Ballpoint pen, and ballpoint pen refill
A retractable ballpoint pen with a polyolefin cylinder coated with a specific gas-impermeable layer addresses air bubble issues, ensuring ink stability and operability while maintaining transparency.
Patent Information
- Application Number
- JP2023079208
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-12
- Publication Date
- 2024-11-22
AI Technical Summary
Ballpoint pens experience air bubble generation in the ink due to air intrusion from gas-permeable materials, which causes smearing and reduces operability, especially in retractable pens like the knock-type, and existing solutions compromise transparency or operability.
A retractable ballpoint pen with a polyolefin ink storage cylinder coated with a thin gas-impermeable layer containing a hydroxy group-containing resin and an inorganic layered compound, maintaining a specific thickness-to-compression load ratio to suppress air bubbles and enhance operability.
The solution effectively prevents air bubble formation, maintains transparency, and ensures easy handling and operability of the refill, even in retractable pens.
Smart Images

Figure 2024163516000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a ballpoint pen and a ballpoint pen refill. [Background technology]
[0002] A retractable ballpoint pen is known in which a refill biased by a compression spring is placed inside the barrel of the ballpoint pen, and the refill is extended or retracted by operating an operating part protruding from the barrel (for example, Patent Documents 1 and 2). Mechanisms for extending and retracting the refill include a knock type in which the refill is extended or retracted by pressing (knocking) an operating member (such as a knock rod) protruding from the barrel, and a slide type in which a member that can slide back and forth is provided on the side of the barrel, and the refill is extended or retracted by sliding the member.
[0003] As a refill (ballpoint pen refill) to be attached to a ballpoint pen, for example, there is known one in which ink is stored inside an ink storage tube made of polyolefin and a tip is attached to the tip. Unlike a metal ink storage tube, a polyolefin ink storage tube has the advantage that the color of the stored ink can be easily identified from the outside.
[0004] In ballpoint pen refills, measures to enhance the gas barrier properties of ink reservoir tubes have been studied for the purpose of preventing the evaporation of the ink solvent contained therein and preventing the deterioration of the ink. Patent Document 3 describes a configuration in which a barrier resin layer made of a resin with low gas permeability is provided on the entire surface of an ink reservoir tube for storing ink (ink) for writing instruments. Patent Document 4 describes a configuration in which a label, seal, or shrink film with gas barrier properties is provided on the surface of a barrel body made of polypropylene in an applicator using the barrel body, and a ballpoint pen is exemplified as the applicator. Patent Document 5 describes a configuration in which a resin layer with low gas permeability is provided on the tip holder part of a ballpoint pen. In all of the measures in Patent Documents 3 to 5, the gas barrier properties of the member in which the ink is stored are enhanced, thereby preventing the evaporation of the ink (solvent) and the deterioration of the ink. An example of a material that provides gas barrier properties is polyvinylidene chloride. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] JP 2016-117274 A [Patent Document 2] JP 2020-104339 A [Patent Document 3] JP 2019-31077 A [Patent Document 4] Japanese Patent Application Publication No. 9-141180 [Patent Document 5] JP 2013-136165 A Summary of the Invention [Problem to be solved by the invention]
[0006] In a ballpoint pen, if air bubbles are generated in the ink in the ballpoint pen refill, this causes smearing during writing. Therefore, measures are required to suppress air bubbles in the ink as much as possible. Here, one of the causes of air bubbles being generated in the ink is thought to be air intrusion from the outside of the refill. For example, when the ink reservoir is made of a gas-permeable material such as polyolefin, air is thought to intrude from the surface of the ink reservoir. In addition, in the case of a retractable ballpoint pen such as a knock type, minute air bubbles are generated in the ink due to the impact during operation (when knocking), and these may grow over time to form air bubbles. In this respect, a ballpoint pen refill attached to a knock type ballpoint pen is under conditions that make it easier for air bubbles to be generated.
