etc.). In addition, it is possible to exhibit excellent effects such as weather resistance and stain resistance, and therefore it is possible to maintain a good finished state for a long period of time. In the present invention, the isocyanate group content is defined as the content (weight %) of isocyanate groups contained in the solid content of the polyisocyanate compound, and is a value obtained by back titration with hydrochloric acid after neutralizing the isocyanate groups with an excess amine.
[0037] The mixing ratio of the (B) component may be set in consideration of the molar ratio [NCO] / [OH] between the isocyanate groups of the (B) component and the hydroxyl groups of the (A) component. The molar ratio [NCO] / [OH] between the isocyanate groups of the (B) component and the hydroxyl groups of the (A) component is preferably 0.6 to 1.4 (more preferably 0.8 to 1.3). With such a ratio, the effects of the present invention can be further enhanced.
[0038] The mixing ratio (weight ratio) of the (A) component and the (B) component is set depending on the hydroxyl value of the (A) component and the isocyanate group content of the (B) component. In the coating material of the present invention, the mixing ratio of the (B) component is preferably 5 to 50 parts by weight (more preferably 10 to 40 parts by weight) per 100 parts by weight of the resin solid content of the (A) component.
[0039] The silicate compound (C) (hereinafter also referred to as "component (C)") mainly acts to improve the weather resistance of the formed coating and to impart hydrophilicity. Examples of such component (C) that can be used include tetraalkoxysilane, tetraalkoxysilane condensates, and modified products thereof. Examples of tetraalkoxysilane include tetramethoxysilane, tetraethoxysilane, tetra-n-propoxysilane, tetraisopropoxysilane, tetra-n-butoxysilane, tetraisobutoxysilane, tetra-sec-butoxysilane, tetra-t-butoxysilane, tetraphenoxysilane, monoethoxytrimethoxysilane, monobutoxytrimethoxysilane, monopentoxytrimethoxysilane, monohetoxytrimethoxysilane, dimethoxydiethoxysilane, and dimethoxydibutoxysilane. These can be used alone or in combination of two or more.
[0040] In the present invention, it is preferable to use a tetraalkoxysilane condensate (c1) (hereinafter referred to as "component (c1)") containing an alkoxyl group having 1 to 2 carbon atoms and an alkoxyl group having 3 to 12 carbon atoms. In particular, it is preferable that component (c1) be one in which 5 to 50% by weight of the alkoxyl groups in the entire compound are alkoxyl groups having 3 to 12 carbon atoms.
[0041] Examples of alkoxyl groups having 3 to 12 carbon atoms include linear alkoxyl groups such as n-propoxy, n-butoxy, n-pentyloxy, n-hexyloxy, n-octyloxy, and n-dodecyloxy groups, and branched alkoxyl groups such as isopropoxy, isobutoxy, t-butoxy, sec-butoxy, isopentyloxy, neopentyloxy, isohexyloxy, 3-methylpentyloxy, 1-methylhexyloxy, 1-ethylpentyloxy, 2,3-dimethylbutoxy, 1,5-dimethylhexyloxy, 2-ethylhexyloxy, 1-methylheptyloxy, and t-octyloxy groups.
[0042] Such a component (c1) can be produced by a known method, such as a method of modifying a tetraalkoxysilane condensate having an alkoxyl group having 1 to 2 carbon atoms with an alcohol having 3 to 12 carbon atoms.
[0043] The mixing ratio of component (C) is preferably 0.1 to 50 parts by weight (more preferably 1 to 30 parts by weight) per 100 parts by weight of the resin solid content of component (A). If component (C) is in this range, excellent weather resistance, stain resistance, and other effects can be obtained.
[0044] The mixing ratio of the (B) component to the (C) component is preferably 5 to 80 parts by weight (more preferably 10 to 60 parts by weight) of the (C) component per 100 parts by weight of the solid content of the (B) component. If the (C) component is in this range, excellent weather resistance, stain resistance, and other effects can be obtained.
[0045] The curing agent of the present invention can be produced by uniformly stirring and mixing the above components (B) and (C) by a conventional method.
