Development of Advanced Barrier Nickel Oxide (BNiO) Coatings for Process Chamber Components

A nickel oxide barrier layer on semiconductor chamber components addresses corrosion and contamination issues by enhancing resistance to fluorine-containing gases, thereby extending chamber lifespan and improving process consistency.

JP2024536969AActive Publication Date: 2024-10-10APPLIED MATERIALS INC
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
JP2024504178
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-10-04
Filing Date
2022-09-29
Publication Date
2024-10-10
Estimated Expiration
2042-09-29

AI Technical Summary

Technical Problem

Semiconductor manufacturing processes face challenges with device uniformity and reproducibility due to reactions between chamber components and corrosive gases, leading to metal fluoride formation, particle deposition, and contamination, which reduce chamber lifetime and process consistency.

Method used

Application of a nickel-containing metal plating with a protective nickel oxide barrier layer on chamber components to prevent interaction with fluorine-containing gases, formed by oxidizing the metal plating using hydrofluoric or nitric acid, enhancing the chamber's resistance to corrosion and reducing contamination.

Benefits of technology

The nickel oxide barrier layer significantly extends the chamber component's lifespan by a factor of ten, reduces particle contamination, and improves process consistency by minimizing the need for preventive maintenance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024536969000001_ABST
    Figure 2024536969000001_ABST
Patent Text Reader

Abstract

Described herein is a chamber component that includes a metal layer that includes nickel and a barrier layer of nickel oxide on the metal layer. The nickel oxide barrier layer may be formed by treating the chamber component with an oxidizing agent that includes hydrofluoric acid and / or nitric acid.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] FIELD OF THE DISCLOSURE Embodiments of the present disclosure generally relate to corrosion-resistant metal oxide coated chamber components and methods of making and using such coated chamber components. [Background technology]

[0002] In the semiconductor industry, devices are fabricated by a number of manufacturing processes that produce structures of ever decreasing size. As device geometries decrease, it becomes much more difficult to control the process uniformity and repeatability of the devices.

[0003] Various semiconductor manufacturing processes involve high temperatures, (NF 3 , C.F. 4 These extreme conditions involve the use of high energy plasmas (such as remote and direct fluorine plasmas), mixtures of corrosive gases, corrosive cleaning chemicals (e.g., hydrofluoric acid) and combinations thereof. Under these extreme conditions, reactions between the material of components in the process chamber and the plasma gases or corrosive gases can occur, resulting in the formation of metal fluorides, particles, other trace metal contaminants and high vapor pressure gases (e.g., AlF x ) may be formed. Such gases may readily sublime and deposit on other components in the chamber. During subsequent process steps, the deposited material may detach from other components, such as particles, and fall onto the wafer, creating defects. Additional problems caused by such reactions include deposition rate drift, etch rate drift, compromised film uniformity, and compromised etch uniformity. It is beneficial to reduce these defects with a stable, non-reactive coating on the chamber parts to limit sublimation and / or the formation of particles and metal contaminants on the chamber parts in the chamber.

[0004] Therefore, to reduce these defects, some semiconductor processing chamber parts (e.g., liners, doors, lids, showerheads, etc.) include an electroless nickel plated (ENP) surface. However, the ENP surface has been found to develop a fluorine-containing layer after use in a fluorine-based atmosphere and at higher temperatures of about 150° C. or higher. Without being limited to theory, the fluorine-containing layer develops due to contamination during use, and thus the fluorine-containing layer can be considered a contamination layer. Furthermore, after processing hundreds of wafers, the fluorine-containing layer has been found to reduce the life of one or more components of the process chamber and the mean wafers between cleaning (MWBC) metric. Summary of the Invention

[0005] In some embodiments of the present disclosure, a chamber component for a processing chamber may include a body, a metal plating on at least one surface of the body, the metal plating comprising nickel, and a barrier layer on the metal plating. In some embodiments, the barrier layer may comprise nickel oxide. In some embodiments, the metal plating may comprise nickel and phosphorous. In some embodiments, the metal plating may comprise nickel and is free of phosphorous. In some embodiments, the body comprises aluminum, an aluminum alloy, aluminum nitride, alumina, or a combination thereof. In some embodiments, the metal plating has a thickness of about 20 microns to about 75 microns, and the barrier layer has a thickness of about 2 nm to about 50 nm. In some embodiments, the barrier layer has an average surface roughness (Ra) of about 2 microinches to about 60 microinches. In some embodiments, the chamber component may be a showerhead for a process chamber.

[0006] In another embodiment of the present disclosure, a method of protecting a chamber component includes forming a metal plating on a body of the chamber component, where the metal plating may include nickel, and contacting the metal plating with an oxidizing agent to form a barrier layer on the metal plating, where the barrier layer may include nickel oxide. In some embodiments, the oxidizing agent may include at least one of hydrofluoric acid, oxalic acid, or nitric acid. In some embodiments, the barrier layer may have a thickness of about 2 μm to about 60 μm. In some embodiments, forming the metal plating may include performing electroless metal plating, where the metal plating further includes phosphorus. In some embodiments, the body may include an aluminum alloy, aluminum nitride, alumina, or a combination thereof. In some embodiments, the method may include removing a native oxide from the metal plating prior to forming the barrier layer. In some embodiments, the method may include forming a nickel fluoride (NiF2) or nickel oxyfluoride layer on the metal plating by contacting the metal plating with ammonium fluoride after forming the metal plating. In some embodiments, the method may also include placing the chamber parts in an acid bath comprising 5-25% hydrofluoric acid and 75-95% water to contact the metal plating with an oxidizing agent, then placing the chamber parts in a deionized water bath, then placing the chamber parts in the acid bath, and then placing the chamber in a deionized water bath.

[0007] In another embodiment of the present disclosure, a method of repairing a used chamber part may include removing a contamination layer from a metal plating on the used chamber part using a first acid solution, the metal plating comprising nickel, and then contacting the metal plating with an oxidizing agent to form a barrier layer on the metal plating, the barrier layer comprising nickel oxide. In some embodiments, the contamination layer may include nickel fluoride. In some embodiments, removing the contamination layer may include placing the used chamber part in a first acid bath, then rinsing the used chamber part with deionized water, then drying the used chamber part, then placing the used chamber part in a second acid bath, then rinsing the used chamber part with deionized water, then drying the used chamber part. In some embodiments, the oxidizing agent may include at least one of hydrofluoric acid or nitric acid. In some embodiments, the barrier layer may have a thickness of about 2 μm to about 60 μm.

