Unsupported bimetallic hydrotreating catalysts, their preparation and applications.

Unsupported bimetallic hydroprocessing catalysts in the form of a metal-organic complex address diffusion limitations in heterogeneous reactions, enhancing catalytic activity and efficiency with a simplified, environmentally friendly preparation process.

JP2024538238APending Publication Date: 2024-10-18CHINA PETROLEUM & CHEMICAL CORP +1
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2024524606
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-10-25
Filing Date
2022-10-21
Publication Date
2024-10-18

AI Technical Summary

Technical Problem

Existing bimetallic hydroprocessing catalysts are limited by diffusion stages in heterogeneous reactions, leading to reduced catalytic activity and efficiency, and their preparation methods are complex, generate waste, and have high energy consumption.

Method used

Development of unsupported bimetallic hydroprocessing catalysts in the form of a metal-organic complex with a formula (M1M2Oa[R(COO)b) that allows for homogeneous catalytic reactions, reducing diffusion limitations and simplifying the preparation process.

Benefits of technology

The unsupported catalysts exhibit high dispersibility, stability, and hydrogenation activity with improved metal content and storage stability, while minimizing material and energy consumption.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024538238000001_ABST
    Figure 2024538238000001_ABST
Patent Text Reader

Abstract

Disclosed is an unsupported bimetallic hydrotreating catalyst, its preparation and its applications. The catalyst comprises a complex formed by bonding a metal central atom or ion with an organic ligand through a coordinate bond. The catalyst has the general formula (I)M 1 M 2 O a [R(COO) x ] b The composition is roughly represented by the formula: 1 and M. 2 represents a metal, and R(COO) x represents the organic ligand, R represents a hydrocarbyl group of the organic ligand, COO represents a coordinating group of the organic ligand, x represents the number of coordinating groups in the organic ligand, a represents the molar ratio of oxygen atoms bonded to the metal via a non-coordinating bond to the total amount of the metal, and b represents the molar ratio of the organic ligand to the total amount of the metal. When used in the hydrogenation of hydrocarbons, the catalyst and the composition thereof exhibit high dispersibility in an oil phase, high hydrogenation activity, and high selectivity to the target product.
Need to check novelty before this filing date? Find Prior Art

Description

Detailed Description of the Invention

[0001] [Technical field] This application relates to the field of hydrotreating catalysts, in particular to unsupported bimetallic hydrotreating catalysts, their preparation and applications.

[0002] [Background technology] In 2020, China's dependence on foreign crude oil exceeded 70%, with most of the imported crude oil being low-quality heavy crude oil from the Middle East and South America, with residual oil accounting for more than 50%. Therefore, the effective use of oil resources, especially deep processing of residual oil, can improve the utilization rate of oil resources and alleviate China's energy security crisis.

[0003] In crude oil processing, supported catalysts are the hydrotreating catalysts that have been studied for the longest time and are widely used in the most industrial applications. Supported catalysts are composed of three components: catalytic active components, cocatalyst active components and supports, where the catalytic active components and cocatalyst active components are mainly metals, and the supports are silicon-based or aluminum-based materials or porous materials such as alumina, silica, kaolin, and molecular sieves. In order to improve the properties of the metal active sites on the catalyst and improve the activity, selectivity and stability of the catalyst, hydrotreating catalysts have been developed toward bimetallic and polymetallic catalysts. Mo-Ni and W-Ni hydrotreating catalysts are used for hydrotreating distillate oil, and W-Mo-Ni catalysts are mainly used for hydrotreating pretreatment of vacuum distillate oil. Non-precious metal hydrotreating catalysts such as Mo, W, and Ni mostly exist in the form of sulfides and are supported in the pore channels of the support. The influence of the co-metal elements is discussed using the embedded model (Co or Ni is MoS 2 or W.S. 2 embedded structure), synergistic model (Co is embedded in Co 9 S 8 (structure existing as MoO 3 or WO 3 There are theories such as "a structure in which auxiliary metal elements are distributed on the support as a monolayer," which can explain the effect of auxiliary metal elements on the sulfide structure of the main metal or the distribution of the main metal elements on the support.

[0004] Since all existing bimetallic catalysts are supported catalysts, the hydrogenation reaction of hydrocarbons using such catalysts is a heterogeneous catalytic reaction that goes through seven steps: the molecules of the raw material diffuse onto the outer surface of the catalyst → the molecules of the raw material diffuse into the pore channels of the catalyst → the molecules of the raw material are adsorbed onto the active centers of the catalyst → the molecules of the raw material undergo a surface catalytic reaction with the active centers of the catalyst → the reaction products are desorbed from the surface of the active centers of the catalyst → the reaction products diffuse outward from the pore channels of the catalyst → the reaction products diffuse from the outer surface of the catalyst into the liquid phase. Among these steps, the diffusion step has a significant effect on the occurrence probability and efficiency of the hydrogenation reaction using supported bimetallic hydrotreating catalysts, limiting the catalytic activity of the catalyst.

[0005] In order to improve the dispersion and oil solubility of the catalyst, many researchers at home and abroad have carried out related research. China Patent No. ZL201510275523.1 discloses an oil-soluble Mo-Ni bimetallic catalyst and its preparation and application. In the disclosed method, nickel nitrate and ammonium molybdate are dissolved in 15-25 mass times of distilled water, a small amount of glycol is added, and then ammonia water is added to adjust the pH to alkaline; the solution is heated to 130-160°C under stirring and reacted for 3-5 hours, and the resulting product is filtered to obtain a solid intermediate product. The solid intermediate product is degassed at 100°C under normal pressure, mixed with oleic acid, and reacted at 230-260°C for 2-4 hours to obtain an oil-soluble Mo-Ni bimetallic catalyst. The catalyst can flexibly adjust the mass ratio of bimetals, and has high hydrogenation activity and good coke inhibition effect. However, in the above-mentioned patent document, glycol and aqueous ammonia are added in the first step, the reaction product obtained in the first step is filtered to obtain an intermediate product, and the intermediate product is dried and then subjected to the reaction in the second step, so that the process steps are complicated, waste is generated due to filtration, and the metal content of the target product is low.

[0006] Chinese Patent No. ZL201610862714.2 discloses a molybdenum-nickel catalyst for hydrocracking and a method for its preparation. In this method, a hexavalent molybdenum source compound is dissolved and dispersed in a solvent, an inorganic acid catalyst and a C1-C5 organic acid are added to react at a temperature of 40°C to 150°C for 5 hours to 10 hours, and a C6-C16 organic acid or a C6-C16 ester is added to the reaction product obtained in step (1) and reacted at a temperature of 160°C to 320°C for 2 hours to 22 hours. The product obtained in step (2) is cooled to 20°C to 80°C, a nickel-containing inorganic material is added, and the reaction is carried out at a temperature of 50°C to 95°C for 3 to 10 hours, and then heated to 100°C to 180°C for 1 hour to 8 hours; the product obtained in step (3) is separated to remove the solvent phase, and the oil phase is washed with water, and then the light components are removed by vacuum distillation to obtain a molybdenum-nickel hydrocracking catalyst. When this catalyst is used in the hydrocracking reaction of heavy oil, it shows high conversion and high yield of light oil. However, the preparation method of the catalyst has many steps, complicated operation, expensive starting materials, and poor environmental performance because a large amount of wastewater is generated due to washing the reaction product with water. In addition, since the timing and steps of adding the two types of metals during synthesis are different, it is not possible to distinguish whether the final synthesized product is a mixture of two types of organometallic compounds or a single bimetallic organometallic compound.

[0007] U.S. Patent No. 7,842,635 B2 discloses a method for preparing an oil-soluble bimetallic catalyst. In this method, a molybdenum source compound is reacted with N 2 and H 2 In the mixed gas stream, molybdenum is reacted with an organic carboxylic acid to obtain a molybdenum-organic compound, another metal compound is reacted with the organic carboxylic acid to obtain the corresponding organometallic compound, and the two organometallic compounds are mixed in a predetermined ratio to obtain a bimetallic-organic mixture. However, the above methods involve three-phase reactions of gas, liquid, and solid phases, resulting in low conversion rates, high energy consumption, and large amounts of wastewater, waste gas, and solid waste.

[0008] DISCLOSURE OF THEINVENTION The purpose of the present application is to provide an unsupported bimetallic hydrotreating catalyst, its preparation and its application, which comprises an organometallic complex with high oil phase dispersibility, and when used as a catalyst for the hydrogenation reaction of hydrocarbon compounds, the reaction belongs to homogeneous catalytic reaction, thereby eliminating the diffusion step of heterogeneous catalytic reaction and being beneficial to improving the hydrogenation activity.