[0007] A measure to suppress the intrusion of air from the surface of an ink reservoir made of a gas-permeable material is to increase the thickness of the ink reservoir. However, this measure impairs the transparency of the ink reservoir, and there is a risk that the color of the ink may become difficult to distinguish from the outside. A measure to provide a gas-impermeable layer made of polyvinylidene chloride on the surface of the ink reservoir can suppress the intrusion of air with high efficiency, but the slipperiness of the ink reservoir surface is poor, and the handling of the refill itself may be reduced. In the case of a knock-type ballpoint pen, it is possible to reduce the impact during operation by reducing the compression load of the compression spring that biases the refill, but this measure may result in poor return when knocked, and may impair the operability of the knock-type ballpoint pen.
[0008] SUMMARY OF THE PRESENT EMBODIMENTS The present invention aims to provide a retractable ballpoint pen and ballpoint pen refill that suppresses the generation of air bubbles in the ink and is easy to use. [Means for solving the problem]
[0009] The present inventor has studied ways to provide a gas-impermeable coating layer on the surface of a ballpoint pen refill. As a result, it has been found that the thickness of the coating layer can be made very small by using a coating layer containing a specific component. Furthermore, it has been found that the above problems in retractable ballpoint pens can be solved by setting the thickness of the coating layer to a specific range relative to the compression load of the compression spring that biases the ballpoint pen refill.
[0010] One aspect of the present invention is a ballpoint pen comprising a ballpoint pen refill biased and held by a compression spring, and an operating part for moving the ballpoint pen refill in the axial direction, and the ballpoint pen refill is extended or retracted by operating the operating part, the ballpoint pen refill comprising a cylindrical ink holding tube, a tip attached to the tip of the ink holding tube, and ink held in the ink holding tube, the ink holding tube being made of polyolefin, the outer peripheral surface of the ink holding tube being provided with a cylindrical coating layer, the coating layer being a gas-impermeable coating film containing a hydroxyl group-containing resin and an inorganic layered compound, the thickness of the coating layer being A micrometers, the compression load of the compression spring when the ballpoint pen refill is protruded being B Newtons, and the value of A / B being 1.0 or greater.
[0011] This embodiment relates to a retractable ballpoint pen that projects and retracts a ballpoint pen refill. In this embodiment, the coating layer provided on the outer peripheral surface of the ink reservoir is made of a gas-impermeable coating film containing a hydroxyl group-containing resin and an inorganic layered compound. Therefore, compared with a coating film made of polyvinylidene chloride, the refill surface has good slipperiness and the coating film thickness can be made very small. In addition, since the coating does not dry quickly when applied, the coating layer can be easily provided. Furthermore, in this embodiment, when the thickness of the coating layer is A micrometers and the compression load of the compression coil spring in the state where the ballpoint pen refill is projected (in a writable state) is B Newtons, the value of A / B is a specific value or more. According to this embodiment, a retractable ballpoint pen such as a knock type that is excellent in suppressing air bubbles in the ink, handling of the refill, transparency of the refill, and operability when the refill projects and retracts can be provided.
[0012] Preferably, the hydroxyl group-containing resin is polyvinyl alcohol or an ethylene-vinyl alcohol copolymer, and the inorganic layered compound is a clay mineral.
[0013] Preferably, the compression load is 0.29 Newtons or greater.
[0014] Preferably, the coating layer has a thickness of 0.5 micrometers or more and 7.5 micrometers or less.
[0015] Preferably, the ink is sintered at 20° C. and a shear rate of 1 s -1 It is a water-based ink with a viscosity measured at 0.05 Pa·s to 8 Pa·s.
[0016] Preferably, the writing implement is a multi-function writing implement including a plurality of ballpoint pen refills, the ballpoint pen refills being selectively protruding and retracting.
[0017] Preferably, the compression load is 0.29 Newtons or more, the thickness of the coating layer is 0.5 micrometers or more and 7.5 micrometers or less, and the ink is sintered at 20° C. and a shear rate of 1 s -1 The water-based ink has a viscosity of 0.05 Pa·s to 8 Pa·s as measured by a pressure sensor. The multi-function writing instrument is provided with a plurality of the ballpoint pen refills, and the ballpoint pen refills are selectively protruded and retracted.
