Semiconductor device

The semiconductor device stabilizes breakdown voltage by using a semi-insulating film with a specific silicon-to-nitrogen atomic ratio, enhancing electron flow and reducing crack formation, thus ensuring consistent performance.

JP2024164886APending Publication Date: 2024-11-28RENESAS ELECTRONICS CORP
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
JP2023080585
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-16
Publication Date
2024-11-28

AI Technical Summary

Technical Problem

The breakdown voltage in semiconductor devices fluctuates unpredictably due to variations in the semi-insulating film composition, leading to inconsistent performance.

Method used

A semiconductor device design incorporating a semi-insulating film made of silicon and nitrogen, with a specific atomic ratio of silicon to nitrogen atoms ranging from 0.64 to 0.74, which stabilizes the breakdown voltage by allowing easier electron flow and escape, reducing fluctuations.

Benefits of technology

The design effectively suppresses variations in breakdown voltage, enhances electron trapping and escape, and minimizes crack formation in the semi-insulating film, ensuring consistent device performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024164886000001_ABST
    Figure 2024164886000001_ABST
Patent Text Reader

Abstract

To provide a semiconductor device capable of suppressing variations in voltage-withstanding.SOLUTION: A semiconductor device comprises a semiconductor substrate, an insulating film, a first electrode and a second electrode, and a semi-insulating film. The semiconductor substrate has a first surface. The semiconductor substrate has an element region and a termination region surrounding the element region in plan view. The semiconductor substrate has a first impurity region formed on the first surface in the termination region. The insulating film covers the first surface in the termination region. The first electrode is electrically connected to the first impurity region and opposed to the first impurity region with the insulating film interposed therebetween. The second electrode is arranged on the insulating film so as to surround the first electrode while being spaced apart from the first electrode in plan view. The semi-insulating film is arranged so as to stretch over the insulating film between the first electrode and the second electrode in plan view. The semi-insulating film contains silicon and nitrogen.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a semiconductor device. [Background technology]

[0002] For example, Japanese Patent Application Laid-Open No. 2022-074323 (Patent Document 1) describes a semiconductor device. The semiconductor device described in Patent Document 1 has a semiconductor substrate, a first electrode, a second electrode, an insulating film, and a semi-insulating film. The semiconductor substrate has a first region and a second region surrounding the first region in a plan view. The semiconductor substrate has a first surface and a second surface opposite to the first surface in the thickness direction of the semiconductor substrate. The semiconductor substrate has an impurity region formed on the first surface in the first region. The insulating film covers the first surface in the second region. The first electrode faces the impurity region with the insulating film interposed therebetween. The second electrode is arranged on the insulating film so as to surround the first electrode while being spaced from the first electrode in a plan view. The semi-insulating film is arranged so as to straddle the insulating film between the first electrode and the second electrode. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Patent Publication No. 2022-074323 Summary of the Invention [Problem to be solved by the invention]

[0004] In the semiconductor device described in Patent Document 1, the breakdown voltage may vary every time a voltage is applied. Other problems and novel features will become apparent from the description of this specification and the accompanying drawings. [Means for solving the problem]

[0005] The semiconductor device of the present disclosure includes a semiconductor substrate, an insulating film, a first electrode, a second electrode, and a semi-insulating film. The semiconductor substrate has a first surface. The semiconductor substrate has, in a plan view, an element region and a termination region surrounding the element region. The semiconductor substrate has a first impurity region formed in the first surface in the termination region. The insulating film covers the first surface in the termination region. The first electrode is electrically connected to the first impurity region and faces the first impurity region with the insulating film interposed therebetween. The second electrode is disposed on the insulating film so as to surround the first electrode while being spaced apart from the first electrode in a plan view. The semi-insulating film is disposed so as to straddle the insulating film between the first electrode and the second electrode in a plan view. The semi-insulating film includes silicon and nitrogen. In the semi-insulating film, the ratio of the number of silicon atoms to the total number of silicon atoms and nitrogen atoms is 0.64 or more. Effect of the Invention

[0006] According to the semiconductor device of the present disclosure, fluctuations in the breakdown voltage can be suppressed. [Brief description of the drawings]

[0007] [Figure 1] FIG. 2 is a plan view of the semiconductor device DEV1. [Diagram 2] 2 is a cross-sectional view of the semiconductor device DEV1 taken along line II-II in FIG. [Diagram 3] 1 is a manufacturing process diagram of the semiconductor device DEV1. [Figure 4] FIG. 2 is a cross-sectional view illustrating a preparation step S1. [Diagram 5] FIG. 4 is a cross-sectional view illustrating an epitaxial growth step S2. [Figure 6] FIG. 11 is a cross-sectional view illustrating a first insulating film forming step S3. [Figure 7] FIG. 11 is a cross-sectional view illustrating an impurity region forming step S4. [Figure 8] FIG. 11 is a cross-sectional view illustrating a second insulating film forming step S5. [Figure 9] FIG. 11 is a cross-sectional view illustrating a first electrode forming step S6. [Figure 10] 11 is a cross-sectional view illustrating a semi-insulating film forming step S7. FIG. [Figure 11] FIG. 11 is a cross-sectional view illustrating a second electrode forming step S8. [Figure 12] 1 is a graph showing the relationship between the ratio of the number of silicon atoms to the total number of silicon atoms and nitrogen atoms in a semi-insulating film SIF and the number of silicon-hydrogen bonds. [Figure 13] 1 is a graph showing the relationship between the number of times the withstand voltage is measured and the withstand voltage. [Figure 14] 1 is a graph showing the relationship between the refractive index of a semi-insulating film SIF and the ratio of the number of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF. [Figure 15] 11 is a graph showing the relationship between the refractive index of the semi-insulating film SIF and the variation in thickness T1 of the semi-insulating film SIF. [Figure 16] FIG. 2 is a cross-sectional view of the semiconductor device DEV2. [Figure 17] 11A to 11C are manufacturing process diagrams of the semiconductor device DEV2. [Figure 18] FIG. 13 is a cross-sectional view of the semiconductor device DEV3. [Figure 19] 11 is a manufacturing process diagram of the semiconductor device DEV3. [Figure 20] 10 is a cross-sectional view illustrating a first impurity region forming step S10. FIG. [Figure 21] 11 is a cross-sectional view illustrating a first insulating film forming step S3 in the manufacturing method of the semiconductor device DEV3. FIG. [Figure 22] 11 is a cross-sectional view illustrating a second impurity region forming step S11. FIG. [Figure 23] FIG. 13 is a cross-sectional view of the semiconductor device DEV4. [Figure 24] 11 is a manufacturing process diagram of the semiconductor device DEV4. [Diagram 25] 11 is a cross-sectional view illustrating a first insulating film forming step S3 in the manufacturing method of the semiconductor device DEV4. FIG. [Figure 26] 11 is a cross-sectional view illustrating a third impurity region forming step S12. FIG. [Figure 27]FIG. 11 is a cross-sectional view illustrating a fourth impurity region forming step S13. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0008] The details of the embodiments of the present disclosure will be described with reference to the drawings. In the following drawings, the same or corresponding parts are designated by the same reference numerals, and redundant description will not be repeated.

