Carbon nanotube synthesis equipment
The carbon nanotube manufacturing apparatus addresses the inefficiencies of fluidized bed reactors by using a plasma device to vaporize catalysts into nanoparticles, enabling high-quality and uniform carbon nanotube synthesis with continuous operation.
Patent Information
- Application Number
- JP2024522105
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-10-19
- Filing Date
- 2022-10-19
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2042-10-19
AI Technical Summary
Existing carbon nanotube synthesis methods face limitations in producing high-quality carbon nanotubes in large quantities efficiently and uniformly, particularly with fluidized bed reactors, which suffer from wide particle size distribution and non-uniform growth times.
A carbon nanotube manufacturing apparatus comprising a plasma device and a CVD reactor, where the plasma device vaporizes catalyst raw materials into nanoparticles using an inductively coupled RF plasma torch, and the CVD reactor synthesizes carbon nanotubes with controlled nanoparticle catalysts, allowing for continuous operation and independent process control.
The apparatus enables the production of high-quality carbon nanotubes in a shorter time with improved uniformity and efficiency, achieving superior physical properties and continuous manufacturing.
Smart Images

Figure 2024538074000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a carbon nanotube production apparatus capable of synthesizing high-quality carbon nanotubes by using a plasma device and a CVD reactor in combination. [Background technology]
[0002] Carbon nanotubes are nanostructures in which graphene, with a thickness of one carbon atom, is rolled into a cylindrical shape. They are classified into single-walled and multi-walled carbon nanotubes depending on the number of shell layers that surround them. Generally, carbon nanotubes have a diameter of several to tens of nm, and a length that is several tens to several thousand times longer than the diameter. Depending on the chiral index (the diameter of the tube and the rolling angle expressed as integers (n, m)), they can be metallic or semiconducting. Single-walled carbon nanotubes are often aligned in a "bundle" shape, with multiple tubes bound together by the Van der Waals force. On the other hand, multi-walled carbon nanotubes are composed of multiple shells, with each layer having a different diameter and chiral index. Multi-walled carbon nanotubes have defects (sp 3 C, vacancies, etc.) and have poor mechanical properties.
[0003] Carbon nanotubes have properties such as higher electrical and thermal conductivity and superior strength compared to conventional materials, making them useful in various fields such as energy, nanotechnology, optics, and materials engineering. For example, carbon nanotubes have high mechanical elasticity of several thousand GPa and high strength of several tens of GPa.
[0004] In terms of applications, carbon nanotubes can be used as a new electrode material, a conductive material for the positive and negative electrodes of lithium-ion batteries. Due to the excellent strength, conductivity, and low density of carbon nanotubes, it is possible to improve the life and capacity of batteries during charging / discharging compared to conventional carbon black conductive materials. In particular, single-walled carbon nanotubes have a clear life improvement effect when applied to silicon anodes, even though the amount used is only 1 / 10 of that of multi-walled carbon nanotubes.
[0005] Various research is also being conducted on the manufacturing methods of carbon nanotubes for industrial use. Conventional methods for synthesizing carbon nanotubes include the arc discharge method, laser deposition method, and chemical vapor deposition method. The arc discharge method is a method for producing carbon nanotubes by inducing an arc discharge between carbon rods in an argon or hydrogen atmosphere at a pressure lower than atmospheric pressure. For example, single-walled carbon nanotubes that are highly pure and highly crystalline as well as have a uniform diameter can be produced using a Ni·Y catalyst. The arc discharge method has the advantage of being able to produce high-quality carbon nanotubes with few defects, but has the disadvantage that amorphous carbon is also produced at the same time, making it unsuitable for mass synthesis.
[0006] Laser deposition is a method of manufacturing carbon nanotubes by irradiating a strong pulsed light such as a laser onto a carbon target mixed with a metal catalyst such as nickel or cobalt in a high-temperature atmosphere of over 900 degrees Celsius. Laser deposition has the advantage of being able to manufacture high-purity carbon nanotubes and to some extent adjust the diameter of the carbon nanotubes by changing the conditions of the irradiated pulsed light, but there is a limit to mass production when considering the competitiveness of production scale.