[0018] One aspect of the present invention is a ballpoint pen refill that is attached to a ballpoint pen, the ballpoint pen comprising: the ballpoint pen refill biased and held by a compression spring; and an operating part that moves the ballpoint pen refill in an axial direction; the ballpoint pen refill is extended or retracted by operating the operating part; the ballpoint pen refill comprises a cylindrical ink holding tube, a tip attached to the tip of the ink holding tube, and ink held in the ink holding tube; the ink holding tube is made of polyolefin; and a cylindrical coating layer is provided on the outer peripheral surface of the ink holding tube; the coating layer is a gas-impermeable coating film that contains a hydroxyl group-containing resin and an inorganic layered compound; and the coating layer has a thickness of 0.5 micrometers or more and 7.5 micrometers or less.
[0019] This embodiment relates to a ballpoint pen refill that is attached to a retractable ballpoint pen. In this embodiment, the coating layer provided on the outer peripheral surface of the ink reservoir is a gas-impermeable coating film containing a hydroxyl group-containing resin and an inorganic layered compound. The coating layer has a thickness of 0.5 micrometers to 7.5 micrometers. According to this embodiment, it is possible to provide a ballpoint pen refill that is suitable for a retractable ballpoint pen, which has excellent ink bubble suppression, handling properties, and transparency.
[0020] Preferably, the hydroxyl group-containing resin is polyvinyl alcohol or an ethylene-vinyl alcohol copolymer, and the inorganic layered compound is a clay mineral.
[0021] Preferably, the ink is sintered at 20° C. and a shear rate of 1 s -1 It is a water-based ink with a viscosity measured at 0.05 Pa·s to 8 Pa·s. Effect of the Invention
[0022] According to the present invention, it is possible to provide a retractable ballpoint pen that is excellent in both suppressing air bubbles in the ink and in ease of handling, and a ballpoint pen refill suitable for the same. [Brief description of the drawings]
[0023] [Figure 1] 1A to 1C are diagrams showing a ballpoint pen refill according to one embodiment of the present invention, where (a) is a front view, (b) is a vertical cross-sectional view of (a), and (c) is an enlarged view of the AA cross-section of (a). [Diagram 2] 2A and 2B are perspective views showing the appearance of a retractable ballpoint pen equipped with the ballpoint pen refill of FIG. 1, where (a) is an example of a knock type ballpoint pen, and (b) is an example of a slide type ballpoint pen. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0024] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. In order to facilitate understanding of the invention, the size and thickness of each component are partially exaggerated in each drawing, and may not necessarily correspond to the actual size and ratio. In addition, the vertical and horizontal directions in the following description are based on the postures in Fig. 1(a) and Fig. 1(b). The lower side of Fig. 1(a) and Fig. 1(b) corresponds to the tip side of the ballpoint pen refill, the upper side corresponds to the rear end side of the ballpoint pen refill, and the vertical direction corresponds to the axial direction. In addition, some hatching is omitted in Fig. 1(b).
[0025] 1(a) to 1(c) show a ballpoint pen refill (hereinafter simply referred to as refill) 1 according to one embodiment of the present invention, which is used, for example, in a multi-function writing instrument (multi-color ballpoint pen) that selectively protrudes and retracts a plurality of refills 1. The refill 1 comprises an ink reservoir 2, a tip 3 attached to the tip of the ink reservoir 2, and ink 5 contained within the ink reservoir 2.
[0026] The ink holding cylinder 2 is a member for holding the ink 5, and occupies most of the refill 1. The ink holding cylinder 2 is an elongated cylindrical shape. The ink holding cylinder 2 is also an elongated tube, and is hollow inside. The ink holding cylinder 2 has an outer diameter of about 2.6 mm to 3.5 mm, preferably about 2.6 mm, an inner diameter of about 1.2 mm to 2.7 mm, preferably about 1.6 mm, and a thickness of about 0.4 mm to 0.7 mm, preferably about 0.5 mm. The ink holding cylinder 2 is made of polyolefin and has gas permeability. Specific examples of polyolefin include polypropylene and polyethylene.
