Tire manufacturing method and tire vulcanizer
The tire manufacturing method employs a high-pressure initial inflation phase in the bladder to expedite the shaping process, addressing inefficiencies in existing methods and improving tire production efficiency.
Patent Information
- Application Number
- JP2023079364
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-12
- Publication Date
- 2024-11-22
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing tire vulcanizing processes are inefficient, leading to prolonged shaping times and reduced tire productivity.
A tire manufacturing method utilizing a tire vulcanizer with a bladder that inflates at a higher pressure during a predetermined initial period of the shaping process, followed by a controlled pressure adjustment to achieve rapid inflation and deflation, thereby reducing the overall shaping time.
The method significantly shortens the shaping process time while maintaining tire quality, enhancing productivity by optimizing the bladder inflation and deflation cycles.
Smart Images

Figure 2024163607000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a tire vulcanizing bladder and a tire vulcanizer. [Background technology]
[0002] JP 2020-55203 A discloses a method for manufacturing a tire. The tire manufacturing method disclosed here includes a shaping step in which a bladder is expanded in a cavity of a raw tire including a first bead portion and a second bead portion separated in the tire axial direction, and the raw tire is shaped into a predetermined shape. The shaping step includes a first step in which the bladder is expanded in a first region, which is a region on the first bead portion side of the cavity of the raw tire, to shape only the first region of the raw tire, and a second step, which is performed subsequent to the first step, in which the expanded bladder is gradually expanded into a second region, which is a region on the second bead portion side of the cavity of the raw tire, to shape both the first region and the second region of the raw tire. This method is said to suppress the occurrence of scratches on a vulcanized tire due to misalignment of the set position, etc. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2020-55203 A Summary of the Invention [Problem to be solved by the invention]
[0004] The objective of the present invention is to shorten the shaping process time for tire vulcanizing bladders and tire vulcanizers, thereby improving tire productivity. [Means for solving the problem]
[0005] The tire manufacturing method disclosed herein is a tire manufacturing method in which tires are manufactured by a tire vulcanizer. Here, the tire vulcanizer includes a bladder arranged at the center, a molding die arranged to surround the bladder, and a mechanism for opening and closing the die. The bladder is configured to expand when a pressurized medium is supplied and to contract when the pressurized medium is discharged. The manufacturing method includes a step of arranging a row cover to surround the bladder in a deflated state, and a shaping step of supplying a pressurized medium to the bladder and expanding the bladder. In the shaping step, the pressurized medium is supplied to the bladder at a pressure higher than that in other periods during a first period determined in advance from the start of supply of the pressurized medium to the bladder.
[0006] The tire vulcanizer disclosed herein comprises a bladder arranged in the center, a molding die arranged to surround the bladder, a mechanism for opening and closing the die, a supply device for supplying pressurized medium to the bladder, a discharge device for discharging the pressurized medium from the bladder, and a control device. The control device is configured to supply the pressurized medium to the bladder at a higher pressure than in other periods during a predetermined first period from the start of supply of the pressurized medium to the bladder during a shaping process in which the pressurized medium is supplied to the bladder and the bladder is expanded. Effect of the Invention
[0007] According to the tire manufacturing method and tire vulcanizer disclosed herein, the time required for the shaping process is shortened. [Brief description of the drawings]
[0008] [Figure 1] FIG. 1 is a schematic diagram of a tire vulcanizer 10. As shown in FIG. [Diagram 2] FIG. 2 is a schematic diagram of a tire vulcanizer 10. As shown in FIG. [Diagram 3] FIG. 3 is a time chart showing changes in the supply pressure of the pressurized medium in the shaping process. [Figure 4]FIG. 4 is a time chart showing the change in the internal pressure of the bladder 40 during the shaping process. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0009] An embodiment of the invention disclosed herein will be described below with reference to the drawings. The present invention is not limited to the following embodiment. Each drawing is drawn diagrammatically and does not necessarily reflect the actual product. Each drawing shows only an example, and does not limit the present invention unless otherwise specified. Members and parts that perform the same function are appropriately given the same reference numerals, and duplicated explanations are omitted. In this specification, a notation such as "X to Y" indicating a numerical range means "X or more and Y or less" unless otherwise specified.
[0010] <Tire vulcanizer 10> Figures 1 and 2 are schematic diagrams of a tire vulcanizer 10. Figure 1 illustrates a state in which a mold 20 is open, and Figure 2 illustrates a state in which the mold 20 is closed. In Figure 1, hatching of cross sections of a bladder 40 and a row cover 200 is omitted. Here, Figures 1 and 2 show one embodiment of a tire vulcanizer, and the tire vulcanizer is not limited to the form of Figures 1 and 2 unless otherwise specified.
[0011] As shown in FIGS. 1 and 2, the tire vulcanizer 10 includes a bladder 40, a mold 20, and a mechanism 30 for opening and closing the mold 20.