[0009] (First embodiment) The semiconductor device DEV1 according to the first embodiment will be described.

[0010] <Configuration of semiconductor device DEV1> The configuration of the semiconductor device DEV1 will be described below.

[0011] Fig. 1 is a plan view of the semiconductor device DEV1. Fig. 2 is a cross-sectional view of the semiconductor device DEV1 taken along line II-II in Fig. 1. As shown in Figs. 1 and 2, the semiconductor device DEV1 has a semiconductor substrate SUB. The semiconductor substrate SUB has a first surface FS and a second surface SS on the opposite side to the first surface FS in the thickness direction of the semiconductor substrate SUB. The semiconductor substrate SUB is made of, for example, single crystal silicon (Si).

[0012] The semiconductor substrate SUB has an element region SUB1 and a termination region SUB2. The termination region SUB2 surrounds the element region SUB1 in plan view.

[0013] The semiconductor substrate SUB has an impurity region R1, an impurity region R2, an impurity region R3, an impurity region R4, and an impurity region R5. The conductivity type of the impurity region R1 and the conductivity type of the impurity region R2 are a first conductivity type. The first conductivity type is, for example, an n-type. The conductivity type of the impurity region R3 and the conductivity type of the impurity region R4 are a second conductivity type. The second conductivity type is, for example, a p-type. The conductivity type of the impurity region R5 is the first conductivity type or the second conductivity type.

[0014] The impurity region R1 is formed in the second surface SS. The impurity region R2 is formed in the first surface FS. The impurity region R2 is in contact with the impurity region R1 on the side opposite to the first surface FS. The impurity region R1 and the impurity region R2 form, for example, a cathode of a fast recovery diode (FRD).

[0015] The impurity region R3 is formed in the first face FS in the element region SUB1. The impurity region R4 is formed in the first face in the termination region SUB2. The impurity region R3 is pn-junctioned with the impurity region R2. The impurity region R3 forms, for example, an anode of the FRD. In this manner, the semiconductor device DEV1 has the FRD formed in the element region SUB1.

[0016] The impurity region R4 is formed in the first face FS in the termination region SUB2. The impurity region R4 straddles the boundary between the element region SUB1 and the termination region SUB2 in a planar view. The impurity region R4 surrounds the impurity region R3 in a planar view. The impurity region R4 is in contact with the impurity region R3. That is, the impurity region R4 is electrically connected to the impurity region R3. The impurity region R4 forms a pn junction with the impurity region R2. The impurity concentration in the impurity region R4 is lower than the impurity concentration in the impurity region R3. That is, the impurity region R4 has a RESURF (REduced SUrface Field) structure. The impurity region R5 is formed in the first face FS in the termination region SUB2. The impurity region R5 surrounds the impurity region R4 in a planar view. The impurity region R5 is spaced apart from the impurity region R4.

[0017] The semiconductor device DEV1 further has an insulating film ISL. The insulating film ISL is disposed on the first face FS. The insulating film ISL covers at least the first face FS in the termination region SUB2. The insulating film ISL partially covers the first face FS in the element region SUB1. An opening OP1 and an opening OP2 are formed in the insulating film ISL. The opening OP1 is formed on the impurity region R3. The opening OP2 is formed on the impurity region R5.

[0018] The insulating film ISL has a first insulating film ISL1 and a second insulating film ISL2. The first insulating film ISL1 and the second insulating film ISL2 are made of a material such as silicon oxide (SiO 2 ). The first insulating film ISL1 covers the first surface FS between the impurity region R3 and the impurity region R5. The second insulating film ISL2 covers the first insulating film ISL1. Therefore, a step is formed on the upper surface of the insulating film ISL.

[0019] The semiconductor device DEV1 further includes a first electrode EL1 and a second electrode EL2. The first electrode EL1 and the second electrode EL2 are made of, for example, aluminum (Al) or an aluminum alloy.

[0020] The first electrode EL1 has an outer peripheral portion EL1a. The outer peripheral portion EL1a faces the impurity region R4 with the insulating film ISL therebetween. The outer peripheral portion EL1a functions as a field plate. The first electrode EL1 is connected to the impurity region R3 through the opening OP1. As described above, the impurity region R3 is in contact with the impurity region R4, and therefore the first electrode EL1 is electrically connected to the impurity region R4. The second electrode EL2 is disposed on the insulating film ISL. The second electrode EL2 surrounds the first electrode EL1 in a plan view. The second electrode EL2 is spaced apart from the first electrode EL1. The second electrode EL2 is connected to the impurity region R5 through the opening OP2. The second electrode EL2 is set to, for example, a ground potential.

[0021] The semiconductor device DEV1 further includes a semi-insulating film SIF. The semi-insulating film SIF is made of a material containing silicon and nitrogen (N). The semi-insulating film SIF is made of a material such as silicon nitride (Si 3 N 4 From another point of view, a part of the silicon contained in the semi-insulating film SIF is bonded to hydrogen.

