Temperature stabilization of convertible functional inks by blocking conductive paths
By integrating high aspect ratio particles and a polymer network into convertible inks, the conversion to a conductive phase during thermal processes is prevented, maintaining the insulating state and ensuring pattern integrity.
Patent Information
- Application Number
- JP2024521840
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2022-10-07
- Filing Date
- 2022-10-11
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2042-10-11
AI Technical Summary
Convertible inks used in electronic structures face issues where insulating materials unintentionally convert to a conductive phase during thermal processes like soldering or microelectronic packaging, rendering patterning ineffective.
Incorporating high aspect ratio particles and a three-dimensional polymer network into the ink to form a stabilizing layer that blocks conductive paths, using a polymer network with acrylate polymer and high aspect ratio particles to fill gaps and prevent coalescence of conductive particles during thermal exposure.
The stabilizing layer effectively maintains the insulating state of the ink even after thermal exposure, ensuring the integrity of the intended conductive patterns.
Smart Images

Figure 2024539615000001_ABST
Abstract
Description
[Technical field]
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS This application claims priority to U.S. Provisional Patent Application No. 63 / 254,230, filed October 11, 2021, which is incorporated by reference in its entirety, and to U.S. Nonprovisional Patent Application No. 17 / 938,688, filed October 7, 2022, which is incorporated by reference in its entirety. [Background technology]
[0002] TECHNICAL FIELD This disclosure relates to convertible inks, and more particularly, to temperature stabilization of convertible inks.
[0003] Convertible inks can be used to create electronic structures. Examples of convertible inks include composite materials that have an insulating or dielectric phase after curing, but can be selectively converted to a conductive or resistive phase by methods such as heat treatment or laser sintering. Summary of the Invention
[0004] According to one or more embodiments, the ink stabilizing composition comprises a polymer network comprising an acrylate polymer and a plurality of high aspect ratio particles, each of the high aspect ratio particles having an aspect ratio of about 2:1 to about 30:1 and an average particle size of about 0.5 to about 1.2 micrometers.
[0005] According to another embodiment, the stabilizing ink includes a plurality of conductive particles, a plurality of insulating particles, a plurality of high aspect ratio stabilizing particles, and a polymer in voids between the plurality of conductive particles and the plurality of insulating particles, the stabilizing ink being in an insulating phase.
[0006] Further, according to some embodiments, a method of stabilizing a convertible ink includes disposing a stabilizing material on the convertible ink. The stabilizing material includes a polymer network and a plurality of high aspect ratio particles, each having an aspect ratio of about 2:1 to about 30:1 and an average particle size of about 0.5 to about 1.2 micrometers. The convertible ink includes a plurality of conductive particles and a plurality of insulating particles.
[0007] Additional features and advantages are realized through the techniques of the present disclosure. Other embodiments and aspects of the present disclosure are described in detail herein and are considered a part of the claimed disclosure. For a better understanding of the present disclosure, together with its advantages and features, reference is made to the description and drawings.
[0008] For a more complete understanding of this disclosure, reference is now made to the following brief description in conjunction with the accompanying drawings and detailed description, where like reference numerals represent like parts, and in which: [Brief description of the drawings]
[0009] [Figure 1A] a laser sintering method for converting a dielectric portion of a convertible ink into a conductive portion; [Figure 1B] 1 is a close-up of a dielectric portion of a convertible ink; [Figure 1C] A close-up of the conductive pathways of the convertible ink after laser sintering; [Figure 2A] Depicts the dielectric portion of the convertible ink; [Figure 2B] Shown is the convertible ink after application of a layer of stabilizing material; [Figure 2C] showing the interruption of the conductive pathway after application of a stabilizing material layer and laser sintering; [Diagram 3] 1 is a graph showing the change in resistance of a convertible ink with and without a stabilizing layer; [Figure 4A] FIG. 1 is a top view of a patterning stabilization layer on a transformable ink layer; and [Figure 4B] FIG. 4B is a side view of FIG. 4A. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] A convertible ink is a composite material that has an insulating or dielectric phase after curing, but is selectively converted to a conductive or resistive phase by methods such as heat treatment or laser sintering. A convertible ink can include, for example, a composite blend of conductive and insulating particles. Non-limiting examples of convertible inks include conductive metal nanoparticles (e.g., silver) and insulating nanoparticles (e.g., barium strontium titanate) blended in a ratio such that the ink contains an insulating phase after curing, but provides a conductive (and resistive) phase after high temperature heat treatment (e.g., temperatures above 125 degrees Celsius), such as selective laser sintering with an ultraviolet laser. Selective laser sintering can be performed using most lasers, but lasers with wavelengths of 400-450 nanometers (nm) provide optimal results. It should be noted that the surface plasmon resonance of silver (Ag) nanoparticles is about 400-450 nm, so if silver is used in the convertible ink, exciting the surface plasmon resonance of the Ag nanoparticles will efficiently melt the silver nanoparticles due to the localized heating generated by the surface plasmon resonance excitation. In addition, other lasers, such as 830 nm lasers in particular, are also suitable for sintering silver nanoparticles to form conductive patterns. The laser wavelength used is tailored to the conductive nanoparticles. For example, if gold nanoparticles are used, a 532 nm laser can be used to excite the surface plasmon resonance of gold. However, any wavelength laser may be used and tailored to the particular conductive nanoparticle.
