Polymer manufacturing method
Using specific dispersant mixtures of hydroxyalkylmethylcellulose in the polymerization process addresses the issue of polymer fines in macroporous polymer production, resulting in enhanced polymer quality and yield.
Patent Information
- Application Number
- JP2024529642
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-11-18
- Filing Date
- 2022-11-15
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2042-11-15
AI Technical Summary
There is a need for a process that can reduce the polymer particulate fraction during the preparation of macroporous polymers, as existing methods like suspension polymerization often result in undesirable polymer fine particle formation.
The use of specific dispersant mixtures comprising hydroxyalkylmethylcellulose with defined molecular weights and substitution degrees, such as hydroxypropyl methyl cellulose and hydroxyethyl methyl cellulose, in the polymerization process to reduce the polymer fines fraction.
The process effectively reduces the polymer fines fraction, leading to improved polymer quality and yield, as demonstrated by the examples provided.
Smart Images

Figure 2024540757000001 
Figure 2024540757000002 
Figure 2024540757000003
Abstract
Description
[Technical field]
[0001] The present invention relates to the preparation of polymers in the presence of a dispersing agent mixture and to the use of a dispersing agent mixture for preparing polymers in order to make ion exchangers from the polymers. [Background technology]
[0002] It is known that polymers can be prepared, for example, from vinyl aromatic compounds, such as styrene, in combination with crosslinking agents, such as divinylbenzene, by suspension polymerization.
[0003] In suspension polymerization, a monomer phase containing a monomer-soluble initiator is partitioned as droplets in a phase that is substantially immiscible with the monomer and cured by increasing the temperature. The immiscible phase is usually an aqueous phase, which may contain additives such as salts, dispersants, or protective colloids, or other water-soluble organic compounds, also referred to as the continuous phase. The mixture of the selected water-insoluble monomer and additives and initiators dissolved therein forms the dispersed phase.
[0004] In addition to polymers in gel form, macroporous polymers can also be produced in suspension polymerization by using porogens such as high boiling aliphatic hydrocarbons, alcohols, ethers, nitro compounds, or esters.
[0005] It is known from (Non-Patent Document 1) that during the suspension polymerization of methyl methacrylate, some emulsion polymerization also occurs at the same time, resulting in the formation of an undesirable polymer fine particle fraction. The polymer fine particle fraction formed by emulsion polymerization can be reduced by adding a free radical inhibitor soluble in the aqueous phase.
[0006] US Patent No. 5,399,633 discloses a process for preparing bead polymers in gel form with reduced content of soluble polymers, in which a peroxyester is used as an initiator to reduce the soluble fraction. [Prior art documents] [Patent documents]
[0007] [Patent Document 1] European Patent Application Publication No. A-0964002 [Non-patent literature]
[0008] [Non-Patent Document 1] F. Jahanzad, S. Sajjadi, B. Brooks, Polymer, 2013, 54, 16-23 Summary of the Invention [Problem to be solved by the invention]
[0009] In view of the known prior art, there remains a need for a process that can reduce the polymer fine particle fraction when preparing macroporous polymers. [Means for solving the problem]
[0010] It has now surprisingly been discovered that when certain dispersant mixtures are used during polymerization, the polymer fines fraction can be reduced.
[0011] The present invention therefore relates to a process for preparing a polymer, comprising reacting at least one monoethylenically unsaturated compound and at least one multiethylenically unsaturated compound in the presence of at least one initiator, in the presence of water, in the presence of a porogen, and a) at least one hydroxyalkyl methylcellulose having a number average molecular weight of 80,000 g / mol to 110,000 g / mol; b) at least one hydroxyalkyl methylcellulose having a number average molecular weight of 25,000 g / mol to 42,000 g / mol; The present invention provides a process for reacting in the presence of a dispersant mixture comprising: DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] The term "molecular weight" as used herein refers to number average molecular weight, unless expressly stated or otherwise specified.
[0013] As the hydroxyalkyl methylcellulose of a) it is preferred to use hydroxypropyl methylcellulose and / or hydroxyethyl methylcellulose having a molecular weight of 80000 g / mol to 110000 g / mol.
[0014] As the hydroxyalkyl methylcellulose of b), it is preferable to use hydroxypropyl methylcellulose and / or hydroxyethyl methylcellulose having a molecular weight of 25000 g / mol to 42000 g / mol.
[0015] In a), it is preferable to use 2-hydroxypropyl methylcellulose having a degree of 2-hydroxypropyl substitution of 3 to 15 mol %, a degree of methoxy substitution of 26 to 31 mol % and a molecular weight of 80000 g / mol to 110000 g / mol.
[0016] In a), it is preferable to use hydroxyethyl methylcellulose having a degree of methoxy substitution of 26 to 31 mol %, a degree of hydroxyethoxy substitution of 5 to 15 mol % and a molecular weight of 80 000 g / mol to 110 000 g / mol.