[0012] Bladder 40 is a member that molds the inner surface of the tire. Bladder 40 is an annular member that expands and contracts within mold 20 when molding a tire. Bladder 40 is configured to expand when a pressurized medium is supplied and to contract when the pressurized medium is discharged. Mold 20 is disposed to surround bladder 40, is configured as a split mold made up of multiple molds, and is attached to mechanism 30 that opens and closes mold 20.
[0013] In the embodiment shown in FIG. 1 and FIG. 2, the mold 20 includes a lower side mold 21, a plurality of tread molds 23, and an upper side mold 22. Here, the lower side mold 21 is a mold disposed on the lower side around the bladder 40. The plurality of tread molds 23 are molds for forming the tread portion of the tire, and are constituted by split molds divided in the circumferential direction. The tread mold 23 is disposed on the outer diameter side around the bladder 40, and is attached to a mechanism 31 that moves in the radial direction relative to the bladder 40. The upper side mold 22 is a mold disposed on the upper side around the bladder 40, and is attached to a mechanism 32 that moves up and down relative to the lower side mold 21. Here, a configuration example of the mold 20 used in the tire vulcanizer 10 is shown, and the mold 20 is not limited to such a form unless otherwise specified. For example, the mold used in the tire vulcanizer may be a split mold consisting of an upper mold and a lower mold.
[0014] <Low Cover 200> The low cover 200 is an unvulcanized tire before vulcanization and is also called a raw tire. The low cover 200 is a cylindrical member in which unvulcanized sidewall rubber and tread rubber are bonded to a base material such as a bead wire, a carcass, or a belt. Bead portions 201 and 202 are provided on the periphery of both sides of the low cover 200.
[0015] 1 and 2, the tire vulcanizer 10 includes a lower container 11, an upper container 12, a bladder holding mechanism 50, a medium supply pipe 80, and a control device 400 in addition to the bladder 40 and the mold 20. The tire vulcanizer 10 shown in FIGS. 1 and 2 will be described in more detail below.
[0016] <Lower Container 11> The lower container 11 is a member supported by a table (not shown) of a press machine or the like, and includes a lower plate 13. A part of a mold 20 is attached to the lower container 11. In this embodiment, a lower side mold 21 is attached on the lower plate 13 as a part of the mold 20 attached to the lower container 11. A lower bead ring 21b that holds a bead portion 201 on the lower side of the low cover 200 is attached on the lower side mold 21. The lower bead ring 21b is provided with a portion 21b1 that holds the bead portion 201 on the lower side of the low cover 200, and a gripping portion 21b2 that grips a lower end peripheral portion 42 of the bladder 40. The gripping portion 21b2 is provided on the inner diameter side of the portion 21b1 that holds the bead portion 201 on the lower side of the low cover 200.
[0017] <Upper container 12> The upper container 12 includes an upper plate 17 and an expansion / contraction guide 18. The upper plate 17 is a plate member attached to, for example, a press plate of a press machine (not shown), and is disposed above the lower plate 13.
[0018] The expansion / contraction guide 18 includes a slider 18a and a pusher 18b. The slider 18a is configured to move inward and outward in the radial direction along the lower surface of the upper plate 17. A tapered surface 18a1 that widens outward as it goes downward is formed on the outer surface of the slider 18a. The pusher 18b is a member that extends downward so as to contact the outer surface of the slider 18a. The pusher 18b is provided with a tapered surface 18b1 that widens outward as it goes downward so as to face the tapered surface 18a1 of the slider 18a. In this embodiment, the sliders 18a are arranged radially in the circumferential direction. When the upper container 12 descends and the pusher 18b descends, the sliders 18a move inward, the intervals between the sliders 18a become closer, and the sliders 18a are formed into a substantially circular ring shape. The pusher 18b may be attached to a press machine and configured to move up and down together with the upper plate 17.
[0019] A part of a mold 20 is attached to the upper container 12. In this embodiment, an upper side mold 22 and a tread mold 23 are attached to the upper container 12 as parts of the mold 20. The upper side mold 22 is attached below the upper plate 17. An upper bead ring 22b that holds an upper bead portion 202 of the low cover 200 is attached to the edge of the inner diameter side of the upper side mold 22. The tread mold 23 is composed of a plurality of molds that can be divided in the circumferential direction, and is attached to the inner peripheral surface of the slider 18a.
[0020] In this way, among the mechanism 30 for opening and closing the mold 20, the mechanism 32 for moving the upper side mold 22 up and down relative to the lower side mold 21 may be composed of a mechanism that moves up and down, such as a press machine. Also, among the mechanism 30 for opening and closing the mold 20, the mechanism 31 for moving the tread mold 23 in the radial direction relative to the bladder 40 may be composed of the slider 18a and pusher 18b attached to the press machine.
[0021] <Bladder 40> The bladder 40 is a member that molds the inner surface of the tire. The bladder 40 is a cylindrical elastic body made of rubber. Here, the bladder 40 is disposed in the center surrounded by the mold 20 between the lower container 11 and the upper container 12, and is attached to a bladder holding mechanism 50.