[0046] (covering material) The coating material of the present invention is a multi-liquid coating material having the above-mentioned base agent and the above-mentioned curing agent, and is used by uniformly stirring and mixing the base agent and curing agent in a conventional manner when applied. Furthermore, the coating material of the present invention is characterized by including a curing catalyst (D) (hereinafter also referred to as "component (D)"). Component (D) is a substance that mainly acts to promote the reaction between component (A) and component (B), and can impart excellent initial curing properties. This allows for curing properties that allow walking on the day after application to be obtained. It is considered best that this curing time can be adjusted to 17 hours or less throughout the year. Examples of such component (D) include various types of amine catalysts, organometallic catalysts, and inorganic catalysts. Examples of amine catalysts include ethylenediamine, triethylenediamine, triethylamine, ethanolamine, diethanolamine, and hexamethylenediamine, or derivatives thereof, or mixtures thereof with solvents. Examples of organometallic catalysts include organometallic compounds such as dibutyltin dilaurate and dibutyltin diacetate; and organometallic salts such as potassium acetate, zinc stearate, calcium stearate, lead stearate, aluminum stearate, and tin octoate. Examples of inorganic catalysts include tin chloride. These may be used alone or in combination with two or more kinds, and may also be used in combination with a solvent. In the present invention, it is particularly preferable that the catalyst contains an organometallic catalyst.
[0047] The component (D) may be mixed into at least one of the base agent and the curing agent, but may also be added when the base agent and the curing agent are mixed. Specific coating material responses include: A two-component coating material in which the base agent contains components (A) and (D) and the hardener contains components (B) and (C), A two-component coating material in which the base agent contains component (A) and the hardener contains components (B), (C), and (D); A two-component coating material in which the base agent contains components (A) and (D) and the hardener contains components (B), (C), and (D); A three-component coating material in which the base agent contains component (A), the hardener contains components (B) and (C), and further contains a separate component (D), etc.
[0048] The content (active ingredient) of the (D) component is preferably 0.005 to 3 parts by weight (more preferably 0.01 to 2 parts by weight) per 100 parts by weight of the solid content of the (A) component, and is preferably 0.01 to 3 parts by weight (more preferably 0.02 to 2 parts by weight) per 100 parts by weight of the solid content of the (B) component.
[0049] Furthermore, the coating material of the present invention preferably contains a dehydrating agent (E) (hereinafter also referred to as "component (E)") in addition to the above-mentioned components in the base agent and / or curing agent. Examples of component (E) include tosyl isocyanate, vinyltrimethoxysilane, calcium oxide, zeolite, p-toluenesulfonyl isocyanate, 3-ethyl-2-methyl-2-(3-methylbutyl)-1,3-oxazolidine, trimethyl orthoformate, triethyl orthoformate, trimethyl orthoacetate, and triethyl orthoacetate. These can be used alone or in combination of two or more. The (E) component may be mixed with at least one of the base agent and the curing agent. In the present invention, it is particularly preferable to mix the (E) component with the curing agent. By including the (E) component in the curing agent, the storage stability of the (B) component can be ensured, and therefore, when mixed with the base agent, the (A) component and the (B) component can react sufficiently to form a coating, thereby further enhancing the effects of the present invention.
[0050] The content (active ingredient) of the (E) component is preferably 0.005 to 5 parts by weight (more preferably 0.01 to 3 parts by weight) per 100 parts by weight of the solid content of the (A) component, and is preferably 0.01 to 10 parts by weight (more preferably 0.02 to 5 parts by weight) per 100 parts by weight of the solid content of the (B) component.
[0051] Furthermore, the coating material of the present invention preferably contains a powder component (F) (hereinafter also referred to as "component (F)") in addition to the above-mentioned components in the base agent and / or curing agent. Examples of component (F) include color pigments and extender pigments.
[0052] As the color pigment, a chromatic pigment, a white pigment, a black pigment, etc. can be used. By including such a color pigment, it is possible to express various colors. Among them, the chromatic pigment is a pigment that exhibits a chromatic color such as yellow, orange, red, green, blue, purple, etc. Examples of such chromatic pigments include inorganic pigments such as ferric oxide, ferric oxide hydrous, ultramarine, cobalt blue, and cobalt green, and organic pigments such as azo, naphthol, pyrazolone, anthraquinone, perylene, quinacridone, disazo, isoindolinone, benzimidazole, phthalocyanine, and quinophthalone. On the other hand, the white pigment is a pigment that exhibits white color, and examples thereof include titanium oxide, zinc oxide, and aluminum oxide. The black pigment is a pigment that exhibits a black color, and examples thereof include inorganic pigments such as iron black, iron-manganese composite oxide, iron-copper-manganese composite oxide, iron-chromium-cobalt composite oxide, copper-chromium composite oxide, copper-manganese-chromium composite oxide, and carbon black. These can be used alone or in combination of two or more. The surface of the pigment may be treated in some way.
