Method for manufacturing soft-magnetic material laminate body
By laminating thin plates of soft magnetic materials with resin and applying heat treatment, the method addresses manufacturing issues of nanocrystalline and amorphous materials, achieving lower iron loss and improved performance for motor cores.
Patent Information
- Application Number
- JP2023085985
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-25
- Publication Date
- 2024-12-05
- Estimated Expiration
- 2043-05-25
AI Technical Summary
Nanocrystalline and amorphous soft magnetic materials face challenges in manufacturing processes such as thinness, sagging, brittleness, and inability to be caulked, leading to increased iron loss when resin impregnation is used for fixation.
A method involving laminating thin plates of soft magnetic materials with resin impregnation, followed by resin curing and heat treatment at 110 to 190°C, reduces iron loss by releasing stress after curing.
The method results in a soft magnetic material laminate with reduced iron loss compared to conventional methods, suitable for use as motor cores.
Smart Images

Figure 2024168924000001
Abstract
Description
[Technical field]
[0001] The present disclosure relates to a method for manufacturing a soft magnetic material lamination. [Background technology]
[0002] Conventionally, laminates of electromagnetic steel sheets (laminated cores) have been used as motor cores. From the viewpoint of reducing motor loss, various researches on motor cores have been conducted.
[0003] Incidentally, Patent Document 1 discloses a laminate in which soft magnetic ribbons having a nanocrystalline structure are laminated, characterized in that an organic SOG film formed by curing a resin is provided between the ribbons. Patent Document 1 discloses an embodiment in which the organic SOG film is formed by thermally curing a polysiloxane resin. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2009-200428 A Summary of the Invention [Problem to be solved by the invention]
[0005] In order to reduce motor loss, the inventors investigated the application of nanocrystalline soft magnetic materials, which are thought to have lower loss than conventional electromagnetic steel sheets, and amorphous soft magnetic materials to motors, for example to motor cores.
[0006] However, nanocrystalline soft magnetic materials and amorphous soft magnetic materials have problems in the manufacturing process, such as being thin and prone to sagging, being brittle and not capable of being crimped, etc. In order to solve this problem, the present inventors considered impregnating resin between thin plates of at least one type of soft magnetic material selected from nanocrystalline soft magnetic materials and amorphous soft magnetic materials, and fixing them, but found that impregnating and fixing with resin worsens the iron loss of the nanocrystalline soft magnetic material laminate and the amorphous soft magnetic material laminate.
[0007] An object of the present disclosure is to provide a method for manufacturing a soft magnetic material laminate having reduced core loss compared to conventional methods. [Means for solving the problem]
[0008] The present inventors conducted intensive research to solve the above problems, and discovered that iron loss can be reduced by fixing the layers of the laminate with resin and then performing a specific heat treatment, which led to the present disclosure.
[0009] An example aspect of this embodiment is described as follows.
[0010] (1) preparing a resin-containing laminate in which a plurality of thin plates of at least one type of soft magnetic material selected from a nanocrystalline soft magnetic material and an amorphous soft magnetic material are laminated, and a resin is impregnated between the thin plates; A step of heating the resin-containing laminate to cure the resin and fix the layers of the laminate; and The method for producing a soft magnetic material laminate comprises a step of heat treating the laminate at 110 to 190°C after the fixing. (2) The method for producing a soft magnetic laminate according to (1), wherein the resin is impregnated between the layers of the thin plate in the form of a resin-containing varnish. (3) The method for producing a soft magnetic laminate according to (1) or (2), wherein the heat treatment is carried out at 120 to 180° C. (4) The method for producing a soft magnetic material laminate according to any one of (1) to (3), wherein the soft magnetic material laminate is a motor core. Effect of the Invention
[0011] The present disclosure makes it possible to provide a method for manufacturing a soft magnetic material laminate having reduced core loss compared to conventional methods. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] The method for producing the soft magnetic material laminate of this embodiment will be described in detail below. The method for producing the soft magnetic material laminate of this embodiment includes a step of preparing a resin-containing laminate in which a plurality of thin plates of at least one type of soft magnetic material selected from nanocrystalline soft magnetic materials and amorphous soft magnetic materials are laminated and resin is impregnated between the thin plates, a step of heating the resin-containing laminate to harden the resin and fix the laminate between the layers, and a step of heat-treating the laminate at 110 to 190°C after the fixing. The soft magnetic material laminate obtained by the manufacturing method of this embodiment can be used as, for example, a motor core (laminated core). The motor core is a concept that includes both a core used in the rotor of a motor and a core used in the stator. In other words, the motor core is a general term for a so-called rotor core and a stator core.
