Metal rolled sheet and manufacturing method for metal product
The rolled metal sheet with non-perpendicular angles addresses durability and breakage issues by parallel cutting, enhancing bending resistance and reducing oil pit-induced fractures in miniaturized metal products.
Patent Information
- Application Number
- JP2024118009
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2024-07-23
- Publication Date
- 2024-11-19
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing metal products, such as leaf springs, connectors, and terminals, face issues with reduced durability due to perpendicular alignment with oil pits and bending, which worsens with miniaturization and thinning, leading to fractures and decreased flexibility.
A rolled metal sheet with non-perpendicular angles between the longitudinal direction of the metal product and the direction of oil pits, allowing for parallel cutting to improve durability and resistance to breakage, maintaining the same cutting method.
Enhances durability against bending and reduces breakage from oil pits without altering the cutting process, ensuring a balanced performance in miniaturized metal products.
Smart Images

Figure 2024161389000001_ABST
Abstract
Description
[Technical field]
[0001] FIELD OF THE DISCLOSURE The present disclosure relates to rolled metal sheets and methods of making metal products that include cutting metal products from rolled metal sheets. [Background technology]
[0002] Metal products such as leaf springs, connectors, and terminals are generally manufactured through a process of press-punching a metal sheet that has been rolled to a predetermined thickness into a predetermined shape. In order to facilitate subsequent processes (bending by pressing or connecting to other parts), the press-punching process is generally performed so that the longitudinal direction of the metal product (301) is perpendicular to the longitudinal direction (typically the rolling direction) of the metal sheet (300), as shown in Fig. 3 (Patent Document 1, Patent Document 2). [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2005-206942 A [Patent Document 2] JP 2015-60770 A Summary of the Invention [Problem to be solved by the invention]
[0004] When manufacturing a metal sheet (300) by rolling, the longitudinal direction of the metal sheet (300) generally coincides with the rolling direction from the viewpoint of production efficiency. In this case, if the longitudinal direction of the metal product (301) cut out from the metal sheet (300) is perpendicular to the longitudinal direction of the metal sheet (300), there is a problem that the durability when the portion extending in the longitudinal direction is bent so that the bending axis is perpendicular to the longitudinal direction, for example, the bending property of the BADWAY in press processing, is likely to decrease. For this reason, in order to improve the bending property of the portion extending in the longitudinal direction of the metal product (301), it is considered desirable that the longitudinal direction of the metal product (301) cut out from the metal sheet (300) is parallel to the longitudinal direction of the metal sheet (301).
[0005] On the other hand, the metal sheet (300) produced by rolling inevitably develops streak-like depressions called oil pits (306) that extend in a direction perpendicular to the rolling direction due to the lubricating oil. In this case, if the longitudinal direction of the metal product (301) cut out from the metal sheet (300) is parallel to the longitudinal direction of the metal sheet (300), the longitudinal direction of the metal product (301) will be perpendicular to the longitudinal direction of the oil pits (306). However, if the longitudinal direction of the metal product (301) is perpendicular to the longitudinal direction of the oil pits (306), there is a problem that the metal product is more likely to break starting from the oil pits (306). Examples of breaks starting from oil pits include breaks caused by the impact of dropping an electronic device to the ground and breaks caused by metal fatigue when repeatedly bending the electronic device.
[0006] In recent years, there has been a remarkable demand for miniaturization of metal products for electronic devices, such as leaf springs, connectors, and terminals, and it is thought that the problem will become more serious as metal products become thinner.