[0008] The present invention is illustrated by way of example, and not limitation, in the figures of the accompanying drawings in which like reference numbers indicate like elements. It should be noted that in this disclosure, different references to "an embodiment" or "an embodiment" are not necessarily references to the same embodiment, and such references mean at least one. [Brief description of the drawings]

[0009] [Figure 1A] FIG. 2 illustrates a cross-sectional view of one embodiment of a processing chamber. [Figure 1B] FIG. 2 illustrates a cross-sectional view of one embodiment of a showerhead for a processing chamber. [Diagram 2] FIG. 2 illustrates an embodiment of a bottom view of a showerhead, according to one embodiment. [Figure 3A] 1 illustrates a method for forming an advanced barrier oxide layer according to one embodiment. [Figure 3B]5A-5C illustrate another method for repairing and forming a high barrier oxide layer according to another embodiment. [Figure 4] FIG. 1 illustrates an example architecture of a manufacturing system. [Diagram 5] 1 is a flow chart illustrating a method for forming an advanced barrier oxide layer, according to one embodiment. [Figure 6] 4 is a flow chart illustrating a method for repairing and forming an advanced barrier layer according to another embodiment. [Figure 7] 1 is a flow chart illustrating a method of forming an advanced barrier layer having a nickel fluoride (NiF2) or nickel oxyfluoride (NiOF) layer on a metal plated or metal coated chamber component according to one embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0010] In the embodiments disclosed herein, coated articles, coated chamber parts, methods of coating articles and chamber parts, methods of reducing or eliminating particles from a semiconductor processing chamber, and methods of using the coated articles and chamber parts and processing chambers containing the coated chamber parts are described. A metal layer with a barrier layer (which may be, for example, a metal coating or metal plating) is included to reduce reactions between the component material and reactive chemicals and / or plasmas that form metal fluorides, particles, other trace metal contaminants, and / or high vapor pressure gases. The metal layer may be a nickel-containing layer (e.g., a pure nickel layer or a layer having nickel as a main component and further containing other materials such as phosphorus and / or vanadium). The barrier layer may be a nickel oxide layer formed under controlled conditions. The barrier layer may be added to new chamber parts to improve the service life of the chamber parts and / or to reduce or eliminate the build-up of contamination layers on the chamber parts. Additionally, to improve the life of the coated articles, or coated chamber parts (which may be new or used chamber parts), they may be treated to remove the contamination layer and to add a barrier layer over the metal layer on the chamber part.

[0011] It has been found that there is an interaction between fluorine and metal layers on chamber parts (e.g., ENP with nickel) that adds oxides and / or fluorides to the metal layers. Native oxides form naturally on metal layers upon exposure to air. However, native oxides have undesirable properties. In particular, native oxides interact with process gases (e.g., fluorine) to form a contamination layer. The interaction of native oxides with fluorine forms a black film (contamination layer) on the metal coating that causes discoloration and produces particles that can contaminate the processed substrate. If the black film / contamination layer is present on chamber parts such as a showerhead, there can be a loss of yield for substrates processed by a process chamber that includes a showerhead with a contamination layer.

[0012] Additionally, if there is a black film / contamination layer that forms while the chamber parts are in use, the chamber parts are removed and replaced.

[0013] Thus, the embodiments improve the surface of a chamber part, such as a showerhead, to prevent the formation of a black film / contamination layer on the metal layer of the chamber part. It would be advantageous to have a protective barrier layer to prevent chemical decomposition of the surface metal layer and the formation of a black film / contamination layer. Such chamber parts with a protective barrier layer may also degrade and / or become contaminated more slowly than chamber parts without a barrier layer, which may result in a chamber part with a barrier layer over the metal layer having a higher average wafers between cleanings than a chamber part with a metal layer and no barrier layer. The average wafers between cleanings represents the average number of wafers processed between each cleaning of the chamber part. Such increased average wafers between cleanings may be particularly noticeable for chamber parts used in chambers performing processes at higher temperatures, about 200° C. or higher.

[0014] Among the embodiments disclosed herein are chamber parts for a processing chamber and / or a processing chamber including such a chamber part (e.g., a semiconductor processing chamber), the chamber part including a chamber part and a metal layer (e.g., a metal plating or metal coating) on ​​at least one surface of the chamber part. The metal layer may include an advanced barrier layer in embodiments.

[0015] In some embodiments, the chamber component may include a metal layer on a surface of the substrate. The chamber component or portions thereof may be composed of, but are not limited to, one or more of metals, such as aluminum, stainless steel, and / or titanium, ceramics, such as alumina, silica, and / or aluminum nitride, and / or combinations thereof. The metal layer may be an electroless metal plating including nickel, or an electrolytic metal plating including nickel.

[0016] In some embodiments, the chamber component may be plated using an electroless plating process to form an electroless metal plating on one or more surfaces of the chamber component. In embodiments, the electroless metal plating may be a nickel phosphorus plating. The electroless plating process may directly form a metal plating on a surface of the chamber component. In some embodiments, the chamber component may be plated using an electrolytic metal plating process. For example, the electrolytic plating process may form a layer including nickel, silver, and / or gold. In some embodiments, one or more surfaces of the chamber component may be coated using a sputtering process, such as a sputtering process that sputters a nickel-containing coating onto one or more surfaces of the chamber component. The nickel-containing coating may include, for example, 98-99 atomic % nickel and 1-2 atomic % vanadium.

[0017] In some embodiments, when the chamber parts are coated by an electroless plating process, the chamber parts are placed in a bath containing nickel and phosphorus. The bath may include about 84% nickel and about 16% phosphorus, about 86% nickel and 14% phosphorus, about 88% nickel and about 12% phosphorus, about 90% nickel and about 10% phosphorus, about 92% nickel and about 8% phosphorus, about 94% nickel and about 6% phosphorus, and about 96% nickel and about 4% phosphorus. For example, the bath may include about 84-96% nickel and about 4-16% phosphorus.

[0018] In some embodiments, when the chamber parts are plated by an electrolytic metal plating process, the coating is phosphorus-free. For example, the plating can be 100% nickel. In some embodiments, the chamber parts are coated with sputtered nickel. The sputtered nickel can include nickel and vanadium, as will be understood by those skilled in the art. Vanadium can be present in the sputtered nickel at about 1% to about 2%.