[0053] The average particle size of the color pigment is preferably 1 μm or less, more preferably 0.01 to 0.9 μm. The average particle size of the color pigment is a value measured by a laser diffraction particle size distribution measuring device. The mixing ratio of the color pigment is preferably 1 to 200 parts by weight (more preferably 5 to 150 parts by weight) per 100 parts by weight of the solid content of the component (A).
[0054] The extender pigment can be used for the purpose of, for example, adjusting the solid content, adjusting the viscosity, adjusting the gloss (reducing the gloss, etc.), or improving the storage stability and pigment miscibility. Examples of the extender pigment include heavy calcium carbonate, light calcium carbonate, kaolin, clay, bentonite, china clay, diatomaceous earth, hydrous fine powder of silicic acid, talc, baryte powder, barium sulfate, precipitated barium sulfate, barium carbonate, magnesium carbonate, silica powder, aluminum hydroxide, etc., which may be subjected to some treatment (surface treatment, etc.). These can be used alone or in combination of two or more kinds.
[0055] The average particle size of the extender pigment is preferably 0.01 to 10 μm (more preferably 0.05 to 5 μm). The average particle size of the extender pigment is a value measured by a laser diffraction particle size distribution measuring device. The blending ratio of the extender pigment is preferably 1 to 150 parts by weight (more preferably 5 to 100 parts by weight) per 100 parts by weight of the solid content of component (A).
[0056] The mixing ratio of the (F) component is preferably 1 to 300 parts by weight (more preferably 5 to 250 parts by weight) relative to 100 parts by weight of the solid content of the (A) component. When the (F) component contains a powder component (f1) (hereinafter also referred to as "(f1) component") having a specific gravity of 3.0 or more, it is preferable to contain a powder component (f2) (hereinafter also referred to as "(f2) component") having a specific gravity of less than 3.0 in combination. The mixing weight ratio [(f1) / (f2)] of the (f2) component to the (f1) component is preferably 99.5 / 0.5 to 70 / 30 (more preferably 99 / 1 to 80 / 20). This enhances the dispersion stability of the (F) component relative to the (A) component, and allows excellent pigment compatibility, color stability, and gloss to be obtained. It is also advantageous in improving weather resistance. The reason why such an effect is exhibited is not limited, but it is presumed that by using component (f2) in combination with component (f1), which has a large specific gravity, component (f2) acts as a spacer for component (f1), thereby enhancing the dispersion stability of component (f1).
[0057] The coating material of the present invention may contain various components in the base agent and / or curing agent in addition to the above-mentioned components to the extent that the effect of the present invention is not affected. Examples of such components include plasticizers, preservatives, antifungal agents, anti-algae agents, defoamers, leveling agents, pigment dispersants, thickeners, antiskinning agents, matting agents, UV absorbers, light stabilizers, antioxidants, solvents, etc. Also, the coating material of the present invention may contain resin components other than the above-mentioned component (A). The coating material of the present invention is a multi-liquid type coating material having a base agent and a curing agent, and is used by mixing at least the base agent and the curing agent when applying.
[0058] The covering material of the present invention can be applied mainly to buildings, civil engineering structures, etc. In particular, the covering material of the present invention can be suitably applied to roofing materials, etc. Roofing materials are materials that constitute roof parts, and examples thereof include metal roofing materials and ceramic roofing materials. Examples of metal roofing materials include iron, cold-rolled steel, aluminum steel, stainless steel, copper steel, hot-dip galvanized steel, hot-dip zinc-aluminum alloy plated steel, electrolytic galvanized steel, electrolytic alloy plated steel, alloy plated steel, copper plated steel, tin plated steel, and the like, as well as materials which have been surface-treated (for example, with a phosphate-based treatment agent, a chromate-based treatment agent, or the like). Examples of ceramic roofing materials include ceramic tiles, clay tiles, concrete tiles, slate boards, and fiber-reinforced cement boards. The above metal roofing materials and ceramic roofing materials may have various existing coatings, such as at least one coating selected from organic coatings, inorganic coatings, and organic-inorganic composite coatings.
[0059] The above-mentioned metal roofing materials generally have high thermal conductivity and are prone to condensation and the like, but the covering material of the present invention can ensure sufficient resistance to moisture such as condensation, even when a coating is formed on a metal roofing material.
[0060] The coating material of the present invention can be diluted when applied. As the diluent, the above-mentioned aliphatic hydrocarbon-containing non-aqueous solvent is preferable.