[0007] The present invention has been made in consideration of the above circumstances, and an object of the present invention is, in one aspect, to provide a metal rolled sheet suitable for cutting out metal products having an excellent balance between resistance to breakage caused by oil pits and durability against bending. In another aspect, the present invention has an object of providing a method for manufacturing a metal product having a longitudinal direction using the metal rolled sheet according to the present invention. [Means for solving the problem]
[0008] The present invention is exemplified below. (1) A rectangular metal rolled sheet having an edge extending in a first direction and an edge extending in a second direction perpendicular to the first direction, wherein an angle A1 between the longitudinal direction of an oil pit and the first direction and an angle A2 between the longitudinal direction of the oil pit and the second direction are both non-right angles. (2) The rolled sheet according to (1), having a thickness of 5 to 100 μm. (3) The rolled sheet according to (1) or (2), wherein the angle A1 and the angle A2 are both 5 to 85°. (4) The rolled sheet according to any one of (1) to (3), which is made of copper or a copper alloy. (5) The rolled sheet according to any one of (1) to (4), having a tensile strength in the rolling direction of 500 MPa or more. (6) A method for producing a metal product having a longitudinal direction, comprising cutting out a rolled sheet described in any one of (1) to (5) so that the longitudinal direction is parallel to a first direction or a second direction. (7) The manufacturing method according to (6), wherein the metal product is a leaf spring, a connector or a terminal. Effect of the Invention
[0009] According to the metal rolled sheet of one embodiment of the present invention, when a metal product is cut out from the rolled sheet so that the longitudinal direction of the metal product is parallel to the first or second direction of the rolled sheet, the longitudinal direction of the metal product is not perpendicular to the rolling direction (the direction perpendicular to the longitudinal direction of the oil pit). In other words, the rolling direction is oblique to the longitudinal direction of the metal product. This improves durability when the portion extending in the longitudinal direction of the metal product is bent so that the bending axis is perpendicular to the longitudinal direction.
[0010] In addition, when the metal product is cut out from the rolled sheet so that the longitudinal direction of the metal product is parallel to the first or second direction of the rolled sheet, the longitudinal direction of the metal product is not perpendicular to the longitudinal direction of the oil pits. In other words, the extension direction of the oil pits is oblique to the longitudinal direction of the metal product. Therefore, the cut out metal product is less susceptible to breakage caused by the oil pits.
[0011] In other words, by using the metal rolled sheet, it is possible to produce a metal product that has an excellent balance between resistance to breakage caused by oil pits and durability against bending, without changing the cutting method such as press punching that has been used in the past. In addition, since there is no change in the cutting method, there is no impact on the subsequent processes (bending by pressing or connection with other parts). [Brief description of the drawings]
[0012] [Figure 1] FIG. 2 is a schematic diagram showing an example of a method for cutting out a metal rolled sheet according to an embodiment of the present invention from a metal rolled plate. [Diagram 2] FIG. 2 is a schematic diagram showing an example of a method for cutting out a metal product from a rolled metal sheet according to the present invention. [Diagram 3] FIG. 1 is a schematic diagram showing an example of a conventional method for cutting metal products from a rolled metal sheet. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0013] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. However, the present invention is not limited to the following embodiment, and it should be understood that design changes, improvements, etc. may be made as appropriate based on the ordinary knowledge of those skilled in the art without departing from the spirit of the present invention.
[0014] FIG. 1 is a schematic diagram showing an example of a method for cutting out a metal rolled sheet (100) according to one embodiment of the present invention from a rolled metal plate. The rolled metal plate (110) has long sides (112) extending in the rolling direction and short sides (114) extending in a direction perpendicular to the rolling direction. The metal rolled sheet (100) according to this embodiment can be obtained by cutting out a rectangular shape from the rolled metal plate (110) such that the four sides are not parallel to any of the long sides (112) and the short sides (114). A plurality of oil pits (106) extending in a direction perpendicular to the rolling direction are formed on the surface of the rolled metal plate (110).
[0015] The metal rolled sheet (100) is a rectangular metal rolled sheet having a side (102) extending in a first direction and a side (104) extending in a second direction perpendicular to the first direction, and the angle A1 (in the range of 0 to 90°) between the longitudinal direction of the oil pit (106) and the first direction, and the angle A2 (in the range of 0 to 90°) between the longitudinal direction of the oil pit and the second direction are both non-right angles. The length of the side (102) extending in the first direction can be the same as or longer than the length of the side (104) extending in the second direction. Since the side extending in the first direction of the metal rolled sheet (100) is longer than the side extending in the second direction, a long metal rolled sheet (100) is obtained, which has the advantage of making it easier to increase the number of metal products obtained from one metal rolled sheet (100). Note that A1+A2=90°.
