Filling management method of cement-based material
The cement-based material filling management method uses a two-core electric wire detection probe to accurately and cost-effectively detect filling status, addressing issues of poor control accuracy and complexity in existing technologies, thereby preventing construction defects.
Patent Information
- Application Number
- JP2024068416
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-19
- Filing Date
- 2024-04-19
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2044-04-19
AI Technical Summary
Existing methods for detecting the filling status of cement-based materials, such as concrete and mortar, suffer from poor control accuracy, high cost, complexity, and difficulty in visually inspecting closed spaces, leading to potential construction defects like formwork deformation and cold joints.
A cement-based material filling management method using a detection probe made of a two-core covered electric wire with uncovered portions, where capacitance is measured to detect filling status by applying alternating current voltage, allowing for accurate and cost-effective detection of filling height and position.
Enables easy and low-cost detection of filling positions in closed spaces, ensuring uniform filling and preventing construction defects by providing real-time visual management of filling status.
Smart Images

Figure 2024167053000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for managing the filling of cement-based materials such as pre-hardened concrete (fresh concrete) and pre-hardened mortar (fresh mortar), and more particularly to a method for managing the filling status of cement-based materials in filling spaces such as tunnel lining concrete and pneumatic caissons. [Background technology]
[0002] In general, when constructing a concrete structure, fresh concrete or the like is filled into a closed space surrounded by a formwork. For example, in mountain tunnel construction, a tunnel arch-shaped formwork called a center is used when pouring lining concrete to cover the ground surface of the excavated interior. The general length of the formwork used for such purposes is 9 to 12 m, and one span of concrete is filled along that length, after which it is moved sequentially in the direction of the tunnel for construction. In general, the excavated ground surface is covered with a waterproof sheet, and the space between the inner surface of the waterproof sheet and the outer surface of the center is filled with lining concrete using a concrete pump truck, using an inspection window provided on the center formwork surface as the filling port.
[0003] A vibrator is used to compact the concrete every 50cm or so of pouring height, and the inspection window is switched to ensure that the concrete is poured at a horizontal level on both sides.Then, the inspection window is switched upwards depending on the concrete pouring height, and finally the concrete is filled in by pouring it from a single blowout port at the top end.
[0004] Until pouring from the top end blowout port, concrete must be poured continuously as evenly and horizontally as possible to avoid applying uneven pressure to the center formwork, and if there is a large difference in the height of the concrete on the left and right sides when pouring, large pressure or uneven pressure will act on the center, causing it to vibrate horizontally, causing the center position to move, or the uneven load may cause formwork deformation or extrusion, resulting in problems with the construction joints. Also, if the pouring time is long, it may cause cold joints.
[0005] In order to prevent such construction defects, it is important for quality control to control the pouring height of the concrete, but in the past, this was checked by workers visually checking the pouring height while shining light through multiple inspection windows in the narrow center. Also, it was sometimes difficult to visually check places away from the inspection windows.
[0006] In addition, when filling the enclosed space between the tunnel top and the center tunnel top with lining concrete, it is important to fill every corner of the tunnel top densely. To do this, it is necessary to check that the concrete is being filled reliably along the longitudinal direction of the top, but because it is an enclosed space, this cannot be checked visually, and workers must estimate the filling status by observing the leak status and location of the filling concrete and bleeding water from the end formwork during filling.
[0007] Therefore, the following proposals have been made to check the filling of concrete and to detect the filling height.For example, a method for checking concrete filling using capacitance has been proposed (Patent Document 1), in which a detection unit consisting of two conductors spaced at a fixed distance is fixed at a predetermined position in a concrete filling formwork, concrete is filled into the gap between the detection units while densely filling the formwork, the capacitance at the time of filling is measured, and the degree of filling of the filled concrete is found by comparing the capacitance at the time of filling with the capacitance at the time of filling.
[0008] Other methods that have been proposed include installing a level sensor equipped with at least a pair of electrode rods extending opposite each other along the height direction of the concrete to be filled, checking the concrete material being poured based on the capacitance of the electrode rods, and measuring the rise height of the filled concrete based on the change in capacitance (Patent Document 2), and installing a level sensor consisting of a pair of electrode wires covered with an insulating material that extend vertically parallel to each other at a fixed horizontal distance within a void, and calculating the rise height of the concrete filled in the void based on the change in capacitance that occurs between the pair of electrode wires in accordance with the dielectric constant of the concrete as the void is filled with concrete (Patent Document 3).
[0009] Also, a method has been proposed in which a waterproof sheet is attached to the inner wall surface of a tunnel so as to cover the inner wall surface, and a long, thin level sensor whose detection amount changes depending on the length of contact with the concrete is attached to the waterproof sheet with its longitudinal direction extending along the longitudinal or circumferential direction of the tunnel, and the level sensor detects using the electrostatic capacitance generated between a pair of electrode wires (Patent Document 4).
[0010] Furthermore, a method has been proposed in which a fresh concrete sensor equipped with two rod-shaped electrodes is placed at a location where the filling status is to be checked, and an AC voltage supplied from a commercial power source is applied to the fresh concrete sensor to measure the electrical resistance, thereby detecting the filling of fresh concrete (Patent Document 5), and a method has been proposed in which the filling status of a filling material such as a lining concrete is detected using a sheet member and a sensor that detects the filling status of the filling material, the sheet member having a base material and lead wires wired along the base material, and the sensor is composed of a piezoelectric sensor or a capacitance sensor in which an upper electrode layer, a piezoelectric layer, and a lower electrode layer are stacked in that order, and a resistance sensor in which two electrodes are arranged opposite each other with a predetermined distance between them (Patent Document 6). [Prior art documents] [Patent documents]
[0011] [Patent Document 1] Japanese Patent Application Publication No. 6-229968 [Patent Document 2] Japanese Patent Application Publication No. 11-287045 [Patent Document 3] JP 2012-172375 A [Patent Document 4] JP 2019-78047 A [Patent Document 5] Japanese Patent Application Publication No. 9-228639 [Patent Document 6] JP 2018-179995 A Summary of the Invention [Problem to be solved by the invention]
[0012] In the proposal of Patent Document 1, a detection unit consisting of two conductors spaced at a fixed interval measures the capacitance when concrete is filled in a concrete filling formwork, and the degree of filling of the filled concrete is determined by comparing the measurements. The capacitance is detected only by the conductor parts of the two electric wires, and the capacitance when filling is compared with the capacitance when filling to detect the degree of filling in stages in the height direction when concrete is filled at that position. However, this method is an intermittent measurement, and there is a problem of poor management accuracy.
[0013] The proposal in Patent Document 2 claims that the height of concrete build-up can be continuously measured based on the capacitance of at least a pair of electrodes that are installed facing each other. However, in this case, a level sensor equipped with a pair of electrodes must be installed, which results in a large facility. In addition, the relationship between the capacitance and the height of concrete build-up is not specifically described.