[0019] In embodiments, when the chamber components include a metal layer that is electroless nickel plated or electrolytic Ni plated, the layer can be about 20 microns to about 75 microns, about 25 microns to about 70 microns, about 30 microns to 60 microns, or about 35 microns to about 50 microns in thickness.

[0020] In some embodiments, the metal layer may have a hardness of about 450HV to about 500HV. The roughness of the metal layer may be less than 50 microns in embodiments.

[0021] The thickness of the metal layer formed by electroless plating can be targeted based on the amount of time the chamber parts are in the bath. The chamber parts can be in the bath for about 1 minute to about 3 minutes to form a metal layer having the target thickness.

[0022] In some embodiments, a contamination layer may be found on the metal layer. The contamination layer may include a combination of nickel, fluorine, and / or oxygen. In an embodiment, the metal layer is a nickel layer that slowly fluorides over time due to exposure to fluorine-rich chemicals. For example, a contamination layer of nickel fluoride and / or nickel oxyfluoride may form on the surface of the metal layer. The contamination layer may react to process gases differently than the metal layer and cause slight changes in process chemistry. Additionally or alternatively, the contamination layer may flake off the chamber parts and / or cause particulate contamination on substrates processed in the process chamber in which the chamber parts are installed. As a result, periodic maintenance may be performed on the chamber parts to remove those chamber parts containing the contamination layer and replace the removed chamber parts with new chamber parts without the contamination layer.

[0023] In an embodiment, the chamber component includes a barrier layer comprising nickel oxide on a metal layer (e.g., a nickel layer). In an embodiment, the formation of a barrier layer (e.g., a nickel oxide barrier layer) on the metal layer protects the metal layer from attack by process gases, particularly against attack by fluorine-containing plasmas and other fluorine-containing chemicals. Thus, the barrier layer may be referred to as a protective layer. The nickel oxide barrier layer may be formed using an oxidation process, which may include immersing the chamber component (or a portion of the chamber component that is to have the nickel oxide barrier layer) in a bath containing an oxidizing agent (e.g., a bath containing hydrofluoric acid and / or nitric acid with water).

[0024] In some embodiments, the chamber components are treated with nickel fluoride (NiF) after removing the contaminant layer and before forming the barrier layer. 2 The nickel fluoride or nickel oxyfluoride layer is formed by depositing the metal plated chamber parts with ammonium fluoride (NH 4 The nickel fluoride layer may be produced by placing the nickel plated chamber part in a bath having an ammonium fluoride (NiF) solution. The ammonium fluoride solution may have a concentration of about 0.5M to about 3M. The metal plated chamber part remains in the bath for about 5 minutes to about 60 minutes at a temperature of about 35 to about 45°C to form a nickel fluoride or nickel oxyfluoride layer. When a nickel fluoride layer is formed, Ni is present in an amount of about 60% by weight and F is present in an amount of about 40% by weight. When a nickel oxyfluoride layer is formed, Ni is present in an amount of about 62% by weight, F is present in an amount of about 20% by weight and O is present in an amount of about 17% by weight. This nickel fluoride (NiF 2 After the nickel oxyfluoride (NiOF) layer is formed, a nickel oxide barrier layer may then be formed using the oxidation process described herein.

[0025] Experiments have shown that the use of a nickel oxide barrier layer over a nickel layer on a chamber component increases the useful life of the chamber component by a factor of 10. Thus, as compared to the number and / or frequency of preventive maintenance performed to inspect and / or replace chamber components having an exposed nickel layer, preventive maintenance may be reduced by a factor of 2 to 10 in embodiments.

[0026] Some embodiments are described herein with respect to showerheads and are particularly useful for coating chamber parts having both high aspect ratio features and areas directly exposed to bombardment by plasma. However, the barrier layers described herein may also be beneficially used on many other chamber parts having metal layers exposed to plasma, such as chamber parts for plasma etchers (also known as plasma etch reactors) or other processing chambers, including walls, liners, bases, rings, viewports, lids, nozzles, substrate holding frames, electrostatic chucks (ESCs), faceplates, selectivity control devices (SMDs), plasma sources, pedestals, etc.

[0027] Additionally, embodiments are described herein with respect to plated or coated chamber parts and other articles that may result in reduced particle contamination when used in process chambers for plasma-rich processes. However, it should be understood that the plated or coated articles described herein may also provide reduced particle contamination when used in process chambers for other processes, such as non-plasma etchers, non-plasma purifiers, chemical vapor deposition (CVD) chambers, physical vapor deposition (PVD) chambers, etc.

[0028] Referring now to the drawings, FIG. 1A is a cross-sectional view of a processing chamber 100 (e.g., a semiconductor processing chamber) having one or more chamber parts including a metal layer and a nickel oxide-containing barrier layer over the metal layer according to an embodiment of the present disclosure. The processing chamber 100 may be used for processes in which a corrosive plasma environment and / or corrosive chemicals are provided therein. For example, the processing chamber 100 may be a plasma etch reactor (also known as a plasma etcher), a plasma purifier, a chamber for performing plasma-enhanced atomic layer deposition (ALD), other deposition chambers, etc. Examples of chamber parts that may include a metal layer and a barrier layer over the metal layer include a substrate support assembly 148, an electrostatic chuck (ESC), a ring (e.g., a process kit ring or a single ring), chamber walls, a base, a showerhead 130, a gas distribution plate, a liner, a liner kit, a shield, a plasma screen, a flow equalizer, a cooling base, a chamber viewport, a chamber lid, a nozzle, a process kit ring, etc.

[0029] In one embodiment, the metal layer is a nickel-containing layer (e.g., 100% nickel or nickel in combination with one or more additional materials such as phosphorous and / or vanadium). In one embodiment, the barrier layer is a nickel oxide-containing layer (e.g., 100% nickel oxide or nickel oxide with one or more additional materials such as phosphorous and / or vanadium). The metal layer and the barrier layer can be conformal thin films.

[0030] In one embodiment, the processing chamber 100 includes a chamber body 102 and a showerhead 130 that surrounds the interior volume 106. The showerhead 130 may or may not include a gas distribution plate. For example, the showerhead may be a multi-piece showerhead including a showerhead base and a showerhead gas distribution plate bonded to the showerhead base. Alternatively, the showerhead 130 may be replaced by a lid and a nozzle in some embodiments, or by multiple pie-shaped showerhead sections and plasma generation units in other embodiments. The chamber body 102 may be made of aluminum, stainless steel, or other suitable materials. The chamber body 102 generally includes a sidewall 108 and a bottom 110. Any of the showerhead 130 (or the lid and / or the nozzle), the sidewall 108, and / or the bottom 110 may include a multi-layer plasma-resistant coating.