[0009] In accordance with the above objectives, in one aspect, the present application provides an unsupported bimetallic hydroprocessing catalyst comprising a complex formed by the bonding of a metal central atom or ion with an organic ligand via a coordinate bond, the catalyst having the general composition represented by formula (I): M 1 M 2 O a [R(COO) x ] b (I), Here, M 1 and M. 2 represents a metal, and R(COO) x represents an organic ligand, R represents a hydrocarbyl group of the organic ligand, COO represents a coordinating group of the organic ligand, x represents the number of coordinating groups in the organic ligand, a represents the molar ratio of oxygen atoms bonded to the metal via non-coordinating bonds to the total amount of the metal, and b represents the molar ratio of the organic ligand to the total amount of the metal: M 1 and M. 2 are different from each other and each is independently one metal selected from the group consisting of Group VB metals, Group VIB metals, Group VIII metals, and Group IB metals having hydrogenation activity; R is a C3-C19 hydrocarbyl group; x is 1, 2 or 3, preferably 1 or 2; a is a positive number from 0 to 5, preferably from 1 to 3; and b is a positive number of 1 to 6, preferably 2 to 5.

[0010] Here, the catalyst has a molecular weight of 700 to 1000 cm -1 , 1350~1450cm -1 and 1500~1610cm -14 shows an infrared spectrum with a characteristic peak at position .

[0011] In another aspect, the present application provides a method for preparing an unsupported bimetallic hydroprocessing catalyst, comprising the steps of: 1) mixing a first metal source or a dispersion thereof with an organic ligand compound; 2) reacting the mixture obtained in step 1) at temperature T1 for a time t1; 3) reacting the material obtained in step 2) at temperature T2 for time t2; 4) optionally adding a second metal source or a dispersion thereof to the material obtained in step 3) and reacting the resultant at a temperature T2 for a time t3; and 5) Recovering the resulting liquid product.

[0012] Here, the first and second metal sources are each independently selected from the group consisting of elemental metals, metal oxides, metal hydroxides, metal oxyacids, metal inorganic salts, or combinations thereof, and the metals of the first and second metal sources are the same as or different from each other and each independently represent one or two metals selected from the group consisting of Group VB metals, Group VIB metals, Group VIII metals, and Group IB metals having hydrogenation activity.

[0013] The organic ligand compound is selected from the group consisting of a C4-C20 organic carboxylic acid or anhydride.

[0014] The molar ratio of the organic ligand compound to the total amount of the metals in the first and second metal sources is 1 to 10:1.

[0015] The temperature T1 is 50° C. to 150° C., the time t1 is 5 minutes to 180 minutes, The temperature T2 is 100° C. to 350° C., and the time t2 is 1 to 8 hours. The time t3 is from 1 hour to 8 hours.

[0016] However, when only the first metal source is used or the metal of the second metal source is the same as the metal of the first metal source, the metal of the first metal source is two metals selected from the group consisting of Group VB metals, Group VIB metals, Group VIII metals, and Group IB metals having hydrogenation activity.

[0017] In yet another aspect, the present application provides a bimetallic hydrotreating catalyst composition comprising an unsupported bimetallic hydrotreating catalyst and at least one organic ligand compound and / or organic solvent, wherein the organic ligand compound is selected from a C4-C20 organic carboxylic acid and the organic solvent is selected from the group consisting of an aliphatic hydrocarbon, an aromatic hydrocarbon, a cycloaliphatic hydrocarbon, a halogenated hydrocarbon, an alcohol solvent, an ether solvent, an ester solvent, a ketone solvent, or a combination thereof.

[0018] In yet another aspect, there is provided a process for hydrotreating a hydrocarbon feedstock, the process comprising contacting the hydrocarbon feedstock with an unsupported bimetallic hydrotreating catalyst or a bimetallic hydrotreating catalyst composition according to the present application to hydrotreat the hydrocarbon feedstock.

[0019] In yet another aspect, the present application provides an unsupported catalyst composition comprising, by weight, 10% to 45% of a hydroprocessing catalyst component, 45% to 80% of a dispersing medium, and 1.0% to 10% of an activator.

[0020] The hydrotreating catalyst component comprises an unsupported bimetallic hydrotreating catalyst according to the present application and, optionally, an organic ligand compound selected from C4-C20 organic carboxylic acids.

[0021] The dispersion medium is selected from the group consisting of an organic solvent, a petroleum fraction, or a combination thereof, the organic solvent is selected from the group consisting of an aliphatic hydrocarbon, an aromatic hydrocarbon, an alicyclic hydrocarbon, a halogenated hydrocarbon, an alcohol solvent, an ether solvent, an ester solvent, a ketone solvent, or a combination thereof, and the petroleum fraction is selected from a distillate oil having a distillation range of 150°C to 524°C or a residual oil component having a boiling point >524°C.

[0022] The activator is selected from the group consisting of elemental sulfur, a sulfur-containing compound, or a combination thereof.

[0023] In yet another aspect, there is provided the use of the unsupported catalyst composition of the present application in the hydroupgrading of heavy oil.

[0024] In yet another aspect, the present application provides a process for hydroupgrading of heavy oil, comprising subjecting a heavy oil feedstock to a hydroupgrading reaction under heating conditions in the presence of hydrogen and the unsupported catalyst composition of the present application, which may optionally be presulfided.

[0025] When used in the hydrogenation reaction of hydrocarbons, the unsupported bimetallic hydrotreating catalyst and its composition according to the present application exhibit high dispersibility in the oil phase, stability, hydrogenation activity and selectivity to the target product. Meanwhile, the preparation method of the catalyst according to the present application has the advantages of a green and efficient preparation procedure with a small number of raw materials, simple preparation steps, low material and energy consumption, and the obtained catalyst, especially the metal complex contained therein, has a high metal content and good storage stability.

[0026] Other features and advantages of the present application are detailed in the detailed description below.

[0027] BRIEF DESCRIPTION OF THE DRAWINGS The drawings forming part of this specification are provided to aid in the understanding of the present application and should not be considered limiting. The present application can be read with reference to the drawings in combination with the following detailed description herein. In the drawings: [FIG. 1] FIG. 1 is an IR spectrum of the product obtained in Example 1; [Figure 2] Figure 2 is an IR spectrum of the product obtained in Example 2; [Figure 3] Figure 3 is an IR spectrum of the product obtained in Example 3; [Figure 4] Figure 4 is an IR spectrum of the product obtained in Example 4; [Figure 5] Figure 5 is an IR spectrum of the product obtained in Example 5; [Figure 6] Figure 6 is an IR spectrum of the product obtained in Example 6; FIG. 7 is an image showing the result of dissolving the catalyst obtained in Example 1 in toluene; and FIG. 8 is an image showing the result of dissolving the catalyst obtained in Example 3 in toluene. DETAILED DESCRIPTION OF EMBODIMENTS OF THE PRESENTINVENTION

[0028] The present application will now be described in more detail with reference to the drawings and specific embodiments thereof, which are provided for illustrative purposes only and are not intended to be limiting in any way.

[0029] Any specific numerical value including the endpoints of a numerical range described in the context of this application should not be construed as being limited to that exact value, but should further be construed as including all values ​​close to that exact value, for example, all values ​​within ±5% of that exact value. Furthermore, with respect to any numerical range described herein, any combination between the endpoints of the range, between each endpoint and any specific value within the range, or between any two specific values ​​within the range, can be made to provide one or more new numerical ranges, which new numerical ranges should also be considered to be specifically described herein.

[0030] Unless otherwise stated, terms used herein have the same meaning as commonly understood by one of ordinary skill in the art, and if a term is defined herein and that definition differs from the normal understanding in the art, the definition provided herein shall control.

[0031] In the context of this application, in addition to the explicitly described matters, the undescribed matters or matters shall be regarded as the same as those known in the art without any modification.Furthermore, any of the embodiments described herein may be freely combined with one or more other embodiments described herein, and any technical solution or idea thus obtained shall be regarded as part of the original disclosure or original description of this application, and shall not be regarded as a new matter not disclosed or anticipated herein, unless it is obvious to a person skilled in the art that such a combination is obviously unreasonable.

[0032] All patent and non-patent literature cited herein, including but not limited to texts and articles, is hereby incorporated by reference in its entirety.