[0014] The proposal in Patent Document 3 is a method for calculating only the rise height of the filled concrete based on the change in capacitance that occurs between a pair of electrode wires as concrete is filled into a void extending vertically.
[0015] The proposal in Patent Document 4 detects the height of the concrete and whether it has soaked into the horizontal part based on the capacitance that occurs when concrete is filled between a pair of electrode wires that extend along the longitudinal or circumferential direction of the waterproof sheet on the inner wall of the tunnel. However, it is not possible to know at what position on the level sensor the concrete has been filled in the horizontal part at the top end.
[0016] The proposal in Patent Document 5 is to measure the electrical resistance when fresh concrete reaches between the rod-shaped electrodes, thereby detecting that the fresh concrete has been filled at the position of the rod-shaped electrodes. However, it is necessary to manufacture rod-shaped electrodes with lead wires for each position where the filling status is to be detected, and costs are incurred for each detection unit.
[0017] In the proposal of Patent Document 6, the sheet member has a piezoelectric sensor, a capacitance sensor, and a resistance sensor as sensors for detecting the filling status of the sheet member and the filling material, and the filling status of the filling concrete is judged comprehensively. However, there is a problem that the sensors are complicated and expensive.
[0018] The present invention has been made in consideration of the above circumstances, and an object of the present invention is to provide a method for managing the filling of cement-based materials, which makes it possible to easily and low-costly detect the filling position of fresh concrete during filling using a detection probe with a simple structure. [Means for solving the problem]
[0019] The method for managing the filling of cement-based materials of the present invention has been made to solve the above technical problems, and has the following features.
[0020] First, the method for managing the filling of a cement-based material of the present invention is a method for managing the filling of a cement-based material, comprising: disposing a detection probe made of a two-core coated electric wire in a filling space of the cement-based material; and detecting a filling condition of the cement-based material by measuring a capacitance using the detection probe, A first detection probe in which an uncoated portion is provided in the middle of a two-core coated electric wire by removing the coating of each of the two cores, one end of the two cores is insulated, and the other end is used as a connection line for inputting electricity and for measuring devices, and the coated portion and the uncoated portion are integrally formed; and / or a non-coated portion is provided at the middle of one core of a two-core coated electric wire by removing the coating, and a terminal on one end of each of the two cores is insulated, and the other end is used as a connection line for an electrical input and a measuring device, and a second detection probe is installed in which the coated portion and the non-coated portion are integrally formed; When filling the cement-based material into the filling space, an AC voltage is applied to the first detection probe and / or the second detection probe to measure the capacitance between the two cores, and the filling status of the cement-based material is detected based on a change in the capacitance value. Secondly, in the method for managing filling of a cement-based material according to the first aspect of the present invention, the first detection probe and / or the second detection probe are installed in the filling space of the cement-based material so that the probe is vertical and the uncovered portion is at a predetermined position on the upper end side; The capacitance is measured at the two-core coating to measure the filling height, In the first detection probe, a capacitance is measured at a two-core uncoated portion provided at a predetermined position on the upper end side, It is preferable that the second detection probe measures the capacitance of the one-core uncoated portion and detects a predetermined position of the uncoated portion based on the change in capacitance between the two-core coated portion and the uncoated portion. Thirdly, in the method for managing filling of a cement-based material according to the first or second invention, in a state where the second detection probe is vertically installed in the filling space of the cement-based material, It is preferable to correct the filling height detected by detecting a change in capacitance in the coated portion of the two cores of the second detection probe to a height detected as a fixed point height where one core is coated and the other core is uncoated. Fourthly, in the method for managing filling of a cement-based material according to the first to third aspects of the present invention, it is preferable to start measurement by correcting an initial value of the capacitance in a state before filling of the cement-based material to 0 F. Fifth, in the method for managing the filling of cement-based materials according to the first to fourth aspects of the present invention, it is preferable to investigate in advance the filling status of the cement-based material and the change in capacitance associated with changes in the hardening temperature and hardening time of the cement-based material, obtain a proportional constant of the capacitance relative to the filling status, and reflect this in the detection of the actual filling status of the cement-based material. Sixth, in the method for managing the filling of cement-based materials according to the first to fifth aspects of the present invention, it is preferable to arrange one or more of the first detection probe and / or the second detection probe horizontally at a detection position for detecting the filling status of the cement-based material, and detect the filling status of the cement-based material based on a change in the electrostatic capacitance and / or the electric resistance of the covered and uncovered parts. Seventh, in the method for managing filling of a cement-based material according to the first to sixth aspects of the present invention, the two-core coated electric wire in the first detection probe and / or the second detection probe is preferably a flat cable. Eighth, in the method for managing filling of cement-based materials according to any one of the first to seventh aspects of the present invention, the method for measuring capacitance comprises measuring impedance and phase angle while applying an AC current to the first detection probe and / or the second detection probe, calculating capacitive reactance, and determining capacitance, and it is preferable that the AC current is in the range of 5 mVrms to 5 Vrms and the frequency is in the range of 1 KHz to 5 MHz. Ninth, in the method for managing the filling of cement-based materials according to any one of the first to eighth aspects of the present invention, it is preferable to connect a two-wire coated conductor to the end of the first detection probe and / or the second detection probe on the connection line side of the electrical input and measuring device using a connection connector. Tenth, in the method for managing the filling of cement-based materials of any one of the first to ninth inventions, it is preferable that the other end of the first detection probe and / or the second detection probe is connected to a measuring device using a conductor different from that of the detection probe. Eleventhly, in the method for managing filling of a cement-based material according to any one of the first to tenth aspects of the present invention, it is preferable that detection data on the filling state of the cement-based material is transmitted to a display device by a wireless communication device. Twelfthly, in the method for managing filling of a cement-based material according to any one of the first to eleventh aspects of the present invention, it is preferable that the filling status of the cement-based material is displayed on a screen. Effect of the Invention
[0021] According to the method for managing filling of cement-based materials of the present invention, the filling position of fresh concrete during filling can be detected easily and at low cost using a detection probe with a simple structure. This method is particularly effective for checking the filling height, etc., in places where the filling status of fresh concrete in an enclosed space cannot be visually observed, such as the secondary lining of a tunnel or the workroom of a pneumatic caisson. In addition, according to the method for managing filling of concrete, the filling status can be displayed precisely and visually, and detailed management of the filling steps, compliance with the filling speed, and pouring time can be performed. [Brief description of the drawings]