[0017] In b), it is preferred to use 2-hydroxypropyl methylcellulose having a degree of 2-hydroxypropyl substitution of 3 to 15 mol % and a degree of methoxy substitution of 18 to 25 mol % and a molecular weight of 25000 g / mol to 42000 g / mol.
[0018] In b), it is preferable to use hydroxyethylmethylcellulose having a degree of methoxy substitution of 18 to 25 mol %, a degree of hydroxyethoxy substitution of 5 to 15 mol % and a molecular weight of 25 000 g / mol to 42 000 g / mol.
[0019] It is particularly preferable to use a mixture containing a) 2-hydroxypropyl methylcellulose having a degree of 2-hydroxypropyl substitution of 3 to 15 mol%, a degree of methoxy substitution of 26 to 31 mol%, and a molecular weight of 80,000 g / mol to 110,000 g / mol, and b) 2-hydroxypropyl methylcellulose having a degree of 2-hydroxypropyl substitution of 3 to 15 mol%, a degree of methoxy substitution of 18 to 25 mol%, and a molecular weight of 25,000 g / mol to 42,000 g / mol.
[0020] It is very particularly preferable to use a mixture comprising a) 2-hydroxypropyl methylcellulose having a degree of 2-hydroxypropyl substitution of 3 to 8 mol%, a degree of methoxy substitution of 26 to 31 mol% and a molecular weight of 80000 g / mol to 110000 g / mol, and b) 2-hydroxypropyl methylcellulose having a degree of 2-hydroxypropyl substitution of 6 to 13 mol%, a degree of methoxy substitution of 18 to 25 mol% and a molecular weight of 25000 g / mol to 42000 g / mol.
[0021] The hydroxyalkyl methylcelluloses of a) and b) are known and can be prepared by generally known processes, for example by reacting cellulose with an alkali metal hydroxide and then with an alkyl halide.
[0022] Hydroxyalkyl methylcelluloses are also commercially available. Particularly preferred for use as hydroxyalkyl methylcelluloses a) are Methocel® F4M (2-hydroxypropyl methylcellulose with a molecular weight of 95000 g / mol) (DOW Chemical Company) (CAS number 9004-65-3), Walocel® VPM4937 (CAS number 9032-42-2) (hydroxyethyl methylcellulose with a molecular weight of 100000 g / mol) and Tylose® E707002 (CAS number 9004-65-3) (2-hydroxypropyl methylcellulose with a molecular weight of 95000 g / mol) or mixtures of these compounds.
[0023] Particularly preferred for use as b) hydroxyalkyl methylcellulose are Methocel® K100 (2-hydroxypropyl methylcellulose having a molecular weight of 33,500 g / mol) (CAS number 9004-65-3) and Metolose® 90SH-100 (CAS number 9004-65-3) (2-hydroxypropyl methylcellulose having a molecular weight of 33,000 g / mol) or mixtures of these compounds.
[0024] The 2-hydroxypropyl methylcellulose preferably used in a) and having a degree of 2-hydroxypropyl substitution of 3 to 15 mol %, a degree of methoxy substitution of 26 to 31 mol % and a molecular weight of 80,000 g / mol to 110,000 g / mol preferably has a viscosity of 3,000 to 9,000 mPas.
[0025] The hydroxyethyl methylcellulose preferably used in a) having a degree of methoxy substitution of 26 to 31 mol %, a degree of hydroxyethoxy substitution of 5 to 15 mol % and a molecular weight of 80000 to 110000 g / mol preferably has a viscosity of 3000 to 9000 mPas.
[0026] The 2-hydroxypropyl methylcellulose preferably used in b) having a degree of 2-hydroxypropyl substitution of 3 to 15 mol %, a degree of methoxy substitution of 18 to 25 mol %, and a molecular weight of 25,000 g / mol to 42,000 g / mol preferably has a viscosity of 80 to 500 mPas.
[0027] Preferably in b) the hydroxyethyl methylcellulose having a degree of methoxy substitution of 18-25 mol %, a degree of hydroxyethoxy substitution of 7-10 mol % and a molecular weight of 25000-42000 g / mol preferably has a viscosity of 80-500 mPas.
[0028] The 2-hydroxypropyl methylcellulose and hydroxyethyl methylcellulose used in a) and b) preferably have a heat gelling temperature of greater than 60°C.
[0029] The hydroxyalkyl methylcelluloses a) and b) can be mixed with each other in any ratio. The weight ratio of the hydroxyalkyl methylcelluloses a) and b) is preferably 3:1 to 1:1.
[0030] The total concentration of the hydroxyalkyl methylcelluloses a) and b) is preferably 0.15 to 0.3% by weight based on the aqueous phase.
