Short fiber multi-phase reinforced thermoplastic resin structure with different fiber content, joint body thereof, and manufacturing method thereof

The short fiber multi-phase reinforced thermoplastic resin structure addresses mechanical, electrical, and thermal conductivity issues by varying fiber content and using laser irradiation to enhance strength and conductivity, reducing costs and enabling complex shapes.

JP2024166633AActive Publication Date: 2024-11-29TODO META COMPOSITES CONTRACT CO
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2023082848
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-19
Publication Date
2024-11-29
Estimated Expiration
2043-05-19

AI Technical Summary

Technical Problem

Existing methods using short fibers for reinforcing thermoplastic resin structures face issues with mechanical properties, electrical conductivity, thermal conductivity, and increased manufacturing costs, while long fibers result in reduced strength and surface irregularities during 3D printing.

Method used

A short fiber multi-phase reinforced thermoplastic resin structure with locally varying fiber content, where a first short fiber with high content is arranged on the surface and a second short fiber with lower content is used elsewhere, combined with laser irradiation to create recesses exposing high-fiber content regions, enhancing mechanical, electrical, and thermal properties.

Benefits of technology

The method reduces manufacturing costs and increases strength while ensuring electrical and thermal conductivity by locally increasing fiber content, allowing for complex shapes and improved surface properties.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024166633000001_ABST
    Figure 2024166633000001_ABST
Patent Text Reader

Abstract

To provide a short fiber multi-phase reinforced thermoplastic resin structure having multiple phases of short fibers with different fiber contents, a joint body thereof, and a manufacturing method thereof.SOLUTION: Before laser irradiation, a short carbon fiber SC of a short carbon fiber reinforced thermoplastic resin structure 1 is arranged discretely and spaced apart along a X direction (orientation direction). A laser beam L from a laser light source 31 is locally irradiated onto a portion 1a of a surface of the short carbon fiber reinforced thermoplastic resin structure 1, heating the thermoplastic resin to a temperature above its melting point and causing it to move or evaporate. After the laser irradiation, recesses 31 are formed in the short carbon fiber reinforced thermoplastic resin structure 1, and as a result, a short carbon fiber reinforced multi-phase thermoplastic resin structure 3 having different fiber contents is formed. In the recesses 31, the thermoplastic resin disappears, so that the short carbon fibers SC are locally exposed at a bottom of the recesses 31 and overlap with each other, essentially converting into short carbon fibers SC' having a high fiber content.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a short fiber multi-phase reinforced thermoplastic resin structure containing short fiber multi-phase fibers with different fiber contents, a bonded body thereof, and a manufacturing method thereof. [Background technology]

[0002] Methods for reinforcing thermoplastic resin structures molded by 3D printers, injection molding, compression molding, etc., with fibers include those that use short fibers and those that use long fibers (continuous fibers) (see Patent Document 1). In particular, carbon fiber reinforced plastic (CFRP) is superior to metals in terms of specific rigidity and specific strength (see Non-Patent Document 1). [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Patent Publication No. 2022-98042 [Non-patent literature]

[0004] [Non-Patent Document 1] T. Gerngross, D. Nieberl, “Automated manufacturing of large, three-dimensional CFRP parts from dry textiles”, CEAS Aeronautical Journal, 7(2), 2016, 241-257. Summary of the Invention [Problem to be solved by the invention]

[0005] However, when short fibers are used as reinforcing materials, molding that takes advantage of the advantages of short fibers is possible, but there is a problem that the mechanical properties are not so great. In particular, when electrical conductivity is required, short carbon fibers have low or no electrical conductivity compared to carbon nanotubes and carbon black, and the electrical conductivity of the short carbon fiber reinforced thermoplastic resin structure cannot be ensured. On the other hand, when long fibers are used as reinforcing materials, the mechanical properties are large, but when a long fiber reinforced thermoplastic resin structure with a complex shape is molded, the long fibers are folded back and the strength of that part decreases. As a countermeasure, a cutting mechanism is provided to cut the long fiber reinforced thermoplastic resin structure at a predetermined length. As a result, there is a problem that the manufacturing cost of the long fiber reinforced thermoplastic resin structure increases. In addition, in 3D printing, if only long fiber thermoplastic resin is molded, unevenness will occur on the surface, so short fiber thermoplastic resin is used for the entire surface, which means that the electrical conductivity of the surface cannot be ensured and the thermal conductivity cannot be ensured. Furthermore, when the volume content of continuous short fibers is high during 3D printing, there is the issue that they are prone to clogging the nozzle and are difficult to bend, which limits the curvature of the printing path, making it impossible to print with a large volume content. [Means for solving the problem]

[0006] In order to solve the above-mentioned problems, the short fiber multi-phase reinforced thermoplastic resin structure of the present invention has a first short fiber having a high fiber content locally arranged on at least a portion of the surface of the short fiber multi-phase reinforced thermoplastic resin structure, and a second short fiber having a lower fiber content than the first short fiber arranged in the short fiber multi-phase reinforced thermoplastic resin structure other than at least a portion of the surface.