[0027] The tip 3 is attached to the tip of the ink reservoir 2. Specifically, a part of the tip 3 is inserted into and joined to one end of the ink reservoir 2. A writing ball (not shown) is rotatably held within the tip 3, and the ink 5 in the ink reservoir 2 is guided to the writing ball, and the ink 5 is applied to paper or the like as the writing ball rotates. The tip 3 is a typical one made of a metal such as stainless steel. A cross section of the tip 3 is not shown in FIG. 1(b).
[0028] The ink 5 is contained in the ink containing cylinder 2. The ink 5 is filled so as to occupy about 60 to 80% of the total length of the ink containing cylinder 2. The front end of the ink 5 is in contact with the rear end of the tip 3. The ink 5 may be either an oil-based ink or a water-based ink. In one embodiment, the ink 5 is heated at 20° C. at a shear rate of 1 s -1 The viscosity of the water-based ink is from 0.05 Pa·s to 8 Pa·s, as measured. Preferably, the viscosity is in the range of from 3.5 Pa·s to 4.5 Pa·s. At the rear end of the ink 5, a backflow prevention agent 8 for preventing evaporation of the ink 5 is contained.
[0029] 1(a) to 1(c), a cylindrical coating layer 6 is provided on the outer circumferential surface of the ink holding cylinder 2. The coating layer 6 preferably covers the entire outer circumferential surface of the portion filled with ink 5, and in this embodiment, the coating layer 6 is provided on approximately the entire outer circumferential surface of the ink holding cylinder 2.
[0030] The coating layer 6 is composed of a gas-impermeable coating film containing a hydroxyl group-containing resin and an inorganic layered compound.
[0031] Examples of the hydroxyl group-containing resin include polyvinyl alcohol (PVA), vinylamine-vinyl alcohol copolymer, (meth)acrylic acid-vinyl alcohol copolymer, ethylene-vinyl alcohol copolymer (EVOH), polysaccharides, and derivatives thereof. Polyvinyl alcohol or ethylene-vinyl alcohol copolymer is preferable. The hydroxyl group-containing resin may contain a metal alkoxide hydrolysate. The metal alkoxide hydrolysate is preferably a condensate of tetraethoxysilane hydrolysate and / or a condensate of triisopropoxyaluminum hydrolysate, more preferably a condensate of tetraethoxysilane hydrolysate. These hydroxyl group-containing resins may be used alone or in combination of two or more.
[0032] Examples of inorganic layered compounds include clay minerals. Examples of clay minerals include kaolinite, dickite, nacrite, halloysite, antigorite, chrysotile, pyrophyllite, montmorillonite, beidellite, nontronite, saponite, sauconite, stevensite, hectorite, tetrasilylic mica, sodium teniolite, muscovite, margarite, talc, vermiculite, phlogopite, xanthophyllite, chlorite, hydrotalcite, etc. Smectite clay minerals such as montmorillonite, beidellite, nontronite, saponite, sauconite, stevensite, and hectorite are preferred, and montmorillonite is more preferred. These inorganic layered compounds may be used alone or in combination of two or more.
[0033] The coating film constituting the coating layer 6 can be formed using a coating liquid containing a hydroxyl group-containing resin and an inorganic layered compound. An example of the coating liquid is STRADER NOH3000 (Sumitomo Chemical Co., Ltd.).
[0034] The thickness of the coating layer 6 is not particularly limited, but is, for example, 0.5 μm (micrometers) or more, preferably 1 μm or more, and more preferably about 2 μm. In this embodiment, the coating layer 6 is composed of a coating film containing a hydroxyl group-containing resin and an inorganic layered compound, so that even an extremely thin thickness such as 0.5 μm can sufficiently prevent air from entering. There is no particular upper limit to the thickness of the coating layer 6, but it can be, for example, 100 μm or less, preferably 10 μm or less, and more preferably 7.5 μm or less. Note that the thickness of the coating layer 6 is exaggerated in Figures 1(b) and 1(c). If the coating layer 6 is too thick, the transparency may decrease, making it difficult to distinguish the ink color from the outside, whereas if the coating layer 6 is too thin, it may not exhibit sufficient gas barrier properties.