[0031] An outer liner 116 may be disposed adjacent the sidewall 108 to protect the chamber body 102. The outer liner 116 may be made of Al 2 O 3 or Y 2 O 3 The outer liner 116 may be a halogen-containing gas resistant material, such as, for example, a multi-layer plasma resistant ceramic coating, in some embodiments.

[0032] An exhaust port 126 may be defined in the chamber body 102 and may couple the interior volume 106 to a pumping system 128. The pumping system 128 may include one or more pumps and a throttle valve that are utilized to evacuate and regulate the pressure of the interior volume 106 of the processing chamber 100.

[0033] The showerhead 130 may be supported on the sidewall 108 of the chamber body 102 and / or on an upper portion of the chamber body. The showerhead 130 (or lid) may open to allow access to the interior volume 106 of the processing chamber 100 and may provide a seal for the processing chamber 100 while closed. A gas panel 158 may be coupled to the processing chamber 100 to provide process gases and / or cleaning gases to the interior volume 106 through the showerhead 130 or through the lid and nozzles. The showerhead 130 includes a plurality of gas supply holes 132 throughout the showerhead 130. The showerhead 130 may be or include aluminum, anodized aluminum, an aluminum alloy (e.g., Al6061), or anodized aluminum alloy. In some embodiments, the showerhead includes a gas distribution plate (GDP) bonded to the showerhead. The GDP may be, for example, Si or SiC. The GDP may further include a plurality of holes that match the holes in the showerhead.

[0034] FIG. 1B shows an enlarged view of a portion of the showerhead 130 of FIG. 1A. Referring to FIG. 1B, in an embodiment, the showerhead 130 is coated with a metal layer 150 and a barrier layer 152. In particular, in some embodiments, the surface of the showerhead and the walls of the holes 132 in the showerhead are coated with a thin conformal metal layer 150. In addition, the back surface of the showerhead 130 and the outer walls of the showerhead may also be coated with the conformal metal layer 150. A non-line of sight deposition technique, such as ALD or plating (e.g., electroplating or electroless plating), may be used to deposit or form the metal layer 150 on the surface of the showerhead 130 and on the walls of the holes 132 in the showerhead 130. Alternatively, a line of sight deposition technique, such as sputtering, may be used to form the metal layer. The metal layer 150 may be nickel, nickel doped with phosphorus, or nickel doped with vanadium, in an embodiment.

[0035] The barrier layer 152 covers the metal layer 150 in some or all areas of the surface of the showerhead 130. The barrier layer 152 may be formed using an oxidation process, which may be a dry oxidation process or a wet oxidation process (e.g., by immersing the showerhead 130 in a bath containing an oxidizing agent, such as hydrofluoric acid or nitric acid). The barrier layer 152 may cover the metal layer on all surfaces of the chamber components, including on the interior walls of the holes in the showerhead 130. The barrier layer may be a grown layer and, in embodiments, may be conformal and uniform. A uniform barrier layer, in embodiments, may have a difference in thickness of less than about 10% across the surface of the showerhead.

[0036] Examples of process gases that may be used to process the substrate in the process chamber 100 include, among others, C 2 F 6 ,SCIENCE FICTION 6 , SiCl 4 , HBr, NF 3 , C.F. 4 , CHF 3 , C.H. 2 F 3 , F, Cl 2 , CCl 4 , BCl 3 and SiF 4 Halogen-containing gases such as O 2 , or N 2 There are other gases such as O. An example of a carrier gas is N, which is inert to the process gas. 2 , He, Ar, and other gases (e.g., non-reactive gases). Fluorine-based gases may cause fluoride deposits to build up on the holes of a standard showerhead and / or may cause a contamination layer to form on the holes of the showerhead. However, the holes 132 of the showerhead 130 may be resistant to such fluoride buildup due to the barrier layer 152.

[0037] 1A , a substrate support assembly 148 is disposed in the interior volume 106 of the processing chamber 100 below the showerhead 130. The substrate support assembly 148 holds a substrate 144 (e.g., a wafer) during processing. The substrate support assembly 148 may include an electrostatic chuck that secures the substrate 144 during processing, a metal cold plate bonded to the electrostatic chuck, and / or one or more additional components. An inner liner may cover the periphery of the substrate support assembly 148. The inner liner may be Al 2 O 3 or Y 2 O 3 The substrate support assembly, portions of the substrate support assembly, and / or the inner liner may be coated with a metal layer and a barrier layer in some embodiments.

[0038] FIG. 2 illustrates one embodiment of a bottom view of a showerhead 200. The showerhead 200 may have a series of gas conduits 204 arranged concentrically (also called holes) that evenly distribute plasma gas directly over the substrate or wafer to be etched or processed. The showerhead is shown here as having approximately 1100 gas conduits 204 arranged in evenly distributed concentric rings for even distribution of gas. In another embodiment, the gas conduits 204 may be arranged in alternative geometric configurations on the underside 205 of the showerhead (or on the underside of a GDP coupled to the showerhead). For example, the showerhead may have a square or rectangular configuration with rows and columns of gas conduits 204. It should be understood that other shapes (e.g., triangular, pentagonal, etc.) may be implemented and may be coated with a ceramic coating (e.g., HPM coating) as described above. The showerhead 200 may have a large number of gas conduits 204 as shown, or as few as appropriate, depending on the type of reactor and / or process utilized.

[0039] In an embodiment, some or all of the gas conduits 204 do not include branches (e.g., each gas conduit may have a single inlet point and a single outlet point). Furthermore, the gas conduits may have various lengths and orientation angles. Gas may be supplied to the gas conduits 204 via one or more gas supply nozzles. Some gas conduits 204 may receive gas before other gas conduits 204 (e.g., due to their proximity to the gas supply nozzles). However, the gas conduits 204 may be configured to supply gas to a substrate below the showerhead at approximately the same time based on varying the orientation angle, diameter, and / or length of the gas conduits 204 or by using additional flow equalizers. For example, the gas conduits 204 that receive gas first may be longer and / or have a larger angle (e.g., an angle even greater than 90 degrees) than the conduits that receive gas later.

