Double-shielding welding method

The double shield TIG welding method stabilizes welding by adjusting inner gas flow rates and arc rigidity based on electrode protrusion and current, ensuring stable and customizable welding conditions.

JP2024167531AInactive Publication Date: 2024-12-04DAIHEN CORP
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023083669
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-22
Publication Date
2024-12-04
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The double shield TIG welding method becomes unstable when the electrode protrusion length is increased beyond 2 to 3 mm, affecting welding stability.

Method used

A double shield TIG welding method that adjusts the flow rate of inner gas based on the welding current and electrode protrusion length, using a welding torch with inner and outer nozzles, and includes an adjustment section to fine-tune the arc rigidity.

Benefits of technology

Maintains a stable welding state even with increased electrode protrusion lengths, enhancing welding workability and allowing adjustment to preferred arc stiffness according to operator preference.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024167531000001_ABST
    Figure 2024167531000001_ABST
Patent Text Reader

Abstract

To stably maintain a welding state even when the projecting length of an electrode is prolonged in a double-shielding welding method.SOLUTION: In this double-shielding welding method which uses a welding torch WT provided with an inner nozzle 4 for jetting an inner gas 7 and an outer nozzle 5 for jetting an outer gas 9, projects an electrode 1 by a projecting length L from the tip position of the inner nozzle 4, and generates arc 3 and supplies welding current Iw between the electrode 1 and a base material 2 to weld them, a flow rate Fi of the inner gas 7 is set according to a setting value Ir of the welding current Iw, and the set flow rate Fi of the inner gas 7 is corrected according to the projecting length L of the electrode 1.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a double shielded TIG welding method. [Background technology]

[0002] A double-shielded TIG welding method is commonly used in which welding is performed using a welding torch equipped with an inner nozzle for ejecting an inner gas and an outer nozzle for ejecting an outer gas (see, for example, Patent Document 1). As the inner gas and the outer gas, inert gases such as argon and helium are used. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2020-15048 A Summary of the Invention [Problem to be solved by the invention]

[0004] In the double shield TIG welding method, the electrode is protruded from the tip position of the inner nozzle by a certain length, and an arc is generated between the electrode and the base metal to perform welding. Normally, the electrode protrusion length is about 2 to 3 mm. Depending on the shape of the base metal, the electrode protrusion length may be increased to about 5 to 10 mm to improve the workability of welding. However, when the electrode protrusion length is increased, the welding state may become unstable.

[0005] Therefore, an object of the present invention is to provide a double shielded TIG welding method capable of maintaining a stable welded state even if the electrode extension length is increased. [Means for solving the problem]

[0006] In order to solve the above-mentioned problems, the invention of claim 1 comprises: A welding torch having an inner nozzle for ejecting an inner gas and an outer nozzle for ejecting an outer gas is used, The electrode is protruded from the tip position of the inner nozzle by a protruding length, In a double shield TIG welding method, an arc is generated between the electrode and the base metal to pass a welding current therethrough, A flow rate of the inner gas is set according to a value of the welding current; a flow rate of the inner gas, which is set according to the value of the welding current, is corrected according to the extension length of the electrode; This is a double shielded TIG welding method characterized by the above.

[0007] The invention of claim 2 is as follows: An adjustment unit for adjusting the stiffness of the arc is provided, The adjustment unit increases or decreases a flow rate of the inner gas that is set according to a value of the welding current and the extension length of the electrode. 2. The double shielded TIG welding method according to claim 1,

[0008] The invention of claim 3 is as follows: resetting an increase or decrease in the flow rate of the inner gas by the adjustment unit to 0 when at least one of the conditions of the value of the welding current and the extension length of the electrode is changed; 3. The double shielded TIG welding method according to claim 2, Effect of the Invention

[0009] According to the double shield TIG welding method of the present invention, a stable welded state can be maintained even if the electrode extension length is increased. [Brief description of the drawings]

[0010] [Figure 1] 1 is a block diagram of a welding apparatus for carrying out a double-shielded TIG welding method according to an embodiment of the present invention. [Diagram 2]2 is a timing chart of each signal in the welding apparatus of FIG. 1 illustrating a double-shielded TIG welding method according to an embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] Hereinafter, an embodiment of the present invention will be described with reference to the drawings.