[0013] (Soft magnetic material) In the method for producing the soft magnetic material laminate of the present embodiment, at least one soft magnetic material selected from a nanocrystalline soft magnetic material and an amorphous soft magnetic material is used. Specifically, the soft magnetic material is used in the step of preparing the resin-containing laminate described below.
[0014] Amorphous soft magnetic materials are also called amorphous alloys, and nanocrystalline soft magnetic materials are materials in which an amorphous alloy is crystallized to disperse nanocrystalline grains of a ferromagnetic phase in the remaining amorphous phase.
[0015] Examples of the nanocrystalline soft magnetic material and the amorphous soft magnetic material include, but are not limited to, those containing at least one magnetic metal selected from the group consisting of Fe, Co, and Ni as a constituent element. As the nanocrystalline soft magnetic material and the amorphous soft magnetic material, it is preferable to use the nanocrystalline soft magnetic material.
[0016] Examples of the nanocrystalline soft magnetic material include Fe-based nanocrystalline soft magnetic materials. Examples of the Fe-based nanocrystalline soft magnetic material include soft magnetic materials in which the main component is Fe and nanocrystals are dispersed in an amount of 30% by volume or more in the material.
[0017] Examples of the nanocrystalline soft magnetic material include, for example, a composition formula: Fe 100-a-b-c-d Cu a B b Si c Sn d The material represented by is preferable. In the above composition formula, a, b, c, and d are atomic percentages, and it is preferable that 0.6 ≦ a ≦ 1.6, 6 ≦ b ≦ 20, 0 < c ≦ 17, 0.005 ≦ d ≦ 0.2, and 7 ≦ b + c ≦ 24. The nanocrystalline soft magnetic material is preferably an alloy composed of a structure in which fine crystal grains having an average crystal grain diameter of 60 nm or less are dispersed in an amorphous matrix phase at a volume fraction of 30% or more.
[0018] The soft magnetic material is used as a thin plate. The thickness of the soft magnetic material is, for example, 40 μm or less, preferably 35 μm or less. The lower limit of the thickness of the soft magnetic material is not particularly limited, but is, for example, 15 μm or more. Within the above range, the soft magnetic material laminate tends to have excellent magnetic properties and can be particularly preferably used as a motor core.
[0019] (Resin) The resin may be any resin that is cured by heating, and so-called thermosetting resins are usually used. The thermosetting resin is not particularly limited, and examples thereof include phenol-based resins, urea-based resins, melamine-based resins, diallyl phthalate-based resins, polyester-based resins, epoxy-based resins, aniline-based resins, silicone-based resins, furan-based resins, polyurethane-based resins, alkylbenzene-based resins, guanamine-based resins, xylene-based resins, and imide-based resins. The resin may be used alone or in combination of two or more.
[0020] (varnish) In the manufacturing method of the present disclosure, the resin may be used as a varnish containing a resin. The varnish is a liquid composition containing a resin and other components. By using the varnish, the resin can be easily impregnated between the layers of the thin plate of the soft magnetic material. Components other than the resin contained in the varnish are not particularly limited, and include a diluent, a hardener, a filler (e.g., an organic filler, an inorganic filler), and the like. Commercially available products may be used as the resin and varnish.
[0021] (Step of Preparing Resin-Containing Laminate) The manufacturing method of the present disclosure includes a step of preparing a resin-containing laminate. This step is a step of preparing a resin-containing laminate in which a plurality of thin plates of nanocrystalline soft magnetic material are laminated and the spaces between the thin plates are impregnated with resin. This step can also be called a preparation step of a resin-containing laminate. Hereinafter, this step will also be referred to as a "preparation step".
[0022] In the preparation step, for example, a resin-containing laminate may be prepared by pouring a resin, for example as a varnish, onto a thin plate of a soft magnetic material and stacking another thin plate on top of it, or a resin-containing laminate may be prepared by stacking thin plates of a soft magnetic material without using a resin, fixing them using a jig, immersing the stacked thin plates of a soft magnetic material in a container containing a resin such as varnish, and then removing them.
[0023] There is no particular limit to the number of thin plates of the soft magnetic material that can be laminated, and it can be determined according to the material and thickness of the thin plates, the desired motor performance, etc. The number of laminated thin plates can be appropriately set depending on, for example, the volume of the motor and the thickness of each thin plate.
[0024] (Step of fixing layers of laminate) The manufacturing method of the present disclosure includes a step of heating the resin-containing laminate to cure the resin and fix the layers of the laminate. In this step, the heating conditions may be set according to the type of resin, and the type of varnish if a varnish is used. In this step, the resin can be cured, for example, by heating at 150 to 175°C for 0.7 to 2 hours.