[0022] [Figure 1] FIG. 1(a) is a front view showing a state in which a cement-based material is filled in a coated portion of a first detection probe used in measurements in the cement-based material filling management method of the present invention, and FIG. 1(b) is a front view showing a state in which a cement-based material is filled up to an uncoated portion of the first detection probe. [Diagram 2] 1 is a graph showing the relationship between the length of fresh concrete filled in a covered electric wire and the capacitance. [Diagram 3] FIG. 1(a) is a schematic diagram of an embodiment in which the coating of two opposing feeder wires is removed in a first detection probe, and FIG. 1(b) is a graph showing the relationship between the length of the uncoated part in fresh concrete in FIG. 1(a) and the capacitance. [Figure 4] FIG. 1(a) is a schematic diagram of an embodiment of the first detection probe in which the uncoated portions are spaced apart from each other in a single-core, two-wire flat cable, and FIG. 1(b) is a graph showing the relationship between the length of the uncoated portion separation in fresh concrete in FIG. 1(a) and the capacitance. [Diagram 5]FIG. 1(a) is a schematic diagram showing an embodiment of the second detection probe in which the coating part of one core of the feeder wire has been removed, and FIG. 1(b) is a graph showing the relationship between the length of the uncoated part in fresh concrete in FIG. 1(a) and the capacitance. [Figure 6] 11 is a graph showing the relationship between the filling height of fresh concrete in a feeder line and the filling and capacitance in a first detection probe. [Figure 7] 13 is a graph showing the relationship between the filling height of fresh concrete in the feeder line and the filling and capacitance in the second detection probe. [Figure 8] 1A is an oblique view of the case where the filling height of fresh concrete and the filling at the top end are measured using the detection probe of the present invention in a space in the secondary lining of a tunnel, and FIG. 1B is a cross-sectional view of FIG. 1A. [Figure 9] This is a front cross-sectional view of the space inside a work chamber of a pneumatic caisson, showing the height of fresh concrete filling and the filling at the top end of the work chamber being measured using the detection probe of the present invention. [Figure 10] FIG. 1 is a perspective view showing an embodiment in which a plurality of single-wire, two-core detection probes having detection units are installed longitudinally at the top end of a tunnel secondary lining. [Figure 11] This is a cross-sectional view and a plan view showing an embodiment in which multiple single-wire, two-core detection probes with detection units are installed on the ceiling of a work chamber in a pneumatic caisson. [Figure 12] (a) is the electrical resistance of a covered electric wire in fresh concrete, and (b) is the electrical resistance of an uncovered electric wire in fresh concrete. [Figure 13] FIG. 2A is a plan view of a detection probe using a flat cable provided with a plurality of pairs of uncoated portions, and FIG. 2B is a cross-sectional view taken along the line AA of FIG. [Figure 14] FIG. 1A is a front view showing electric wires connected to each other using a connector to form a detection probe, and FIG. [Figure 15] FIG. 13 is a front view showing an embodiment in which a coaxial cable is connected to the other end of the detection probe. [Figure 16] FIG. 11 is a perspective view of an embodiment in which data measured by a measuring device is transmitted to a display device by a wireless device. [Figure 17] (a) is a diagram showing the screen display of the filling height of fresh concrete in the secondary lining of a tunnel, and (b) is a diagram showing the filling status of the top end of the fresh concrete in the secondary lining of a tunnel. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0023] An embodiment of the method for managing filling of cement-based materials according to the present invention will be described in detail below with reference to the drawings. Fig. 1(a) is a front view showing a state in which concrete is filled in the coated part of a first detection probe used for measurement in the method for managing filling of cement-based materials according to the present invention, and (b) is a front view showing a state in which concrete is filled up to the uncoated part of the first detection probe. Fig. 5(a) is a schematic diagram showing an embodiment in which the coating part of one core is removed in the feeder wire of the second detection probe. It should be noted that the present invention is not limited to this embodiment.
[0024] The method for managing the filling of a cement-based material of this embodiment is a method for managing the filling of a cement-based material 20, in which a detection probe 1 consisting of a two-core coated wire is placed in the filling space of the cement-based material 20, and the detection probe 1 measures the electrostatic capacitance to detect the filling status of the cement-based material 20.
[0025] In addition, in the method for managing the filling of cement-based materials of this embodiment, at least one of the following is used: a first detection probe 12(1) in which an uncoated portion 11 is provided in the middle of one core of a two-core insulated electric wire, with the coating 10 of each core removed, and one end of the two cores is insulated, with the other end used as an electrical input and a connection line for a measuring device 3, and the coating portion 10 and the uncoated portion 11 are integrally formed; or a second detection probe 13(1) in which an uncoated portion 11 is provided in the middle of one core of a two-core insulated electric wire, with the coating portion 10 of each core removed, and one end of the two cores is insulated, with the other end used as an electrical input and a connection line for a measuring device 3, and the coating portion 10 and the uncoated portion 11 are integrally formed.
[0026] The detection probe 1 of this embodiment is one in which the covering 10 of the two or one conductor of a two-core covered electric wire is partially removed, and examples thereof include an embodiment of a first detection probe 12(1) in which the covering 10 of both conductors of a two-core feeder wire is removed to form an uncovered portion 11 as shown in Fig. 3(a), and an embodiment of a second detection probe 13(1) in which a part of the covering 10 of one of the two wires is removed to form an uncovered portion 11 as shown in Fig. 5(a). In both the first detection probe 12(1) and the second detection probe 13(1), one end of each of the two wires is insulated, and the other end is formed as a connection line for electrical input and a measuring device 3.
[0027] For the detection probe 1, any electric wire can be used as long as it is a two-core coated electric wire, and there is no limitation thereto, but for example, a state in which the coatings face each other and are spaced apart can be achieved by removing a certain length of the coating 10 of two parallel wires facing each other in a feeder wire to form an uncoated portion 11. Also, in a single-wire two-core coated electric wire, as shown in Fig. 4(a), an embodiment can be exemplified in which a certain length of the coating 10 is removed from positions spaced apart from each other and shifted forward and backward from the two parallel wires to form the uncoated portion 11.
[0028] Furthermore, in a typical insulated electric wire with two twisted wire cores, a certain length of the insulated portion 10 at a position spaced apart from the front and rear of the two parallel wires can be removed to form the uninspired portion 11. When the twisted wire is thin, the strength of the uninspired portion 11 can be increased by soldering multiple twisted wires together, or by cutting the uninspired portion 11 and reconnecting it using a metal crimp sleeve or the like. The other end of the electric wire is connected directly to the measuring device 3 as the input of electricity and the connection line for the measuring device 3.
[0029] The detection probe 1 can be used singly or in multiples depending on the location to be detected. It is sufficient that one end of each of the two cores is insulated, and the insulation method can be a method of insulating the end with an insulating resin material such as silicon resin, or by attaching insulating tape. In addition, a parallel feeder wire is particularly suitable as the feeder wire.
[0030] The removal range, removal locations, and number of removals of the covering portion 10 in the detection probe 1 can be appropriately determined depending on the intended use of the detection probe 1, etc., but it is preferable to provide one location for each of the two cores in the first detection probe 12(1) and multiple locations for one core in the second detection probe 13(1).
