Wafer receiving, electrochemical porosification apparatus and method of using same - Patents.com

The wafer receiver with a vacuum-assisted mechanism and resilient sealing element addresses deformation issues in existing devices, ensuring uniform hole growth and improved quality of porous semiconductor wafers.

JP2024537753APending Publication Date: 2024-10-16ソクプラ シオンス エ ジェニ エスウーセ
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2024518865
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-09-27
Filing Date
2022-09-27
Publication Date
2024-10-16

AI Technical Summary

Technical Problem

Existing electrochemical porosification devices disturb the front surface of semiconductor wafers and may deform them, limiting the area for hole growth and compromising the quality of porous semiconductor wafers.

Method used

A wafer receiver with an electrode body, annular sealing element, and vacuum-assisted mechanism that maintains the wafer in place without deformation, allowing for uniform hole growth by creating a vacuum to compress the sealing element and bring the wafer's back surface into contact with the electrode, using a resilient material resistant to etching solutions.

Benefits of technology

The solution ensures uniform hole growth across the semiconductor wafer's surface without deformation, enhancing the quality of porous layers by maintaining the wafer's integrity during the porosification process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024537753000001_ABST
    Figure 2024537753000001_ABST
Patent Text Reader

Abstract

A wafer receiver for use in an electrochemical porosification process is described, the wafer receiver generally comprising an electrode body having a first planar surface and a second planar surface opposite the first planar surface, a groove recessed from the first planar surface and running within a central region of the electrode body, a pedestal extending annularly around the central region of the electrode body and recessed from the first planar surface, a conduit in fluid communication with the groove and connectable to a vacuum pump; and an annular sealing element received in the pedestal, the annular sealing element being made of a resilient material that is resistant to the electrochemical porosification process, the annular sealing element having a wafer receiving surface that protrudes from the first planar surface when received in the pedestal.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] Field The present improvements relate generally to semiconductor wafers and, more specifically, to electrochemical porosification processes performed on semiconductor wafers. [Background technology]

[0002] background Electrochemical porosification is a process that creates a porous layer in a semiconductor wafer, such as a silicon or germanium wafer. The porous silicon or germanium layers resulting from such processes have been found to be useful in many applications, including microelectromechanical systems (MEMS), solar cells, distributed Bragg reflectors, microcavities, and waveguides, to name a few. The porosification process can be carried out using an electrochemical porosification apparatus that contacts the backside of the semiconductor wafer with a first electrode and exposes the frontside of the semiconductor wafer to an etching solution, such as a solution containing hydrofluoric (HF) acid. A voltage is then applied between the first electrode and a second electrode that is immersed in the etching solution. When key parameters are appropriately set, hole growth by semiconductor dissolution begins, as known in the art, where the semiconductor wafer is exposed to the etching solution. To maintain the semiconductor wafer in place within the etching solution, it is known to press the semiconductor wafer against a first electrode by pressing an annular member onto a peripheral region of a first side of the semiconductor wafer, thereby exposing a central region of the front side of the semiconductor wafer to the etching solution by virtue of the annular member being hollow. Although existing electrochemical porosification devices are somewhat satisfactory, there remains room for improvement. Summary of the Invention

[0003] overview It has been found that there is a need in the art for an electrochemical porosification apparatus and method that avoids disturbing a portion of the front surface of the semiconductor wafer and increases the area over which pores can grow. It has further been found that, at least in some circumstances, the force exerted by the annular member on the semiconductor wafer can undesirably deform it, which can be detrimental when high quality porous semiconductor wafers are desired.

[0004] According to a first aspect of the present disclosure, there is provided a wafer receiver for use in an electrochemical porosification process, the wafer receiver comprising: an electrode body having a first planar surface and a second planar surface opposite the first planar surface, a groove recessed from the first planar surface and running within a central region of the electrode body, a pedestal extending annularly around the central region of the electrode body and recessed from the first planar surface, a conduit in fluid communication with the groove and connectable to a vacuum pump; and the wafer receiver comprising an annular sealing element received in the pedestal. the annular sealing element is made of a resilient material that is resistant to the electrochemical porosification process, the annular sealing element having a wafer receiving surface that protrudes from the first planar surface when received on the pedestal; a vacuum pump is operable to create a vacuum to draw air from the conduits and grooves when a semiconductor wafer is received on the wafer receiving surface of the annular sealing element, the vacuum drawing the semiconductor wafer toward the first planar surface, the drawing including compressing the annular sealing element to bring the wafer receiving surface flush with the first planar surface and causing a backside of the semiconductor wafer and the first planar surface to be in physical contact with each other.