[0022] <Bladder retention mechanism 50> The bladder holding mechanism 50 includes an upper clamp member 54, a lower clamp member 56, and a center post 58. The center post 58 is an axial member that penetrates the center of the lower container 11 and extends in the vertical direction between the lower container 11 and the upper container 12. The upper clamp member 54 and the lower clamp member 56 are attached to the center post 58.
[0023] The upper clamp member 54 is a member that grips the upper end of the bladder 40. In this embodiment, the upper clamp member 54 is a disk-shaped member attached to the upper end of the center post 58. A gripping portion 54a that grips the upper end peripheral portion 41 of the bladder 40 is provided on the outer periphery of the upper clamp member 54. Although not shown in the figure, the upper clamp member 54 can be, for example, a member that can be separated into upper and lower portions and has a structure that sandwiches and holds the upper end peripheral portion 41 of the bladder 40.
[0024] The lower clamp member 56 is a member that grips the lower end of the bladder 40. In this embodiment, the lower clamp member 56 is a disk-shaped member that is attached to the center post 58 and spaced apart from the lower side of the upper clamp member 54. The lower clamp member 56 is attached to the upper surface of the lower bead ring 21b, and a gripping portion 56a that grips the lower end peripheral portion 42 of the bladder 40 is provided on the outer circumferential edge of the lower clamp member 56. The lower end peripheral portion 42 of the bladder 40 is held by being sandwiched between the outer circumferential edge of the lower clamp member 56 and a gripping portion 21b2 provided on the lower bead ring 21b.
[0025] <Medium supply pipe 80> In this embodiment, the medium supply pipe 80 is attached around the center post 58. One end of the medium supply pipe 80 communicates with the inside of the bladder 40 through an opening formed in the lower clamp member 56. The medium supply pipe 80 is a pipe that supplies the pressurized medium and nitrogen into the bladder 40 and recovers the drain. The medium supply pipe 80 is connected to a medium supply and discharge device 82. The bladder 40 expands when the pressurized medium is supplied through the medium supply pipe 80, and contracts when the pressurized medium is discharged. The supply and discharge of the pressurized medium to and from the bladder 40 through the medium supply pipe 80 is controlled by a control device 400.
[0026] The medium supply / discharge device 82 may include a medium supply device 82a, a medium discharge device 82b, and a drain recovery device 82c. The medium supply device 82a is a device that supplies the pressurized medium to the bladder 40. The medium supply device 82a may include a pump and a mechanism for forcibly sending the pressurized medium to the bladder 40. The medium discharge device 82b is a device that removes the pressurized medium from the bladder 40. The medium discharge device 82b may include a mechanism for forcibly discharging the pressurized medium from the bladder 40, and may utilize the pump of the medium supply device 82a. The drain recovery device is a device that discharges liquid liquefied in the bladder 40 when the pressurized medium supplied to the bladder 40 is pressurized steam. In the drain recovery device, a drain pipe may be connected to a part of the medium supply pipe 80.
[0027] <Shaping process> In this manner, the bladder 40 is configured to expand when the pressurized medium is supplied and to contract when the pressurized medium is discharged. In Fig. 1, the deflated state of the bladder 40 is indicated by a two-dot chain line. The raw cover 200 is set at a predetermined position of the tire vulcanizer 10 so as to surround the bladder 40 when the bladder 40 is in the deflated state. Then, as shown in Fig. 1, the raw cover 200 is held by the bladder 40 by inflating the bladder 40. In the process of inflating the bladder 40 from the deflated state to hold the raw cover 200 by the bladder 40, the process of inflating the bladder 40 is called a shaping process.
[0028] The pressurized medium is supplied to the bladder 40 at a predetermined supply pressure. In this case, the supply of the pressurized medium to the bladder 40 is started by increasing the pressure to a predetermined supply pressure, and then stabilizing the supply pressure at the predetermined supply pressure to supply the pressurized medium to the bladder 40. The internal pressure of the bladder 40 gradually increases. This allows the internal pressure of the bladder 40 to reach a desired final pressure. In this case, since the supply pressure of the pressurized medium is constant, it is easy to adjust the internal pressure of the bladder 40 to a target pressure. In the tire vulcanizer 10, the shaping process for inflating the bladder 40 may be divided into two steps to inflate the bladder 40.
[0029] In this case, for example, in the first shaping step, the pressurized medium is supplied to the bladder 40 by increasing the pressure from the start of the supply of the pressurized medium to a predetermined supply pressure. Then, after the desired internal pressure is reached in the first shaping step, the pressurized medium is once removed from the bladder 40, a step of depressurizing the bladder 40 is carried out, and then a second shaping step is carried out. In the second shaping step, after the step of depressurizing the bladder 40, the pressure is again increased from the start of the supply of the pressurized medium to a predetermined supply pressure, and the pressurized medium is supplied to the bladder 40 at the predetermined supply pressure. In the second shaping step, the internal pressure of the bladder is allowed to reach the predetermined internal pressure.
[0030] Here, the main purpose of the first shaping process is to hold the raw cover 200 by the bladder 40. The main purpose of the second shaping process is to press the bladder 40 against the inner surface of the raw cover 200 so that no air remains between the raw cover 200 and the bladder 40.