[0016] When cutting out the metal product (108) from the rolled metal sheet (100), the contour of the metal product is often patterned so that the longitudinally extending portion (108a) of the metal product (108) extends in a direction parallel to the first direction or the second direction. For example, when the longitudinally extending portion (108a) of the metal product (108) extends in a direction parallel to the first direction, the angle A1 should be as small as possible to improve resistance to breakage caused by oil pits, but the angle A1 should be as large as possible to improve durability against bending. Also, when the longitudinally extending portion (108a) of the metal product (108) extends in a direction parallel to the second direction, the angle A2 should be as small as possible to improve resistance to breakage caused by oil pits, but the angle A2 should be as large as possible to improve durability against bending.
[0017] For this reason, in order to manufacture a metal product having an excellent balance between resistance to breakage caused by oil pits and durability against bending, it is preferable that angles A1 and A2 are both in the range of 5 to 85°, more preferably in the range of 10 to 80°, even more preferably in the range of 20 to 70°, even more preferably in the range of 30 to 60°, and most preferably in the range of 40 to 50°. Furthermore, by setting angles A1 and A2 in such ranges, not only is the balance between resistance to breakage caused by oil pits and durability against bending improved for the main portion extending in the longitudinal direction of the metal product, but also, in the case where the metal product has a secondary portion extending in a direction perpendicular to the longitudinal direction, the balance between resistance to breakage caused by oil pits and durability against bending is improved for the secondary portion.
[0018] In this disclosure, the longitudinal direction of a metal product refers to the longitudinal direction (the direction in which the long side extends) of the largest rectangle that can enclose the metal product after it has been cut out.
[0019] The thinner the metal rolled sheet (100), the greater the effect of breakage due to oil pits, and therefore the greater the effect of the present invention. For this reason, the upper limit of the thickness of the metal rolled sheet (100) is preferably 100 μm or less, more preferably 80 μm or less, even more preferably 60 μm or less, and even more preferably 40 μm or less. However, if the thickness of the metal rolled sheet (100) is too thin, the handling properties deteriorate, so the thickness is preferably 5 μm or more, more preferably 10 μm or more, and even more preferably 15 μm or more.
[0020] There is no particular limitation on the material of the metal rolled sheet (100). For example, copper, copper alloy, aluminum, aluminum alloy, iron, iron alloy, stainless steel, nickel, nickel alloy, titanium, titanium alloy, gold, gold alloy, silver, silver alloy, platinum group, platinum group alloy, chromium, chromium alloy, magnesium, magnesium alloy, tungsten, tungsten alloy, molybdenum, molybdenum alloy, lead, lead alloy, tantalum, tantalum alloy, zirconium, zirconium alloy, tin, tin alloy, indium, indium alloy, zinc, zinc alloy, etc., and further, known metal materials can also be used. Metal materials standardized by JIS standard, CDA, etc. can also be used.
[0021] Among metals, when electronic components such as leaf springs, connectors, and terminals are manufactured, copper or a copper alloy is preferred in consideration of the balance between strength and electrical conductivity.
[0022] The copper typically includes copper having a purity of 95% by mass or more, more preferably 99.90% by mass or more, such as phosphorus-deoxidized copper (JIS H3100 alloy number C1201, C1220, C1221), oxygen-free copper (JIS H3100 alloy number C1020), and tough pitch copper (JIS H3100 alloy number C1100) as specified in JIS H0500 and JIS H3100. Copper or a copper alloy containing at least one of Sn, Ag, Au, Co, Cr, Fe, In, Ni, P, Si, Te, Ti, Zn, B, Mn, and Zr in total at 0.001 to 4.0% by mass may also be used.