[0005] Further, according to the first aspect of the present disclosure, the elastic material can be, for example, a fluoroelastomer material.

[0006] Still further, according to the first aspect of the present disclosure, the elastic material may be, for example, a polytetrafluoroethylene (PTFE) material.

[0007] Still further, according to the first aspect of the present disclosure, the groove may, for example, include a plurality of grooves in fluid communication with at least the conduit.

[0008] Still further, according to the first aspect of the present disclosure, the electrode body may be made of, for example, a corrosion resistant material.

[0009] Still further, according to the first aspect of the present disclosure, in the rest position the wafer receiving surface may have a plane that is spaced apart from the plane of the first planar surface of the electrode body, for example by a spacing.

[0010] Still further, according to the first aspect of the present disclosure, the spacing may, for example, be in the range of about 0.5 mm to 3 mm, preferably in the range of about 1 mm to 2 mm, and most preferably in the range of about 1 mm to 1.5 mm.

[0011] Still further, according to the first aspect of the present disclosure, the annular sealing element may have, for example, a rectangular cross-sectional shape.

[0012] Still further, according to the first aspect of the present disclosure, the annular sealing element may have, for example, an outer surface and a core extending within the outer surface, the outer surface being resistant to the electrochemical porosification process and the core being made of a resilient material.

[0013] According to a second aspect of the present disclosure, there is provided an electrochemical porosification apparatus having: a container defining an internal cavity; a first electrode located within the internal cavity; a wafer receiver located within the internal cavity and spaced from the first electrode, the wafer receiver having: an electrode body having a first planar surface and a second planar surface opposite the first planar surface, a groove recessed from the first planar surface and running within a central region of the electrode body, a pedestal extending annularly around the central region of the electrode body and recessed from the first planar surface, a conduit in fluid communication with the groove and connectable to a vacuum pump; and the wafer receiver having an annular sealing element received in the pedestal, the annular sealing element being made of a resilient material that is resistant to acid, the annular sealing element having a wafer receiving surface that protrudes from the first planar surface when received in the pedestal; The electrochemical porosification apparatus has a vacuum pump in fluid communication with the conduit and operable to create a vacuum to draw air from the conduit and the groove, the vacuum pulling a semiconductor wafer received on the wafer receiving surface of the annular sealing element toward the first planar surface, the pulling including compressing the annular sealing element to make the wafer receiving surface flush with the first planar surface and causing the backside of the semiconductor wafer and the first planar surface to be in physical contact with each other; the electrochemical porosification apparatus has an etching solution source in fluid communication with the internal cavity and configured to flood at least a portion of the internal cavity with an etching solution; and the electrochemical porosification apparatus has a current source configured to convey an electric current across the etching solution using a first electrode and an electrode body, the electric current and the etching solution creating pores in the exposed surface of the semiconductor wafer.

[0014] Furthermore, according to the second aspect of the present disclosure, the elastic material can be, for example, a fluoroelastomer material.

[0015] Still further, according to a second aspect of the present disclosure, the elastic material may be, for example, a polytetrafluoroethylene (PTFE) material.

[0016] Still further, according to the second aspect of the present disclosure, the groove may, for example, include a plurality of grooves in fluid communication with at least the conduit.

[0017] Still further, according to the second aspect of the present disclosure, the electrode body may be made of, for example, a corrosion resistant material.

[0018] Still further, according to the second aspect of the present disclosure, in the rest position, the wafer receiving surface may have a plane spaced apart from the plane of the first planar surface of the electrode body by a distance, for example, in the range of about 1 mm to 5 mm, preferably in the range of about 1 mm to 3 mm, and most preferably in the range of about 1 mm to 2 mm.