[0031] The inventor of the present invention is considering improving the productivity of tires. In particular, he believes that if the time required for vulcanization molding can be shortened, the productivity of tires can be improved. During such consideration, he came up with a new idea for how to inflate the bladder 40 in the shaping process.
[0032] FIG. 3 is a time chart showing the change in the supply pressure of the pressurized medium in the shaping process. In FIG. 3, a time chart of the supply pressure of the pressurized medium in the shaping process is shown typically. The vertical axis of FIG. 3 is the supply pressure of the pressurized medium, and the horizontal axis is time. Here, the supply pressure of the pressurized medium is shown, for example, as the pressure of the pressurized medium flowing through the medium supply pipe 80. As shown in FIG. 1, the medium supply pipe 80 may be provided with sensors 80a such as a pressure sensor and a temperature sensor, and an adjustment valve 80b. The measured values measured by the sensors 80a such as the pressure sensor and the temperature sensor may be configured to be transmitted to the control device 400. The pressure of the pressurized medium flowing through the medium supply pipe 80 may be detected, for example, by a pressure sensor provided in the medium supply pipe 80. The control device 400 is preferably configured to adjust the opening degree of the medium supply device 82a and the regulating valve 80b based on the pressure of the pressurized medium flowing through the medium supply pipe 80 detected by the pressure sensor, thereby adjusting the pressure of the pressurized medium flowing through the medium supply pipe 80.
[0033] The dashed line As in Fig. 3 is a time chart for the case where, in the shaping process, the supply pressure of the pressurized medium to the bladder 40 is gradually increased (s1) after the supply of the pressurized medium to the bladder 40 is started, and the pressurized medium is supplied to the bladder 40 at a predetermined supply pressure (s2). In contrast, the time chart shown by the solid line At in Fig. 3 is a time chart for the tire manufacturing method proposed here. The dashed line As and the solid line At in Fig. 3 are drawn slightly offset from each other so as not to overlap, although the predetermined supply pressure (L1) in another period (t2) is actually the same.
[0034] As shown by the solid line At in FIG. 3, in the tire manufacturing method proposed here, in the shaping process, during a first period (t1) determined in advance from the start of supply of the pressurized medium to the bladder 40, the pressurized medium is supplied to the bladder 40 at a pressure higher than that during other periods (t2). Specifically, as shown by the solid line At in FIG. 3, when the supply of the pressurized medium to the bladder 40 is started in the shaping process, the pressure of the pressurized medium flowing through the medium supply pipe 80 is suddenly increased to be significantly higher than the supply pressure during other periods (t11). Thereafter, the supply pressure is gradually lowered (t12) and adjusted to a predetermined supply pressure (L1) during the other periods (t2). In this case, the amount of pressurized medium supplied to the bladder 40 is increased during the first period (t1) immediately after the supply of the pressurized medium to the bladder 40 is started. Therefore, the time required to supply the pressurized medium to the bladder 40 as a whole is shorter than that shown by the dashed line As in FIG. 3.
[0035] Fig. 4 is a time chart showing the change in the internal pressure of the bladder 40 during the shaping process. Fig. 4 shows a schematic time chart of the internal pressure of the bladder 40 during the shaping process. The vertical axis of Fig. 4 represents the internal pressure of the bladder 40, and the horizontal axis represents time.
[0036] The time chart indicated by dashed line Bs in Fig. 4 shows a change in the internal pressure of bladder 40 when the supply pressure of the pressurized medium to bladder 40 is gradually increased after the supply of the pressurized medium to bladder 40 is started and the pressurized medium is supplied to bladder 40 at a predetermined supply pressure in the shaping process. The time chart indicated by dashed line Bs corresponds to an example in which the pressurized medium is supplied to bladder 40 in the manner indicated by dashed line As in Fig. 3.
[0037] 4, the time chart indicated by the solid line Bt shows a case where the pressurized medium is supplied to the bladder 40 at a higher pressure than in other periods during a predetermined first period (t1) from the start of supply of the pressurized medium to the bladder 40 in the shaping process. The time chart of the solid line Bt corresponds to an example where the pressurized medium is supplied to the bladder 40 in the manner indicated by the solid line At in FIG.
[0038] The time charts Bs and Bt shown in FIG. 4 show the shaping process of the tire vulcanizer 10 in which the bladder 40 is inflated in two separate steps. Here, in the first shaping step C1, the bladder 40 is inflated until the pressure inside the bladder 40 reaches a predetermined pressure. In the first shaping step C1, after the desired internal pressure is reached, the pressurized medium is once removed from the bladder 40. In the second shaping step C2, the bladder 40 is inflated again, and the pressurized medium is supplied until the internal pressure reaches a predetermined internal pressure (Bp1) higher than that in the first shaping step C1.