[0025] In this process, the resin-containing laminate is usually heated while applying a load to harden the resin. By applying a load to the resin-containing laminate, the amount of resin present between the layers can be reduced, and the overall thickness at the time of hardening can be reduced. On the other hand, if the load is too large, the characteristics of the soft magnetic material may deteriorate and the iron loss may increase. For this reason, the load is preferably more than 0 MPa and 1.5 MPa or less.
[0026] (Heat treatment process) The manufacturing method of the present disclosure includes a step of heat-treating the laminate at 110 to 190° C. after fixing. Surprisingly, the inventors of the present invention have found that iron loss is reduced by heat-treating again after thermal curing. The reason for this is unclear, but the inventors of the present invention speculate that this is because part of the stress during curing is released by performing heat treatment after curing.
[0027] Unlike the fixing step described above, the heat treatment step is preferably performed without applying stress. The heat treatment is preferably performed at 120 to 180°C, more preferably at 130 to 170°C. The heat treatment is preferably performed for 150 hours or more. It is also preferable that the heat treatment is performed for 270 hours or less. EXAMPLES
[0028] The present embodiment will be described below with reference to examples, but the present disclosure is not limited to these examples.
[0029] In the examples and comparative examples, WP-2008 manufactured by Hitachi Chemical Co., Ltd. was used as the varnish.
[0030] (Examples and Comparative Examples) A varnish was poured onto the surface of a ring-shaped nanocrystalline soft magnetic material (thickness about 30 μm), and another ring-shaped nanocrystalline soft magnetic material was layered on top of it. This operation was repeated 29 times to obtain a resin-containing laminate with 30 ring-shaped nanocrystalline soft magnetic materials and with the varnish impregnated between each layer.
[0031] The resin-containing laminate was placed in an oven set at 170° C. for 1 hour while applying a load of 0.5 MPa to cure the resin and fix the layers of the laminate together.
[0032] Thereafter, without applying a load to the laminate, a heat treatment was performed for 250 hours at the temperatures shown in Table 1 to obtain a nanocrystalline soft magnetic material laminate. The examples in which the heat treatment was performed at 75°C and 100°C correspond to comparative examples, and the examples in which the heat treatment was performed at 120°C, 150°C, and 180°C correspond to examples.
[0033] The obtained nanocrystalline soft magnetic material laminate was placed in a resin case and wound with copper wire. The iron loss was then measured at variable frequencies using an AC magnetic property measuring device. The iron loss was evaluated as the iron loss (W / kg) at 1T and 400Hz. Table 1 shows the reduction rate (%) of iron loss after heat treatment when the iron loss before heat treatment is taken as 100%. Since the operations before heat treatment are the same for each example and comparative example, it can be determined that the higher the reduction rate of iron loss, the better.
[0034] [Table 1]
[0035] It was found from Table 1 that the nanocrystalline soft magnetic material laminate obtained by the manufacturing method of this embodiment had reduced iron loss. In addition, the iron loss value after heat treatment was about 4.5 to 8 (W / kg), which was sufficiently lower than the values when other soft magnetic materials were used.
[0036] The upper limit and / or lower limit of the numerical ranges described in this specification can be arbitrarily combined to define a preferred range. For example, the upper limit and lower limit of the numerical range can be arbitrarily combined to define a preferred range, the upper limit of the numerical range can be arbitrarily combined to define a preferred range, and the lower limit of the numerical range can be arbitrarily combined to define a preferred range.
[0037] Although the present embodiment has been described in detail above, the specific configuration is not limited to this embodiment, and even if there are design changes within the scope that does not deviate from the gist of this disclosure, they are included in this disclosure.
Claims
[Claim 1] A step of preparing a resin-containing laminate in which a plurality of thin plates of at least one type of soft magnetic material selected from a nanocrystalline soft magnetic material and an amorphous soft magnetic material are laminated, and a resin is impregnated between the thin plates; A step of heating the resin-containing laminate to cure the resin and fix the layers of the laminate; and The method for producing a soft magnetic material laminate includes a step of heat treating the laminate at 110 to 190° C. after the fixing.
Citation Information
Patent Citations
Manufacture of magnetic core
JP1986065418A
Iron-based amorphous alloy sheet strip excellent in soft magnetic property, and its manufacture
JP1998324961A
Magnetic base material, laminate from magnetic base material and method for production thereof
WO2003060175A1
Laminate of magnetic base material and method for production thereof
WO2005031767A1
Layered product, and its manufacturing method
JP2009200428A