[0022] In the semi-insulating film SIF, the ratio of the number of silicon atoms to the total number of silicon atoms and nitrogen atoms (i.e., the value obtained by dividing the number of silicon atoms by the total number of silicon atoms and nitrogen atoms) is 0.64 or more. In the semi-insulating film SIF, the ratio of the number of silicon atoms to the total number of silicon atoms and nitrogen atoms may be 0.74 or less. The ratio of the number of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF is measured by XPS (X-ray Photoelectron Spectroscopy).

[0023] The semi-insulating film SIF has a refractive index of, for example, 2.55 or more. The semi-insulating film SIF has a refractive index of, for example, 2.90 or less. The refractive index of the semi-insulating film SIF is measured by optical measurement using a spectroscopic ellipsometer.

[0024] The semi-insulating film SIF is disposed so as to straddle the insulating film ISL between the first electrode EL1 and the second electrode EL2. The semi-insulating film SIF has an inner peripheral edge portion SIFa. The inner peripheral edge portion SIFa is disposed on the outer peripheral edge portion EL1a. The semi-insulating film SIF covers the second electrode EL2.

[0025] The thickness T1 of the semi-insulating film SIF is, for example, 50 nm or more and 1000 nm or less. The variation of the thickness T1 is, for example, 0.02 or less. The variation of the thickness T1 is defined as the larger of the value obtained by subtracting the average value of the thickness T1 from the maximum value of the thickness T1 and dividing the value obtained by subtracting the minimum value of the thickness T1 from the average value of the thickness T1 and dividing the value obtained by subtracting the minimum value of the thickness T1 from the average value of the thickness T1. The thickness T2 of the insulating film ISL is, for example, 0.5 μm or more and 3.0 μm or less. The thickness T2 is measured in a portion between the first surface FS and the semi-insulating film SIF. The thickness T3 of the first electrode EL1 and the second electrode EL2 is, for example, 2.0 μm or more and 6.0 μm or more from the viewpoint of securing a margin during wire bonding.

[0026] The semiconductor device DEV1 further includes a third electrode EL3. The third electrode EL3 is made of, for example, aluminum or an aluminum alloy. The third electrode EL3 is disposed on the second surface SS.

[0027] The semiconductor device DEV1 further includes a passivation film PV, which is formed of, for example, polyimide, and is disposed on the semi-insulating film SIF.

[0028] <Manufacturing Method of Semiconductor Device DEV1> A method for manufacturing the semiconductor device DEV1 will be described below.

[0029] Fig. 3 is a manufacturing process diagram of the semiconductor device DEV1. As shown in Fig. 3, the manufacturing method of the semiconductor device DEV1 includes a preparation step S1, an epitaxial growth step S2, a first insulating film forming step S3, an impurity region forming step S4, a second insulating film forming step S5, a first electrode forming step S6, a semi-insulating film forming step S7, a second electrode forming step S8, and a passivation film forming step S9.

[0030] FIG. 4 is a cross-sectional view illustrating the preparation step S1. As shown in FIG. 4, in the preparation step S1, a semiconductor substrate SUB is prepared. At this stage, the semiconductor substrate SUB has only an impurity region R1. FIG. 5 is a cross-sectional view illustrating the epitaxial growth step S2. As shown in FIG. 5, in the epitaxial growth step S2, an impurity region R2 is epitaxially grown on the impurity region R1. The impurity region R2 is formed, for example, by a CVD (Chemical Vapor Deposition) method.

[0031] Fig. 6 is a cross-sectional view illustrating the first insulating film forming step S3. As shown in Fig. 6, in the first insulating film forming step S3, the first insulating film ISL1 is formed. In the first insulating film forming step S3, first, a constituent material of the first insulating film ISL1 is formed on the first surface FS by a thermal oxidation method or a CVD method. Second, the formed constituent material of the first insulating film ISL1 is etched using a resist pattern formed by a photolithography method.

[0032] FIG. 7 is a cross-sectional view illustrating the impurity region forming step S4. As shown in FIG. 7, in the impurity region forming step S4, impurity region R3, impurity region R4, and impurity region R5 are formed. In the impurity region forming step S4, first, a resist pattern is formed on the first face FS and the first insulating film ISL1 by a photolithography method. Second, ion implantation is performed from the first face FS side using the resist pattern as a mask. Third, the resist pattern is removed. Fourth, the semiconductor substrate SUB is annealed to thermally diffuse the implanted impurity ions. As a result, the impurity region R4 is formed. In a similar process, the impurity region R3 and the impurity region R5 are also formed.

[0033] Fig. 8 is a cross-sectional view illustrating the second insulating film forming step S5. As shown in Fig. 8, in the second insulating film forming step S5, the second insulating film ISL2 is formed. In the second insulating film forming step S5, first, a constituent material of the second insulating film ISL2 is deposited so as to cover the first insulating film ISL1 by, for example, a CVD method. Second, the deposited constituent material of the second insulating film ISL2 is etched using a resist pattern formed by a photolithography method.

[0034] Fig. 9 is a cross-sectional view illustrating the first electrode forming step S6. As shown in Fig. 9, in the first electrode forming step S6, a first electrode EL1 and a second electrode EL2 are formed. In the first electrode forming step S6, first, a material for the first electrode EL1 (second electrode EL2) is deposited on the first surface FS and the insulating film ISL by, for example, a sputtering method. Second, the deposited material for the first electrode EL1 (second electrode EL2) is etched using a resist pattern formed by a photolithography method.

[0035] FIG. 10 is a cross-sectional view illustrating the semi-insulating film forming step S7. As shown in FIG. 10, in the semi-insulating film forming step S7, a semi-insulating film SIF is formed. In the semi-insulating film forming step S7, first, a constituent material of the semi-insulating film SIF is formed by, for example, a CVD method so as to cover the first electrode EL1, the second electrode EL2, and the insulating film ISL. Second, the constituent material of the formed semi-insulating film SIF is patterned by etching using a resist pattern formed by a photolithography method. Note that the ratio of the number of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF is determined by the amount of monosilane (SiH 4 ) and nitrogen gas (N 2 The larger the value obtained by dividing the flow rate of monosilane by the flow rate of nitrogen gas, the larger the ratio of the number of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF becomes.