[0039] In the time chart Bt shown in Fig. 4, in both the first shaping process C1 and the second shaping process C2, the pressurized medium is supplied to the bladder 40 at a higher pressure than in other periods during a predetermined first period (t1) from the start of supply of the pressurized medium to the bladder 40. For this reason, as shown in the time chart Bt of Fig. 4, in both the first shaping process C1 and the second shaping process C2, the internal pressure of the bladder 40 is significantly higher during the first period (t1) immediately after the start of supply of the pressurized medium to the bladder 40. As a result, in the time chart Bt shown in Fig. 4, the time is shortened in both the first shaping process C1 and the second shaping process C2, compared to the time chart Bs.
[0040] This result can be evaluated in terms of the entire shaping process by the time Ts, Tt required for the internal pressure of the bladder 40 to be increased to a predetermined pressure (Bp1) in the second shaping process. As shown in Fig. 4, the time Tt in the time chart Bt in which the supply pressure is increased in the first period (t1) immediately after the start of the supply of pressurized medium to the bladder 40 is significantly shorter than the time Ts in the time chart Bs. According to the inventor's findings, even in this manner in which the supply pressure of the pressurized medium to the bladder 40 is increased in the first period (t1), the quality of the tire to be molded is not affected.
[0041] According to the findings of the present inventor, in a tire designated as 245 / 60R18, when the pressurized medium is supplied to the bladder 40 at a constant supply pressure of 40 kPa, the time required to inflate the bladder 40 to a predetermined internal pressure in the second shaping step C2 was approximately 34.3 seconds in total. In contrast, the first period (t1) is set to 1 second from the start of the supply of the pressurized medium to the bladder 40, and the supply pressure of the pressurized medium to the bladder 40 in the first period (t1) is set to 300 kPa, and thereafter, the pressurized medium is supplied to the bladder 40 at a constant supply pressure of 40 kPa. In this case, the time required to inflate the bladder 40 to a predetermined internal pressure in the second shaping step C2 was shortened to approximately 28.5 seconds in total. In other words, in this case, the time required for the shaping step was shortened by approximately 17%.
[0042] In this case, too, the supply pressure of the pressurized medium is constant in the period after the first period (t1). Therefore, the internal pressure of the bladder 40 is easily adjusted to a target pressure in each shaping process. Furthermore, there is no problem or effect on the quality of the tire to be molded. The supply pressure of the pressurized medium to the bladder 40 in the first period (t1) and the first period (t1) may be determined according to each embodiment so as not to affect the quality of the tire. For example, the first period (t1) may be set to a time up to 10% of the total time for supplying the pressurized medium in each shaping process, assuming that the total time is 100%. If the time is up to 10% of the shaping process, the quality of the tire is not affected.
[0043] According to the findings of the present inventor, the first period (t1) may be set to a time of 3% to 15% inclusive, assuming that the total time for supplying the pressurized medium in each shaping step is 100%. For example, in the first shaping step and the second shaping step, the first period (t1) may be set to an appropriate time, depending on the size of the tire and the performance of the tire vulcanizer 10. Specifically, in the total time for supplying the pressurized medium in each shaping step is 100%, the first period (t1) may be set to, for example, about 8% to 12% inclusive. The first period (t1) may be set to, for example, a time of 0.5 seconds to 2 seconds inclusive, from the start of supply of the pressurized medium in the shaping step. The first period (t1) refers to the time from the start of supply of pressurized medium to bladder 40 until the pressure of the pressurized medium circulating through medium supply pipe 80 is suddenly increased to a level significantly higher than the supply pressure in other periods (t11), and then the supply pressure is gradually decreased (t12) until it is adjusted to a predetermined supply pressure (L1) for another period (t2).
[0044] In the shaping process, the pressurized medium may be supplied to the bladder at a predetermined constant supply pressure as shown in FIG. 3 during periods other than the first period t1. By supplying the pressurized medium to the bladder at a predetermined constant supply pressure, it is easy to adjust the internal pressure of the bladder 40 to the final desired pressure. Here, regarding the supply of the pressurized medium to the bladder at a predetermined constant supply pressure, slight fluctuations in the supply pressure caused by control may be tolerated. In addition, at the end of the period, for example, a period in which the supply pressure is reduced may occur. The maximum value of the supply pressure of the pressurized medium in the first period t1 may be, for example, at least 3.5 times larger than the maximum value of the supply pressure set in the other periods. For example, the maximum value of the supply pressure of the pressurized medium in the first period t1 may be, for example, 5 times or more larger than the maximum value of the supply pressure set in the other periods. As a result, even if the first period t1 is a short time, such as 3% to 15% of the time of the shaping process, an advantageous effect can be obtained in terms of shortening the time required for the shaping process. From the viewpoint of shortening the time required for the shaping process, the maximum value of the supply pressure of the pressurized medium in the first period t1 may be, for example, two or three times the maximum value of the supply pressure set in other periods.