[0007] In addition, the joint of short fiber multi-phase reinforced thermoplastic resin structures according to the present invention has a first short fiber having a high fiber content locally arranged on at least a portion of the surface of each of the first and second short fiber multi-phase reinforced thermoplastic resin structures, and a second short fiber having a lower fiber content than the first short fiber arranged in the first and second short fiber multi-phase reinforced thermoplastic resin structures other than at least a portion of the surface, at least a portion of the surface of the first short fiber multi-phase reinforced thermoplastic resin structure and at least a portion of the surface of the second short fiber multi-phase reinforced thermoplastic resin structure are melt-bonded, and the first and second short fibers are electrically conductive or highly thermally conductive.

[0008] Furthermore, the manufacturing method of the short fiber reinforced multiphase thermoplastic resin structure according to the present invention comprises a molding step for molding a short fiber reinforced thermoplastic resin structure composed of first short fibers, and a resin melting step for locally melting, moving or evaporating at least a part of the thermoplastic resin on the surface of the short fiber reinforced thermoplastic resin structure, thereby converting at least a part of the surface of the short fiber reinforced thermoplastic resin structure into second short fibers having a higher fiber content than the first short fibers. Effect of the Invention

[0009] According to the present invention, since short fibers with different fiber content are used as reinforcing materials, it is possible to reduce the manufacturing cost of a composite material having locally different physical properties, and to increase the strength by locally increasing the fiber content. If the short fibers on the surface are made electrically conductive and thermally conductive, the electrical conductivity and thermal conductivity of the surface can be ensured. [Brief description of the drawings]

[0010] [Figure 1] FIG. 1 is a diagram for explaining a short carbon fiber reinforced thermoplastic resin structure molding process in an embodiment of a method for manufacturing a short fiber multi-phase reinforced thermoplastic resin structure according to the present invention, in which (A) is a cross-sectional view showing a short carbon fiber reinforced thermoplastic resin structure, and (B) is a diagram showing a 3D printer. [Diagram 2]FIG. 1 is a diagram for explaining a laser irradiation step as a heating step in an embodiment of a method for producing a short fiber multi-phase reinforced thermoplastic resin structure according to the present invention, in which (A) is a cross-sectional view and an electron microscope image of a short carbon fiber reinforced thermoplastic resin structure before laser irradiation, (B) is a cross-sectional view of the short carbon fiber reinforced thermoplastic resin structure during laser irradiation, and (C) is a cross-sectional view and an electron microscope image of the short carbon fiber multi-phase reinforced thermoplastic resin structure after laser irradiation. [Diagram 3] 3 shows another short carbon fiber reinforced multiphase thermoplastic resin structure after laser irradiation, where (A) is an electron microscope image, (B) is a photograph of water droplets when they are dropped onto the short carbon fiber reinforced thermoplastic resin structure before laser irradiation, and (C) is a photograph of water droplets when they are dropped onto the short carbon fiber reinforced thermoplastic resin structure before laser irradiation. [Figure 4] FIG. 3 is a diagram showing an application example of the short carbon fiber multi-phase reinforced thermoplastic resin structure of FIG. 1 and FIG. 2. [Diagram 5] 3A and 3B are diagrams for explaining the joints of the short carbon fiber multiphase reinforced thermoplastic resin structures of FIG. 1 and FIG. 2, in which (A) shows a joint interface type resin fusion joining, (B) shows one-sided current type resin fusion joining, and (C) shows a vice pressure joint interface type resin fusion joining. [Figure 6] 3 is a diagram illustrating another bonding method for the short carbon fiber multi-phase reinforced thermoplastic resin structure shown in FIG. 1 and FIG. 2. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] 1 and 2 are diagrams for explaining an embodiment of a method for producing a short fiber multi-phase reinforced thermoplastic resin structure according to the present invention.