[0040] As can be seen in FIG. 3A, a schematic diagram 300 of oxidizing a metal plated coated chamber part is shown. In FIG. 3A, the metal plated chamber part includes a nickel layer 301 and a bare aluminum body 302 of the chamber part, the nickel layer 301 being on the surface of the bare aluminum body 302. The metal plated chamber part is subjected to an oxidation process 305 according to the present disclosure. After being oxidized, the metal plated chamber part includes a dense barrier layer 303 of nickel oxide on the surface of the nickel layer 301. The NiO barrier layer 303 may prevent tarnishing of the metal layer. The barrier layer 303 may also prevent the chamber part from being a source of particles on the substrate being processed. The NiO barrier layer 303 may also inhibit the reaction of fluorine with the nickel in the nickel layer 301 to prevent the formation of a tarnishing / contaminated layer.

[0041] Additionally, the barrier layer 303 may prevent native oxide from forming on the nickel layer 1 .

[0042] In some embodiments, the chamber part may be a used chamber part that was used to perform one or more processes on a substrate, which processes exposed the substrate to a fluorine-rich environment. The chamber part may not have been coated with a barrier layer prior to use. Thus, the chamber part may include a contamination layer on top of the metal layer 302. In some embodiments, the chamber part may be refurbished by removing the contamination layer to expose the metal layer and then forming a barrier layer on the metal layer. Such an embodiment is shown generally in schematic 350 of FIG. 3B.

[0043] 3B, the chamber component includes an aluminum body 302 having a metal layer 301 disposed thereon and a contamination layer 310 on the metal layer 301. The chamber component may be subjected to a cleaning process 315 to strip the contamination layer 310 from the metal layer 301. The chamber component with the cleaned metal layer 301 may then be treated using an oxidation process 305 to form a barrier layer 303, as described in more detail in this disclosure. After cleaning and oxidation, the contamination layer 310 is removed and a dense nickel oxide barrier layer 303 is present on the metal layer 301.

[0044] 4 illustrates an exemplary architecture of a manufacturing system 400. The manufacturing system 400 may be a manufacturing system for applying plating and / or coatings to articles, such as chamber parts. In one embodiment, the manufacturing system 400 includes a manufacturing machine 401 (e.g., processing equipment) connected to an equipment automation layer 415. The manufacturing machine may include a polisher 402, one or more wet cleaners 403, a plating system 404, a sputtering system 405, an oxidation system 406, and / or other machines. The manufacturing system 400 may further include one or more computing devices 420 connected to the equipment automation layer 415. In alternative embodiments, the manufacturing system 400 may include more or fewer components. For example, the manufacturing system 400 may include a manufacturing machine 401 that is operated manually (e.g., offline) without the equipment automation layer 415 or the computing device 420.

[0045] The polisher 402 is a machine configured to polish or smooth the surface of an article, such as a chamber part for a processing chamber. The polisher 402 can be, for example, a chemical mechanical planarization (CMP) device or an abrasive polisher. For example, a motorized polishing pad can be used to smooth the surface of the article. A sander can rotate or vibrate the polishing pad while it is pressed against the surface of the article. The roughness achieved by the polishing pad can depend on the applied pressure, the vibration or rotation rate and / or the roughness of the polishing pad.

[0046] The wet cleaner 403 is a cleaning device that cleans an article (e.g., an article) using a wet cleaning process. The wet cleaner 403 includes a wet bath filled with liquid, and a substrate is immersed in the wet bath to clean the substrate. The wet cleaner 403 may use ultrasound to agitate the wet bath during cleaning to improve the cleaning effect, which is referred to herein as sonicating the wet bath.

[0047] In some embodiments, the wet cleaner 403 includes a first wet cleaner containing deionized (DI) water and a second wet cleaner containing an acidic solution, which in embodiments may be a hydrofluoric acid (HF) solution, a hydrochloric acid (HCl) solution, a nitric acid (HNO 3 ) solution, or a combination thereof. The acidic solution may remove surface contaminants from the article and / or remove oxides from the surface of the article. Cleaning the article having a metal layer with an acidic solution prior to forming a barrier layer thereon may improve the quality of the barrier layer formed on the metal layer. In one embodiment, an acidic solution containing about 5-15% by volume HF is used to clean a chamber part having a nickel layer. In one embodiment, an acidic solution containing about 5-15% by volume HNO is used to clean an article having a nickel layer. 3 An acidic solution containing is used.

[0048] The wet cleaner 403 may clean the article at multiple stages during processing. For example, the wet cleaner 403 may clean the article after a substrate is polished, before performing plating (e.g., electroplating), before forming a barrier layer over a metal plating, etc.

[0049] In other embodiments, alternative types of cleaners may be used to clean the article, such as dry cleaners. Dry cleaners may clean the article by applying heat, applying gas, applying plasma, etc.

[0050] The plating system 404 is a system that performs electroplating (e.g., of Ni) or electroless plating (e.g., of Ni). The plating system 404 may be an electroplating system that applies an electric current to reduce dissolved metal cations so that they form a thin, adherent metal coating on the article (e.g., on the surface of a chamber part, such as an aluminum chamber part). In particular, the article to be plated may be the cathode of the circuit, and the metal donor may be the anode of the circuit. The article and the metal donor may be immersed in an electrolyte containing one or more dissolved metal salts and / or other ions that increase the conductivity of the electrolyte. Metal from the metal donor then plates the surface of the article.

[0051] Another type of plating system that may be used is an electroless plating system, which performs electroless plating. Electroless plating, also known as chemical plating or autocatalytic plating, is a non-galvanic plating method that involves several simultaneous reactions in an aqueous solution, which occur without the use of external power. The reaction is accomplished when a reducing agent, usually sodium hypophosphite or thiourea, releases hydrogen and oxidizes, thereby creating a negative charge on the surface of the part.

[0052] The equipment automation layer 415 may interconnect some or all of the manufacturing machines 401 with the computing device 420, other manufacturing machines, metrology tools, and / or other devices. The equipment automation layer 415 may include a network (e.g., a location area network (LAN)), routers, gateways, servers, data stores, etc. The manufacturing machines 401 may connect to the equipment automation layer 415 via a Semiconductor Equipment Communication Standard / Generic Manufacturing Equipment Interface, via an Ethernet interface, and / or via other interfaces. In one embodiment, the equipment automation layer 415 enables process data (e.g., data collected by the manufacturing machines 401 during process execution) to be stored in a data store (not shown). In an alternative embodiment, the computing device 420 connects directly to one or more of the manufacturing machines 401.