[0036] Fig. 11 is a cross-sectional view for explaining the second electrode forming step S8. As shown in Fig. 11, in the second electrode forming step S8, the constituent material of the third electrode EL3 is deposited on the second surface SS by, for example, a sputtering method, thereby forming the third electrode EL3. In the passivation film forming step S9, the passivation film PV is formed. In the passivation film forming step S9, first, the constituent material of the passivation film PV is deposited so as to cover the semi-insulating film SIF and the first electrode EL1. Second, the constituent material of the deposited passivation film PV is patterned by a photolithography method. In the above manner, the structure of the semiconductor device DEV1 shown in Figs. 1 and 2 is formed.

[0037] In the above example of the manufacturing method, the semiconductor substrate SUB having only the impurity region R1 is prepared in the preparation step S1, but the semiconductor substrate SUB having only the impurity region R2 may be prepared in the preparation step S1. In this case, the epitaxial growth step S2 is not performed, and the impurity region R1 is formed by ion implantation from the second surface SS side. The formation of the impurity region R1 by this ion implantation is performed before the second electrode formation step S8.

[0038] <Modification> In the above, an example has been shown in which an FRD is formed in the element region SUB1, but a semiconductor element other than an FRD may be formed in the element region SUB1. For example, an IGBT (Insulated Gate Bipolar Transistor) may be formed in the element region SUB1.

[0039] <Effects of semiconductor device DEV1> The effects of the semiconductor device DEV1 will be described below in comparison with a semiconductor device according to a comparative example. The configuration of the semiconductor device according to the comparative example is the same as that of the semiconductor device DEV1, except that the ratio of the number of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF is less than 0.64.

[0040] In the semiconductor device DEV1 and the semiconductor device according to the comparative example, since the semi-insulating film SIF is semi-insulating, a weak leakage current flows through the semi-insulating film SIF, which relaxes the electric field in the semiconductor substrate SUB facing the semi-insulating film SIF via the insulating film ISL, thereby improving the breakdown voltage. At this time, electrons are induced and trapped in the semi-insulating film SIF.

[0041] Fig. 12 is a graph showing the relationship between the ratio of the number of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF and the number of silicon-hydrogen bonds. The graph in Fig. 12 was obtained by performing FT-IR (Fourier Transformation InfraRed spectroscopy) analysis on samples 1 to 6 of the semi-insulating film SIF. The ratio of the number of silicon atoms to the total number of silicon atoms and nitrogen atoms in each sample is greatest in the order of sample 1, sample 2, sample 3, sample 4, sample 5, and sample 6. The ratio of the number of silicon atoms to the total number of silicon atoms and nitrogen atoms in samples 1 to 3 is less than 0.64, and the ratio of the number of silicon atoms to the total number of silicon atoms and nitrogen atoms in samples 4 to 6 is 0.64 or more.

[0042] 12, no silicon-hydrogen bonds are detected in Samples 1 to 3. On the other hand, peaks derived from silicon-hydrogen bonds are detected in Samples 4 to 6. That is, while amorphous silicon is contained in the semi-insulating film SIF in the semiconductor device DEV1, amorphous silicon is not contained in the semi-insulating film SIF in the semiconductor device according to the comparative example.

[0043] In the semiconductor device according to the comparative example, the semi-insulating film SIF does not contain amorphous silicon through which a current easily flows, so that electrons induced and trapped in the semi-insulating film SIF are unlikely to escape from the semi-insulating film SIF. The electrons induced and trapped in the semi-insulating film SIF are a factor in fluctuations in the breakdown voltage. On the other hand, in the semiconductor device DEV1, the semi-insulating film SIF contains amorphous silicon through which a current easily flows, so that the induced and trapped electrons flow to the second electrode EL2 and are likely to escape from the semi-insulating film SIF. Therefore, the semiconductor device DEV1 can suppress fluctuations in the breakdown voltage.

[0044] FIG. 13 is a graph showing the relationship between the number of measurements of the withstand voltage and the withstand voltage. In FIG. 13, sample 2 in FIG. 12 is applied as the semi-insulating film SIF of the semiconductor device according to the comparative example, and sample 4 or sample 6 is applied as the semi-insulating film SIF of the semiconductor device DEV1. The vertical axis of the graph in FIG. 13 shows the difference between the withstand voltage in the nth measurement (n is an integer between 1 and 10) and the withstand voltage in the first measurement. The value on the vertical axis in the first measurement is (withstand voltage in the first measurement)-(withstand voltage in the first measurement), and is therefore 0. As shown in FIG. 13, in the semiconductor device according to the comparative example in which the ratio of the number of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF is less than 0.64, the withstand voltage fluctuates greatly as the number of measurements increases. On the other hand, in the semiconductor device DEV1 in which the ratio of the number of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF is 0.64 or more, the fluctuation in the withstand voltage is small even if the number of measurements increases.

[0045] 14 is a graph showing the relationship between the refractive index of the semi-insulating film SIF and the ratio of the number of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF. As shown in FIG. 14, as the refractive index of the semi-insulating film SIF increases, the ratio of the number of silicon atoms to the refractive index of the semi-insulating film SIF and the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF increases. More specifically, if the ratio of the number of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF is set to 0.64 or more, the refractive index of the semi-insulating film SIF is 2.55 or more. Also, if the ratio of the number of silicon atoms to the refractive index of the semi-insulating film SIF and the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF is set to 0.74 or less, the refractive index of the semi-insulating film SIF is 2.90 or less. In this way, by setting the refractive index of the semi-insulating film SIF to 2.55 or more, the semiconductor device DEV1 can suppress fluctuations in the breakdown voltage.

