Probe cleaning sheet and manufacturing method thereof

A silicone glass fiber cloth with bonded high and low-density polishing layers addresses bending and bubble issues in probe cleaning cloths, ensuring a flat and efficient cleaning sheet through controlled manufacturing processes.

JP2024159285AActive Publication Date: 2024-11-08CKT TEK

Patent Information

Application Number
JP2023075169
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-28
Publication Date
2024-11-08
Estimated Expiration
2043-04-28

AI Technical Summary

Technical Problem

Existing probe cleaning cloths face issues such as bending, curling, and bubble formation due to thermal expansion and contraction, requiring multiple materials with different temperature characteristics and adhesion processes, which are time-consuming and prone to material deformation.

Method used

A probe cleaning sheet is manufactured using a silicone glass fiber cloth with high and low-density polishing layers bonded through a two-stage printing and firing process, eliminating the need for adhesives and ensuring uniform material properties through controlled baking and cooling.

Benefits of technology

The process prevents denting, curling, and bubble formation, ensuring a flat and durable cleaning sheet with enhanced cleaning efficiency and reduced production time, maintaining probe cleanliness without material deformation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024159285000001_ABST
    Figure 2024159285000001_ABST
Patent Text Reader

Abstract

To provide a probe cleaning cloth that improves the problems of bending, curling, and air bubble generation or the like after process work of thermal expansion, cooling and contraction.SOLUTION: A structural part of a probe cleaning sheet of a low-puncture process comprises a silicone glass fiber cloth layer 103 including a plurality of glass fibers 1031 and silicone 1032 therein, and the silicone 1032 is coated in a gap between the glass fibers 1031 and on surfaces thereof. An abrasive layer set 40 is printed on one side of the silicone glass fiber cloth layer 103. The abrasive layer set 40 includes a high-density abrasive layer 20 and a low-density abrasive layer 30. The high-density abrasive layer 20 is printed and bonded to one side of the silicone glass fiber cloth layer 103. The silicone 1032 is bonded to the high-density abrasive layer 20. The low-density abrasive layer 30 is printed and bonded to an uppermost surface of the high-density abrasive layer 20, and faces the silicone glass fiber cloth layer 103.SELECTED DRAWING: Figure 4
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a probe cleaning sheet with low puncture process and its manufacturing method, which is mainly used for cleaning probes, especially in electromechanical field technology. [Background technology]

[0002] Probes are used as testing equipment to contact the electrodes of various electronic components and perform electrical tests. They are widely used to test a wide variety of electronic components, including semiconductors, liquid crystal panels, blank boards, mounted printed circuit boards, connectors, capacitors, sensors, batteries, etc. In addition to checking electrical continuity, the tests also include collecting data to be used in tests to check whether the components work within a circuit (circuit tests) and checking operation during functional tests (functional tests). If the probe has impurities, defects, or missing parts, it may affect the test results of the electronic components.

[0003] In addition to the above, the most common way to remove the dirt accumulated on the probe is to lightly brush the tip of the probe with QA's natural fiber brush (TBR-1). Finally, remove the dust with a vacuum cleaner or wipe it off with a probe cleaning cloth commonly found on the market. However, the probe cleaning cloths on the market are made by layering different materials during the manufacturing process, and the polymerization between the different materials requires adhesives to adhere them, so the known probe cleaning cloths need to go through the baking heating and cooling processes during the manufacturing process. The different materials will change the properties of the main body due to the above-mentioned heating and cooling processes, and the amount of change will be different after thermal expansion and cooling contraction, and the ductility will change, and the probe cleaning cloth will have a concave and curved shape, and when it is concave and curved, gaps will occur between the different materials, which will generate air bubbles.