[0031] The detection probe 1 of the present embodiment can be installed in any space 2 filled with a cementitious material 20, and specific examples include installation in a concrete-filled space 2 for building foundation construction, a cement-filled space 2 in a tunnel lining, a filled space 2 in a pneumatic caisson construction method, etc. Examples of the cementitious material 20 filled in the filled space 2 in the present invention include cement, concrete, mortar, etc.
[0032] FIG. 1(a) is a front view showing a state in which a first detection probe 12(1) of this embodiment is installed in a filling space 2 and a cement-based material 20 is filled up to a part of a coated portion 10 of the first detection probe 12(1), and FIG. 1(b) is a front view showing a state in which the cement-based material 20 is further filled up to an uncoated portion 11.
[0033] The first detection probe 12(1) of the embodiment shown in Fig. 1 is the first detection probe 12(1) of the embodiment shown in Fig. 3(a), and both of the two-core uncoated portions 11 are provided adjacent to each other at the same distance from the lower end. That is, the uncoated portions 11 are formed in a state where the conductor is exposed and the uncoated portions 11 are opposed to each other and spaced apart from each other.
[0034] Then, this first detection probe 12(1) is placed in the filling space 2, and an alternating current with a measurement frequency within an appropriate range is applied to the two-core detection probe 1. When the cementitious material 20 is filled in the state shown in FIG. 1(a) to FIG. 1(b), the capacitance between the two cores is measured by the measuring device 3, and the filling status of the filled cementitious material 20 is detected based on the difference in capacitance between the coated portion 10 and the uncoated portion 11.
[0035] In the present invention, the method for measuring capacitance is to measure the impedance and phase angle of the first detection probe 12(1) or the second detection probe 13(1) to calculate the capacitive reactance and substitute it into the following equation to obtain the capacitance C. XC=1 / (2πfC) (XC: capacitive reactance, f: frequency of AC voltage, C: capacitance) As the measuring device 3, a device capable of measuring the capacitance of an input AC signal, such as an LCR meter, a multimeter, or an impedance analyzer, can be suitably used. The conditions for applying the AC current for measurement are preferably 5 mVrms to 5 Vrms and the measurement frequency is preferably in the range of 1 KHz to 5 MHz. In addition, it is preferable to use a measuring device 3 that has a capacitance measurement range of 1 pF to 500 nF and can automatically switch the unit display from pF to nF.
[0036] The following describes capacitance measurement experiments (Experiments 1 to 6) carried out using the first and second detection probes 12(1) and 13(1) of the above embodiment.
[0037] <Experiment 1> In experiment 1, the capacitance was measured when fresh concrete 20 was filled into the coated and uncoated parts 10 and 11 of different electric wires in the first detection probe 12(1). The capacitance was measured with a measurement AC signal of 0.63 Vrms and a measurement frequency of 100 KHz. The same was true for the subsequent experiments.
[0038] Figure 2 is a graph showing the results of the relationship between the length of fresh concrete 20 filled into the covered electric wire and the capacitance. In the graph of Figure 2, (1) is the feeder wire, and the capacitance C (pF) of the feeder wire in fresh concrete 20 increases almost in proportion to the length of the electric wire immersed in fresh concrete 20, and the increase in capacitance C (pF) / m per unit length was about 97 pF / m.
[0039] Also, (2) is a single-wire 2-core parallel wire, and the capacitance C (pF) of the single-wire 2-core parallel wire in fresh concrete 20 increases almost in proportion to the length of the wire immersed in fresh concrete 20, and the increase in capacitance C (pF) / m per unit length was about 54 pF / m. In this experiment 1, the capacitance values of the feeder wire and the single-wire 2-core parallel wire in the environment before they were immersed in fresh concrete 20 were subtracted to set the initial value to zero (0F).
[0040] <Experiment 2> In experiment 2, the relationship between the length of the uncoated portion 11 in the first detection probe 12(1) and the capacitance was confirmed. Fig. 3(a) is a schematic diagram showing the relationship between the length of the uncoated portion 11 of the detection probe 1 in which the coating portions 10 of the two opposing feeder wires in the first detection probe 12(1) have been removed, and the capacitance was measured in this experiment 2 when fresh concrete 20 was filled from the bottom to the top for four cases in which the length L1 of the uncoated portion 11 in the detection probe in Fig. 3(a) was 5 mm, 10 mm, 15 mm, and 20 mm.
[0041] FIG. 3(b) is a graph showing the results of investigating the relationship between the length of the uncoated portion 11 in the fresh concrete 20 in FIG. 3(a) and the capacitance. The results of Experiment 2 show that the capacitance was 10 pF in all four cases when the coated portion 10 was filled, but increased significantly to 60-300 nF when the uncoated portion 11 was filled. This results in a phenomenon in which the capacitance increases suddenly when the filling position of the fresh concrete 20 moves from the coated portion 10 to the uncoated portion 11 of the wire. This confirms that it is possible to determine whether the fresh concrete 20 is immersing the coated portion 10 or the uncoated portion 11 by measuring the capacitance.
[0042] In addition, the length L1 of the uncovered portion 11 and the capacitance are approximately proportional to each other. Thus, it can be seen that the value of the capacitance when the fresh concrete 20 is filled varies depending on the length of the uncovered portion 11.
[0043] <Experiment 3> In experiment 3, the relationship between the length of the uncoated portion 11 and the capacitance in the first detection probe 14(1) of another embodiment was confirmed. Fig. 4(a) is a schematic diagram of an embodiment in which the uncoated portions 11 are spaced apart from each other in a single-core two-wire flat cable in the first detection probe 14(1) of another embodiment. In this experiment 3, the length of the uncoated portion 11 was set to 5 mm in common, and the spacing length of the uncoated portion 11 was set to 5 mm, 10 mm, 15 mm, and 20 mm, and the capacitance was measured when fresh concrete 20 was filled from the bottom to the top in each of the four cases.
[0044] FIG. 4(b) is a graph showing the results of investigating the relationship between the distance between the uncovered parts 11 in the fresh concrete 20 in FIG. 4(a) and the capacitance. According to the results of Experiment 3, the capacitance was 40 pF when the covered parts 10 were filled in all four cases, but it increased significantly to 70-60 nF when the uncovered parts 11 were filled. Also, the length L1 of the uncovered parts 11 and the capacitance are almost inversely proportional. Thus, the value of the capacitance when the fresh concrete 20 is filled differs depending on the distance between the uncovered parts 11.
[0045] As described above, it has been confirmed that the first detection probe 14(1) of another embodiment shown in FIG. 4(a) can also detect that the fresh concrete 20 has been filled up to the position of the uncoated portion 11 of the wire due to the large difference in capacitance between the coated portions 10 and the uncoated portions 11 when the fresh concrete 20 is filled into the filling space 2.