[0053] In one embodiment, some or all of the manufacturing machines 401 include a programmable controller that can load, store, and execute process recipes. The programmable controller may control temperature settings, gas and / or vacuum settings, time settings, etc. of the manufacturing machines 401. The programmable controller may include a main memory (e.g., read only memory (ROM), flash memory, dynamic random access memory (DRAM), static random access memory (SRAM), etc.) and / or a secondary memory (e.g., a data storage device, such as a disk drive). The main memory and / or the secondary memory may store instructions for performing the thermal treatment processes described herein.

[0054] The programmable controller may also include a processing device coupled (e.g., via a bus) to the main memory and / or secondary memory for executing instructions. The processing device may be a general-purpose processing device, such as a microprocessor, central processing unit, etc. The processing device may also be a special-purpose processing device, such as an application specific integrated circuit (ASIC), a field programmable gate array (FPGA), a digital signal processor (DSP), a network processor, etc. In one embodiment, the programmable controller is a programmable logic controller (PLC).

[0055] In one embodiment, the manufacturing machine 401 is programmed to execute recipes that cause the manufacturing machine to polish an article, clean the article, plate the article, form a barrier layer on the article, etc. In one embodiment, the manufacturing machine 401 is programmed to execute recipes that perform operations of a multi-step process for manufacturing an article having a metal layer and a barrier layer, as described with reference to Figures 5-6. The computing device 420 may store one or more plating, oxidation, cleaning and / or polishing recipes 425 that may be downloaded to the manufacturing machine 401 to cause the manufacturing machine 401 to manufacture an article according to an embodiment of the present disclosure.

[0056] FIG. 5 is a flow chart depicting a method 500 of repairing an advanced barrier oxide layer and forming an advanced barrier oxide layer on a chamber component, according to one embodiment. The method 500 may be performed on a chamber component having a metal layer (e.g., metal plated) that has been used to perform one or more cycles of one or more manufacturing processes that expose the chamber component to chemicals that cause a contamination layer to form on the metal layer. The contamination layer may include oxygen, fluorine, and / or one or more process elements. The contamination layer may cause particulate contamination and / or adversely affect future processes performed in the process chamber in an embodiment. Thus, in some embodiments of the present disclosure, when a contamination layer is present on a metal plated chamber component, the chamber component is placed in a first bath 502. The first bath is a mixture of water and a first acid (e.g., hydrofluoric acid, nitric acid (HNO 3 ), sulfuric acid (H 2 SO 4 ), oxalic acid (HC 2 O 4 ), or ammonium fluoride (NH 4 F). The hydrofluoric acid may be included in the bath in an amount of about 5% to about 15% by weight, based on the total composition of the first bath. The water may be included in the bath in an amount of about 85% to about 95% by weight, based on the total composition of the bath. In some embodiments, the first bath includes about 5% by weight hydrofluoric acid and about 95% by weight water. The first bath may be at a temperature of about 25° C. to about 35° C. The used metal-plated chamber parts may be placed in the first bath for about 1 minute to about 30 minutes to strip the contaminant layer. After immersion in the first bath, the metal-plated chamber parts may include the stripped contaminant layer. The metal-plated chamber parts may then be rinsed (e.g., with deionized water) and dried in block 504 to remove the stripped contaminant layer.

[0057] The metal plated chamber parts are then placed in a first or second bath at block 506. The second bath includes water and an acid (e.g., hydrofluoric acid). The acid may be included in the bath in an amount of about 5% to about 15% by weight, based on the total composition of the first or second bath. The water may be included in the bath in an amount of about 85% to about 95% by weight, based on the total composition of the first or second bath. In some embodiments, the second bath includes about 5% by weight hydrofluoric acid and about 95% water. The second bath may be at a temperature of about 25° C. to about 35° C. The used metal plated chamber parts may be placed in the second bath for about 1 minute to about 30 minutes, and any remaining contaminant layer may be removed. After the second bath, the metal plated chamber parts may be rinsed (e.g., with deionized water) and dried 508.

[0058] The metal plated chamber part may then be polished 510 after removing the contamination layer. The metal plated chamber part may be polished using an automated polisher with different polishing sheets, such as Scotch-Brite® sheets, or another advanced method to uniformly polish the surface. The metal plated coated chamber part may be polished until the surface roughness is about 10 μin to about 20 μin in one embodiment. After polishing, the metal plated coated chamber part may undergo an oxidation treatment 512. The oxidation treatment may be performed by placing the metal plated coated chamber part in a third bath. The third bath may be a mixture of water and an acid (e.g., nitric acid (HNO 3 ), sulfuric acid (H 2 SO 4 ), oxalic acid (HC 2 O 4 ), or ammonium fluoride (NH 4F). The acid may be present in the bath in an amount of about 5% to about 25% by weight, based on the total composition of the third bath. The water may be present in the bath in an amount of about 75% to about 95% by weight, based on the total composition of the third bath. In some embodiments, the third bath may include about 5% by weight hydrofluoric acid and about 95% by weight water. The third bath may be at a temperature of about 25° C. to about 35° C. The metal plated chamber parts may be placed in the third bath for about 1 minute to about 30 minutes. The oxidized metal plated chamber parts may be rinsed (e.g., with deionized water) and a nickel oxide layer may be formed on the surface of the metal plating layer. The nickel oxide layer may be between about 5 nanometers and about 35 nanometers in one embodiment.

[0059] In another embodiment, the metal plated coated chamber part may be a new component, and the new component may be oxidized by a second method 600. FIG. 6 is a flow chart depicting a method of forming an advanced barrier layer on a metal plated or metal coated chamber part, according to one embodiment. In the second method 600, the metal plated chamber part is placed 602 in a first bath. The first bath may include water and an acid (e.g., hydrofluoric acid). The hydrofluoric acid may be included in the bath in an amount of about 5% to about 25% by weight, based on the total composition of the first bath. The water may be included in the bath in an amount of about 75% to about 95% by weight, based on the total composition of the bath. In some embodiments, the first bath includes about 5% by weight hydrofluoric acid and about 95% by weight water. The first bath may be at a temperature of about 25° C. to about 35° C. The metal plated chamber part may be placed in the first bath for about 1 minute to about 30 minutes. After the first bath 604, the metal plated chamber parts may be rinsed (eg, with deionized water) and dried 606.