[0011] For example, Figure 1A is a laser sintering method for converting a dielectric portion of a convertible ink to a conductive portion. After curing, the convertible ink becomes an insulating phase. A laser 110 converts the insulating portion 102 of the convertible ink to a conductive portion 106. Figure 1B is a close-up of the dielectric portion 102 of the convertible ink, which includes a blend of conductive particles 122 and insulating particles 120. Figure 1C is a close-up of the conductive portion 106 showing how the conductive pathways of the convertible ink are formed after laser sintering or thermal sintering, which fuses the conductive particles 122.
[0012] The convertible inks can be used as printable inks printed as films that can be easily patterned to create conductive traces by the application of localized heat. However, it is desirable for the insulating material to remain in an insulating state after the traces have been patterned. However, in some applications, a subsequent thermal process (e.g., soldering or other packaging process) can unintentionally convert the desired pattern to a conductive state, negating the patterning process.
[0013] Thus, described herein are stabilizing materials, and methods of making and using same, that introduce high aspect ratio particles and three-dimensional polymer networks into the convertible ink and prevent the formation of conductive paths in the film, even after thermal exposure such as soldering or microelectronic packaging processes. The stabilizing materials can be used as patterned masks to selectively define conductive traces in the dielectric portion of the convertible ink. As used herein, the term "convertible ink" and other similar terms refer to a composite of conductive and non-conductive particles that is converted from an insulating phase to a conductive / resistive phase by thermal or laser sintering.
[0014] FIG 2A shows the dielectric portion of the convertible ink after curing, which includes a blend of conductive particles 224 and insulating particles 222 with air gaps 202 between them. FIG 2B shows the convertible ink after applying a layer of stabilizing material to the convertible ink. The stabilizing layer includes polymer 204 and high aspect ratio particles 260 that fill the air gaps 202 in the convertible ink. FIG 2C shows the convertible ink after thermal exposure, such as laser sintering or thermal sintering, and the interruption of conductive pathways 230 by high aspect ratio particles 260. Both polymer 204 and high aspect ratio particles 260 are necessary to prevent the formation of conductive pathways 230.
[0015] The conductive particles 224 in the convertible ink include conductive metal particles. Non-limiting examples of conductive metal particles include silver particles, gold particles, copper particles, or combinations thereof.
[0016] In one or more embodiments, the conductive particles 224 are present in the convertible ink in an amount of about 55 to about 70 weight percent (wt%). In other embodiments, the conductive particles 224 are present in the convertible ink in an amount of about 60 to about 65 wt%. Additionally, in some embodiments, the conductive particles 224 are present in the convertible ink in an amount of about 62.5 wt%.
[0017] In some embodiments, the average diameter of the conductive particles 224 is about 20 to about 200 nanometers (nm). In other embodiments, the average diameter of the conductive particles 224 is about 80 to about 120 nm. However, in some embodiments, the average diameter of the conductive particles 224 is about 100 nm. To find a homogeneous distribution after curing, the average diameters of the conductive particles 224 and the insulating particles 222 must be very close.
[0018] The insulating particles 222 in the convertible ink include an insulating (dielectric) material or alloy. A non-limiting example of the insulating particles 222 includes barium strontium titanate particles. In one or more embodiments, the insulating particles 222 have a melting point of at least 700 degrees Celsius.
[0019] In some embodiments, the insulating particles 222 have an average diameter of about 20 to about 200 nanometers (nm). In other embodiments, the insulating particles 222 have an average diameter of about 80 to about 120 nm. Additionally, in some embodiments, the insulating particles 222 have an average diameter of about 100 nm.