[0031] The molar substitution of hydroxypropyl and methoxy groups of 2-hydroxypropyl methylcellulose is determined according to ASTM D-2363-72 / USA.
[0032] The molar substitution of the methoxy group of the hydroxyethyl methylcellulose is determined in accordance with ASTM D-1347-72 / USA.
[0033] The molar substitution of the hydroxyethoxy groups of the hydroxyethyl methylcellulose is determined in accordance with ASTM D-2364-75 / USA.
[0034] The molar substitution is1 H NMR and 13 It can be further determined by C NMR spectroscopy.
[0035] The molecular weight of the hydroxyalkyl methyl cellulose can be determined by the method described in Journal of Polymer Science and Technology, 39(4), 293-298 (1982).
[0036] The heat gelling temperature can be determined in accordance with paragraph
[0028] of EP B1-1983004.
[0037] The viscosity of the hydroxyalkyl methylcellulose can be determined by conventional methods known to those skilled in the art, preferably by using a rotational viscometer at 25°C.
[0038] The 2-hydroxypropyl methylcellulose is preferably poly(O-2-hydroxypropyl, O-methyl)cellulose (CAS number 9004-65-3).The hydroxyethyl methylcellulose is preferably 2-hydroxyethyl methylcellulose (CAS number 9032-42-2).
[0039] In the process according to the invention, the hydroxyalkylmethylcelluloses a) and b) can be added separately to the reaction. However, the hydroxyalkylcelluloses can be mixed first and then added to the reaction mixture, or the hydroxyalkylmethylcelluloses can be charged as a mixture first and the buffer substances, monomers, crosslinking agents, porogens and initiators are added. This can be done sequentially or as a mixture. It is preferred that the hydroxyalkylmethylcelluloses a) and b) are mixed first and charged first. It is then preferred to add the buffer substances. It is then preferred that the monoethylenic and polyethylenic compounds, porogens and initiators are added as a mixture to the hydroxyalkylmethylcelluloses.
[0040] In the process according to the invention, at least one monoethylenically unsaturated compound and at least one polyethylenically unsaturated compound are used.
[0041] However, it is also possible to use mixtures of two or more monoethylenically unsaturated compounds and mixtures of two or more polyethylenically unsaturated compounds.
[0042] Monoethylenically unsaturated compounds (monomers) for the purposes of the present invention are compounds having one free-radically polymerizable C=C double bond per molecule. Preferred compounds of this type include aromatic monoethylenically unsaturated compounds, such as vinyl and vinylidene derivatives of benzene and naphthalene, such as preferably vinylnaphthalene, vinyltoluene, ethylstyrene, α-methylstyrene, chlorostyrene, preferably styrene, and non-aromatic vinyl and vinylidene compounds, such as preferably acrylic acid, methacrylic acid, C1-C8-alkyl acrylates, C1-C8-alkyl methacrylates, acrylonitrile, methacrylonitrile, acrylamide, methacrylamide, vinyl chloride, vinylidene chloride and vinyl acetate. Non-aromatic monoethylenically unsaturated compounds are preferably used in smaller amounts, preferably 0.1% to 50% by weight, particularly preferably 0.5% to 20% by weight, based on the aromatic monoethylenically unsaturated compounds. It is preferred that only aromatic monoethylenically unsaturated compounds are used.
[0043] The monoethylenically unsaturated compound is preferably used in an amount of more than 50% by weight, based on the mixture of the monoethylenically unsaturated compound and the polyethylenically unsaturated compound, and particularly preferably in an amount of 80% to 98% by weight, based on the mixture of the monoethylenically unsaturated compound and the polyethylenically unsaturated compound.
[0044] For the purposes of the present invention, aromatic monoethylenically unsaturated compounds preferably used in the process according to the invention are styrene, vinyltoluene, ethylstyrene, α-methylstyrene, chlorostyrene or chloromethylstyrene.
[0045] It is particularly preferable to use styrene or a mixture of styrene with the abovementioned monomers, preferably ethylstyrene.
[0046] The polyethylenically unsaturated compound is a compound containing two or more, preferably two to four, free radically polymerizable C=C double bonds per molecule. Preferred aromatic polyethylenically unsaturated compounds are divinylbenzene, divinyltoluene, trivinylbenzene, divinylnaphthalene, triallyl cyanurate, triallyl isocyanurate, and trivinylnaphthalene. Preferred non-aromatic polyethylenically unsaturated compounds are diethylene glycol vinyl ether, octa-1,7-diene, hexa-1,5-diene, ethylene glycol dimethacrylate, triethylene glycol dimethacrylate, trimethylolpropane trimethacrylate, allyl methacrylate, and N,N'-methylenebisacrylamide. It is particularly preferred that the polyethylenically unsaturated compound used is divinylbenzene. For most applications, commercially available grades of divinylbenzene, which in addition to the isomers of divinylbenzene also contain ethylvinylbenzene, are sufficient.
