Non-viscous metal vessel and non-stick pan
The PVD multi-metallic film with a micron-order roughened surface and micro-nanometer-order pores addresses the issues of coating degradation and short lifespan in non-stick pots, providing long-lasting non-stick performance and safety.
Patent Information
- Application Number
- JP2023136920
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-07-13
- Filing Date
- 2023-08-25
- Publication Date
- 2024-11-21
- Estimated Expiration
- 2043-08-25
AI Technical Summary
Conventional non-stick pots with anti-stick coatings face issues such as coating degradation at high temperatures, release of toxic substances, and short non-stick lifespan due to wear from frequent use.
A PVD multi-metallic film with a micron-order roughened surface and micro-nanometer-order porous structure is applied, comprising layers of metals like titanium, chromium, and aluminum, forming an oil lock mechanism to enhance non-stick performance and durability.
The film achieves long-lasting non-stick performance, reduces surface energy, and prevents toxic substance release, with excellent wear resistance and antibacterial properties, maintaining non-stick performance even after 5000 abrasion tests.
Smart Images

Figure 2024162953000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to the field of cookware technology, in particular to non-stick metalware and non-stick pans. , which significantly improves the non-stick effect of metal utensils. [Background technology]
[0002] Conventional non-stick pans generally have a layer of anti-stick coating on the inner wall of the pan. The most commonly used coating material is Teflon, whose scientific name is , polytetrafluoroethylene, which solves the problem of sticking to the pan well, It brings convenience to people's lives. However, the anti-stick coating on the inner wall of the pot is During use, especially when roasted at high temperatures, the anti-stick coating is easy to fall off and If the non-stick pan is heated empty, it will be more likely to cause the anti-stick coating to fall off. Polytetrafluoroethylene itself is non-toxic, but if the pan is heated at high temperatures or left unheated, When placed in a location where it is difficult to handle, polytetrafluoroethylene can carbonize, split, and release minute amounts of toxic substances. It releases gases and substances that contaminate the food being cooked and cause the food being fried to burn in the pan. This can cause problems such as nicking and ingesting the chemical coating.
[0003] On this basis, non-stick pans have appeared in the prior art, which utilize the lotus effect. The anti-sticking structure is made on the inner wall of the pot by using a sintering agent. The anti-sticking structure is made of protrusions periodically distributed on the inner wall. The size of the protrusions and depressions is from several microns to several tens of microns. The inner wall surface of a non-stick pan changes to a rough surface with micron-order roughness. This changes the contact surface between the food being cooked and the inner wall of the non-stick pan into a composite contact surface. The gas is absorbed in the recessed areas between the protrusions of the adhesion prevention structure and in the recessed areas of the depressions. This creates an air bed layer that prevents the food from coming into contact with the inner wall of the nonstick pan. Effectively reduce the contact area, prevent food from burning, prevent physical adhesion, zero coating Zero coating non-stick even when frying at high temperatures or when the pan is empty The pan does not release any toxic substances and gases, contaminating the food being cooked and the kitchen environment. This allows for safer cooking.
[0004] However, this structure is applied to the surface of a non-stick pan, creating a physical non-stick layer. Forming is still not enough. When using a non-stick pan, it needs to be heated. Therefore, the air bed layer formed in the recessed area described in the above solution is not broken down in a heated environment. It will be destroyed, thereby defeating the purpose of the physical non-stick.