[0023] Further examples of copper alloys include titanium copper, phosphor bronze, Corson alloy, red brass, brass, nickel silver, and other copper alloys. Copper or copper alloys specified in JIS H 3100 to JIS H 3510, JIS H 5120, JIS H 5121, JIS C 2520 to JIS C 2801, and JIS E 2101 to JIS E 2102 can also be used in the present invention. In this specification, unless otherwise specified, the JIS standards given to indicate metal standards refer to the 2001 edition of the JIS standards.
[0024] Titanium copper typically contains 0.5 to 5.0 mass% Ti, with the remainder being copper and unavoidable impurities. Titanium copper may further contain one or more of Fe, Co, V, Nb, Mo, B, Ni, P, Zr, Mn, Zn, Si, Mg, and Cr in a total amount of 2.0 mass% or less.
[0025] Phosphor bronze typically refers to a copper alloy containing copper as the main component, Sn, and a smaller amount of P. As an example, phosphor bronze has a composition containing 3.5 to 11 mass% Sn, 0.03 to 0.35 mass% P, and the remainder being copper and unavoidable impurities. Phosphor bronze may contain elements such as Ni and Zn in a total amount of 1.0 mass% or less.
[0026] Corson alloy is a copper alloy that typically contains Si and an element that forms a compound with Si (e.g., one or more of Ni, Co, and Cr) and precipitates as second phase particles in the matrix. As an example, the Corson alloy has a composition that contains 1.0 to 5.0 mass% Ni, 0.2 to 1.6 mass% Si, and the balance is copper and unavoidable impurities. As another example, the Corson alloy has a composition that contains 1.0 to 5.0 mass% Ni, 0.2 to 1.6 mass% Si, and 0.03 to 0.5 mass% Cr, and the balance is copper and unavoidable impurities. As yet another example, the Corson alloy has a composition that contains 1.0 to 5.0 mass% Ni, 0.2 to 1.6 mass% Si, and 0.1 to 3.5 mass% Co, and the balance is copper and unavoidable impurities. As yet another example, the Corson alloy has a composition that contains 1.0 to 5.0 mass% Ni, 0.2 to 1.6 mass% Si, 0.1 to 3.5 mass% Co, and 0.03 to 0.5 mass% Cr, with the balance being copper and unavoidable impurities. As yet another example, the Corson alloy has a composition that contains 0.2 to 1.6 mass% Si, 0.1 to 3.5 mass% Co, with the balance being copper and unavoidable impurities. Other elements (e.g., Mg, Sn, B, Ti, Mn, Ag, P, Zn, As, Sb, Be, Zr, Al, and Fe) may be added to the Corson alloy as desired. These other elements are generally added up to a total of about 4.0 mass%. For example, as yet another example, Corson alloy has a composition containing 1.0 to 5.0 mass% Ni, 0.2 to 1.6 mass% Si, 0.01 to 2.0 mass% Sn, 0.01 to 2.0 mass% Zn, with the remainder being copper and unavoidable impurities.
[0027] In the present invention, red brass refers to an alloy of copper and zinc, which contains 1 to 20 mass % of zinc, more preferably 1 to 10 mass % of zinc. Red brass may also contain 0.1 to 1.0 mass % of tin.
[0028] In the present invention, brass refers to an alloy of copper and zinc, particularly a copper alloy containing 20% by mass or more of zinc. The upper limit of the zinc content is not particularly limited, but is 60% by mass or less, preferably 45% by mass or less, or 40% by mass or less.
[0029] In the present invention, nickel silver refers to a copper alloy containing copper as the main component, 60 to 75 mass % of copper, 8.5 to 19.5 mass % of nickel, and 10 to 30 mass % of zinc.