[0019] Still further, according to the second aspect of the present disclosure, the annular sealing element may have, for example, a rectangular cross-sectional shape.

[0020] According to a third aspect of the present disclosure, there is provided a method of performing an electrochemical porosification process on a semiconductor wafer, the method comprising: receiving a backside of the semiconductor wafer onto an annular sealing element, the annular sealing element being resistant to an etching solution and resilient; creating a vacuum in a cavity enclosed by the backside of the semiconductor element, the vacuum drawing air from the cavity pulling the semiconductor wafer towards a flat surface of an electrode body, said pulling including compressing the annular sealing element to bring a wafer receiving surface of the annular sealing element flush with the flat surface and causing the backside and flat surfaces of the wafer to be in physical contact with each other; while maintaining the vacuum, immersing an exposed surface of the semiconductor wafer in an etching solution and conveying an electric current across the etching solution using another electrode spaced apart from the electrode body, the etching solution and electric current creating pores in the exposed surface of the semiconductor wafer.

[0021] Further, according to a third aspect of the present disclosure, the method may further include, for example, upon removal of the vacuum, the annular sealing element expanding and moving the semiconductor wafer away from the electrode body.

[0022] Still further, according to a third aspect of the present disclosure, the semiconductor wafer may be, for example, one of a silicon wafer and a germanium wafer.

[0023] Still further, according to a third aspect of the present disclosure, the etching solution may include, for example, a hydrogen fluoride (HF) solution.

[0024] According to a fourth aspect of the present disclosure, there is provided a wafer receiver for use in an electrochemical porosification process, the wafer receiver comprising: an electrode body having a first planar surface and a second planar surface opposite the first planar surface, a groove recessed from the first planar surface and running within a central region of the electrode body, a pedestal extending annularly around the central region of the electrode body and recessed from the first planar surface, a conduit in fluid communication with the groove and connectable to a vacuum pump; and an annular sealing element received in the pedestal, the annular sealing element being made of a resilient material that is resistant to the electrochemical porosification process, the annular sealing element having a wafer receiving surface that protrudes from the first planar surface when received in the pedestal.

[0025] According to a fifth aspect of the present disclosure, a container is provided defining an internal cavity; a first electrode is provided positioned within the internal cavity; and a wafer receiver is provided positioned within the internal cavity and spaced from the first electrode, the wafer receiver having: an electrode body having a first planar surface and a second planar surface opposite the first planar surface, a groove recessed from the first planar surface and running within a central region of the electrode body, a pedestal extending annularly around the central region of the electrode body and recessed from the first planar surface, a conduit in fluid communication with the groove and connectable to a vacuum pump; and the wafer receiver is connected to the pedestal. The seat has an annular sealing element that is received therein, the annular sealing element being made of a resilient material that is resistant to acid, the annular sealing element having a wafer receiving surface that protrudes from the first planar surface when received in the seat; a vacuum pump is provided, the vacuum pump is in fluid communication with the conduit and is activatable to create a vacuum in the conduit that draws the semiconductor wafer against the annular sealing element; an etching solution source is provided, the etching solution source is in fluid communication with the internal cavity and is configured to flood at least a portion of the internal cavity with an etching solution; and a current source is provided that is configured to convey an electric current across the etching solution using the first electrode and the electrode body.

[0026] In this disclosure, the term "elastic material" may be any material that can bounce back to its original shape after bending, stretching, or compression. In the context of annular sealing elements, it is understood that the elastic material of the annular sealing element will only be elastically deformed when sandwiched between a semiconductor wafer and an electrode body by a vacuum. As soon as the vacuum is turned off, the elastic material of the annular sealing element will bounce back to its pre-vacuum shape.