[0005] However, simply applying the physical non-stick coating to the surface of the pan will not provide long-lasting heat. Not enough to achieve perfect non-stick, the pot and shovel are Since it needs to be rubbed against the surface of the pot repeatedly, prolonged friction can cause physical damage to the nonstick surface. This problem will wear down the non-stick layer and prevent the long-term non-stick effect from being achieved. The issue is also waiting for a prompt resolution. Summary of the Invention [Problem to be solved by the invention]
[0006] The technical problem that the present invention aims to solve is to provide a highly durable Non-stick metal utensils and non-stick materials that have wear resistance and can achieve sustained non-stick properties The PVD multi-metal film is a low surface area coating made of multi-metals. Energy micro-nano structure with micron-order roughened surface for outstanding non-stick effect Improve. [Means for solving the problem]
[0007] In order to achieve the above object, the present invention provides a non-viscous metal article, The present invention relates to a method for manufacturing a semiconductor device, comprising: a main body, an inner surface of which is roughened to a micron order; A PVD multi-element metal film is attached onto the micron-order roughened surface, and the PVD multi-element metal film is A micron-order roughened surface is coated with a low surface energy micron-order porous layer. The micron-order roughened surface is configured to form an illlock structure. is formed by sandblasting, preferably by adopting multi-stage sandblasting. It can also be manufactured into a micron-order rough surface by adopting other methods. The roughness of the micron-order roughened surface formed by the blasting process is generally Rz2 It can reach 5~100μm, and the roughness Rz refers to the height of ten microscopic irregularities. Then, the average of the five largest profile peak heights and the five largest loop heights in the sampling length L are calculated. It refers to the sum of the average value of the valley depth.
[0008] The above technical solution can be further improved by the following measures:
[0009] In one embodiment, the thickness h value of the PVD multi-metal film is The thickness range of the PVD multi-element metal film is 0.7 to 4.0 μm. The body includes a first metal layer, a heat isolating layer, and a second metal layer in this order from the inside to the outside. The first metal layer and the second metal layer are integrated together via a heat spreader layer, The first metal layer is a stainless steel layer, and the uniform heating is performed. The layer is an aluminum layer and the second metal layer is a stainless steel layer.
[0010] In one embodiment, the PVD multi-metal film comprises a bottom layer and an intermediate layer, deposited in bottom-to-top order. and a surface layer. The bottom layer includes metallic titanium and / or metallic chromium. The intermediate layer includes , chromium nitride and aluminum nitride, wherein the content of chromium nitride is 60 to 80 % by weight, where the aluminum nitride content is 20-40 wt. %, or The intermediate layer includes chromium carbide, and the chromium carbide content is 85 to 95 wt %. The surface layer contains metallic copper and aluminum oxide, and the content of the metallic copper is The surface layer further contains iron oxide, and the iron oxide is 3 to 1.0 wt %. 5 wt%. The thickness of the bottom layer is 0.1 to 1.0 μm, and the thickness of the intermediate layer is The thickness of the surface layer is 0.1 to 1.0 μm. The hardness range of the metal film is HV1100 to 3500. The thickness range of the PVD multi-metal film is The surface energy of the PVD multi-metal film is 0.7 to 4.0 μm. The water droplet angle is also smaller than 95°.
[0011] Specifically, the PVD multi-metal film is in accordance with the Chinese national standard GB / T32095.2-201 After conducting a flat surface abrasion resistance test 5,000 times in accordance with JIS Z 2010-1505, the results of the egg roll non-stickiness test were The evaluation level of the results is Grade I.
[0012] The present invention further provides a non-stick pan, which is configured as the above-mentioned non-stick metalware. It is done. Effect of the Invention
[0013] By adopting the above technical solutions, the present invention has the following beneficial effects:
[0014] The non-stick metal utensils and non-stick pans of the present invention have a low surface energy layer on the roughened surface of the inner metal layer. In order to further deposit a PVD multi-metal film of the energy, and to control the thickness of the PVD multi-metal film, A low surface energy porous layer on a micron-order roughened surface. It can form an oil lock structure, which has excellent non-stick effect. In addition, it can significantly improve the adhesion of the PVD multi-metal film to the bottom layer, and improve the non-stickiness. It also extends the service life of metal utensils. It also reduces the amount of heat generated in metal utensils during cooking. In order to solve the technical problem of the metal film being destroyed by heat, the pot of the present invention further has two layers of gold. An aluminum heat-uniform layer is installed between the metals, and the aluminum heat-uniform layer allows the bottom of the pot to distribute heat more evenly. This will help to extend the non-stick life of your non-stick pans. Lengthen.
