The alloy steel composition with controlled oxide film formation and resin filling addresses the limitations of existing methods by maintaining high hardness and strength, ensuring electrical insulation and minimal dimensional changes, thus enhancing wear resistance and toughness.
Patent Information
- Application Number
- JP2024043113
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-18
- Filing Date
- 2024-03-19
- Publication Date
- 2024-11-28
AI Technical Summary
Existing methods for manufacturing alloy steel parts with insulation properties face issues such as insufficient wear resistance, toughness, and high material costs, as well as dimensional instability and environmental concerns from high-temperature oxide layer formation, which compromise the hardness and strength required for high-load environments.
An alloy steel composition with specific weight percentages of C, Si, Mn, Cr, Mo, Al, and V, along with optional W and Co, is treated to form an oxide film on its surface, which is then filled with resin to create an electrolytic corrosion prevention part with a hardness exceeding 58 HRC, using controlled oxidation at 500°C to 600°C to minimize dimensional changes.
The alloy steel maintains high hardness and strength while ensuring electrical insulation and minimal dimensional changes, addressing the limitations of existing methods by providing a cost-effective solution with improved wear resistance and toughness.
Abstract
Description
[Technical field]
[0001] The present invention relates to an alloy steel containing chromium, molybdenum, etc., an electrolytic corrosion prevention part using the same, and a method for manufacturing the same. [Background technology]
[0002] Conventionally, when manufacturing parts that require insulation using steel, measures to impart insulation have been taken by replacing part of the part with insulating ceramics such as alumina, or by covering the surface of the part with a resin such as PPS (see Patent Document 1).
[0003] Alternatively, some steel materials manufactured with a specified composition can be heated at high temperatures to form an insulating oxide layer on the surface of the part, thereby giving the part insulating properties (see Patent Documents 2 and 3). [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2009-236259 A [Patent Document 2] JP 2013-199674 A [Patent Document 3] JP 2004-84767 A Summary of the Invention [Problem to be solved by the invention]
[0005] However, when some of the parts disclosed in Patent Document 1 were replaced with resin and added, there were problems with the wear resistance and strength being insufficient compared to steel. Also, ceramics lacked toughness compared to steel, and there were problems with workability. In addition, the material costs of all of these materials were higher than steel, which increased the cost of the entire part.
[0006] On the other hand, as disclosed in Patent Document 2, when the surface of a steel material is oxidized to impart insulating properties to the parts, this is advantageous in terms of cost, but the hardness of conventional alloy steel is below 50HRC (HRC: Rockwell hardness C scale), and it is difficult to use such steel for long periods of time as parts in high-load environments that require wear resistance, fatigue strength, and the like.
[0007] This is because the carbon content, which contributes greatly to the hardness of alloy steel, is extremely low. In addition, the temperature required to form the oxide layer is in the high range of about 980 to 1220°C, so even if the material had high hardness before treatment, it may soften.
[0008] Even if high hardness could be achieved by heating to about 1200°C for both quenching and oxidation, the dimensions would vary greatly before and after the treatment. Therefore, in order to manufacture high-precision parts, grinding or other processes would be required after oxidation, and the oxide layer that had been so carefully formed would be ground away.
[0009] Furthermore, the material disclosed in Patent Document 3 also describes a method of oxidizing the surface of the steel material to give the part insulation, but does not disclose any information on the hardness or strength of the material, nor does it state any particular consideration. In addition, the method of forming the oxide layer involves immersion in an acid solution, which poses problems such as a decrease in material strength due to hydrogen embrittlement and a burden on the natural environment.