[0033] As mentioned above, in a first aspect, the present application provides an unsupported bimetallic hydrotreating catalyst comprising a complex formed by bonding a central atom or ion of a metal with an organic ligand via a coordinate bond, the metal being two selected from the group consisting of hydrogenation-active Group VB metals, Group VIB metals, Group VIII metals and Group IB metals. The organic ligand comprises a hydrocarbyl moiety and a coordinating group which is a -C(=O)-O group, and forms a coordinate bond with the central metal atom or ion via an oxygen atom, the catalyst having the general composition represented by formula (I): M 1 M 2 o a [R(COO) x ] b (I) Here, M 1 , M 2 represents a metal, and R(COO) xrepresents the organic ligand, R represents a hydrocarbyl group of the organic ligand, COO represents a coordinating group of the organic ligand, x represents the number of coordinating groups in the organic ligand, a represents the molar ratio of oxygen atoms bonded to the metal via a non-coordinating bond to the total amount of the metal, and b represents the molar ratio of the organic ligand to the total amount of the metal: M 1 and M. 2 are different from each other and each is independently one metal selected from the group consisting of Group VB metals, Group VIB metals, Group VIII metals, and Group IB metals having hydrogenation activity; R is a C3-C19 hydrocarbyl group, preferably selected from the group consisting of C5-C11 normal alkyl, C5-C11 isomeric alkyl, C5-C12 alkyl with a cycloalkyl moiety, and C6-C12 aryl; x is 1, 2 or 3, preferably 1 or 2; a is a positive number from 0 to 5, preferably from 1 to 3; and b is a positive number of 1 to 6, preferably 2 to 5.

[0034] Here, the catalyst is -1 ~1000cm -1 , 1350cm -1 ~1450cm -1 and 1500 cm -1 ~1610cm -1 4 shows an infrared spectrum with a characteristic peak at position .

[0035] According to the present application, the unsupported bimetallic hydroprocessing catalyst consists only of the complex and does not include a solid support component. However, if desired, the unsupported bimetallic hydroprocessing catalyst of the present application can also be present and used in the form of a composition having liquid components in which the catalyst can be dispersed, such as an organic solvent and an organic ligand compound.

[0036] According to the present application, the hydrogenation-active Group VB, VIB, VIII and IB metals in the complexes of the present application may be in the form of a central atom or a central ion, depending on the metal used.

[0037] According to the present application, the unsupported bimetallic hydrotreating catalyst may be a mixture of several different complexes, and the total amount of metal in the catalyst (i.e., metal M 1 and M. 2 The molar ratios a and b of oxygen atoms and organic ligands to the total amount of M in the composition may be non-integer values ​​because they are calculated values ​​based on the analysis of metal content and elemental composition. 1 , M 2 indicates only which metals are present, not the molar ratio between the metals.

[0038] In a preferred embodiment, at least a portion of the complexes in the catalyst have a structure represented by formula (I-1):

[0039] [ka] Here, M 1 and M. 2 represent metals which are different from each other and each independently have hydrogenation activity and are one selected from the group consisting of Group VB metals, Group VIB metals, Group VIII metals, and Group IB metals; → represents a coordinate bond; R is a C3-C19 hydrocarbyl group, preferably selected from the group consisting of C5-C11 normal alkyl, C5-C11 isomeric alkyl, C5-C12 alkyl with a cycloalkyl moiety, and C6-C12 aryl; x represents the number of coordination groups in the organic ligand, which is 1 or 2, preferably 1; n represents a coordination number and is a positive number of 1 to 6, preferably 2 to 5; y is a metal M 1 and metal M 2 represents the number of oxygen atoms bonded to both the z is a metal M 2 represents the number of oxygen atoms linked only to the group, and is a positive number of 0 to 2, preferably 0 or 1.

[0040] In a preferred embodiment, the catalyst has a peak at 1350 cm -1 ~1450cm -1 The characteristic peak at 1500 cm -1 ~1610cm -1 The distance between the characteristic peaks is 145 cm. -1 Greater than.

[0041] In preferred embodiments, the hydrogenation active Group VB, VIB, VIII and IB metals are selected from the group consisting of V, Cr, Mo, W, Fe, Co, Ru, Ni, Cu and Pd, more preferably selected from the group consisting of Mo, Ni, W, Fe, V and Co.

[0042] As used herein, the term "C3-C19 hydrocarbyl" refers to a hydrocarbyl group having 3 to 19 carbon atoms, which may be saturated or unsaturated and may be normal hydrocarbyl, isomeric hydrocarbyl, or hydrocarbyl with a cycloalkyl moiety, including, but not limited to, C3-C19 normal alkyl, C3-C19 isomeric alkyl, C5-C19 alkyl with a cycloalkyl moiety, and C6-C19 aryl.

[0043] In this application, the term "C3-C19 normal alkyl" refers to a normal alkyl group having 3 to 19 carbon atoms, preferably 5 to 11 carbon atoms, such as n-pentyl, n-hexyl, n-heptyl, n-octyl, n-nonyl, n-decyl, and n-undecyl.

[0044] In this application, the term "C3-C19 isomeric alkyl" refers to isomeric alkyl groups having 3 to 19 carbon atoms, preferably 5 to 11 carbon atoms, such as isopentyl, isohexyl, isoheptyl, isooctyl, isononyl, isodecyl, isoundecyl.

[0045] As used herein, the term "C5-C19 alkyl having a cycloalkyl moiety" refers to a saturated hydrocarbyl group having 5 to 19 carbon atoms, preferably 5 to 12 carbon atoms, including a saturated carbocyclic ring, such as cyclopentyl, cyclohexyl, methylcyclohexyl, decahydronaphthyl, methyldecahydronaphthyl, ethyldecahydronaphthyl, and the like.

[0046] In the present application, the term "C6-C19 aryl" refers to a hydrocarbyl group having 6 to 19 carbon atoms constituting an aromatic ring, such as phenyl, naphthyl, anthracyl, p-tolyl, benzyl, methylnaphthyl, methylanthracenyl, etc., and is preferably an aryl group having 6 to 12 carbon atoms.

[0047] According to the present application, the C3-C19 hydrocarbyl groups, the C3-C19 normal alkyl groups, the C3-C19 isomeric alkyl groups, the C5-C19 alkyl groups having a cycloalkyl moiety, and the C6-C19 aryl groups may be, for example, optionally substituted with one or more groups selected from halo, nitro, sulfonic acid groups, etc., or may be unsubstituted.

[0048] In a preferred embodiment, the organic ligand in the complex is derived from a C4-C20 organic carboxylic acid, preferably from one or more selected from the group consisting of C4-C20 normal or isomeric alkyl carboxylic acids, C6-C20 naphthenic carboxylic acids having a saturated carbon ring, and C7-C20 aromatic carboxylic acids having an aromatic ring, more preferably from one or more selected from the group consisting of C6-C12 normal or isomeric alkyl carboxylic acids, C6-C13 naphthenic carboxylic acids having a saturated carbon ring, and C7-C13 aromatic carboxylic acids having an aromatic ring, and even more preferably from one or more selected from the group consisting of succinic acid, hexanoic acid, adipic acid, heptanoic acid, octanoic acid, nonanoic acid, ethylhexanoic acid, oleic acid, petroleum acid, salicylic acid, benzoic acid, and phenylacetic acid.

[0049] In a preferred embodiment, the unsupported bimetallic hydrotreating catalyst has a metal content, based on the weight of the catalyst, of 5% to 35%, preferably 8% to 30%, more preferably 10% to 25%, and especially preferably 10% to 20%.

[0050] In a preferred embodiment, the unsupported bimetallic hydrotreating catalyst is obtained by directly reacting a hydrogenation active Group VB metal, Group VIB metal, Group VIII metal and / or Group IB metal, its oxide, its hydroxide, its metal oxyacid and / or its metal inorganic salt with an organic ligand compound selected from the group consisting of a C4-C20 organic carboxylic acid, preferably a C4-C20 normal or isomeric alkyl carboxylic acid, a C6-C20 naphthenic carboxylic acid having a saturated carbocyclic ring, a C7-C20 aromatic carboxylic acid having an aromatic ring, or a combination thereof.

[0051] According to the present application, the term "C4-C20 normal alkyl carboxylic acid" refers to a carboxylic acid having 4 to 20 carbon atoms obtained by binding one or more carboxyl groups to a normal alkane, such as butyric acid, succinic acid, valeric acid, hexanoic acid, adipic acid, heptanoic acid, octanoic acid, nonanoic acid, ethylhexanoic acid, tridecanoic acid, oleic acid, etc.

[0052] According to the present application, the term "C4-C20 isomeric alkyl carboxylic acid" refers to a carboxylic acid having 4 to 20 carbon atoms obtained by attaching one or more carboxyl groups to an isomeric alkane, such as isobutyric acid, isovaleric acid, isohexanoic acid, ethylhexanoic acid, etc.

[0053] According to the present application, the term "C6-C20 naphthenic acid having a saturated carbocyclic ring" refers to a carboxylic acid having 6 to 20 carbon atoms obtained by linking one or more carboxyl groups to an alkane compound having a saturated carbocyclic ring, such as cyclohexanecarboxylic acid, cyclohexanoic acid, cyclohexanedicarboxylic acid, cyclohexanedicarboxylic acid, decahydronaphthoic acid, decahydronaphthoic acid, decahydronaphthalenedicarboxylic acid, etc.