[0027] Many further features and combinations of the present improvements will be apparent to those of skill in the art upon reading this disclosure. [Brief description of the drawings]

[0028] Description of the drawings In the figure,

[0029] [Figure 1] FIG. 1 is a cross-sectional perspective view of an example electrochemical porosification apparatus, according to one or more embodiments, shown with an exemplary wafer receiver. [Diagram 2] FIG. 2 is a perspective view of the wafer receiver of FIG. 1 according to one or more embodiments. [Figure 2A] FIG. 2A is a cross-sectional view of the annular sealing element of the wafer receiver of FIG. 2 taken along section 2A-2A according to one or more embodiments. [Diagram 3] FIG. 3 is a cross-sectional perspective view of the electrochemical porosification apparatus of FIG. 1 shown with a semiconductor wafer received therein, in accordance with one or more embodiments. [Figure 4A] FIG. 4A is a cross-sectional view of an example wafer receiver for receiving a semiconductor wafer, shown prior to drawing a vacuum, in accordance with one or more embodiments. [Figure 4B] FIG. 4B is a cross-sectional view of the wafer receiver of FIG. 4 during a vacuum pull according to one or more embodiments. [Diagram 5] FIG. 5 is a flow chart of a method of performing an electrochemical porosification process using a wafer holder according to one or more embodiments. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0030] Detailed Description FIG. 1 shows a cross-sectional view of an example electrochemical porosification device 10, according to an embodiment. As depicted, the device 10 includes a container 12 defining an internal cavity 14, a first electrode 16 located within the internal cavity 14, and a wafer receiver 18 also located within the internal cavity 14 and spaced apart from the first electrode 16. The wafer receiver 18 includes an electrode body 20 having a first planar surface 22, a second planar surface 24 opposite the first planar surface 22, and a groove 26 that is recessed from the first planar surface 22 and runs within a central region of the electrode body 20. The wafer receiver 18 also includes a pedestal 30 that extends annularly around the central region of the electrode body 20 and is recessed from the first planar surface 22. As shown, a conduit 32 extends within the electrode body and is in fluid communication with the groove 26. As shown, the conduit 32 is connectable to a vacuum pump 34. The apparatus 10 has a vacuum pump 34 connectable to the conduit 32 of the electrode body 20. The vacuum pump 34 is drivable to create a vacuum in at least a predetermined portion of the vessel's internal cavity 14 via the conduit 32 and the groove 26. The apparatus 10 includes an etching solution source 36 in fluid communication with the internal cavity 14 and configured to flood at least a portion of the internal cavity 14 with an etching solution (not shown). A current source 38 is also provided to convey a current i across the etching solution between the first electrode 16 and the wafer receiver 18 when the internal cavity 14 is partially or completely filled with the etching solution.

[0031] As best shown in FIG. 2, the wafer receiver 18 has an annular sealing element 40 that is received in the seat 30 of the electrode body 20. The annular sealing element 40 is resistant to the etching solution, and more specifically, in this embodiment, is acid-resistant. Furthermore, the annular sealing element 40 is elastic in the sense that it can be compressed upon application of a force thereto and can assume its original shape upon release of the force. Thus, when the internal cavity is filled with the etching solution, the annular sealing element 40 remains in good condition and performs its function. In this particular example, the grooves include three annular grooves 26' of increasing diameter and two linear grooves 26'' that run perpendicular to each other. The linear grooves 26'' fluidly connect each one of the three annular grooves 26' with each other. The grooves 26' and 26'' may have any other suitable shape, so long as they run along the central region of the electrode body 20. The electrode body 20 may be made of any conductive material. For example, the electrode body may be made of copper, graphite, titanium, brass, silver, mixed metal oxides, platinum, glassy carbon, etc. The electrode body may be made of grafoil, graphite-plastic composite, silicon, diamond-like coated silicon, etc. In embodiments where the device is to be cleanroom compatible, grafoil is a highly conductive material in addition to being corrosion resistant, so it has been found convenient to use it for the electrode body in some embodiments.