[0047] For the purposes of the present invention, preferred polyethylenically unsaturated compounds in the process according to the invention are divinylbenzene, divinyltoluene, trivinylbenzene, divinylnaphthalene, triallyl cyanurate, triallyl isocyanurate or trivinylnaphthalene. It is particularly preferred to use divinylbenzene.
[0048] The polyethylenically unsaturated compound is preferably used in an amount of 1% to 20% by weight, particularly preferably 2% to 12% by weight, particularly preferably 4% to 10% by weight, based on the amount of the monoethylenically unsaturated compound. The type of polyethylenically unsaturated compound (crosslinker) is selected with reference to the subsequent use of the polymer.
[0049] The macroporous polymer is formed by adding at least one porogen to the monoethylenically unsaturated and polyethylenically unsaturated compounds in the polymerization to create a macroporous structure in the polymer. Particularly preferred porogens are hexane, octane, isooctane, isododecane, pentamethylheptane, methyl ethyl ketone, butanol or octanol and their isomers. Isododecane is very particularly preferred for use as a porogen. Particularly suitable are organic substances, such as aliphatic hydrocarbons, which dissolve in the monoethylenically unsaturated compounds but are poor solvents or poor swelling agents (precipitants for the polymer) for the polymer. The macroporous polymer is preferably prepared by polymerization at a concentration of 20 to 100 m. 2 The polymer has a BET surface area of 100 / g.
[0050] The porogen is preferably used in an amount of 25% to 45% by weight based on the amount of the organic phase.
[0051] The polymers prepared by the process according to the invention can be prepared in heterodisperse or monodisperse form.
[0052] The suspension polymerization on which the process is based preferably gives heterodisperse polymers.
[0053] The heterodisperse polymers are preferably prepared by the process according to the present invention.
[0054] Macroporous polystyrene-divinylbenzene copolymers are particularly preferably prepared by the preparation process described above.
[0055] The scope of the present invention encompasses all definitions of radicals, parameters and explanations detailed above and below and mentioned in general terms or within preferred ranges, including any combinations between each other, i.e. between the respective ranges and the preferred ranges.
[0056] In a preferred embodiment of the present invention, microencapsulated monomer droplets are preferably used for the preparation of monodisperse polymers in the process according to the present invention.
[0057] Materials useful for the microencapsulation of small droplets of monomers are those known for use as complex coacervates, particularly polyesters, natural and synthetic polyamides, polyurethanes, or polyureas.
[0058] It is preferred to use gelatin as a natural polyamide. It is used in particular as a coacervate and complex coacervate. For the purposes of the present invention, gelatin-containing complex coacervates are particularly understood to mean a combination of gelatin with a synthetic polyelectrolyte. Suitable synthetic polyelectrolytes are, for example, copolymers incorporating units of maleic acid, acrylic acid, methacrylic acid, acrylamide and methacrylamide. It is particularly preferred to use acrylic acid and acrylamide. Gelatin-containing capsules can be hardened using conventional hardeners, for example formaldehyde or glutardialdehyde. The encapsulation of monomer microdroplets with gelatin, gelatin-containing coacervates and gelatin-containing complex coacervates is described in detail in EP-A0 046 535. Methods of encapsulation with synthetic polymers are known. Interfacial condensation is preferred, in which a reactive component (especially an isocyanate or an acid chloride) dissolved in monomer microdroplets is reacted with a second reactive component (especially an amine) dissolved in an aqueous phase.
[0059] The heterodisperse or optionally microencapsulated, monodisperse monomer microdroplets preferably contain at least one initiator or a mixture of initiators (combination of initiators) that cause polymerization.Suitable initiators for the process according to the invention are peroxy compounds, particularly preferably dibenzoyl peroxide, dilauroyl peroxide, bis(p-chlorobenzoyl) peroxide, dicyclohexyl peroxydicarbonate, tert-butyl peroctoate, tert-butyl peroxy-2-ethylhexanoate, 2,5-bis(2-ethylhexanoylperoxy)-2,5-dimethylhexane or tert-amyl peroxy-2-ethylhexane, and azo compounds, such as 2,2'-azobis(isobutyronitrile) or 2,2'-azobis(2-methylisobutyronitrile).It is particularly preferred to use dibenzoyl peroxide as initiator. If a polymerization inhibitor is used, it is quite particularly preferable to use tert-butyl peroxy-2-ethylhexanoate as initiator.
[0060] The initiator is preferably used in an amount of 0.05% to 2.5% by weight, particularly preferably 0.1% to 1.5% by weight, based on the monomer mixture.