[0054] According to the present application, the term "C7-C20 aromatic carboxylic acid having an aromatic ring" refers to a carboxylic acid having 7 to 20 carbon atoms obtained by linking one or more carboxyl groups to an aromatic hydrocarbon, i.e., a hydrocarbon compound having an aromatic ring, such as benzoic acid, phenylacetic acid, phthalic acid, and phenylpropionic acid.

[0055] In a further preferred embodiment, the organic ligand compound is selected from the group consisting of C6-C12 normal or isomeric alkyl carboxylic acids, C6-C13 naphthenic carboxylic acids having saturated carbon rings, C7-C13 aromatic carboxylic acids having aromatic rings, or combinations thereof, and more preferably, is selected from the group consisting of succinic acid, hexanoic acid, adipic acid, heptanoic acid, octanoic acid, nonanoic acid, ethylhexanoic acid, oleic acid, petroleum acid, salicylic acid, benzoic acid, phenylacetic acid, or combinations thereof.

[0056] In a second aspect, the present application provides a method for preparing an unsupported bimetallic hydroprocessing catalyst comprising the steps of: 1) mixing a first metal source or a dispersion thereof with an organic ligand compound; 2) reacting the mixture obtained in step 1) at temperature T1 for a time t1; 3) reacting the material obtained in step 2) at temperature T2 for time t2; 4) optionally adding a second metal source or a dispersion thereof to the material obtained in step 3) and reacting the resultant at a temperature T2 for a time t3; and 5) Recovering the resulting liquid product.

[0057] wherein the first and second metal sources are each independently selected from the group consisting of elemental metals, metal oxides, metal hydroxides, metal oxyacids, metal inorganic salts, or combinations thereof, the metals of the first and second metal sources are the same as or different from each other, and each independently are one or two selected from the group consisting of Group VB metals, Group VIB metals, Group VIII metals, and Group IB metals having hydrogenation activity; The organic ligand compound is selected from a C4-C20 organic carboxylic acid or anhydride thereof; a molar ratio of the organic ligand compound to the total amount of metals in the first and second metal sources is 1 to 10:1; The temperature T1 is 50° C. to 150° C., preferably 80° C. to 120° C., and the time t1 is 5 minutes to 180 minutes, preferably 10 minutes to 150 minutes. The temperature T2 is 100° C. to 350° C., preferably 160° C. to 260° C., and the time t2 is 1 hour to 8 hours, preferably 2 hours to 5 hours. The time t3 is 1 hour to 8 hours, preferably 2 hours to 5 hours, However, when only the first metal source is used or the metal of the second metal source is the same as the metal of the first metal source, the metal of the first metal source is two metals selected from the group consisting of Group VB metals, Group VIB metals, Group VIII metals, and Group IB metals having hydrogenation activity.

[0058] The preparation method of the catalyst of the present application adds a pre-reaction step 2) (i.e., performing a pre-reaction at a temperature T1 for a time t1), thereby providing a metal complex with a higher metal content and improved storage stability.

[0059] According to the present application, the pressure and reaction atmosphere used in steps 2), 3) and 4) are not particularly limited, but for example, the reaction pressure may be atmospheric pressure, and the reaction atmosphere may be air, nitrogen or an inert atmosphere.

[0060] In a preferred embodiment, the mixture obtained in step 1) is composed of the first metal source and the organic ligand compound, or is composed of the first metal source, a dispersion medium for dispersing the first metal source, and the organic ligand compound.

[0061] According to the present application, the C4-C20 organic carboxylic acid used as the organic ligand compound in step 1) may be one specifically described in the first aspect of the present application. For example, in a preferred embodiment, the organic ligand compound is selected from the group consisting of C4-C20 normal or isomeric alkyl carboxylic acids, C6-C20 naphthenic carboxylic acids having saturated carbon rings, C7-C20 aromatic carboxylic acids having aromatic rings, or combinations thereof, preferably selected from the group consisting of C6-C12 normal or isomeric alkyl carboxylic acids, C6-C13 naphthenic carboxylic acids having saturated carbon rings, C7-C13 aromatic carboxylic acids having aromatic rings, or combinations thereof, more preferably selected from the group consisting of succinic acid, hexanoic acid, adipic acid, heptanoic acid, octanoic acid, nonanoic acid, ethylhexanoic acid, oleic acid, petroleum acid, salicylic acid, benzoic acid, phenylacetic acid, or combinations thereof.

[0062] According to the present application, the first and second metal sources may each independently comprise one or two hydrogenation-active group VB, VIB, VIII or IB metals. When comprising two of these metals, the first and second metal sources may each independently be a single metal source comprising the two metals or a mixture of two or more metal sources each comprising one or two metals.

[0063] In a preferred embodiment, when step 4) is used, at least some of the metals contained in the second metal source are different from the metals contained in the first metal source, for example the first metal source contains one metal and the second metal source contains one metal different from the former, or the first metal source contains one metal and the second metal source contains two metals, one of which is the same as the metal contained in the first metal source. More preferably, the first metal source and the second metal source each contain one metal, and the metals contained in the two metal sources are different.

[0064] According to the present application, the molar ratio of the first metal source to the second metal source calculated based on metal can be any value and is not particularly limited. In a preferred embodiment, the ratio of the first metal source to the second metal source is 1:1-5.

[0065] In some particular embodiments, the method comprises the steps of: i) dispersing a first metal source in a dispersion medium to obtain a dispersion of the first metal source; ii) adding an organic ligand compound to the dispersion obtained in step i), heating the mixture to a temperature T1, and reacting the mixture at the temperature T1 for a time t1; iii) heating the material obtained in step ii) to a temperature T2 and reacting at said temperature T2 for a time t2; and iv) After the reaction is completed, the reaction is cooled and the resulting liquid product is recovered.

[0066] In another particular embodiment, the method comprises the steps of: i) dispersing a first metal source directly in an organic ligand compound; ii) heating the mixture obtained in step i) to a temperature T1 and reacting at said temperature T1 for a time t1; iii) heating the material obtained in step ii) to a temperature T2 and reacting at said temperature T2 for a time t2; and iv) After the reaction is completed, the reaction is cooled and the resulting liquid product is recovered.

[0067] In another particular embodiment, the method comprises the steps of: a) adding a first metal source or a dispersion thereof to an organic ligand compound; b) heating the mixture obtained in step a) to a temperature T1 and reacting at said temperature T1 for a time t1; c) heating the material obtained in step b) to a temperature T2 and reacting at said temperature T2 for a time t2; d) adding a second metal source to the material obtained in step c) and reacting at temperature T2 for a time t3; and e) After the reaction is completed, the reaction is cooled and the resulting liquid product is recovered.

[0068] According to the method of the present application, the metal inorganic salt can be an inorganic acid salt of the metal, such as a chloride, sulfide, sulfate, nitrate, carbonate, or a metal oxyacid salt of the metal, such as an ammonium salt of a metal oxyacid. In a preferred embodiment, the first and second metal sources are each independently selected from the group consisting of a metal oxide, metal hydroxide, metal chloride, metal sulfide, metal sulfate, metal nitrate, metal carbonate, metal oxyacid, or metal oxyacid salt, such as the oxides, hydroxides, chlorides, sulfides, sulfates, nitrates, and carbonates of V, Mo, W, Fe, Co, Ni, Cu, and Zn, molybdic acid, tungstic acid, various forms of ammonium molybdate, ammonium tungstate, or combinations thereof.

[0069] According to the method of the present application, the dispersion medium in the dispersion of the metal source may be an inorganic dispersion medium which may be selected from the group consisting of water, carbonic acid, hydrochloric acid, sulfuric acid, or phosphoric acid, or an organic dispersion medium selected from the group consisting of an aliphatic hydrocarbon, an aromatic hydrocarbon, an alicyclic hydrocarbon, a halogenated hydrocarbon, an alcohol solvent, an ether solvent, an ester solvent, a ketone solvent, or a combination thereof, and more preferably selected from the group consisting of ethanol, toluene, xylene, petroleum ether, gasoline, diesel, or a combination thereof.

[0070] In a preferred embodiment, the weight ratio of the dispersion medium to the first metal source in the first metal source dispersion liquid, and the weight ratio of the dispersion medium to the second metal source in the second metal source dispersion liquid are each independently 1 to 25:1, preferably 2 to 8:1.

[0071] In a preferred embodiment, the first metal source and the second metal source are used in a molar ratio of 1:1 to 5, calculated on the basis of the metals.

[0072] In the present application, the reaction step is not particularly limited in reaction pressure and reaction atmosphere, for example, the reaction pressure may be atmospheric pressure, and the reaction atmosphere may be air, nitrogen or an inert atmosphere.

[0073] According to the present application, the reaction can be carried out in the presence or absence of water (for example, in the presence of water in an amount of 0 to 10 times the weight of the organic ligand compound).

[0074] According to the present application, the reaction can be carried out in the absence of other components (e.g., catalysts, basic pH adjusters, etc.) in addition to the metal source, the organic ligand compound, and any solvent (e.g., water and organic solvents such as toluene, ethanol, diesel, etc.).