[0032] Referring now to the particular embodiment shown in FIG. 2A, the annular sealing element 40 includes an outer surface 42 and a core 44 extending within the outer surface 42. In these embodiments, the outer surface 42 may be made of an acid-resistant material while the core 44 may be made of a resilient material. Additionally or alternatively, the outer surface 42 may be resilient while the core 44 may be acid-resistant. In some embodiments, the outer surface may be provided in the form of a jacket or sheath. In some embodiments, the annular sealing element is made of a unitary material selected to be resilient in addition to being acid-resistant. As shown, the annular sealing element 40 has a wafer receiving surface 46 upon which a semiconductor wafer 48 (shown in dashed lines) may be received during use. FIG. 3 illustrates the apparatus 10 with the wafer receiver 18 (more specifically, the wafer receiving surface 46 of the annular sealing element 40) receiving the semiconductor wafer 48. In some embodiments, the outer surface 42 may be made of Viton. TM In some embodiments, the core 44 is made of a vulcanized, polymerized, or otherwise solidified fluoroelastomer material such as Viton. TM The core is made of an emulsified fluoroelastomer material, such as a foam. Such fluoroelastomers are known to be acid resistant, and more specifically, to hydrofluoric (HF) acid. In some other embodiments, other acid resistant materials may be used. For example, the core may be made of polytetrafluoroethylene (PTFE) (Teflon), another example of an acid resistant material. TM ) foam material.

[0033] Returning to Figures 2 and 2A, the annular sealing element 40 is intended to be sized and shaped to be snugly received in the seat 30 of the electrode body 40. For example, in this example, the seat 30 forms a right angle R between the radially extending wall 50 and the axially extending wall 52 of the electrode body 20. Thus, as shown, the annular sealing element 40 has a rectangular cross-sectional shape that snugly fits therein when received therein. In some embodiments, the annular sealing element 40 has a cross-sectional dimension d that is in the range of about 1 mm to 20 mm, preferably in the range of about 5 mm to 15 mm, and preferably in the range of about 7 mm to 12 mm. In some embodiments, the outer surface 42 of the annular sealing element 40 has a thickness t that is in the range of about 0.1 mm to 5 mm, preferably in the range of about 0.1 mm to 3 mm, and preferably in the range of about 0.1 mm to 1 mm.

[0034] FIG. 4 shows that in the rest state, when the annular sealing element 40 is received in the seat 30 of the electrode body 20, the wafer receiving surface 46 protrudes from the first flat surface 22. Thus, in the rest state, a gap 47 exists between the semiconductor wafer 48 and the first flat surface 22 of the electrode body 20. In some embodiments, the gap 47 may be in the range of about 1 mm to 5 mm, preferably in the range of about 1 mm to 3 mm, and most preferably in the range of about 1 mm to 2 mm. Thus, when creating a vacuum in the conduit 32, as shown in FIG. 4B, air is sucked from the conduit 32 and the groove 26, thereby pulling the semiconductor 48 toward the first flat surface 22 of the electrode body 20. In doing so, the annular sealing element 40 is compressed by the movement of the semiconductor 48, bringing the wafer receiving surface 46 to the same height as the first flat surface 22, which then brings the back surface 50 of the semiconductor wafer 48 and the first flat surface 22 into physical contact with each other. As can be appreciated, in such a vacuum state, the interior cavity may be filled with an etching solution, and when a current i travels between the first electrode and the electrode body across the etching solution and the semiconductor wafer, the current I and the etching solution together create a hole in the exposed surface 52 of the semiconductor wafer 48. The difference in thickness of the annular sealing element between the quiescent state and the vacuum state is preferably intended to correspond to the gap 47 introduced with reference to FIG.

[0035] FIG. 5 illustrates an example method for performing an electrochemical process on a semiconductor wafer.