[0030] In the present invention, the other copper alloy refers to a copper alloy containing one or more of Zn, Sn, Ni, Mg, Fe, Si, P, Co, Mn, Zr, Cr and Ti in a total amount of 8.0 mass% or less, optionally containing other elements in an amount of 20 mass% or less, or optionally containing other elements in an amount of 10 mass% or less, with the balance being unavoidable impurities and copper. The other elements are not particularly limited.
[0031] The aluminum and aluminum alloys usable herein may include those containing, for example, 40% by mass or more of Al, 80% by mass or more, or 99% by mass or more of Al. For example, aluminum and aluminum alloys specified in JIS H 4000 to JIS H 4180, JIS H 5202, JIS H 5303, or JIS Z 3232 to JIS Z 3263 may be used. For example, aluminum or its alloys containing 99.00% by mass or more of Al, such as aluminum alloy numbers 1085, 1080, 1070, 1050, 1100, 1200, 1N00, and 1N30 specified in JIS H 4000, may be used.
[0032] As nickel and nickel alloys, those containing, for example, 40 mass% or more of Ni, 80 mass% or more, or 99.0 mass% or more of Ni can be used. For example, nickel or nickel alloys specified in JIS H 4541 to JIS H 4554, JIS H 5701, JIS G 7604 to JIS G 7605, and JIS C 2531 can be used. In addition, nickel or its alloys containing 99.0 mass% or more of Ni, such as alloy numbers NW2200 and NW2201 specified in JIS H4551, can be used.
[0033] As the iron and iron alloy, for example, stainless steel, mild steel, carbon steel, iron-nickel alloy, steel, etc. can be used. For example, iron or iron alloys described in JIS G 3101 to JIS G 7603, JIS C 2502 to JIS C 8380, JIS A 5504 to JIS A 6514, or JIS E 1101 to JIS E 5402-1 can be used. As the stainless steel, SUS 301, SUS 304, SUS 310, SUS 316, SUS 430, SUS 631 (all JIS standards) can be used. As the mild steel, mild steel with carbon of 0.15 mass% or less can be used, and mild steel described in JIS G3141 can be used. As the iron-nickel alloy, Ni is contained in 35 to 85 mass%, with the balance being Fe and unavoidable impurities, and specifically, an iron-nickel alloy described in JIS C2531 can be used.
[0034] As zinc and zinc alloys, for example, those containing 40 mass% or more of Zn, 80 mass% or more, or 99.0 mass% or more of Zn can be used. For example, zinc or zinc alloys described in JIS H 2107 to JIS H 5301 can be used.
[0035] The lead and lead alloys that can be used include those that contain, for example, 40% by mass or more of Pb, 80% by mass or more, or 99.0% by mass or more of Pb. For example, lead or lead alloys that are standardized in JIS H 4301 to JIS H 4312 or JIS H 5601 can be used.
[0036] The magnesium and magnesium alloys that can be used include those containing, for example, 40% or more by mass of Mg, 80% or more by mass, or 99.0% or more by mass of Mg. For example, magnesium and magnesium alloys that are standardized in JIS H 4201 to JIS H 4204, JIS H 5203 to JIS H 5303, and JIS H 6125 can be used.
[0037] As the tungsten and tungsten alloy, for example, those containing 40 mass% or more, 80 mass% or more, or 99.0 mass% or more of W can be used. For example, tungsten and tungsten alloys standardized in JIS H 4463 can be used.
[0038] As the molybdenum and molybdenum alloy, for example, those containing 40 mass % or more of Mo, 80 mass % or more, or 99.0 mass % or more of Mo can be used.
[0039] As titanium and titanium alloys, those containing, for example, 40 mass% or more of Ti, 80 mass% or more, or 99.0 mass% or more of Ti can be used. For example, titanium and titanium alloys standardized in JIS H 4600 to JIS H 4675 and JIS H 5801 can be used.
[0040] The tantalum and tantalum alloys that can be used include those containing, for example, 40 mass % or more of Ta, 80 mass % or more of Ta, or 99.0 mass % or more of Ta. For example, tantalum and tantalum alloys that are specified in JIS H 4701 can be used.