[0004] In addition to the above problems, the conventional probe cleaning cloth is made of a hard material, which takes time and effort to manufacture, and it will break if care is not taken. Therefore, it is necessary for related parties to improve the problems of the conventional probe cleaning cloth. Summary of the Invention [Problem to be solved by the invention]

[0005] The main objective of the present invention is to provide a conventional probe cleaning cloth that can be manufactured more quickly and avoids the product becoming dented, curled, or having bubbles, and that alleviates problems such as bending, curling, and the generation of bubbles after the process of thermal expansion, cooling, and contraction, which are caused by different materials simply polymerizing and adhering to each other, and each material having its own temperature characteristics. [Means for solving the problem]

[0006] In order to achieve the above objects and effects, the steps of the method for producing the probe cleaning sheet of the present invention include the following: In the material preparation step, a rolled silicone fiberglass cloth is prepared, and the silicone fiberglass cloth is cut to a required size and fed into a printing machine. In the first printing step, the printing machine is opened, the silicon glass fiber cloth is wound around the printing machine jig, and the printing machine performs high-density printing on one side of the silicon glass fiber cloth to form a high-density abrasive layer on one side of the silicon glass fiber cloth. In the primary baking step, the silicon glass fiber cloth on which the high-density abrasive layer is formed is placed in a baking machine to perform a primary baking operation, thereby bonding between the silicon on the silicon glass fiber cloth and the high-density abrasive layer. In the primary cooling step, after the above-mentioned primary firing step is completed, the silicon glass fiber cloth having the high-density abrasive layer is then placed in a cooling machine, and the primary cooling operation is carried out at the temperature determined by the cooling machine, so as to bond between the silicon in the silicon glass fiber cloth and the high-density abrasive layer. In the secondary printing step, the silicon glass fiber cloth after the primary cooling step described above is put into the printing machine again, and low-density printing is performed by the printing machine to form a low-density abrasive layer on one side of the high-density abrasive layer, and the low-density abrasive layer faces the silicon glass fiber cloth. In the second baking step, the silicon glass fiber cloth is put into the baking machine again to perform the second baking operation, so that the low-density abrasive layer and the high-density abrasive layer can be bonded together. In the second cooling step, after the second firing step is completed, the low-density abrasive layer is hardened and firmly bonded to the high-density abrasive layer by cooling again in the cooling machine.

[0007] The low puncture process probe cleaning sheet of the present invention comprises: The silicone fiberglass cloth layer has a plurality of glass fibers and silicone therein, the silicone being applied to the gaps between and on the surfaces of each of the glass fibers. An abrasive layer set is printed on one side of the silicon fiberglass cloth layer, the abrasive layer set including at least one high density abrasive layer and at least one low density abrasive layer. The at least one high density abrasive layer is printed on one side of the silicon fiberglass cloth layer, the silicon adheres the at least one high density abrasive layer. The at least one low density abrasive layer is printed on the top surface of the at least one high density abrasive layer and faces the silicon fiberglass cloth layer. The silicon glass fiber cloth layer and the abrasive layer set are printed together, and the high temperature resistance and high tensile strength of the silicon glass fiber cloth layer are utilized to prevent the probe cleaning sheet from being dented, curved or curled. Furthermore, the work time required for printing to bond the silicon glass fiber cloth layer and the abrasive layer set is further shortened, further improving production efficiency. Effect of the Invention

[0008] The present invention has high tensile strength as a cloth characteristic of the silicon glass fiber cloth layer. After the polishing layer set is combined with the silicon glass fiber cloth, the problems of concave curvature and curling are eliminated, the product is flatter, and air bubbles are prevented from entering the probe cleaning sheet, which affects the cleaning of the probe. In addition, in the manufacture of the probe cleaning sheet, the high-density polishing layer is printed and attached to the silicon glass fiber cloth by printing operation, which greatly reduces the need to add new adhesive between layers, saves the time to wait for the adhesive to dry, and more importantly, does not require consideration of the different baking and cooling temperatures suitable for each material. This reliably prevents the occurrence of problems such as deformation, concave curvature, curling, and air bubbles in the probe cleaning sheet. As a result, the present invention is practical and inventive, has excellent industrial applicability, and can contribute to society. [Brief description of the drawings]