[0046] Fig. 15 is a graph showing the relationship between the refractive index of the semi-insulating film SIF and the variation in the thickness T1 of the semi-insulating film SIF. As shown in Fig. 15, when the refractive index of the semi-insulating film SIF exceeds 2.90, that is, when the ratio of the number of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF exceeds 0.74, the variation in the thickness T1 becomes large. On the other hand, when the ratio of the number of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF is in the range of 0.64 to 0.74, the variation in the thickness T1 is 0.02 or less. From this, by setting the ratio of the number of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF to 0.64 to 0.74, it is possible to suppress the variation in the thickness T1 while suppressing the fluctuation in the breakdown voltage.

[0047] As thickness T1 increases, current flows more easily through the semi-insulating film SIF, and induced and trapped electrons are more likely to escape. On the other hand, if thickness T1 is too large, the semi-insulating film SIF is hard and prone to cracks. Therefore, by setting thickness T1 to 50 nm or more and 1000 nm or less, it is possible to suppress the occurrence of cracks in the semi-insulating film SIF while suppressing the breakdown voltage fluctuation.

[0048] As the thickness T2 increases, the capacitance formed by the semi-insulating film SIF, the insulating film ISL, and the semiconductor substrate SUB decreases, and fluctuations in the breakdown voltage are suppressed. On the other hand, if the thickness T2 is too large, the embeddability of the first electrode EL1 and the second electrode EL2 deteriorates. Also, if the thickness T2 is too large, a step formed on the upper surface of the insulating film ISL becomes large, and the step makes it easy for cracks to occur in the semi-insulating film SIF. Therefore, by setting the thickness T2 to 0.5 μm or more and 3.0 μm or less, it is possible to suppress the occurrence of cracks in the semi-insulating film SIF and the deterioration of the embeddability of the first electrode EL1 and the second electrode EL2 while suppressing fluctuations in the breakdown voltage.

[0049] Second embodiment A semiconductor device DEV2 according to the second embodiment will be described below. Here, differences from the semiconductor device DEV1 will be mainly described, and overlapping descriptions will not be repeated.

[0050] <Configuration of semiconductor device DEV2> The configuration of the semiconductor device DEV2 will be described below.

[0051] Fig. 16 is a cross-sectional view of the semiconductor device DEV2. Fig. 16 shows a cross section at a position corresponding to II-II in Fig. 1. As shown in Fig. 16, the semiconductor device DEV2 has a semiconductor substrate SUB, an insulating film ISL, a first electrode EL1 and a second electrode EL2, a semi-insulating film SIF, and a passivation film PV. In the semiconductor device DEV2, the ratio of the number of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF is 0.64 or more. In these respects, the configuration of the semiconductor device DEV2 is common to the configuration of the semiconductor device DEV1.

[0052] In the semiconductor device DEV2, the semi-insulating film SIF is disposed on the insulating film ISL. More specifically, in the semiconductor device DEV2, the semi-insulating film SIF is disposed inside a step formed on the upper surface of the insulating film ISL. In the semiconductor device DEV2, the semi-insulating film SIF has an inner peripheral edge portion SIFa and an outer peripheral edge portion SIFb. The inner peripheral edge portion SIFa and the outer peripheral edge portion SIFb are covered by a first electrode EL1 and a second electrode EL2, respectively. In these respects, the configuration of the semiconductor device DEV2 differs from the configuration of the semiconductor device DEV1.

[0053] <Modification> In the above, an example has been described in which the ratio of the number of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF is 0.64 or more, but in the semiconductor device DEV2, the ratio of the number of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF may be less than 0.64. Also, in the semiconductor device DEV2, the semi-insulating film SIF may be formed of a material other than silicon and nitrogen containing material (for example, polycrystalline silicon).

[0054] <Manufacturing Method of Semiconductor Device DEV2> A method for manufacturing the semiconductor device DEV2 will be described below.

[0055] Fig. 17 is a manufacturing process diagram of the semiconductor device DEV2. As shown in Fig. 17, the manufacturing method of the semiconductor device DEV2 includes a preparation step S1, an epitaxial growth step S2, a first insulating film forming step S3, an impurity region forming step S4, a second insulating film forming step S5, a first electrode forming step S6, a semi-insulating film forming step S7, a second electrode forming step S8, and a passivation film forming step S9. In this respect, the manufacturing method of the semiconductor device DEV2 is common to the manufacturing method of the semiconductor device DEV1.

[0056] In the manufacturing method of the semiconductor device DEV2, the semi-insulating film forming step S7 is performed after the second insulating film forming step S5. In the manufacturing method of the semiconductor device DEV2, the first electrode forming step S6 is performed after the semi-insulating film forming step S7. In this respect, the manufacturing method of the semiconductor device DEV2 differs from the manufacturing method of the semiconductor device DEV1.

[0057] <Effects of semiconductor device DEV2> The effects of the semiconductor device DEV2 will be described below.

[0058] A step is formed on the upper surface of the insulating film ISL. As a result, in the semiconductor device DEV1, a step is also formed on the upper surface of the first electrode EL1 and the upper surface of the second electrode EL2, and the semi-insulating film SIF may be disposed on the step. Since stress concentration is likely to occur near such a step, cracks are likely to occur in the semi-insulating film SIF in the semiconductor device DEV1. As the composition ratio of silicon in the semi-insulating film SIF becomes higher, its properties become closer to silicon and it becomes more brittle, so that when the ratio of the number of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF is 0.64 or more, there is a concern that such cracks will occur.

[0059] On the other hand, in the semiconductor device DEV2, the inner peripheral portion SIFa and the outer peripheral portion SIFb are covered by the first electrode EL1 and the second electrode EL2, respectively. That is, in the semiconductor device DEV2, the semi-insulating film SIF does not have a portion disposed on the first electrode EL1 and the second electrode EL2. Therefore, in the semiconductor device DEV2, the semi-insulating film SIF is not affected by the steps formed on the upper surfaces of the first electrode EL1 and the second electrode EL2, and cracks are unlikely to occur in the semi-insulating film SIF.

[0060] Third embodiment A semiconductor device DEV3 according to the third embodiment will be described below. Here, differences from the semiconductor device DEV1 will be mainly described, and overlapping descriptions will not be repeated.