[0007] Chemical vapor deposition is the most widely used method in the industrial field because it allows for mass synthesis. Types of chemical vapor deposition include fluidized bed chemical vapor deposition (FBCVD) and floating catalyst chemical vapor deposition (FCCVD). Chemical vapor deposition is a method for producing carbon nanotubes in the gas phase by reacting a reactant gas containing a raw material gas, a reducing gas, and a carrier gas with a catalyst at high temperature. That is, a carbon raw material gas is decomposed by a nanoparticle catalyst, and solid carbon nanotubes are formed on the surface of the liquid nanoparticle catalyst. As a specific example, single-walled carbon nanotubes can be synthesized at a temperature range of 500°C to 900°C using a silica-supported Fe:Mo catalyst and methane (CH4) as raw materials. However, there are limitations in terms of productivity and yield when mass-synthesizing single-walled carbon nanotubes using a supported catalyst or a catalyst precursor.
[0008] Therefore, there is a need for research into new manufacturing methods and apparatus that can solve the problems of the conventional carbon nanotube synthesis methods described above and that can mass-synthesize high-quality carbon nanotubes in an economical and consistent manner. [Prior art documents] [Patent documents]
[0009] [Patent Document 1] US8048396B2 [Patent Document 2] KR10-2012-0112918A Summary of the Invention [Problem to be solved by the invention]
[0010] An object of the present invention is to provide a carbon nanotube production apparatus capable of synthesizing high-quality carbon nanotubes. [Means for solving the problem]
[0011] In order to solve the above problems, the present invention provides an apparatus for producing carbon nanotubes. Specifically, (1) the present invention provides a carbon nanotube production apparatus comprising a plasma device 1 and a CVD reactor 2, the plasma device comprising a raw material input section 11 into which a catalyst raw material is input, a plasma torch 12 which vaporizes the input catalyst raw material to form a catalyst vapor, and a quenching zone 13 in which the catalyst vapor is condensed to produce a nanoparticle catalyst, and the CVD reactor comprising a catalyst input section 21 into which the catalyst produced in the quenching zone is input, a gas input section 22 which inputs a raw material gas, and a muffle 23 in which a carbon nanotube synthesis reaction takes place.
[0012] (2) In the present invention, there is provided a carbon nanotube production apparatus as described in (1) above, wherein the quenching zone includes a first quenching zone 131 adjacent to the plasma torch and a second quenching zone 132 adjacent to the first quenching zone.
[0013] (3) In the present invention, there is provided the carbon nanotube synthesis apparatus according to (1) or (2) above, wherein the quenching zone includes a cooling gas inlet 130 for injecting a quenching gas.
[0014] (4) In the present invention, there is provided the carbon nanotube synthesis apparatus according to any one of (1) to (3), wherein the cooling gas inlet portion includes a flow rate control means.
[0015] (5) In the present invention, there is provided a carbon nanotube production apparatus according to any one of (1) to (4), wherein the first quenching zone and the second quenching zone each include a cooling gas input section 130 for inputting a quenching gas, and the second quenching zone further includes a hydrogen gas input section 133 for inputting hydrogen gas.
[0016] (6) In the present invention, there is provided the carbon nanotube production apparatus according to any one of (1) to (5), wherein the CVD reactor further comprises a heating means for heating the inside, and a dispersion plate for providing a uniform airflow inside.
[0017] (7) The present invention provides the carbon nanotube synthesis apparatus according to any one of (1) to (6), wherein the gas input section includes a preheating means 221 for preheating the raw material gas to be input.
[0018] (8) The present invention provides the carbon nanotube production apparatus according to any one of (1) to (7), further comprising a recovery device 3 connected to the CVD reactor for recovering powdered carbon nanotubes synthesized.
[0019] (9) The present invention provides the carbon nanotube production apparatus according to any one of (1) to (8), wherein the recovery device includes at least one of a cyclone and a filter.
[0020] (10) The present invention provides the apparatus for producing carbon nanotubes according to any one of (1) to (9) above, wherein the apparatus is operated continuously.
[0021] (11) The present invention provides the carbon nanotube production apparatus according to any one of (1) to (10) above, wherein the synthesized carbon nanotubes are single-walled carbon nanotubes, multi-walled carbon nanotubes, or a mixture thereof.
[0022] (12) The present invention provides the apparatus for producing carbon nanotubes according to any one of (1) to (11) above, wherein the synthesized carbon nanotubes are in a powder form. Effect of the Invention
[0023] When the carbon nanotube production apparatus of the present invention is used, high quality carbon nanotubes can be produced in a short time compared to the conventional carbon nanotube production method using a supported catalyst and a fluidized bed reactor.
