Climatic steaming at controlled humidity and temperature conditions followed by standard steam treatment addresses the issue of frequency drift in Nb-Ti alloy hairsprings, achieving a drift reduction to less than 3 seconds per day.
Patent Information
- Application Number
- JP2024079968
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-24
- Filing Date
- 2024-05-16
- Publication Date
- 2024-12-05
- Estimated Expiration
- 2044-05-16
AI Technical Summary
Existing steam treatments for Nb-Ti alloy hairsprings in watch movements fail to adequately reduce frequency drift over time, with a drift of more than 6 seconds per day still observed after one year.
A climatic steaming process is applied to Nb-Ti alloy hairsprings at controlled humidity levels between 60 and 99% and temperatures between 30 and 100°C, followed by a standard steam treatment, to stabilize the native oxide layer and reduce speed drift.
The method achieves a significant reduction in speed drift to less than 3 seconds per day after 5 months, improving the long-term stability of the hairspring.
Smart Images

Figure 2024169346000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for treating a balance spring for a timepiece movement. It also relates to the balance spring obtained from this treatment method. [Background technology]
[0002] Watchmakers are well aware that the frequency of a balance spring oscillator drifts as a function of time.
[0003] To reduce this drift, it is common to perform a steam treatment, which consists of heating the hairspring at temperatures between 100 and 250°C for 6 to 24 hours. The steam treatment has the effect of restoring the material and also allowing the diffusion and rearrangement of the interstitial elements, i.e. carbon, nitrogen and oxygen, and of stabilizing the native oxide layer. Despite the steam treatment, a speed drift of more than 6 s / d was still observed after one year in hairsprings made of Nb-Ti alloys. Summary of the Invention
[0004] The object of the present invention is to propose a new method for treating hairsprings to reduce their speed drift, which applies to hairsprings made of paramagnetic alloys, in particular to hairsprings made of Nb-Ti alloys, in which the weight percentage of Ti relative to the total weight of the alloy is between 40 and 90%, preferably between 40 and 50%.
[0005] According to the invention, the method for treating the hairspring includes a step of steam treatment, called climate steaming, since this steam treatment is carried out in an atmosphere having a controlled level of relative humidity.
[0006] More specifically, the present invention relates to a method for treating at least one hairspring intended to equip a timepiece movement, said hairspring being made from a Nb-Ti alloy, the method comprising a step of steam treatment, called climatic steaming, at temperatures ranging from 30 to 100°C, in an atmosphere having a relative humidity between 60 and 99%.
[0007] Tests have shown a clear reduction in the speed drift of the hairsprings treated by the method according to the invention. This improvement can be attributed to the generation and growth of different forms of TiO2 on the surface of the hairspring due to humidity. It can also be related to the presence of water molecules adsorbed on the surface of the hairspring.
[0008] The present invention also relates to a hairspring characterized in that after 5 months of use from the time the climatic steaming step has been performed, its speed is less than or equal to 3 s / d.
[0009] Other features and advantages of the present invention will become apparent from the following description and figures. [Brief description of the drawings]
[0010] [Figure 1] FIG. 2 shows the speed (s / d) as a function of time (months) for a hairspring treated using the method according to the invention and, by comparison, for two hairsprings: an untreated hairspring and one treated using the standard steaming method. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] The present invention relates to a method for treating a hairspring intended to equip the balance wheel of a watch movement.
[0012] According to the invention, the treatment method can be carried out on an individual hairspring or on several hairsprings in a batch process. It can be carried out, for example, on a plate containing several hairsprings in a barrel. It can also be carried out on the entire watch movement on which the hairspring is mounted. By way of example, it can be an assembly including the hairspring and a collet, or an assembly formed by an oscillator including a balance, a hairspring, a plate and an axis.
[0013] The balance spring is made from a paramagnetic alloy, in particular a Nb-Ti alloy, containing between 40 and 90% by weight titanium, with possible traces of one or more elements chosen from O, H, C, Fe, Ta, N, Ni, Si, Cu, Al, each of said elements being between 0 and 1600 ppm of the total weight, the remainder being constituted by niobium, 100%.
[0014] According to the invention, the method for treating the hairspring comprises a steaming step at a temperature range between 30 and 100° C. in an atmosphere having a relative humidity between 60 and 99%. Preferably, the temperature range is between 40 and 80° C., more preferably between 40 and 60° C. Preferably, the relative humidity is between 70 and 97%, preferably between 85 and 95%, more preferably between 87 and 95%. More preferably, the test is carried out at normal pressure. It is also possible to carry out the test at partial pressures between 1 and 1000 mbar. It is also possible, for example, to carry out the overpressure test at pressures between 1 and 5 bar in a steamer. Different holding times are possible in a fairly wide range, from 10 minutes to 100 hours, the time having no significant effect on the result.
[0015] The climate steaming treatment according to the invention is preferably preceded by a standard steaming treatment known in the prior art, which is preferably carried out under ambient humidity at a temperature between 100 and 250° C. and for a period of between 1 and 30 hours.