[0045] Thus, the tire manufacturing method proposed here includes a step of arranging the raw cover 200 so as to surround the bladder 40, and a shaping step. The shaping step is a step of supplying a pressurized medium to the bladder 40 to expand the bladder 40. In this shaping step, the pressurized medium is supplied to the bladder 40 at a higher pressure than in other periods during a first period t1 (see Figs. 3 and 4) that is determined in advance from the start of supplying the pressurized medium to the bladder 40. This allows the time required for the shaping step to be significantly shortened. Therefore, the shaping time can be shortened while maintaining the tire quality, and the vulcanization capacity (production volume) of the tire vulcanizer 10 can be improved. According to this tire manufacturing method, the time required for the shaping step can be shortened while maintaining the quality of the manufactured tires.
[0046] The shaping step may be performed in two steps as described above. That is, the shaping step may include a first shaping step, a step of reducing the pressure of the bladder 40 after the first shaping step, and a second shaping step. In this case, in both the first and second shaping steps, the pressurized medium may be supplied to the bladder 40 at a higher pressure than in other periods during a predetermined first period from the start of supply of the pressurized medium to the bladder 40. This makes it possible to shorten the time required for the shaping steps. Furthermore, the first period during which the pressurized medium is supplied to the bladder 40 at a higher pressure than in other periods may be set for at least one of the first shaping step and the second shaping step. In this case as well, it is possible to shorten the time required for the shaping steps.
[0047] Control device 400 Here, the tire manufacturing method can be embodied in a tire vulcanizer 10. As shown in Fig. 1, the tire vulcanizer 10 includes a bladder 40 arranged at the center, a molding die 20 arranged to surround the bladder 40, a mechanism 30 for opening and closing the die 20, a medium supplying device 82a for supplying a pressurized medium to the bladder 40, a medium discharging device 82b for discharging the pressurized medium from the bladder 40, and a control device 400.
[0048] The control device 400 is typically a computer, and includes a storage device (such as a memory) and an arithmetic device (such as a CPU). The control device 400 is a device that performs various processes of the tire vulcanizer 10. Each process of the control device 400 is embodied as a processing module executed by a predetermined program. Each function of the control device 400 can be appropriately embodied by cooperation between the physical components of the tire vulcanizer 10 and control based on the calculation results by the control device 400 performed according to a predetermined program. For example, each configuration and process of the control device 400 can be embodied as a database that stores data embodied by a computer in a predetermined format, a data structure, a processing module that performs a predetermined calculation process according to a predetermined program, or a part of them.
[0049] The processing of the control device 400 may be executed by one computer. Also, the processing of the control device 400 may be executed by multiple computers. Also, the processing of the control device 400 may be executed in cooperation with a computer incorporated inside the tire vulcanizer 10 and an external computer placed at a position remote from the tire vulcanizer 10. For example, the computer incorporated inside the tire vulcanizer 10 and the external computer placed at a position remote from the tire vulcanizer 10 may be communicably connected through a communication network. The information stored in the control device 400 or a part of the information may be stored by an external computer. Also, the processing executed by the control device 400 or a part of the processing may be executed by an external computer.
[0050] The control device 400 may be configured to supply the pressurized medium to the bladder 40 at a higher pressure than the pressure in the other periods t2 during a first period t1 that is determined in advance from the start of supply of the pressurized medium to the bladder 40 during the shaping process in which the pressurized medium is supplied to the bladder 40 and the bladder 40 is expanded. This can shorten the time required for the shaping process.
[0051] In this case, the first period t1 may be set to be, for example, a period of 15% or less from the start of supply of the pressurized medium to the bladder 40 when the total time for supplying the pressurized medium to the bladder 40 in the shaping process is taken as 100%. The control device 400 may be configured to supply the pressurized medium to the bladder 40 at, for example, a predetermined constant supply pressure during the other period. The supply pressure of the pressurized medium during the first period t1 may be set to be, for example, at least 3.5 times larger than the maximum supply pressure set during the other period t2.
[0052] Here, the shaping step may include a first shaping step, a step of depressurizing the bladder 40 after the first shaping step, and a second shaping step, as described above. In this case, the control device 400 may be configured to supply the pressurized medium to the bladder 40 at a higher pressure in a first period t1 from the start of supplying the pressurized medium to the bladder 40 in at least one of the first shaping step and the second shaping step (see FIG. 3 ) than in the other periods t2. For example, the control device 400 may be configured to supply the pressurized medium to the bladder 40 at a higher pressure in a first period from the start of supplying the pressurized medium to the bladder 40 in both the first shaping step and the second shaping step.
[0053] Although the invention disclosed herein has been described in various ways, the invention disclosed herein is not limited to the above-mentioned embodiments and modifications unless otherwise specified. Furthermore, the configurations of the various embodiments and modifications mentioned above can be appropriately combined as long as they are not mutually inhibiting.
[0054] As described above, the present invention (1) relates to a method for manufacturing a tire. The method for producing a tire according to the present invention (1) includes the steps of: A tire manufacturing method for manufacturing a tire by a tire vulcanizer, The tire vulcanizer comprises: The bladder is placed in the center, A molding die arranged to surround the bladder; A mechanism for opening and closing the mold; Equipped with The bladder is The pressure adjusting device is configured to expand when a pressurized medium is supplied thereto and to contract when the pressurized medium is discharged therefrom, The manufacturing method includes: a step of disposing the row cover so as to surround the bladder in a deflated state; a shaping step of supplying a pressurized medium to the bladder to expand the bladder; Including, In the shaping step, the pressurized medium is supplied to the bladder at a higher pressure during a predetermined first period from the start of supply of the pressurized medium to the bladder, compared to other periods.