[0024] In addition, the carbon nanotube production apparatus of the present invention can be operated continuously, so that carbon nanotubes can be produced efficiently, and the particle size of the nanoparticle catalyst produced through the plasma device can be controlled within an appropriate range, so that carbon nanotubes with excellent physical properties can be produced. Furthermore, in the carbon nanotube production apparatus of the present invention, the plasma device in which the catalyst is produced and the CVD reactor in which the carbon nanotubes are synthesized are physically separated, so that the control of process variables in the catalyst production process and the control of process variables in the carbon nanotube synthesis process can be performed independently. As a result, when using the carbon nanotube production apparatus of the present invention, it is easy to optimize the overall carbon nanotube synthesis process. [Brief description of the drawings]
[0025] [Figure 1] 1 is a diagram of an apparatus for producing carbon nanotubes according to an embodiment of the present invention; [Diagram 2] 1 is a process flow diagram of a carbon nanotube production apparatus according to an embodiment of the present invention. [Diagram 3] 1 is a SEM image of the carbon nanotubes produced in Example 3 of the present invention, taken at a magnification of 100K. [Figure 4] 1 is a SEM image of the carbon nanotubes produced in Example 3 of the present invention, taken at a magnification of 50K. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0026] The present invention will now be described in more detail. The terms and words used in this specification and the claims should not be interpreted in a limited manner to their ordinary or dictionary meanings, but should be interpreted in a manner that is consistent with the technical idea of the present invention, based on the principle that the inventors can appropriately define the concepts of terms in order to best describe their invention.
[0027] Carbon nanotube manufacturing equipment A method that is often used in the industrial field to produce a large amount of carbon nanotubes is to use a fluidized bed reactor. Specifically, in this method, carbon nanotubes are produced by filling a fluidized bed reactor with a support containing a metal catalyst, then introducing a raw material gas, heating the reactor, and growing carbon nanotubes on the surface of the catalyst particles. Such a fluidized bed chemical vapor deposition (FBCVD) method has the advantages of being able to produce a large amount of carbon nanotubes and to synthesize carbon nanotubes stably, but it also has the following disadvantages.
[0028] 1) When synthesizing carbon nanotubes using a fluidized bed reactor, there is a limit to how much improvement can be made in the quality of carbon nanotubes. Catalysts used in fluidized bed reactors are manufactured by calcining metal catalyst precursors, but catalysts manufactured in this manner have a relatively wide particle size distribution, which means that the uniformity of the diameter of the carbon nanotubes manufactured using this method is somewhat poor, making it difficult to obtain uniform carbon nanotube products. In addition, due to the characteristics of fluidized bed reactors, the inside of the reactor is filled with carbon nanotubes that have already been synthesized, so the growth time for each individual carbon nanotube is not constant, which can also worsen the uniformity of the carbon nanotubes ultimately manufactured. Furthermore, in the case of multi-walled carbon nanotubes synthesized at temperatures below 800°C, the crystallinity (I G / I D It also has the disadvantages of having a low elastic modulus (ratio) of 1 and weak mechanical properties.
[0029] 2) When synthesizing carbon nanotubes using a fluidized bed reactor, there is a limit to how much the efficiency of the manufacturing process can be improved. When using a fluidized bed reactor, it is necessary to fill the inner space of the reactor with a bed before starting the reactor, and it is also necessary to obtain the grown carbon nanotubes after the reaction is completed, making it difficult to realize a continuous manufacturing process. In addition, since it is necessary to heat the reactor after the reaction starts, the time spent on the actual reaction is short compared to the overall process operation time, and there is a limit to how much the efficiency of the manufacturing process can be improved in terms of time.
[0030] Therefore, the present invention aims to propose a manufacturing apparatus that can improve the efficiency of the carbon nanotube manufacturing process in terms of time, while ensuring the uniformity and quality of the synthesized carbon nanotubes.
[0031] Specifically, the present invention provides a carbon nanotube production apparatus comprising a plasma device 1 and a CVD reactor 2, the plasma device comprising a raw material input section 11 into which a catalyst raw material is input, a plasma torch 12 which vaporizes the input catalyst raw material to form a catalyst vapor, and a quenching zone 13 in which the catalyst vapor is condensed to produce a nanoparticle catalyst, and the CVD reactor comprising a catalyst input section 21 into which the catalyst produced in the quenching zone is input, a gas input section 22 which inputs a raw material gas, and a muffle 23 in which a carbon nanotube synthesis reaction takes place.