[0015] The PVD multi-metal film in the present invention is a multi-metal film (chromium and aluminum, titanium The low surface layer is composed of nitrides, carbides and oxides of the elements such as tantalum, copper, iron, etc. It has an energy micro-nano porous oil lock structure, and its bottom layer is mainly made of metal titanium and and / or metallic chromium, which can improve the adhesion of the PVD multi-metallic film on the body. This further extends the service life of the metal film. The surface layer is made of metallic copper and aluminum oxide. Thus, a single oxide film is formed on the surface of the PVD multi-metal film, and the PVD multi-metal film is Prevents the original metal film from oxidizing and discoloring during the process In addition, metallic copper can play an effective antibacterial role, especially against Escherichia coli and Staphylococcus aureus. It has an antibacterial effect of over 99.99% against bacteria and contains less than 10wt% copper. The PVD multi-metal film of the present invention has a better non-stick effect when the coating is applied to a surface of the substrate. The surface energy of the water droplet can reach below 40 dynes and the water droplet angle can reach above 95 degrees. It has a porous oil lock structure on the order of micro-nanometers, It has excellent wear resistance and non-stick properties, and meets the Chinese national standard GB / T32095. 2~2015, after 5000 times of flat surface wear resistance test, non-stick level can still achieve Class I non-stick. [Brief description of the drawings]
[0016] In order to more clearly describe the technical solutions of the embodiments of the present invention, the following briefly describes the drawings of the embodiments. It will be appreciated that the drawings in the following description are merely illustrative of some embodiments of the present invention. However, it is not a limitation on the present invention. [Figure 1] FIG. 2 is a cross-sectional view of the non-viscous metal article in Example 1. [Diagram 2] FIG. 2 is an enlarged view of A in FIG. [Diagram 3] 1 is a schematic diagram of the non-stick structure of the non-viscous metal utensil in Example 1. FIG. [Figure 4] 1 is a surface morphology diagram (magnification: 500x) of the non-viscous metal article in Example 1. [Diagram 5]1 is a surface morphology diagram (1000x) of the non-viscous metal article in Example 1. [Figure 6] 1 is a surface morphology diagram (magnification: 5000) of the non-viscous metal article in Example 1. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0017] In order to make the objectives, technical solutions and advantages of the embodiments of the present invention clearer, the following is combined with the drawings. The invention will now be described in more detail with reference to the drawings, which are generally indicated and illustrated in the drawings. Assemblies of embodiments of the present invention can be arranged and designed in a variety of different configurations. Based on the embodiments in the present disclosure, all other inventions obtained by a person skilled in the art without any creative effort are All of the above embodiments are within the scope of protection of the present invention.
[0018] Please note that like reference numbers and letters refer to like parts in the following drawings. In order to represent items that are defined in one drawing, an item must be defined in the following drawings. There is no need to further define or interpret it.
[0019] Unless otherwise noted, technical or scientific terms used in this patent document are intended to be understood as meaning those to which the invention pertains. The term "common name" should have a common meaning as would be understood by a person of ordinary skill in the relevant field. The terms "first," "second," and similar terms used in the present patent specification and claims are intended to be used interchangeably. The words used do not denote any order, quantity or importance, but are intended to distinguish between different components. Similarly, words such as "one", "one" or "the" and similar words do not limit the quantity. It does not indicate the presence of one or more, but indicates the presence of at least one. The word "include" or "includes" means that the element or component appearing before "includes" or "includes" is included after "includes" or "includes". The term "component" refers to the inclusion of the elements or components listed in the preceding paragraph and equivalents thereof, and does not exclude other elements or components. "Center", "Top", "Bottom", "Left", "Right", "Vertical", "Horizontal", "Inside", "Outside" "Far" and "near" are merely used to express relative positions, and do not represent the absolute position of the object being described. After the position is changed, this relative position may change accordingly, which is The above-mentioned devices are merely intended to facilitate the description and simplify the description of the invention. or indicating that the element has a particular orientation and must be configured and operated in a particular orientation. No limitation to the present invention is intended or should be implied and should not be understood as a limitation to the present invention.