[0012] First, the short carbon fiber reinforced thermoplastic resin structure molding process will be described with reference to Fig. 1. In addition, (A) is a cross-sectional view of the short carbon fiber reinforced thermoplastic resin structure, and (B) is a front view of the 3D printer.

[0013] The short carbon fiber reinforced thermoplastic resin structure 1 shown in FIG. 1(A) is molded by a 3D printer 2 shown in FIG. 1(B).

[0014] As shown in FIG. 1B, the short carbon fiber reinforced filament F wound around the loop 11 is supplied to the 3D printer 2. The 3D printer 2 is, for example, the X-Plus manufactured by QiDi Tech, and is composed of an extruder 21, a nozzle 22 with a heater, and a print bed 23. The short carbon fiber reinforced filament F wound around the loop 11 is a thermoplastic composite material containing short carbon fibers (SCFRP). The higher the carbon fiber content of this thermoplastic composite material, the higher its strength is, but the short carbon fiber reinforced filament F becomes hard and brittle. As a result, it becomes impossible to wind it around the loop 11. Therefore, the fiber content of the short carbon fiber reinforced filament F is small, at 10 to 25%.

[0015] In (B) of Fig. 1, the short carbon fiber reinforced filament F is adjusted and extruded by two gears 21a and 21b of an extruder 21, and is injected from a heater nozzle 22 having a heater temperature of about 270 to 290°C. The thermoplastic resin of the short carbon fiber reinforced filament F is, for example, Nylon (registered trademark), and the short carbon fibers are short, about 50 to 300 µm in length on average.

[0016] The obtained short carbon fiber reinforced thermoplastic resin structure 1 shown in FIG. 1(A) is laminated in multiple layers in the Z direction, and the short carbon fibers in each layer are oriented along the X direction (orientation direction) shown in FIG. 1(B).

[0017] Next, the laser irradiation step as a heating step will be described with reference to Fig. 2. The laser irradiation step is also performed during the molding step using the filament F. Fig. 2(A) is a cross-sectional view and an electron microscope image of the short carbon fiber reinforced thermoplastic resin structure before the laser irradiation step, Fig. 2(B) is a diagram explaining the laser irradiation, and Fig. 2(C) is a cross-sectional view and an electron microscope image of the short carbon fiber multiphase reinforced thermoplastic resin structure after the laser irradiation step.

[0018] 2A, the short carbon fibers SC of the short carbon fiber reinforced thermoplastic resin structure 1 before laser irradiation are arranged discretely and spaced apart along the X direction (orientation direction). Therefore, the carbon fiber content is small throughout the short carbon fiber reinforced thermoplastic resin structure 1, and therefore the strength of the short carbon fiber reinforced thermoplastic resin structure 1 is not very high.

[0019] 2B, a laser beam L from a laser source 31 is locally irradiated onto a portion 1a of the surface of the short carbon fiber reinforced thermoplastic resin structure 1. For example, the conditions of the laser beam L are as follows. Semiconductor laser with wavelength of 455 nm Laser power: 40% Focal length F: 40mm Therefore, the laser light L is absorbed by the surface portion 1a of the short carbon fiber reinforced thermoplastic resin structure 1, and as a result, the thermoplastic resin is heated above its melting point and moved or evaporated. In this case, if the laser light L is too strong, too much thermoplastic resin is burned and disappeared. To prevent this, the defocus amount DF of the laser light L is adjusted to, for example, 20 mm. Also, a galvano scanning mirror can be provided to extend the portion 1a in the X or Y direction, and the laser light L can be scanned at, for example, 5 mm / s.

[0020] After the laser irradiation, as shown in FIG. 2C, a recess 31 is formed in the short carbon fiber reinforced thermoplastic resin structure 1, and as a result, a short carbon fiber multi-phase reinforced thermoplastic resin structure 3 consisting of short carbon fibers with different fiber contents is formed. That is, since the thermoplastic resin disappears in the recess 31, the short carbon fibers SC are locally exposed at the bottom of the recess 31 and overlap with each other, and are substantially converted into short carbon fibers SC'. As a result, the bottom region of the recess 31 becomes a short carbon fiber region with a high fiber content, and the fiber content becomes high, for example, 45 to 50%, and therefore the strength becomes high. This results in a short carbon fiber multi-phase reinforced thermoplastic resin structure 3 having both a region of short carbon fibers SC and a region of short carbon fibers SC'. In this way, a short carbon fiber multi-phase reinforced thermoplastic resin structure 3 that achieves both low manufacturing cost and high strength is realized. In addition, when the short carbon fibers SC' are included, high electrical conductivity can also be achieved.