[0061] The optionally monodisperse microencapsulated monomer microdroplets may also optionally contain up to 30% by weight (based on monomer) of crosslinked or non-crosslinked polymers. Preferred polymers are those derived from the above-mentioned monomers, particularly preferably styrene.
[0062] In the preparation of monodisperse or heterodisperse polymers in the process according to the invention, the aqueous phase of a further preferred embodiment may contain dissolved polymerization inhibitors. Useful inhibitors in this case include both inorganic and organic substances. Preferred inorganic inhibitors include salts of transition metals, such as copper(II) chloride, copper(II) sulfate, iron(III) chloride, iron(II) sulfate, manganese(II) chloride, and inorganic nitrogen compounds, particularly preferably hydroxylamine, hydrazine, sodium nitrite and potassium nitrite, salts of phosphorous acid, such as sodium hydrogen phosphite, and also sulfur-containing compounds, such as sodium dithionite, sodium thiosulfate, sodium sulfite, sodium bisulfite, sodium thiocyanate and ammonium thiocyanate. Examples of organic inhibitors are phenolic compounds, such as hydroquinone, hydroquinone monomethyl ether, resorcinol, catechol, tert-butylcatechol, pyrogallol, and condensation products of phenols with aldehydes. Further suitable organic inhibitors are organic nitrogen-containing compounds. Particularly preferred are hydroxylamine derivatives, such as N,N-diethylhydroxylamine, N-isopropylhydroxylamine, and sulfonated or carboxylated N-alkylhydroxylamines or N,N-dialkylhydroxylamine derivatives, hydrazine derivatives, such as N,N-hydrazinodiacetic acid, nitroso compounds, such as preferably N-nitrosophenylhydroxylamine, N-nitrosophenylhydroxylamine ammonium salt or N-nitrosophenylhydroxylamine aluminum salt. The concentration of the inhibitors is preferably 5 to 1000 ppm, particularly preferably 10 to 500 ppm, very particularly preferably 10 to 250 ppm (based on the aqueous phase).
[0063] Preferably, in the process according to the invention, at least one polymerization inhibitor is used. Sodium nitrite or resorcinol are particularly preferred as inhibitors.
[0064] In addition to the dispersant mixture used in the process according to the invention, further dispersants may be added. Suitable additional dispersants are natural or synthetic water-soluble polymers, preferably gelatin, starch, polyvinyl alcohol, polyvinylpyrrolidone, polyacrylic acid, polymethacrylic acid, or copolymers of (meth)acrylic acid and (meth)acrylic acid esters. Gelatin is particularly preferred. The amount of additionally used dispersants is generally 0.05% to 10% by weight, preferably 0.05% to 5% by weight, based on the dispersant mixture of a) and b) used in the present invention. It is preferred not to add further dispersants in addition to the dispersant mixture used in the process according to the invention.
[0065] In an alternative preferred embodiment, the polymerization to obtain heterodisperse or monodisperse polymers can be carried out in the presence of a buffer system (buffer system). Buffer systems are preferred which allow the pH of the aqueous phase to be adjusted to a value between 14 and 6, preferably between 12 and 8, before the start of the polymerization. Under these conditions, the dispersants having carboxylic acid groups are present wholly or partly as salts. This has a favorable effect on the action of the dispersants. Particularly suitable buffer systems contain salts of phosphoric or boric acid. For the purposes of the present invention, "phosphates" and "borates" also encompass the condensates of the ortho-form of the corresponding acids and salts. The phosphates or concentrations in the aqueous phase are preferably between 0.5 and 500 mmol / L, particularly preferably between 2.5 and 100 mmol / L.
[0066] The stirring speed in the polymerization to obtain monodisperse polymers is not very important and does not affect the particle size in contrast to conventional polymerization. A low stirrer speed is used that is sufficient to keep the suspended monomer droplets in suspension and to facilitate the removal of the heat of polymerization. For this operation, various stirrer types can be used. A particularly suitable stirrer is the axially acting gate stirrer.
[0067] The volume ratio of the monomer microdroplets to the aqueous phase is preferably 1:0.75 to 1:20, particularly preferably 1:1 to 1:6. It is irrelevant whether heterodisperse or monodisperse polymers are prepared.
[0068] The polymerization temperature for obtaining heterodisperse or monodisperse polymers is determined by the decomposition temperature of the initiator used. It is preferably 50 to 180°C, particularly preferably 55 to 130°C. The polymerization is preferably continued for 0.5 to about 20 hours. It has been found to be useful to start the polymerization at a low temperature, preferably 60°C, and to use a temperature program in which the reaction temperature is increased as the polymerization conversion progresses. In this way, it is possible to achieve very effectively the requirements, for example a reliable reaction progress and a high polymerization conversion rate. After the polymerization reaction, the polymer is isolated by conventional methods, for example by filtration or decantation, and may be optionally washed.