[0046] <Test 4> In experiment 4, the relationship between the length of the uncoated portion 11 in the second detection probe 13(1) and the capacitance was confirmed. Fig. 5(a) is a schematic diagram of an embodiment of the second detection probe 13(1) in which the coated portion 10 is removed from the middle of one core in the feeder wire. In this experiment 4, the capacitance was measured for four cases in which the length L1 of the uncoated portion 11 was 5 mm, 10 mm, 15 mm, and 20 mm, when fresh concrete 20 was filled from the bottom to the top, and the position where the fresh concrete 20 was immersed in the uncoated portion 11 moved from the coated portion 10.
[0047] FIG. 5(b) is a graph showing the results of investigating the relationship between the length of the uncoated portion 11 in the fresh concrete 20 in FIG. 5(a) and the capacitance. According to the experimental results, in all cases, when moving from the coated portion 10 to the uncoated portion 11, the capacitance increased by 9 to 10. Taking into consideration the above-mentioned formation and installation method of the detection probe 1, when the filling space 2 is filled with fresh concrete 20, it is possible to detect that the fresh concrete 20 has been filled up to the position of the uncoated portion 11 of the electric wire due to the large difference in capacitance between the coated portions 10 and the uncoated portions 11.
[0048] Furthermore, the length L1 of the uncovered portion 11 and the capacitance are approximately proportional to each other. In this manner, the value of the capacitance when the fresh concrete 20 is filled varies depending on the length of the uncovered portion 11.
[0049] <Test 5> In experiment 5, the relationship between the capacitance in the feeder wire of the first detection probe 12(1) and the filling height and filling of the fresh concrete 20 was confirmed. FIG. 6 is a graph showing the relationship between the capacitance in the feeder wire and the filling height and filling of the fresh concrete 20 in filling using the first detection probe 12(1). This graph shows the change in capacitance when the capacitance is measured at the covered part 10 in the lower part and the non-covered part 11 in the upper part in a case where the filling space 2 is closed and has a height space and a top end position inside, and an electric wire is installed to detect the filling height of the fresh concrete 20 and the filling above, and measurements are made.
[0050] As fresh concrete 20 is gradually filled upward into the covered portion 10 of the detection probe 1, the air in the filling space 2 around the covered portion 10 of the detection probe 1 is replaced by fresh concrete 20 from bottom to top, and it is assumed that the capacitance of the covered portion 10 of the detection probe 1 increases in proportion to the length of time that it is immersed in the fresh concrete 20, and when the fresh concrete 20 then fills the uncovered portion 11, the capacitance becomes significantly larger.
[0051] In an actual experiment, as shown in FIG. 6, the relationship between the capacitance of the coated portion 10 of the wire and the height is such that, as fresh concrete 20 is filled, the height is measured at the coated portion 10 at the lower part of the wire. At a filling height of 150 cm, the capacitance is 152 pF (101 pF / m), and when the fresh concrete 20 reaches a position 2 cm into the uncoated portion 11 at a height of 175 cm, the capacitance becomes 20 nF (1000 nF / m).
[0052] As shown in the results, the capacitance at the position of the wire in the uncoated portion 11 is approximately 10,000 times that at the position of the wire in the coated portion 10, and it is found that the capacitance of the uncoated portion C0 >> the capacitance of the coated portion CS, meaning that the capacitance of the uncoated portion 11 is significantly larger. From this, it can be determined that when the filling position of the fresh concrete 20 moves from the coated portion 10 of the wire to the uncoated portion 11, the capacitance increases suddenly, and fresh concrete 20 has been filled in the uncoated portion 11.
[0053] In actual measurements, since the characteristics of cementitious material 20 such as fresh concrete (concrete before hardening) and fresh mortar (mortar in an unhardened state) are not uniform due to the influence of the materials used, the mix ratio, the water content, etc., it is desirable to determine the proportional constant between the capacitance and the immersion length of first detection probe 12(1) and second detection probe 13(1) in covered portion 10 before carrying out the measurement, and also to determine the capacitance value at uncovered portion 11 of first detection probe 12(1) and second detection probe 13(1). In addition, any measuring device 3 that can measure by applying an AC voltage can be used for measuring electrical resistance without any restrictions.
[0054] <Experiment 6> In experiment 6, the relationship between the capacitance of the feeder line of the second detection probe 13(1) and the filling height and filling of the fresh concrete 20 was confirmed. Figure 7 is a graph showing the relationship between the filling height of the fresh concrete 20 in the feeder line and filling and the capacitance when filling using the second detection probe 13(1). Figure 7 shows the change in capacitance when the capacitance is measured from the covered part 10 at the lower part, and also when the capacitance is measured after passing the uncovered part 11 on the way and the fresh concrete 20 is immersed in the covered part 10, the uncovered part 11, and the covered part 10.
[0055] In this case, the capacitance of the covered portion 10 of the second detection probe 13(1) increases in proportion to the length of immersion in the fresh concrete 20. Since the uncovered portion 11 has one core on one side, the capacitance increases when the fresh concrete 20 is filled into the uncovered portion 11. However, with reference to the graph in Figure 5(b), it is assumed that the capacitance is not as large as in the case of Figure 7, where the uncovered portion 11 has two cores.
[0056] In an actual experiment, as shown in FIG. 7, based on the relationship between the capacitance and height of the coated part 10 of the wire, as fresh concrete 20 is filled, the height is measured at the coated part 10 of the lower part of the wire, and as the fresh concrete 20 is gradually filled, the filling height and the capacitance become proportional, and after the capacitance reaches a value of 90 pF at a filling height of 90 cm, when one core is at a position 2 cm in length from the uncoated part 11, the capacitance becomes 100 pF, and then it moves to the uncoated part 11, and the filling height and capacitance become proportional again, and a capacitance of 160 pF is detected up to a filling height of 160 cm.
[0057] At this time, by installing the second detection probe 13(1) so that the uncoated part 11 of one core is at a fixed height, it is possible to check and correct the filling height of the fresh concrete 20 during filling, and it is possible to improve the detection accuracy by responding to installation errors of the detection probe 1 and changes in the proportionality constant due to hardening of the fresh concrete 20.
[0058] An embodiment in which the detection probe 1 is used in tunnel construction will be described in detail below. Fig. 8(a) is a perspective view showing a state in which the detection probe 1 of the present invention is used to measure the filling height of the concrete 20 in the filling space 2 of the concrete 20 in the secondary lining of a tunnel 4 and the filling at the tunnel top end 41. Specifically, in the secondary lining of the tunnel 4, the detection probe 1 with two single wire cores is disposed on a waterproof sheet 42 in the circumferential direction, and the capacitance is measured at the covered part 10 in the lower part, and by extension, the capacitance is measured at the uncovered part 11 at the tunnel top end 41.