[0012] 1 is a block diagram of a welding apparatus for carrying out a double shielded TIG welding method according to an embodiment of the present invention. Each block will be described below with reference to the diagram.

[0013] The welding torch WT mainly comprises an electrode 1, an inner nozzle 4 surrounding the electrode 1, and an outer nozzle 5 surrounding the inner nozzle 4. The tip position of the electrode 1 is a position protruding from the tip position of the inner nozzle 4 by a predetermined protrusion length l (mm). A tungsten electrode or the like is used for the electrode 1. For example, the inner diameter of the inner nozzle 4 is 5 mm, and the inner diameter of the outer nozzle 5 is 13 mm.

[0014] The start switch ON outputs a start signal On that goes to a high level when it is turned on and goes to a low level when it is turned off. This start switch ON is a torch switch provided on the welding torch WT. The start signal On may also be output from the robot control device.

[0015] The current setting circuit IR outputs a predetermined current setting signal Ir.

[0016] The extension length setting circuit LR outputs an extension length setting signal Lr for setting the extension length L of the electrode 1. The welding operator attaches the electrode 1 to the welding torch WT so that the extension length L [mm] is set by the extension length setting signal Lr. The extension length L ranges from about 2 to 10 mm.

[0017] The inner gas flow rate setting circuit FIR receives the current setting signal Ir [A], the extension length setting signal Lr [mm], and the arc rigidity adjustment signal Hr (described later) as inputs, inputs them to a predetermined inner gas flow rate setting function, and outputs the calculated value as the inner gas flow rate setting signal Fir [l / min]. An example of the inner gas flow rate setting function is shown below. Fir=(Ir-75) / 50+3.5+(Lr-2)×0.1+Hr (1) Formula However, within the range of 75≦Ir≦150, when Ir<75, it is the same value as Ir=75, and when Ir>150, it is the same value as Ir=150. Also, within the range of 2≦Lr≦10, when Lr<2, it is the same value as Lr=2, and when Lr>10, it is the same value as Lr=10.

[0018] The inner gas flow regulator CI is a commonly used mass flow controller that receives the above-mentioned start signal On and the above-mentioned inner gas flow setting signal Fir as inputs, and when the start signal On becomes high level, it adjusts the flow rate Fi of the inner gas 7 from the inner gas cylinder 6 to a value determined by the inner gas flow setting signal Fir and sprays it.

[0019] The outer gas flow rate setting circuit FOR receives the current setting signal Ir and inputs it to a predetermined outer gas flow rate setting function, and outputs the calculated value as an outer gas flow rate setting signal For [l / min]. An example of the outer gas flow rate setting function is shown below. For = (Ir-75) / 50+5.5 (2) However, the range is 75≦Ir≦150, and when Ir<75, the value is the same as Ir=75, and when Ir>150, the value is the same as Ir=150.

[0020] The outer gas flow regulator CO is a commonly used mass flow controller that receives the above-mentioned start signal On and the above-mentioned outer gas flow setting signal For as inputs. When the start signal On becomes high level, it adjusts the flow rate Fo of the outer gas 9 from the outer gas cylinder 8 to a value determined by the outer gas flow setting signal For and sprays it.

[0021] An inner gas 7 flows through a passage inside the inner nozzle 4. An outer gas 9 flows through a passage outside the inner nozzle 4 and inside the outer nozzle 5. An inert gas such as argon or helium is used as the inner gas 7 and the outer gas 9. The arc 3 is generated with the electrode 1 serving as the negative electrode and the base material 2 serving as the positive electrode.

[0022] The welding power source PS receives as input the above-mentioned start signal On and the above-mentioned current setting signal Ir, and when the start signal On goes to high level, it applies a high frequency high voltage between the electrode 1 and the base material 2, and when an arc 3 is generated, it begins outputting the welding current Iw set by the current setting signal Ir, and when the start signal On goes to low level, it stops outputting the welding current Iw.