[0020] In the description of the present invention, unless otherwise clearly defined or limited, Therefore, the terms "attach," "connect," and "connect" should be understood broadly. For example, it may be a fixed connection, a separate connection, or an integral connection. The connection may be a mechanical connection, an electrical connection, or a direct connection. Alternatively, the connection may be indirect through an intermediate medium, or the connection may be internal communication between the two elements. Those skilled in the art will be able to determine the specific meaning of the above terms in the present invention depending on the specific circumstances. can be understood.
[0021] Several embodiments of the present invention will be described in detail below in conjunction with the drawings. Unless conflicting, the features in the following embodiments can be combined with each other.
[0022] Example 1: The non-viscous metal article 100 shown in FIGS. 1 to 6 includes a first metal layer 101 and a second metal layer 102. The first metal layer 101 is configured as an inner layer, and the inner surface of the first metal layer 101 is The surface is roughened to the micron order having chromium-order holes. The polished surface is formed by sandblasting, preferably by multi-stage sandblasting. In another embodiment, a knurling process may be used. A PVD multi-element metal film 104 is plated on the micron-order roughened surface, and the PVD multi-element metal film 1 04 Micro-nanometer order pores are distributed on the surface, forming a porous oil lock structure. The first metal layer 101 and the second metal layer 102 are integrally formed through a heat-uniform layer 103. The heat spreader layer 103 has a higher thermal conductivity than the first metal layer 101, and the heat spreader layer 103 is This prevents localized areas of 101 from becoming too hot and damaging the PVD multi-metal film 104 .
[0023] Physical Vapor Deposition (PVD) Technology is a method of converting the surface of a material source (solid or liquid) into gas-state atoms or molecules by using physical methods under vacuum conditions. or partially ionized into ions and then decomposed by a low-pressure gas (or plasma) process. Physical vapor deposition refers to the technology of depositing a film with special functions on the surface of a body. It is one of the main surface treatment technologies. PVD (Physical Vapor Deposition) film plating technology is, Mainly vacuum evaporation film plating, vacuum sputtering film plating and vacuum ion film plating The main methods of physical vapor deposition are vacuum deposition, sputtering, and plating. Film plating, arc plasma film plating, ion film plating and molecular beam epitaxy The applicable vacuum film plating equipment is vacuum evaporation film plating machine and , including vacuum sputtering film plating machine and vacuum ion film plating machine. Due to the difference in the thickness, PVD (physical vapor deposition) film plating technology is further developed into tool plating and equipment plating. In order to ensure the thickness of the PVD multi-metal film, the process By using the plating method, the PVD multi-metal film can reach 0.7~4.0 microns. Preferably, the thickness of the PVD multi-metal film is 1.0 to 2.5 microns. Specifically, the thickness of the PVD multi-metal film is 2.0 microns. In another embodiment, In some embodiments, the thickness may be 3 or 4 microns. The thickness of the metal film should be compatible with the micron-order roughened surface, and the thickness of the PVD metal film should be micron-order roughened surface. The Rz value of the PVD metal film must be smaller than that of the chronologically roughened surface. The oil-lock structure is formed on the roughened surface of the micron-order. It can be formed without covering the micron-order roughened surface, and in this application, it is called micro-nano The meter-order porous oil-lock structure is formed on the basis of the micron-order roughened surface. can be.