[0032] As shown in FIGS. 1 and 2, the carbon nanotube production apparatus of the present invention broadly includes a plasma device and a CVD reactor, and each device of the present invention will be described separately below.
[0033] Plasma Equipment From the viewpoint of catalysts for synthesizing carbon nanotubes, when nanoparticle catalysts in an aerosol state are produced using a plasma device, the average particle size of the catalyst particles is low and the particle size distribution is narrow, so that uniform carbon nanotubes can be produced at high speed. Therefore, the carbon nanotube production device of the present invention produces nanoparticle catalysts in an aerosol state using a plasma device, more specifically, an inductively coupled RF (radio frequency) plasma device, and feeds the produced catalyst together with a raw material gas into a high-temperature CVD reactor to synthesize carbon nanotubes.
[0034] Specifically, the inductively coupled plasma device includes a raw material input section 11 into which a catalyst raw material is input, a plasma torch 12 that vaporizes the input catalyst raw material to form a catalyst vapor, and a quenching zone 13 in which the catalyst vapor is condensed to produce a nanoparticle catalyst.
[0035] The feeder is for feeding the catalyst raw material into the plasma device. The form and type of the feeder may vary depending on the state and form of the metal raw material to be fed, and a skilled technician can select and apply an appropriate feeder depending on the state and form of the catalyst raw material. The catalyst raw material may be liquid or solid, more specifically, a solution in which the catalyst raw material precursor is dissolved in a liquid, a powdered catalyst raw material precursor, or a metal itself. In particular, when the catalyst raw material is powdered, the powder should have good fluidity to facilitate feeding into the plasma device. Therefore, when the catalyst raw material is powdered, the feeder may have a form that allows the powder to have good fluidity, for example, a form having a gradient structure.
[0036] Meanwhile, the plasma device may include a plasma torch. The plasma torch is for forming plasma and vaporizing the input catalyst raw material, and any plasma torch known to ordinary technicians may be used as the plasma torch of the present invention without any particular limitation. The plasma torch may use gas such as argon, hydrogen, nitrogen, etc., alone or in combination, as the working gas.
[0037] More specifically, the plasma torch may be an inductively coupled RF plasma torch. The high energy density RF thermal plasma generated by the inductively coupled RF plasma torch has a temperature sufficient to vaporize the catalyst raw material at an ultra-high temperature, and the vaporization rate at this time is at the level of 99%. The catalyst raw material is vaporized and the catalyst vapor formed is transported to the quenching zone by convection and diffusion, forming a vapor concentration profile. The catalyst vapor is then condensed to generate a nanoparticle catalyst in an aerosol state, and the uniformity in the catalyst vapor can be improved by convection and diffusion during the transport process, thereby making it possible to effectively generate the nanoparticle catalyst.
[0038] More specifically, when the catalyst vapor is transported through convection and diffusion, the nanoparticle catalyst may have a narrow particle size distribution in the form of a log-normal distribution. In contrast, when the catalyst vapor is condensed immediately after formation without convection and diffusion, the nanoparticles may be mixed with a portion of the catalyst raw material powder that was not completely vaporized during the condensation process, making it difficult to condense the catalyst vapor more effectively, and the particle size distribution of the nanoparticle catalyst obtained thereafter may be bimodal and broad.
[0039] Meanwhile, the inner space of the plasma device including the quenching zone may be a reactor made of a high-temperature refractory material such as graphite, or other suitable reactor structure and material having high-temperature refractory properties may be selected and applied, in that the temperature of the inner center line of the reactor should be at least 3000K or more.
[0040] The transported catalyst vapor can be condensed by quenching to form a nanoparticle catalyst in an aerosol state. For example, iron vapor is known to condense at about 1820K and undergo nucleation of nanoparticles. In the quenching process, the faster the cooling rate is, the shorter the solid particle growth time is, and the narrower the particle size distribution is, and the smaller the average particle size is, the more nanoparticle catalyst can be produced.
[0041] The quenching may be performed by injecting a quenching gas into the quenching zone, and the quenching zone may include a quenching gas inlet for this purpose. As the quenching gas, a suitable gas may be selected from among cooling gases known to be used for cooling and applied to the present invention, and for example, argon gas or nitrogen gas may be applied as the cooling gas.