[0059] The detection probe 1 is arranged in the circumferential direction toward the top end 41 on the waterproof sheet 42 placed on the excavation surface for the required number of times, and is then aligned in the longitudinal direction from the tunnel top end 41 and connected to the measuring device 3 and display device 5 outside the gable formwork side 43. The detection probe 1 can be arranged on the waterproof sheet 42 by welding a band-shaped mounting member to the waterproof sheet 42 to support the detection probe 1, or by attaching it using tape or the like.
[0060] Fresh concrete 20 is filled between the waterproof sheet 42 and the center 44, and as the concrete 20 is gradually filled above the covered portion 10, the capacitance increases, and the filling height of the concrete 20 in the circumferential direction can be measured based on this value. This measurement makes it easier to manage the construction so that the filling height is equal on the left and right. After detection of the filling height of the concrete 20 has been completed, the capacitance is measured with the separated uncovered portion 11 of the further extended detection probe 1 to detect the filling of concrete 20 at the position of the uncovered portion 10 at the top end 41. This detection makes it possible to reliably confirm that the top end 41 has been filled.
[0061] Since the difference in filling height varies depending on the fluidity of the concrete 20, it is preferable to determine the number of detection probes 1 according to the fluidity of the concrete 20 used, and usually, it is considered to install about 2 to 4 probes on each side. In this case, the number of filling detection points at the top end 41 will be 4 to 8, including the detection probes 1 on both sides. Filling detection at the top end 41 can also be detected by switching the measurement target to electrical resistance and measuring the electrical resistance.
[0062] Furthermore, if a reinforcing bar is installed between the waterproof sheet 42 and the center 44, the detection probe 1 can also be disposed on the reinforcing bar. The reinforcing bar is installed to increase the strength of the filled concrete 20 as a structure, and is installed when a high load is applied to the tunnel 4. The detection probe 1 can be attached to the reinforcing bar with a binding wire or the like.
[0063] In addition, when measuring, the relative dielectric constant of the fresh concrete 20 depends on the temperature, and the higher the temperature of the fresh concrete 20, the lower the relative dielectric constant, and it is considered that the proportionality constant may change slightly. In addition, when filling the fresh concrete 20, if it takes a long time to fill depending on the filling conditions, the fresh concrete 20 already filled in the lower part may harden over time, causing a decrease in water content, and the proportionality constant between the height and the capacitance may change slightly. Therefore, in actual construction, it is preferable to find out the proportionality constant between the height and the capacitance in advance for the fresh concrete 20 to be used, taking into account the temperature and hardening time, and to reflect this in the calculation of the actual height measurement.
[0064] Fig. 8(b) is a cross-sectional view of Fig. 8(a). In this embodiment, the covered portion 10 of the detection probe 1 is disposed along the waterproof sheet 42 so as to face from the bottom to the top, and the uncovered portion 11 is disposed at the position of the tunnel top end 41. Since the covered portion 10 is disposed at a position on an arc, the relationship between the immersion length of the covered portion 10 and the filling height is obtained in advance from the cross-sectional shape, and the filling height of the fresh concrete 20 can be obtained.
[0065] 9 is a front cross-sectional view of the detection probe 1 of the present invention measuring the filling height of the fresh concrete 20 and the filling of the top end of the work chamber 61 in the space 2 in the work chamber during construction of the pneumatic caisson 6. Usually, after the pneumatic caisson 6 has completed sinking, the work chamber 61 is filled with fresh concrete 20, but in the case of a caisson with a large cross section, the monitoring camera 62 may not be able to capture every corner of the work chamber 61 during the filling work. Therefore, instead of a steel staff set up vertically, the detection probe 1 of the present invention is installed on the side wall of the work chamber 61 at the ceiling or ceiling corner of the work chamber 61 to measure the filling height of the buried concrete 20, and then the non-covered part 11 is installed on the ceiling or ceiling corner of the work chamber 61 to check the filling status.
[0066] As shown in Figures 8(a) to 9, in a closed filled space 2 during the construction of a tunnel 4 or a pneumatic caisson 6, the height of fresh concrete 20 can be measured by measuring the capacitance, and at the same time, the filling of the top end 41 or ceiling can be detected.
[0067] 10 is a perspective view of a plurality of single-wire two-core detection probes 1 having detection units installed in the longitudinal direction at the top end 41 of the secondary lining of a tunnel 4. When fresh concrete 20 is filled at the tunnel top end 41 and between each of the uncovered parts 11, the capacitance of the fresh concrete 20 is detected to detect that the fresh concrete 20 has been filled at each position of the top end 41. The detection probe 1 can be attached to the waterproof sheet 42 by welding a band-shaped object to the waterproof sheet 42 to support the detection probe 1, or by attaching it using tape or the like.
[0068] 11 is a cross-sectional view and a plan view of a plurality of single-wire two-core detection probes 1 with detection units installed on the ceiling of a work chamber 61 in a pneumatic caisson 6. When the ceiling of the work chamber 61 is filled with filler concrete 20 and the filler concrete 20 is filled between each of the uncovered parts 11, it is possible to detect that the filler concrete 20 has been filled in each position of the ceiling and haunch parts of the work chamber 61 by detecting the capacitance of the filler concrete 20. The detection probes 1 can be attached to the ceiling of the work chamber 61 by fastening them in places with bands or the like to concrete nails driven into the ceiling.
[0069] Fig. 12(a) shows the electrical resistance of a covered electric wire in fresh concrete 20. It is a graph showing the relationship between the length of the covered electric wire and the electrical resistance when filled with fresh concrete 20. When fresh concrete 20 is filled into the covered electric wire having only the covering portion 10 in Fig. 12(a), the electrical resistance is 250 kΩ when the filling length of the fresh concrete 20 is 20 cm, and 49 kΩ when it is 90 cm, and the electrical resistance is almost inversely proportional to the increase in the filling length of the fresh concrete 20.
[0070] Figure 12(b) shows the electrical resistance of an uncoated electric wire in fresh concrete 20. It is a graph showing the relationship between the length of the uncoated electric wire and the electrical resistance when filled with fresh concrete 20. When fresh concrete 20 is filled into the uncoated electric wire in Figure 12(b) that is only uncoated, the electrical resistance is 25 Ω at a fresh concrete 20 filling length of 20 cm, and 6 Ω at 90 cm, and the electrical resistance is roughly inversely proportional to the increase in the filling length of fresh concrete 20.
[0071] In this way, when comparing the values of electrical resistance when fresh concrete 20 is filled in each of the covered electric wire and the uncovered electric wire, the electrical resistance of the uncovered electric wire is much smaller than the electrical resistance of the covered electric wire. From this, when the filling position of the fresh concrete 20 moves from the covered part 10 of the electric wire to the uncovered part 11, the electrical resistance suddenly decreases, and it can be determined that the fresh concrete 20 has been filled in the uncovered part 11. It can also be said that the value of electrical resistance is inversely proportional to the filling length of the fresh concrete 20 in each of the covered electric wire and the uncovered electric wire. Therefore, it can be seen that it is possible to detect the filling of fresh concrete 20 at a single or multiple positions of the tunnel top end 41, the ceiling in the work room 61 of the pneumatic caisson 6, and the haunch part by electrical resistance as well as capacitance.