[0024] Furthermore, the micro-nanometer order porous oil-lock structure The alloy is a multi-metal alloy (containing at least chromium and aluminum, and also titanium, copper, and iron). The nitrides, carbides and oxides of the carbide and oxides are micro-plated by PVD film plating technology. The nanoparticles are deposited on the roughened surface, forming micro- and nanometer-order holes. The hole diameter of the nanopores is in the range of 0.1 to 3.0 microns, and in this embodiment, it is 0.1 to 1.0 microns. The specific size of the micron-order holes was measured using a Zeiss microscope. It can be measured by Axioplan 2imaging (model no.) and is in the nanometer order. The pore sizes were all measured using a scanning electron microscope (FEI) Nova 400. This can be measured using a NanoSEM (model no.).
[0025] In one preferred embodiment, the useful life of the PVD plating layer 104 is further extended. To this end, the non-adhesive metal article adopts a steel-aluminum-steel composite structure, in which the first metal layer 101 is a stainless steel layer, the heat-uniform layer 103 is an aluminum layer, and the second metal layer 102 is a stainless steel layer, for example SUS430. The stainless steel to be selected is Most preferably, the first metal layer 101 is food grade, for example, SUS304. The second metal layer 102 mainly serves a protective function and may be made of other metals than stainless steel, e.g. For example, titanium alloy may be selected. To this end, a plurality of etching grooves are first etched in an array on the inner surface, and then the sample is The grooves may be formed by chemical etching or laser etching techniques. It may be manufactured by using a technique such as knurling or embossing. The grooves are then etched to form a micron-order roughened surface. , a lotus structure can be formed inside the inviscid metal object 100, thereby forming a nonce Improve tick effect.
[0026] In this embodiment, the micro-nanopores contract and expand as the temperature changes when exposed to heat. When using animal fats or vegetable oils to heat and maintain the pan, The nanopores expand as the temperature of the pan body increases and contract as the temperature of the pan body decreases. He further explained that when the user heats the pot body, the micro-nano pores expand and allow oil and fat to enter and exit. When the heating of the pan body is stopped, the pan body temperature gradually cools down, The chromium nanopores shrink, and when the oil enters the holes, it is locked in them, providing an oil lock function. This further achieves the non-stick performance of the pan surface. The micro-nano pores, with a width of 0.1 to 1 μm, provide excellent oil storage and oil locking function. This improves the non-stick effect of the pan surface. The specific drawing is shown in FIG. 3. The micro-nano porous structure of the PVD multi-metal film of the present invention After storing oil, the hydrophobic contact angle can reach 95 or more, so This invention has excellent non-stick properties.
[0027] In this embodiment, the PVD multi-metal film contains primarily titanium, chromium, and aluminum. Here, the chromium content is 20 to 50 at %, and the aluminum content is 50 The titanium content is 1 to 10 at%. When the content is between 1 and 10 at%, the surface energy can be effectively reduced, The titanium element content is preferably 3 to 6 at%. Specifically, the titanium element content may be 3 at %. The aluminum element contained in the film can reduce its surface energy, The anti-adhesion effect is improved by adding aluminum, and the aluminum content is preferably about 30 at %. The chromium element contained in the coating can not only reduce the surface energy, but also In addition, it is possible to improve the corrosion resistance and prevent the deposition of heavy metals. The chromium content is preferably The PVD multi-metal film is made up of a bottom layer and an intermediate layer, which are deposited in order from bottom to top. and a surface layer. The bottom layer includes metallic titanium and / or metallic chromium, Titanium and chromium are both present in metallic form, which is why PVD multi-metal films and roughened surfaces are It is used to improve the adhesion of the first metal layer and also to remove heavy metal substances from the first metal layer. It is also important to explain that it is possible to prevent the deposition of toxic substances and their effects on the body's health. In the bottom layer, titanium and chromium may be present alone or simultaneously; Both can achieve the purpose of preventing adhesion and heavy metal deposition, but titanium and chromium At the same time the performance is better.