[0042] Meanwhile, specifically, the quenching gas inlet is not particularly limited as long as it is for injecting gas into the quenching zone, and may have the form of a line directly connected to the quenching zone, and more preferably, may have the form of a hole provided on the wall surface of the quenching zone so that uniform cooling can be performed throughout the quenching zone. The size and shape of the hole are not particularly limited, and a person skilled in the art can select an appropriate size and shape of the hole in consideration of factors such as the type of gas used for cooling, the temperature of the cooling gas, and the temperature of the plasma.
[0043] The cooling gas inlet may include a flow rate control unit, and the average particle size of the nanoparticle catalyst can be controlled by controlling the flow rate of the gas used for quenching.
[0044] Meanwhile, as shown in FIG. 2, the quenching zone may include a first quenching zone 131 adjacent to the plasma torch and a second quenching zone 132 adjacent to the first quenching zone, and the first quenching zone and the second quenching zone may each be provided with a cooling gas input section 130 for inputting a quenching gas, and the second quenching zone may further be provided with a hydrogen gas input section 133 for inputting hydrogen gas.
[0045] As described above, when the quenching zone is divided into two zones and different types of gas are introduced into each zone, there is a technical advantage in terms of controlling the size of the nanoparticle catalyst.
[0046] CVD Reactor Carbon nanotubes can be synthesized in a CVD reactor 2 using a nanoparticle catalyst in an aerosol state produced by a previous plasma device. Specifically, the CVD reactor may include a catalyst input section 21 into which the catalyst produced in the quenching zone is input, a gas input section 22 into which a raw material gas is input, and a muffle 23 in which a synthesis reaction of carbon nanotubes takes place. In addition, the CVD reactor may further include a heating means for heating the inside of the reactor, and may include a dispersion plate for enabling a uniform air flow. The floating reactor may be a reactor used in a conventional chemical vapor deposition (CVD), catalytic chemical vapor deposition (CCVD), or floating catalyst chemical vapor deposition (FCCVD).
[0047] The catalyst input unit is for inputting the nanoparticle catalyst in an aerosol state formed by the above-mentioned plasma device into the inside of the CVD reactor, and may be connected to an outlet of a quenching zone of the plasma device where the nanoparticle catalyst in an aerosol state is finally formed. The catalyst input unit must be in a form that allows the nanoparticle catalyst in an aerosol state to be smoothly input, and is particularly preferably located at the bottom of the CVD reactor so that the catalyst can be uniformly distributed and suspended inside the CVD reactor to synthesize carbon nanotubes.
[0048] The gas input unit is for inputting a raw material gas, which is a raw material for carbon nanotubes, into the CVD reactor. The gas input unit is not particularly limited as long as it is a means for inputting a gas into the reactor, and is preferably provided at the inlet side of the CVD reactor so that the raw material gas and the nanoparticle catalyst input from the plasma device can be smoothly mixed. In addition, the raw material gas input through the gas input unit may be heated to a temperature of 200° C. or more before being input into the CVD reactor, and for this purpose, the gas input unit may further include a preheating means 221.
[0049] Meanwhile, the raw material gas is a carbon source gas that can be decomposed by the nanoparticle catalyst to generate solid carbon nanotubes on the surface of the liquid nanoparticle catalyst, and various carbon-containing compounds such as aliphatic alkanes, aliphatic alkenes, aliphatic alkynes, and aromatic compounds can be used as specific examples. More specifically, the raw material gas may include one or more selected from the group consisting of carbon monoxide, natural gas, C1-10 aliphatic hydrocarbons, C6-20 aromatic hydrocarbons, C1-6 alcohols, and acetone. More specifically, compounds such as methane, ethane, ethylene, acetylene, methylacetylene, vinylacetylene, propane, butane, pentane, hexane, propylene, carbon monoxide, natural gas, butadiene, benzene, toluene, cyclopentadiene, cyclohexane, ethanol, methanol, propanol, and acetone can be used. It is particularly preferable to use methane in terms of economy and efficiency.
[0050] Meanwhile, the carbon nanotube production apparatus of the present invention may further include a recovery device 3 connected to the CVD reactor for recovering the carbon nanotubes synthesized by the CVD reactor, and the recovery device may include at least one of a cyclone and a filter. The carbon nanotubes synthesized by the CVD reactor may be obtained in a state where they are grown with a nanoparticle catalyst, and therefore a recovery device is required to selectively separate only the solid powder, and a cyclone or a filter that is often used to separate solids from a gas-solid mixture may be used as the recovery device of the present invention.