[0021] Furthermore, when the laser irradiation conditions are changed or a thermoplastic resin with low transparency is used, the surface of the thermoplastic resin becomes hairy, as shown in the electron microscope image of Fig. 3(A). When a water droplet is placed directly on this hairy surface, the contact angle of the water droplet is about 30° or less, as shown in Fig. 3(B), and it was found to exhibit hydrophilicity. Note that, as shown in Fig. 3(C), before irradiation with the laser light L, the contact angle of the water droplet is 90°, exhibiting hydrophobicity. In this way, the surface of the short carbon fiber multiphase reinforced thermoplastic resin structure 3 can be modified.

[0022] When the thermoplastic resin is a polyamide resin (PA-6), for example, Nylon (registered trademark), the laser light L passes through Nylon (registered trademark) and is absorbed by the short carbon fibers SC, causing Nylon (registered trademark) to melt and fly away as described above. Therefore, in order to make the surface of Nylon (registered trademark) hair-like, a dye is added to Nylon (registered trademark) to reduce the transmittance of Nylon (registered trademark).

[0023] When the thermoplastic resin is polyetherimide (PEI), the laser light L is absorbed by the surface of the polyetherimide (PEI), and only the resin melts and vaporizes. Thus, a hairy surface is formed with short carbon fibers SC half embedded in it. To create a conductive surface with polyetherimide (PEI), an infrared laser is used, or a multi-step laser process is required, such as removing the resin with a laser light of intensity A, followed by a laser light of intensity B applied by the short carbon fibers.

[0024] FIG. 4 is a top view for explaining an application example in which the short carbon fiber multi-phase reinforced thermoplastic resin structure of FIG. 1 and FIG. 2 is made to function as a strain sensor.

[0025] As shown in (A), (B), (C), (D), and (E) of Fig. 4, in the short carbon fiber multi-phase reinforced thermoplastic resin structures 3-A, 3-B, 3-C, 3-D, and 3-E having a length L = 120 mm × width W = 18 mm × thickness 1.6 mm, the recesses 31-A, 31-B, 31-C, 31-D, and 31-E having a depth of 65% of the short carbon fiber region having a high fiber content are formed in the shape of the electrode parts E1 and E2 having a size of 5 mm × 15 mm and the current path part E3 having a width of 1 mm connected between the electrode parts E1 and E2. In this case, the current path part E3 of the short carbon fiber multi-phase reinforced thermoplastic resin structures 3-A, 3-B, 3-C, 3-D, and 3-E has the number of folds 0, 1, 2, 3, and 4, and the lengths are 30 mm, 64 mm, 8.2 mm, 116 mm, and 134 mm. As a result, the initial resistance values ​​of the short carbon fiber multi-phase reinforced thermoplastic resin structures 3-A, 3-B, 3-C, 3-D, and 3-E were 0.68 kΩ, 6.42 kΩ, 7.29 kΩ, 7.72 kΩ, and 13.29 kΩ. In this way, the initial resistance value of the short carbon fiber multi-phase reinforced thermoplastic resin structure 3 can be adjusted by changing the pattern of the recesses 31, and it can be made to function as a strain sensor.

[0026] In the above-mentioned short carbon fiber multi-phase reinforced thermoplastic resin structure 3, the fiber content of the bottom of the recess 31 where the surface resin has been moved or evaporated by the laser light L is high, and therefore the electrical resistance value is low. Therefore, two short carbon fiber multi-phase reinforced thermoplastic resin structures 3 can be joined by melting the resin through resistance heating.

[0027] FIG. 5 is a diagram for explaining a joined body of the short carbon fiber multi-phase reinforced thermoplastic resin structures shown in FIG. 1 and FIG.

[0028] In Fig. 5(A), two short carbon fiber multi-phase reinforced thermoplastic resin structures 3, 3' are joined by joint interface type resin fusion joining. That is, electrodes E3, E4 are provided on the recesses 31, 31' of the short carbon fiber regions with a high fiber content of the short carbon fiber multi-phase reinforced thermoplastic resin structures 3, 3'. Then, while the recesses 31, 31' of the short carbon fiber regions with a high fiber content of the short carbon fiber multi-phase reinforced thermoplastic resin structures 3, 3' are in contact with each other, current is passed between the electrodes E3, E4 to fusion-join the two structures by Joule heat. The recesses 31, 31' do not need to be formed entirely, and may be formed partially, for example, linearly.