[0061] <Configuration of semiconductor device DEV3> The configuration of the semiconductor device DEV3 will be described below.

[0062] Fig. 18 is a cross-sectional view of the semiconductor device DEV3. Fig. 18 shows a cross section at a position corresponding to II-II in Fig. 1. As shown in Fig. 18, the semiconductor device DEV3 has a semiconductor substrate SUB, an insulating film ISL, a first electrode EL1 and a second electrode EL2, a semi-insulating film SIF, and a passivation film PV. In the semiconductor device DEV3, the ratio of the number of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF is 0.64 or more. In these respects, the configuration of the semiconductor device DEV3 is common to the configuration of the semiconductor device DEV1.

[0063] In the semiconductor device DEV3, a recess RCS1 is formed in the first surface FS. The first surface FS is recessed toward the second surface SS at the recess RCS1. The recess RCS1 is arranged so as to overlap with the impurity region R4 in a plan view. The recess RCS1 may extend to the vicinity of the impurity region R5. In the semiconductor device DEV3, the first insulating film ISL1 is embedded in the recess RCS1, and the second insulating film ISL2 is arranged on the first surface FS in the termination region SUB2 so as to cover the first insulating film ISL1. In the semiconductor device DEV3, the first insulating film ISL1 is, for example, thicker than the second insulating film ISL2. In these respects, the configuration of the semiconductor device DEV3 is different from the configuration of the semiconductor device DEV1.

[0064] <Modification> In the above, an example has been described in which the ratio of the number of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF is 0.64 or more, but in the semiconductor device DEV3, the ratio of the number of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF may be less than 0.64. Also, in the semiconductor device DEV3, the semi-insulating film SIF may be formed of a material other than silicon and nitrogen-containing material (for example, polycrystalline silicon).

[0065] <Manufacturing Method of Semiconductor Device DEV3> A method for manufacturing the semiconductor device DEV3 will be described below.

[0066] Fig. 19 is a manufacturing process diagram of the semiconductor device DEV3. As shown in Fig. 19, the manufacturing method of the semiconductor device DEV3 includes a preparation step S1, an epitaxial growth step S2, a first insulating film forming step S3, a second insulating film forming step S5, a first electrode forming step S6, a semi-insulating film forming step S7, a second electrode forming step S8, and a passivation film forming step S9. In this respect, the manufacturing method of the semiconductor device DEV3 is common to the manufacturing method of the semiconductor device DEV1.

[0067] The method for manufacturing the semiconductor device DEV3 includes a first impurity region forming step S10 and a second impurity region forming step S11 instead of the impurity region forming step S4.

[0068] The first impurity region forming step S10 is performed after the epitaxial growth step S2. FIG. 20 is a cross-sectional view illustrating the first impurity region forming step S10. As shown in FIG. 20, in the first impurity region forming step S10, an impurity region R4 is formed. In the first impurity region forming step S10, first, a resist pattern is formed on the first face FS by a photolithography method. Second, ion implantation is performed from the first face FS side using the resist pattern as a mask. Third, the semiconductor substrate SUB is annealed, thereby thermally diffusing the implanted impurity ions.

[0069] In the manufacturing method of the semiconductor device DEV3, the first insulating film forming step S3 is performed after the first impurity region forming step S10. FIG. 21 is a cross-sectional view for explaining the first insulating film forming step S3 in the manufacturing method of the semiconductor device DEV3. As shown in FIG. 21, in the manufacturing method of the semiconductor device DEV3, in the first insulating film forming step S3, the recess RCS1 and the first insulating film ISL1 are formed. In the first insulating film forming step S3 in the manufacturing method of the semiconductor device DEV2, first, a resist pattern is formed on the first surface FS by a photolithography method. Second, the first surface FS is etched using the resist pattern as a mask to form the recess RCS1. Third, polycrystalline silicon is partially embedded in the recess RCS1 by, for example, a CVD method. Fourth, the embedded polycrystalline silicon is thermally oxidized to become the first insulating film ISL1. When the first insulating film ISL1 protrudes from the recess RCS1, the protruding first insulating film ISL1 may be removed by a CMP (Chemical Mechanical Polishing) method. In the above example, the first insulating film ISL1 is formed by partially filling the recess RCS1 with polycrystalline silicon and then performing thermal oxidation, but the first insulating film ISL1 may be formed only by thermal oxidation.

[0070] In the manufacturing method of the semiconductor device DEV3, the second impurity region forming step S11 is performed after the first insulating film forming step S3. Fig. 22 is a cross-sectional view explaining the second impurity region forming step S11. As shown in Fig. 22, in the second impurity region forming step S11, impurity regions R3 and R5 are formed. In the second impurity region forming step S11, first, ion implantation is performed from the first surface FS side using the first insulating film ISL1 as a mask. Second, the semiconductor substrate SUB is annealed to thermally diffuse the implanted impurity ions.

[0071] In the manufacturing method of the semiconductor device DEV3, after the second impurity region forming step S11, the second insulating film forming step S5, the first electrode forming step S6, the semi-insulating film forming step S7, the second electrode forming step S8, and the passivation film forming step S9 are performed in this order.

[0072] <Effects of semiconductor device DEV3> The effects of the semiconductor device DEV3 will be described below.

[0073] In the semiconductor device DEV3, the first insulating film ISL1 is embedded in the recess RCS1, and the second insulating film ISL2 is disposed so as to cover the first insulating film ISL1, so that steps are unlikely to be formed on the upper surface of the insulating film ISL, and further on the upper surfaces of the first electrode EL1 and the second electrode EL2. Therefore, according to the semiconductor device DEV3, even if the semi-insulating film SIF is disposed on the first electrode EL1 and the second electrode EL2, cracks due to stress concentration are unlikely to occur in the semi-insulating film SIF.