[0009] [Figure 1] FIG. 2 is a step flow diagram of the present invention. [Diagram 2] FIG. 2 is a schematic flow diagram of the present invention. [Diagram 3] FIG. 2 is a perspective view of the probe cleaning sheet of the present invention; [Figure 4] FIG. 4 is a cross-sectional view taken along line IV-IV of FIG. [Diagram 5] FIG. 2 is a perspective view showing another embodiment of the present invention; [Figure 6]6 is a cross-sectional view of the high-density abrasive layer and the low-density abrasive layer taken along the line VI-VI in FIG. 5. [Figure 7] FIG. 11 is a perspective view showing still another embodiment of the present invention; [Figure 8] 8 is a cross-sectional view taken along line VIII-VIII in FIG. 7. [Figure 9] FIG. 11 is a perspective view showing still another embodiment of the present invention; [Figure 10] FIG. 10 is a cross-sectional view taken along the line XX in FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0010] (One embodiment) In order to clarify the above-mentioned objects and advantages achieved by the present invention, the following diagrams and examples are presented to describe the features and advantages of the present invention in detail. As shown in Figures 1 to 4, the steps of the present invention's step flow are defined, the method for producing the probe cleaning sheet of the present invention, and the steps of producing the probe cleaning sheet 100 include: Regarding the material preparation step S1, it prepares a rolled and molded silicon glass fiber cloth 10, cuts the silicon glass fiber cloth 10 into a required size, and puts it into the printing machine 101. In the primary printing step S2, the printer 101 is opened to insert the piece of silicon glass fiber cloth 10, and the printer 101 performs high-density printing on one side of the silicon glass fiber cloth 10 to form a high-density abrasive layer 20 on one side of the silicon glass fiber cloth 10. In the primary firing step S3, the silicon glass fiber cloth 10 on which the high-density abrasive layer 20 is formed is placed in a firing machine 201 to perform a primary firing operation, thereby bonding the high-density abrasive layer 20 to the silicon 1032 of the silicon glass fiber cloth 10. Regarding the primary cooling step S4, after the above-mentioned primary firing step S3 is completed, the silicon glass fiber cloth 10 having the high-density polishing layer 20 is then put into a chiller 202, and a primary cooling operation is carried out in the chiller 202. In the secondary printing step S5, the silicon glass fiber cloth 10 after the above-mentioned primary cooling step S4 is put into the printer 101 again, and low-density printing is performed by the printer 101 to form a low-density abrasive layer 30 on one side of the high-density abrasive layer 20, and the low-density abrasive layer 30 faces the silicon glass fiber cloth 10. In the secondary baking step S6, the silicon glass fiber cloth 10 is put into the baking machine 201 again to perform the secondary baking operation, so that the low-density abrasive layer 30 and the high-density abrasive layer 20 can be bonded together. In the second cooling step S7, after the above-mentioned second firing step S6 is completed, the product is again placed in the cooler 202 for cooling. In the first firing step S3 and the second firing step S6, a two-stage firing method is adopted, and the first stage is pre-firing at 60-70°C for 5-10 minutes. The second stage is firing at 180-200°C for 20-30 minutes.

[0011] The structure is defined according to the above-mentioned manufacturing method (the already defined parts are not defined again). In the structure part of the present invention, the probe cleaning sheet 100 mainly includes: The inside of the silicon glass fiber cloth layer 103 (i.e., the aforementioned silicon glass fiber cloth 10 is only distinguished by its manufacturing method and pure structural definition) has a plurality of glass fibers 1031 and silicon 1032, and the silicon 1032 is applied to the gaps between and on the surface of each glass fiber 1031. The abrasive layer set 40 is printed on one side of the silicon fiberglass cloth layer 103, and the abrasive layer set 40 includes at least one high density abrasive layer 20 and at least one low density abrasive layer 30. The at least one high density abrasive layer 20 is printed on one side of the silicon fiberglass cloth layer 103, and the silicon 1032 adheres the at least one high density abrasive layer 20. The at least one low density abrasive layer 30 is printed on the top surface of the at least one high density abrasive layer 20 and faces the silicon fiberglass cloth layer 103. The silicon glass fiber cloth layer 103 and the abrasive layer set 40 are printed together, and the high tensile strength of the silicon glass fiber cloth layer 103 prevents the probe cleaning sheet 100 from being dented, curved or curled. Furthermore, the time required for printing to bond the silicon glass fiber cloth layer 103 and the abrasive layer set 40 is further shortened, further improving production efficiency.