[0023] The arc rigidity adjustment circuit HR is provided on the front panel of the welding power source PS, and is equipped with an increase button and a decrease button. The circuit receives the current setting signal Ir and the extension length setting signal Lr as inputs, and outputs an arc rigidity adjustment signal Hr that increases by a predetermined value each time the increase button is pressed and decreases by a predetermined value each time the decrease button is pressed. The arc rigidity adjustment signal Hr is reset to 0 when the value of either the current setting signal Ir or the extension length setting signal Lr changes. For example, the predetermined value is 0.1 (l / min). At this time, if the increase button is pressed five times, Hr=0.5 (l / min). If the decrease button is then pressed twice, Hr=0.5-0.2=0.3 (l / min).

[0024] Below, we will explain numerical examples in which the flow rates of the inner gas and outer gas are set according to the value of the welding current, the flow rates of the inner gas and / or outer gas set according to the extension length L of the electrode 1 are corrected, and the arc rigidity is further adjusted. (1) Setting the inner gas flow rate When the extension length setting signal Lr is 2 mm and the arc rigidity adjustment signal Hr is the initial value of 0 l / min, the inner gas flow rate Fi is calculated by inputting the current setting signal Ir from the above formula (1). Since Fi = (Ir-75) / 50 + 3.5 + (Lr-2) x 0.1 + Hr, When Ir = 75A, Fi = 3.5 (l / min), and when Ir = 150A, Fi = 5.0 (l / min). Here, when the extension length setting signal Lr is changed to 10 mm, the inner gas flow rate Fi increases by 0.8 (l / min) from the above. Furthermore, by adjusting the arc rigidity signal Hr, the above automatically set inner gas flow rate can be increased or decreased from the median value.

[0025] (2) Setting the outer gas flow rate From the above equation (2), the outer gas flow rate Fo is calculated by inputting the current setting signal Ir. Since Fo = (Ir - 75) / 50 + 5.5, when Ir = 75A, Fo = 5.5 (l / min), and when Ir = 150A, Fo = 7.0 (l / min).

[0026] Fig. 2 is a timing chart of each signal in the welding device of Fig. 1, which shows a double-shielded TIG welding method according to an embodiment of the present invention. Fig. 2(A) shows the time change in electrode extension length L [mm], Fig. 2(B) shows the time change in welding current Iw [A], Fig. 2(C) shows the time change in inner gas flow rate Fi [l / min], and Fig. 2(D) shows the time change in outer gas flow rate Fo [l / min]. Below, the operation during welding will be explained with reference to the figures.

[0027] As shown in FIG. 1(B), welding current Iw is applied during the period from time t1 to t2, is stopped during the period from time t2 to t3, and is applied during the period from time t3 to t4. As shown in FIG. 1(A), the electrode extension length L is a first extension length during the period from time t1 to t2, and changes to a longer second extension length during the period from time t3 to t4. As shown in FIG. 1(B), welding current Iw is set by current setting signal Ir of FIG.

[0028] As shown in Fig. 1C, the inner gas flow rate Fi is calculated by substituting the values ​​of the current setting signal Ir in Fig. 1 and the extension length setting signal Lr in Fig. 1, which sets the extension length L of the electrode shown in Fig. 1A, into the above-mentioned formula (1). As shown in Fig. 1D, the outer gas flow rate Fo is calculated by substituting the value of the current setting signal Ir in Fig. 1 into the above-mentioned formula (2). For example, when the current setting signal Ir=150A, and the first extension length of the extension length setting signal Lr=2mm and the second extension length=8mm, the inner gas flow rate Fi and the outer gas flow rate Fo are calculated as follows. 1) The period from time t1 to time t2 Fi=(150-75) / 50+3.5+(2-2)×0.1=5 Fo = (150-75) / 50+5.5=7 2) The period from time t3 to time t4 Fi=(150-75) / 50+3.5+(8-2)×0.1=5.6 Fo is the same value as before time t1 As a result, as shown in Fig. 1C, the inner gas flow rate Fi is 5 l / min during the period from time t1 to t2, and increases to 5.6 l / min during the period from time t3 to t4, and as shown in Fig. 1D, the outer gas flow rate Fo is 7 l / min throughout the entire period.