[0069] The preparation of monodisperse polymers using the jet or seed-feed method is known in the prior art and is described, for example, in US-A 4 444 961, EP-A 0 046 535, US-A 4 419 245 or WO 93 / 12167.
[0070] Preferably, monodisperse polymers are prepared using the jet or seed-feed method.
[0071] Preferably, macroporous heterodisperse polymers are prepared by the process according to the invention.
[0072] The macroporous polymers are preferably used to prepare ion exchangers. They can be functionalized by known methods, for example by sulfonation, or chloromethylation, or phthalamidation, and reacted with alkylamines to give cation or anion exchangers and chelating resins.
[0073] The invention thus also relates to a method for preparing a macroporous polymer, a) at least one hydroxyalkyl methylcellulose having a molecular weight of 80,000 g / mol to 110,000 g / mol; b) at least one hydroxyalkyl methylcellulose having a molecular weight of 25,000 g / mol to 42,000 g / mol; The present invention also includes the use of a dispersant mixture comprising:
[0074] The invention further relates to the use of a macroporous polymer prepared with the dispersing agent mixture for the manufacture of an ion exchanger.
[0075] <Method> [Measurement of polymer fine particle fraction] To measure the polymer fine particle fraction, the reaction mixture containing the polymer and the aqueous phase was sieved through a sieve with a mesh size of 100 μm. The filtrate from this sieve was then fed to a 20 μm sieve. In this way, it became possible to fractionate and weigh the polymer fine particle fraction as a target particle of the 20-100 μm fraction. Any fine particle fraction and the aqueous phase remaining after the 20 μm sieve were evaporated and dried to a constant weight. The polymer fine particle fraction was then weighed and calculated as a percentage based on the polymer yield. EXAMPLES
[0076] Example 1 (according to the present invention) First, a glass reactor is charged with deionized water (869 mL) and 96.6 g of a 2 wt % aqueous solution of a) 2-hydroxypropyl methylcellulose (HPMC), CAS: 9004-65-3, average viscosity, 2% in water @ 20 ° C: 4550 mPas, methoxyl: 28.5 mol %, hydroxypropyl: 5.75 mol %, number average molecular weight: 95000 g / mol (Type A), and b) 2-hydroxypropyl methylcellulose (HPMC), CAS: 9004-65-3, average viscosity, 2% in water @ 20 ° C: 100 mPas, methoxyl: 21.5 mol %, hydroxypropyl: 9.5 mol %, number average molecular weight: 33500 g / mol (Type B) (weight ratio 1:1). Disodium hydrogen phosphate decahydrate (4.69 g, 0.48 wt % based on the aqueous phase) is further dissolved in the solution. The pH of the aqueous phase is then adjusted to 11 by adding NaOH (1M, 8-12 mL). A mixture of styrene (540.3 g, 80.4 wt%), divinylbenzene (5.5 wt%, 59.7 g), isododecane (351.5 g, 32 wt%), and dibenzoyl peroxide (BPO) (4.69 g, 0.43 wt%) (based on the organic phase) is added to the aqueous phase. A stream of nitrogen is introduced into the vessel at 20 L / h. The mixture is heated first to 73° C. at 190 rpm for 1 h, then held at this temperature for 7 h, then heated up to 95° C. over 1 h, held at this temperature again for 2 h, then cooled to room temperature. In this example, 559 g of polymer and 3.9 g of fine particle fraction were isolated.
[0077] Example 2 (according to the present invention) Example 1 is repeated, but using 3.23 g of tert-butylperoxy-2-ethylhexanoate (T21s) instead of the initiator benzoyl peroxide (BPO). In this example, 582 g of polymer and 5.7 g of fine particle fraction were isolated.
[0078] Example 3 (according to the present invention) Example 1 is repeated, but instead of the initiator benzoyl peroxide (BPO), 3.23 g of tert-butyl peroxy-2-ethylhexanoate (T21s) is used. In addition, resorcinol (c=0.08 g / L in aqueous phase) is added to the aqueous phase. In this example, 587 g of polymer and 3.1 g of fine particle fraction are isolated.
[0079] Example 4 (not according to the invention, without the low molecular weight dispersant component b) First, a glass reactor is charged with deionized water (869 mL) and 96.6 g of a 2 wt % aqueous solution of 2-hydroxypropylmethylcellulose (HPMC), CAS: 9004-65-3, average viscosity, 2% in water @ 20 °C: 4550 mPas, methoxyl: 28.5 mol %, hydroxypropyl: 5.75 mol %, number average molecular weight: 95000 g / mol (Type A). Disodium hydrogen phosphate decahydrate (4.69 g, 0.48 wt % based on aqueous phase) is further dissolved in the solution. The pH of the aqueous phase is then adjusted to 11 by adding NaOH (1 M, 8-12 mL). To the aqueous phase is added a mixture of styrene (540.3 g, 80.4 wt%), divinylbenzene (5.5 wt%, 59.7 g), isododecane (351.5 g, 32 wt%), and dibenzoyl peroxide (BPO) (4.69 g, 0.43 wt%) (based on the organic phase). A stream of nitrogen is introduced into the vessel at 20 L / h. The mixture is heated first to 73° C. at 190 rpm for 1 hour, then held at this temperature for 7 hours, then heated over 1 hour up to 95° C., again held at this temperature for 2 hours, then cooled to room temperature. In this example, 569 g of polymer and 6.9 g of fine particle fraction are isolated.