[0010] Therefore, an objective of the present invention is to provide an alloy steel that can maintain high strength (or hardness) while having electrical insulation between adjacent metal products, an electrolytic corrosion prevention part using the same, and a method for manufacturing the electrolytic corrosion prevention part. [Means for solving the problem]
[0011] In order to solve the above-mentioned problems, the invention of the alloy steel is an alloy steel containing, by weight percent, 0.01-1.0% C, 0.2-4.0% Si, 0.2-2.0% Mn, 1.0-9.0% Cr, 1.5-6.0% Mo, 0.01-5.0% Al, 0.01-1.2% V, with the balance being Fe and unavoidable impurities. Alternatively, the alloy steel may further contain, by weight percent, 0.01-2.0% W, or may further contain, by weight percent, 0.1-4.0% Co.
[0012] Next, the invention of the electrolytic corrosion prevention part is an electrolytic corrosion prevention part in which the recesses on the surface of the alloy steel are coated with an oxide film filled with resin using the above-mentioned alloy steel invention. The surface hardness of this alloy steel can be 58HRC or more on the Rockwell C scale.
[0013] The method for manufacturing the electrolytic corrosion prevention part includes forming an oxide film on the surface of the above-mentioned alloy steel at a temperature range of 500° C. to 600° C., and then filling the recesses formed on the surface of the oxide film with a resin. At this time, the oxide film may be formed on the surface of the alloy steel in an atmosphere containing at least either oxygen or water vapor. Effect of the Invention
[0014] The alloy steel of the present invention has a specific composition and can form an insulating oxide layer (oxide film) on the surface of the steel while maintaining a hardness exceeding 58HRC (Rockwell hardness C scale). In addition, the electrolytic corrosion prevention part of the present invention can achieve a hardness exceeding 58HRC by subjecting the alloy steel to heat treatment by quenching and tempering, and then by performing finish processing to ensure the dimensional accuracy of the part and then performing oxidation heat treatment, even if an insulating oxide film is formed, the dimensional change of the part due to the oxidation treatment can be kept relatively small. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0015] The content of each element contained in the alloy steel according to one embodiment of the present invention will be described. The chemical composition of the alloy steel of the present invention satisfies the following conditions: (1) the composition range allows an insulating oxide layer to be formed on the surface, (2) the composition range does not allow conductive precipitate particles (such as carbides) of a size large enough to penetrate the oxide layer to be formed, and (3) the composition range does not allow softening even when oxidation treatment is performed after quenching and tempering, and allows a hardness exceeding 58HRC to be obtained.
[0016] 《C (Carbon)》 The C content (C amount) is set to the range of 0.01 to 1.0% by weight. If the C amount exceeds this range, the toughness of the alloy steel may decrease, and the carbides in the matrix structure may become coarse. In addition, the hot workability of the alloy steel may deteriorate. On the other hand, if the C amount is less than this range, the surface hardness of the alloy steel becomes less than 58HRC.
[0017] Silicon The Si content (Si amount) is set to the range of 0.2 to 4.0% by weight. If the Si amount exceeds this range, the toughness of the alloy steel may decrease, or the hot workability may deteriorate. On the other hand, if the Si amount is below this range, the insulating property of the oxide layer formed on the surface may decrease, or the machinability may deteriorate.
[0018] Manganese The Mn content (Mn amount) is set to the range of 0.2 to 2.0% by weight. If it exceeds this range, there is a risk of the workability being deteriorated. On the other hand, if it is below this range, it is necessary to carefully select the raw materials, which will result in an increase in material costs.
[0019] 《Cr (Chromium)》 The Cr content (Cr amount) is in the range of 1.0 to 9.0% by weight. If it exceeds this range, the oxide layer of the alloy steel becomes thin and the insulating properties of the oxide layer decrease. If it falls below this range, the insulating properties of the oxide layer of the alloy steel decrease.
[0020] Mo (Molybdenum) The Mo content (Mo amount) is set to the range of 1.5 to 6.0% by weight. If it exceeds this range, the carbides may become coarse or the toughness of the alloy steel may decrease. On the other hand, if it is below this range, the surface hardness of the alloy steel after oxidation treatment may become less than 58HRC.