[0051] The carbon nanotube production apparatus of the present invention may be continuously operated. In the carbon nanotube production apparatus of the present invention, the nanoparticle catalyst may be continuously produced by feeding the catalyst raw material, and the raw material gas may also be continuously fed from the gas feed section. This allows the entire apparatus to be operated continuously. In the case of a carbon nanotube production system using a conventional supported catalyst and a fluidized bed reactor, it is generally operated in a batch manner because it is necessary to fill the inside of the reactor with the support before the start of the reaction and to obtain the finally produced carbon nanotubes from the reactor. However, when using the production apparatus of the present invention, continuous production is possible, so that carbon nanotubes can be produced more efficiently than before.
[0052] The carbon nanotubes produced by the production apparatus of the present invention may be single-walled carbon nanotubes, multi-walled carbon nanotubes, or a mixture thereof. The carbon nanotubes produced by the production apparatus of the present invention may be in powder form.
[0053] The carbon nanotubes produced by the production apparatus of the present invention may be bundled. The term "bundled" carbon nanotubes means that a plurality of carbon nanotubes are aligned or arranged in a certain direction to form a bundle-like or rope-like secondary structure, and the bundled carbon nanotubes are particularly suitable for use as a conductive material, etc.
[0054] Hereinafter, the present invention will be described in more detail with reference to examples and experimental examples in order to specifically explain the present invention, but the present invention is not limited to these examples and experimental examples. The examples of the present invention may be modified in various different forms, and the scope of the present invention should not be interpreted as being limited to the examples described below. The examples of the present invention are provided to more specifically explain the present invention to those having average knowledge in the art.
[0055] material As the catalyst raw material, Fe powder and FeS powder having a particle size of 10 to 50 μm were mixed and used, and the catalyst raw material was dried in a vacuum oven to remove moisture before being fed into a feeder.
[0056] Example 1 Carbon nanotubes were synthesized using the carbon nanotube production apparatus shown in FIG. 2. To ignite plasma in a vacuum state, Ar (32 lpm) and H2 (1.4 lpm) were injected into the plasma torch as sheath gas, and Ar (12 lpm) was injected as central gas. After completion of ignition, the pressure in the plasma apparatus was normal pressure (14.7 psi), and the catalyst raw material (FeS content 16 wt%) of the material was supplied to the feeder (carrier gas: Ar, flow rate: 5 lpm) of the RF thermal plasma apparatus, and the catalyst raw material was vaporized by the plasma torch. The formed catalyst vapor was transported to the quenching zone by convection and diffusion, and quenching gas Ar was injected into the first quenching zone and the second quenching zone at 75 lpm and 175 lpm, respectively, to quench and condense the catalyst vapor. Meanwhile, H2 gas was injected into the second quenching zone together with Ar at a flow rate of 30 lpm. The catalyst vapor passing through both the first and second quenching zones was condensed to form nanoparticle catalyst in an aerosol state, which was then introduced into a CVD reactor preheated to 1350°C.
[0057] In addition to the nanoparticle catalyst, methane gas as a raw material gas was injected into the CVD reactor at a flow rate of 4 lpm and passed through a preheater heated to 500° C. before injection.
[0058] The nanoparticle catalyst and the raw material gas were fed into the CVD reactor, and the synthesis of carbon nanotubes was started, and the synthesis process was carried out for 20 minutes. After the process was completed, the gas injection was stopped, the CVD reactor was cooled, and carbon nanotubes were obtained.
[0059] Example 2 Carbon nanotubes were obtained in the same manner as in Example 1, except that the catalyst raw material was a mixture containing 20% by weight of FeS, the temperature of the CVD reactor was heated to 1400°C, and methane gas was injected into the CVD reactor at a flow rate of 3 lpm and hydrogen gas was injected into the reactor at a flow rate of 9.5 lpm.
[0060] Example 3 Carbon nanotubes were obtained in the same manner as in Example 2, except that methane gas was injected into the CVD reactor at a flow rate of 3 lpm and hydrogen gas was injected into the reactor at a flow rate of 50 lpm.
[0061] Comparative Example 1 Carbon nanotubes were obtained in the same manner as in Example 2, except that 4 lpm of methane gas and 9.5 lpm of hydrogen gas were premixed with an aerosol-state nanoparticle catalyst using a small chamber before being injected into the CVD reactor, and the CVD reactor was heated to a temperature of 1300°C. The production conditions in the above examples and comparative examples are summarized in Table 1 below.