[0041] As the zirconium and zirconium alloy, for example, those containing 40 mass% or more of Zr, 80 mass% or more of Zr, or 99.0 mass% or more of Zr can be used. For example, zirconium and zirconium alloys standardized in JIS H 4751 can be used.
[0042] As the tin and tin alloy, for example, those containing 40 mass% or more of Sn, 80 mass% or more, or 99.0 mass% or more of Sn can be used. For example, tin and tin alloys standardized in JIS H 5401 can be used.
[0043] As the indium and indium alloy, for example, those containing 40 mass % or more of In, 80 mass % or more, or 99.0 mass % or more of In can be used.
[0044] As the chromium and chromium alloy, for example, those containing 40 mass % or more of Cr, 80 mass % or more, or 99.0 mass % or more of Cr can be used.
[0045] As the silver and silver alloy, for example, those containing 40 mass % or more of Ag, 80 mass % or more of Ag, or 99.0 mass % or more of Ag can be used.
[0046] The gold and gold alloys that can be used include those containing, for example, 40 mass % or more of Au, 80 mass % or more of Au, or 99.0 mass % or more of Au.
[0047] The platinum group metals are a general term for ruthenium, rhodium, palladium, osmium, iridium, and platinum. As the platinum group metals and platinum group alloys, those containing at least one element selected from the group consisting of Pt, Os, Ru, Pd, Ir, and Rh in an amount of 40% by mass or more, 80% by mass or more, or 99.0% by mass or more can be used.
[0048] In one embodiment, the metal rolled sheet (100) has a tensile strength in the rolling direction of 500 MPa or more, preferably 800 MPa or more, and more preferably 1100 MPa or more. A tensile strength in the rolling direction of 500 MPa or more has the advantage that a leaf spring having a high contact pressure can be designed. There is no particular upper limit set for the tensile strength of the metal rolled sheet (100), but in consideration of manufacturing costs, it is preferably 2000 MPa or less, and more preferably 1500 MPa or less. In the present disclosure, the tensile strength is measured in accordance with the metallic material tensile test specified in JIS Z2241:2011.
[0049] Various metal products can be manufactured by cutting out from the metal rolled sheet (100). There are no particular limitations on the cutting method, but examples include press punching, etching, laser processing, and wire electric discharge processing (also commonly known as "wire cutting"). Among these, press punching is preferred due to its low cost and high productivity. According to one embodiment of the present invention, there is provided a method for manufacturing a metal product having a longitudinal direction, which includes cutting out a metal product from the metal rolled sheet (100) with the longitudinal direction parallel to a first direction or a second direction.
[0050] Examples of metal products include leaf springs, connectors (FPC connectors, server connectors, etc.), terminals, switches, sockets, jacks, and relays.
[0051] If necessary, the metal product may be subjected to various surface treatments such as plating, chemical polishing, anodizing, chemical conversion coating, etc. The surface treatment may be performed before or after the metal product shape is cut out from the metal rolled sheet. [Explanation of symbols]
[0052] 100 Metal rolled sheet 102 Edge extending in the first direction 104 Edge extending in the second direction 106 Oil Pit 108 Metal products 108a The longitudinally extending portion of the metal product 110 Rolled metal plate 112 Long side 114 Short side 300 sheets 301 Metal products 306 Oil Pit
Claims
【Request 1】 A rectangular metal rolled sheet having a side extending in a first direction and a side extending in a second direction perpendicular to the first direction, wherein the angle A between the longitudinal direction of the oil pit and the first direction is 1 and the angle A between the longitudinal direction of the oil pit and the second direction 2 A rolled metal sheet in which all of the surfaces are non-right-angled.
Citation Information
Patent Citations
PRESS-BLANKING MATERIAL, AND Sn PLATING TREATMENT METHOD
JP2005206942A
Connector terminal fitting and manufacturing method therefor
JP2015060770A