[0016] The standard steaming process and the climate steaming process are carried out after the hairspring fixing step, which is a heat treatment well known to those skilled in the art.
[0017] The method for manufacturing the hairspring of the present invention therefore comprises the following steps with steps a) to f) well known to a person skilled in the art: a) Manufacturing of a blank made of a Nb-Ti alloy having the above chemical composition. b) A melt quenching treatment of said blank, known as β type, in order to bring the titanium and niobium into an essentially β-phase solid solution. c) applying a deformation sequence to the alloy, optionally with one or more heat treatments. Deformation means deformation by drawing and / or rolling. Drawing may require the use of one or more dies in the same sequence or in a different sequence, as appropriate. The wire is drawn until it has a round cross section. Rolling may be carried out in the same deformation sequence as drawing or in a different sequence. Advantageously, the last sequence applied to the alloy is rolling, preferably with a rectangular profile adapted to the entrance cross section of the winding spindle. d) Winding to form a balance spring. e) Final heat treatment for fixation. f) Any standard steaming process. g) Climate steaming process according to the present invention.
[0018] The invention also relates to a hairspring obtained from the treatment method according to the invention, characterized in that it contains titanium oxide and potentially adsorbed water molecules on its surface, and also characterized in that after 5 months of use after the climatic steaming step, its speed is less than 3s / d, or even less than 2s / d.
[0019] Tests were carried out after the climatic steaming step. The results are shown in FIG. 1. The vertical axis is the speed (s / d) measured with a Witschi Chronomaster device at room temperature, and the horizontal axis is the time in months. Tests were carried out on a Nb-Ti alloy hairspring with a weight percentage of Ti of 47%. According to the method of the invention, this hairspring was subjected to the standard steaming method according to step f) carried out at 150° C. for 24 hours at ambient humidity, and then to the climatic steaming method according to step g) carried out at a temperature of 50° C. for 4 hours in an atmosphere of 93% relative humidity under normal pressure. As a comparison, a hairspring of the same chemical composition that was not subjected to the treatment according to steps f) or g) was also tested. A hairspring of the same chemical composition that was only subjected to the standard steaming according to step f) carried out at 150° C. for 24 hours at ambient humidity was also tested. A clear reduction in the speed drift was observed for the hairsprings made using the treatment method according to the invention. After five months, the rate was on the order of 2 s / d compared with values on the order of 5 s / d for the control hairspring.
Claims
1. 1. A method for treating at least one hairspring intended to equip a timepiece movement, comprising the steps of: the hairspring is made of a Nb-Ti alloy; The method includes a step of steam treatment, called climate steaming, in an atmosphere having a relative humidity between 60 and 99%, at a temperature range between 30° C. and 100° C.
2. 2. The method of claim 1, wherein the step of climate steaming precedes a standard steaming step carried out under ambient air in a temperature range between 100 and 250°C.
3. 2. The method according to claim 1, characterized in that the temperature range of the climate steaming step is between 40 and 80°C, preferably between 40 and 60°C.
4. 2. The method of claim 1, wherein the relative humidity is between 70 and 97%, preferably between 85 and 95%, and more preferably between 87 and 95%.
5. 2. The method according to claim 1, which is carried out under normal pressure.
6. 2. The process according to claim 1, characterized in that it is carried out under a partial pressure of between 1 and 1000 mbar or under overpressure with a pressure of between 1 and 5 bar.
7. 2. The method according to claim 1, characterized in that the method is carried out under normal pressure in an atmosphere containing a relative humidity between 87 and 95% having a temperature between 40 and 60°C.
8. 2. The process according to claim 1, characterized in that said Nb-Ti alloy comprises a weight percentage of Ti between 40 and 90%, preferably between 40 and 50%, with possible traces of one or more other elements selected from O, H, C, Fe, Ta, N, Ni, Si, Cu and Al, each of said elements being between 0 and 1600 ppm of the total weight, the balance being 100% constituted by Nb.
9. 2. A method according to claim 1, which is carried out on individual hairsprings, including a number of hairsprings in a plate or a single hairspring mounted in an assembly of the timepiece movement, and which is carried out on several hairsprings simultaneously, the treatment being applied to each of the plates or the assemblies.
10. The assembly includes the hairspring and a collet, 10. The process according to claim 1, characterized in that the assembly is formed by an oscillator including a balance, a hairspring, a plate and an axis.
11. 2. A method for manufacturing at least one hairspring, comprising a fixing step prior to the processing method according to claim 1.
12. 12. A hairspring obtained by the manufacturing method according to claim 11, characterized in that after 5 months of use from the step of climate steaming, its speed is less than or equal to 3 s / d.
Citation Information
Patent Citations
Self-compensation type spiral for mechanical spiral balance-wheel oscillator and its treatment method
JP2000321371A
Resonator with reduced sensitivity to climate change
JP2016513244A
Balance spring and method for manufacturing balance spring
JP2020095027A
Mainspring for watch movement and its manufacturing method
JP2023504079A