[0036] In step 502, the backside of a semiconductor wafer is received onto the annular sealing element. The semiconductor wafer may be a silicon wafer, a germanium wafer, a silicon carbide (SiC) wafer, an indium phosphide (InP) wafer, a gallium arsenide (GaAs) wafer, a gallium nitride (GaN) wafer, or any other suitable semiconductor wafer. For example, the wafer may be a silicon, silicon nitride (SiN), silicon-on-insulator (SOI), silicon nitride (Si3N4), silicon carbide (SiC), gallium nitride (GaN), indium gallium arsenide (InGaAs), lithium niobate (LiNbO3), indium antimonide (InSb), mercury cadmium telluride (MCT), indium arsenide (InAs), lead selenide (PbSe), lead sulfide (PbS), sulfide-based materials, selenide-based materials, telluride-based materials, and the like. The annular sealing element may involve any type of semiconductor material, including, but not limited to, any doped semiconductor, including chalcogenide-based materials, n-type doping, p-type doping, germanium doping, silicon doping, boron doping, arsenic doping, carbon doping, helium doping, antimony doping, and / or active laser material doping (such as rare earth ion doping, such as erbium, ytterbium), quantum dots, gases, or any combination thereof. As explained above, the annular sealing element is resistant to the etching solution. Typical etching solutions generally include HF acid or other types of acids, and thus the annular sealing element is acid resistant. The annular sealing element is also elastic, as explained above. The compressibility of the annular sealing element is based on its configuration and / or composition. For example, the annular sealing element may have an outer surface made of a solid material and a core made of an elastic material that fills the outer surface. In some embodiments, the solid material of the outer surface is Viton. TM The elastic material is a fluoroelastomer such as Viton. TM The foam may be a fluoroelastomer foam, such as foam. In some other embodiments, other acid resistant materials may be used.

[0037] In step 504, a vacuum is created in a cavity enclosed by the backside of the semiconductor wafer. The vacuum draws air from the cavity, thereby pulling the semiconductor wafer towards the flat surface of the electrode body. The pulling then compresses the annular sealing element, bringing the wafer receiving surface of the annular sealing element flush with the flat surface, thereby bringing the backside and flat surface of the wafer into physical contact with one another. The compressibility of the annular sealing element is intended to be sufficient to avoid any bending of the semiconductor wafer as the vacuum draws it towards the electrode body.

[0038] In step 506, while maintaining the vacuum of step 504, the exposed surface of the semiconductor wafer is immersed in the etching solution and a current is conducted across the etching solution using another electrode spaced from the electrode body. As in a conventional porosification process, the etching solution and current create holes in the exposed surface of the semiconductor wafer. In this manner, the entire exposed surface of the semiconductor wafer can be porosified at once.

[0039] In some embodiments, upon removing the vacuum created in step 504 and maintained in step 506, the annular sealing element expands and moves the semiconductor wafer away from the electrode body. The semiconductor wafer may then be pulled away from the annular sealing element.

[0040] As can be understood, the examples described and shown above are intended to be exemplary only. For example, while an electrode body is shown having multiple grooves, other electrode bodies may only have a single groove extending through a central region thereof. The scope is indicated by the appended claims.

Claims

1. 1. A wafer receiver for use in an electrochemical porosification process, the wafer receiver comprising: an electrode body having a first planar surface and a second planar surface opposite the first planar surface, a groove recessed from the first planar surface and running within a central region of the electrode body, a seat extending annularly around the central region of the electrode body and recessed from the first planar surface, and a conduit in fluid communication with the groove and connectable to a vacuum pump; and an annular sealing element received in said pedestal, said annular sealing element being made of a resilient material that is resistant to said electrochemical porosification process, said annular sealing element having a wafer receiving surface that protrudes from said first planar surface when received in said pedestal; when a semiconductor wafer is received on the wafer receiving surface of the annular sealing element, the vacuum pump is operable to create a vacuum to draw air from the conduit and the groove, the vacuum pulling the semiconductor wafer toward the first planar surface, the pulling including compressing the annular sealing element to cause the wafer receiving surface to be flush with the first planar surface, and causing a backside of the semiconductor wafer and the first planar surface to be in physical contact with each other. The wafer receiver.

2. The wafer receiver of claim 1 , wherein the resilient material is a fluoroelastomer material.

3. The wafer receiver of claim 1 , wherein the elastic material is a polytetrafluoroethylene (PTFE) material.

4. The wafer receiver of claim 1 , wherein the groove comprises a plurality of grooves in fluid communication with at least the conduit.

5. The wafer receiver of claim 1 , wherein the electrode body is made of a corrosion resistant material.

6. 2. The wafer receiving apparatus of claim 1, wherein in a rest position, said wafer receiving surface has a planar surface spaced from a plane of said first planar surface of said electrode body by a space.

7. 7. The wafer receiver of claim 6, wherein the spacing is in the range of about 0.5 mm to 3 mm, preferably in the range of about 1 mm to 2 mm, and most preferably in the range of about 1 mm to 1.5 mm.