[0028] In the intermediate layer, the nitrides and / or carbides containing chromium aluminum are Specifically, titanium nitride (TiN), chromium nitride (CrN), and / or carbides may be included. Aluminum (CrN), Aluminum Nitride (AlN), Titanium Carbide (TiC), Chromium Carbide (Cr C), aluminum carbide (AlC), aluminum titanium nitride (AlTiN) and aluminum nitride Aluminum Chromium Nitride (AlCrN), Aluminum Titanium Nitride (AlTiN), Aluminum Nitride Aluminum chromium nitride (AlCrN) and aluminum chromium carbide (Cr2AlC). The specific content of the multi-element metal can be adjusted by those skilled in the art within the above range. It should be noted that chromium aluminum nitrides and carbides may exist independently. In particular, chromium carbide contributes to the hardness and wear resistance of PVD multi-metallic films, as well as to the It can significantly improve the corrosion resistance and corrosion resistance of PVD multi-metal films. In another embodiment, chromium carbide can be added to the surface layer. The hydrophobicity of the PVD multi-metal film can be further improved. Aluminum nitride has good thermal stability and good thermal shock resistance, while aluminum nitride has a ceramic-like It has excellent thermal conductivity and prevents the PVD film from being destroyed by excessive heat in certain areas. Chromium nitride has good corrosion resistance and can reduce the friction coefficient of the PVD film. This reduces the wear and tear and gives the titanium chrome alloy excellent wear resistance. The combination of aluminum nitride and carbide has higher hardness and wear resistance. In addition, the intermediate layer further provides the PVD film of the present invention with good mechanical and thermal shock resistance. In addition, it can be used when cooking with tools such as metal shovels. In the case of a localized heat, the PVD film is not easily destroyed. Metal films have low surface energy and extremely high hardness and non-stick properties. Specifically, its hardness can reach HV1000 to 5000, and its surface energy The flow rate can reach up to 40 dynes and the drop angle is more than 95 degrees.
[0029] Specifically, in this embodiment, the interlayer contains chromium nitride and aluminum nitride, Here, the content of chromium nitride is 60 to 80 wt%, specifically 75 wt%. Here, the content of aluminum nitride is 20 to 40 wt%, specifically 25 wt In another embodiment, the intermediate layer comprises chromium carbide, where the content of chromium carbide is is 85-95wt%, and the other components are one of aluminum nitride and titanium nitride. or a combination of the two, which may further include components such as aluminum carbide. The surface layer contains metallic copper and aluminum oxide, and the content of the metallic copper is 1.0 to 10 wt%, specifically 5 wt%. The surface layer further contains iron oxide, The iron oxide is 3 to 15 wt%, specifically 10 wt%, and further 5 wt% or 1 The surface layer may be made of metallic copper and aluminum oxide. Except for aluminum and iron oxide, the content of other elements and impurities is less than 5wt%.
[0030] In this embodiment, the PVD film is a non-viscous metal film whose main elements are chromium and aluminum. The aluminum element contained in the PVD multi-metal film lowers its surface energy. The chromium content can be reduced, thereby improving the anti-adhesion effect. Not only can the surface energy be reduced, but also the corrosion resistance can be improved. This prevents the deposition of heavy metals. The components are titanium, aluminum, chromium, iron and copper, and the non-metallic components are mainly oxygen and carbon. It contains nitrogen and silicon.
[0031] The surface layer may further include oxides of titanium and chromium, specifically titanium and chromium oxides. One of the oxides, for example titanium oxide, or a combination of titanium oxide and chromium oxide The combination of metallic copper and aluminum oxide (metallic copper and aluminum oxide) may include at least The combination of aluminum iron oxide gives the surface good non-stick properties. The surface layer can form a layer of oxide on the surface of the PVD film, which can prevent subsequent use. This prevents the color change problem from occurring during the process. At the same time, aluminum oxide is also compatible with metallic copper. This can prevent the formation of toxic copper oxide due to oxidation of copper.
[0032] By increasing the amount of metallic copper in the PVD multi-metal film, the PVD multi-metal film has antibacterial properties. In the case where the copper content is 10 wt% or less, the PVD multi-metal film is also used. The anti-adhesive effect can be improved.