[0074] In the semiconductor device DEV3, the impurity region R4 is formed before the first insulating film ISL1 is formed, so that the ion implantation for forming the impurity region R4 is performed without passing through the first insulating film ISL1. Therefore, in the semiconductor device DEV3, it is possible to lower the acceleration voltage when performing the ion implantation for forming the impurity region R4. Also, in the semiconductor device DEV3, the first insulating film ISL1 can be used as a mask when performing the ion implantation for forming the impurity regions R3 and R5, so that it is not necessary to separately form a resist pattern for the ion implantation for forming the impurity regions R3 and R5, and it is possible to simplify the process.

[0075] (Fourth embodiment) A semiconductor device DEV4 according to the fourth embodiment will be described below. Here, differences from the semiconductor device DEV3 will be mainly described, and overlapping descriptions will not be repeated.

[0076] <Configuration of semiconductor device DEV4> The configuration of the semiconductor device DEV4 will be described below.

[0077] Fig. 23 is a cross-sectional view of the semiconductor device DEV4. Fig. 23 shows a cross section at a position corresponding to II-II in Fig. 1. As shown in Fig. 23, the semiconductor device DEV4 has a semiconductor substrate SUB, an insulating film ISL, a first electrode EL1 and a second electrode EL2, a semi-insulating film SIF, and a passivation film PV. In the semiconductor device DEV4, the ratio of the number of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF is 0.64 or more. In these respects, the configuration of the semiconductor device DEV4 is common to the configuration of the semiconductor device DEV3.

[0078] In the semiconductor device DEV4, a plurality of recesses RCS2 and a recess RCS3 are formed on the first surface FS. The first surface FS is recessed toward the second surface SS at the recesses RCS2 and RCS3. The recesses RCS2 are arranged so as to overlap with the impurity region R4 in a plan view. The recesses RCS2 are arranged at intervals along a direction from the element region SUB1 toward the termination region SUB2. The recess RCS3 is arranged between the outermost recess RCS2 in the direction from the element region SUB1 toward the termination region SUB2 and the impurity region R5. The recess RCS3 may extend to a position adjacent to the impurity region R5.

[0079] In the semiconductor device DEV4, the first insulating film ISL1 is embedded in each of the recesses RCS2 and the recess RCS3, and the second insulating film ISL2 is disposed on the first surface FS in the termination region SUB2 so as to cover the first insulating film ISL1. In these respects, the configuration of the semiconductor device DEV4 differs from the configuration of the semiconductor device DEV3.

[0080] <Modification> In the above, an example has been described in which the ratio of the number of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF is 0.64 or more, but in the semiconductor device DEV4, the ratio of the number of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film SIF may be less than 0.64. Also, in the semiconductor device DEV4, the semi-insulating film SIF may be formed of a material other than silicon and nitrogen-containing material (for example, polycrystalline silicon).

[0081] Fig. 24 is a manufacturing process diagram of the semiconductor device DEV4. As shown in Fig. 24, the manufacturing method of the semiconductor device DEV4 includes a preparation step S1, an epitaxial growth step S2, a first insulating film forming step S3, a second insulating film forming step S5, a first electrode forming step S6, a semi-insulating film forming step S7, a second electrode forming step S8, and a passivation film forming step S9. In this respect, the manufacturing method of the semiconductor device DEV4 is common to the manufacturing method of the semiconductor device DEV3.

[0082] In the method for manufacturing the semiconductor device DEV4, a first insulating film forming step S3 is performed after the epitaxial growth step S2. Fig. 25 is a cross-sectional view illustrating the first insulating film forming step S3 in the method for manufacturing the semiconductor device DEV4. As shown in Fig. 25, in the method for manufacturing the semiconductor device DEV4, a plurality of recesses RCS2, recesses RCS3, and first insulating films ISL1 are formed in the first insulating film forming step S3.

[0083] In the first insulating film forming step S3 in the manufacturing method of the semiconductor device DEV4, first, a resist pattern is formed on the first surface FS by photolithography. Second, the first surface FS is etched using the resist pattern as a mask to form a plurality of recesses RCS2 and RCS3. Third, polycrystalline silicon is partially filled into the plurality of recesses RCS2 and RCS3 by, for example, CVD. Fourth, the filled polycrystalline silicon is thermally oxidized to become the first insulating film ISL1. Note that, when the first insulating film ISL1 protrudes from the recess RCS1, the protruding first insulating film ISL1 may be removed by CMP.

[0084] The manufacturing method of the semiconductor device DEV4 includes a third impurity region forming step S12 instead of the first impurity region forming step S10. The third impurity region forming step S12 is performed after the first insulating film forming step S3. FIG. 26 is a cross-sectional view illustrating the third impurity region forming step S12. As shown in FIG. 26, in the third impurity region forming step S12, an impurity region R4 is formed. In the third impurity region forming step S12, first, ion implantation is performed from the first surface FS side using the first insulating film ISL1 as a mask. As a result, impurity ions are implanted between two adjacent recesses RCS2. Third, the semiconductor substrate SUB is annealed, thereby thermally diffusing the implanted impurity ions.

[0085] The manufacturing method of the semiconductor device DEV4 has a fourth impurity region forming step S13 instead of the second impurity region forming step S11. The fourth impurity region forming step S13 is performed after the third impurity region forming step S12. FIG. 27 is a cross-sectional view for explaining the fourth impurity region forming step S13. As shown in FIG. 27, in the fourth impurity region forming step S13, an impurity region R3 and an impurity region R5 are formed. In the fourth impurity region forming step S13, first, a resist pattern is formed on the first face FS by a photolithography method. Second, ion implantation is performed from the first face FS side using the resist pattern as a mask. Third, the semiconductor substrate SUB is annealed, thereby thermally diffusing the implanted impurity ions.

[0086] In the manufacturing method of the semiconductor device DEV4, after the fourth impurity region forming step S13, a second insulating film forming step S5, a first electrode forming step S6, a semi-insulating film forming step S7, a second electrode forming step S8, and a passivation film forming step S9 are performed in this order.