[0012] In the above description of the manufacturing process and structure of the probe cleaning sheet 100, the silicon glass fiber cloth 10 is used, and the high-density polishing layer 20 and the low-density polishing layer 30 are further bonded by printing. The silicon glass fiber cloth 10 body has the characteristics of high temperature resistance, corrosion resistance, high tensile strength, high insulation, heat resistance from low temperatures of -50 degrees to high temperatures of 250 degrees, chemical corrosion resistance, deterioration resistance and wear resistance. Therefore, during the baking and cooling processes in the manufacturing process, the probe cleaning sheet 100 is unlikely to be dented, curved or curled. The finished product has good flatness and integrity, and no gaps or bubbles are generated, so that the probe can be reliably cleaned during the probe operation process and the outer surface of the probe is not affected. In addition, in terms of manufacturing, since the silicon glass fiber cloth 10 is used, the high-density abrasive layer 20 can be printed directly on the surface of the silicon glass fiber cloth 10, not only does it not damage the silicon glass fiber cloth 10, but it can also reliably print the high-density abrasive layer 20 on the silicon glass fiber cloth 10, and there is no need to add a sizing agent such as an adhesive. Furthermore, since the silicon 1032 contained in the silicon glass fiber cloth 10 itself is used, there is no need to consider problems such as thermal expansion and contraction caused by changes in firing and cooling.

[0013] Now that the main features of the manufacturing process of the present invention have been clarified, the detailed features of the manufacturing method will be described in detail. First, as shown in FIG. 4, the surface treatment step S8 is carried out after the secondary cooling step S7 so that the probe cleaning sheet 100 can be stored after completion of manufacturing and its surface can be protected when not in use. After a treatment agent is applied to the surface of the silicon glass fiber cloth 10 opposite to the high-density polishing layer 20, an adhesive 70 is attached, and a release film 60 is attached to the surface of the low-density polishing layer 30. The release film 60 can be freely attached and peeled off from the low-density polishing layer 30. The main purpose of the release film 60 is to prevent the adhesion of foreign matter. When the release film 60 is peeled off, the needle tip of the probe pierces the surface of the low-density polishing layer 30 and is cleaned by polishing, and then pierces the high-density polishing layer 20 and is further polished and cleaned, effectively removing dirt from the surface of the probe needle. Furthermore, the negative charge and oleophilic properties of the silicon 1032 itself in the silicon glass fiber cloth 10 transfers the dirt of the probe onto the abrasive layer set 40 (including the low-density abrasive layer 30 and the high-density abrasive layer 20) and the silicon 1032 of the silicon glass fiber cloth 10. The use of the multiple glass fibers 1031 of the silicon glass fiber cloth 10 also prevents the needle tip from being damaged by the overpressure of the probe directly hitting the machine base. The adhesive 70 is used to attach the probe cleaning sheet 100 onto the required machine base.

[0014] In addition, in forming the high-density abrasive layer 20 and the low-density abrasive layer 30 of the present invention, a printing material is added to the printer 101 used in the first printing step S2 and the second printing step S5. This printing material is mainly composed of ink A and a plurality of abrasive grains B, and each abrasive grain B is mainly added into the ink A, followed by stirring and refrigeration. Among them, the ink A is made of silicon material, and the abrasive grains B are aluminum oxide. The grains of each abrasive grain B have a diameter of 2 to 5 um, and the abrasive grains B are subjected to a surface treatment with silicon affinity in order to increase the cross-linking force with the ink A and prevent the abrasive grains B from peeling off during use. In addition, the difference between the high-density abrasive layer 20 and the low-density abrasive layer 30 lies in the distance between each abrasive grain B added to the ink A, and the distance between each abrasive grain B of the high-density abrasive layer 20 is smaller than the distance between each abrasive grain B of the low-density abrasive layer 30, so that the high-density abrasive layer 20 and the low-density abrasive layer 30 have different cleaning effects on the probe tip. As shown in Figures 3 and 5.