[0035] In this embodiment, the refill 1 is built into a retractable ballpoint pen. Specifically, the refill 1 is biased and held in the barrel of a knock-type or slide-type retractable ballpoint pen by a compression spring (not shown). By operating an operating part provided on the ballpoint pen, the refill 1 can be moved in the axial direction, and the tip 3 of the refill 1 can be protruded and retracted.
[0036] 2(a) and 2(b) show an example of a retractable ballpoint pen equipped with a refill 1. The ballpoint pen 10 shown in Fig. 2(a) is a knock-type ballpoint pen, and is equipped with a refill 1 inside a ballpoint pen body (barrel) 11, and the refill 1 is biased and held by a compression spring (not shown). The refill 1 can be extended or retracted by pressing (knocking) an operating member 12 protruding from the rear end of the ballpoint pen body 11.
[0037] 2(b) is a multi-function writing instrument that selectively pops out and retracts a plurality of refills, and includes a plurality of refills 1 inside a ballpoint pen body 21, with each refill 1 being biased and held by a compression spring (not shown). A plurality of slide members 22 corresponding to each refill 1 are provided on the side of the ballpoint pen body 21. By sliding the slide members 22, the corresponding refill 1 can be popped out and retracted.
[0038] In this embodiment, the compression load of the compression spring when the refill 1 is protruding (in a writing state) is 30 gf (0.29 N) or more, preferably 35 gf (0.34 N) or more, more preferably 40 gf (0.39 N) or more, and even more preferably about 70 gf (0.69 N). If the compression load is less than 30 gf, the refill 1 may not return well when retracted, which may reduce operability. The upper limit of the compression load is usually about 100 gf (0.98 N), but even if it is about 250 gf (2.45 N), it is practically acceptable. If the compression load is too large, a strong force is required to operate the operation part, which may make it difficult to extend and retract the refill. If the compression load is too small, the protruding refill may not return smoothly when retracted. In addition, the refill may easily come off from the ballpoint pen body.
[0039] In this embodiment, the value of A / B (A divided by B) is 1.0 or more when the thickness of the covering layer 6 is A micrometers (μm) and the load of the compression spring when the refill 1 is protruding is B Newtons (N). The A / B value is preferably 1.2 or more. There is no particular upper limit for the A / B value, but it can be set to, for example, 14 or less, preferably 11 or less. If the A / B value is too large, the load of the compression spring when compressed may be insufficient, and the protruding refill may not return well when retracted. In addition, the refill may easily come off from the ballpoint pen body. In addition, the thickness of the covering layer may be too large, and the transparency may decrease, making it difficult to distinguish the ink color from the outside. If the A / B value is too small, the thickness of the covering layer may be insufficient, and sufficient gas barrier properties may not be exhibited. In addition, the load of the compression spring when compressed may be too large, requiring a strong force when operating the operating part, and making it difficult to operate the refill.
[0040] The refill 1 of this embodiment is particularly suitable for use in retractable ballpoint pens, which are susceptible to physical shocks, but can also be used suitably in capped ballpoint pens.