[0029] In FIG. 5B, two short carbon fiber multi-phase reinforced thermoplastic resin structures 3, 3' are one-sided current-type resin fusion bonding. That is, electrodes E3, E4 are provided in the recesses 31 or 31' of the short carbon fiber region with a high fiber content of one of the short carbon fiber multi-phase reinforced thermoplastic resin structures 3, 3'. Then, while the recesses 31, 31' of the short carbon fiber region with a high fiber content of the short carbon fiber multi-phase reinforced thermoplastic resin structures 3, 3' are in contact with each other, current is passed between the electrodes E3, E4 to fusion bond both of them by Joule heat. In this case, the recesses 31, 31' do not need to be formed entirely, and may be formed partially, for example, linearly.

[0030] In Fig. 5(C), two short carbon fiber multi-phase reinforced thermoplastic resin structures 3, 3' are bonded by a vice-processed joint interface type resin fusion bonding. That is, like Fig. 5(A), electrodes E3, E4 are provided in the recesses 31 of the short carbon fiber regions of the short carbon fiber multi-phase reinforced thermoplastic resin structures 3, 3' with a high fiber content. In a state where the recesses 31 of the short carbon fiber regions of the short carbon fiber multi-phase reinforced thermoplastic resin structures 3, 3' with a high fiber content are brought into contact with each other and pushed back by the suction cups 4, 4', an electric current is passed between the electrodes E3, E4 to melt and bond the two structures by Joule heat. In this case, the recesses 31, 31' do not need to be formed entirely, and may be formed partially, for example, linearly.

[0031] Incidentally, the one-sided current-type resin fusion joining shown in FIG. 5(B) may also be made into a one-sided current-type resin fusion joining by using a vice.

[0032] The joining methods of (A), (B), and (C) in Fig. 5 can also be applied to joining two short carbon fiber multi-phase reinforced thermoplastic resin structures 3, 3' having completely different lamination directions as shown in Fig. 6. That is, in Fig. 6, the lamination direction of the short carbon fiber multi-phase reinforced thermoplastic resin structure 3 is the Z direction, while the lamination direction of the short carbon fiber multi-phase reinforced thermoplastic resin structure 3' is the X direction, and the lamination directions are almost perpendicular to each other. Even in this case, the joining methods of (A), (B), and (C) in Fig. 5 can be used to melt-join the short carbon fiber multi-phase reinforced thermoplastic resin structures 3, 3'.

[0033] 2B, the laser irradiation is performed locally on a part 1a of the surface of the short carbon fiber multi-phase reinforced thermoplastic resin structure 1, but it may be performed on the entire surface. In this case, a region of short carbon fibers SC' with a high fiber content is formed on the entire surface of the short carbon fiber multi-phase reinforced thermoplastic resin structure 1, while the short carbon fiber multi-phase reinforced thermoplastic resin structure 1 other than the surface remains as a region of short carbon fibers SC with a low fiber content.

[0034] In FIG. 2B, the short carbon fibers SC on the surface of the short carbon fiber reinforced thermoplastic resin structure 1 are converted to short carbon fibers SC' by laser irradiation, but other local heat rays than laser light, such as xenon lamp light, may be used. Alternatively, a solvent that melts the thermoplastic resin may be used. For example, if the thermoplastic resin is polyamide resin, such as nylon (registered trademark), the short fibers are left on the surface by locally melting it using a dissolving solution "e-solv 21RS" (registered trademark) manufactured by Kaneko Chemical Co., Ltd. After that, high-temperature resin or adhesive may be dripped.

[0035] Furthermore, in the above-described embodiment, the recesses 31, 31' are formed, but if protrusions are formed before the heating step and the heating step is then performed on these protrusions, the recesses 31, 31' will not exist.

[0036] Furthermore, in the above-described embodiment, carbon fibers are used as the conductive fibers, but other conductive fibers, such as metal fibers such as metal whiskers, ceramic fibers, or organic fibers, may be used.

[0037] Furthermore, the thermoplastic resin may be a polyamide resin such as nylon (registered trademark) or other resin such as polyphenylene sulfide resin (PPS), polyetherimide (PEI), or polyetheretherketone (PEEK).