[0075] In a third aspect, the present application provides a bimetallic hydroprocessing catalyst composition comprising an unsupported bimetallic hydroprocessing catalyst according to the present application and at least one organic ligand compound and / or an organic solvent, wherein the organic ligand compound is selected from a C4-C20 organic carboxylic acid.

[0076] According to the present application, the C4-C20 organic carboxylic acid contained as an organic ligand compound in the bimetallic hydrotreating catalyst composition may be one specifically described in the first aspect of the present application. For example, in a preferred embodiment, the organic ligand compound is selected from the group consisting of C4-C20 normal or isomeric alkyl carboxylic acids, C6-C20 naphthenic carboxylic acids having a saturated carbon ring, C7-C20 aromatic carboxylic acids having an aromatic ring, or combinations thereof, preferably selected from the group consisting of C6-C12 normal or isomeric alkyl carboxylic acids, C6-C13 naphthenic carboxylic acids having a saturated carbon ring, C7-C13 aromatic carboxylic acids having an aromatic ring, or combinations thereof, more preferably selected from the group consisting of succinic acid, hexanoic acid, adipic acid, heptanoic acid, octanoic acid, nonanoic acid, ethylhexanoic acid, oleic acid, petroleum acid, salicylic acid, benzoic acid, phenylacetic acid, or combinations thereof.

[0077] In the present application, the organic solvent is not particularly limited as long as it can be dispersed or miscible with the unsupported bimetallic hydrotreating catalyst, and may be selected from the group consisting of, for example, aliphatic hydrocarbons, aromatic hydrocarbons, alicyclic hydrocarbons, halogenated hydrocarbons, alcohol solvents, ether solvents, ester solvents, ketone solvents, or combinations thereof, and is preferably selected from the group consisting of toluene, gasoline, ethanol, diesel, or combinations thereof.

[0078] In a preferred embodiment, based on the weight of the composition, the unsupported bimetallic hydrotreating catalyst is present in an amount of 50% to 95%, preferably 80% to 95%, and the total amount of the organic ligand compound and the organic solvent is 5% to 50%, preferably 5% to 20%.

[0079] In a preferred embodiment, the composition comprises at least one organic ligand compound, and the composition has a molecular weight of 700 to 1000 cm -1 , 1350~1450cm -1 , 1500~1100cm -1 and 1700-1750cm-1 The infrared spectrum has a characteristic peak at the position of 700 to 1000 cm. -1 , 1350~1450cm -1 and 1500~1610cm -1 The characteristic peak at the position of 1700 to 1750 cm is a characteristic peak of the complex. -1 The characteristic peak at the position is a characteristic peak of the organic ligand compound.

[0080] In a further preferred embodiment, the hydrotreating catalyst composition is composed of the unsupported bimetallic hydrotreating catalyst and at least one organic ligand compound. In this case, the composition of the hydrotreating catalyst composition is represented by the formula (I), M 1 M 2 O a [R(COO) x ] b In addition, the compound can be represented diagrammatically using the formula: 1 , M 2 , a, R and x are as defined above, and b is a metal M 1 and M. 2 This represents the molar ratio of the total amount of the organic ligand and the organic ligand compound to the total amount of the organic ligand and the organic ligand compound.

[0081] In some particular embodiments, the hydrotreating catalyst composition may further comprise other components for improving oil solubility, storage stability, and oxidation resistance, such as organic materials having reducing and stabilizing properties, such as formic acid, oxalic acid, formaldehyde, ethylenediamine, oleylamine, etc., and the other components may be present in an amount of 0% to 80% by weight, preferably 0% to 50% by weight of the composition.

[0082] In a fourth aspect, there is provided the use of an unsupported bimetallic hydroprocessing catalyst or a bimetallic hydroprocessing catalyst composition according to the present application in the hydrogenation of hydrocarbons.

[0083] In a fifth aspect, there is provided a process for hydrotreating a hydrocarbon feedstock, the process comprising contacting said hydrocarbon feedstock for a hydrogenation reaction with an unsupported bimetallic hydrotreating catalyst or a bimetallic hydrotreating catalyst composition according to the present application.

[0084] According to the present application, the hydrocarbon feedstock can be various unsaturated hydrocarbon compounds such as benzene, alkylbenzene, naphthalene, alkylnaphthalene, anthracene, alkylanthracene, etc.; or a mixture of unsaturated hydrocarbon compounds such as crude oil, gasoline, diesel, vacuum gas oil, residual oil, etc.

[0085] In a preferred embodiment, the hydrogenation reaction conditions are a reaction temperature of 380° C. to 430° C., an initial hydrogen pressure of 5 MPa to 20 MPa, and a reaction time of 0.05 h. -1 ~1.0h -1 and a catalyst concentration (calculated on a metals basis) of 50 μg / g to 10,000 μg / g for the total feed.

[0086] In a sixth aspect, the present application provides an unsupported catalyst composition comprising 10% to 45% by weight of a hydrotreating catalyst component, 45% to 80% by weight of a carrier fluid, and 1.0% to 10% by weight of an activator, the hydrotreating catalyst component being comprised of the unsupported bimetallic hydrotreating catalyst of the present application and optionally an organic ligand compound, the organic ligand compound being selected from a C4-C20 organic carboxylic acid.

[0087] According to the present application, examples of C4-C20 organic carboxylic acids that can be contained in the hydrotreating catalyst component as an organic ligand compound include those specifically described in the first aspect of the present application, but detailed description thereof will be omitted here.

[0088] According to the present application, the dispersing medium suitable for use in the unsupported catalyst composition can be any liquid material capable of promoting dissolution and dispersion of the metal-organic complex in the unsupported bimetallic hydrotreating catalyst, including, but not limited to, organic solvents and petroleum fractions capable of dispersing the catalyst or being miscible with the catalyst. The organic solvent can be selected from the group consisting of aliphatic hydrocarbons, aromatic hydrocarbons, alicyclic hydrocarbons, halogenated hydrocarbons, alcohol solvents, ether solvents, ester solvents, ketone solvents, or combinations thereof, preferably selected from the group consisting of aliphatic hydrocarbons, aromatic hydrocarbons, alicyclic hydrocarbons, or combinations thereof, such as n-octane, cyclohexane, toluene, and decahydronaphthalene, more preferably aromatic solvents. The petroleum fraction can be selected from distillate oils having a distillation range of 150°C to 524°C, or residual oil components having a boiling point above 524°C, such as solvent gasoline, AGO fractions, LCO, oil slurries, furfural extracts, atmospheric residues, and vacuum residues, preferably aromatic-rich petroleum fractions.

[0089] According to the present application, an activator suitable for the unsupported catalyst composition is a material capable of activating the MO bonds in the metal-organic complexes of the unsupported bimetallic hydroprocessing catalyst to form MS bonds in the hydrogenation active phase, which may be, for example, elemental sulfur, a sulfur-containing compound, a mixture of sulfur-containing compounds, or a combination thereof, and is preferably selected from the group consisting of thiols, thioethers, carbon disulfide, sulfur, thiophene compounds, or a combination thereof.

[0090] In a preferred embodiment, the hydrotreating catalyst component is present in an amount of 10% to 45%, preferably 10% to 30%, based on the weight of the unsupported catalyst composition, the dispersing medium is present in an amount of 45% to 80%, preferably 60% to 80%, and the activator is present in an amount of 1.0% to 10%, preferably 3.0% to 10.0%.

[0091] In a seventh aspect, there is provided the use of the unsupported catalyst composition of the present application in the hydroupgrading of heavy oil.

[0092] In an eighth aspect, the present application provides a process for hydroupgrading a heavy oil comprising subjecting a heavy oil feedstock to a hydroupgrading reaction under heating conditions in the presence of hydrogen and an unsupported hydroprocessing catalyst composition of the present application, the hydroprocessing catalyst composition being optionally presulfurized.