[0015] Finally, in order to enhance the cleaning power of the probe, the abrasive layer set 40 of the present invention (including the high-density abrasive layer 20 and the low-density abrasive layer 30) may be installed in multiple layers as shown in Figure 4 and Figure 5, in addition to being installed one layer at a time as shown in Figure 3, and the number of the high-density abrasive layer 20 and the low-density abrasive layer 30 may be two layers each, and each layer may be installed in an alternating arrangement. By installing multiple layers, the cleaning power of the probe cleaning sheet 100 for the probe tip is enhanced. Furthermore, in order to meet the needs of users, the amount of silicone 1032 in the silicone fiberglass cloth layer 103 can be adjusted. In addition to filling both the upper and lower layers of the spun glass fiber 1031 with silicone 1032 as shown in Figure 4, the silicone 1032 can be filled only on one side of the spun glass fiber 1031 as shown in Figures 7 and 8, and the adhesive 70 can be directly attached to another side of the spun glass fiber 1031, so that the thickness of the probe cleaning sheet 100 can be adjusted according to the user's needs. Alternatively, the abrasive layer set 40 (including the high-density abrasive layer 20 and the low-density abrasive layer 30) can be printed on both the upper and lower layers of the spun silicon glass fiber cloth layer 103. Finally, by protecting it with a release film 60, as shown in Figures 9 and 10, a single probe cleaning sheet 100 can be used on both sides. [Explanation of symbols]

[0016] 10 Silicone Fiberglass Cloth 100 Probe Cleaning Sheets 101 Printing machine 103 Silicone fiberglass cloth layer 1031 Glass Fiber 1032 Silicon 20 High-density polishing layer 201 Baking machine 202 Cooler 30 Low density polishing layer 40 Abrasive Layer Set 50 polishing machine 60 Release film 70 Adhesive A Ink B Abrasive grain S1 Material preparation step S2 First printing step S3 First firing step S4 Primary cooling step S5 Secondary Print Step S6 Secondary firing step S7 Secondary cooling step S8 Surface treatment step

Claims

1. In the method for producing a probe cleaning sheet, A material preparation step of preparing a rolled silicon glass fiber cloth, cutting the silicon glass fiber cloth to a required size, and placing the cloth on a jig of a printing machine; a primary printing step of opening the printer and performing high density printing on one side of the silicon glass fiber cloth using the printer to form a high density abrasive layer on one side of the silicon glass fiber cloth; a primary firing step of placing the silicon glass fiber cloth on which the high-density abrasive layer is formed in a firing machine and performing a primary firing operation to bond the high-density abrasive layer to the silicon of the silicon glass fiber cloth; After the primary firing step is completed, the silicon glass fiber cloth having the high density polishing layer is put into a cooling machine and the primary cooling process is performed according to the temperature of the cooling machine. The silicon glass fiber cloth after the first cooling step is put into the printer again, and low-density printing is performed by the printer to form a low-density abrasive layer on one side of the high-density abrasive layer, and the low-density abrasive layer faces the silicon glass fiber cloth in a second printing step; a secondary firing step in which the silicon glass fiber cloth is placed in the firing machine again to perform a secondary firing operation, thereby bonding the low-density abrasive layer and the high-density abrasive layer; After the secondary firing step is completed, the product is placed in the cooling machine again for a secondary cooling step; A method for producing a probe cleaning sheet, comprising:

2. 2. The method for manufacturing a probe cleaning sheet according to claim 1, further comprising the step of: after the secondary cooling step, performing a surface treatment step, in which a treatment agent is applied to one side of the silicon glass fiber cloth facing the high-density abrasive layer in the surface treatment step.