[0029] The effects of this embodiment will be described below. According to this embodiment, the flow rate of the inner gas is set according to the value of the welding current, and the flow rate of the inner gas set according to the value of the welding current is corrected according to the protruding length of the electrode. Usually, the protruding length of the electrode is about 2 to 3 mm. Depending on the shape of the base material, the protruding length of the electrode may be increased to about 5 to 10 mm in order to improve the workability of welding. However, when the protruding length of the electrode is increased, the welding state may become unstable. In this embodiment, the flow rate of the inner gas is optimized according to the value of the welding current. Then, the flow rate of the inner gas is corrected so that the flow rate increases as the protruding length of the electrode increases. As a result, in this embodiment, the welding state can be maintained stably even if the protruding length of the electrode is increased.

[0030] More preferably, according to this embodiment, an adjustment unit for adjusting the rigidity of the arc is provided, and the adjustment unit increases or decreases the flow rate of the inner gas set according to the value of the welding current and the extension length of the electrode. The welding state can be improved by optimizing the flow rate of the inner gas according to the welding current and the extension length of the electrode. In addition, the rigidity of the arc desired by each welding operator is different. Some welding operators prefer a hard arc with strong rigidity, and others prefer a soft arc with weak rigidity. If the rigidity of the arc can be adjusted to a state desired by the welding operator, the welding workability can be improved. In this embodiment, an adjustment unit for finely adjusting the rigidity of the arc is provided, and the adjustment unit can increase or decrease the flow rate of the inner gas set according to the welding current and the extension length of the electrode. If the flow rate of the inner gas is increased, the rigidity of the arc becomes stronger, resulting in a harder arc. If the flow rate of the inner gas is decreased, the rigidity of the arc becomes weaker, resulting in a softer arc. As a result, in this embodiment, the stiffness of the arc can be adjusted to a state desired by the welding operator, thereby improving workability.

[0031] More preferably, according to this embodiment, when at least one of the conditions of the welding current value and the electrode extension length is changed, the increase or decrease value of the flow rate of the inner gas by the adjustment unit is reset to 0. Even if the increase or decrease value by the adjustment unit is the same depending on the combined conditions of the welding current value and the electrode extension length, the degree of the arc rigidity varies. Therefore, when at least one of these conditions is changed, the increase or decrease value is reset to 0 to temporarily return the arc rigidity to the standard state. After that, the adjustment unit is again used to return the arc rigidity to a desired state. [Explanation of symbols]

[0032] 1 electrode 2 Base material 3. Arc 4 Inner nozzle 5 Outer nozzle 6 Inner gas cylinder 7. Inner Gas 8 Outer gas cylinder 9. Outer Gas CI Inner Gas Flow Regulator CO outer gas flow regulator Fi Inner gas flow rate FIR inner gas flow rate setting circuit Fir inner gas flow rate setting signal Fo Outer gas flow rate FOR outer gas flow rate setting circuit For outer gas flow rate setting signal HR Arc stiffness adjustment circuit Hr Arc stiffness adjustment signal IR current setting circuit Ir Current setting signal Iw Welding current L Electrode extension length LR extension length setting circuit Lr Extension length setting signal ON Start switch On Start signal PS Welding Power Source WT Welding Torch

Claims

1. A welding torch having an inner nozzle for ejecting an inner gas and an outer nozzle for ejecting an outer gas is used, The electrode is protruded from the tip position of the inner nozzle by a protruding length, In a double shield TIG welding method, an arc is generated between the electrode and the base metal to pass a welding current therethrough, A flow rate of the inner gas is set according to a value of the welding current; a flow rate of the inner gas, which is set according to the value of the welding current, is corrected according to the extension length of the electrode; A double shielded TIG welding method.

2. An adjustment unit for adjusting the stiffness of the arc is provided, The adjustment unit increases or decreases a flow rate of the inner gas that is set according to a value of the welding current and the extension length of the electrode. The double shielded TIG welding method according to claim 1 .

3. resetting an increase or decrease in the flow rate of the inner gas by the adjustment unit to 0 when at least one of the conditions of the value of the welding current and the extension length of the electrode is changed; The double shielded TIG welding method according to claim 2 .

Citation Information