[0062] [Table 1]
[0063] Experimental Example 1. Confirmation of the crystallinity of the produced carbon nanotubes The I and I D values of the carbon nanotubes produced in the examples and comparative examples were measured using Raman spectroscopy, and the average crystallinity and maximum crystallinity were calculated and are shown in Table 2 below.
[0064] [Table 2]
[0065] As can be seen from Table 2, the carbon nanotubes produced in the examples of the present invention exhibited high crystallinity with a maximum crystallinity of 40 or more, whereas the carbon nanotubes produced in Comparative Example 1 exhibited a crystallinity of less than 1. This means that the crystallinity of the carbon nanotubes produced in Comparative Example 1 is significantly inferior to that of the examples, and that the method for producing carbon nanotubes of the present invention can be used to produce high quality carbon nanotubes.
[0066] Experimental Example 2. Confirmation of SEM images of carbon nanotubes produced in the examples The carbon nanotubes prepared in Example 3 were observed by SEM imaging at magnifications of 100K and 50K, and the results are shown in FIGS.
[0067] As can be seen from FIGS. 3 and 4, when the carbon nanotube manufacturing method of the present invention is used, it is confirmed that a plurality of thin and flexible carbon nanotubes are manufactured in a bundled form. [Explanation of symbols]
[0068] 1: Plasma device 11: Raw material input section 12: Plasma torch 13:Quenching zone 130: Cooling gas inlet 131: First quenching zone 132: Second quenching zone 133: Hydrogen gas input section 2: CVD reactor 21:Catalyst injection part 22: Gas input section 221: Preheating means 23: Muffle 3: Recovery device
Claims
1. A plasma device (1), A CVD reactor (2); Including, The plasma device includes a raw material input section (11) into which a catalyst raw material is input, a plasma torch (12) for vaporizing the input catalyst raw material to form a catalyst vapor, and a quenching zone (13) in which the catalyst vapor is condensed to produce a nanoparticle catalyst, The CVD reactor is a carbon nanotube production apparatus comprising a catalyst input section (21) into which the catalyst produced in the quenching zone is input, a gas input section (22) into which a raw material gas is input, and a muffle (23) in which a carbon nanotube synthesis reaction takes place.
2. The quenching zone comprises: a first quenching zone (131) adjacent to the plasma torch; 2. The carbon nanotube production apparatus of claim 1, further comprising a second quenching zone (132) adjacent to the first quenching zone.
3. The carbon nanotube manufacturing apparatus according to claim 1 , wherein the quenching zone comprises a cooling gas input section (130) for inputting a quenching gas.
4. 4. The carbon nanotube manufacturing apparatus according to claim 3, wherein the cooling gas supply section includes a flow rate control means.
5. The first quenching zone and the second quenching zone each include a cooling gas input section (130) for inputting a quenching gas; 3. The carbon nanotube synthesis apparatus according to claim 2, wherein the second quenching zone further comprises a hydrogen gas input section (133) for inputting hydrogen gas.
6. 2. The carbon nanotube synthesis apparatus according to claim 1, wherein the CVD reactor further comprises a heating means for heating the inside thereof, and a dispersion plate for uniform airflow therein.
7. 2. The carbon nanotube synthesis apparatus according to claim 1, wherein the gas input section includes a preheating means for preheating the raw material gas to be input.
8. 2. The carbon nanotube manufacturing apparatus according to claim 1, further comprising a recovery device (3) connected to the CVD reactor for recovering the powdered carbon nanotubes synthesized.
9. The carbon nanotube producing apparatus according to claim 8 , wherein the recovery device includes at least one of a cyclone and a filter.
10. 2. The carbon nanotube synthesis apparatus according to claim 1, wherein the apparatus is operated continuously.
11. 2. The carbon nanotube production apparatus according to claim 1, wherein the synthesized carbon nanotubes are single-walled carbon nanotubes, multi-walled carbon nanotubes, or a mixture thereof.
12. 12. The carbon nanotube producing apparatus according to claim 1, wherein the synthesized carbon nanotubes are in a powder form.
Citation Information
Patent Citations
Carbon nanotube preparation device and method
CN110217777A
Process and apparatus for the production of carbon nanotubes
WO2015082936A1
Continuous carbon nano-tube manufacturing apparatus and method
KR1020120112918A
Method for manufacturing single-walled carbon nanotubes
US8048396B2