[0080] Example 5 (not according to the invention, without the low molecular weight dispersant component b) and with the initiator of Example 2 of EP-A-0964002) Example 4 is repeated, but using 3.23 g of tert-butylperoxy-2-ethylhexanoate (T21s) instead of the initiator benzoyl peroxide (BPO). In this example, 522 g of polymer and 10.2 g of fine particle fraction were isolated.
[0081] Example 6 (not according to the invention, without the use of high molecular weight dispersant component a) Example 4 was repeated, but using the same weight of the following instead of Type A: 2-hydroxypropylmethylcellulose (HPMC), CAS: 9004-65-3, average viscosity, 2% in water @ 20°C: 100 mPas, methoxyl: 21.5 mol%, hydroxypropyl: 9.5 mol%, number average molecular weight: 33500 g / mol (Type B) (weight ratio of Type A to Type B: 1:1). In this example, 574 g of polymer and 7.8 g of fine particle fraction were isolated.
[0082] Example 7 (not according to the invention, without the use of the high molecular weight dispersant component a) and with the initiator of Example 2 of EP-A-0964002) Repeat Example 4, but use the same weight of the following instead of Type A: 2-hydroxypropylmethylcellulose (HPMC), CAS: 9004-65-3, average viscosity, 2% in water @ 20°C: 100 mPas, methoxyl: 21.5 mol%, hydroxypropyl: 9.5 mol%), number average molecular weight: 33500 g / mol (Type B). In addition, replace the initiator BPO with 3.23 g of tert-butylperoxy-2-ethylhexanoate (T21s). In this example, 570 g of polymer and 9.8 g of fine particle fraction were isolated.
[0083] Example 8 (not according to the invention, but comparative example 1 of EP-A-0964002, using resorcinol instead of sodium nitrite as inhibitor) First, a glass reactor is charged with deionized water (869 mL) and 96.6 g of a 2 wt. % aqueous solution of methylcellulose (average viscosity 4000 mPas, Sigma Aldrich). Disodium hydrogen phosphate decahydrate (4.69 g, 0.48 wt. % based on the aqueous phase) and resorcinol (c=0.08 g / L in the aqueous phase) are further dissolved in this solution. The pH of the aqueous phase is then adjusted to 11 by adding NaOH (1 M, 8-12 mL). A mixture of styrene (540.3 g, 80.4 wt. %), divinylbenzene (5.5 wt. %, 59.7 g), isododecane (351.5 g, 32 wt. %) and dibenzoyl peroxide (BPO) (4.69 g, 0.43 wt. %) (based on the organic phase) is added to the aqueous phase. A stream of nitrogen is introduced into the vessel at 20 L / h. The mixture is heated first to 73°C at 190 rpm for 1 hour, then held at this temperature for 7 hours, then heated up to 95°C over 1 hour, held at this temperature again for 2 hours, then cooled to room temperature. In this example, 569 g of polymer and 7.2 g of fine particle fraction were isolated.
[0084] Example 9 (according to the present invention) Example 1 is repeated, but now, instead of the mixture of types A and B, the same weight of a mixture of hydroxyethyl methylcellulose (methoxy substitution degree: 28.5 mol %, hydroxyethoxy substitution degree: 10 mol %, number average molecular weight: 95000 g / mol) and 2-hydroxypropyl methylcellulose (HPMC) (CAS: 9004-65-3, average viscosity, 2% in water @ 20 ° C: 100 mPas, methoxyl: 21.5 mol %, hydroxypropyl: 9.5 mol %, number average molecular weight: 33500 g / mol (type B)) is used as dispersant (1:1 weight ratio). Additional resorcinol (0.08 g / L) is added to the reaction mixture. In this example, 582 g of bead polymer and 5.7 g of fine particle fraction were isolated.
[0085] [Table 1]
[0086] Examples 1 to 3 and 9 according to the invention show that by using a dispersant mixture containing a particular hydroxyalkylmethylcellulose, the polymer fines fraction can be surprisingly reduced in the preparation of a polymer.