[0020] In one or more embodiments, the insulating particles 222 are present in the convertible ink in an amount of about 30 to about 45 weight percent (wt%). In other embodiments, the insulating particles 222 are present in the convertible ink in an amount of about 35 to about 40 wt%. Furthermore, in some embodiments, the insulating particles 222 are present in the convertible ink in an amount of about 37.5 wt%.
[0021] According to one or more embodiments, the conductive particles 224 are silver particles and the insulating particles 222 are barium strontium titanate particles.
[0022] To make the convertible ink, the conductive particles 224 and insulating particles 222 are combined in a solvent(s) and, optionally, one or more additives. Non-limiting examples of solvents include 1-methoxy-2-propanol, ethylene glycol, or any combination thereof. In one or more embodiments, the solvent is a glycol solvent.
[0023] The mixture of conductive particles 224 and insulating particles 222 in the solvent(s) and optional additives is then cured by application of heat. After curing, the convertible ink remains in the insulating / dielectric phase and contains only conductive particles 222 and insulating particles 224.
[0024] Curing is accomplished, for example, by heating for a period of time. The temperature and time of curing will vary depending on the composition of the convertible ink. According to one or more embodiments, curing is accomplished by heating at a temperature between about 75 degrees Celsius and about 125 degrees Celsius. In other embodiments, curing is accomplished by heating at a temperature between about 80 degrees Celsius and about 100 degrees Celsius.
[0025] Once the convertible ink has been formed and cured, a layer of stabilizing material is applied and cured with UV light.
[0026] The stabilization layer includes a polymer 204 and high aspect ratio particles 260 that fill the air gaps 202 in the convertible ink (see FIG. 2B). FIG. 2C shows the convertible ink and the interruption of conductive pathways 230 by high aspect ratio particles 260 after a thermal treatment such as ultraviolet laser sintering. The relatively large high aspect ratio particles 260 reduce the ratio of conductive particles 224 to insulating particles 222 in the initially cured convertible ink. The relatively large high aspect ratio particles 260 further impede the coalescence of conductive particles 224 during thermal sintering as conductive pathways 230 are formed.
[0027] According to one or more embodiments, the high aspect ratio particles 260 are hexagonal boron nitride particles. In some embodiments, the high aspect ratio particles 260 have an aspect ratio of about 2:1 to about 30:1. In other embodiments, the high aspect ratio particles 260 have an aspect ratio of about 10:1 to about 20:1.
[0028] According to one or more embodiments, the high aspect ratio particles 260 have an average diameter of about 0.5 to about 1.2 micrometers. In other embodiments, the high aspect ratio particles 260 have an average diameter of about 0.8 to about 1.0 micrometers.
[0029] In one or more embodiments, the high aspect ratio particles 260 are present in the stabilizing layer in an amount of about 5 to about 20 wt %. In other embodiments, the high aspect ratio particles 260 are present in the stabilizing layer in an amount of about 12 to about 15 wt %.
[0030] According to one or more embodiments, the polymer 204 that fills the air gaps 202 in the convertible ink is an acrylate polymer. Other non-limiting examples of polymers include trimethylolpropane ethoxylate triacrylate, urethane acrylate, epoxy acrylate, polyester acrylate, or any combination thereof. In some embodiments, the polymer 204 is a triacrylate polymer, which creates a strong three-dimensional polymer network as a result of three unsaturated sites. The three-dimensional network of polymer created by the polymer 204 fills the air gaps 202 and minimizes reflow of the conductive particles 224.
[0031] The polymer 204, which forms a three-dimensional network, can withstand high temperatures without decomposing. In some embodiments, the polymer 204 can withstand temperatures of about 100 degrees Celsius to about 250 degrees Celsius without decomposing. In other embodiments, the polymer 204 can withstand temperatures of about 200 to about 225 degrees Celsius without decomposing.
[0032] To form the stabilization layer, one or more photoinitiators are combined with the polymer 204 precursor (i.e., oligomers and / or monomers), the high aspect ratio particles 260, and optionally one or more additives, such as one or more photoinitiators. If added, the one or more optional additives are added in an amount of about 0.25 to about 5 wt %. The combination is mixed until no agglomerations are visible.
[0033] In one or more embodiments, the polymer precursors (e.g., oligomers and / or monomers) are present in the stabilizing layer in an amount of about 70 to about 89 wt %. In other embodiments, the polymer precursors (e.g., oligomers and / or monomers) are present in the stabilizing layer in an amount of about 80 to about 85 wt %.