[0072] Fig. 13(a) is a plan view of a detection probe 1 using a flat cable provided with multiple pairs of uncoated portions 11. This is an example of a detection probe 1 that can be used in the embodiments of Figs. 10 and 11. A plurality of uncoated portions 11 are formed by shifting the uncoated portions 11 for a pair of two-core electric wires. Since the uncoated portions 11 are parallel to each other at a certain distance, similar detection portions are formed by determining the length of the uncoated portions 11 and the distance between adjacent uncoated portions 11, and therefore individual differences in detection values can be minimized. The uncoated portions 11 are formed at locations where the filling position of the fresh concrete 20 is detected.
[0073] Fig. 13(b) is a cross-sectional view taken along line AA in Fig. 13(a). This embodiment is for 10 pairs of single wires, but the number of pairs required for the number of filling detection points is used. The inside is composed of a conductor and an insulator that insulates the conductor. This cross section shows a cross section with one coated portion 10 removed, and the capacitance or electrical resistance is measured by using two uncoated portions 11 as a pair of coated portions 10.
[0074] Furthermore, feeder wires, particularly parallel feeder wires, are suitable as electric wires for use in the detection probe 1. In parallel feeder wires, there is a certain distance between adjacent copper wires, so even if the non-coated portions 11 are formed facing each other, the copper wires do not come into contact with each other, and by determining the length of the non-coated portions 11, similar detection portions are formed, so that individual differences in detection values can be minimized.
[0075] Fig. 14(a) is a front view of an example in which electric wires are connected to each other using a connector 7 to form a detection probe 1. Fig. 14(b) is a plan view of an embodiment in which electric wires are connected to each other using a connector 7 to form a detection probe 1. In Figs. 14(a) and 14(b), the electric wires are connected by shifting the connections back and forth, inserting a plug-side housing 71 having a non-coated portion 11 formed thereon into a receptacle-side housing 72, and connecting contact terminals that are crimp-connected to the non-coated portion 11 electric wires.
[0076] The detection probe 1 is attached to a location where the filling detection of the cement-based material 20 or the height measurement and filling detection are performed, but since an electric wire is connected from the insulating part at the end of the detection probe 1 to the measuring device 3, the detection probe 1 may become long depending on the measurement and detection conditions. In this case, it is considered that the detection probe 1 is difficult to handle because it is long, and installation is time-consuming and inefficient. In consideration of such a case, it is possible to deal with it by connecting the electric wires using a connector 7 to make a long detection probe 1.
[0077] The connection using the above-mentioned connector 7 is only a part of the embodiment, and other connectors can be used for connection as long as they can provide a reliable connection.
[0078] In this example, the uncoated portion 11 is formed on the electric wire, but the uncoated portion 11 may be formed in another manner by connecting the conductive connection terminal 73 in an exposed state. The exposed portion becomes the uncoated portion 11 and can detect the filling. In addition, the electric wires of the flat cable detection probe 1 can also be connected together in a waterproof state using the connector 7.
[0079] In the present invention, the other end of the detection probe 1 and the measurement device 3 can be connected using a conductor different from the detection probe 1. FIG. 15 is a front view showing a state in which the other end of the detection probe 1 is connected to a coaxial cable 15 as a connection line. The other end of the detection probe 1 (the other end of the terminal in which one end of each of the two cores is insulated) may be connected directly to the measurement device 3 as a feeder line (two-core coated wire) as the detection probe 1 as shown in FIG. 1, or may be connected to the measurement device 3 via another conductor different from the feeder line. Examples of the other conductor different from the feeder line include another two-core coated wire that is thinner and easier to handle than the feeder line, and a coaxial cable that is less susceptible to electromagnetic waves coming from the outside.
[0080] In particular, since the measurement method of the present invention uses high frequencies in the range of 1 KHz to 5 MHz, it is preferable to use a coaxial cable 15 used as a cable for transmitting high frequency signals, taking into consideration cases where the conductor distance is long or where electromagnetic waves with frequencies close to the measurement frequency are generated in the surrounding area.
[0081] 15, a coaxial cable 15 may be used as a connection line to the detection probe 1, and further connected to the measuring device 3 via a vinyl wire 16. In this embodiment, connectors 151 are provided on both ends of the coaxial cable 15, one end of the coaxial cable 15 is connected to the other end of the detection probe 1 via the connector 151, and the other end of the coaxial cable 15 is connected to the vinyl wire 16 via the connector 151. Note that when multiple detection probes 1 are used or when a flat cable is used, a multi-core coaxial cable can be used.
[0082] 16 is a perspective view of an embodiment in which data measured by a measuring device 3 is transmitted to a display device 5 by a wireless communication device 8. This is a case in which the filling height is measured in the secondary lining of a tunnel 4 and the filling at the tunnel top end 41 is detected. The measuring device 3, which detects with a detection probe 1, is installed on the outside of the end of the tunnel, and the measurement data is wirelessly transmitted by the wireless communication device 8 to a display device 5 such as a personal computer.
[0083] When filling the work chamber 61 of the pneumatic caisson 6 with the filling concrete 20, the measuring device 3 is installed in the man shaft 63, which is an entrance for people to the caisson, or in the material shaft, through which buckets of soil and sand, equipment inside the caisson, etc. are carried in and out, and the measurement data can be transmitted wirelessly to the display device 5 such as a personal computer by the wireless communication device 8 in the same manner. The wireless communication device 8 can also be used in filling the top end 41 of the secondary lining of the tunnel 4 at multiple locations, and in filling the top end 41 of the pneumatic caisson 6 at multiple locations with the filling concrete 20. In this way, by using the wireless communication device 8, communication in a narrow space can be changed from wired to wireless, which eliminates the risk of cutting the electric wire and improves workability. Of course, the wireless communication device 8 can also be used in combination with the electric wire connector 7.
[0084] FIG. 17(a) is an explanatory diagram showing the filling height of fresh concrete 20 in the secondary lining of tunnel 4 displayed on the monitor 5. Here, a pair of electrodes are attached to the inside of the waterproof sheet 42 at three points on the existing side, the center, and the gable side, and are measured. The upper figure is a view from the side of the tunnel 4, and the lower figure is a view from the cross section of the tunnel 4. By displaying and illustrating the height of the fresh concrete 20 in this way, the filling status can be grasped in real time. In this case, since the cross section of the tunnel 4 is arch-shaped, the relationship between the length of the detection probe 1 immersed in the fresh concrete 20 and the rise height at that time is calculated in advance according to the arch shape, and the filling height is calculated.