[0041] As described above, the refill 1 is also suitable for use in a multi-function writing instrument (multi-color ballpoint pen) in which multiple refills are selectively inserted and removed. In the case of a multi-color ballpoint pen, since the space inside the ballpoint pen body is limited, it is preferable that the outer diameter of each built-in refill is as small as possible. Here, in this embodiment, the thickness of the covering layer 6 can be made very thin, which has the advantage that the outer diameter of the refill can be made small. In addition, a multi-color ballpoint pen usually includes a guide member having multiple through holes. Then, by having each ballpoint pen refill penetrate each through hole, the guide member functions as a guide for moving the ballpoint pen refill back and forth. Here, in this embodiment, since polyvinylidene chloride is not used for the covering layer 6, the refill surface has good slipperiness. As a result, when the ballpoint pen refill moves back and forth, it is less likely to get caught on the guide member, and there is also less interference between the refills, so that smoother back and forth movement can be achieved. EXAMPLES
[0042] 1. Preparation of ink A ballpoint pen ink having the following composition (unit: parts by weight) was prepared. <Composition> Antiseptic and antifungal agent: 0.44 Water-soluble organic solvent: 6.00 Ion exchange water: 68.26 Thickener: 0.26 Sodium benzoate: 0.26 Caustic soda: 0.34 Phosphate surfactant: 0.75 Wetting agent: 14.0 Carbon Black: 8.01 Dispersant: 1.60 Rust inhibitor: 0.08
[0043] 2. Making ballpoint pen refills A cylindrical polypropylene pipe (total length 85 mm, inner diameter 1.6 mm, wall thickness 0.5 mm) was prepared as the ink reservoir. STRADER NOH3000 (Sumitomo Chemical Co., Ltd.) was prepared as a gas barrier coating agent containing a hydroxyl group-containing resin and an inorganic layered compound (hereinafter referred to as the new coating agent). As a control gas barrier coating agent, polyvinylidene chloride was dissolved in tetrahydrofuran (THF) to prepare a 20% solution of polyvinylidene chloride.
[0044] A tip and a tip were attached to a polypropylene pipe. The ink was filled into the pipe, and the back end of the ink was filled with a backflow prevention agent. The ink and the backflow prevention agent were brought to the tip side by centrifugal treatment. In order to make the coating agent adhere to the pipe, surface treatment (plasma irradiation treatment, frame treatment, application of anchor agent, application of adhesive layer, etc.) was performed in advance on the pipe. A gas barrier coating agent (a new coating agent or a polyvinylidene chloride solution) was applied to the pipe portion and dried to prepare a ballpoint pen refill. In this way, various ballpoint pen refills were prepared, each of which was provided with a coating layer having a predetermined thickness and made of a coating film made of the new coating agent or polyvinylidene chloride. Experimental Examples 1 to 6 and 10 to 11 were provided with a coating layer made of the new coating agent, Experimental Examples 7 to 9 were provided with no coating layer, and Experimental Examples 12 to 13 were provided with a coating layer made of polyvinylidene chloride.
[0045] 3. Making a Ballpoint Pen The ballpoint pen refill was attached to the barrel of a knock-type ballpoint pen together with a compression spring to produce various knock-type ballpoint pens. The compression load of the compression spring when the ballpoint pen refill was protruding was set to 20 gf (0.20 N), 40 gf (0.39 N), 70 gf (0.69 N), or 100 gf (0.98 N).
[0046] 4. How to evaluate refill return The refill was attached to the knock-type ballpoint pen body and knocked. If it returned to its original position without getting caught, it was rated as "A" (excellent), and if it got caught or did not return to its original position at all, it was rated as "C" (poor).
[0047] 5. Method for evaluating the effect of suppressing air bubble generation The refill was left to stand overnight in an environment at 10°C. The refill was attached to a knock-type ballpoint pen body and knocked 10 times. The refill was removed and left to stand for 7 days in an environment at 50°C. After standing, the presence or absence of air bubbles was confirmed using an X-ray irradiation device (SOFTEX M-60, Softex Co., Ltd.). Ten pens of each type were subjected to the test, and the air bubble generation rate (%) was calculated using the following formula. Air bubble occurrence rate (%) = Number of pieces with air bubbles / Number of pieces used in the test x 100 The evaluation was based on a three-point scale, with a bubble occurrence rate of less than 20% being "A" (excellent), 20% to less than 40% being "B" (good), and 40% or more being "C" (poor).
[0048] 6. Method for evaluating the effect of suppressing ink loss The weight of the ink filled and the weight of the refill after filling with ink were measured in advance, and the refill was stored at 50°C for 3 days. After storage, the weight of the refill was measured. The weight of the ink lost was calculated and compared with that of a refill that did not have a coating layer. The ink weight loss rate (%) was calculated using the following formula. Ink weight loss rate (%) = Ink weight loss with coating layer / Ink weight loss without coating layer x 100 The evaluation was done on a two-level scale, with an ink loss rate of less than 80% being rated "A" (excellent) and 80% or more being rated "C" (poor).