[0093] In a preferred embodiment, the hydro-upgrading conditions include: an amount of the unsupported catalyst composition, calculated on a metal basis, of 50 μg / g to 10,000 μg / g, preferably 50 μg / g to 3,000 μg / g, based on the weight of the heavy oil feedstock; an initial hydrogen pressure of 5 MPa to 20 MPa, preferably 5 to 15 MPa; a reaction temperature of 360°C to 480°C, preferably 390°C to 450°C; and a reaction time of 0.05 h. -1 ~2.0h -1 , preferably 0.05 to 1.0 h -1 and a hydrogen to oil volume ratio of 300 to 2000, preferably 500 to 1500. [Example] The present application will be further described with reference to the following examples, but the present application is not limited thereto. In the following examples, unless otherwise specified, the reagents and materials used are commercially available products and are chemically pure. In the following examples, the metal content of the obtained product was measured by inductively coupled plasma optical emission spectrometry (ICP-OES) using a plasma optical emission spectrometer ARCOS SOP manufactured by SPECTRO, with the optical chamber sealed and filled with argon gas, and measured by vertical observation at wavelengths of 130 to 770 nm. In the following examples, the elemental composition of the obtained products was determined as follows: the contents of elements C, H were determined by using an Italian Cara Erba EA1110 elemental analyzer according to the SH0656 method; the content of element S was measured according to the energy dispersive X-ray fluorescence spectroscopy GB 17040 method; and the content of element O was measured by the O-content method. In the following examples, the infrared spectra of the obtained products were measured using a Thermo Fisher NICOLET IS50 spectrometer with a scanning wavelength of 400 to 4000 cm -1 The measurement was performed with 16 scans. A ZnSe crystal and a HgCdTe infrared detector were used to measure the attenuated total reflectance (ATR) of the sample at 4 cm -1 The measurements were performed with a resolution of . Examples 1-6 and Comparative Example 1 The amount of compounds shown in Table 1 was weighed out and placed in a three-neck flask, and reacted under the conditions shown in Table 1. After the reaction was completed, the metal compounds in the flasks of Examples 1-5 were completely dissolved, and the unreacted metal compounds remained in the flask of Example 6. The liquid reaction products in the flasks obtained in Examples 1-5 were poured out to obtain the target catalyst products, and the product of Example 6 was filtered to remove the unreacted metal compounds, thereby obtaining the target catalyst products. Comparative Example 1 was carried out using the same raw materials as Example 1, but in a slightly different manner. The metal content of the catalyst was measured using inductively coupled plasma optical emission spectroscopy (ICP-OES), and the elemental composition of the catalyst was measured using a corresponding method, and the composition of the catalyst was determined according to the measurement results of the metal content and elemental composition. The raw materials used, reaction conditions, and test results of Examples 1-6 and Comparative Example 1 are shown in Table 1. [Table 1] JPEG2024538238000004.jpg76169As shown in Table 1, the metal content of the unsupported bimetallic catalyst or bimetallic hydrotreating catalyst composition of the present application can be 12.30-33.3%, and the molar ratio of the organic ligand to the total amount of metal in the catalyst, or the molar ratio of the combined amount of the organic ligand and the organic ligand compound to the total amount of metal in the catalyst, is 1.7-3.7.

[0094] The results of elemental analysis of the product obtained in Example 1 are shown in Table 2. a (I C 7 H 16 COO) bThe values ​​of a and b in the product composition represented by the formula (I) can be calculated from the data shown in Table 2 as b = 0.54 / (0.10 + 0.10) = 2.70 and a = (1.26 - 2.0 × 0.54) / 0.20 = 0.9.

[0095] [Table 2] The results of elemental analysis of the catalyst obtained in Example 3 are shown in Table 3. a (C 7 H 16 COO) b The values ​​of a and b in the catalyst composition represented by the formula (1) are calculated from the data shown in Table 3 to be b = 0.54 / (0.11 + 0.11) = 2.45 and a = (1.36 - 2.0 × 0.54) / 0.22 = 1.27.

[0096] [Table 3] The IR spectra of the catalysts obtained in Examples 1 to 6 are shown in Figures 1 to 6. As is clear from Figures 1 to 6, the catalysts of all Examples have a peak intensity of 700 to 1000 cm -1 , 1350~1450cm -1 and 1500~1610cm -1 A characteristic peak is shown at the position.

[0097] As shown in FIG. 1, the catalyst of Example 1 has a peak density of 700 to 1000 cm -1 The characteristic peak of MO vibration is shown at 1350-1450 cm -1 and 1500~1610cm -1 The characteristic peak of the coordination between the -C(=O)-O group and the metal is shown at the position of 1350-1450 cm -1 A characteristic peak at 1500-1610 cm -1 The distance between the characteristic peaks at the positions (i.e., the difference in wave numbers corresponding to the positions of the apexes of those peaks) is 145 cm -1 This indicates that the catalyst contains a complex having a monodentate structure represented by the following formula:

[0098] [ka] The data in Table 1 show that by adding step (2) (i.e., pre-reaction at temperature T1 for time t1) in the preparation of the catalyst, the complex obtained in Example 1 has a higher metal content than the complex obtained in Comparative Example 1. In addition, the data in Table 4 show that the complex obtained in Example 1 exhibits higher storage stability than the complex obtained in Comparative Example 1.

[0099] [Table 4] Examples 7-8 The catalyst products obtained in Examples 1 and 3 were each dispersed in toluene to evaluate the oil solubility of the unsupported hydrotreating catalyst obtained by the method of the present application. The dissolution and dispersion results in toluene of the products of Examples 1 and 3 are shown in Figures 7 and 8, respectively. As can be seen from the figures, the unsupported hydrotreating catalyst synthesized according to the present application is completely miscible with toluene, indicating that the unsupported hydrotreating catalyst has good oil solubility.

[0100] Examples 9-10 The products obtained in Examples 1 and 4 were used as catalysts for the hydrotreating of aromatic hydrocarbons, i.e., phenanthrene, and tetralin was used as a solvent. The mass fraction of phenanthrene in 10 g of the total reactants (phenanthrene + solvent) was 10%, and the reaction was carried out in a 100 ml continuous stirring autoclave under the following test conditions: initial hydrogen pressure 9 MPa, reaction temperature 420°C, reaction time 60 minutes, catalyst concentration (calculated based on metal) 2500 μg / g (relative value to the weight of the total reactants). The test results are shown in Table 5.

[0101] Comparative Example 2 The test was carried out in the same manner as in Example 9, except that the product obtained in Example 1 was replaced with a conventional supported catalyst (Ni-Mo supported catalyst for residual oil hydrotreating, Mo content 9.3 mass%, Ni content 2.52 mass%) in terms of metal amount equivalent. The test results are shown in Table 5.

[0102] [Table 5] As can be seen from the results in Table 5, the unsupported bimetallic catalyst of the present invention showed higher phenanthrene conversion and higher yield of deep hydrogenation products compared with the supported catalyst, and the number of moles of hydrogenated phenanthrene was increased by 72-98% compared with the supported catalyst.

[0103] Examples 11-12 The product obtained in Example 1 and an organic ligand compound (i.e., ethyl hexanoate) were blended in a composition with a mass ratio of 95:5. This composition and the product obtained in Example 6 were used as catalysts to carry out the hydrogenolysis reaction of an alkyl-substituted aromatic hydrocarbon, i.e., dodecylpyrene. Decahydronaphthalene was used as a solvent, the mass fraction of dodecylpyrene in 10 g of the total reactants (dodecylpyrene + solvent) was 10%, and the reaction was carried out in a 100 ml autoclave with stirring under test conditions including an initial hydrogen pressure of 9 MPa, a reaction temperature of 420°C, a reaction time of 60 minutes, and a catalyst concentration (calculated on a metal basis) of 2500 μg / g (calculated on a weight basis of the total reactants). The test results are shown in Table 6.

[0104] [Table 6] The results in Table 6 show that the unsupported bimetallic catalyst and its composition of the present application can both achieve a dodecylpyrene decomposition conversion rate of 100% and a dodecylpyrene condensation rate of 0%. Compared with the product of Example 6, the catalyst composition to which an organic ligand compound is further added exhibits high hydrogen consumption, and the catalyst composition of the present application has higher hydrogen activation activity and higher hydrogen consumption under the same conditions than the catalyst itself.

[0105] Examples 13-15 Using 200 g of vacuum residue A with an asphaltene content of 14%, a Conradson carbon residue value of 26.4%, and a heavy metal (Ni+V) content of 210 μg / g as the raw material, a catalytic hydrothermal conversion test of the residual oil was carried out with stirring in a 2 L batch autoclave under the catalyst and reaction conditions shown in Table 7. The test results are shown in Table 7.

[0106] Comparative Example 3 The test was carried out in the same manner as in Example 13, except that the catalyst used in Example 13 was replaced with a conventional supported catalyst (Ni-Mo supported catalyst for residual oil hydrotreating, Mo content 9.3 mass%, Ni content 2.52 mass%). The test results are shown in Table 7.

[0107] [Table 7] As can be seen from the results in Table 7, the unsupported bimetallic hydrotreating catalyst of the present invention has a higher residual oil cracking rate, a lower coke rate, and a higher distillate yield under the same reaction conditions compared to conventional supported catalysts.

[0108] Examples 16-18 The catalyst products, carrier, and activator of Examples 1 and 6 were used to form unsupported hydrotreating catalyst compositions. The content of each component in the resulting unsupported hydrotreating catalyst composition is shown in Table 8.

[0109] [Table 8] Example 19 The catalyst composition obtained in Example 17 was subjected to a preliminary sulfurization treatment under conditions of a reaction temperature of 360° C., an initial hydrogen pressure of 5 MPa, and a reaction time of 30 minutes, and the reaction product was recovered after the test.