[0033] In this embodiment, the bottom layer is attached onto the micron-order roughened surface, and the top layer is attached onto the surface of the intermediate layer. The thickness of the surface layer and the bottom layer are relatively small, specifically, both are 0.1 In this embodiment, the thickness is 0.3 μm or less, and in other embodiments, the thickness is 0.5 μm or less. The thickness of the intermediate layer is 5 to 6.8 μm, specifically. is 6.4 μm.
[0034] The inner surface of the PVD multi-metal film 104 is a polished surface, for example, by using high pressure water to polish or The thickness of the PVD multi-metal film 104 is in the range of 0.7 to 6.0 μm. Preferably, the thickness of the PVD multi-metal film 104 is in the range of 2 to 5 μm. The thickness range of the D multi-metal film 104 is 2 μm.
[0035] Based on the above technical content, the purpose is to construct a porous oil lock structure with low surface energy. Those skilled in the art can adjust the proportions of various components according to actual needs. On the basis of the metal, other metal or nonmetallic components can be added, for example silicon element. By adding, iron silicide with high melting point is formed. Through the detection, the hardness range of the PVD multi-metal film 104 is as follows: The hardness range of the PVD multi-element metal film 104 is HV 1000 to 5000. The hardness is preferably HV1100 to 3500, and more preferably HV2000 to 3500. VD multi-metal films have a relatively low surface energy, but their hardness and wear resistance are extremely low. Therefore, the present invention has good anti-adhesive effect, high hardness and abrasion resistance. This has the beneficial effects of providing good durability and a long service life.
[0036] In this embodiment, the wear resistance of the PVD multi-metal film 104 is in accordance with the Chinese national standard GB / T32 095.2~2015 Non-stick surface performance and test standard for household food metal cookware No. Part 2: After 5,000 wear resistance tests in accordance with the "Non-sticky and Wear Resistance Test Standards" In addition, the egg frying test can be carried out without oil to achieve Class I non-stick. refers to using a plastic shovel to remove the eggs without damaging them and leaving no debris behind. Class II eggs cannot be removed without damaging them using a plastic shovel, This means that the residue can be removed by wiping lightly with a wet sponge or cloth. The non-stick performance of the non-stick metal utensil 100 of the present invention is Class I. After several tests, the results showed that the first-class eggs could reach 7-9, with the highest record being 20. It reaches the first-class eggs and far exceeds the requirements of the Chinese standard for three eggs.
[0037] The present invention further provides a non-stick pan 100 with a PVD multi-metallic coating 104, The non-viscous metal utensil 100 is a non-viscous pot that can be used as a frying pan. Those with a chromium carbide surface layer are used as the inner pots of electric rice cookers, electric pressure cookers, etc. It is possible.
[0038] As can be seen from the above description, the present invention has the following beneficial effects.
[0039] The inviscid metal article 100 and the PVD multi-component metal film 104 of the present invention The non-stick pan 100 further includes a PVD multi-metal film 104 on the roughened surface of the inner metal layer. In order to control the thickness of the PVD multi-component metal film 104, the multi-component metal film 104 is deposited on a micron-order roughened surface. The micron-order pores can be made to be micro-nanometer-order pores. This allows the inner metal surface to have a good non-stick effect. During the process, the bottom of the pot is easily overheated, causing the PVD multi-metal film 4, causing the pan to lose its non-stick performance. In order to solve this technical problem, the present invention The pot adopts an aluminum heat-equalizing layer 103 between the two layers of metal, and the aluminum The aluminum heat equalizing layer 103 allows the bottom of the pot to receive heat more uniformly, thereby This will extend the non-stick life of your pan.
[0040] In summary, the non-stick metal utensil (non-stick pan) 100 of the present invention has excellent properties. It has non-stick properties and its non-stick level has been improved after 5000 abrasion resistance tests. The pot bottom can still reach Class I non-stick. This ensures that the pan receives heat evenly, thereby further extending the life of the non-stick properties. In addition, the materials used in the present invention meet the food hygiene index requirements and are free of heavy metal elements that are harmful to the human body. It is free of harmful substances and is safe and healthy.