[0049] 7. Method for evaluating uneven drying of coating agents After coating the refill with the coating agent, it was dried with hot air (hair dryer). If the surface after drying was transparent and the refill was visible, it was rated as "A" (excellent), and if there were white streaks or lumps and some areas of transparency were lost, it was rated as "C" (poor).
[0050] 8. Overall rating If all four of the above items received an "A" rating, the overall rating was "A" (excellent); if even one item received a "C" rating, the overall rating was "C" (poor); and in all other cases, the overall rating was "B" (good).
[0051] 9.Results The results are shown in Table 1. In Table 1, "spring strength" indicates the load applied to the compression spring when the ballpoint pen refill is protruded.
[0052] Experimental Examples 1 to 6, which had a coating layer made from the new coating agent, showed excellent performance in all items (overall evaluation A). In particular, even Experimental Example 4, which had an extremely thin coating layer thickness of 0.5 μm, demonstrated excellent gas barrier properties, and by appropriately setting the spring strength, it received high evaluations for the air bubble generation rate and ink loss rate. The spring strength of Experimental Examples 1 to 6 was 40 to 100 gf (0.39 to 0.98 N), and the A / B value (μm / N) was in the range of 1.3 to 7.3.
[0053] In Experimental Example 10, in which the thickness of the coating layer made of the new coating agent was set to 0.5 μm and the spring strength was set to 70 gf, air bubbles were generated in the ink (evaluation C). A comparison of Experimental Example 4 and Experimental Example 10 showed that the balance between the thickness of the coating layer and the spring strength is important.
[0054] In Experimental Example 11, in which the thickness of the coating layer made of the new coating agent was set to 10 μm, high evaluations were obtained for the rate of air bubble generation and the rate of ink loss (evaluation A). However, unevenness in the coating occurred (evaluation: C).
[0055] In Experimental Examples 7 to 9, in which no coating layer was provided, air bubbles occurred in the ink (Ratings B and C). The ink loss rate was also rated low (Rating C). Even in Experimental Example 7, in which the spring strength was lowered to 20 gf (0.20 N), the occurrence of air bubbles could not be completely prevented (Rating B). In fact, in Experimental Example 7, the spring strength was insufficient, and the refill return was rated low, resulting in poor operability (Rating C).
[0056] In Experimental Examples 12 and 13, in which a coating layer made of polyvinylidene chloride was provided, the coating agent dried unevenly (evaluation C). Specifically, the coating layer was white and had some areas where transparency was lost. In Experimental Example 12, in which the coating layer was 10 μm thick, the gas barrier properties were insufficient, and air bubbles were generated in the ink (evaluation C).
[0057] Since the A / B value of Experimental Example 4 was 1.3 and the A / B value of Experimental Example 10 was 0.73, a preferable example of the lower limit of the A / B value was considered to be about 1.0. Also, since the A / B value of Experimental Example 3 was 7.3 and the A / B value of Experimental Example 11 was 15, a preferable example of the upper limit of the A / B value was considered to be about 11.
[0058] From the above, it was shown that by providing a coating layer made of a new coating agent on the surface of the refill and appropriately selecting the thickness and spring strength of the coating layer, it is possible to provide a retractable ballpoint pen such as a knock type that suppresses the generation of ink bubbles, suppresses ink loss, has refill transparency, and is easy to use. In particular, it was shown that a retractable ballpoint pen with excellent performance can be provided by setting the A / B value to 1.0 or more.