[0060] Once dried, the metal plated chamber parts are then rinsed with an acid (e.g., hydrofluoric acid or nitric acid (HNO 3)) 608. The metal plated coated chamber part may be treated for a time period between about 1 minute and about 30 minutes until a target thickness of the nickel oxide layer is achieved. The nickel oxide layer may be between about 5 nanometers and about 30 nanometers, such as about 15 nanometers, in embodiments. The metal plated coated chamber part is then rinsed with deionized water and dried in block 610.

[0061] In another embodiment, the metal plated coated chamber parts may have a nickel fluoride or nickel oxyfluoride layer, which may be a new component to oxidize the chamber parts. FIG. 7 shows the deposition of nickel fluoride (NiF) in accordance with one embodiment. 2 7 is a flow chart depicting a method of forming an advanced barrier layer on a metal plated or metal coated chamber component having a nickel oxyfluoride (NiOF) layer or a nickel oxyfluoride (NiOF) layer. The chamber component is placed in a first bath and rinsed in steps 702-706 as described in steps 602-606 of FIG. 6. After rinsing and drying the chamber component, the chamber component is then placed 708 in a second bath containing an ammonium fluoride solution to form a nickel fluoride or nickel oxyfluoride layer. The ammonium fluoride solution has a concentration of about 0.5M to about 3M. The chamber component remains in the second bath for about 5 minutes to about 60 minutes, and the second bath contains a nickel oxyfluoride (NiOF) layer. 2 6, or a temperature of about 35-45° C. to form a NiOF layer. The chamber parts are then removed from the bath 710. The chamber parts are then rinsed and dried in step 712, as described above for step 606 of FIG. 6. 2 After formation of the NiOF layer, the chamber component is oxidized 718 with an acid (e.g., hydrofluoric acid or nitric acid (HNO )) to oxidize the metal plating layer and form a nickel oxide layer, as described above in steps 512 and 608 of FIG. 5 and FIG. 6 , respectively. 3 )) can be processed.

[0062] In another embodiment, the metal plated chamber part can be oxidized by an in situ method. The method can be performed in the same chamber in which the chamber part is coated with the nickel plated coating or in the chamber in which the part is to be used. In the first step of the in situ method, the metal plated chamber part can be treated with a gas and moisture while the chamber part is in the chamber. The gas can be NH 3 , N.F. 3 , HF or H 2 In some embodiments, the gas may be selected from the group consisting of NH 3 and NF 3 or in combination with NH 3 and NF 3 and HF. The gas may be at a concentration of about 5 sccm to about 2000 sccm of total gas. The gas reacts with ambient moisture in the chamber. The temperature of the chamber may be about 150° C. to about 220° C. The nickel oxide coating layer may have a thickness of about 4 nm to about 50 nm.

[0063] By treating the part with an oxidation treatment to form a barrier layer as described herein, the inventors have discovered that the life of the part can be more than 10 times longer than the life of the original coating without the barrier layer. When chamber parts with an ENP coated layer are used, the standard life is about 3000 cycles. When a barrier nickel oxide layer is present on the ENP coated layer, the life of the part is extended by more than nearly 10 times the standard life of the part, with the life exceeding 10,000 cycles.

[0064] Additionally, the inventors have discovered that the oxidation method can be used to coat new parts and to repair existing parts where a contamination layer has formed. EXAMPLES

[0065] Illustrative Examples The following examples are provided to aid in understanding the present disclosure and should not be construed as explicitly limiting the present disclosure as described and claimed herein. Variations of the present disclosure, including the substitution of all equivalents now known or later developed that would be within the purview of one of ordinary skill in the art, and changes in formulation or minor changes in experimental design should be considered to fall within the scope of the present disclosure, which is incorporated herein.

[0066] Example 1 - Pretreatment of a showerhead to be ENP coated A showerhead having nickel plating and a nickel oxide barrier layer on the nickel plating is exemplified herein. First, the showerhead was coated with a nickel layer using a metal plating process. Prior to the intentional formation of the nickel oxide layer, a native oxide layer was formed on the nickel plating. The native nickel oxide layer has inferior properties and also prevents the formation of a target nickel oxide layer that reduces particulate contamination and improves the life of chamber components. The native nickel oxide layer may have a thickness of about 2-3 nm. The showerhead was then oxidized by placing the showerhead in a bath of 5% (5%-25%) hydrofluoric acid and 95% water at a temperature between 25°C and 35°C. After 40 minutes, the showerhead was removed from the bath and rinsed with deionized water. A barrier nickel oxide layer was formed on the nickel layer. The barrier nickel oxide (NiO) layer on the metal layer had a thickness of about 6 nm to about 22 nm.

[0067] Example 2 - Cleaning and Oxidation of an ENP Coated Showerhead A showerhead with nickel plating (nickel ENP) was used as an example herein, and a contamination layer was formed on the showerhead as a result of use. The total thickness of the contamination layer (i.e., fluorinated or oxyfluorinated layer) was greater than 5-200 nm.

[0068] To remove the contamination layer, the showerhead was cleaned by placing it in a first bath of 5% (5%-25%) hydrofluoric acid and 95% water at 25-40° C. for 40 minutes. The showerhead was then removed from the first bath, rinsed with deionized water, and dried. After drying the showerhead, the showerhead was then placed in a second bath of 25% hydrofluoric acid and 75% water at 25-40° C. for 40 minutes. The showerhead was then removed from the second bath, rinsed again with deionized water, and dried.

[0069] As a result of the cleaning, the contamination layer was removed from the showerhead. The showerhead was then treated and oxidized by placing it in a bath of 5% hydrofluoric acid to form a barrier layer on the ENP layer. As a result of the treatment and oxidation, a barrier nickel oxide layer was formed on the ENP layer. The barrier nickel oxide (NiO) layer on the ENP coating layer had a composite thickness of about 22 nm. The EDS line profile of the barrier NiO layer on the ENP layer showed that nickel was present in the barrier NiO layer and that there was no phosphorus in such layer. Also, TEM images and EDS line profiles were taken inside the small holes in the showerhead, which showed that the barrier layer had a thickness between 6.3 nm and 31.2 nm.

[0070] They also measured that the barrier layer on the backside of the showerhead had a thickness of about 19-30 nm, which was also shown in the EDS line profile, confirming that the barrier nickel oxide layer formed along the entire showerhead and was not limited to just the front side of the showerhead.