[0055] The present invention (2) is a method for producing a tire according to the present invention (1), The first period is a period of 15% or less from the start of supply of the pressurized medium to the bladder, when the total time during which the pressurized medium is supplied to the bladder in the shaping step is taken as 100%.
[0056] The present invention (3) is a method for producing a tire according to the present invention (1) or (2), During the other period, the pressurized medium is supplied to the bladder at a predetermined constant supply pressure.
[0057] The present invention (4) is a method for producing a tire according to any one of the present inventions (1) to (3), The maximum value of the supply pressure of the pressurized medium in the first period is at least twice as large as the maximum value of the supply pressure set in the other period.
[0058] The present invention (5) is a method for producing a tire according to any one of the present inventions (1) to (4), The shaping step includes: a first shaping step in which the pressure of the pressurized medium is increased to a predetermined supply pressure from the start of supply of the pressurized medium, and the pressurized medium is supplied to the bladder at the predetermined supply pressure; After the first shaping step, depressurizing the bladder; a second shaping step of increasing the pressure from the start of supply of the pressurized medium to a predetermined supply pressure, supplying the pressurized medium to the bladder at the predetermined supply pressure, and causing the internal pressure of the bladder to reach the predetermined internal pressure after the depressurizing step; Including, In at least one of the first shaping process and the second shaping process, the pressurized medium is supplied to the bladder at a higher pressure than in other periods during a predetermined first period from the start of supply of the pressurized medium to the bladder.
[0059] The present invention (6) is a method for producing a tire according to the present invention (5), In both the first shaping process and the second shaping process, during a predetermined first period from the start of supply of the pressurized medium to the bladder, the pressurized medium is supplied to the bladder at a pressure higher than that during other periods.
[0060] The present invention (7) relates to a tire vulcanizer. The tire vulcanizer in the present invention (7) is The bladder is placed in the center, A molding die arranged to surround the bladder; A mechanism for opening and closing the mold; A supply device for supplying a pressurized medium to the bladder; a discharge device for discharging the pressurized medium from the bladder; Control device and Equipped with The control device includes: During the shaping process in which a pressurized medium is supplied to the bladder and the bladder is expanded, the pressurized medium is supplied to the bladder at a higher pressure during a predetermined first period from the start of supply of the pressurized medium to the bladder than during other periods.
[0061] The present invention (8) is a tire vulcanizer according to the present invention (7), The first period is set to be a period of 15% or less from the start of supply of the pressurized medium to the bladder in the shaping process, when the total time for supplying the pressurized medium to the bladder in the shaping process is taken as 100%.
[0062] The present invention (9) is a tire vulcanizer according to the present invention (7) or (8), The control device is configured to supply pressurized medium to the bladder at a predetermined constant supply pressure during the other period.
[0063] The present invention (10) is a tire vulcanizer according to any one of the present inventions (7) to (9), The supply pressure of the pressurized medium is set so that the maximum value of the supply pressure of the pressurized medium in the first period is at least 3.5 times larger than the maximum value of the supply pressure set in the other periods.
[0064] The present invention (11) is a tire vulcanizer according to any one of the present inventions (7) to (10), The shaping step includes: a first shaping step in which the pressure of the pressurized medium is increased to a predetermined supply pressure from the start of supply of the pressurized medium, and the pressurized medium is supplied to the bladder at the predetermined supply pressure; After the first shaping step, depressurizing the bladder; a second shaping step of increasing the pressure from the start of supply of the pressurized medium to a predetermined supply pressure, supplying the pressurized medium to the bladder at the predetermined supply pressure, and causing the internal pressure of the bladder to reach the predetermined internal pressure after the depressurizing step; Including, The control device is configured so that, in at least one of the first shaping process and the second shaping process, the pressurized medium is supplied to the bladder at a higher pressure during a predetermined first period from the start of supply of the pressurized medium to the bladder than during other periods.