[0061] As a coating method, various methods can be used, such as brush coating, roller coating, spray coating, etc. The amount of coating applied during coating is preferably 30 to 250 g / m per coating. 2 , more preferably 50 to 200 g / m 2 In addition, after painting is performed once and the coating film has dried, the next painting (recoating) can be performed. The drying temperature is preferably -10 to 50°C, more preferably 5 to 45°C. The number of coatings is preferably two or more.
[0062] The coating film formed by the coating material of the present invention may be either glossy or matte (including 70% gloss, 50% gloss, 30% gloss, etc.). In the present invention, even if the coating film is glossy, it is possible to form a coating film with excellent finish (gloss, etc.) by suppressing defects such as gloss reduction caused by moisture such as condensation. The glossy coating film is a coating film with a specular gloss of 70 or more (preferably 75 to 90). In addition, the "specular gloss" is a value measured in accordance with JIS K5600-4-7 "specular gloss". Specifically, it is a value obtained by applying a topcoat material to one side of a glass plate using a film applicator with a gap of 150 μm, placing the coated surface horizontally, and drying for 72 hours under standard conditions, and measuring the specular gloss (measurement angle 60 degrees). EXAMPLES
[0063] The following examples will clarify the features of the present invention. (A) Polyol compound (A1) Acrylic polyol compound dispersion (solid content: 50% by weight, hydroxyl value (solid content): 55 KOHmg / g, medium: mineral spirits) (A2) Silicone-containing acrylic polyol compound dispersion (solid content: 50% by weight, hydroxyl value (solid content): 55 KOH mg / g, silicone component content: 3% by weight (SiO 2 conversion), medium: mineral spirits) (A3) Acrylic polyol compound dispersion (solid content: 50% by weight, hydroxyl value (solid content): 28 KOH mg / g, medium: mineral spirits) (A4) Acrylic polyol compound solution (solid content: 50% by weight, hydroxyl value (solid content): 65 KOHmg / g, medium: methyl ethyl ketone) (A5) Acrylic polyol compound solution (solid content: 50% by weight, hydroxyl value (solid content): 40 KOH mg / g, medium: mineral spirits) (A6) Acrylic polyol compound solution (solid content: 50% by weight, hydroxyl value (solid content): 28 KOH mg / g, medium: mineral spirits) The above (A1) to (A3) are non-aqueous dispersion type resins (a1), and the above (A4) to (A6) are soluble type resins (a2). (B) Polyisocyanate compound (hexamethylene diisocyanate derivative solution, solid content: 100% by weight, isocyanate group content: 21% by weight) (C) Silicate compounds (C1) Tetramethoxysilane (C2) i-Butyl alcohol modified tetramethoxysilane compound (average condensation degree 4, ester exchange rate 30%, residual silica rate 40%) (D) Dibutyltin dilaurate solution (active ingredient: 10% by weight, medium: mineral spirits) (E) p-Toluenesulfonyl isocyanate (F) Pigments (F1) Rutile titanium dioxide (specific gravity 4, average particle size 0.45 μm) (F2) Kaolin clay (specific gravity 2.6, average particle size 0.8 μm) (F3) Organically modified bentonite (specific gravity 1.5, average particle size 0.5 μm) (solvent) Aliphatic hydrocarbon-containing non-aqueous solvents: mineral spirits (Additives) Defoamers, thickeners, etc.
[0064] <Preparation of Coating Material 1> ·Main ingredient manufacturing Base agent 1 was prepared by mixing and stirring 48 parts by weight of component (A1), 12 parts by weight of component (A5), 25 parts by weight of component (F1), 10 parts by weight of solvent, and 5 parts by weight of additive. - Hardener manufacturing Curing agent 1 was prepared by mixing and stirring 5.8 parts by weight of component (B), 3 parts by weight of component (C1), 0.05 parts by weight of component (D), 0.2 parts by weight of component (E), and 10.95 parts by weight of solvent. Preparation of coating material The base material 1 (100 parts by weight) and the hardener 1 (20 parts by weight) were mixed ([NCO] / [OH]=1.04) and stirred immediately before painting to obtain the coating material 1.
[0065] <Preparation of coating materials 2 to 14> Except for changing the formulation to that shown in Table 1, the components were mixed and stirred in the same manner as in Coating Material 1 to prepare the base resin and hardener, which were then mixed just before painting to obtain the coating material.
[0066] [Table 1]
[0067] (Examples 1 to 7, Comparative Examples 1 to 7) The following evaluations were carried out on the above Coating Materials 1 to 14. The results are shown in Table 2.