[0021] Aluminum (Aluminum) The Al content (Al amount) is set to the range of 0.01 to 5.0% by weight. If it exceeds this range, the surface hardness of the alloy steel after oxidation treatment may be less than 58HRC, or nonmetallic inclusions may increase, causing a decrease in fatigue strength. On the other hand, if it is below this range, the insulating properties of the oxide layer may decrease.
[0022] Vanadium The V content (V amount) may be within the range of 0.01 to 1.2% by weight. If this range is exceeded, the carbides may become coarse or the toughness of the alloy steel may decrease.
[0023] The alloy may further contain tungsten (W) in the range of 0.01 to 2.0% by weight, and may further contain cobalt (Co) in the range of 0.1 to 4.0% by weight.
[0024] Next, an embodiment of the present invention, an electrolytic corrosion prevention part using alloy steel and a manufacturing method thereof, will be described. In the invention of the electrolytic corrosion prevention part using alloy steel of the present invention, resin is filled into the recesses of the oxide film formed on the surface of the alloy steel, which is the base material. At this time, the surface hardness of the alloy steel, which is the base material, is preferably 58HRC or more on the Rockwell C scale.
[0025] Furthermore, even if the alloy steel, which has been quenched and tempered in advance, is heat treated again at a temperature range of 500°C or higher and 600°C or lower, the alloy steel has sufficient temper softening resistance characteristics and can fully maintain a hardness of more than 58HRC (hardness of alloy steel).
[0026] In the oxidation heat treatment step, the alloy steel is heat treated in an atmosphere containing either oxygen or water vapor, or in an atmosphere containing both oxygen and water vapor, to form an oxide film on the surface of the alloy steel. After the oxide film is formed, recesses formed on the surface of the oxide film are filled with a resin.
[0027] In this case, it is desirable to carry out the treatment after the final processing such as molding or cutting of the electrolytic corrosion prevention part. This is because even if heat treatment is carried out in an oxygen atmosphere after the final processing, the heating temperature is relatively low at 500 to 600°C, and the dimensional change of the electrolytic corrosion prevention part is very small.
Claims
1. An alloy steel comprising, by weight percent, 0.01-1.0% C, 0.2-4.0% Si, 0.2-2.0% Mn, 1.0-9.0% Cr, 1.5-6.0% Mo, 0.01-5.0% Al, 0.01-1.2% V, with the balance being Fe and unavoidable impurities.
2. The alloy steel according to claim 1, further comprising, by weight percent, W: 0.01 to 2.0%.
3. The alloy steel according to claim 2, further comprising, by weight percent, Co: 0.1 to 4.0%.
4. 4. An electrolytic corrosion prevention part using the alloy steel according to claim 1, characterized in that the surface of the alloy steel is coated with an oxide film, and a recess formed on the surface of the oxide film is filled with resin.
5. 5. The electrolytic corrosion prevention part according to claim 4, wherein the surface hardness of said alloy steel is 58 HRC or more on the Rockwell C scale.
6. 5. The method for manufacturing an electrolytic corrosion prevention part according to claim 4, characterized in that after forming the oxide film on the alloy steel at a temperature range of 500° C. or more and 600° C. or less, a resin is filled into recesses formed on the surface of the oxide film.
7. 6. The method for manufacturing an electrolytic corrosion prevention part according to claim 5, characterized in that after forming the oxide film on the alloy steel at a temperature range of 500° C. or more and 600° C. or less, recesses formed on the surface of the oxide film are filled with resin.
8. The method for producing an electrolytic corrosion-preventing part according to claim 6, characterized in that the oxide film is formed on the surface of the alloy steel in an atmosphere containing at least either oxygen or water vapor.
9. The method for producing an electrolytic corrosion-preventing part according to claim 7, characterized in that the oxide film is formed on the surface of the alloy steel in an atmosphere containing at least either oxygen or water vapor.
Citation Information
Patent Citations
Roller bearing
JP2004084767A
Insulating rolling bearing for electrical corrosion prevention
JP2009236259A
Stainless steel material with good insulation and method for producing the same
JP2013199674A