[0110] Examples 20-23 The catalyst composition products of Examples 17, 18 and 19 and the catalyst product of Example 1 were mixed with 200g of vacuum residue B raw material having asphaltene content of 12.8%, Conradson carbon residue number of 26.3% and heavy metal (Ni+V) content of 220μg / g, respectively, and subjected to a vacuum residue hydrothermal conversion test in a 2L batch autoclave under the conditions of reaction temperature 425℃, initial hydrogen pressure 9MPa and reaction time 130min. The test results are shown in Table 9.

[0111] [Table 9] Comparing the results of Example 21 and Example 20 in Table 9, it can be seen that the unsupported catalyst composition of Example 17 containing an activator has a slightly higher residual oil conversion rate, a higher asphaltene upgrading rate, and a 47% reduction in the coke rate, compared to the product of Comparative Example 1 containing no activator, and thus has excellent asphaltene condensation reaction inhibition performance.

[0112] On the other hand, as can be seen from a comparison of the results of Example 22 and Example 20 shown in Table 9, the unsupported catalyst composition product of Example 17 containing an organic ligand compound (i.e., ethylhexanoic acid) exhibits a higher residual oil conversion rate, an asphaltene upgrading rate, and a lower coke rate compared to the unsupported catalyst composition product of Example 18 not containing an organic ligand compound.

[0113] Furthermore, as can be seen from the comparison of the results of Example 23 and Example 20 in Table 9, when the unsupported catalyst composition product of Example 17 is subjected to pre-sulfurization treatment, the residual oil conversion rate and asphaltene upgrading rate can be further improved, and the coke rate can be further reduced.

[0114] Although the present application has been described in detail herein with reference to preferred embodiments, it is not intended to be limited to these embodiments. Various modifications can be made in accordance with the inventive concept of the present application, and these modifications are intended to be within the scope of the present application.

[0115] It should be noted that the various technical features described in the above embodiments can be combined in any suitable manner without contradiction, and in order to avoid unnecessary repetition, the various possible combinations are not described in this specification, but such combinations are also within the scope of this specification.

[0116] Furthermore, the various embodiments of the present application may be combined in any manner unless such combination deviates from the spirit of the present application, and such combined embodiments should be considered as the disclosure of the present application. [Brief description of the drawings]

[0117] The drawings forming part of this specification are provided to aid in the understanding of the present application and should not be considered limiting. The present application can be read with reference to the drawings in combination with the following detailed description herein. In the drawings: [Figure 1] FIG. 1 is an IR spectrum of the product obtained in Example 1; [Diagram 2] FIG. 2 is an IR spectrum of the product obtained in Example 2; [Diagram 3] FIG. 3 is an IR spectrum of the product obtained in Example 3; [Figure 4] FIG. 4 is an IR spectrum of the product obtained in Example 4; [Diagram 5] FIG. 5 is an IR spectrum of the product obtained in Example 5; [Figure 6] FIG. 6 is an IR spectrum of the product obtained in Example 6; [Figure 7] FIG. 7 is an image showing the result of dissolving the catalyst obtained in Example 1 in toluene; and [Figure 8] FIG. 8 is an image showing the result of dissolving the catalyst obtained in Example 3 in toluene.

Claims

1. An unsupported bimetallic hydrotreating catalyst comprising a complex formed by bonding a metal central atom or ion to an organic ligand via a coordinate bond, said catalyst having an approximate composition represented by formula (I): M 1 M 2 O a [R(COO) x b Formula (I)​ Here, M 1 and M. 2 represents a metal, and R(COO) x represents an organic ligand, R represents a hydrocarbyl group of the organic ligand, COO represents a coordinating group of the organic ligand, x represents the number of coordinating groups in the organic ligand, a represents the molar ratio of oxygen atoms bonded to the metal via non-coordinating bonds to the total amount of the metal, and b represents the molar ratio of the organic ligand to the total amount of the metal; M 1 and M. 2 are different from each other and each is independently one metal selected from the group consisting of Group VB metals, Group VIB metals, Group VIII metals, and Group IB metals having hydrogenation activity; R is a C3-C19 hydrocarbyl group, preferably selected from the group consisting of C5-C11 normal alkyl, C5-C11 isomeric alkyl, C5-C12 alkyl with a cycloalkyl moiety, and C6-C12 aryl; x is 1, 2 or 3, preferably 1 or 2; a is a positive number from 0 to 5, preferably from 1 to 3; and b is a positive number from 1 to 6, preferably from 2 to 5; The catalyst is 700 cm -1 ~1000cm -1 , 1350 cm -1 ~1450cm -1 and 1500 cm -1 ~1610cm -1 4. An unsupported bimetallic hydrotreating catalyst having an infrared spectrum with a characteristic peak at

2. At least a portion of the complex in the catalyst has a structure represented by formula (I-1): 【Chemistry 1】 Here, M 1 , M. 2 , R and x are as defined in claim 1; → represents a coordinate bond; x represents the number of coordinating groups in the organic ligand, which is 1 or 2, preferably 1; n represents a coordination number and is a positive number from 1 to 6, preferably from 2 to 5; y is a metal M 1 and the metal M 2 represents the number of oxygen atoms bonded to both z is a metal M 2 2. The unsupported bimetallic hydrotreating catalyst according to claim 1, wherein R represents the number of oxygen atoms bonded only to R, and is a positive number from 0 to 2, preferably 0 or 1.

3. In the IR spectrum of the catalyst, -1 and a characteristic peak at 1500-1610 cm -1 The distance between the characteristic peaks at the positions is 145 cm -1 3. The unsupported bimetallic hydrotreating catalyst of claim 1 or 2, wherein

4. 4. An unsupported bimetallic hydrotreating catalyst according to any one of claims 1 to 3, wherein the hydrogenation active Group VB, VIB, VIII and IB metals are selected from the group consisting of V, Cr, Mo, W, Fe, Co, Ru, Ni, Cu and Pd, preferably selected from the group consisting of Mo, Ni, W, Fe, V and Co.

5. The unsupported bimetallic hydrotreating catalyst according to any one of claims 1 to 4, wherein the organic ligand is derived from a C4-C20 organic carboxylic acid, preferably from one or more selected from the group consisting of C4-C20 normal or isomeric alkyl carboxylic acids, C6-C20 naphthenic carboxylic acids containing a saturated carbocyclic ring, and C7-C20 aromatic carboxylic acids containing an aromatic ring, more preferably from one or more selected from the group consisting of C6-C12 normal or isomeric alkyl carboxylic acids, C6-C13 naphthenic carboxylic acids containing a saturated carbocyclic ring, and C7-C13 aromatic carboxylic acids containing an aromatic ring, and even more preferably from one or more selected from the group consisting of succinic acid, hexanoic acid, adipic acid, heptanoic acid, octanoic acid, nonanoic acid, ethylhexanoic acid, oleic acid, petroleum acid, salicylic acid, benzoic acid, and phenylacetic acid.

6. 6. Unsupported bimetallic hydrotreating catalyst according to any one of claims 1 to 5, wherein the catalyst has a metal content, calculated on a metal basis relative to the weight of the catalyst, of 5% to 35%, preferably 8% to 30%, more preferably 10% to 25%, particularly preferably 10% to 20%.

7. A process for preparing the unsupported bimetallic hydrotreating catalyst of any one of claims 1 to 6, comprising the steps of: 1) mixing a first metal source or a dispersion thereof with an organic ligand compound; 2) reacting the mixture obtained in step 1) at temperature T1 for a time t1; 3) reacting the material obtained in step 2) at temperature T2 for a time t2; 4) optionally adding a second metal source or a dispersion thereof to the material obtained in step 3) and reacting the resultant at a temperature T2 for a time t3; and 5) recovering the resulting liquid product; the first and second metal sources are each independently selected from the group consisting of elemental metals, metal oxides, metal hydroxides, metal oxyacids, metal inorganic salts, or combinations thereof, the metals of the first and second metal sources are the same as or different from each other, and each independently are one or two selected from the group consisting of Group VB metals, Group VIB metals, Group VIII metals, and Group IB metals having hydrogenation activity; The organic ligand compound is selected from a C4-C20 organic carboxylic acid or anhydride thereof, preferably selected from the group consisting of a C4-C20 normal or isomeric alkyl carboxylic acid, a C6-C20 naphthenic carboxylic acid containing a saturated carbocyclic ring, a C7-C20 aromatic carboxylic acid or anhydride thereof containing an aromatic ring, or a combination thereof; the molar ratio of said organic ligand compound to the total amount of metal in said first and second metal sources is 1 to 10:1; The temperature T1 is 50° C. to 150° C., preferably 80° C. to 120° C., and the time t1 is 5 minutes to 180 minutes, preferably 10 minutes to 150 minutes. the temperature T2 is 100° C. to 350° C., preferably 160° C. to 260° C., and the time t2 is 1 hour to 8 hours, preferably 2 hours to 5 hours; The time t3 is 1 hour to 8 hours, preferably 2 hours to 5 hours, However, when only the first metal source is used or when the metal of the second metal source is the same as the metal of the first metal source, the metal of the first metal source is two metals selected from the group consisting of Group VB metals, Group VIB metals, Group VIII metals, and Group IB metals having hydrogenation activity.