[0071] Example 3 - Fluorination and oxidation of ENP coated showerhead A fluoride (NiF) film having a thickness of about 6 nm to about 50 nm is 2 To convert the NiOF or NiOxyfluoride (NiOF) layers, ammonium fluoride (NH) with a concentration of 0.5M to 3M was used. 4Exemplary herein are showerheads with nickel plating (Nickel ENP) coatings that have been treated with a solution of NiO (NiENP) by placing the showerhead in a bath of 5% (5%-25%) hydrofluoric acid and 95% water at a temperature between 25-35° C. to have a NiO thickness of about 6 nm to about 50 nm.

[0072] We also took SEM images of the barrier layer on the ENP-coated showerhead. From the SEM images, the weight percentages of C, O, P and Ni were calculated and presented in Table 1. Note that P comes from the ENP layer. TIFF2024536969000002.tif74170

[0073] The foregoing description sets forth numerous specific details, such as examples of specific systems, components, methods, etc., to provide a good understanding of some embodiments of the present invention. However, it will be apparent to those skilled in the art that at least some embodiments of the present invention may be practiced without these specific details. In other instances, well-known components or methods are not described in detail or are presented in simple block diagram form to avoid unnecessarily obscuring the present invention. Thus, the specific details described are merely examples. It is contemplated that a particular implementation may differ from these exemplary details and still be within the scope of the present invention.

[0074] References throughout this specification to "one embodiment" or "an embodiment" mean that a particular feature, structure, or characteristic described with respect to an embodiment is included in at least one embodiment. Thus, the appearances of the phrases "in one embodiment" or "in an embodiment" in various places throughout this specification do not necessarily all refer to the same embodiment. Furthermore, the term "or" is intended to mean an inclusive "or" rather than an exclusive "or". When the term "about" or "approximately" is used herein, this is intended to mean that the nominal value presented is accurate to within ±10%.

[0075] Although the operations of the methods herein have been illustrated and described in a particular order, the order of the operations of each method may be changed such that some operations may be performed in the reverse order, or such that certain operations may be performed at least in part concurrently with other operations. In alternative embodiments, instructions, or sub-operations of separate operations, may be performed intermittently and / or alternately.

[0076] It should be understood that the above description is illustrative, and not restrictive. Many other embodiments will be apparent to those skilled in the art upon reading and understanding the above description. The scope of the invention should therefore be determined with reference to the appended claims, along with the full scope of equivalents to which such claims are entitled.

Claims

1. 1. A chamber component for a processing chamber, comprising: The main body, a metal plating on at least one surface of the body, the metal plating comprising nickel; and a barrier layer on the metal plating, the barrier layer comprising nickel oxide; and A chamber component for a processing chamber comprising:

2. The chamber component of claim 1 , wherein the metal plating comprises nickel and phosphorous.

3. The chamber component of claim 1 , wherein the metal plating comprises nickel and is phosphorous-free.

4. The chamber component of claim 1 , wherein the body comprises aluminum, an aluminum alloy, aluminum nitride, alumina, or a combination thereof.

5. 10. The chamber component of claim 1, wherein the metal plating has a thickness of about 20 microns to about 75 microns and the barrier layer has a thickness of about 2 nm to about 50 nm.

6. 10. The chamber component of claim 1, wherein the barrier layer has an average surface roughness (Ra) of about 2 microinches to about 60 microinches.

7. The chamber part of claim 1 , wherein the chamber part comprises a showerhead for a process chamber.

8. 1. A method for protecting a chamber component, comprising: forming a metal plating on a body of the chamber component, the metal plating comprising nickel; contacting the metal plating with an oxidizing agent to form a barrier layer on the metal plating, the barrier layer comprising nickel oxide; A method for protecting a chamber part, comprising:

9. The method of claim 8 , wherein the oxidizing agent comprises at least one of hydrofluoric acid, oxalic acid, or nitric acid.

10. The method of claim 8 , wherein the barrier layer has a thickness of about 2 μm to about 60 μm.

11. The method of claim 8 , wherein forming the metal plating comprises performing electroless metal plating, the metal plating further comprising phosphorus.

12. The method of claim 8 , wherein the body comprises an aluminum alloy, aluminum nitride, alumina, or a combination thereof.

13. removing native oxide from said metal plating prior to forming said barrier layer; The method of claim 8 , further comprising:

14. 9. The method of claim 8, further comprising, after said forming said metal plate, forming a nickel fluoride (NiF2) or nickel oxyfluoride layer on said metal plate by contacting said metal plate with ammonium fluoride.

15. placing the chamber parts in an acid bath comprising 5 to 25% hydrofluoric acid and 75 to 95% water to contact the metal plating with the oxidizing agent; Thereafter, placing the chamber parts in a deionized water bath; Thereafter, placing the chamber parts in the acid bath; Thereafter, placing the chamber in the deionized water bath. The method of claim 8 , further comprising:

16. 1. A method for refurbishing a used chamber part, comprising: removing a contaminant layer from a metal plating on the used chamber part using a first acidic solution, the metal plating comprising nickel; thereafter, contacting the metal plating with an oxidizing agent to form a barrier layer on the metal plating, the barrier layer comprising nickel oxide; A method comprising:

17. The method of claim 15 , wherein the contamination layer comprises nickel fluoride.

18. removing the contaminant layer, placing the used chamber parts in a first acid bath; Thereafter, rinsing the used chamber parts with deionized water; Thereafter, drying the used chamber parts; Thereafter, placing the used chamber part in a second acid bath; Thereafter, rinsing the used chamber parts with deionized water; Thereafter, drying the used chamber parts.

20. The method of claim 17, comprising:

19. The method of claim 15 , wherein the oxidizing agent comprises at least one of hydrofluoric acid or nitric acid.

20. The method of claim 15 , wherein the barrier layer has a thickness of about 2 μm to about 60 μm.

Citation Information

Patent Citations

  • Formation of black film

    JP1986253383A

  • Method and system for cleaning process under high temperature, corrosive plasma environment

    JP1998312976A

  • Metal material or metal film having fluorinated surface layer and fluorinating method

    JP1999092912A

  • Heat resistant and corrosion resistant member for vacuum use, vacuum apparatus having parts obtained by using the same member and coating method therefor

    JP2003342752A

  • Corrosion resistant material, and its production method

    JP2004360066A