[0034] Non-limiting examples of photoinitiators include 1-hydroxycyclohexyl phenyl ketone, phenylbis(2,4,6,7-trimethylbenzoyl)phosphine oxide, 2-methyl-4'-(methylthio)-2-morpholinopropionophenone, benzophenone, 4-benzoyl-4'-methyldiphenyl sulfide, benzyl dimethyl ketal, 2-benzyl-2-dimethylamino-1-(4-morpholinophenyl)-1-butanoate, or any combination thereof.
[0035] A layer of stabilizing material is applied to the surface of the convertible ink in its dielectric phase. When applied, the stabilizing layer prevents the formation of conductive pathways that would otherwise convert the ink to a conductive phase under thermal treatment (see FIG. 3).
[0036] A stabilizing layer is formed over the cured convertible ink layer. In some embodiments, the stabilizing layer is patterned as a mask. Figures 4A and 4B show top and side views, respectively, of a patterned stabilizing layer 402 over a convertible ink layer 404, which is a cured dielectric phase. Portions of the stabilizing layer 402 are removed to expose selected portions of the underlying convertible ink, and the uncovered portions are selectively heat treated, for example by laser sintering, to form selected conductive portions 406. The stabilizing layer 402 protects the unexposed portions of the convertible ink layer 404. EXAMPLES
[0037] Example 1: Stabilizing Layer Formulation An example of a stabilizing layer formulation is shown in Table 1 below. [Table 1]
[0038] The oligomer, boron nitride, and photoinitiator are placed in a glass jar covered with aluminum foil. The jar is then agitated with 10 second on-off cycles for 2 hours. The sample is checked every minute for agglomerations. If agglomerates are present, the mixture is mixed by hand until broken down. The final mixture should be free of visible agglomerations. EXAMPLES
[0039] Example 2: Changes in resistance measurements Thermal stability testing of the silver barium strontium titanate convertible ink was performed. The convertible ink was laser sintered and Figure 3 is a graph showing the change in resistance of the convertible ink with and without a stabilizing layer. When the convertible ink was protected with a stabilizing layer (UV96), the resistance did not change significantly. However, without the stabilizing layer, the measured resistance changed significantly, indicating that the insulating material was fully converted to a conductor.
[0040] The following definitions and abbreviations should be used in interpreting the claims and the specification. As used herein, the terms "comprises," "comprising," "includes," "including," "has," "having," "contains," or "containing," or any other variation thereof, are intended to cover a non-exclusive inclusion. For example, a composition, mixture, process, method, article, or device that includes a list of elements is not necessarily limited to only those elements, but can include other elements not expressly listed or inherent to such composition, mixture, process, method, article, or device.
[0041] Moreover, the term "exemplary" is used herein to mean "serving as an example, instance, or illustration." Any embodiment or design described herein as "exemplary" should not necessarily be construed as preferred or advantageous over other embodiments or designs. The terms "at least one" and "one or more" are understood to include any integer number greater than or equal to one, i.e., 1, 2, 3, 4, etc. The term "plurality" is understood to include any integer number greater than or equal to two, i.e., 2, 3, 4, 5, etc. The term "connected" can include indirect and direct "connections."
[0042] References in the specification to "one embodiment," "embodiment," "exemplary embodiment," and the like indicate that the described embodiment may include a particular feature, structure, or characteristic, but every embodiment may or may not include the particular feature, structure, or characteristic. Moreover, such phrases do not necessarily refer to the same embodiment. Moreover, it is submitted that when a particular feature, structure, or characteristic is described in connection with an embodiment, it is within the knowledge of one of ordinary skill in the art to affect such feature, structure, or characteristic in connection with other embodiments, whether or not explicitly described.
[0043] For purposes of the following description, the terms "above," "below," "right," "left," "vertical," "horizontal," "top," "bottom," and their derivatives refer to the structures and methods described as oriented in the drawings. The terms "overlying," "on," "above," "located on," or "located on" mean that a first element, such as a first structure, is on a second element, such as a second structure, and that an intervening element, such as an interface structure, may be between the first and second elements. The term "direct contact" means that a first element, such as a first structure, and a second element, such as a second structure, are connected without any intermediate conductive, insulating, or semiconducting layer at the interface of the two elements.