8. The wafer receiver of claim 1 , wherein the annular sealing element has a rectangular cross-sectional shape.

9. 2. The wafer receiver of claim 1, wherein said annular sealing element has an outer surface and a core extending within said outer surface, said outer surface being resistant to said electrochemical porosification process and said core being made of a resilient material.

10. 1. An electrochemical porosification device, the electrochemical porosification device comprising: having a container defining an interior cavity; a first electrode located within the internal cavity; a wafer receiver located within the internal cavity and spaced from the first electrode, the wafer receiver comprising: an electrode body having a first planar surface and a second planar surface opposite the first planar surface, a groove recessed from the first planar surface and running within a central region of the electrode body, a seat extending annularly around the central region of the electrode body and recessed from the first planar surface, and a conduit in fluid communication with the groove and connectable to a vacuum pump; and an annular sealing element received in said pedestal, said annular sealing element being made of a resilient material that is resistant to acid, said annular sealing element having a wafer receiving surface that protrudes from said first planar surface when received in said pedestal; a vacuum pump in fluid communication with the conduit and operable to create a vacuum to draw air from the conduit and the groove, the vacuum pulling a semiconductor wafer received on the wafer receiving surface of the annular sealing element toward the first planar surface, the pulling including compressing the annular sealing element to cause the wafer receiving surface to be flush with the first planar surface and causing a backside of the semiconductor wafer and the first planar surface to be in physical contact with each other; an etching solution source in fluid communication with the internal cavity and configured to flood at least a portion of the internal cavity with an etching solution; and a current source configured to transmit a current across the etching solution using the first electrode and the electrode body, the current and the etching solution creating holes in the exposed surface of the semiconductor wafer; The electrochemical porosification device.

11. The electrochemical porosification device of claim 10 , wherein the elastic material is a fluoroelastomer material.

12. The electrochemical porosification device of claim 10, wherein the elastic material is a polytetrafluoroethylene (PTFE) material.

13. The electrochemical porosification device of claim 10 , wherein the groove comprises a plurality of grooves in fluid communication with at least the conduit.

14. The electrochemical porosification device of claim 10 , wherein the electrode body is made of a corrosion resistant material.

15. 11. The electrochemical porosification device of claim 10, wherein in a rest position, the wafer receiving surface has a plane spaced from the plane of the first planar surface of the electrode body by a distance in the range of about 1 mm to 5 mm, preferably in the range of about 1 mm to 3 mm, and most preferably in the range of about 1 mm to 2 mm.

16. The electrochemical porosification device of claim 10 , wherein the annular sealing element has a rectangular cross-sectional shape.

17. 1. A method for performing an electrochemical porosification process on a semiconductor wafer, the method comprising: receiving a backside of the semiconductor wafer over an annular sealing element, the annular sealing element being resistant to an etching solution and resilient; creating a vacuum in a cavity enclosed by the back surface of the semiconductor wafer, the vacuum drawing air from the cavity pulling the semiconductor wafer toward a flat surface of an electrode body, the pulling including compressing the annular sealing element to bring a wafer receiving surface of the annular sealing element flush with the flat surface and causing the back surface of the wafer and the flat surface to come into physical contact with each other; immersing the exposed surface of the semiconductor wafer in an etching solution while maintaining the vacuum, and conducting an electric current across the etching solution using another electrode spaced from the electrode body, the etching solution and the electric current creating holes in the exposed surface of the semiconductor wafer. The method.

18. 20. The method of claim 17, further comprising: upon removing the vacuum, the annular sealing element expands and moving the semiconductor wafer away from the electrode body.

19. 20. The method of claim 17, wherein the semiconductor wafer is one of a silicon wafer and a germanium wafer.

20. The method of claim 17 , wherein the etching solution comprises a hydrogen fluoride (HF) solution.

Citation Information

Patent Citations

  • Anode formation equipment and related equipment and method

    JP1998275798A

  • Anodization apparatus and method for anodization

    JP2003218086A

  • Anodic chemical conversion method and apparatus therefor

    JP2006131969A

  • Adsorption pat and substrate treatment device

    JP2007297657A