Claims
1. A method for producing a polymer, comprising: reacting at least one monoethylenically unsaturated compound and at least one polyethylenically unsaturated compound in the presence of at least one initiator, in the presence of water, in the presence of a porogen, and a) at least one hydroxyalkyl methylcellulose having a number average molecular weight of 80,000 g / mol to 110,000 g / mol and mixtures of these compounds, and b) at least one hydroxyalkylmethylcellulose having a number average molecular weight of 25,000 g / mol to 42,000 g / mol and mixtures of these compounds reacting in the presence of a dispersant mixture comprising:
2. 2. The method for producing a polymer according to claim 1, characterized in that the hydroxyalkyl methylcellulose in a) and b) is selected from the group of 2-hydroxypropyl methylcellulose or hydroxyethyl methylcellulose and mixtures of these compounds.
3. 3. The method for producing a polymer according to claim 1, wherein the initiator used is dibenzoyl peroxide, dilauroyl peroxide, bis(p-chlorobenzoyl)peroxide, dicyclohexylperoxydicarbonate, tert-butylperoctoate, tert-butylperoxy-2-ethylhexanoate, 2,5-bis(2-ethylhexanoylperoxy)-2,5-dimethylhexane or tert-amylperoxy-2-ethylhexane, 2,2'-azobis(isobutyronitrile) or 2,2'-azobis(2-methylisobutyronitrile), or a mixture of these initiators.
4. 4. The process for producing a polymer according to claim 1, wherein the monoethylenically unsaturated compound used is styrene, vinyltoluene, ethylstyrene, α-methylstyrene, chlorostyrene, or chloromethylstyrene, or a mixture of these compounds.
5. 5. The process for producing a polymer according to claim 1, wherein the polyethylenically unsaturated compound used is divinylbenzene, divinyltoluene, trivinylbenzene, divinylnaphthalene, or trivinylnaphthalene, or a mixture of these compounds.
6. 6. The method for producing a polymer according to claim 1, wherein the monoethylenically unsaturated compound used is styrene and the polyethylenically unsaturated compound used is divinylbenzene.
7. 7. A process for the preparation of a polymer according to claim 1, characterized in that the pH of the aqueous phase before polymerization is adjusted to a value between 12 and 8.
8. 8. A process for producing a polymer according to claim 1, wherein the component a) used is 2-hydroxypropyl methylcellulose having a degree of 2-hydroxypropyl substitution of 3 to 15 mol % and a degree of methoxy substitution of 26 to 31 mol %.
9. 9. A process for producing a polymer according to claim 1, wherein the component b) used is 2-hydroxypropylmethylcellulose having a degree of hydroxypropyl substitution of 3 to 15 mol % and a degree of methoxy substitution of 18 to 25 mol %.
10. 10. A method for producing a polymer according to any one of claims 1 to 9, characterized in that the weight ratio of the hydroxyalkyl methylcellulose a) and b) is from 3:1 to 1:
1.
11. 11. A method for producing a polymer according to any one of claims 1 to 10, characterized in that the total combined concentration of the hydroxyalkyl methylcelluloses a) and b) is 0.15 to 0.3% by weight, based on the aqueous phase.
12. 12. Process for the preparation of polymers according to any one of claims 1 to 11, characterized in that an inhibitor is used, which is in particular selected from the group of sodium dithionite, sodium thiosulfate, sodium sulfite, sodium bisulfite, sodium thiocyanate, ammonium thiocyanate, hydroquinone, hydroquinone monomethyl ether, resorcinol, catechol, tert-butylcatechol or pyrogallol.
13. 13. Process for the preparation of polymers according to any one of claims 1 to 12, characterized in that a porogen is used, which is in particular selected from the group of hexane, octane, isooctane, isododecane, methyl ethyl ketone, methyl isobutyl ketone, methyl isobutyl carbinol or octanol.
14. A process for the preparation of a polymer according to any one of claims 1 to 13, characterized in that the polymerization is carried out at a temperature of from 55 to 130°C.
15. For producing macroporous polymers, a) at least one hydroxyalkyl methylcellulose having a number average molecular weight of 80,000 g / mol to 110,000 g / mol, and b) at least one hydroxyalkyl methylcellulose having a number average molecular weight of 25,000 g / mol to 42,000 g / mol; Use of a dispersant mixture comprising:
16. 16. The use according to claim 15, wherein the preparation of macroporous polymers concerns polystyrene-divinylbenzene copolymers.
17. 17. The use according to claim 15 or 16, wherein the polymer is used as a base material for producing an ion exchanger.
Citation Information
Patent Citations
Production of bulky high density vinyl resin
JP1987000504A
Method for producing monodisperse polymer particles
JP2002542318A
Manufacturing method of monodisperse gel-type ion exchanger
JP2005535778A
Process for preparing cross-linked spherical beads
EP0964002A1
Cited By
Power transmission device
JP2026149826A