[0085] Fig. 17(b) is an explanatory diagram showing the filling status of the top end 41 of fresh concrete 20 in the secondary lining of the tunnel 4 displayed on the monitor 5. At this point in time, there are 10 locations (No. 1 to No. 10) along the length of the top end 41 that are scheduled for detection, and the five colored locations (No. 1, No. 2, No. 5, No. 6, No. 8) show the filled status.
[0086] In this way, by displaying the filling height and the filling status of the top end 41 on a screen using a display such as a personal computer, the progress of filling of the fresh concrete 20 can be displayed precisely and visually. This can be useful for managing the filling steps, compliance with the filling speed, pouring time, etc. Also, when pouring by switching the valves of the pouring inlet piping, the pouring height of the concrete at the pouring location can be known at the same time, so the timing of switching each valve can be grasped in a timely manner, allowing efficient construction.
[0087] The embodiment of the present invention has been described above, but the method for managing the filling of cement-based materials using the two-core detection probe 1 according to the present invention can be used for measuring the filling height of cement-based materials and for detecting filling at a desired position, in addition to the above-mentioned embodiment, to manage the filling of cement-based materials in road piers, box culverts, and forms in construction work, and the detection of a desired position can also be applied to detecting the filling of grout in PC sheath pipes, detecting the filling of air mortar in tunnel backfilling, detecting the filling of cement-based materials on the underside of CFT diaphragms and precolumns, and checking the filling of high-density reinforcement and other places that are difficult to visually inspect. It is also effective for detecting grout filling at places that are difficult to visually inspect.
[0088] Furthermore, the present invention is suitable for a method of controlling the filling of cement-based materials including fresh concrete and fresh mortar, but can also be applied to measuring the height and controlling the filling of liquids such as water and solutions. [Explanation of symbols]
[0089] 1. Detection probe 10 Covering part 11 Uncoated part 12 First detection probe 13 Second detection probe 14. First Detection Probe of Other Embodiments 15 Coaxial Cable 151 Connector 16 Vinyl Wire 2 Filling space 20 Cementitious materials (concrete, fresh concrete) 3. Measurement equipment 4. Tunnels 41 Tunnel top 42 Tarpaulin 43 Gable side 44 Centre 45 Natural ground 5. Display device (monitor) 6 Pneumatic caisson 61 Work Room 62 Surveillance Camera 63 Manschaft 7 Connectors 71 Plug side housing 72 Receptacle side housing 73 Connection terminal 8. Wireless communication devices
Claims
1. A method for controlling filling of a cement-based material, comprising: disposing a detection probe made of a two-core coated electric wire in a filling space of the cement-based material; and detecting a filling state of the cement-based material by measuring a capacitance using the detection probe, A first detection probe in which an uncoated portion is provided in the middle of a two-core coated electric wire by removing the coating of each of the two cores, one end of the two cores is insulated, and the other end is used as a connection line for inputting electricity and for a measuring device, and the coated portion and the uncoated portion are integrally formed; and / or a non-coated portion is provided at the middle of one core of a two-core coated electric wire by removing the coating, and a terminal on one end of each of the two cores is insulated, and the other end is used as a connection line for inputting electricity and for a measuring device, and a second detection probe is installed in which the coated portion and the non-coated portion are integrally formed; A method for managing the filling of a cement-based material, comprising: applying an AC voltage to the first detection probe and / or the second detection probe when filling the cement-based material into the filling space of the cement-based material, measuring a capacitance between the two cores, and detecting a filling status of the cement-based material based on a change in the capacitance value.
2. The first detection probe and / or the second detection probe are installed in the filling space of the cement-based material so that they are vertical and the uncovered portion is at a predetermined position on the upper end side; The capacitance is measured at the two-core coating to measure the filling height, In the first detection probe, a capacitance is measured at a two-core uncoated portion provided at a predetermined position on the upper end side, The method for managing the filling of cement-based materials according to claim 1, characterized in that the second detection probe measures the capacitance of the one-core uncoated portion, and detects a predetermined position of the uncoated portion based on a change in the capacitance of the two-core coated portion and the capacitance of the uncoated portion.
3. In a state where the second detection probe is vertically installed in the filling space of the cement-based material, The method for managing the filling of cement-based materials as described in claim 1, characterized in that the filling height detected by detecting a change in capacitance in the covered portion of the two cores of the second detection probe is corrected to a height detected by a fixed point height where one core is the covered portion and the other core is the uncovered portion.
4. 2. The method for managing filling of a cement-based material according to claim 1, wherein an initial value of the capacitance in a state before filling of the cement-based material is corrected to 0 F and measurement is started.
5. The method for managing the filling of cement-based materials according to claim 1, characterized in that the filling status of the cement-based material and the change in capacitance due to changes in the hardening temperature and hardening time of the cement-based material are examined in advance, a proportional constant of the capacitance to the filling status is obtained, and this is reflected in the detection of the actual filling status of the cement-based material.
6. The method for managing the filling of cement-based materials according to claim 1, characterized in that one or more of the first detection probe and / or the second detection probe are horizontally arranged at a detection position for detecting the filling status of the cement-based material, and the filling status of the cement-based material is detected based on a change in the electrostatic capacitance and / or the electric resistance of the covered and uncovered parts.
7. 2. The method for managing filling of a cement-based material according to claim 1, wherein the two-core coated electric wire in the first detection probe and / or the second detection probe is a flat cable.
8. The method for managing filling of cement-based materials according to claim 1, characterized in that the method for measuring capacitance comprises measuring impedance and a phase angle while applying an AC current to the first detection probe and / or the second detection probe, calculating a capacitive reactance, and determining the capacitance, wherein the AC current is in the range of 5 mVrms to 5 Vrms and has a frequency in the range of 1 KHz to 5 MHz.
9. The method for managing the filling of cement-based materials as described in claim 1, characterized in that another two-core insulated electric wire is connected to the end of the first detection probe and / or the second detection probe on the electrical input and measurement device connection side using a connection connector.
10. The method for managing the filling of cement-based materials as described in claim 1, characterized in that the other end of the first detection probe and / or the second detection probe is connected to a measuring device using a conductor different from that of the detection probe.
11. 2. The method for managing filling of a cement-based material according to claim 1, further comprising the step of transmitting detection data on the filling state of the cement-based material to a display device by a wireless communication device.
12. 2. The method for managing filling of cementitious materials according to claim 1, further comprising displaying a filling status of the cementitious material on a screen.
Citation Information
Patent Citations
Method for confirming concrete fill by electrostatic capacity
JP1994229968A
Concrete state measuring sensor, measuring system and measuring method
JP2002207021A
Inspection method and device of casted concrete
JP2009008521A
Sensor cable, and method for manufacturing the same
JP2013205327A
Concrete installation height measuring apparatus
JP2018040681A