3. 3. The method for manufacturing a probe cleaning sheet according to claim 2, further comprising attaching a release film to the surface of the low-density abrasive layer after the surface treatment step, the release film being capable of being freely attached and detached from the low-density abrasive layer.

4. 4. The method for producing a probe cleaning sheet according to claim 3, further comprising the step of applying an adhesive to the side of the silicon glass fiber cloth opposite to the high density abrasive layer.

5. A method for manufacturing a probe cleaning sheet as described in any one of claims 1 to 4, characterized in that in the primary printing step, the high-density abrasive layer printed on the silicon glass fiber cloth and the low-density abrasive layer printed on the high-density abrasive layer further contain ink and a plurality of abrasive grains, the ink and the abrasive grains are mixed and stirred with each other, and the distance between each abrasive grain in the high-density abrasive layer is smaller than the distance between each abrasive grain in the low-density abrasive layer.

6. 6. The method for manufacturing a probe cleaning sheet according to claim 5, wherein the ink is made of a silicon material, the abrasive particles are spherical aluminum oxide particles, and the particle diameter of each abrasive particle is 2 to 5 um.

7. a silicone fiberglass cloth layer having a plurality of glass fibers and silicone therein, the silicone being applied to gaps between the glass fibers and to the surface; a polishing layer set printed on one side of the silicon glass fiber cloth layer, the polishing layer set including at least one high density polishing layer and at least one low density polishing layer, the at least one high density polishing layer being printed on one side of the silicon glass fiber cloth layer, the silicone adhering the at least one high density polishing layer, the at least one low density polishing layer being printed on the top surface of the at least one high density polishing layer, the polishing layer set facing the silicon glass fiber cloth layer; In a probe cleaning sheet with a low puncture process comprising: The probe cleaning sheet has a low puncture process, characterized in that the silicone glass fiber cloth layer and the abrasive layer set are printed together, and the elasticity of the silicone glass fiber cloth layer prevents the probe cleaning sheet from being concavely curved or curled. Furthermore, the work time required for printing to bond the silicone glass fiber cloth layer and the abrasive layer set is further shortened, thereby further improving production efficiency.

8. The probe cleaning sheet for the low puncture process described in claim 7, characterized in that the probe cleaning sheet for the low puncture process further has a release film attached to the surface of the at least one low-density abrasive layer, and the release film can be freely adhered to and peeled from the at least one low-density abrasive layer.

9. 9. The probe cleaning sheet according to claim 8, further comprising an adhesive applied to the silicon glass fiber cloth layer on the opposite side to the high density abrasive layer.

10. The probe cleaning sheet for a low puncture process as described in claim 7, characterized in that the at least one high-density abrasive layer and the at least one low-density abrasive layer further contain ink and a plurality of abrasive grains, the ink and the abrasive grains are mixed and stirred with each other, and the distance between each abrasive grain in the high-density abrasive layer is smaller than the distance between each abrasive grain in the low-density abrasive layer.

11. The probe cleaning sheet according to claim 10, wherein the ink is made of silicon material, the abrasive particles are spherical aluminum oxide particles, and the diameter of each abrasive particle is 2 to 5 μm.

Citation Information

Patent Citations

  • Method and equipment for electrical inspection of base

    JP1999006864A

  • Member and method for cleaning of probe tip, and test method for semiconductor wafer

    JP1999087438A

  • Member for cleaning tip of probe, device for cleaning probe, and method of cleaning tip of probe

    JP2004271389A

  • Apparatuses, device, and methods for cleaning tester interface contact elements and support hardware

    JP2011117938A

  • Cleaning sheet, transfer member provided with cleaning function, and method for cleaning substrate processing apparatus

    WO2007049462A1

Cited By

  • Boiling-type heat transfer tube and method for manufacturing boiling-type heat transfer tube

    WO2026058840A1