[0065] The present invention (12) is a tire vulcanizer according to the present invention (11), The control device is configured so that, in both the first shaping process and the second shaping process, the pressurized medium is supplied to the bladder at a higher pressure during a predetermined first period from the start of supply of the pressurized medium to the bladder than during other periods. [Explanation of symbols]
[0066] 10 Tire vulcanizer 11 Lower Container 12 Upper container 13 Lower plate 17 Upper Plate 18 Scale Guide 18a Slider 18a1 Tapered surface 18b Pusher 18b1 Tapered surface 20 Mold 21 Lower side mold 21b Lower bead ring 21b1 A portion for holding the bead portion 201 21b2 Grip part 22 Upper side mold 22b Upper bead ring 23 Tread mold 30 Mechanism for opening and closing the mold 20 31 Mechanism for moving radially relative to the bladder 40 32 Mechanism for moving up and down relative to the lower side mold 21 40 Vlada 41 Upper edge 42 Lower edge 50 Bladder retention mechanism 54 Upper clamp member 54a Gripping part 56 Lower clamp member 56a Gripping part 58 Center Post 80 Media supply pipe 80a Sensors 80b Regulating valve 82 Media supply / discharge device 82a Media supply device 82b Media ejector 82c Drain recovery device 200 Low Cover 201,202 Bead section 400 Control device
Claims
1. A tire manufacturing method for manufacturing a tire by a tire vulcanizer, The tire vulcanizer comprises: The bladder is placed in the center, A molding die arranged to surround the bladder; A mechanism for opening and closing the mold; Equipped with The bladder is The pressure adjusting device is configured to expand when a pressurized medium is supplied thereto and to contract when the pressurized medium is discharged therefrom, The manufacturing method includes: a step of disposing the row cover so as to surround the bladder in a deflated state; a shaping step of supplying a pressurized medium to the bladder to expand the bladder; Including, In the shaping step, the pressurized medium is supplied to the bladder at a higher pressure during a predetermined first period from a start of supply of the pressurized medium to the bladder than during other periods. A method for manufacturing tires.
2. 2. The manufacturing method according to claim 1, wherein the first period is a period of 15% or less from a start time of supplying the pressurized medium to the bladder in the shaping process, when a total time for supplying the pressurized medium to the bladder in the shaping process is taken as 100%.
3. The method for manufacturing a tire according to claim 1 , wherein during the other period, the pressurized medium is supplied to the bladder at a predetermined constant supply pressure.
4. The manufacturing method according to claim 1 , wherein a maximum value of the supply pressure of the pressurized medium in the first period is at least twice as large as a maximum value of the supply pressure set in the other period.
5. The shaping step includes: a first shaping step of increasing the pressure of the pressurized medium to a predetermined supply pressure from the start of supply of the pressurized medium and supplying the pressurized medium to the bladder at the predetermined supply pressure; After the first shaping step, depressurizing the bladder; a second shaping step of increasing the pressure from the start of supply of the pressurized medium to a predetermined supply pressure, supplying the pressurized medium to the bladder at the predetermined supply pressure, and causing the internal pressure of the bladder to reach the predetermined internal pressure after the depressurizing step; Including, In at least one of the first shaping step and the second shaping step, the pressurized medium is supplied to the bladder at a higher pressure during a first period from a start time of supplying the pressurized medium to the bladder than during other periods. A method for manufacturing a tire according to any one of claims 1 to 4.
6. 6. The tire manufacturing method according to claim 5, wherein in both the first shaping step and the second shaping step, the pressurized medium is supplied to the bladder at a higher pressure during a predetermined first period from a start of supply of the pressurized medium to the bladder than during other periods.
7. The bladder is placed in the center, A molding die arranged to surround the bladder; A mechanism for opening and closing the mold; A supply device for supplying a pressurized medium to the bladder; a discharge device for discharging the pressurized medium from the bladder; Control device and Equipped with The control device includes: In a shaping process in which a pressurized medium is supplied to the bladder and the bladder is inflated, the pressurized medium is supplied to the bladder at a pressure higher than that in other periods during a predetermined first period from a supply start time when the supply of the pressurized medium to the bladder is started. Tire vulcanizer.
8. 8. The tire vulcanizer according to claim 7, wherein the first period is set to be a period of 15% or less from a supply start time of starting supply of the pressurized medium to the bladder, when a total time for supplying the pressurized medium to the bladder in the shaping process is taken as 100%.
9. 8. The tire vulcanizer according to claim 7, wherein the control device is configured to supply the pressurized medium to the bladder at a predetermined constant supply pressure during the other period.
10. 8. The tire vulcanizer according to claim 7, wherein the supply pressure of the pressurized medium is set so that a maximum value of the supply pressure of the pressurized medium in the first period is at least twice as large as a maximum value of the supply pressure set in the other periods.
11. The shaping step includes: a first shaping step of increasing the pressure of the pressurized medium to a predetermined supply pressure from the start of supply of the pressurized medium and supplying the pressurized medium to the bladder at the predetermined supply pressure; After the first shaping step, depressurizing the bladder; a second shaping step of increasing the pressure from the start of supply of the pressurized medium to a predetermined supply pressure, supplying the pressurized medium to the bladder at the predetermined supply pressure, and causing the internal pressure of the bladder to reach the predetermined internal pressure after the depressurizing step; Including, The control device is configured to supply the pressurized medium to the bladder at a higher pressure during a predetermined first period from a supply start time of starting the supply of the pressurized medium to the bladder in at least one of the first shaping process and the second shaping process, than during other periods. A tire vulcanizer according to any one of claims 7 to 10.
12. The tire vulcanizer of claim 11, wherein the control device is configured so that, in both the first shaping process and the second shaping process, the pressurized medium is supplied to the bladder at a higher pressure during a predetermined first period from the start of supply of the pressurized medium to the bladder than during other periods.
Citation Information
Patent Citations
Tire manufacturing method
JP2020055203A