[0038] Furthermore, the present invention can be applied to any modifications within the obvious scope of the above-described embodiments. [Explanation of symbols]

[0039] 1: Short carbon fiber multi-phase reinforced thermoplastic resin structure 11: Loop F: Short carbon fiber multi-phase reinforcing filament 2:3D printer 21: Extruder 21a, 21b: Gear 22: Heated nozzle 23: Print head 4, 4′: Vice SC: Short carbon fiber SC': Short carbon fiber with high fiber content (overlap of exposed short carbon fiber) 3, 3-A, 3-B, 3-C, 3-D, 3-E, 3-F, 3-G, 3,3′: Short carbon fiber multi-phase reinforced thermoplastic resin structures with different fiber contents 31, 31′: recess

Claims

1. A short fiber multi-phase reinforced thermoplastic resin structure, A first short fiber is locally contained in at least a part of the surface of the short fiber multi-phase reinforced thermoplastic resin structure, A short fiber multi-phase reinforced thermoplastic resin structure, in which the short fiber multi-phase reinforced thermoplastic resin structure other than at least a portion of the surface contains second short fibers having a fiber content lower than that of the first short fibers.

2. The short fiber multi-phase reinforced thermoplastic resin structure according to claim 1, wherein the surface of the part of the short fiber multi-phase reinforced thermoplastic resin structure is in a hair-like state.

3. 2. The short fiber multi-phase reinforced thermoplastic resin structure according to claim 1, wherein said first and second short fibers are electrically conductive.

4. 2. The short fiber multi-phase reinforced thermoplastic resin structure according to claim 1, wherein said first and second short fibers are carbon fibers.

5. The short fiber multiphase reinforced thermoplastic resin structure according to claim 3, wherein the portion has two electrode regions when viewed from the surface and a current path region that connects the two electrode regions and has a width smaller than that of the electrode regions, and acts as a strain sensor.

6. The short fiber multi-phase reinforced thermoplastic resin structure according to claim 5 , wherein the current path region has a folded portion.

7. A bonded body of first and second short fiber multi-phase reinforced thermoplastic resin structures, The first short fibers are locally contained in at least a portion of the surface of each of the first and second short fiber multi-phase reinforced thermoplastic resin structures, The first and second short fiber multi-phase reinforced thermoplastic resin structure other than the at least a part of the surface contains second short fibers having a fiber content lower than that of the first short fibers, At least a portion of the surface of the first short fiber multi-phase reinforced thermoplastic resin structure and at least a portion of the surface of the second short fiber multi-phase reinforced thermoplastic resin structure are melt-bonded; A bonded body of short fiber multi-phase reinforced thermoplastic resin structures, wherein the first and second short fibers are electrically conductive.

8. 8. The short fiber multi-phase reinforced thermoplastic resin structure according to claim 7, wherein the first and second short fibers are short carbon fibers.

9. The laminate of the first short fiber reinforced thermoplastic resin structure and the laminate of the second short fiber reinforced thermoplastic resin structure are different from each other in the lamination direction of the first short fiber reinforced thermoplastic resin structure.

10. A molding step for molding a short fiber reinforced thermoplastic resin structure made of the first short fibers; a resin melting step for locally melting, moving or evaporating at least a part of the thermoplastic resin on the surface of the short fiber reinforced thermoplastic resin structure, and converting the at least a part of the short fiber reinforced thermoplastic resin structure into second short fibers having a higher fiber content than the first short fibers; A method for producing a short fiber multi-phase reinforced thermoplastic resin structure comprising:

11. The method for producing a short fiber multi-phase reinforced thermoplastic resin structure according to claim 10, wherein the resin melting step uses laser light, xenon lamp light, or a solvent for the thermoplastic resin.

12. The method for producing a short fiber multi-phase reinforced thermoplastic resin structure according to claim 10, wherein the first and second short fibers are electrically conductive.

13. The method for producing a short fiber multi-phase reinforced thermoplastic resin structure according to claim 12, wherein the first and second short fibers are carbon fibers.

14. a molding step for molding a filament made of a first short fiber; a laser melting step for locally melting, moving or evaporating at least a part of the thermoplastic resin on the surface of the filament by a laser beam during the forming step, thereby converting the at least a part of the filament into a second staple fiber having a higher fiber content than the first staple fiber; A method for producing a short fiber multi-phase reinforced thermoplastic resin structure comprising:

Citation Information

Patent Citations

  • Method of fusing cfrtp material

    JP2012187903A

  • Method of joining metal member with resin member and resin member used for the same

    JP2016068128A

  • Methof for manufacturing leafspring with electrodes for railcar truck

    WO2017043079A1

  • Fiber-reinforced thermoplastic resin filament for 3D printer and molded article of the same

    JP2022098042A