[0059] [Table 1]
[0060] 10. Friction resistance of coating film The friction resistance of coatings formed from the new coating agent and polyvinylidene chloride was investigated. The test was conducted by sliding on the same material, in accordance with JIS K7125. As a result, the static friction coefficient was 0.335 for the new coating agent coating and 0.722 for the polyvinylidene chloride coating. This confirmed that the new coating agent coating has better slipperiness than the polyvinylidene chloride coating. The dynamic friction coefficient was 0.147 for the new coating agent coating and 0.139 for the polyvinylidene chloride coating, with no significant difference. [Explanation of symbols]
[0061] 1 ballpoint pen refill 2 Ink container 3. Chip 5 Ink 6 Covering layer 10,20 Ballpoint pen 12,22 Operation unit
Claims
1. A ballpoint pen comprising a ballpoint pen refill biased and held by a compression spring, and an operating part for moving the ballpoint pen refill in an axial direction, the ballpoint pen refill being extended and retracted by operating the operating part, The ballpoint pen refill comprises a cylindrical ink reservoir, a tip attached to a tip of the ink reservoir, and ink contained in the ink reservoir, The ink reservoir is made of polyolefin, The ink reservoir has an outer circumferential surface provided with a cylindrical coating layer, the coating layer is a gas-impermeable coating film containing a hydroxyl group-containing resin and an inorganic layered compound, A ballpoint pen characterized in that, when the thickness of the coating layer is A micrometers and the compression load of the compression spring when the ballpoint pen refill is protruded is B Newtons, the value of A / B is 1.0 or more.
2. 2. The ballpoint pen according to claim 1, wherein the hydroxyl group-containing resin is polyvinyl alcohol or an ethylene-vinyl alcohol copolymer, and the inorganic layer compound is a clay mineral.
3. 3. The ballpoint pen according to claim 1, wherein the compression load is 0.29 Newtons or more.
4. 3. The ballpoint pen according to claim 1, wherein the coating layer has a thickness of 0.5 micrometers or more and 7.5 micrometers or less.
5. The ink was mixed at 20° C. and a shear rate of 1 s -1 3. The ballpoint pen according to claim 1, wherein the ink is a water-based ink having a viscosity of 0.05 Pa·s to 8 Pa·s as measured by a viscosity measuring method.
6. 3. The ballpoint pen according to claim 1, wherein the ballpoint pen is a multi-function writing instrument having a plurality of ballpoint pen refills, the ballpoint pen refills being selectively protruding and retracting.
7. The compression load is 0.29 Newtons or more, The thickness of the coating layer is 0.5 micrometers or more and 7.5 micrometers or less, The ink was mixed at 20° C. and a shear rate of 1 s -1 The ink has a viscosity of 0.05 Pa·s to 8 Pa·s, 3. The ballpoint pen according to claim 2, wherein the ballpoint pen is a multi-function writing instrument having a plurality of ballpoint pen refills, the ballpoint pen refills being selectively protruding and retracting.
8. A ballpoint pen refill for use in a ballpoint pen, The ballpoint pen includes the ballpoint pen refill biased and held by a compression spring, and an operating part for moving the ballpoint pen refill in an axial direction, and the ballpoint pen refill is extended or retracted by operating the operating part; The ink cartridge comprises a cylindrical ink reservoir, a tip attached to a tip of the ink reservoir, and ink contained in the ink reservoir, The ink reservoir is made of polyolefin, The ink reservoir has an outer circumferential surface provided with a cylindrical coating layer, the coating layer is a gas-impermeable coating film containing a hydroxyl group-containing resin and an inorganic layered compound, A ballpoint pen refill, wherein the coating layer has a thickness of 0.5 micrometers or more and 7.5 micrometers or less.
9. 9. The ballpoint pen refill according to claim 8, wherein the hydroxyl group-containing resin is polyvinyl alcohol or an ethylene-vinyl alcohol copolymer, and the inorganic layer compound is a clay mineral.
10. The ink was mixed at 20° C. and a shear rate of 1 s -1 10. The ballpoint pen refill according to claim 8, wherein the ink is a water-based ink having a viscosity of 0.05 Pa·s to 8 Pa·s as measured by a viscosity measuring method.
Citation Information
Patent Citations
Application utensil
JP1997141180A
Tip holder for writing instrument and writing instrument using the same
JP2013136165A
Retractable writing utensil
JP2016117274A
Ink storage tube and writing instrument
JP2019031077A
Writing instrument
JP2020104339A