[0087] In the semiconductor device DEV4, the first insulating film ISL1 is embedded in the recesses RCS2 and RCS3, and the second insulating film ISL2 is disposed so as to cover the first insulating film ISL1, so that steps are unlikely to be formed on the upper surface of the insulating film ISL, and further on the upper surfaces of the first electrode EL1 and the second electrode EL2. Therefore, according to the semiconductor device DEV4, even if the semi-insulating film SIF is disposed on the first electrode EL1 and the second electrode EL2, cracks due to stress concentration are unlikely to occur in the semi-insulating film SIF.

[0088] In the semiconductor device DEV3, ion implantation for forming the impurity region R4 is performed between two adjacent recesses RCS2 without the first insulating film ISL1. Therefore, in the semiconductor device DEV3, it is possible to lower the acceleration voltage when performing ion implantation for forming the impurity region R4. In the semiconductor device DEV4, the first insulating film ISL1 can be used as a mask for ion implantation for forming the impurity region R4, so there is no need to separately form a resist pattern for ion implantation for forming the impurity region R4, and the process can be simplified.

[0089] The invention made by the inventor has been specifically described above based on an embodiment, but it goes without saying that the present invention is not limited to the above embodiment and can be modified in various ways without departing from the gist of the invention. [Explanation of symbols]

[0090] DEV1,DEV2,DEV3,DEV4 Semiconductor device, EL1 1st electrode, EL1a outer edge, EL2 2nd electrode, EL3 3rd electrode, FS 1st surface, ISL insulation film, ISL1 1st insulation film, ISL2 2nd insulation film, OP1, OP2 opening, PV passivation film, R1,R2,R3,R4,R5 Impurity region, RCS1, RCS2, RCS3 recess, S1 preparation process, S2 epitaxial growth process, S3 first insulating film formation process, S4 impurity region formation process, S5 second insulating film formation process, S6 first electrode formation process, S7 formation process, S8 second electrode formation process, S9 passivation film formation process, S10 first impurity region formation process, S11 Second impurity region formation step, S12 Third impurity region formation step, S13 Fourth impurity region formation step, SIF semi-insulating film, SIFa Inner edge, SIFb outer edge, SS second surface, SUB semiconductor substrate, SUB1 element region, SUB2 termination region, T1, T2, T3 thicknesses.

Claims

1. A semiconductor substrate; An insulating film; A first electrode and a second electrode; A semi-insulating film; the semiconductor substrate has a first surface; the semiconductor substrate has, in a plan view, an element region and a termination region surrounding the element region; the semiconductor substrate has a first impurity region formed in the first surface in the termination region; the insulating film covers the first surface in the termination region; the first electrode is electrically connected to the first impurity region and faces the first impurity region with the insulating film interposed therebetween; the second electrode is disposed on the insulating film so as to surround the first electrode while being spaced apart from the first electrode in a plan view; the semi-insulating film is disposed so as to straddle the insulating film between the first electrode and the second electrode in a plan view, the semi-insulating film contains silicon and nitrogen; a ratio of the number of silicon atoms to the total number of silicon atoms and nitrogen atoms in the semi-insulating film is 0.64 or more.

2. 2. The semiconductor device according to claim 1, wherein in said semi-insulating film, a ratio of the number of silicon atoms to a total number of silicon atoms and nitrogen atoms is 0.74 or less.

3. 2. The semiconductor device according to claim 1, wherein a part of silicon in said semi-insulating film is bonded to hydrogen.

4. 2. The semiconductor device according to claim 1, wherein said semi-insulating film is a mixed crystal of silicon nitride and amorphous silicon.

5. 2. The semiconductor device according to claim 1, wherein the semi-insulating film has a thickness of 50 nm or more and 1000 nm or less.

6. 2. The semiconductor device according to claim 1, wherein the insulating film has a thickness of 0.5 [mu]m or more and 3.0 [mu]m or less.

7. The semiconductor device according to claim 1 , wherein the first electrode and the second electrode are electrically connected to each other by the semi-insulating film.

8. the semiconductor substrate has a second impurity region formed in the first surface in the element region; the first electrode is connected to the second impurity region; 2. The semiconductor device according to claim 1, wherein an impurity concentration in said second impurity region is higher than an impurity concentration in said first impurity region.

9. The semiconductor device according to claim 1 , further comprising a passivation film formed so as to cover said semi-insulating film.

10. the first electrode has a peripheral edge; the semi-insulating film has an inner periphery; the semi-insulating film covers the second electrode, The semiconductor device according to claim 1 , wherein the inner periphery covers the outer periphery.

11. The semi-insulating film has an inner periphery and an outer periphery, The semiconductor device according to claim 1 , wherein the first electrode and the second electrode cover the inner periphery and the outer periphery, respectively.

12. the semiconductor substrate has a second surface on an opposite side to the first surface in a thickness direction of the semiconductor substrate; a first recess is formed in the first surface so as to overlap with the first impurity region in a plan view and is recessed toward the second surface; 2 . The semiconductor device according to claim 1 , wherein the insulating film comprises a first insulating film buried in the first recess, and a second insulating film disposed on the first surface so as to cover the first insulating film.

13. The semiconductor device according to claim 12 , wherein the first insulating film is thicker than the second insulating film.

14. the semiconductor substrate has a second surface on an opposite side to the first surface in a thickness direction of the semiconductor substrate; a plurality of second recesses are formed in the first surface so as to overlap with the first impurity region in a plan view and are recessed toward the first surface; the second recesses are arranged at intervals along a direction from the element region toward the termination region, 2. The semiconductor device according to claim 1, wherein the insulating film comprises a first insulating film filled in each of the plurality of second recesses, and a second insulating film disposed on the first surface so as to cover the first insulating film.

15. The semiconductor device according to claim 1 , wherein an FRD is formed in said element region.

16. 2. The semiconductor device according to claim 1, wherein an IGBT is formed in said element region.

Citation Information

Patent Citations

  • High withstand voltage planar element

    JP1991171774A

  • High breakdown strength semiconductor device

    JP1999214670A

  • Semiconductor device

    JP2018147937A

  • Semiconductor device

    JP2021068833A

  • Semiconductor device

    JP2022074323A