[0041] The above is only a specific embodiment of the present invention, but the scope of protection of the present invention is not limited thereto. The present invention is not limited to the above-mentioned modifications or variations that are easily conceivable to those skilled in the art within the scope of the present invention. Any replacement should be included within the scope of the present invention. The scope of protection should conform to that of the claims. [Explanation of symbols]
[0042] 100. Non-stick pan (non-stick metal utensil), 101. First metal layer, 102. Second Metal layer, 103. Thermal uniformity layer, 104. PVD multi-metal film.
Claims
1. A non-viscous metal object including a body, The inner surface of the body is roughened to a micron order, Here, a PVD multi-element metal film is attached onto the micron-order roughened surface, and the PVD multi-element metal film is The metal film is formed on this micron-order roughened surface with low surface energy of micron-order nanometers. The present invention is characterized in that the porous oil lock structure can be formed. A non-viscous metal object.
2. The PVD multi-metal film includes a bottom layer, a middle layer, and a surface layer, which are deposited in this order from bottom to top.
2. The non-viscous metal article according to claim 1.
3. 3. The method according to claim 2, wherein the bottom layer comprises metallic titanium and / or metallic chromium. A non-viscous metal object.
4. The intermediate layer comprises chromium nitride and aluminum nitride, wherein the content of chromium nitride is is 60-80 wt%, where the aluminum nitride content is 20-40 wt% or The intermediate layer comprises chromium carbide, wherein the chromium carbide content is 85 to 95 wt% 4. The non-viscous metal article according to claim 3, wherein
5. The surface layer contains metallic copper and aluminum oxide, and the content of the metallic copper is 1 5. The non-viscous metal article according to claim 4, characterized in that the content of the non-viscous metal is 0 to 10 wt %.
6. The thickness range of the PVD multi-metal film is 0.7 to 4.0 μm. The non-viscous metal article according to any one of claims 2 to 5.
7. 6. The method according to claim 2, wherein the thickness of the surface layer is 0.1 to 1.0 μm.
1. A non-viscous metal article according to any one of claims 1 to 9.
8. The hardness range of the PVD multi-metal film is HV1100 to HV3500. The non-viscous metal article according to any one of claims 2 to 5.
9. The surface energy of the PVD multi-metal film is less than 40 dynes and after storage in oil The method according to any one of claims 2 to 5, characterized in that the hydrophobic angle of Inviscid metal objects.
10. The PVD multi-metal film is in accordance with the Chinese national standard GB / T32095.2-2015. After performing the flat surface abrasion resistance test 5,000 times, the evaluation level of the results of the egg roll non-stickiness test was The non-viscous metal article according to any one of claims 2 to 5, characterized in that the non-viscous metal article is of class I. 。
11. The main body has an inner surface including grooves, and the roughened surface is formed on the grooves.
2. The non-viscous metal article according to claim 1 .
12. The body includes, from inside to outside, a first metal layer, a heat spreader layer, and a second metal layer, in that order; The first metal layer and the second metal layer are integrated together via a heat spreader layer.
2. The non-viscous metal article according to claim 1, wherein the metal layer is uniformly heated.
13. The first metal layer is a stainless steel layer, the heat isotropic layer is an aluminum layer, and The non-viscous metal layer according to claim 12, wherein the second metal layer is a stainless steel layer. genus.
14. A PVD multi-metallic film non-stick pan according to any one of claims 1 to 13. A non-stick pan made of a non-viscous metal ware, with a PVD multi-metal film.
Citation Information
Patent Citations
Non-stick pan with anti-stick structure
CN107495826A
Physical non-stick pan with concave-convex structure
CN212546564U
Pot with oil locking function
CN218942932U
Cited By
Cooking utensil
JP2026012019A