[0044] The terms "about," "substantially," and "approximately," as well as variations thereof, are intended to include the degree of error associated with measurement of a particular quantity based on equipment available at the time of filing. For example, "about" can include a range of ±10%, 9%, 8%, 7%, 6%, or 5%, 4%, 3%, 2%, or 1% of a given value.
[0045] The corresponding structures, materials, acts, and equivalents of all means or step-plus-function elements in the following claims are intended to include any structures, materials, or acts for performing functions in combination with other claimed elements as specifically claimed. The description of the present disclosure has been presented for purposes of illustration and description, but is not intended to be exhaustive or to limit the disclosure to the detailed form set forth. Many changes and modifications will be apparent to those skilled in the art without departing from the scope and spirit of the present disclosure. The selection and description of the embodiments have been made in order to best explain the principles and practical applications of the present disclosure, and to enable others skilled in the art to understand the various embodiments with various modifications suitable for the particular applications intended.
[0046] While preferred embodiments have been described, it will be appreciated that those skilled in the art, both now and in the future, may make various improvements and enhancements that fall within the scope of the following claims, which should be interpreted to maintain the appropriate protection for the disclosure originally described.
Claims
1. A polymer network comprising an acrylate polymer; and a plurality of high aspect ratio particles, each having an aspect ratio of about 2:1 to about 30:1 and an average particle size of about 0.5 to about 1.2 micrometers; 1. An ink stabilizing composition comprising:
2. The ink stabilizing composition of claim 1 , wherein the acrylate polymer is a triacrylate polymer.
3. 10. The ink stabilizing composition of claim 1, wherein the acrylate polymer is trimethylolpropane ethoxylate triacrylate, urethane acrylate, epoxy acrylate, polyester acrylate, or any combination thereof.
4. The ink stabilizing composition of claim 1 , wherein each of the plurality of high aspect ratio particles has an aspect ratio of about 10:1 to about 20:
1.
5. The ink stabilizing composition of claim 1 , wherein each of the plurality of high aspect ratio particles has an average particle size of about 0.8 to about 1.0 micrometers.
6. The ink stabilizing composition of claim 1 , wherein each of the plurality of high aspect ratio particles is boron nitride.
7. The ink stabilizing composition of claim 1 further comprising a photoinitiator.
8. A plurality of conductive particles; A plurality of insulating particles; a plurality of high aspect ratio stabilized particles; a polymer in voids between the plurality of conductive particles and the plurality of insulating particles, The stabilized ink is an insulating phase.
9. The stabilized ink of claim 8 , wherein the polymer is an acrylate polymer.
10. The stabilized ink of claim 9, wherein the acrylate polymer is a triacrylate polymer.
11. 10. The stabilized ink of claim 9, wherein the acrylate polymer is trimethylolpropane ethoxylate triacrylate, urethane acrylate, epoxy acrylate, polyester acrylate, or any combination thereof.
12. 9. The stabilized ink of claim 8, wherein each of the plurality of high aspect ratio stabilized particles has an aspect ratio of about 10:1 to about 20:
1.
13. 9. The stabilized ink of claim 8, wherein each of the plurality of high aspect ratio stabilized particles has an average particle size of about 0.8 to about 1.0 micrometers.
14. The stabilized ink of claim 8 , wherein the plurality of high aspect ratio particles are boron nitride.
15. 1. A method for stabilizing a convertible ink, comprising: disposing a stabilizing material over the convertible ink; the stabilizing material comprises a polymer network and a plurality of high aspect ratio particles, each having an aspect ratio of about 2:1 to about 30:1 and an average particle size of about 0.5 to about 1.2 micrometers; The method, wherein the convertible ink comprises a plurality of conductive particles and a plurality of insulating particles.
16. The method of claim 15 , wherein the polymer network comprises an acrylate polymer.
17. The method of claim 16 , wherein the acrylate polymer is a triacrylate polymer.
18. 17. The method of claim 16, wherein the acrylate polymer is trimethylolpropane ethoxylate triacrylate, urethane acrylate, epoxy acrylate, polyester acrylate, or any combination thereof.
19. The method of claim 15 , wherein said each of said plurality of high aspect ratio particles is boron nitride.
20. The method of claim 15 , wherein the stabilizing material further comprises a photoinitiator.
Citation Information
Patent Citations
Photosensitive conductive paste
JP2012094508A
Laminate, solar cell rear surface protection sheet using same, and solar cell module
WO2018034117A1
Heat-conducting layer, photosensitive layer, photosensitive composition, method for producing heat-conducting layer, and laminate and semiconductor device
WO2019203178A1