8. The mixture obtained in step 1) consists of the first metal source and the organic ligand compound; or The method according to claim 7, wherein the mixture obtained in step 1) consists of the first metal source, a dispersion medium for dispersing the first metal source, and the organic ligand compound.

9. 9. The method of claim 7 or 8, wherein the first and second metal sources are each independently selected from the group consisting of elemental metals, metal oxides, metal hydroxides, metal chlorides, metal sulfides, metal sulfates, metal nitrates, metal carbonates, metal oxyacids, salts of metal oxyacids, or combinations thereof.

10. When a dispersion of a metal source is used, the dispersion medium in the dispersion is an inorganic dispersion medium selected from the group consisting of water, carbonic acid, hydrochloric acid, sulfuric acid, or phosphoric acid, or an organic dispersion medium selected from the group consisting of ethanol, toluene, xylene, petroleum ether, gasoline, diesel, or a combination thereof; 10. The method of any one of claims 7 to 9, wherein the weight ratio of the dispersing medium in the dispersion of the first metal source to the first metal source, and the weight ratio of the dispersing medium in the dispersion of the second metal source to the second metal source are each independently from 1 to 25:1, more preferably from 2 to 8:

1.

11. The method according to any one of claims 7 to 10, wherein the first metal source and the second metal source are used in a molar ratio of 1:1-5, calculated on the basis of the metals.

12. A bimetallic hydrotreating catalyst composition comprising the unsupported bimetallic hydrotreating catalyst according to any one of claims 1 to 6 and at least one organic ligand compound and / or organic solvent, The organic ligand compound is selected from C4-C20 organic carboxylic acids, preferably C4-C20 normal or isomeric alkyl carboxylic acids, C6-C20 naphthenic carboxylic acids containing saturated carbon rings, C7-C20 aromatic carboxylic acids containing aromatic rings, or combinations thereof, more preferably C6-C12 normal or isomeric alkyl carboxylic acids, C6-C13 naphthenic carboxylic acids containing saturated carbon rings, C7-C13 aromatic carboxylic acids containing aromatic rings, or combinations thereof, and even more preferably succinic acid, hexanoic acid, adipic acid, heptanoic acid, octanoic acid, nonanoic acid, ethylhexanoic acid, oleic acid, petroleum acid, salicylic acid, benzoic acid, phenylacetic acid, or combinations thereof; The organic solvent is selected from the group consisting of aliphatic hydrocarbons, aromatic hydrocarbons, alicyclic hydrocarbons, halogenated hydrocarbons, alcohol solvents, ether solvents, ester solvents, ketone solvents, or combinations thereof, and is preferably selected from the group consisting of toluene, gasoline, ethanol, diesel, or combinations thereof.

13. The composition includes at least one organic ligand compound, and the composition has a molecular weight of 700 to 1000 cm -1 , 1350-1450cm -1 , 1500-1610cm -1 and 1700-1750 cm -1 13. The composition of claim 12, exhibiting an infrared spectrum having a characteristic peak at

14. 14. The composition according to claim 12 or 13, wherein the unsupported bimetallic hydrotreating catalyst is present in an amount of 50% to 95%, preferably 80% to 95%, and the total amount of the organic ligand compound and the organic solvent is 5% to 50%, preferably 5% to 20%, based on the weight of the composition.

15. A method for hydrotreating a hydrocarbon feedstock, comprising the step of contacting the hydrocarbon feedstock with the unsupported bimetallic hydrotreating catalyst according to any one of claims 1 to 6 or the bimetallic hydrotreating catalyst composition according to any one of claims 12 to 14 to carry out a hydrotreating reaction, wherein the hydrocarbon feedstock is an unsaturated hydrocarbon compound such as benzene, alkylbenzene, naphthalene, alkylnaphthalene, anthracene, alkylanthracene, or a mixture containing unsaturated hydrocarbon compounds such as crude oil, gasoline, light oil, vacuum gas oil, residual oil, or the like.

16. An unsupported catalyst composition suitable for hydrogenation of heavy oil, comprising 10 wt. % to 45 wt. % of a hydrotreating catalyst component, 45 wt. % to 80 wt. % of a dispersing medium, and 1.0 wt. % to 10 wt. % of an activator; The hydrotreating catalyst component comprises an unsupported bimetallic hydrotreating catalyst according to any one of claims 1 to 6, and optionally an organic ligand compound, the organic ligand compound being selected from C4-C20 organic carboxylic acids; The dispersion medium is selected from the group consisting of an organic solvent, a petroleum fraction, or a combination thereof, the organic solvent is selected from the group consisting of an aliphatic hydrocarbon, an aromatic hydrocarbon, an alicyclic hydrocarbon, a halogenated hydrocarbon, an alcohol solvent, an ether solvent, an ester solvent, a ketone solvent, or a combination thereof, and the petroleum fraction is selected from a distillate oil having a distillation range of 150°C to 524°C or a residual oil component having a boiling point above 524°C; The composition, wherein the activator is selected from the group consisting of elemental sulfur, a sulfur-containing compound, or a combination thereof, preferably selected from the group consisting of a thiol, a thioether, carbon disulfide, sulfur, a thiophene compound, or a combination thereof.

17. The composition according to claim 16, wherein the organic ligand compound is selected from the group consisting of C4-C20 normal or isomeric alkyl carboxylic acids, C6-C20 naphthenic carboxylic acids containing saturated carbocyclic rings, C7-C20 aromatic carboxylic acids containing aromatic rings, or combinations thereof, preferably selected from the group consisting of C6-C12 normal or isomeric alkyl carboxylic acids, C6-C13 naphthenic carboxylic acids containing saturated carbocyclic rings, C7-C13 aromatic carboxylic acids containing aromatic rings, or combinations thereof, more preferably selected from the group consisting of succinic acid, hexanoic acid, adipic acid, heptanoic acid, octanoic acid, nonanoic acid, ethylhexanoic acid, oleic acid, petroleum acid, salicylic acid, benzoic acid, phenylacetic acid, or combinations thereof.

18. 18. The unsupported catalyst composition according to claim 16 or 17, wherein the hydrotreating catalyst component has a metal content of 5% to 35%, preferably 8% to 30%, more preferably 10% to 25%, particularly preferably 10% to 20%, and an organic ligand compound content of 0% to 50%, preferably 5% to 50%, more preferably 5% to 20%, based on the weight of the hydrotreating catalyst component.

19. The unsupported catalyst composition according to any one of claims 16 to 18, wherein the hydrotreating catalyst component is the liquid product obtained by the process according to any one of claims 7 to 11.

20. Use of the unsupported catalytic composition according to any one of claims 16 to 19 in hydroupgrading of heavy oil.

21. 20. A method for hydroupgrading heavy oil, comprising subjecting a heavy oil feedstock to a hydroupgrading reaction under heated conditions in the presence of hydrogen and the unsupported catalyst composition of any one of claims 16 to 19, wherein the unsupported catalyst composition is optionally presulfided.

22. The conditions of the hydro-upgrading are: the amount of the unsupported catalyst composition calculated based on the weight of the heavy oil feedstock on a metal basis is 50 μg / g to 10,000 μg / g; the initial hydrogen pressure is 5 MPa to 20 MPa; the reaction temperature is 360° C. to 480° C.; the liquid hourly space velocity is 0.05 h -1 ~2.0h -1 and a volume ratio of hydrogen to oil of 300 to 2000; Preferably, the hydro-upgrading conditions are: the amount of the unsupported catalyst composition calculated on a metal basis relative to the weight of the heavy oil feedstock is 50 μg / g to 3000 μg / g; the initial hydrogen pressure is 5 MPa to 15 MPa; the reaction temperature is 390° C. to 450° C.; and the liquid hourly space velocity is 0.05 to 1.0 h . -1 22. The use according to claim 20 or the method according to claim 21, comprising a volume ratio of hydrogen to oil of 500 to 1500.

Citation Information

Patent Citations

  • Hydrocracking nickel-molybdenum catalyst and preparation method thereof

    CN107866279A

  • Complex containing molybdenum and iron, preparation method of complex, hydrogenation catalyst and application thereof

    CN112745357A

  • Hydrocracking catalyst and process in suspension bed

    CN1362489A

  • Hydrocarbon Soluble Bimetallic Catalyst Precursor and Method of Making Same

    JP2009522102A