[0068] Rating 1 (initial hardening) Each coating material was applied to the tin plate at a rate of 0.15 kg / m 2 The coating was applied with a roller and dried for 16 hours in an environment of 5℃ and 65% relative humidity, after which the presence or absence of tackiness was evaluated by walking on the coating under standard conditions (temperature 23℃, relative humidity 50%). The evaluation was done on a four-point scale (A>B>C>D: poor), with "A" being smooth to walk on and "D" being strongly tacky.
[0069] Rating 2 (moisture and water resistance) First, each coating material was applied to an aluminum plate at a coating amount of 0.10 kg / m 2 The paint was roller-coated with the composition and left to dry for 72 hours under standard conditions (temperature 23°C, relative humidity 50%) to prepare a test specimen [blank]. Next, each coating material was applied to the aluminum plate in an amount of 0.10 kg / m 2 The coating was roller-coated with 100g of water, left to stand for 2 hours in a 5°C incubator, and then left to stand for 5 minutes under standard conditions (air temperature 23°C, relative humidity 50%) (this cycle allowed condensation to form). This cycle was repeated three times, and then left to stand for 24 hours in a 5°C incubator and 24 hours under standard conditions. The appearance of the coating obtained by the above method was compared with that of the test specimen [blank], and the coating was rated on a four-point scale (A>B>C>D: poor), with "A" indicating no change in appearance and "D" indicating a change (loss of gloss, etc.).
[0070] Rating 3 (weather resistance) Each coating material was spray-painted onto slate roofing materials (amount of paint applied per application: 0.15 kg / m 2 Test specimen [I] was prepared by applying two coats of paint (100% ... The above specimen [I] was exposed for 500 hours using an accelerated weathering tester (Metal Weather; manufactured by Daipla Wintes Co., Ltd.), after which the appearance changes (gloss, color, lifting, peeling, cracking) of the surface of specimen [I] were observed. The appearance changes were compared with those of the specimen before exposure, and the evaluation was performed on a 5-point scale (excellent: AA>A>B>C>D: poor), with "AA" indicating no change and "D" indicating loss of gloss, discoloration, lifting, peeling, or cracking.
[0071] Rating 4 (stain resistance) Each coating material was applied to a tinplate (150mm x 50mm x 0.3mm) so that the dry thickness was 75μm, and the plate was dried for 7 days to prepare a test specimen [II]. All painting and drying were performed under standard conditions. Carbon dispersion (1%) was sprayed onto the specimen [II] prepared by the above method, and after drying (60°C, 1 hour), it was washed with water. The difference in brightness (ΔL value) of the specimen before and after contamination was measured, and the stain resistance test was evaluated. The ΔL value was measured using a TC-1800 color difference meter (manufactured by Tokyo Denshoku Co., Ltd.). The evaluation criteria are: AA: Lightness difference (ΔL value) is less than 5 A: Lightness difference (ΔL value) is 5 or more and less than 10 B: Lightness difference (ΔL value) is 10 or more and less than 20 C: Lightness difference (ΔL value) is 20 to 30 D: Lightness difference (ΔL value) is 30 or more
[0072] Rating 5 (tracking ability) Each coating material was applied to a tinplate (150mm x 50mm x 0.3mm) so that the dry thickness was 75μm, and the plate was dried for 7 days to prepare a test specimen [II]. All painting and drying were performed under standard conditions. For each test piece [II], the test plate was bent according to the JIS K5600-5-1 "Flexibility" method (mandrel diameter: 2 mm), and then the surface condition was observed. Evaluation was performed on a four-level scale (A>B>C>D: poor), with "A" indicating high conformability to the substrate and no cracks, and "D" indicating low conformability to the substrate and cracks.
[0073] [Table 2]
Claims
1. A coating material having a base agent and a curing agent, The base material contains a hydroxyl group-containing resin (A), The curing agent contains a polyisocyanate compound (B) and a silicate compound (C), The coating material further contains a curing catalyst (D), The hydroxyl-containing resin (A) includes a non-aqueous dispersion type resin (a1) having a hydroxyl value of 30 mgKOH / g or more, and a soluble type resin (a2) having a hydroxyl value of 30 mgKOH / g or more, A coating material characterized in that the hydroxyl value of the non-aqueous dispersion type resin (a1) is greater than the hydroxyl value of the soluble type resin (a2).
2. 2. The coating material according to claim 1, wherein the hydroxyl-containing resin (A) contains a silicone component.
3. 3. The coating material according to claim 1, wherein the non-aqueous dispersion type resin (a1) contains a silicone component.
Citation Information
Patent Citations
Heat-insulating paint composition
JP2016160395A